Novel organic compound for cover layer and organic light emitting element containing the same
By using aromatic amine compounds such as benzoxazole and benzothiazole substituted by elements such as O, S, and N as covering layer materials, the problems of insufficient film stability and external light extraction efficiency of organic light-emitting elements when exposed to ultraviolet rays are solved, achieving Organic light-emitting components with high efficiency, high color purity and long life.
Patent Information
- Application Number
- CN202011007445.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-23
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2040-09-23
AI Technical Summary
Existing organic light-emitting elements have deficiencies in external light extraction efficiency and stability. In particular, the film is prone to instability when exposed to ultraviolet light, affecting its lifespan and efficiency.
Use aromatic amine compounds including more than two benzozoles, benzothiazoles, etc. substituted by O, S, N and other elements as the covering layer material. By improving the refractive index and absorption wavelength, the stability to ultraviolet rays is enhanced, and through amination The reaction forms a compound for the covering layer with a high refractive index.
It improves external quantum efficiency and color purity, maintains high refractive index and stability against ultraviolet rays, prevents molecular recrystallization, and extends the life of organic light-emitting components.
Smart Images

Figure CN112538060B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to an organic compound for a covering layer and an organic light-emitting element comprising the organic compound for a covering layer. Background Art
[0002] Materials used as the organic layer in an organic light-emitting element can be roughly divided into light-emitting materials, hole injection materials, hole transport materials, electron transport materials, and electron injection materials according to their functions.
[0003] In addition, the above-mentioned luminescent materials can be divided into fluorescent materials originating from the singlet excited state of electrons and phosphorescent materials originating from the triplet excited state of electrons according to the luminescence mechanism, and can also be divided into blue, green, and red luminescent materials according to the luminescent color.
[0004] A common organic light-emitting element may adopt a structure in which an anode is formed on the upper part of a substrate, and a hole transport layer, a light-emitting layer, an electron transport layer and a cathode are sequentially formed on the upper part of the anode. Among them, the hole transport layer, the light-emitting layer and the electron transport layer are organic thin films composed of organic compounds.
[0005] The driving principle of the organic light emitting element having the above structure is as follows.
[0006] When a voltage is applied between the anode and the cathode, holes injected from the anode move to the light-emitting layer via the hole transport layer, and electrons injected from the cathode move to the light-emitting layer via the electron transport layer.
[0007] The holes and electrons are recombined in the light-emitting layer to generate excitons, and light is generated in the process of the excitons converting from an excited state to a ground state.
[0008] The efficiency of organic light-emitting elements can generally be divided into internal luminescence efficiency and external luminescence efficiency. The internal luminescence efficiency is related to the efficiency of generating excitons and realizing light conversion in organic layers between the first electrode and the second electrode, such as the hole transport layer, the light-emitting layer, and the electron transport layer. Theoretically, the internal luminescence efficiency of fluorescence is 25%, while that of phosphorescence is 100%.
[0009] In addition, the external luminous efficiency refers to the efficiency of extracting light generated in the organic layer to the outside of the organic light-emitting element. It is currently known that generally about 20% of the internal luminous efficiency can be extracted to the outside.
[0010] As a method of improving the above-mentioned light extraction efficiency, in order to prevent the light irradiated to the outside from being lost due to total reflection, various organic compounds with a refractive index of 1.7 or above are usually used as a covering layer. In order to improve the performance of organic light-emitting elements, efforts have been made to develop an organic compound with a high refractive index and thin film stability that can improve the external light-emitting efficiency.
[0011] Prior art literature
[0012] Patent Literature
[0013] (Patent Document 1) Korean Patent Publication No. 10-2004-0098238 Summary of the invention
[0014] The object of the present invention is to provide a method of Aromatic amine compounds including two or more condensed rings substituted by elements such as O, S, and N, such as azole and benzothiazole, are used as materials for the covering layer, which can improve the absorption intensity in the ultraviolet region and improve the refractive index due to the excellent film arrangement between molecules. It can also improve the stability to external air and moisture while preventing recrystallization between molecules and maintain the stability of the film when heat is generated during the driving process, thereby improving the external quantum efficiency and realizing a covering layer compound for an organic light-emitting element with high efficiency, high color purity, and long life, as well as an organic light-emitting element containing the above-mentioned covering layer organic compound.
[0015] As a means to solve the above problems,
[0016] An embodiment of the present invention provides a compound for a cover layer, which is a compound for a cover layer of an organic light-emitting element and is represented by the following Chemical Formula 1.
[0017]
Chemical formula 1
[0018]
[0019] In the above chemical formula 1,
[0020] X, X 1 , X 2 and X 3 are each independently C, CR, O, S, N, Se, Te, NR, CRR`, SiRR` or GeRR`, two or more of which are each independently O, S, N, Se, Te, NR, CRR`, SiRR` or GeRR`,
[0021] wherein R and R' are each independently hydrogen, deuterium, halogen, nitro, nitrile, substituted or unsubstituted C1-C30 alkyl, substituted or unsubstituted C2-C30 alkenyl, substituted or unsubstituted C1-C30 alkoxy, substituted or unsubstituted C1-C30 thiol, substituted or unsubstituted C6-C50 aryl, or substituted or unsubstituted C2-C50 heteroaryl, and adjacent R and R' or multiple R's may or may not form a ring by combining with each other,
[0022] Ar 1 and Ar 2 are each independently a substituted or unsubstituted C6-C50 aryl group, or a substituted or unsubstituted C2-C50 heteroaryl group,
[0023] L is a directly bonded, substituted or unsubstituted C6-C50 arylene group, or a substituted or unsubstituted C2-C50 heteroarylene group.
