A flexible gear and manufacturing equipment and manufacturing method thereof
The method of molding molten amorphous alloy through molds solves the problems of high cost and low production efficiency in flexible gear manufacturing, and realizes amorphous alloy flexible gears with high strength, low elastic modulus and corrosion resistance, which are suitable for high-precision applications. and high-load transmission applications.
Patent Information
- Application Number
- CN201810300931.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-04-04
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2038-04-04
AI Technical Summary
Existing flexible gear manufacturing technology has problems such as high processing costs, complex processes, and difficulty in rapid mass production. In particular, high-performance alloy steel and plastic materials perform poorly in high-precision and high-load transmission processes.
The mold is used to perform flexible gear molding on molten amorphous alloy, and the detachable mold core and runner system design are used to achieve an efficient and precise molding process through the mold device, which reduces manufacturing costs and improves production efficiency.
It achieves the high strength, low elastic modulus, excellent fatigue resistance and corrosion resistance of amorphous alloy flexible gears, improves production efficiency and precision, reduces manufacturing costs, and is suitable for high-precision and high-load transmission processes.
Smart Images

Figure CN108361352B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of flexible gear manufacturing, and in particular relates to a flexible gear and a manufacturing device and a manufacturing method thereof. Background Art
[0002] Harmonic drive is an important new type of mechanical transmission that emerged in the late 1950s with the development of aerospace technology. It has the advantages of high motion accuracy, small backlash, large transmission ratio, light weight, small size, large load-bearing capacity, and can work normally in sealed space and radiation medium. Its most widely used application is harmonic reducer, and its core component is flexible gear. During the operation of harmonic reducer, the flexible gear follows the harmonic generator bearing and continuously undergoes elliptical deformation. At the same time, the teeth of the flexible gear and the teeth of the steel wheel continuously undergo a reciprocating cycle of meshing, meshing, meshing out, disengaging and then meshing in. The stress of the cylinder wall of the flexible gear is the superposition of the stress caused by the deformation of the flexible gear and the stress caused by the external load. Among them, the stress caused by elastic deformation is proportional to the elastic modulus E, and the elastic modulus E of high-performance alloy steel is very large, so a large part of the material's fatigue resistance is used to overcome elastic deformation. In this way, the external load capacity of the flexible gear must be small. At present, the main materials for making flexible gears are high-performance alloy steel and plastic. Among them, high-performance alloy steel (such as 30CrMnSi) has high mechanical strength, high elasticity and toughness; however, its elastic modulus E is high, resulting in greater stress on deformation. At the same time, since the rim of the flexible gear is extremely thin, it is easy to deform during processing. Special tools and equipment are required during the manufacturing process, and heat treatment must also be performed, resulting in complex processing technology, difficult manufacturing, high processing costs, and expensive small batch production. Plastic flexible gears (such as nylon 66) have low elastic modulus, good elasticity, less stress during deformation, good corrosion resistance, certain self-lubricating properties, and can be processed through mold injection molding at a low cost. However, its mechanical strength is low and it cannot be used in high-precision and high-load transmission processes.
[0003] The invention patent with application number 201480079552.4, "System and method for realizing bulk metallic glass-based strain wave gears and strain gear components", introduces a system and method for manufacturing flexible gears using bulk metallic glass (amorphous alloy). Bulk metallic glass has high strength, low elastic modulus E, excellent fatigue resistance, large elastic limit and good corrosion resistance, and is a material that is very suitable for the use conditions of flexible gears. In the above-mentioned prior art process method, bulk metallic glass can be produced by casting and thermoplastic molding, and then produced by machining, and no heat treatment is required. However, this method still requires special production tools such as special molds and rollers. There are still problems of high processing costs and difficulty in rapid mass production. Summary of the invention
[0004] In order to solve the deficiencies of the prior art, the present invention provides a flexible gear manufacturing device and method thereof. The flexible gear is an amorphous alloy flexible gear. The amorphous alloy flexible gear has good strength, low elastic modulus, excellent fatigue resistance, large elastic limit and good corrosion resistance. The flexible gear is formed by molding the molten amorphous alloy with a mold, which has high production efficiency and high precision of the flexible gear. The mold core of the mold is detachable, and mold cores with a large degree of wear can be replaced. Mold cores of different models can also be replaced, which reduces manufacturing costs. The front mold core is provided with tooth grooves that can form the teeth of the flexible gear, so that the flexible gear can be formed in one piece, and there is no need to process the teeth of the gear separately.
