Aluminum liquid chute

By using tightly spliced ​​first and second pieces in the aluminum liquid chute and fixing them with chute fixing parts, the problems of chute cracking and deformation are solved, and higher product quality and service life are achieved.

CN110142383BActive Publication Date: 2024-11-01RUYUAN YAO NATIONALITY AUTONOMOUS COUNTY DONGYANGGUANG HIGH PURITY NEW MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201910442153.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-05-24
Publication Date
2024-11-01
Estimated Expiration
2039-05-24

AI Technical Summary

Technical Problem

Existing aluminum liquid chutes are prone to cracking and deforming during use, resulting in irregular bottom cracks and deep passing through the overall thickness, which poses a risk of aluminum leakage, which is difficult to ensure repair, affecting product quality and production efficiency.

Method used

Using a new splicing structure, it is tightly spliced ​​by the first and second pieces and fixed by the chute fixing. The splicing seam is located at the bottom of the inner wall of the chute and is sealed with a sealing component to eliminate the stress during local heat expansion. Concentrate points to avoid cracking and deformation.

Benefits of technology

It effectively avoids cracking and deformation of the chute, maintains the smoothness of the inner wall, reduces the repair workload, avoids the contamination of melt quality by cracks at the bottom of the chute, and improves product quality and service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110142383B_ABST
    Figure CN110142383B_ABST
Patent Text Reader

Abstract

The present invention discloses an aluminum liquid chute, comprising a first component and a second component for splicing into a chute body, and a chute fixing component for fixing the chute body; a splicing surface of the first component for splicing the second component is provided with a protrusion, and the second component is provided with a groove matching the protrusion; the splicing seam between the first component and the second component is located at the bottom of the inner wall of the chute body, and a blocking component is provided in the splicing seam between the first component and the second component. The aluminum liquid chute provided by the present invention eliminates the stress concentration part of the existing prefabricated block chute when it is locally expanded by heat in terms of structural design, can effectively avoid the problems of cracking and deformation, and avoid the hydrogen absorption and impurity pollution caused by cracks at the bottom of the chute to the quality of the melt, which is of great significance to improving product quality.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of casting molten material containers, and more specifically, to an aluminum liquid chute. Background Art

[0002] In the aluminum melt production industry, the chute is an essential basic equipment for production, which is used for transferring aluminum liquid between equipment and transferring and replenishing aluminum liquid between process flows such as degassing, filtration, and casting. The current chute is generally cast in sections using RSK-Ⅱ brown corundum castables. The outer shape is wide at the top and narrow at the bottom, and the inner wall is a regular semi-elliptical shape.

[0003] Compared with the traditional integral casting aluminum chute, the emergence of prefabricated block chute is a major progress in the development of chute. Prefabricated block chute is now widely used, such as Figure 1 As shown, it is cast in sections and then spliced ​​and installed. The main advantages of this type of chute are easy maintenance, flexible replacement, and low production cost. However, the biggest problem found in use is still a series of defects such as cracking and deformation caused by stress concentration. Generally, cracking and deformation occur after 15 to 20 days of use. Figures 2-3 As shown. The cracks at the bottom of the prefabricated block chute are the most serious. The crack lines are extremely irregular and the crack depth penetrates the entire thickness, posing a risk of aluminum leakage. During maintenance and repair, the repair material cannot completely match the inner wall of the chute crack. The repair depth is about 10mm, and it will fall off again after 3 to 5 uses. The repair workload is large, and the fallen repair material and exposed cracks pose a risk of contaminating the melt.

[0004] Therefore, it is necessary to develop an aluminum liquid chute that can avoid cracking and deformation. Summary of the invention

[0005] In order to overcome the defects of easy cracking and deformation described in the above-mentioned prior art, the present invention provides an aluminum liquid chute. The aluminum liquid chute provided adopts a new splicing structure, which can effectively avoid the problems of cracking and deformation, and prevent the cracks at the bottom of the chute from causing hydrogen absorption and impurity pollution to the melt quality, which is of great significance to improving product quality.

[0006] In order to solve the above technical problems, the technical solution adopted by the present invention is:

[0007] A molten aluminum chute, comprising a first building piece and a second building piece for splicing into a chute body, and a chute fixing piece for fixing the chute body;

[0008] The splicing surface of the first building component for splicing the second building component is provided with a protrusion, and the second building component is provided with a groove matching the protrusion; the splicing seam between the first building component and the second building component is located at the bottom of the inner wall of the chute body, and a sealing component is provided in the splicing seam between the first building component and the second building component.