[0024] In addition, another embodiment of the present invention provides an organic light-emitting element, including: a first electrode; a second electrode; an organic layer, located between the inner sides of the first electrode and the second electrode; and a covering layer, arranged on the outer side of any one or more of the first electrode and the second electrode, containing the compound for the covering layer.
[0025] The compound for the cover layer according to one embodiment of the present invention is benzo[pi] Aromatic amine compounds including two or more condensed rings substituted with elements such as O, S, and N, such as oxazole and benzothiazole, can exhibit high color purity by maintaining a wide band gap in the region where visible light cannot be absorbed.
[0026] Furthermore, the absorption wavelength in the ultraviolet region can be increased while maintaining a high refractive index.
[0027] In addition, the external quantum efficiency can be improved and stability can be maintained when exposed to UV light.
[0028] In addition, the thin film arrangement between molecules is excellent, and the stability to external air and moisture can be improved while improving the refractive index.
[0029] In addition, the high Tg and Td can prevent the recrystallization between molecules, and at the same time, the stability of the film can be maintained when heat is generated during the driving process. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 This is a cross-sectional view schematically illustrating the structure of an organic light-emitting element according to an embodiment of the present invention.
[0031] Figure 2This is a graph illustrating the evaluation results of the absorption intensity in the ultraviolet region according to the example of the present invention.
[0032]
Explanation of symbols
[0033] 100: Substrate
[0034] 200: Hole injection layer
[0035] 300: Hole transport layer
[0036] 400: Luminous layer
[0037] 500: Electron transport layer
[0038] 600: Electron injection layer
[0039] 1000: 1st electrode
[0040] 2000: The second electrode
[0041] 3000: Overlay DETAILED DESCRIPTION
[0042] Before describing the present invention in detail, it should be understood that the terms used in this specification are only used to describe specific embodiments and are not intended to limit the scope of the present invention, which shall only be limited by the scope of the appended claims. Unless otherwise expressly stated, all technical terms and scientific terms used in this specification have the same meanings as those commonly understood by people with general knowledge.
[0043] Throughout this specification and claims, unless expressly stated otherwise, terms such as include, comprise, or comprising merely indicate the inclusion of the stated item, step, or series of items and steps, and do not exclude any other item, step, or series of items or steps in advance.
[0044] Throughout the specification and claims, the term "aryl" refers to groups such as phenyl, benzyl, naphthyl, biphenyl, terphenyl, fluorenyl, phenanthrenyl, triphenylene, phenylene, Benzotriphenylene, fluoranthene, benzofluorenyl, benzotriphenylene, benzo The term "heteroaryl" refers to a C5-50 aromatic hydrocarbon ring group having an aromatic ring such as an anthracene ring, an anthracene ring, a stilbene ring and a pyrenyl ring, and the term "heteroaryl" refers to a pyrrolyl, pyrazinyl, pyridyl, indolyl, isoindolyl, furyl, benzofuranyl, isobenzofuranyl, dibenzofuranyl, benzothiophenyl, dibenzothiophenyl, quinolyl, isoquinolyl, quinoxalinyl, carbazolyl, phenanthridinyl, acridinyl, phenanthrolinyl, thienyl and a pyridine ring, pyrazine ring, pyrimidine ring, pyridazine ring, triazine ring, indole ring, quinoline ring, acridinium ring, pyrrolidine ring, dibenzothiophenyl ring, Alkane ring, piperidine ring, morpholine ring, piperazine ring, carbazole ring, furan ring, thiophene ring, Azole ring, Oxadiazole ring, benzo The heterocyclic group composed of an azole ring, a thiazole ring, a thiadiazole ring, a benzothiazole ring, a benzotriazole ring, an imidazole ring, a benzimidazole ring, a pyran ring, or a dibenzofuran ring is a C3-50 aromatic ring containing at least one heteroelement.
[0045] Throughout this specification and claims, the term "substituted or unsubstituted" means substituted or unsubstituted by one or more groups selected from the group consisting of deuterium, halogen, amino, nitro, nitrile, C1-C30 alkyl, C2-C30 alkenyl, C1-C30 alkoxy, C3-C20 cycloalkyl, C3-C20 heteroalkyl, C6-C30 aryl, and C3-C30 heteroaryl. In addition, throughout the specification of this application, unless otherwise explicitly stated, the same symbols have the same meaning.
[0046] In addition, unless otherwise explicitly stated to the contrary, the various embodiments of the present invention may be combined with certain other embodiments. Next, the embodiments of the present invention and their effects will be described.
[0047] Specific examples of the compound for a covering layer of the present invention include compounds for a covering layer represented by the following Chemical Formula 1.
[0048]
Chemical formula 1
[0049]
[0050] In the above chemical formula 1,
[0051] X, X 1 , X 2 and X 3 are each independently C, CR, O, S, N, Se, Te, NR, CRR`, SiRR` or GeRR`, two or more of which are each independently O, S, N, Se, Te, NR, CRR`, SiRR` or GeRR`,
[0052] wherein R and R' are each independently hydrogen, deuterium, halogen, nitro, nitrile, substituted or unsubstituted C1-C30 alkyl, substituted or unsubstituted C2-C30 alkenyl, substituted or unsubstituted C1-C30 alkoxy, substituted or unsubstituted C1-C30 thiol, substituted or unsubstituted C6-C50 aryl, or substituted or unsubstituted C2-C50 heteroaryl, and adjacent R and R' or multiple R's may or may not form a ring by combining with each other,
[0053] Ar 1 and Ar 2 are each independently a substituted or unsubstituted C6-C50 aryl group, or a substituted or unsubstituted C2-C50 heteroaryl group,
[0054] L is a directly bonded, substituted or unsubstituted C6-C50 arylene group, or a substituted or unsubstituted C2-C50 heteroarylene group.