[0005] The technical effects to be achieved by the present invention are achieved through the following solutions:
[0006] A flexible gear is an amorphous alloy flexible gear. The amorphous alloy flexible gear has good strength, low elastic modulus, excellent fatigue resistance, large elastic limit and good corrosion resistance.
[0007] Furthermore, the stiffness value of a single tooth of the flexible gear is 50-80 N / m, so that the gear can withstand torsional force and extrusion force without tooth collapse during rotation.
[0008] Furthermore, the thickness of the flexible gear is 0.5-5 mm. The flexible gear within this thickness range has both good flexibility and sufficient rigidity to withstand pressure.
[0009] A flexible gear manufacturing device, the manufacturing device comprises a mold device, the mold device comprises a front mold and a rear mold, the front mold is provided with a mold frame;
[0010] The mold frame is provided with a detachable front mold core, the number of the front mold cores is 1-20, the front mold core forms a mold core inner cavity in the mold frame, and the inner side of the mold core inner cavity formed by the front mold core is provided with a tooth groove for forming the teeth of the flexible gear; the rear mold is provided with a detachable rear mold core, and after the front mold and the rear mold are closed, the front mold core and the rear mold core form a closed mold cavity.
[0011] During the EDM or CNC processing of the front mold core, due to the irregular shape of the mold core cavity, the number of processed tooth grooves is large, and the tooth grooves are surrounded by a circle, it is difficult for EDM or CNC to process the tooth grooves, or it is difficult to process high-precision tooth grooves. The mold core cavity is not directly formed by a single front mold core, but is formed by a combination of multiple front mold cores. The number of front mold cores is 1-20. On the one hand, it can reduce the processing difficulty of the front mold core and facilitate the processing of the front mold core tooth grooves. On the other hand, it can improve the accuracy of the front mold core tooth grooves and produce more accurate flexible gears.
[0012] The flexible gear manufactured by the mold has high dimensional accuracy, high production speed of the flexible gear, and can reduce the production cost of the flexible gear.
[0013] Furthermore, the hardness of the front and rear mold cores is 45-55HRC.
[0014] Furthermore, the mold device is provided with a stripper plate, the front mold is provided with a branch runner, the stripper plate is provided with a runner groove, and after closing with the front mold, a main runner is formed inside, and the main runner and the branch runner form a runner system. During the forming process of the amorphous alloy flexible gear, the molten amorphous alloy in the runner system will cool to become a sprue material, and when the mold is opened to take out the flexible gear molded part, the sprue material in the runner system is ejected by the ejector pin. The design of the runner system makes it easier for the sprue material to be ejected by the ejector pin of the mold device without affecting the molded part.
[0015] Furthermore, the cross-sections of the main channel and the branch channel are circular, the diameter of the main channel is 2-20 mm, and the diameter of the branch channel is 0.8-10 mm.
[0016] Furthermore, the branch channel is provided with a point gate, and one mold cavity of the mold device is provided with 1-20 point gates for feeding. The uneven feeding of the mold cavity during the molding of the flexible gear will cause large differences in pressure and temperature at different positions of the cavity, and the flexible gear will shrink to different degrees at different positions after cooling, resulting in low precision of the molded flexible gear. The mold cavity has more than one point gate for feeding, and the point gates are evenly distributed on the same surface of the mold cavity.
[0017] The method for manufacturing a flexible gear using the manufacturing equipment comprises the following steps:
[0018] S01: pouring amorphous alloy as raw material into a smelting chamber;
[0019] S02: The clamping mechanism drives the front mold and the rear mold to close to form a closed mold cavity;
[0020] S03: The vacuum exhaust device evacuates the smelting chamber and the mold cavity so that the air pressure in the smelting chamber and the mold cavity reaches the set value;
[0021] S04: heating the raw materials in the smelting chamber to make the raw materials completely molten, wherein the heating temperature is 400-500° C. higher than the melting point of the amorphous alloy;
[0022] S05: the driving device drives the injection rod to inject the molten raw material in the smelting chamber, the mold cavity is filled, and the injection rod stops injecting;
[0023] S06: The flexible gear is formed in the mold cavity, and the driving device drives the front mold to separate from the rear mold to take out the flexible gear.