[0009] The inventors conducted a statistical analysis of the prefabricated block chute of the prior art during actual use and found that the cracking parts are mainly concentrated at the bottom of the chute, that is, the center of the arc; secondly, due to thermal expansion and contraction in the length direction, the two ends of the chute are warped and uneven. When the aluminum melt flows in the chute, the melt pressure and the scouring of the aluminum melt carried by the bottom of the chute are undoubtedly the largest. In addition, the scraping of the bottom of the chute by the slag knife during manual operation will first show signs of surface shedding and scraping. More importantly, the design of the original prefabricated block chute model determines that the bottom of the chute is the most significant stress concentration point. The thickness of the castable in the cross section of the chute varies greatly. When the castable absorbs the heat of the melt to expand or cool down and shrink, the cross section will cause cracks at the bottom of the chute no matter in which direction it deforms. The crack width of the severe cracked part can reach 10 to 12 mm, which poses a great risk of aluminum leakage and is prone to increase the hydrogen content of the melt, affecting product quality. Due to the irregular cracks, repair work is difficult to carry out and the quality of repair is difficult to guarantee. Most cracks will fall off and crack again after being used 3 to 5 times after being repaired. Repeated repairs increase workload, affect production efficiency, and are not conducive to the stability of product quality.

[0010] Different from the existing prefabricated block chute, the aluminum liquid chute of the present invention uses a first building piece and a second building piece that fit closely together to form a chute body and is fixed by a chute fixing piece. The joint seam is located at the bottom of the inner wall of the chute and is blocked by a blocking component. The structural design of the aluminum liquid chute eliminates the stress concentration part of the existing prefabricated block chute when it is partially heated and expanded, thereby solving the problem of cracking and deformation of the chute. After a certain period of use, the inner wall maintains a good finish, no cracks appear at the bottom, only the joint seam is slightly enlarged and needs simple repair, and no aluminum liquid infiltration occurs.

[0011] In summary, the aluminum liquid chute of the present invention can effectively avoid the problems of cracking and deformation, and prevent the cracks at the bottom of the chute from causing hydrogen absorption and impurity pollution to the quality of the melt, which is of great significance to improving product quality.

[0012] Preferably, the joint seam is less than or equal to 3 mm.

[0013] Preferably, the protrusion is semi-cylindrical, and the axis of the protrusion is parallel to the extension direction of the chute body; the groove of the second component is semi-cylindrical to match the protrusion.

[0014] Preferably, the groove is completely consistent with the protrusion.

[0015] Preferably, the joint between the first building element and the second building element is a straight line. In this case, the joint is a straight line, which is convenient for filling the repair material as a plugging component, and the repair material is firmly combined with the first building element and the second building element, further reducing the workload of repair.

[0016] Preferably, the chute fixing member comprises a chute shell for accommodating the chute body, at least two stop blocks located in the chute shell for clamping the first building member and the second building member, and a chute pressing plate. The chute pressing plate is used to press the upper end of the chute body.

[0017] Preferably, the limit blocks are located at the bottom of both sides of the chute shell.

[0018] Preferably, a dry anti-seepage material insulation layer is provided between the chute body and the chute shell. The dry anti-seepage material is filled and compacted between the chute body and the chute shell to form a dry anti-seepage material insulation layer to prevent the first building and the second building from spreading and have a heat preservation effect.

[0019] Preferably, the chute shell is made of steel.

[0020] Preferably, a cross-section of the inner wall of the chute body perpendicular to the extension direction of the chute body is semi-elliptical.

[0021] The blocking component is made of calcium silicate board and / or asbestos wool.

[0022] The first building block and the second building block can be constructed by a person skilled in the art with reference to the prior art. Specifically, the following method can be used:

[0023] Considering the mold processing accuracy and dry drainage performance requirements, wooden molds are used for casting the first and second parts. Mold production requires accurate dimensions, smooth surfaces, and natural curve transitions. In particular, the convex position of the first part and the groove position of the second part must be accurate in size to ensure that the two can completely match each other. The contact position between the mold surface and the castable material must be coated.

