Preparation method for improving bulk density of dialkyl phosphinate

A technology of dialkyl phosphinate and alkyl phosphinate is applied in the field of preparation of increasing the bulk density of dialkyl phosphinate, which can solve the problems of time-consuming, labor-intensive, unfavorable resin molding and processing, and achieve high density. , excellent mechanical properties and flame retardant properties, the effect of small dust

CN103172671AInactive Publication Date: 2013-06-26ZHUHAI WANTONG CHEM
11 Cites 3 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Publication Date
2013-06-26
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 1
    Figure 1
  • Figure 2
    Figure 2
Patent Text Reader

Abstract

The invention discloses a preparation method for improving bulk density of dialkyl phosphinate. The preparation method comprises the following steps: (a), uniformly wetting dialkyl phosphinate by an aqueous solution of volatile acid and / or low-boiling point acid to obtain dialkyl phosphinate-acid turbid liquid; (b), carrying out solid-liquid separation and drying onto to the dialkyl phosphinate-acid turbid liquid to obtain dialkyl phosphinate with improved bulk density, wherein the volatile acid and / or low-boiling point acid is one or more of formic acid, acetic acid, hydrofluoric acid, hydrochloric acid, hydrobromic acid, hydroiodic acid and sulphurous acid. The bulk density of dialkyl phosphinate obtained by the preparation method disclosed by the invention is greatly improved, the loose bulk density is 0.50g / cm<3>-0.70g / cm<3> and the vibration bulk density is 0.60g / cm<3>-0.90g / cm<3>. The preparation method disclosed by the invention is simple and easy to implement, gentle in treatment conditions and pure in product. Besides, obtained high-bulk density dialkyl phosphinate is small in dust content, large in density, capable of effectively reducing the packaging cost and excellent in mechanical performances and flame resistance in modifying high polymer materials including plastics, chemical fibers and the like.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to a preparation method for improving the packing density of dialkyl phosphinate. Background technique

[0002] Dialkylphosphinate is an environmentally friendly flame retardant, which is widely used in polymer materials such as plastics and chemical fibers. As early as the late 1970s and early 1980s, the Pennwalt Company of the United States had tested the properties of various dialkylphosphinates. American Ticona Company has successively studied the performance of zinc / aluminum / calcium phosphinate as flame retardant in PA~NPBT. In recent years, the German Clariant company has devoted itself to the research and development of this new phosphorus-based flame retardant. And established a pilot production line in 2004, developed two metal phosphinate flame retardants added with nitrogen synergist, brand name Exolit OP l311 IIIExolit OP l312, these two flame retardants are mainly used in PA6 and PA66 It achieves a better comprehen...

Examples

Embodiment 1

[0033] At a temperature of 30°C, take 500g of formic acid aqueous solution with a mass concentration of 90%, add it to a stirred reactor, and then add 500g of it to a loose bulk density of 0.22g / cm 3 , the tapped bulk density is 0.45g / cm 3 Diethylphosphinate aluminum salt, slowly stirred until the aluminum diethylphosphinate is evenly wetted, and kept at a constant temperature of 30°C for 30min, and finally the suspension in the reactor was separated from solid and liquid, dried to obtain diethylphosphinate Aluminum salt of phosphonic acid 499.6 g; the loose bulk density of the product obtained is 0.64 g / cm 3 , the tapped bulk density is 0.81g / cm3;

[0034] IR: 778cm-1, 1060cm-1, 1108cm-1, 2882cm-1, 2959cm-1.

Embodiment 2

[0036] At a temperature of 30°C, take 500g of formic acid aqueous solution with a mass concentration of 90%, add it to a stirred reactor, and then add 500g of it to a loose bulk density of 0.22 g / cm 3 , the tapped bulk density is 0.45g / cm 3 Diethylphosphinate aluminum salt, slowly stirred until the aluminum diethylphosphinate is uniformly wetted, and left to stand at a constant temperature of 60°C for 30min, and finally the suspension in the reactor was separated from solid and liquid, and dried to obtain diethylphosphinate Aluminum phosphinate 491.3g; The loose bulk density of the product obtained is 0.68g / cm3, and the tapped bulk density is 0.86g / cm3;

[0037] IR: 778cm-1, 1060cm-1, 1108cm-1, 2882cm-1, 2959cm-1.

Embodiment 3

[0039] At a temperature of 30°C, take 500g of formic acid aqueous solution with a mass concentration of 90%, put it into a stirred reactor, and then add 500g of diethyl ether with a loose bulk density of 0.22g / cm3 and a tapped bulk density of 0.45g / cm3 Diethylphosphinic acid zinc salt, slowly stirred until diethylphosphinic acid zinc is evenly wetted, 90 ℃ constant temperature for 30min, finally the suspension in the reactor was separated from solid and liquid, dried to obtain diethylphosphinic acid zinc Salt 499.5g; The loose bulk density of gained product is 0.69g / cm3, and tapped bulk density is 0.89 g / cm3;

[0040] IR: 778cm-1, 1060cm-1, 1108cm-1, 2882cm-1, 2959cm-1.