Display device

By adopting a combined structure of substrate, display unit, inorganic layer, organic layer, dam and stress release layer in the display device, the stress difference is absorbed and the invalid space area is reduced, thereby solving the problems of invalid space and cracks in the existing technology, and optimizing The bending performance and size of the display device.

CN112151698BActive Publication Date: 2024-10-01SAMSUNG DISPLAY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011124864.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2014-12-30
Filing Date
2015-12-29
Publication Date
2024-10-01
Estimated Expiration
2035-12-29

AI Technical Summary

Technical Problem

There is an increase in the invalid space area in the existing display device, which leads to an increase in the size of the display area and the possibility of cracks, affecting the display effect.

Method used

Using a combined structure of a substrate, a display unit, a first inorganic layer, a first organic layer, a first dam, a stress release layer and a second dam, the stress release layer absorbs stress differences and reduces the formation of ineffective space areas. And reduce compressive stress through protective films and cuts.

Benefits of technology

It effectively reduces the formation of ineffective space areas and prevents the occurrence of cracks. At the same time, it optimizes the bending performance and size of the display device and improves the display effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112151698B_ABST
    Figure CN112151698B_ABST
Patent Text Reader

Abstract

A display device is provided, which includes: a substrate; a display unit located on the substrate; a first inorganic layer located on the display unit; a first organic layer located on the upper part of the first inorganic layer; a second inorganic layer located on the upper surface of the first organic layer; a first dam located at an outer area of ​​the display unit; a second dam separated from the first dam and located at an outer area of ​​the first dam relative to the display unit; and a stress release layer at an end of an area where the first inorganic layer and the second inorganic layer are in direct contact, wherein the end is located between the first dam and the second dam.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of the invention patent application with application date of December 29, 2015, application number 201511009175.X and title “Display Device”. Technical Field

[0002] One or more embodiments of the present invention are directed to a display device. Background Art

[0003] With the advancement in information technology, the market for display devices, which are media devices for connecting users with information, has expanded. Therefore, flat panel displays (FPDs) such as liquid crystal displays (LCDs), organic light emitting display devices, and plasma display panels (PDPs) are widely used.

[0004] In such devices, there is an increasing desire to reduce the dead space region located around the display area. Summary of the invention

[0005] One or more exemplary embodiments of the present invention include a display device.

[0006] Additional aspects will be set forth in part in the description which follows and, in part, will be obvious from the description, or may be learned by practice of the presented embodiments.

[0007] According to one or more embodiments of the present invention, a display device includes: a substrate; a display unit located on the substrate; a first inorganic layer located on the display unit; a first organic layer located on the upper surface of the first inorganic layer; a first dam located at an edge of the first organic layer; a second dam separated from the first dam and located at an outer area of ​​the first dam relative to the display unit; and a stress release layer located between the first dam and the second dam.

[0008] The stress relief layer may include an organic material.

[0009] The stress relaxation layer may include the same material as that of the first organic layer.

[0010] The stress release layer may be formed using an inkjet process.

[0011] The stress relief layer may be located on the first dam and the second dam, and may have a height substantially equal to that of the first organic layer.

[0012] The display device may further include: a second inorganic layer located on an upper surface of the first organic layer.

[0013] The display device may further include: a protective film located under the substrate.

[0014] The protection film may be spaced apart from the display area and may be located inside the display area of ​​the display device.

[0015] The upper edge of the protective film may be rounded.

[0016] The substrate may have a cutout, and the cutout may be spaced apart from an upper edge of the protective film.

[0017] The cutout may have a triangular shape.

[0018] The cutout may have a semicircular shape.

[0019] The cutout may have a rectangular shape.

[0020] A stress relief layer may be located between the ELVSS and the second dam.

[0021] According to one or more embodiments of the present invention, a display device includes: a substrate; a display unit located on the substrate; a first inorganic layer located on the display unit; a first organic layer located on an upper surface of the first inorganic layer; a first dam located at an edge of the first organic layer; and a stress release layer located on the substrate and at an outer area of ​​the first dam relative to the display unit.

[0022] The display device may further include: a second dam spaced apart from the first dam and located at an edge of the stress release layer.

[0023] The display device may further include: a protective film located under the substrate.

[0024] The protective film can have a rounded upper edge.

[0025] The substrate may have a cutout at a lower surface, and the cutout may be spaced apart from an upper edge of the protective film.

[0026] According to one or more embodiments of the present invention, a display device includes: a substrate; a display unit located on the substrate; a first inorganic layer located on the display unit; a first organic layer located on the upper surface of the first inorganic layer; a first dam located at an edge of the first organic layer; and a protective film located under the substrate, wherein the protective film is located under the substrate, wherein the protective film has a rounded upper edge.

[0027] The display device may further include: a second dam spaced apart from the first dam and located at an outer region of the display unit relative to the first dam.

[0028] The display device may further include: a stress release layer between the ELVSS and the second dam and at an outer region of the ELVSS relative to the display unit.

[0029] The stress relief layer may include an organic material.

[0030] The stress relaxation layer may include the same material as that of the first organic layer.

[0031] The stress release layer may be formed using an inkjet process.