[0024] Mix the castable with industrial pure water in a ratio of 8:1, stir thoroughly and fill into the mold. Then use a vibrating tool to compact until the slurry in the castable overflows, remove the excess castable with a tool and smooth the top; demould after standing for 36 hours (the time should be appropriately extended in winter), and let the demoulded parts dry naturally for a week; after natural drying, place the parts together in a preheating furnace, slowly heat from room temperature to 150℃ at 15℃ / h for 3 to 5 hours, continue to heat to 350℃ for 3 to 5 hours, and finally heat to 550℃ for 3 hours, then slowly cool to below 100℃ and take them out of the furnace to cool naturally to room temperature.

[0025] Compared with the prior art, the present invention has the following beneficial effects:

[0026] The aluminum liquid chute of the present invention is spliced ​​into a chute body by a first building piece and a second building piece that fit closely together and fixed by a chute fixing piece, and the splicing seam is located at the bottom of the inner wall of the chute and is blocked by a blocking component. The aluminum liquid chute eliminates the stress concentration part of the existing prefabricated block chute when the local heat expands in the structural design, can effectively avoid the problems of cracking and deformation, and avoid the cracks at the bottom of the chute from causing hydrogen absorption and impurity pollution to the melt quality, which is of great significance to improving product quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 It is a schematic end view of a prefabricated block chute in the prior art.

[0028] Figure 2 This is a picture of cracks in a precast block chute of the prior art.

[0029] Figure 3 This is a picture of cracks in a precast block chute of the prior art.

[0030] Figure 4 Schematic diagram of the first building block and the second building block in the aluminum liquid chute of Example 1 of the present invention.

[0031] Figure 5 This is a schematic diagram of the first building component and the second building component in the aluminum liquid chute of Example 1 of the present invention being spliced ​​into the chute body.

[0032] Figure 6 This is a schematic diagram of the structure of the aluminum liquid chute of Example 1 of the present invention. DETAILED DESCRIPTION

[0033] The present invention will be further described below in conjunction with specific implementation modes.

[0034] The same or similar numbers in the drawings of the embodiments of the present invention correspond to the same or similar parts; in the description of the present invention, it should be understood that if the terms "upper", "lower", "left", "right", "top", "bottom", "inside", "outside" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the drawings, they are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation. Therefore, the terms describing the positional relationship in the drawings are only used for illustrative purposes and cannot be understood as limitations on this patent.

[0035] In addition, if there are terms such as "first" and "second", they are only used for descriptive purposes, mainly to distinguish different devices, elements or components (the specific types and structures may be the same or different), and are not used to indicate or imply the relative importance and quantity of the indicated devices, elements or components, and cannot be understood as indicating or implying relative importance.

[0036] Example 1

[0037] An aluminum liquid chute, such as Figures 4 to 6 As shown, it includes a first building piece 11 and a second building piece 12 for assembling into a chute body 1 , and a chute fixing piece 2 for fixing the chute body 1 .

[0038] The splicing surface 111 of the first building 11 for splicing the second building 12 is provided with a protrusion 112, and the second building 12 is provided with a groove 113 that matches the protrusion 112. The splicing seam 13 between the first building 11 and the second building 12 is located at the bottom of the inner wall of the chute body 1, and a blocking component is provided in the splicing seam 13 between the first building 11 and the second building 12. The protrusion 112 is semi-cylindrical, and the axis of the protrusion 112 is parallel to the extension direction of the chute body 1. The groove 113 of the second building 12 is semi-cylindrical to match the protrusion 112. The splicing seam 13 located at the bottom of the inner wall of the chute body 1 is a straight line. The splicing seam 13 is less than or equal to 3mm. The blocking component is made of calcium silicate board or asbestos wool. The cross section of the inner wall of the chute body 1 perpendicular to the extension direction of the chute body 1 is semi-elliptical.

[0039] The chute fixing member 2 includes a chute shell 21 for accommodating the chute body 1, at least two limit blocks 22 located in the chute shell 21 for clamping the first building 11 and the second building 12, and a chute pressing plate 23. The limit blocks 22 are located at the bottom of both sides of the chute shell 21. The chute pressing plate 23 is used to press the upper end of the chute body 1. A dry anti-seepage material insulation layer 24 is provided between the chute body 1 and the chute shell 21.