[0024] Furthermore, the injection speed of the injection rod is 0.1-20 m / s, and the filling speed in the mold cavity is 0.1-30 m / s.
[0025] The above method is used to manufacture flexible gears, with a high production speed, and the strength, elastic modulus, fatigue resistance, elastic limit and corrosion resistance of the flexible gears are greatly improved.
[0026] The present invention has the following advantages:
[0027] 1. Amorphous alloy flexible gears have good strength, low elastic modulus, excellent fatigue resistance, large elastic limit and good corrosion resistance.
[0028] 2. Use molds to mold molten amorphous alloy into flexible gears, which has high production efficiency and high precision of flexible gears.
[0029] 3. The mold core is detachable, and mold cores with a large degree of wear can be replaced. Mold cores of different models can also be replaced. The same set of molds can manufacture various types of flexible gears, reducing manufacturing costs.
[0030] 4. The front mold core is provided with tooth grooves for forming the teeth of the flexible gear, so that the flexible gear can be formed in one piece, and there is no need to process the teeth of the gear separately, which reduces the manufacturing time of the flexible gear and reduces the manufacturing cost of the flexible gear.
[0031] 5. The front mold core forms a mold core cavity in the mold frame. The number of front mold cores is 1-20. The mold core cavity is not directly formed by processing a single front mold core, which can reduce the processing difficulty of the front mold core, facilitate the processing of the front mold core tooth groove, and improve the accuracy of the front mold core tooth groove to manufacture more accurate flexible gears. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 It is a structural schematic diagram of the flexible gear manufacturing equipment in the present invention;
[0033] Figure 2 It is a structural schematic diagram of the front mold core in the present invention;
[0034] Figure 3 This is a schematic diagram of the structure of the front mold core forming the mold core inner cavity in the present invention:
[0035] Figure 4 It is a structural schematic diagram of the rear mold core in the present invention;
[0036] Figure 5 A schematic diagram of the structure of the flow channel system in the present invention;
[0037] Explanation of the symbols in the accompanying drawings: 1. mold device; 2. injection device; 3. melting device; 4. vacuum device; 11. front mold; 12. rear mold; 13. stripper plate; 111. front mold core; 112. mold cavity; 121. rear mold core; 131. runner system; 21. injection barrel wall; 22. injection rod; 23. driving device; 31. melting chamber; 32. feeding funnel; 41. vacuum pump; 42. vacuum connecting pipe; 1112. mold core cavity; 1113. tooth groove; 1311. main flow channel; 1312. branch flow channel; 100. point gate. DETAILED DESCRIPTION
[0038] The following is combined with Figure 1-5 The embodiments of the present invention are described in detail, and examples of the embodiments are shown in the accompanying drawings, wherein the same reference numerals throughout represent the same elements. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to explain the present invention, but should not be construed as limiting the present invention.
[0039] As attached Figure 1 As shown, the flexible gear manufacturing device of the present invention comprises a mold device 1, which comprises a front mold 11 and a rear mold 12. The front mold is provided with a mold frame (not shown in the figure), and a detachable front mold core 111 is provided in the mold frame. The number of front mold cores in one mold frame is 1-20. Figure 2-3 As shown, the front mold core forms a mold core cavity 1112 in the mold frame, and a tooth groove 1113 is provided on the inner side of the mold core cavity formed by the front mold core for forming the teeth of the flexible gear; the rear mold is provided with a detachable rear mold core 121, and after the front mold and the rear mold are closed, the front mold core and the rear mold core form a closed mold cavity 112.
[0040] In the present invention, the flexible gear is an amorphous alloy flexible gear. The flexible gear is a thin-walled shell structure, has a certain flexibility in the radial direction, and has a certain rigidity in the torsional direction. The flexibility of the flexible gear is relative to the rigid gear that cooperates with it. The flexible gear is deformed by the force during the rotation process. The flexible gear can withstand both a certain torsional force and a certain extrusion force during the rotation of the gear, so the flexible gear is required to have a certain rigidity. In the present invention, the rigidity of a single tooth of the flexible gear is preferably 50-80N / m. The flexible gear within this range can withstand a certain torsional force and extrusion force without tooth collapse during the rotation of the gear.