[0055] As described above, the compound for the covering layer of the present invention is an aromatic amine compound including two or more condensed rings substituted by elements such as O, S, and N. When used in the covering layer of an organic light-emitting element, it can exhibit high color purity by maintaining a wider band gap in the region where visible light cannot be absorbed, and can also improve the external quantum efficiency and maintain stability when exposed to ultraviolet rays.
[0056] In addition, the high Tg and Td can prevent the recrystallization between molecules, and at the same time, the stability of the film can be maintained when heat is generated during the driving process.
[0057] In addition, specific examples of the compound for a covering layer of the present invention include a compound for a covering layer represented by the following Chemical Formula 2.
[0058]
Chemical formula 2
[0059]
[0060] In the above chemical formula 2,
[0061] X, X 1 , X 2 , X 3 ,Ar 1 and Ar 2 Same as the definition in the above chemical formula 1,
[0062] R 1 Same as the definition of R or R' in the above chemical formula 1,
[0063] l is an integer from 0 to 5. Specifically, l may be 1 or more.
[0064] In the above-mentioned compound for a covering layer of the present invention, two or more fused rings substituted with elements such as O, S, and N are bonded to amine directly or via one or more phenylene groups, thereby maintaining a high refractive index.
[0065] In particular, when l is 1 or more, the absorption wavelength in the blue region can be minimized by the phenylene group adjacent to the amine, and the refractive index can also be effectively improved.
[0066] In addition, as specific examples of the compound for a covering layer of the present invention, there is included a compound for a covering layer represented by the following Chemical Formula 3.
[0067]
Chemical formula 3
[0068]
[0069] In the above chemical formula 3,
[0070] X 1 , X 2 , X 3 ,Ar 1 and Ar 2 Same as the definition in the above chemical formula 1,
[0071] Ar 3 Ar in the above chemical formula 1 1 or Ar 2 The definition of is the same, however, Ar 2 with Ar 3 The sum of the number of carbon atoms is less than 50,
[0072] R 2 Same as the definition of R or R' in the above chemical formula 1,
[0073] m is an integer from 0 to 3. Specifically, m may be 1 or more.
[0074] In the above-mentioned compound for covering layer of the present invention, X in the condensed ring is C or CH, and the above-mentioned condensed ring is directly bonded to amine or via one or more 1,4-phenylene groups, thereby maintaining a high refractive index.
[0075] In particular, in the case where m is 1 or more, the absorption wavelength in the ultraviolet region can be increased while having a high refractive index, thereby improving stability when exposed to external ultraviolet rays.
[0076] In addition, specifically, Ar in the above chemical formula 3 2 -Ar 3 It may contain at least 3 or more aryl or heteroaryl groups. For example, Ar 2In the above case, the refractive index can be higher and the absorption in the ultraviolet region can be increased.
[0077] In addition, as specific example compounds of the compound for a covering layer of the present invention, a compound for a covering layer of the following Chemical Formula 4 is included.
[0078]
Chemical formula 4
[0079]
[0080] In the above chemical formula 4,
[0081] X 1 , X 2 , X 3 and Ar 2 Same as the definition in the above chemical formula 1,
[0082] Ar 3 Ar in the above chemical formula 1 1 or Ar 2 The definition is the same as that of 2 with Ar 3 The sum of the number of carbon atoms is less than 50,
[0083] R 2 and R 3 Each independently has the same definition as R or R' in the above chemical formula 1,
[0084] m and n are each independently an integer of 0 to 3. Specifically, m and n may be 1 or more.
[0085] In the above-mentioned compound for covering layer of the present invention, X in the condensed ring is C or CH, and two or more condensed rings as above are contained. In addition, the two condensed rings are each directly bonded to amine or bonded via one or more 1,4-phenylene groups, thereby maintaining a high refractive index.
[0086] In particular, when m and n are 1 or more, the absorption wavelength in the ultraviolet region can be increased while having a high refractive index, thereby improving stability when exposed to external ultraviolet rays.
[0087] In addition, specifically, Ar in the above chemical formula 4 2 -Ar 3 It may contain at least 3 or more aryl or heteroaryl groups. For example, Ar 2 It can be a biphenyl group. In the case described above, with Ar 2 -Ar 3Compared with the case where one or two aromatic groups are included such as phenyl or biphenyl, the refractive index can be higher and the absorption in the ultraviolet region can be increased.
[0088] In addition, specifically, Ar in the above chemical formula 4 3 In the case where the naphthyl group is included as described above, it is possible to have a higher refractive index and maintain a lower deposition temperature, thereby effectively improving thermal stability.
[0089] In addition, as specific example compounds of the compound for a covering layer of the present invention, a compound for a covering layer of the following Chemical Formula 5 is included.
[0090]
Chemical formula 5
[0091]
[0092] In the above chemical formula 5,
[0093] X 1 , X 2 and X 3 Same as the definition in the above chemical formula 1,
[0094] R 2 , R 3 and R 4 Each independently has the same definition as R or R' in the above chemical formula 1,
[0095] m, n and o are each independently an integer of 0 to 3. Specifically, m, n and o may be 1 or more.