[0032] The substrate may have a cutout in a lower surface of the substrate, and the cutout may be spaced apart from an upper edge of the protective film. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] These and / or other aspects will become apparent and more readily understood through the following description of the embodiments in conjunction with the accompanying drawings, in which:

[0034] Figure 1 is a cross-sectional view of a display device according to an embodiment of the present invention;

[0035] Figure 2 is a cross-sectional view of a display unit according to an embodiment of the present invention;

[0036] Figure 3 is a schematic cross-sectional view showing a display device according to another embodiment of the present invention;

[0037] Figure 4 is a schematic cross-sectional view showing a display device according to another embodiment of the present invention;

[0038] Figure 5 is a schematic cross-sectional view showing a display device according to another embodiment of the present invention; and

[0039] Figure 6 is a schematic cross-sectional view showing a display device according to another embodiment of the present invention. DETAILED DESCRIPTION

[0040] Since the present invention allows various changes and many embodiments, the exemplary embodiments will be shown in the drawings and described in detail in the written description. Below, the various aspects and features of the present invention and the methods used to implement them will be more fully described with reference to the accompanying drawings, in which exemplary embodiments of the present invention are shown. However, the present invention can be implemented in many different forms and should not be construed as being limited to the exemplary embodiments set forth herein.

[0041] Hereinafter, exemplary embodiments of the present invention will be described in detail with reference to the accompanying drawings. Those components which are the same or substantially similar are denoted by the same reference numerals regardless of the figure numbers, and redundant explanations thereof will be omitted.

[0042] It will be understood that, although the terms "first," "second," etc., may be used herein to describe various elements, components, regions, layers, or portions, these components should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer, or portion from another element, component, region, layer, or portion. Therefore, the first element, component, region, layer, or portion discussed below may be referred to as a second element, component, region, layer, or portion without departing from the teachings of the exemplary embodiments.

[0043] For ease of description, spatial relative terms such as "under ...", "below ...", "below ...", "above ...", "above ...", etc. may be used here to describe the relationship between an element or feature and other elements or features as shown in the figure. It will be understood that, in addition to the orientation depicted in the figure, the spatial relative terms are also intended to include different orientations of the device in use or operation. For example, if the device in the figure is turned over, the element described as "below" or "below" other elements or features will then be positioned as "above" or "above" other elements or features. Therefore, the term "below ..." can include both "above ..." and "below ..." orientations. The device can be positioned otherwise (rotated 90 degrees or in other orientations), and the spatial relative descriptors used here should be interpreted accordingly. As used herein, the term "use" can be considered synonymous with the term "utilize".

[0044] As used herein, the singular forms "a", "an" and "the" are intended to include the plural forms as well, unless the context clearly indicates otherwise.

[0045] It will be further understood that the terms “include” and / or “comprises” used herein specify the presence of stated features or components, but do not preclude the presence or addition of one or more other features or components.

[0046] It will be understood that when a layer, region or component is referred to as being "formed on" another layer, region or component, the layer, region or component may be directly or indirectly formed on the other layer, region or component. That is, for example, there may be an intermediate layer, intermediate region or intermediate component. When an element is referred to as being "directly formed on" another element or layer, there is no intermediate element or intermediate layer. It will be understood that when an element or layer is referred to as being "on" another element or layer, "connected to" or "bonded to" another element or layer, the element or layer may be directly on the other element or layer, directly connected or directly bonded to other elements or layers, or there may also be one or more intermediate elements or intermediate layers. When an element is referred to as being "directly on" another element or layer, "directly connected to" or "directly bonded to" another element or layer, there is no intermediate element or intermediate layer. For example, when a first element is described as being "bonded to" or "connected to" a second element, the first element may be directly bonded or connected to the second element, or the first element may be indirectly bonded or connected to the second element via one or more intermediate elements.

[0047] For the convenience of explanation, the size of the elements in the drawings may be exaggerated. In other words, since the size and thickness of the components in the drawings may be arbitrarily shown for the convenience of explanation, the subsequent embodiments are not limited thereto.

[0048] Although a particular embodiment may be described in a particular process order, the specific process order may be performed in a different order than that described. For example, two consecutively described processes may be performed at substantially the same time (e.g., simultaneously or in parallel) or may be performed in an order opposite to that described.

[0049] As used herein, the term "and / or" includes any and all combinations of one or more of the associated listed items. Expressions such as "at least one of...", when referring to a list of elements, modify the entire list of elements rather than modifying the individual elements of the list. In addition, the term "exemplary" is intended to indicate an example or illustration.

[0050] Figure 1 is a cross-sectional view of a display device according to an embodiment of the present invention. Figure 2 is a cross-sectional view of a display unit 20 according to an embodiment of the present invention.

[0051] Reference Figure 1 , the display device according to the embodiment of the present invention may include a substrate 10 , a display unit 20 , and an encapsulation unit 30 .

[0052] The substrate 10 may be made of SiO 2However, the material used to form the substrate 10 is not limited thereto, and the substrate 10 may be formed of a transparent plastic material such as polyimide (PI).

[0053] An array of pixels (or sub-pixels) may be formed in a display area A / A of a display unit 20 (formed on a substrate 10). Each pixel may include a thin film transistor and a light emitting device controlled by the thin film transistor. The light emitting device may be a self-emissive device, such as an organic light emitting device.

