Semiconductor devices and semiconductor apparatus
By depositing the base metal layer and additional metal layer on the sub-surface of the substrate, solder prevents the intrusion of the substrate through-holes, the problem of semiconductor device desorption caused by the solder under ambient temperature changes is solved, and the patch strength of the assembled substrate is improved.
Patent Information
- Application Number
- CN202110239519.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-02-15
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2039-02-15
AI Technical Summary
In the prior art, when the substrate through hole is connected to the source pad by solder, the solder repeatedly shrinks and expands under ambient temperature changes, causing the semiconductor device to desorb or weaken the patch to the assembled substrate. strength.
The base metal layer and the additional metal layer are deposited on the sub-surface of the substrate. The additional metal layer has different wettability to the solder, preventing the solder from entering the substrate through-holes, and making the base metal layer partially remove the additional metal layer, making the base metal layer Contact with solder, leaving a vacant space in the substrate through-hole to prevent solder from entering.
Effectively prevent solder from invading the through holes of the substrate, reduce cracks caused by temperature changes, enhance the patch strength of semiconductor devices on the assembled substrate, and avoid the strength reduction caused by solder expansion and contraction.
Smart Images

Figure CN112864028B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority from Japanese patent application JP2018-025680 filed on February 16, 2018, the entire contents of which are incorporated herein by reference. Technical Field
[0003] The present invention relates to a semiconductor device and a semiconductor apparatus. Background Art
[0004] The semiconductor device is usually mounted on the assembly substrate using solder, especially eutectic solder such as gold tin (AuSn). Japanese Patent Application Laid-Open No. JP2015-035495A discloses a method for forming a back metal. In addition, a substrate through hole through the substrate is a common technique for stabilizing the ground potential connected to the source pad, which is connected to the source of a field effect transistor (FET) type semiconductor device. The substrate through hole directly connects the source to the ground line in the back of the substrate.
[0005] However, when a substrate patch having a through-substrate hole is mounted on an assembly substrate by soldering, the solder intrudes into the through-substrate hole and solidifies at the through-substrate hole. Such solder repeatedly contracts and expands according to changes in ambient temperature, which causes the semiconductor device to be detached from the assembly substrate or weakens the strength of the patch to the assembly substrate. Summary of the invention
[0006] One aspect of the present invention relates to a semiconductor device, which includes a substrate having a main surface and a secondary surface opposite to the main surface. The main surface is provided with a semiconductor active device. The semiconductor device also includes a base metal layer deposited on the secondary surface and in a substrate through hole, and an additional metal layer on the base metal layer, the additional metal layer having a different wettability to solder than the base metal layer, whereby the solder can contact the base metal layer and is repelled by the additional metal layer. The semiconductor device is patched on the assembly substrate by inserting solder between the secondary surface of the substrate and the assembly substrate. The base metal layer in a portion other than the substrate through hole and the periphery of the substrate through hole is brought into contact with the solder by partially removing the additional metal layer. There is a vacancy in the substrate through hole. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] For a better understanding of the embodiments, reference will now be made, by way of example only, to the accompanying drawings, in which:
[0008] Figure 1A is a plan view of a semiconductor device according to an embodiment, and Figure 1B It is along Figure 1A A cross-sectional view of a semiconductor device including a cross-sectional view of a semiconductor device taken along line IB-IB shown in FIG.
[0009] FIG. 2A to FIG. 2F yes Figure 1B A cross-sectional view of the semiconductor device shown in FIG. 1 at various steps of a method for forming the semiconductor device;
[0010] FIG. 3A to FIG. 3F yes Figure 1B The semiconductor device shown in Figure 2F cross-sectional views at various steps of the method following the steps shown;
[0011] 4A to 4F yes Figure 1B The semiconductor device shown in Figure 3F cross-sectional views at various steps of the method following the steps shown; and
[0012] Figure 5 is a cross-sectional view of a conventional semiconductor device. Specific implementation plan
[0013] Next, some embodiments according to the present invention will be described with reference to the accompanying drawings. In the description of the accompanying drawings, the same or similar numerals or symbols will refer to the same or similar elements without repeated description.