[0096] In the above-mentioned compound for covering layer of the present invention, X in the condensed ring is C or CH, and the compound contains three condensed rings as above. Furthermore, the three condensed rings are each directly bonded to amine or bonded via one or more 1,4-phenylene groups, thereby maintaining a high refractive index.
[0097] In particular, in the case where m, n, and o are 1 or more, the absorption wavelength in the ultraviolet region can be increased while having a high refractive index, thereby improving stability when exposed to external ultraviolet rays.
[0098] More specifically, at least one of m, n and o may be greater than 2. In this case, a higher refractive index can be achieved while also achieving an effect of increasing absorption in the ultraviolet region.
[0099] The compound for the covering layer of the present invention composed of any one of the above Chemical Formulas 3 to 5 can increase the absorption wavelength in the ultraviolet region while having a high refractive index, thereby improving stability when exposed to external ultraviolet rays, and can also minimize absorption in the blue region, which is conducive to the realization of high efficiency and high color purity.
[0100] As a specific example of the compound for the cover layer of the present invention, in any one of Chemical Formulae 1 to 5, X, X 1 , X 2 and X 3 At least one of the may be composed of O, S or N. Thereby, the bonding length of the heteroatom can be minimized, thereby achieving the effect of reducing the volume characteristics.
[0101] Specifically, in any one of the above Chemical Formulas 1 to 5, X, X 1 , X 2 and X 3 At least one of the may be composed of O. Thereby, the deposition temperature can be effectively lowered by reducing the molecular weight while maintaining a high refractive index.
[0102] More specifically, in any one of the above Chemical Formulas 1 to 5, X 1 , X 2 and X 3 One or more of them may be O, and one or more of them may be N. When each of O and N includes at least one or more as described above, absorption in the visible light region can be minimized, thereby effectively improving color purity and maintaining a low deposition temperature.
[0103] In any one of the above Chemical Formulas 1 to 5, X, X 1 , X 2 and X 3 At least one of the above may be composed of S. This allows the glass transition temperature (Tg) to be high while having a high refractive index, thereby facilitating formation of a stable thin film.
[0104] Specifically, in any one of the above Chemical Formulas 1 to 5, X 1 , X 2 and X 3 One or more of them may be S, and one or more of them may be N. When at least one O and one S are each included as described above, a wider ultraviolet region can be absorbed and the refractive index can be effectively improved.
[0105] As a specific example compound of the compound for the cover layer of the present invention, in any one of Chemical Formulae 1 to 5, R, R', R 1, R 2 , R 3 and R 4 Each of the above compounds of the present invention can be independently composed of hydrogen, deuterium, methyl, methoxy, phenyl or a combination thereof. The compound of the present invention can have a high refractive index by minimizing the volume characteristics of the substituent, and can also increase the absorption in the ultraviolet region, and can present a high refractive index because of the excellent film arrangement between molecules.
[0106] As a specific example compound of the compound for the cover layer of the present invention, in any one of Chemical Formulae 1 to 5, the above Ar 1 To Ar 3 Each of the compounds can be independently composed of phenyl, biphenyl, terphenyl, naphthyl, phenanthryl, triphenylene, carbazolyl, dibenzofuranyl, dibenzothiophene or a combination thereof. The compound of the present invention as described above can have a high refractive index by minimizing the volume characteristics of the substituent, can also increase the absorption in the ultraviolet region, and can present a high refractive index because of the excellent film arrangement between molecules.
[0107] Specifically, the above Ar 1 To Ar 3 One or more of the may include a naphthyl group. The compound of the present invention as described above can have a higher Tg and a lower deposition temperature while maintaining a high refractive index.
[0108] As a specific example compound of the compound for the cover layer of the present invention, in any one of Chemical Formulae 1 to 5, the above Ar 1 To Ar 3 Each can be independently represented by any one of the following structural formulas B-1 to B-7.
[0109]
[0110] In the above B-1 to B-7, q is an integer of 0-5.
[0111] Specifically, the above Ar 1 To Ar 3 Each of them can be independently one of the above structural formulas B-2 to B-7, and can include a substituted or unsubstituted condensed ring formed by condensation of two or more rings as described above. Furthermore, q in this case can be an integer greater than 2.
[0112] As specific example compounds of the compound for a cover layer of the present invention, the above Chemical Formula 1 may be represented by any one of the following compounds.
[0113]
[0114]
[0115]
[0116]
[0117]
[0118]
[0119]
[0120]
[0121]
[0122]
[0123]
[0124]
[0125]
[0126]
[0127]
[0128]
[0129]
[0130]
[0131]
[0132]
[0133]
[0134]
[0135]
[0136]
[0137]
[0138]
[0139]
[0140]
[0141]
[0142]
[0143]
[0144]
[0145]
[0146]
[0147]
[0148]
[0149]
[0150]
[0151]
[0152]
[0153]
[0154]
[0155]
[0156]
[0157]
[0158]
[0159]
[0160]
[0161]
[0162]
[0163]
[0164] One embodiment of the compound for a covering layer of the present invention can be prepared by an amination reaction, and its general reaction formula is shown below.
[0165]
[0166] Next, an organic light emitting element according to an embodiment of the present invention will be described in detail.
[0167] According to an implementation example of the present invention, an organic light-emitting element may include a first electrode, a second electrode, an organic layer between the first electrode and the second electrode, and a covering layer. The covering layer may be arranged outside one or more of the first electrode and the second electrode.