[0040] The first building block 11 and the second building block 12 of the aluminum liquid chute of this embodiment can be prepared by the following method:

[0041] Considering the mold processing accuracy and dry drainage performance requirements, wooden molds are used for casting the first and second parts. Mold production requires accurate dimensions, smooth surfaces, and natural curve transitions, especially the convex position of the first part and the groove position of the second part must be accurate in size to ensure that the two can fit completely. A 35mm diameter PVC pipe can be cut open to fit the mold; the mold surface where the castable contacts must be coated.

[0042] Mix the castable with industrial pure water in a ratio of 8:1, stir thoroughly and fill into the mold. Then use a vibrating tool to compact until the slurry in the castable overflows, remove the excess castable with a tool and smooth the top; demould after standing for 36 hours (the time should be appropriately extended in winter), and let the demoulded parts dry naturally for a week; after natural drying, place the parts together in a preheating furnace, slowly heat from room temperature to 150℃ at 15℃ / h for 3 to 5 hours, continue to heat to 350℃ for 3 to 5 hours, and finally heat to 550℃ for 3 hours, then slowly cool to below 100℃ and take them out of the furnace to cool naturally to room temperature.

[0043] After 90 days of use, the inner wall of the aluminum molten chute of this embodiment maintains a relatively good finish, and no cracks appear at the bottom. Except for the local increase of 1 to 2 mm in the joint seam, the chute does not warp up, indicating that there is no aluminum liquid leakage at the bottom of the chute. The enlarged joint seam is a regular straight line, which is easy to fill with repair materials and is firmly combined with the chute, eliminating cracks at the bottom of the chute and reducing the workload of repair. Avoiding hydrogen absorption and impurity pollution caused by cracks at the bottom of the chute on the quality of the melt is of great significance to improving product quality.

[0044] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the embodiments here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the claims of the present invention.

Claims

1. A method for preparing a component of an aluminum liquid chute, characterized in that: The invention is applied to an aluminum liquid chute, the aluminum liquid chute comprising a first building (11) and a second building (12) for being spliced ​​into a chute body (1), and a chute fixing member (2) for fixing the chute body (1); a splicing surface (111) of the first building (11) for splicing the second building (12) is provided with a protrusion (112), and the second building (12) is provided with a groove (113) matching the protrusion (112); a splicing seam (13) between the first building (11) and the second building (12) is located at the bottom of the inner wall of the chute body (1), and the splicing seam (13) between the first building (11) and the second building (12) is provided with a groove (113) matching the protrusion (112); A blocking component is provided, wherein the protrusion (112) is semi-cylindrical, and the axis of the protrusion (112) is parallel to the extension direction of the chute body (1); the groove (113) of the second building piece (12) is semi-cylindrical and matches the protrusion (112); the joint seam (13) located at the bottom of the inner wall of the chute body (1) is a straight line; the chute fixing member (2) comprises a chute shell (21) for accommodating the chute body (1), at least two limit blocks (22) located in the chute shell (21) for clamping the first building piece (11) and the second building piece (12), and a chute pressing plate (23); the blocking component is made of calcium silicate board or asbestos wool; The method comprises the following steps: Step 1: The first and second components are cast using wooden molds to ensure processing accuracy and dry drainage performance requirements. The mold production requires accurate dimensions, smooth surfaces, and natural curved transitions. The contact area between the mold surface and the castable material must be coated; Step 2: Mix the castable with industrial pure water in a ratio of 8:1, stir thoroughly and fill into the mold, then tamp with a vibrating tool until the slurry in the castable overflows, remove the excess castable with a tool and smooth the top; Step 3: After standing for at least 36 hours, demould the molded parts and let them dry naturally for one week; Step 4: After natural drying, place the components together in a preheating furnace, slowly raise the temperature from room temperature to 150℃ at a rate of 15℃ / h and keep it for 3-5 hours, then continue to raise the temperature to 350℃ and keep it for 3-5 hours, and finally raise the temperature to 550℃ and keep it for 3 hours, then slowly cool down to below 100℃ and take it out of the furnace and cool naturally to room temperature.

2. The method for preparing a component of an aluminum liquid chute according to claim 1, characterized in that: A dry anti-seepage material insulation layer (24) is provided between the chute body (1) and the chute shell (21).