[0014] First embodiment
[0015] Figure 1A 1 is a plan view showing a semiconductor device 100 according to a first embodiment of the present invention. The semiconductor device 100 is a field effect transistor (FET) type, which is provided with a substrate 10, a gate pad 12, a gate finger 13, a source pad 14, a source finger 15, a drain pad 16, and a drain finger 17. The substrate 10 as an insulating substrate may be made of silicon carbide (SiC), sapphire (Al 2 O 3 ) etc. A channel layer made of gallium nitride (GaN), a barrier layer made of aluminum gallium nitride (AlGaN), etc. are formed in the substrate 10, wherein the channel layer and the barrier layer form a two-dimensional electron gas (2DEG) at the interface therebetween, more specifically, a two-dimensional electron gas is formed in the channel layer near the interface between the channel layer and the barrier layer. The channel layer can be used as a channel for electron transmission.
[0016] The substrate 10 is provided with pads 12, 14 and 16 and fingers 13, 15 and 17 in its main surface. The gate finger 13, the source finger 15 and the drain finger 17 extend from the respective pads 12, 14 and 16. One gate finger 13 is placed between one source finger 15 and one drain finger 17 to form one transistor element; and several elements constitute the FET 100. The source finger 15 and the drain finger 17 are formed by stacking titanium (Ti) and aluminum (Al) metals, and the source pad 14 and the drain pad 16 mainly include a gold (Au) layer. The Au layer also covers the source finger 15 and the drain finger 17. The gate pad 12 and the gate finger 13 include stacked metals of nickel (Ni), palladium (Pd) and gold (Au).
[0017] Figure 1B It is along Figure 1A A cross-sectional view of a semiconductor device including a cross-sectional view of a semiconductor device 100 taken along line Ib-Ib shown in FIG. Figure 1A and Figure 1B As shown in FIG. 1 , the substrate 10 is further provided with a substrate through hole 10a that passes through from the secondary surface to the primary surface. The source pad 14 in the primary surface overlaps with the substrate through hole 10a. Figure 1B As shown, the secondary surface of the substrate 10 is provided with a first metal layer 20 and a second metal layer 22, wherein the second metal layer 22 is formed by plating. The first metal layer 20 and the second metal layer 22 are aspects of the base metal layer of the present invention. The first metal layer 20 covering the secondary surface of the substrate 10 and the side of the substrate through hole 10a is in contact with the source pad 14 in the main surface of the substrate 10. The second metal layer 22 partially covering the first metal layer 20 around the substrate through hole 10a can stabilize the ground potential, that is, the second metal layer 22 is provided with a ground line (GND) in the semiconductor active device in the main surface. The second metal layer 22 can be formed by electroplating using the first metal layer 20 as a seed metal. The second metal layer 22 is partially covered by a third metal layer 24 in and around the substrate through hole 10a, wherein the third metal layer 24 prevents the solder 32 from invading the substrate through hole 10a. The third metal layer 24 is an aspect of the additional metal layer of the present invention. Therefore, the substrate through hole 10a leaves a vacancy 50 therein.
[0018] The first metal layer 20 is stacked from the side in contact with the secondary surface of the substrate 10 with a thickness of 50nm to 200nm of an alloy of nickel (Ni) and chromium (Cr) (which is generally referred to as nickel-chromium alloy (NiCr)), and a thickness of 50nm to 200nm of gold (Au); or a stacked metal of Ti and Au, each of which has a thickness substantially the same as those described above. The second metal layer 22 can be made of gold (Au). The third metal layer 24 contains at least Ni and is generally also made of nickel-chromium alloy (NiCr). Compared with the third metal layer 24, the surfaces of the first metal layer 20 and the second metal layer 22 have wettability to the solder 32. The thickness of the second metal layer 22 is 5μm to 10μm, and the thickness of the third metal layer 24 is 20nm to 200nm.
[0019] like Figure 1B As shown, the semiconductor device 100 is mounted on the assembly substrate 30 using solder 32, which may be a resin containing fine powder of eutectic solder such as gold tin (AuSn), silver (Ag), etc. The solder 32 contacts the first metal layer 20 and the second metal layer 22, but is repelled by the third metal layer 24 to leave a vacancy in the substrate through hole 10a.