[0168] Specifically, the thickness of the above-mentioned covering layer can be 100 to
[0169] Among them, the side adjacent to the organic layer between the first electrode and the second electrode is called the inner side, and the side not adjacent to the organic layer is called the outer side. That is, when the covering layer is arranged on the outer side of the first electrode, the first electrode will be between the covering layer and the organic layer, and when the covering layer is arranged on the outer side of the second electrode, the second electrode will be between the covering layer and the organic layer.
[0170] According to an implementation example of the present invention, one or more organic layers may be interposed between the first electrode and the second electrode of the organic light-emitting element, and a covering layer may be formed outside one or more of the first electrode and the second electrode. That is, the covering layer may be formed on the outside of the first electrode and the outside of the second electrode at the same time, or may be formed only on the outside of the first electrode or the outside of the second electrode.
[0171] Furthermore, the above-mentioned covering layer may include the compound for a covering layer according to the present invention, and may include the compound for a covering layer according to the present invention alone, or include two or more or simultaneously include known compounds.
[0172] In addition, the organic layer may include a hole transport layer, a light emitting layer, and an electron transport layer which generally constitute a light emitting portion, but is not limited thereto.
[0173] Specifically, an organic light-emitting element according to an implementation example of the present invention may include one or more organic layers constituting a light-emitting portion such as a hole injection layer (HIL), a hole transport layer (HTL), a light-emitting layer (EML), an electron transport layer (ETL) and an electron injection layer (EIL) between a first electrode (anode) and a second electrode (cathode).
[0174] Figure 1 The organic light emitting element according to an embodiment of the present invention is schematically illustrated in a cross-sectional view. Figure 1The structure shown is manufactured.
[0175] The organic light-emitting element can be formed by stacking a substrate 100, a covering layer 3000, a first electrode 1000, a hole injection layer 200, a hole transport layer 300, a light-emitting layer 400, an electron transport layer 500, an electron injection layer 600, a second electrode 2000 and a covering layer 3000 in this order from the bottom.
[0176] The substrate 100 may be a substrate commonly used in an organic light-emitting element, and in particular, may be a transparent glass substrate or a flexible plastic substrate having excellent mechanical strength, thermal stability, transparency, surface smoothness, ease of handling, and waterproofness.
[0177] The first electrode 1000 is used as a hole injection electrode for injecting holes into the organic light emitting element. The first electrode 1000 is made of a material with a work function as low as possible to achieve hole injection, and can be formed of transparent materials such as indium tin oxide (ITO), indium zinc oxide (IZO) and graphene.
[0178] The hole injection layer 200 can be formed by depositing a hole injection layer material on the upper part of the first electrode 1000 by a method such as vacuum deposition, spin coating, casting, Langmuir-Blodgett (LB) method, etc. When the hole injection layer 200 is formed by vacuum deposition, the deposition conditions will vary depending on the compound used as the material of the hole injection layer 200, the required structure of the hole injection layer 200, and the thermal properties. Generally, the deposition temperature can be 50-500°C, 10 -8 Up to 10 -3 Torr vacuum degree, 0.01 to The deposition rate is The layer thickness can be appropriately selected within a range of 1 to 5 μm. In addition, a charge generation layer can be additionally deposited on the surface of the hole injection layer 200 as needed. As the charge generation layer material, a general material can be used, for example, hexacyano-hexaazatriphenylene (HATCN) can be used.
[0179] Next, the hole transport layer 300 can be formed by depositing a hole transport layer material on the upper part of the hole injection layer 200 using a method such as vacuum deposition, spin coating, casting, Langmuir-Brockett (LB) method, etc. When the hole transport layer 300 is formed by the vacuum deposition method, the deposition conditions will vary depending on the compound used, but it is generally preferred to select conditions that are almost the same as those for the formation of the hole injection layer 200. The hole transport layer 300 can be formed using known compounds. The hole transport layer 300 as described above can be more than one layer, and although in Figure 1 Although not shown in the figure, a light-emitting auxiliary layer may be additionally formed on the upper part of the hole transport layer 300 .
[0180] The light-emitting layer 400 can be formed by depositing the light-emitting layer material on the hole transport layer 300 or the light-emitting auxiliary layer by a method such as vacuum deposition, spin coating, casting, Langmuir-Brødt (LB) method, etc. When the light-emitting layer 400 is formed by the vacuum deposition method, the deposition conditions will vary depending on the compound used, but it is generally preferred to select conditions within the same range as those for forming the hole injection layer 200. As the light-emitting layer material, a known compound can be used as a main agent or a dopant.
[0181] In addition, when a phosphorescent dopant is used in the light-emitting layer material, in order to prevent triplet excitons or holes from diffusing to the electron transport layer 500, a stacked hole blocking material (HBL) can be added on the upper part of the light-emitting layer 400 by vacuum deposition or spin coating. The hole blocking material used in this case is not particularly limited, and any known material can be selected and used. For example, Oxadiazole derivatives or benzotriazole derivatives, o-phenanthroline derivatives or hole blocking materials described in Japanese Patent Laid-Open No. 11-329734 (A1), among which the most representative ones include Balq (bis (8-hydroxy-2-methylquinoline) - (4-phenylphenoxy) aluminum), o-phenanthroline compounds (for example: BCP (bathocuproine) of UDC), etc. As described above, the light-emitting layer 400 of the present invention may include more than one layer or more than two layers of blue light-emitting layers.
[0182] The electron transport layer 500 is formed on the upper part of the light emitting layer 400 and can be formed by methods such as vacuum deposition, spin coating, casting, etc. The deposition conditions of the electron transport layer 500 will vary depending on the compound used, but it is generally preferred to select conditions that are almost the same as those for forming the hole injection layer 200.