[0054] For the convenience of description, only an embodiment in which the display unit 20 is configured as an organic light emitting device will be described below, but the present invention is not limited thereto.

[0055] Now refer to Figure 2 The display unit 20 is described.

[0056] like Figure 2 As shown in FIG. 1 , in the display device according to the present embodiment, a buffer layer 21 may be formed on the substrate 10. The buffer layer 21 may serve as a barrier layer and / or blocking layer for reducing or preventing diffusion of impurity ions and penetration of moisture or external air and for planarizing the surface of the substrate 10.

[0057] The semiconductor layer A of the thin film transistor TFT is formed on the buffer layer 21. The semiconductor layer A may be formed of polysilicon and may include a channel region that is not doped with impurities (e.g., undoped) and a source region and a drain region that are doped with impurities on respective sides of the channel region. The impurities may vary depending on the type of the thin film transistor TFT and may be N-type impurities or P-type impurities.

[0058] The semiconductor layer A may be formed of a semiconductor including amorphous silicon or crystalline silicon, and may be deposited using various deposition methods. For example, crystalline silicon may be formed by crystallizing amorphous silicon. Amorphous silicon may be crystallized using various methods such as rapid thermal annealing (RTA), solid phase crystallization (SPC), excimer laser annealing (ELA), metal induced crystallization (MIC), metal induced lateral crystallization (MILC), and / or sequential lateral solidification (SLS). The semiconductor layer A may be patterned by photolithography.

[0059] The gate insulating layer 23 is deposited on the surface (e.g., the entire surface) of the substrate 10 so that the gate insulating layer 23 can cover the semiconductor layer A. The gate insulating layer 23 can be formed of an inorganic material such as silicon oxide or silicon nitride, and can be formed into a multi-layer or single-layer structure. In some embodiments, the gate insulating layer 23 can be made of silicon nitride (SiN x ), silicon oxide (SiO 2), hafnium oxide (Hf) and / or aluminum oxide. The gate insulating layer 23 may be formed using various deposition methods such as chemical vapor deposition (CVD) and / or plasma enhanced chemical vapor deposition (PECVD). The gate insulating layer 23 insulates the semiconductor layer A from the gate electrode G.

[0060] The gate electrode G can be formed of molybdenum (Mo), aluminum (Al), platinum (Pt), palladium (Pd), silver (Ag), magnesium (Mg), gold (Au), nickel (Ni), neodymium (Nd), iridium (Ir), chromium (Cr), calcium (Ca), titanium (Ti), tungsten (W) and / or copper (Cu).

[0061] The interlayer insulating layer 25 is formed on a surface (eg, the entire surface) of the substrate 10 so that the interlayer insulating layer 25 may cover the gate electrode G. As shown in FIG.

[0062] The interlayer insulating layer 25 may be formed of an inorganic material or an organic material. In some embodiments, the interlayer insulating layer 25 may be formed of an inorganic material. For example, the interlayer insulating layer 25 may be formed of a metal oxide or a metal nitride. The inorganic material may include, for example, silicon oxide (SiO 2 ), Silicon Nitride (SiN x ), silicon oxynitride (SiON), aluminum oxide (Al 2 O 3 ), titanium oxide (TiO 2 ), Tantalum Oxide (Ta 2 O 5 ), hafnium oxide (HfO 2 ) or zirconium oxide (ZrO) etc. The interlayer insulating layer 25 may be made of silicon oxide (SiO x ) and / or silicon nitride (SiN x ) and may be formed as a multi-layer or single-layer structure. In some embodiments, the interlayer insulating layer 25 may have SiO x / SiN y or SiN X / SiO y The interlayer insulating layer 25 may be formed using various deposition methods such as CVD and PECVD.

[0063] The interlayer insulating layer 25 may insulate the gate electrode G from wiring formed on the upper surface of the interlayer insulating layer 25 .

[0064] A source electrode S and a drain electrode D of the thin film transistor TFT are formed on the interlayer insulating layer 25 .

[0065] The planarization layer 27 is formed on the entire surface of the substrate 10 so that the planarization layer 27 may cover the source electrode S and the drain electrode D. The pixel electrode 281 may be formed on the planarization layer 27. The pixel electrode 281 is connected to the drain electrode D of the thin film transistor TFT through the opening VIA (eg, a through hole).

[0066] The planarization layer 27 may be formed of an insulating material. For example, the planarization layer 27 may be formed of an inorganic material, an organic material, or a compound including an organic / inorganic material. The planarization layer 27 may be formed as a multilayer or single layer structure, and may be formed using various deposition methods. In some embodiments, the planarization layer 27 may be formed of a polyacrylate resin, an epoxy resin, a phenolic resin, a polyamide resin, a polyimide resin, an unsaturated polyester resin, a polyphenylene oxide resin, a polyphenylene sulfide resin, and / or benzocyclobutene (BCB).

[0067] An organic light emitting device such as an organic light emitting diode (OLED) may be formed on the thin film transistor TFT. The OLED includes a pixel electrode 281, an intermediate layer 283 including an organic emission layer, and an opposing electrode 285. The OLED may further include a pixel defining layer 29 and a partition.