[0020] Second embodiment
[0021] Figures 2A to 4F 1 is a cross-sectional view of the semiconductor device 100 at various steps of the method for forming the device 100. Figure 2A As shown, the method first forms a gate pad 12, a source pad 14 and a drain pad 16 in the main surface 10c of the substrate 10, wherein Figure 2A The gate pad 12 and the drain pad 16 are omitted. In addition, the method forms the gate finger 13, the source finger 15, and the drain finger 17 in the main surface 10c of the substrate 10. Thereafter, the substrate 10 is attached to the support substrate 40 by, for example, wax 42 so that its main surface 10c faces and is attached to the support substrate 40. Then, as Figure 2B As shown, the method grinds the subsurface 10d of the substrate 10 to a thickness of about 100 μm. Then, a physical deposition technique (usually sputtering) can form a stacked metal layer 44 of NiCr and gold on the subsurface 10d of the substrate 10 and the surface of the supporting substrate 40 (including the surface of the wax 42 and the edge of the substrate 10 and the edge of the wax 42).
[0022] Afterwards, if Figure 2D As shown, a patterned photoresist 46 is formed on the metal layer 44, wherein the patterned photoresist 46 provides an island in a portion overlapping with the source pad 14. That is, the patterned photoresist 46 covers a portion of the metal layer 44 corresponding to the source pad 14. Figure 2EAs shown, the metal layer 44 is used as a seed layer for selective electroplating of gold (Au), and then as shown in FIG. Figure 2F As shown, the patterned photoresist 46 is removed, leaving a metal mask 48 made of Au on the metal layer 44. The metal layer 44 exposed in the opening of the metal mask 48 is removed, and the metal mask 48 can be left on the substrate 10 in a manner that the subsurface 10d of the substrate 10 is exposed in the portion corresponding to the source pad 14.
[0023] Next, if Figure 3A As shown, etching using a metal mask 48 removes portions of the metal layer 44 and the substrate 10 that overlap with the source pad 14, forming a substrate through hole 10a, the width of which can be determined by an aspect ratio of 0.5 to 10 to the thickness of the substrate 10 after grinding. In this embodiment, grinding can thin the substrate 10 to a thickness of about 100 μm (precisely, 100±10 μm), which means that the width of the substrate through hole 10a is about 50 μm to 10 μm. After forming the substrate through hole 10a, as shown in FIG. Figure 3B As shown, the method removes the metal mask 48 and the metal layer 44. Thereafter, as shown in Figure 3C As shown, the second sputtering continuously forms another metal layer 20 (which is referred to as the first metal layer) on the entire sub-surface 10d of the substrate 10, the entire surface of the supporting substrate 40, the inner wall of the substrate through hole 10a, and the surface of the source pad 14, wherein the first metal layer 20 can be a stacked metal of NiCr and Au, and the thickness of each of NiCr and Au is about 50nm to 200nm.
[0024] Afterwards, if Figure 3D As shown, another patterned photoresist 51 partially covers the surface of the metal layer 20. Specifically, the patterned photoresist 51 can cover the periphery of the substrate 10 and the area 10b corresponding to the scribe line. Figure 3E As shown, the selective electroplating performed after forming the patterned photoresist 51 forms a thickened Au layer 22 only in the area on the metal layer 20 exposed from the photoresist 51. The Au layer 22 will be referred to as the second metal layer 22. Figure 3F As shown, removing the photoresist 51 can selectively leave the plated Au layer 22 so as to partially expose the metal layer 20 .