[0183] The electron injection layer 600 may be formed by depositing an electron injection layer material on the electron transport layer 500 , and may be formed by a method such as vacuum deposition, spin coating, or casting.
[0184] The hole injection layer 200 , the hole transport layer 300 , the light emitting layer 400 , and the electron transport layer 500 of the organic light emitting element may be manufactured using the following materials, but are not limited thereto.
[0185]
[0186] The second electrode 2000 is used as an electron injection electrode and can be formed on the upper part of the electron injection layer 600 by vacuum deposition or spin coating. A variety of metals can be used as the material of the second electrode 2000. Specific examples include materials such as aluminum, gold, silver, magnesium, etc., but are not limited thereto.
[0187] The organic light-emitting element of the present invention can not only use the organic light-emitting element as described above including the covering layer 3000, the first electrode 1000, the hole injection layer 200, the hole transport layer 300, the light-emitting layer 400, the electron transport layer 500, the electron injection layer 600, the second electrode 2000 and the covering layer 3000, but can also use organic light-emitting elements of various structures, and can also add one or two intermediate layers as needed.
[0188] Furthermore, the thickness of each organic layer formed by the present invention can be adjusted as required, and specifically can be 10 to 1000 nm, and more specifically can be 20 to 150 nm.
[0189] The above-mentioned covering layer 3000 is as follows Figure 1 As shown in FIG. 1 , the cover layer 3000 may be formed on the outer side of the two side surfaces of the first electrode 1000 where the hole injection layer 200 is not formed. In addition, the cover layer 3000 may be formed on the outer side of the two side surfaces of the second electrode 2000 where the electron injection layer 600 is not formed, but the present invention is not limited thereto. The cover layer 3000 may be formed by a deposition process, and the thickness of the cover layer 3000 may be 100 to 1000 μm. More specifically, it can be 300 to By adjusting the thickness as described above, the problem of a decrease in the transmittance of the cover layer 3000 can be prevented.
[0190] In addition, although Figure 1Although not shown in the figure, according to an embodiment of the present invention, an organic layer for performing various functions may be additionally formed between the cover layer 3000 and the first electrode 1000 or between the cover layer 3000 and the second electrode 2000. Alternatively, an organic layer for performing various functions may also be additionally formed on the upper portion (outer surface) of the cover layer 3000, but the present invention is not limited thereto.
[0191] Next, an organic light emitting element including a cover layer according to an embodiment of the present invention will be described in detail with reference to manufacturing examples and embodiments. The following manufacturing examples and embodiments are only used to illustrate the present invention, and the scope of the present invention is not limited to the following manufacturing examples and embodiments.
[0192] <Production Example 1> Synthesis of Compound 13
[0193]
[0194] Using a round bottom flask, 2-(4-bromophenyl)benzo[d] 2-(4-bromophenyl)benzo[d]oxazole 2.0 g, 4'-(naphthalen-2-yl)-N-(4-(naphthalen-2-yl)phenyl)-[1,1'-biphenyl]-4-amine 4.0 g, t-BuONa 1.0 g, Pd 2 (dba) 3 0.3g, (t-Bu) 3 0.3 ml of P was dissolved in 100 ml of toluene and then refluxed with stirring. The reaction was confirmed by thin layer chromatography (TLC) and the reaction was terminated by adding water. The organic layer was extracted with MC (methylene chloride) and filtered under reduced pressure and then recrystallized to obtain 3.6 g of compound 13 (yield 71%).
[0195] m / z: 690.27 (100.0%), 691.27 (55.6%), 692.27 (15.6%), 693.28 (2.7%)
[0196] <Production Example 2> Synthesis of Compound 61
[0197]
[0198] Compound 61 was prepared by the same method as in Preparation Example 1, except that 4-(naphthalen-2-yl)aniline was used instead of 4'-(naphthalen-2-yl)-N-(4-(naphthalen-2-yl)phenyl)-[1,1'-biphenyl]-4-amine. (Yield: 68%)
[0199] m / z: 605.21 (100.0%), 606.21 (46.6%), 607.22 (10.2%), 608.22 (1.7%)
[0200] <Production Example 3> Synthesis of Compound 62
[0201]
[0202] The same method as in Preparation Example 1 was used to prepare Compound 62, except that 4'-(naphthalen-2-yl)-[1,1'-biphenyl]-4-amine was substituted for 4'-(naphthalen-2-yl)-N-(4-(naphthalen-2-yl)phenyl)-[1,1'-biphenyl]-4-amine. (Yield: 65%)
[0203] m / z: 681.24(100.0%), 682.24(53.0%), 683.25(13.8%), 684.25(2.6%)
[0204] <Production Example 4> Synthesis of Compound 166
[0205]
[0206] The same method as in Preparation Example 1 was used to prepare the product, except that 2-(4-bromophenyl)benzo[d]thiazole and bis(4-(naphthalen-2-yl)phenyl)amine were used instead of 2-(4-bromophenyl)benzo[d]thiazole. Compound 166 was synthesized from 2-(4-bromophenyl)benzo[d]oxazole and 4'-(naphthalen-2-yl)-N-(4-(naphthalen-2-yl)phenyl)-[1,1'-biphenyl]-4-amine. (Yield: 66%)
[0207] m / z: 630.21 (100.0%), 631.22 (49.0%), 632.22 (12.1%), 632.21 (4.9%), 633.21 (2.2%), 633.22 (2.0%), 631.21 (1.5%)
[0208] <Production Example 5> Synthesis of Compound 169
[0209]
[0210] The same method as in Preparation Example 1 was used to prepare the product, except that 2-(4-bromophenyl)benzo[d]thiazole was used instead of 2-(4-bromophenyl)benzo[d] Compound 169 was synthesized from 2-(4-bromophenyl)benzo[d]oxazole (yield: 63%).
