A water-cooling mold for aluminum alloy wheels
By designing the cooling structure of grooves and water-cooling blocks in the aluminum alloy wheel water-cooled mold, and setting gaps and serrated grooves at the parting lines, the problem of rim shrinkage is solved, and the inner rim performance and mold life are improved.
Patent Information
- Application Number
- CN202011206276.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-11-03
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2040-11-03
AI Technical Summary
In the process of improving the performance of the inner rim, existing aluminum alloy wheel water-cooled molds lead to loosening problems in the rim area, affecting subsequent machining and increasing scrap rate.
Design an aluminum alloy wheel water-cooled mold, by setting grooves and water-cooling blocks on the top mold, forming a cooling water channel, and setting gaps and serrated grooves at the parting line to reduce the impact of water channel cooling on the rim. Retains the cooling effect of the inner rim.
It effectively improves the performance of the inner rim, reduces the adverse impact of waterway cooling on the rim, and improves the reliability of welding scars and the life of the mold.
Smart Images

Figure CN112170812B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of wheel casting, in particular to a water-cooling mould for an aluminium alloy wheel. Background Art
[0002] In the production process of low-pressure casting of aluminum wheels, customers have increasingly higher requirements for the performance of the inner rim. The current structural form of the aluminum alloy wheel water-cooling mold is helpful to improve the performance of the inner rim, but it has an adverse effect on the solidification process of the rim, especially for thick inner rim structure wheels. The casting quality of the inner rim position can only be guaranteed by sacrificing metal utilization. Apart from the metal utilization, it still brings great hidden dangers to the shrinkage of the rim in the subsequent machining process, and even leads to batch scrap. Therefore, the current structure of the aluminum alloy wheel water-cooling mold has great limitations and two-sidedness.
[0003] like Figure 1 As shown in the figure, the cooling design of the inner rim part is commonly used at present, which ensures the rapid cooling of the inner rim area and improves the performance of the inner rim by opening an annular water channel 1 at the upper end of the top mold. However, when the water channel 1 is opened, the temperature of the entire top mold area decreases, which greatly affects the shrinkage compensation of the rim area to the inner rim, and even causes shrinkage of the rim area. Summary of the invention
[0004] In view of this, the present invention aims to provide a water-cooling mold for an aluminum alloy wheel, which can effectively improve the performance of the inner wheel rim while avoiding the adverse effects of water channel cooling on the rim or other areas.
[0005] To achieve the above object, the technical solution of the present invention is achieved as follows:
[0006] A water-cooling mold for an aluminum alloy wheel comprises a top mold, wherein the top mold comprises an upper top mold and a lower top mold connected by bolts, the upper top mold is provided with a groove, a water-cooling block and a water-cooling pressing block abutting against the water-cooling block are sequentially arranged in the groove, and the water-cooling block and the bottom surface of the groove of the upper top mold are enclosed to form a cooling water channel.
[0007] In some embodiments, the parting line between the upper top mold and the lower top mold is arranged below the highest point of the inner rim of the wheel.
[0008] In some embodiments, the parting line between the upper top mold and the lower top mold is set 5-15 mm below the highest point of the inner rim of the wheel.
[0009] In some embodiments, the upper top mold protrudes beyond the lower top mold on the left side of the parting line.
[0010] In some embodiments, the upper top mold protrudes 0.2-0.5 mm from the lower top mold on the left side of the parting line.
[0011] In some embodiments, the length of the parting line is 5-10 mm, and the contact surfaces of the upper top mold and the lower top mold corresponding to the parting line are tightly matched.
[0012] In some embodiments, a gap is provided between the installation elevations of the upper top mold and the lower top mold.
[0013] In some embodiments, grooves are machined on both sides of the mating portion between the upper mold and the water cooling block.
[0014] In some embodiments, serrated grooves are machined on the mating surfaces of the water-cooling block and the water-cooling pressure block.
[0015] Compared with the prior art, the aluminum alloy wheel water-cooling mold of the present invention has the following advantages:
[0016] The water-cooled mold disclosed in the present invention retains the water channel cooling at the upper end of the top mold, which can effectively improve the performance of the inner rim, and minimizes the adverse effects of water channel cooling on the rim or other areas, while improving the reliability of weld scars and the life of the mold. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The accompanying drawings, which constitute a part of the present invention, are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute improper limitations on the present invention.
[0018] Figure 1 It is a schematic diagram of the existing water-cooling mold for aluminum alloy wheels.
[0019] Figure 2 This is a schematic diagram of the water-cooling mold for the aluminum alloy wheel of the present invention.
[0020] Figure 3 It is a partial enlarged schematic diagram of the parting surface of the water-cooling mold for the aluminum alloy wheel of the present invention.
[0021] Figure 4 It is a partially enlarged schematic diagram of the cooling water channel of the water-cooling mold for the aluminum alloy wheel of the present invention.
[0022] Description of reference numerals:
[0023] 1-Cooling water channel; 2-Water cooling block; 3-Weld scar; 4-Water cooling block; 5-Upper mold; 6-Bolt; 7-Inlet and outlet water pipes; 8-Lower mold; 9-Parting line. DETAILED DESCRIPTION
[0024] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments may be combined with each other.
[0025] The technical solution of the present invention will be clearly and completely described below with reference to the accompanying drawings and in combination with the embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0026] Reference below Figures 1 to 4 The aluminum alloy wheel water-cooling mold according to the embodiment of the present invention is described in conjunction with the embodiments.