[0041] The thickness of the flexible gear is 0.5-5mm. When the thickness of the tube wall of the flexible gear is too thick, the flexibility of the flexible gear is too low and the deformation effect cannot be achieved; when the thickness of the flexible gear is too thin, the rigidity value of the flexible gear is too small and it cannot withstand the torsion and extrusion force during rotation. Within the above thickness range, the flexible gear has good flexibility and sufficient rigidity. It can not only undergo elastic deformation, but also withstand a certain torsion force to drive the rigid gear to rotate. The thickness of the flexible gear is uniform, and the difference in rigidity values at each position is small, which avoids cracking during rotation due to the rigidity value of a certain place of the flexible gear being too small.
[0042] When the flexible gear rotates with other parts, the teeth play a role of meshing and transmission. Since the precision requirements of the flexible gear are relatively high, tooth processing is one of the main technologies for flexible gear processing. The present invention is no exception, and the technology of flexible gear teeth is also one of the main manufacturing technologies. The diameter of one side of the flexible gear with the gear is slightly larger than the diameter of other places, so the inner cavity shape of the mold core used for forming the front mold core needs to be slightly larger on one side. During the EDM or CNC processing of the front mold core, due to the irregular shape of its mold core cavity, the number of processed tooth grooves is large, and the tooth grooves are surrounded by a circle, it is difficult for EDM or CNC to process the tooth grooves, or it is difficult to process high-precision tooth grooves. The mold core cavity is not directly formed by processing a single front mold core, but is formed by combining multiple front mold cores to form the mold core cavity. Preferably, the number of front mold cores is 1-20. On the one hand, it can reduce the processing difficulty of the front mold core and facilitate the processing of the front mold core tooth grooves. On the other hand, it can improve the accuracy of the front mold core tooth grooves and produce flexible gears with higher precision. As shown in the attached Figure 2 As shown, the number of front mold cores in this embodiment is 2, and the shapes and sizes of the two front mold cores are the same. Similarly, when the number of front mold cores is 3 or other numbers, the shapes and sizes of the front mold cores are the same. When the shapes and sizes of the front mold cores are the same, the processing can be batched, the cost is reduced, and the process of mold assembly is simple.
[0043] The rear mold 12 is provided with a rear mold core 121. It should be noted that the rear mold does not necessarily have a mold frame. It can be provided with a mold frame and assembled with the rear mold core, or the rear mold core can be directly assembled on the rear mold. In this embodiment, the rear mold is not provided with a mold frame, and the rear mold core is directly assembled on the rear mold. In order to facilitate the ejector pin to eject the formed flexible gear from the mold, as shown in the attached Figure 4As shown, the rear mold core is only a simple cylindrical shape, and when the formed flexible gear is ejected from the mold, the side with a larger diameter is pushed out of the mold core cavity first. The front and rear mold cores are detachably installed on the front and rear molds, that is, the front and rear mold cores are replaceable. When the front mold core or the rear mold core is severely worn, the severely worn front mold core or rear mold core can be replaced to ensure the accuracy of the flexible gear; or when the production volume of one type of flexible gear reaches a certain quantity and another type of flexible gear needs to be produced, the front mold core can be replaced with another type of front mold core. The detachable assembly structure of the front and rear mold cores and the mold is a prior art, and is not described in detail in this example, but is not limited in the present invention. It is sufficient that the disassembly structure can achieve the technical purpose of the present invention.
[0044] The front mold core forms a mold core cavity in the mold frame. When the rear mold and the front mold are closed, the rear mold core on the rear mold enters the mold core cavity. There is a gap between the rear mold core and the front mold core, and this gap forms the mold cavity.
[0045] The mold core is made of steel, which has good tensile strength, good impact toughness, is not easy to wear, and is easy to process. As a mold core material, it can better ensure the accuracy of the molded product. Furthermore, the hardness of the steel is preferably 45-55HRC.