[0211] m / z: 706.24 (100.0%), 707.25 (55.6%), 708.25 (15.6%), 708.24 (4.9%), 709.25 (2.9%), 709.24 (2.5%), 707.24 (1.5%)
[0212] <Production Example 6> Synthesis of Compound 70
[0213]
[0214] The same method as in Preparation Example 1 was used to prepare the bis(4-(benzo[d]oxazol-2-yl)phenyl)amine) and 2-(4'-bromo-[1,1'-biphenyl]-4-yl)benzo[d] 2-(4'-bromo-[1,1'-biphenyl]-4-yl)benzo[d]oxazole) substituted with 2-(4-bromophenyl)benzo[d] Compound 70 was synthesized from 2-(4-bromophenyl)benzo[d]oxazole and 4'-(naphthalen-2-yl)-N-(4-(naphthalen-2-yl)phenyl)-[1,1'-biphenyl]-4-amine. (Yield: 71%)
[0215] m / z: 672.22 (100.0%), 673.22 (49.1%), 674.22 (13.0%), 675.23 (1.8%), 673.21 (1.5%)
[0216] <Production Example 7> Synthesis of Compound 58
[0217]
[0218] The same method as in Preparation Example 1 was used to prepare the bis(4-(benzo[d]oxazol-2-yl)phenyl)amine and 4-bromo-1,1'-biphenyl were used to replace 2-(4-bromophenyl)benzo[d] Compound 58 was synthesized from 2-(4-bromophenyl)benzo[d]oxazole and 4'-(naphthalen-2-yl)-N-(4-(naphthalen-2-yl)phenyl)-[1,1'-biphenyl]-4-amine. (Yield: 64%)
[0219] m / z: 555.19 (100.0%), 556.20 (41.5%), 557.20 (9.2%), 558.20 (1.3%), 556.19 (1.1%)
[0220] <Production Example 8> Synthesis of Compound 59
[0221]
[0222] The same method as in Preparation Example 1 was used to prepare the bis(4-(benzo[d]oxazol-2-yl)phenyl)amine and 4-bromo-1,1':4',1"-terphenyl were substituted for 2-(4-bromophenyl)benzo[d] Compound 59 was synthesized by using 2-(4-bromophenyl)benzo[d]oxazole and 4'-(naphthalen-2-yl)-N-(4-(naphthalen-2-yl)phenyl)-[1,1'-biphenyl]-4-amine. (The yield was 59%)
[0223] m / z: 631.23 (100.0%), 632.23 (48.0%), 633.23 (12.0%), 634.24 (1.7%), 632.22 (1.1%)
[0224] <Production Example 9> Synthesis of Compound 69
[0225]
[0226] The same method as in Preparation Example 1 was used to prepare the bis(4-(benzo[d]oxazol-2-yl)phenyl)amine and 2-(4-bromophenyl)benzo[d] 2-(4-bromophenyl)benzo[d]oxazole (2-(4-bromophenyl)benzo[d]oxazole) Compound 69 was synthesized from 2-(4-bromophenyl)benzo[d]oxazole and 4'-(naphthalen-2-yl)-N-(4-(naphthalen-2-yl)phenyl)-[1,1'-biphenyl]-4-amine. (Yield: 56%)
[0227] m / z: 596.18 (100.0%), 597.19 (42.6%), 598.19 (10.1%), 599.19 (1.6%), 597.18 (1.5%)
[0228] Manufacturing of organic light-emitting devices
[0229] according to Figure 1 The organic light emitting element is manufactured according to the structure described in , but a part of the layers are omitted as described below, and a covering layer 3000 is formed only on the upper part. Specifically, the organic light emitting element is manufactured by stacking the first electrode 1000, the hole injection layer 200, the hole transport layer 300, the light emitting layer 400, the electron transport layer 500, the electron injection layer 600, the second electrode 2000 and the covering layer 3000 in this order from the bottom. The substances shown in the following Table 1 are applied to the hole injection layer 200, the hole transport layer 300, the light emitting layer 400 and the electron transport layer 500.
[0230]
Table 1
[0231]
[0232] <Example 1> Manufacturing of organic light-emitting devices
[0233] On an indium tin oxide (ITO) substrate having a reflective layer containing Ag, a hole injection layer HI01 is formed. HATCN Hole transport layer HT01 After film formation, the light emitting layer was doped with 3% BH01:BD01. Then, as the electron transport layer, ET01:Liq (1:1) After film formation, LiF is deposited Next, MgAg was deposited to a thickness of 15 nm, and then the compound prepared in Preparation Example 1 was deposited as a covering layer on the cathode. The organic light emitting element was manufactured by encapsulating the above elements in a glove box.
[0234] <Example 2 to Example 9> Manufacturing of organic light-emitting devices
[0235] The same method as in Example 1 was used to produce organic light-emitting devices by forming a cover layer using the compounds produced in Production Examples 2 to 9, respectively.
[0236] <Comparative Examples 1 to 3>
[0237] The same method as in Example 1 was used to produce organic light-emitting devices, and the cover layers were formed using Comparative Examples 1 (Ref. 1) to 3 (Ref. 3) shown in Table 2 below.