[0068] The pixel electrode 281 may be electrically connected to the drain electrode D of the thin film transistor TFT while filling the opening VIA in the planarization layer 27. The pixel electrode 281 and / or the counter electrode 285 may be formed as a transparent electrode or a reflective electrode. When the pixel electrode 281 and / or the counter electrode 285 are formed as transparent electrodes, the pixel electrode 281 and / or the counter electrode 285 may be made of indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO) and / or indium oxide (In 2 O 3 ). When the pixel electrode 281 and / or the counter electrode 285 are formed as a reflective electrode, the pixel electrode 281 and / or the counter electrode 285 may include a reflective layer formed of silver (Ag), magnesium (Mg), aluminum (Al), platinum (Pt), palladium (Pd), gold (Au), nickel (Ni), neodymium (Nd), iridium (Ir), chromium (Cr), or a suitable combination thereof, and a reflective layer formed of ITO, IZO, ZnO, and / or In 2 O 3 In some embodiments, the pixel electrode 281 or the counter electrode 285 may have an ITO / Ag / ITO structure.

[0069] The pixel defining layer 29 may define a pixel region and a non-pixel region. The pixel defining layer 29 may include an opening exposing the pixel electrode 281, and may be formed to cover a surface (e.g., the entire surface) of the substrate 10. An intermediate layer 283, which will be further described later, may be formed in the opening, and thus, the opening may define the entire or substantially the entire pixel region.

[0070] The intermediate layer 283 may include an organic emission layer. In one embodiment, the intermediate layer 283 includes an organic emission layer. The intermediate layer 283 may also include a hole injection layer (HIL), a hole transport layer (HTL), an electron transport layer (ETL) and / or an electron injection layer (EIL). The present invention is not limited thereto, and in addition to the organic emission layer, the intermediate layer 283 may also include other functional layers.

[0071] The pixel electrode 281, the intermediate layer 283 and the counter electrode 285 together form (eg, constitute) an organic light emitting diode (OLED). Holes and electrons respectively injected from the pixel electrode 281 and the counter electrode 285 of the OLED may combine with each other in the organic emission layer of the intermediate layer 283 to generate light.

[0072] The HIL may be formed of a phthalocyanine compound such as copper phthalocyanine, or TCTA, m-MTDATA, or m-MTDAPB which is a starburst amine.

[0073] The HTL can be formed of N,N'-bis(3-methylphenyl)-N,N'-biphenyl-[1,1-diphenyl]-4,4'-diamine (TPD), N,N'-bis(naphthyl-1-yl)-N,N'-diphenylbenzidine (α-NPD), or the like.

[0074] EIL can be made of materials such as LiF, NaCl, CsF, Li 2 O, BaO or Liq materials are used to form it.

[0075] ETL can be done by Alq 3 form.

[0076] The organic emission layer may include a host material and a dopant material. Examples of the host material of the organic emission layer may include tris(8-hydroxyquinoline)aluminum (Alq3), 9,10-di(naphthalene-2-yl)anthracene (AND), 3-tert-butyl-9,10-di(naphthalene-2-yl)anthracene (TBADN), 4,4'-bis(2,2'-diphenylethylene)-1,1'-biphenyl (DPVBi), 4,4'-bis(2,2-diphenylethylene-1-yl)-4,4'- dimethylphenyl (p-DMDPVBi), tert-(9,9-diarylfluorene) (TDAF), 2-(9,9'-spirobifluorene-2-yl)-9,9'-spirobifluorene (BSDF), 2,7-bis(9,9'-spirobifluorene-2-yl)-9,9'-spirobifluorene (TSDF), bis(9,9-diarylfluorene) (BDAF), 4,4'-bis(2,2-diphenyl-vinyl-1-yl)-4, 4'-Bis-(tert-butyl)phenyl (p-TDPVBi), 1,3-bis(carbazol-9-yl)benzene (mCP), 1,3,5-tris(carbazol-9-yl)benzene (tCP), 4,4',4"-tris(carbazol-9-yl)triphenylamine (TcTa), 4,4'-bis(carbazol-9-yl)biphenyl (CBP), 4,4'-bis(9-carbazolyl)-2,2'-dimethylbiphenyl (CBDP) , 4,4'-bis(carbazol-9-yl)-9,9-dimethyl-fluorene (DMFL-CBP), 4,4'-bis(carbazol-9-yl)-9,9-bis(9-phenyl-9H-carbazole)fluorene (FL-4CBP), 4,4'-bis(carbazol-9-yl)-9,9-di-tolyl-fluorene (DPFL-CBP) and 9,9-bis(9-phenyl-9H-carbazole)fluorene (FL-2CBP), etc.

[0077] Examples of doping materials of the organic emission layer may include 4,4′-bis[4-(di-p-tolylamino)phenylvinyl]biphenyl (DPAVBi), 9,10-di(naphthalene-2-yl)anthracene (AND), 3-tert-butyl-9,10-di(naphthalene-2-yl)anthracene (TBADN), and the like.

[0078] The counter electrode 285 is formed on the intermediate layer 283. The counter electrode 285 forms an electric field together with the pixel electrode 281 so that light is emitted through the intermediate layer 283. The pixel electrode 281 may be patterned for each pixel, and the counter electrode 285 may be formed so that a common voltage is applied to all pixels.

