Process of preparing filter material for reducing fluoride content and improving water quality
A preparation process and filter material technology, which are applied in the field of filter material preparation technology for reducing fluoride and changing water, can solve the problems of difficulty in effectively achieving the purpose of reducing fluoride and changing water, high process cost, unsatisfactory effect, etc., and are convenient for popularization, application and processing. Simple process, obvious effect
Patent Information
- Authority / Receiving Office
- CN · China
- Current Assignee / Owner
- Publication Date
- 2007-12-19
- Estimated Expiration
- Not applicable · inactive patent
Abstract
Description
technical field
[0001] The invention relates to a filter material for reducing the fluorine content in water, in particular to a preparation process of the filter material for improving water by reducing fluorine. Background technique
[0002] Fluorine is a relatively active physiological element in the human body, which can inhibit or stimulate the activity of certain enzymes. Most fluoride exists in hard tissues, but excessive fluoride can cause fluorosis. Endemic fluorosis is a chronic poisoning disease caused by people living in this environment under the influence of specific geological and geographical conditions in fluorine-rich areas and drinking water for a long time that exceeds the physiological requirement. Clinically, the main manifestations are dental fluorosis and skeletal fluorosis, which are endemic diseases that seriously endanger human health. Therefore, high fluoride water needs to be defluoridated.
[0003] At present, the commonly used methods of redu...
Examples
Embodiment Construction
[0041] The present invention will be further described below in conjunction with embodiment.
[0042] A kind of filter material preparation process that is used to reduce fluoride to improve water, its step is,
[0043] (1) It uses natural zeolite as raw material, after being selected, it is crushed to 5-8 mesh;
[0044] (2) Carry out high-temperature roasting of crushed raw materials at a temperature of 900-1000° C. for 3-4 hours, preferably at a temperature of 950° C. and for 3 hours; carry out high-temperature roasting of selected natural zeolite raw materials , the purpose of which is to remove the organic substances in the pores and channels of the zeolite, etc., and control the roasting conditions and time to maximize the adsorption capacity of the zeolite to water after roasting.
[0045] (3) put into the hydrochloric acid of 30% concentration after being put into after roasting for 18-24 hours, carry out acid treatment, preferably 20 hours; It reaches the following pu...