[0238]
Table 2
[0239]
[0240] <Test Example 1> Performance evaluation of organic light emitting element
[0241] By applying voltage to a Kiethley 2400 source measurement unit to inject electrons and holes and measuring the brightness of the emitted light using a Konica Minolta spectroradiometer (CS-2000), the performance of the organic light-emitting elements of Examples 1 to 9 and Comparative Examples 1 to 3, namely, the current density and brightness relative to the applied voltage, were evaluated under atmospheric pressure conditions. The results are shown in Table 3.
[0242]
Table 3
[0243] Op.V <![CDATA[mA / cm 2 ]]> Cd / A CIEx CIE LT97 Example 1 3.40 10 7.81 0.139 0.044 185 Example 2 3.41 10 7.56 0.141 0.045 177 Example 3 3.40 10 7.84 0.140 0.044 183 Example 4 3.41 10 8.01 0.139 0.044 170 Example 5 3.40 10 8.17 0.140 0.043 175 Example 6 3.40 10 8.29 0.140 0.042 190 Example 7 3.41 10 7.34 0.138 0.047 161 Example 8 3.41 10 7.57 0.141 0.045 175 Example 9 3.41 10 7.60 0.141 0.045 178 Comparative Example 1 3.41 10 6.72 0.131 0.054 73 Comparative Example 2 3.42 10 7.05 0.130 0.050 111 Comparative Example 3 3.41 10 6.92 0.133 0.052 105
[0244] By comparing the embodiments of the present invention, it can be found that compared with Comparative Example 1 and Comparative Example 2, the present invention can be The volume characteristics are minimized and the refractive index is high by combining azole and benzothiazole with an aromatic amine, while the absorption wavelength in the ultraviolet region can be increased and the efficiency and life of the organic light-emitting element can be effectively improved at a higher Tg. In addition, compared with Comparative Example 3, the polarizability can be increased by substitution of more than two hetero elements and a stable film can be formed by excellent film arrangement between molecules, so that the refractive index can be effectively improved even with a small molecular weight, thereby realizing an organic light-emitting element with high color purity, high efficiency and long life.
[0245] <Test Example 2> Evaluation of Refractive Index
[0246] The compounds of Preparation Examples 1, 3 and 5 and the compounds of Comparative Examples 1 (Ref. 1), Comparative Examples 2 (Ref. 2) and Comparative Examples 3 (Ref. 3) were used to form a 30 nm thick deposited film on a silicon substrate using a vacuum deposition device, and then the refractive index at 450 nm was measured using an ellipsometer device (JA Woollam Co. Inc, M-2000X). The results are shown in Table 4 below.
[0247]
Table 4
[0248]
[0249] As shown in Table 4, it was confirmed that the compounds of Production Examples 1, 3, and 5 of the present invention exhibited a high refractive index of 2.30 or more, specifically 2.35 or more, and more specifically 2.4 or more.
[0250] <Test Example 3> Evaluation of absorption intensity in the ultraviolet region
[0251] In the ultraviolet region, the compounds of Preparation Examples 1 (Compound 13) and 3 (Compound 62) and the compound of Comparative Example 1 (Ref. 1) were used to form a 30nm thick deposited film on a silicon substrate using a vacuum deposition device, and then the absorption wavelength in the range of 250nm to 1000nm was measured using an ellipsometer device (JA Woollam Co. Inc, M-2000X). The results are as follows: Figure 2 shown.
[0252] In the ultraviolet absorption region of 380 nm, the absorption intensity of the compounds of Preparation Examples 1 and 3 of the present invention is increased to 0.8 or more, specifically, 0.9 or more, and it can be confirmed that the absorption intensity is increased by more than 30%, specifically, more than 50%, compared with the compound of Comparative Example (Ref. 1).
Claims
1. A compound for a covering layer represented by Chemical Formula 3 or Chemical Formula 4, Features: Chemical formula 3 In the above chemical formula 3, X 1 O or S, X 2 C, X 3 For N, R 2 is hydrogen or deuterium, Ar 1 Composed of a phenyl group and a naphthyl group; a biphenyl group and a naphthyl group; or a biphenyl group, Ar 2 is biphenylene, Ar 3 is naphthyl, m is an integer from 0 to 3, but not 3, Chemical formula 4 In the above chemical formula 4, X 1 , X 2 , X 3 ,Ar 2 ,Ar 3 , m and R 2 As defined in the above chemical formula 3, R 3 independently with R in the above chemical formula 3 2 The definition of is the same as that of , with n being 1.
2. The compound for covering layer according to claim 1, Features: In the above Chemical Formula 4, m is 2.
3. The compound for covering layer according to claim 1, Features: The above X 1 is O.
4. The compound for covering layer according to claim 1, Features: The above X 1 For S.
5. The compound for covering layer according to claim 1, Features: The above Ar 1 is a combination of phenyl and naphthyl; or a combination of biphenyl and naphthyl.
6. The compound for covering layer according to claim 1, Features: The above chemical formula 3 is any one of the following compounds 2, 3, 12, 13, 14, 55, 62, 158, 159, 168, 169, 170, 211, and 218, 7. An organic light emitting element, It is characterized in that include: a first electrode and a second electrode; An organic layer, located inside the first electrode and the second electrode; as well as, The covering layer is disposed outside one or more of the first electrode and the second electrode, and contains the compound for a covering layer according to any one of claims 1 to 6.
Citation Information
Patent Citations
Filter assembly for oxygen generator
KR1020040098238A
Organic electroluminescent element
CN107431143A
Organic compound based on heteroaryl amine structure and application thereof to OLED (Organic Light Emitting Diode)
CN109761967A
Heteroaryl amine structure based organic compounds and applications thereof
CN109824659A
Electroluminescent compound and electroluminescent device including same