[0079] The pixel electrode 281 and the counter electrode 285 may be formed as a transparent electrode or as a reflective electrode, or the pixel electrode 281 and the counter electrode 285 may be formed as a transparent electrode and a reflective electrode, respectively. The pixel electrode 281 may serve as an anode, and the counter electrode 285 may serve as a cathode, but the present invention is not limited thereto. For example, the pixel electrode 281 may serve as a cathode, and the counter electrode 285 may serve as an anode.

[0080] Despite Figure 1 Only one OLED is shown in the figure, but the display panel may include multiple OLEDs. A pixel may be formed in each OLED. Each pixel may implement (eg, output) red, green, blue, or white.

[0081] However, the present invention is not limited to this. The intermediate layer 283 can be formed together on the entire pixel electrode 281 without being affected by the position of the pixel. In this embodiment, the organic emission layer can be formed by vertically stacking a luminescent material for emitting (e.g., configured to emit) red light, a luminescent material for emitting green light, and a luminescent material for emitting blue light, or by mixing these materials. Any suitable combination of other colors capable of emitting white light is possible. The organic emission layer may also include a color conversion layer or a color filter that converts white light into light of a certain (e.g., predetermined) color.

[0082] The protective layer may be disposed on the opposing electrode 285 and may cover and protect the OLED. An inorganic insulating layer and / or an organic insulating layer may be used as the protective layer.

[0083] The spacer may be disposed between the pixel areas in the display area A / A. The spacer may be provided to maintain a space between the substrate 10 and the encapsulation unit 30 and prevent display characteristics from being degraded by external impact.

[0084] The spacer may be disposed on the pixel defining layer 29. The spacer may protrude from the pixel defining layer 29 toward the encapsulation unit 30.

[0085] In some embodiments, the spacer may be formed of the same material as the material used to form the pixel defining layer 29 and by using the same process as the process used to form the pixel defining layer 29. For example, the pixel defining layer 29 and the spacer may be formed simultaneously (e.g., in parallel) by adjusting the amount of exposure using a halftone mask during the exposure process. However, the present invention is not limited thereto. The pixel defining layer 29 and the spacer may be formed sequentially or individually and may be independent structures formed of different materials.

[0086] Now refer to Figure 1 A display device according to the present embodiment is described.

[0087] like Figure 1As shown in , the display device according to the present embodiment can be divided into a display area A / A where the display unit 20 emits light and an outer area O / A which is the remaining area of ​​the display device (eg, an area other than the display area A / A).

[0088] The display unit 20 may be Figure 1 The encapsulation unit 30 may be formed on the substrate 10 through the display area A / A and the outer area O / A so that the encapsulation unit 30 may cover the display unit 20 .

[0089] The encapsulation unit 30 has a structure in which a plurality of thin film layers are stacked, for example, a structure in which inorganic layers 31 and organic layers 33 are alternately stacked.

[0090] Despite Figure 1 The first inorganic layer 31a, the first organic layer 33a, and the second inorganic layer 31b are sequentially stacked on the display unit 20, but the number of thin film layers is not limited thereto. As long as the encapsulation layer 30 has a structure in which the inorganic layer 31 and the organic layer 33 are alternately stacked, the encapsulation unit 30 can be formed without limiting the number of thin film layers.

[0091] The inorganic layer 31 may strongly prevent oxygen or moisture from penetrating into the display unit 20 , and the organic layer 33 may absorb stress applied to the inorganic layer 31 to enhance flexibility.

[0092] The inorganic layer 31 may be a single layer or a multi-layer stack including metal oxide and / or metal nitride. For example, the first inorganic layer 31a and the second inorganic layer 31b may include SiN x 、Al 2 O 3 、SiO 2 and / or TiO 2 .

[0093] The organic layer 33 is formed of a polymer and may be a single layer or a multilayer stack formed of, for example, polyethylene terephthalate, polyimide, polycarbonate, epoxy resin, polyethylene and / or polyacrylate. For example, the organic layer 33 may be formed of polyacrylate. For example, the organic layer 33 may include a product of polymerizing a monomer composition including a diacrylate monomer and / or a triacrylate monomer (e.g., may be formed by polymerizing the monomer composition). The monomer composition may also include a monoacrylate monomer. The monomer composition may also include a known photoinitiator such as trimethylbenzoyldiphenylphosphine (TPO), but the present invention is not limited thereto.

[0094] like Figure 1As shown in , the first dam 41 may be formed in the outer area O / A of the substrate 10. The first dam 41 may be formed at the edge of the first organic layer 33a, and may be formed to have a certain height (e.g., a predetermined height) to prevent the first organic layer 33a from unintentionally diffusing when the first organic layer 33a is formed (e.g., the first dam 41 may be formed to include the first organic layer 33a when the first organic layer 33a is formed).

[0095] In some embodiments, the first dam 41 may be formed of the same material as the pixel defining layer 29, and may be formed during the same process as the process used to form the pixel defining layer 29. For example, the pixel defining layer 29 and the first dam 41 may be formed simultaneously (e.g., in parallel) by adjusting the amount of exposure using a halftone mask through an exposure process, but the present invention is not limited thereto.