[0046] The mold device is also provided with a stripper plate 13, and the front mold is also provided with a branch channel 1312. The stripper plate 13 is provided with a flow channel groove (not marked in the figure), which forms a main flow channel after closing with the front mold. Figure 5 As shown, the main channel 1311 and the branch channel 1312 form a flow channel system 131. The cross-sections of the main channel and the branch channel are circular. According to the flow channel system technology of the mold, the diameter of the main channel is designed to be 2-20 mm, and the diameter of the branch channel is designed to be 0.8-10 mm. The branch channel is provided with a point gate 100, and a mold cavity of the mold device is provided with 1-20 point gates for feeding. Uneven feeding of the mold cavity during flexible gear molding will cause large differences in pressure and temperature at different cavity positions, and the degree of shrinkage of different positions of the flexible gear after cooling is different, resulting in low precision of the molded flexible gear. In order to avoid the above situation, in the present invention, one mold cavity has more than one point gate for feeding. Preferably, one mold cavity is provided with 1-20 point gates for feeding, and the point gates are evenly distributed on the same surface of the mold cavity. During the molding process of amorphous alloy flexible gears, the molten amorphous alloy in the runner system will cool down to become sprue material. When the mold is opened to take out the flexible gear molded part, the sprue material in the runner system is ejected by the ejector pin. The design of the runner system makes it easier for the sprue material to be ejected by the ejector pin of the mold device without affecting the molded part.
[0047] The flexible gear manufacturing equipment also includes a melting device 3, an injection device 2 and a vacuum device 4. The melting device includes a melting bin 31 and a feed hopper 32, and the feed hopper is arranged at the upper end of the melting bin; a heating coil (not marked in the figure) is arranged on the inner side of the melting bin, and a valve (not marked in the figure) is arranged at the bottom of the feed hopper for controlling the feeding speed. The injection device includes an injection barrel wall 21, an injection rod 22 and a driving device 23 for driving the injection rod to move in the direction of the inner wall of the injection barrel wall. The vacuum device is connected to the mold device and the melting bin, and vacuums the mold cavity and the melting bin to control the air pressure in the mold cavity and the melting bin. The vacuum device includes a vacuum pump 41 and a vacuum connecting pipe 42. The driving device of the injection rod is one of a cylinder, a hydraulic cylinder or a motor. In this embodiment, the driving device is a cylinder.
[0048] The method for manufacturing a flexible gear using the above manufacturing equipment comprises the following steps:
[0049] S01: Pour the amorphous alloy as raw material into a smelting chamber.
[0050] S02: The clamping mechanism drives the front mold and the rear mold to close to form a closed mold cavity.
[0051] The order of step S01 and step S02 can be interchanged, and the order of these two steps does not affect the manufacture of the flexible gear.
[0052] S03: The vacuum exhaust device evacuates the melting chamber and the mold cavity to make the air pressure in the melting chamber and the mold cavity reach the set value. The air pressure setting value is 1×10 -5 -5×10 2 Pa. The setting of air pressure value ensures the pressure maintenance of flexible gear during the forming process.
[0053] S04: The raw materials are heated in the smelting chamber to completely melt the raw materials. The heating temperature is 400-500°C higher than the melting point of the amorphous alloy. The amorphous alloy can only be melted when the heating temperature is higher than the melting point of the amorphous alloy. The heating temperature is preferably 400-500°C. Within this heating range, the raw amorphous alloy can completely melt and remain molten when leaving the smelting chamber and entering the injection device for injection.
[0054] S05: The driving device drives the injection rod to inject the molten raw material in the injection barrel wall. The mold cavity is filled, and the injection rod stops injecting. The injection rod injection speed is 0.1-20m / s, and the mold filling speed is 0.1-30m / s. The injection speed is also one of the important conditions for amorphous alloy forming. If the injection speed is too fast, the surface of the amorphous alloy flexible gear after forming will have injection marks. If the injection speed is too slow, the surface of the amorphous alloy flexible gear after forming will have flow marks or weld lines. The control of the injection speed can reduce the defective rate to a certain extent. In the present invention, the injection speed of the injection rod is preferably 0.1-20m / s, and the mold filling speed is 0.1-30m / s.
[0055] While step S05 is being performed, the vacuum device continuously evacuates the mold cavity to ensure that the gas is discharged from the mold cavity in a timely manner during the filling process.