[0027] The invention discloses a water-cooling mold for an aluminum alloy wheel, comprising a top mold, wherein the top mold comprises an upper top mold 5 and a lower top mold 8 connected by bolts 6, wherein a groove is provided on the upper top mold 5, wherein a water-cooling block 2 and a water-cooling pressing block 4 abutting against the water-cooling block 2 are arranged in sequence in the groove, and the water-cooling block 2 and the bottom surface of the groove of the upper top mold 5 enclose a cooling water channel 1. A parting line 9 between the upper top mold 5 and the lower top mold 8 is arranged 5-15 mm below the highest point of the inner rim of the wheel. The upper top mold 5 protrudes 0.2-0.5 mm from the lower top mold 8 on the left side of the parting line 9. The length of the parting line is 5-10 mm, and the contact surfaces of the upper top mold 5 and the lower top mold 8 corresponding to the parting line 9 are closely matched. A gap is provided between the installation vertical surfaces of the upper top mold 5 and the lower top mold 8. Grooves are processed on both sides of the matching part between the upper top mold 5 and the water-cooling block 2. A serrated groove is processed on the matching surface of the water-cooling block 2 and the water-cooling pressing block 4.
[0028] In some embodiments, according to the specific characteristics of the wheel shape, a parting line 9 is made between the upper and lower top molds 5-15 mm below the highest point of the inner rim product line. Since the cooling water channel 1 is located in the upper top mold 5, the parting line 9 is located below the highest point of the inner rim, and the highest point of the inner rim is located in the upper top mold 5. The cooling water channel 1 in the upper top mold 5 can fully cool the inner rim.
[0029] At the parting position of the upper top mold 5 and the lower top mold 8, the cooling conduction of the cooling water decreases sharply through the parting surface, and the water channel cooling causes the upper top mold 5 to shrink more than the lower top mold 8. In order to prevent the wheel from being difficult to demould or scratched, Figure 3 The position A enclosed by the middle ellipse retains a misalignment of 0.2-0.5 mm to leave a margin for the contraction of the upper top mold 5.
[0030] like Figure 3 As shown, the mating position B enclosed by the ellipse of the upper top mold 5 and the lower top mold 8 retains a mating surface of 5-10 mm. The upper top mold 5 and the lower top mold 8 are tightly matched on the mating surface, which prevents aluminum from escaping on the one hand and reduces the influence of the cooling of the upper top mold on the lower top mold on the other hand.
[0031] like Figure 3As shown, a gap of 0.5 mm is reserved at the matching positions C and D enclosed by ellipses between the upper top mold 5 and the lower top mold 8. The clearance between the upper top mold 5 and the lower top mold 8 is matched to reduce the influence of the cooling of the upper top mold 5 on the lower top mold 8.
[0032] like Figure 4 As shown, grooves of 0.2 mm are processed on both sides of the matching parts of the upper top mold 5 and the water-cooling block 2 to reduce the diffusion of cooling to both sides of the water channel, making it have better "directivity" to ensure the cooling of the inner rim.
[0033] like Figure 4 As shown, 1mm deep and evenly distributed serrated grooves are processed on the mating surfaces of the water-cooling block 2 and the water-cooling pressing block 4, which reduces the transmission of water channel cooling to the water-cooling pressing block 4 and reduces the drastic contraction and expansion of the water-cooling pressing block 4 during the production cycle, improves the reliability of the water channel weld scar, and ensures the life of the mold.
[0034] Compared with the prior art, the aluminum alloy wheel water-cooling mold of the present invention has the following advantages:
[0035] The water-cooled mold disclosed in the present invention retains the water channel cooling at the upper end of the top mold, which can effectively improve the performance of the inner rim, and minimizes the adverse effects of water channel cooling on the rim or other areas, while improving the reliability of weld scars and the life of the mold.
[0036] In the description of the present invention, it is necessary to understand that the terms "center", "longitudinal", "lateral", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the protection content of the present invention.
[0037] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0038] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or can communicate with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0039] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A water-cooled mold for an aluminum alloy wheel, comprising a top mold, characterized in that: The top mold comprises an upper top mold (5) and a lower top mold (8) connected by bolts (6); a groove is provided on the upper top mold (5); a water-cooling block (2) and a water-cooling pressure block (4) abutting against the water-cooling block (2) are arranged in sequence in the groove; the water-cooling block (2) and the bottom surface of the groove of the upper top mold (5) are enclosed to form a cooling water channel (1); The parting line (9) between the upper top mold (5) and the lower top mold (8) is arranged below the highest point of the inner rim of the wheel. The upper top mold (5) protrudes from the lower top mold (8) on the left side of the parting line (9). The contact surfaces of the upper top mold (5) and the lower top mold (8) corresponding to the parting line (9) are tightly matched. A gap is provided between the installation vertical surfaces of the upper top mold (5) and the lower top mold (8). Grooves are machined on both sides of the mating portion between the upper mold (5) and the water cooling block (2). The matching surfaces of the water-cooling block (2) and the water-cooling pressing block (4) are machined with sawtooth-shaped grooves.
2. The aluminum alloy wheel water-cooling mold according to claim 1, characterized in that: The parting line (9) between the upper top mold (5) and the lower top mold (8) is arranged 5-15 mm below the highest point of the inner rim of the wheel.
3. The aluminum alloy wheel water-cooling mold according to claim 1, characterized in that: The upper top mold (5) protrudes from the lower top mold (8) by 0.2-0.5 mm on the left side of the parting line (9).
4. The aluminum alloy wheel water-cooling mold according to claim 3, characterized in that: The length of the parting line is 5-10 mm.
Citation Information
Patent Citations
Water-cooled mold for casting aluminum alloy wheels and manufacturing method of water-cooled mold
CN105215333A
Water-cooling low-pressure casting mold for aluminum wheel
CN204209100U
Aluminum alloy wheel water cooling die
CN213614079U
Apparatus for molding a wheel for vehicle
KR1020190044800A