[0096] The first dam 41 may be formed on an upper portion of ELVSS (power source, not shown). Figure 1 As shown in FIG. 4 , the first dam 41 may be formed toward the outside of the upper portion of the ELVSS.

[0097] The first and second inorganic layers 31a and 31b may be formed on a portion of the substrate 10 to cover the first dam 41. The first organic layer 33a may be formed inside the display area A / A and inside the outer area O / A where the first dam 41 is formed.

[0098] In one embodiment, the outer region O / A may be divided into an inner cell B (e.g., inner portion) in which the first organic layer 33a is formed and an outer cell A (e.g., outer portion) in which the first dam 41 is formed but the first organic layer 33a is not formed. Since the layers in the inner cell B are deposited in such a manner that the organic layer has a uniform or substantially uniform thickness, although stress acts on the inner cell B during the process of bending the outer region O / A, the stress is absorbed by the organic layer, and thus flexibility can be firmly provided to the inner cell B.

[0099] When a structure like the first organic layer 33 a is not formed in the outer cell A, stress may be completely absorbed during the bending process, and thus cracks may occur due to a difference in tensile stress between the inner cell B and the outer cell A. FIG.

[0100] For example, the outer area of ​​the display area A / A may be bent to form the dead space D / S, and the entire outer cell A and the inner cell B (in other words, the entire outer area O / A) may be bent to minimize the formation of the dead space D / S.

[0101] During this process, stress acts on the substrate and the upper elements or layers thereon due to bending. Therefore, the stress acting on the inner cell B where the organic layer is formed may be different from the stress acting on the outer region A where the organic layer is not formed. As described above, the organic layer can play a role in absorbing stress and ensuring flexibility.

[0102] Therefore, if the formation of the dead space D / S is minimized, there is concern that cracks may occur due to the stress difference between the inner cell B and the outer cell A. If the area where the dead space D / S is formed increases to reduce the chance of cracks occurring, it is undesirable to increase the size of the display device.

[0103] The display device according to this embodiment may include Figure 1 A second dam 43 and a stress relief layer 50 are shown in FIG. 5 , which will be described in further detail below.

[0104] The display device according to this embodiment may further include a second dam 43 that is separated (e.g., spaced apart) from the first dam 41 (e.g., separated by a predetermined distance) and disposed at an outer area of ​​the first dam 41 (e.g., an outer area of ​​the first dam 41 relative to the display unit 20).

[0105] The second dam 43 may be formed at the edges of the first inorganic layer 31a and the second inorganic layer 31b, such as Figure 1 shown.

[0106] In some embodiments, the second dam 43 may be formed of the same material as that of the first dam 41 and through the same process as that used to form the first dam 41. However, the present invention is not limited thereto.

[0107] The stress release layer 50 has a certain height and may be formed in a space (eg, region) between the first dam 41 and the second dam 43 (eg, in the outer cell A). According to one embodiment of the present invention, the stress release layer 50 may be formed between the ELVSS and the second dam 43 .

[0108] The stress release layer 50 may be formed of an organic material, and may be formed by being deposited to have the same or substantially the same height as that of the first organic layer 33 a , but is not limited thereto.

[0109] The stress release layer 50 is formed of a polymer and may be a single layer or a multilayer stack formed of, for example, polyethylene terephthalate, polyimide, polycarbonate, epoxy resin, polyethylene, and / or polyacrylate. For example, the stress release layer 50 may be formed of polyacrylate. For example, the stress release layer 50 may include (a product formed by polymerizing a monomer composition including a diacrylate monomer and / or a triacrylate monomer (e.g., may be formed by polymerizing the monomer composition). The monomer composition may also include a monoacrylate monomer, but the present invention is not limited thereto.

[0110] The stress release layer 50 may be formed of the same material as that of the first organic layer 33 a and through the same process as that used to form the first organic layer 33 a .

[0111] The second dam 43 may function as a dam to prevent the stress release layer 50 from diffusing to the outside of the substrate 10 when the stress release layer 50 is formed (eg, the second dam 43 may contain the stress release layer 50 when the stress release layer 50 is formed).

[0112] The stress release layer 50 may be formed by using various processing methods. For example, in some embodiments, the stress release layer 50 may be formed by inkjet processing to easily control diffusion at its edge. However, the method of forming the stress release layer 50 is not limited thereto.

[0113] Therefore, in some embodiments, after forming the second dam 43 , the stress release layer 50 may be formed between the first dam 41 and the second dam 43 of the same organic material as that of the first organic layer 33 a through an inkjet process.

[0114] In order to reduce the stress difference between the inner cell B and the outer cell A, the stress release layer 50 may be formed by being deposited to have a certain height like the first organic layer 33 a .

[0115] Therefore, when the outer area O / A is bent, since the first organic layer 33 a absorbs stress applied to the inner cell B and the stress release layer 50 absorbs stress applied to the outer area O / A, the possibility of crack formation may be substantially reduced or prevented.

[0116] The display device according to the present embodiment may further include a protective film 60 disposed under the substrate 10 (e.g., at a lower portion or at a lower surface of the substrate 10). The protective film 60 may protect the display device from external impact during a manufacturing process and prevent moisture from penetrating from a lower portion of the substrate 10.