[0056] S06: The flexible gear is formed in the mold cavity, and the driving device drives the front mold to separate from the rear mold to take out the flexible gear.
[0057] The manufacturing method of the flexible gear also includes deburring, grinding and polishing the formed flexible gear.
[0058] The amorphous alloy in the above-mentioned embodiment is a type of amorphous alloy including base materials such as Zr, Ni, Fe, Cu, Al, Mg, Co, V and rare earth. In the present invention, there is no limitation on which amorphous alloy is used as the raw material for forming the flexible gear, but in actual situations, the type of amorphous alloy can be selected according to the required performance of the flexible gear. Amorphous alloys generally have higher strength, lower elastic modulus E, excellent fatigue resistance, larger elastic limit and good corrosion resistance, but amorphous alloys of different base materials still have differences in performance. Flexible gears can choose the type of amorphous alloy according to actual needs. For example, Fe 72 Co 18 Zr 10 , Fe 72 Ni 18 Zr 10 , Fe 68 Co 17 VxD 10 Amorphous alloy materials have a low thermal expansion coefficient. Fe 72 Co 18 Zr 10 , Fe 72 Ni 18 Zr 10 , Fe 68 Co 17 VxD 10etc. as the raw materials for forming flexible gears. Amorphous alloy materials can be applied to mobile phones, watch components, medical implants, dental implants, magnet cores, sports equipment and other fields, and even to aerospace and intelligent robot fields. Similarly, the flexible gears of the present invention can be applied to the above-mentioned fields, and the parts of the above-mentioned fields can be manufactured using the equipment or method of the present invention.
[0059] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the embodiments of the present invention rather than to limit them. Although the embodiments of the present invention have been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solutions of the embodiments of the present invention can still be modified or replaced by equivalents, and these modifications or equivalent replacements cannot cause the modified technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A flexible gear manufacturing device, comprising a mold device, the mold device comprising a front mold and a rear mold, the front mold is provided with a mold frame, characterized in that: The mold frame is provided with a detachable front mold core, the number of the front mold cores is 2-20, and the shapes and sizes of the front mold cores are the same; the front mold core forms a mold core inner cavity in the mold frame, and the mold core inner cavity is provided with tooth grooves; the rear mold is provided with a detachable rear mold core, and after the front mold and the rear mold are closed, the front mold core and the rear mold core form a closed mold cavity; the mold device is provided with a stripper plate, the front mold is provided with a branch flow channel, and the stripper plate is provided with a flow channel groove, which forms a main flow channel after closing with the front mold, and the main flow channel and the branch flow channel form a flow channel system; the flexible gear manufacturing equipment also includes a melting device, an injection device and a vacuum device; The hardness of the front mold core and the rear mold core is 45-55HRC; The cross-sections of the main channel and the branch channel are circular, the diameter of the main channel is 2-20 mm, and the diameter of the branch channel is 0.8-10 mm; The branch runner is provided with a point gate, and one mold cavity of the mold device is provided with 1-20 point gates for feeding materials; The flexible gear manufactured by the flexible gear manufacturing equipment is an amorphous alloy flexible gear; the single tooth stiffness value of the flexible gear is 50-80N / m; and the thickness of the flexible gear is 0.5-5mm.
2. A method for manufacturing a flexible gear using the manufacturing equipment according to claim 1, characterized in that: The steps include: S01: pouring amorphous alloy as raw material into a smelting chamber; S02: The clamping mechanism drives the front mold and the rear mold to close to form a closed mold cavity; S03: The vacuum exhaust device evacuates the smelting chamber and the mold cavity so that the air pressure in the smelting chamber and the mold cavity reaches the set value; S04: heating the raw materials in the smelting bin to make the raw materials completely molten, the heating temperature is 400-500°C; S05: The driving device drives the injection rod to inject the molten raw material in the smelting bin, and the mold cavity is filled. The injection speed of the injection rod is 0.1-20m / s, and the filling speed in the mold cavity is 0.1-30m / s; S06: The flexible gear is formed in the mold cavity, and the driving device drives the front mold to separate from the rear mold to take out the flexible gear.
Citation Information
Patent Citations
Systems and methods for implementing bulk metallic glass-based strain wave gears and strain wave gear components
CN106461038A