[0117] The protective film 60 may be attached to the lower portion of the substrate 10 through a thin adhesive layer. When the adhesive layer is used to attach the protective film 60 to the lower portion of the substrate 10, distortion of the substrate 10 may be effectively prevented.

[0118] The protective film 60 is located in the display area A / A. However, the protective film 60 may be located inside a certain length L from the edge of the display area A / A.

[0119] The protection film 60 prevents the substrate 10 from being damaged when the substrate 10 is bent.

[0120] Figure 3 is a schematic cross-sectional view showing a display device according to another embodiment of the present invention. Figures 1 to 3 The same reference numerals denote the same elements, and thus, redundant descriptions will be omitted for brevity of description.

[0121] The display device according to this embodiment and the display device according to Figure 1 The differences between the display devices of the embodiments are shown in FIG.

[0122] like Figure 3 As shown, the protection film 61 may be disposed below the substrate 10 (eg, at a lower portion of the substrate 10 ) in the display device according to the present embodiment.

[0123] In one embodiment, the protection film 61 may be formed to have a rounded upper edge. The stress release layer 50 may be formed between the ELVSS and the second dam 43 and at an outer region of the ELVSS relative to the display unit.

[0124] During the process of bending the substrate 10 , compressive stress acts on the lower portion of the protective film 61 due to contraction, and tensile stress acts on the upper portion of the protective film 61 due to expansion.

[0125] During a process of manufacturing the display device, a bending process may be repeatedly performed due to an external force, and when a stress greater than a fracture stress acts on the display device, the display device may be damaged.

[0126] In one embodiment, the rounded upper edge of the protection film 61 may be formed to release stress occurring in the lower portion of the substrate 10 and the upper portion of the protection film 61 .

[0127] Figure 4 is a schematic cross-sectional view showing a display device according to another embodiment of the present invention. Figures 1 to 4 The same reference numerals denote the same elements, and thus, redundant descriptions will be omitted for brevity of description.

[0128] like Figure 4As shown, a cutout 110 (eg, a cutout unit) may be formed in a lower surface of a substrate 10 of a display device according to some embodiments of the present invention.

[0129] As described above, during the process of manufacturing the display device, compressive stress acts on the lower portion of the substrate 10 due to shrinkage. In order to remove or reduce the compressive stress, the display device may have a cutout 110 in the lower portion of the substrate 10.

[0130] The cutout 110 may be formed in the lower surface of the substrate 10 in the form of a groove having a certain height and width and spaced a certain distance from the rounded upper edge of the protective film 60. The height and width of the cutout 110 are not limited, and the shape of the cutout 110 is not limited to the illustrated shape.

[0131] The cutout 110 may be formed in the lower surface of the substrate 10, and may be formed in a region where the compressive stress acts most or is most concentrated. Since the cutout 110 (i.e., a groove having a specific shape) is formed in the lower surface of the substrate 10, the compressive stress acting on the lower surface of the substrate 10 may be reduced despite the bending process. As a result, the display device is prevented from being damaged.

[0132] A cutout 110 having a triangular shape may be formed in the lower surface of the substrate 10 of the display device according to the present embodiment. The width and height of the cutout 110 may have various values ​​according to the desired degree of curvature, but are not limited thereto. However, the height of the cutout 110 may have a value smaller than the thickness of the substrate 10.

[0133] Figure 5 is a schematic cross-sectional view showing a display device according to another embodiment of the present invention. Figures 1 to 3 and Figure 5 The same reference numerals denote the same elements, and thus, redundant descriptions will be omitted for brevity of description.

[0134] The display device according to this embodiment is Figure 4 The main difference of the display device of the embodiment is that the cutout 130 has the same Figure 4 The cutouts 110 have different shapes, and therefore, for the convenience of description, the differences between these embodiments will be mainly described.

[0135] like Figure 5 As shown, the display device according to the present embodiment may be formed such that the cutout 130 formed in the lower surface of the substrate 10 has a circular shape (eg, a semicircular shape).

[0136] The radius of the cutout 130 having a circular shape may have various values ​​according to the desired degree of curvature, but is not limited thereto. The radius of the cutout 130 may have a value smaller than that of the thickness of the substrate 10 .

[0137] The cutout 130 may be formed in the lower surface of the substrate 10, and may be formed in a region where the compressive stress acts most or is most concentrated. Since the cutout 130 (i.e., a groove having a specific shape) is formed in the lower surface of the substrate 10, the compressive stress acting on the lower surface of the substrate 10 may be reduced despite the bending process. As a result, the display device is prevented from being damaged.

[0138] Figure 6 is a schematic cross-sectional view showing a display device according to another embodiment of the present invention. Figures 1 to 3 and Figure 6 The same reference numerals denote the same elements, and thus, redundant descriptions will be omitted for brevity of description.

[0139] The display device according to this embodiment is Figure 4 The display device of the embodiments mainly differs in that the cutout 150 has a shape different from the cutout 110, and thus, for convenience of description, the difference between the embodiments will be mainly described.

[0140] like Figure 6 As shown, the display device according to the present embodiment may be formed such that a cutout 150 having a rectangular shape is formed in the lower surface of the substrate 10 .

[0141] The width and height of the cutout 150 having a rectangular shape may have various values ​​according to the desired degree of bending, but are not limited thereto. However, the height of the cutout 150 may have a value smaller than that of the thickness of the substrate 10 .

[0142] The cutout 150 may be formed in the lower surface of the substrate 10 and may be formed in a region where the compressive stress acts most or concentrates most. Since the cutout 150 (i.e., a groove having a specific shape) is formed in the lower surface of the substrate 10, the compressive stress acting on the lower surface of the substrate 10 may be reduced despite the bending process. As a result, the display device is prevented from being damaged.

[0143] As described above, according to one or more of the above-described embodiments of the present invention, the dead space area of ​​the display device is reduced or minimized while preventing cracks from being formed in the substrate.

[0144] It should be understood that the exemplary embodiments described herein should be considered to be descriptive only, and not for the purpose of limitation. Unless otherwise specifically noted, the description of the features or aspects within each embodiment should generally be considered to be applicable to other similar features or aspects in other embodiments.

[0145] While the invention has been particularly shown and described with reference to exemplary embodiments thereof, it will be understood by those skilled in the art that various changes in form and details may be made without departing from the spirit and scope of the invention as defined by the claims and their equivalents.

Claims

1. A display device, the display device include: substrate; A display unit, located on the substrate; A first inorganic layer, located on the display unit; a first organic layer, located on an upper surface of the first inorganic layer; a second inorganic layer, located on an upper surface of the first organic layer; a first dam located at an outer area of ​​the display unit; a second dam spaced apart from the first dam and located at an outer region of the first dam relative to the display unit; as well as The stress release layer directly covers an end portion of a region where the first inorganic layer and the second inorganic layer are in direct contact with each other, wherein the end portion is located between the first dam and the second dam.

2. The display device according to claim 1, It is characterized in that The stress release layer includes an organic material.

3. The display device according to claim 1, It is characterized in that The stress relaxation layer includes the same material as that of the first organic layer.

4. The display device according to claim 1, It is characterized in that The stress release layer is formed by using an inkjet process.

5. The display device according to claim 1, It is characterized in that The stress release layer is located on the first dam and the second dam, and has a height substantially equal to a height of the second inorganic layer.

6. The display device according to claim 1, It is characterized in that The display device further includes: The protective film is located under the substrate.

7. The display device according to claim 6, It is characterized in that The protection film is separated from a display area of ​​the display device and is located inside the display area.

8. The display device according to claim 6, It is characterized in that The upper edge of the protective film is rounded.

9. The display device according to claim 8, It is characterized in that The substrate has a cutout, Wherein, the cutout is separated from the upper edge of the protective film.

10. The display device according to claim 9, It is characterized in that The cutout has a triangular shape.

11. The display device according to claim 9, It is characterized in that The cutout has a semicircular shape.

12. The display device according to claim 9, It is characterized in that The cutout has a rectangular shape.

13. The display device according to claim 1, It is characterized in that The stress release layer is located between the ELVSS and the second dam.

14. A display device, the display device include: substrate; A display unit, located on the substrate; A first inorganic layer, located on the display unit; a first organic layer, located on an upper surface of the first inorganic layer; a second inorganic layer, located on an upper surface of the first organic layer; a first dam located at an outer area of ​​the display unit; a stress release layer, located on the substrate and located at an outer region of the first dam relative to the display unit; as well as a second dam, spaced apart from the first dam and located at an edge of the stress release layer, The end of the region where the first inorganic layer and the second inorganic layer are in direct contact is located between the first dam and the second dam and is directly covered by the stress release layer.

15. The display device according to claim 14, It is characterized in that The display device further includes: The protective film is located under the substrate.

16. The display device according to claim 15, It is characterized in that The protective film has a rounded upper edge.

17. The display device according to claim 16, It is characterized in that The substrate has a cutout at the lower surface, Wherein, the cutout is separated from the upper edge of the protective film.

18. A display device, the display device include: substrate; A display unit, located on the substrate; A first inorganic layer, located on the display unit; a first organic layer, located on an upper surface of the first inorganic layer; a second inorganic layer, located on an upper surface of the first organic layer; a first dam located at an outer area of ​​the display unit; a second dam spaced apart from the first dam and located at an outer region of the first dam relative to the display unit; a stress release layer, located on the substrate and located at an outer region of the first dam relative to the display unit; as well as a protective film, located below the substrate, wherein the protective film has a rounded upper edge, and The end of the region where the first inorganic layer and the second inorganic layer are in direct contact is located between the first dam and the second dam and is directly covered by the stress release layer.

19. The display device according to claim 18, It is characterized in that The display device further includes: A stress release layer is located between the ELVSS and the second dam and at an outer region of the ELVSS relative to the display unit.

20. The display device according to claim 19, It is characterized in that The stress release layer includes an organic material.

21. The display device according to claim 19, It is characterized in that The stress relaxation layer includes the same material as that of the first organic layer.

22. The display device according to claim 19, It is characterized in that The stress release layer is formed by using an inkjet process.

23. The display device according to claim 18, It is characterized in that The substrate has a cutout in a lower surface of the substrate, Wherein, the cutout is separated from the upper edge of the protective film.