[0025] Afterwards, if Figure 4A As shown, another NiCr layer 24 with a thickness of about 40 nm is stacked on the first metal layer 20 and the second metal layer 22 by sputtering for the third time. The NiCr layer 24, which will be referred to as the third metal layer, covers the surface of the support substrate 40, the surface of the substrate 10 (including the inner wall of the substrate through hole 10a), and the surface of the source pad 14. In addition, the third metal layer 24 covers the first metal layer 20 in the area 10b corresponding to the scribe line. Thereafter, as Figure 4BAs shown, another patterned photoresist 52 covers the substrate through hole 10a and the third metal layer 24 around the substrate through hole 10a. The solution containing iodine (I) can selectively remove the third metal layer 24 on the second metal layer 22 exposed from the patterned photoresist 52. The first metal layer 20 does not have to be left in the area 10b because the area 10b is prepared for scribing. However, the present embodiment provides an Au layer on top of the first metal layer 20; therefore, the NiCr layer under the Au layer in the first metal layer 20 is not etched by the above solution and is retained. The first metal layer 20 remaining in the area 10b can enhance the patch strength of the substrate 10 to the solder 32. In addition, the third metal layer 24 remains inside the substrate through hole 10a and around the substrate through hole 10a, wherein the width of the third metal layer 24 remaining around the substrate through hole 10a is about 10μm.
[0026] In an alternative for applications where it is not preferred to leave an Au layer for scribing, especially in the top thereof, the Au layer in the top of the first metal layer 20 in the region 10b for scribing can be removed by wet etching after removing the third metal layer 24. The removal of the top Au layer in the first metal layer 20 also etches the second metal layer 22. However, the thickness of the second metal layer 22 is much greater than the thickness of the previous Au layer on top of the first metal layer 20. Therefore, the removal of the Au layer can expose the NiCr layer of the first metal layer 20 in the region 10b for scribing. In yet another alternative where no metal is left in the region 10b, a second etching using a solution containing iodine (I) after removing the top Au layer in the region 10b can remove the NiCr layer in the first metal layer 20 and expose the substrate 10 in the region 10b.
[0027] This embodiment focuses on an arrangement in which the metal layers 20 and 24 include a NiCr layer; however, the present invention is applicable to the following metals and solutions of these metals; namely, a hydrochloric acid (HCl) solution instead of a solution containing iodine (I) can dissolve NiCr, and the Au layers 24 and 20 are stable to HCl. When the first metal layer 20 is provided with a stacked metal of NiCr and copper (Cu), wherein Cu is provided on top of the first metal layer 20, and the third metal layer 24 is NiCr; ferric chloride (FeCl 3 ) can dissolve NiCr and Cu simultaneously; however, Au layers 24 and 20 are not very effective for FeCl 3 Still stable. Moreover, the third metal layer 24 may include titanium (Ti). When the first metal layer 20 has a stacked metal of NiCr / Cu and the third metal layer 24 is Ti, or the former layer has a stacked metal of NiCr / Au and the third metal layer 24 is Ti; by using argon ions (Ar +) or dry etching using a reactive gas containing fluorine (F) to selectively remove Ti in the third metal layer 24. In addition to sputtering, the first metal layer 20 may be formed by a sequential method of vacuum evaporation and subsequent lift-off technology.
[0028] Afterwards, if Figure 4D As shown, the method removes the patterned photoresist 52 and removes the substrate 10 from the support substrate 40 by heating the support substrate 40 to a temperature of 100° C. to 200° C. to melt the wax 42. Figure 4E As shown, the organic solvent can remove the wax 42. Figure 4F As shown, an expanding tape 54 is attached to the back surface 10d of the substrate 10, and the method can be cut from its top surface 10c to form a Figure 4F The substrate 10 is divided into corresponding semiconductor chips in each region 10b indicated by the arrows. 1 Greater than the width W of the cutting blade 2 (which is substantially equal to the width of the cut); even after cutting, the metal layer 20 can remain at the periphery of each semiconductor chip. That is, the back side 10d of the substrate 10 exposes the first metal layer 20, the second metal layer 22, and the third metal layer 24 from its periphery to the center. Figure 1B , attaching the secondary surface of the semiconductor device 100 to the melted solder 32, such as gold tin (AuSn); the solder 32 diffuses on the first metal layer 20 and the second metal layer 22, but does not diffuse in and around the substrate through hole 10a (width of about 10 μm) because the substrate through hole 10a and its periphery are covered with the third metal layer of NiCr, which shows less wettability to the solder 32. The solder 32 is solidified so that the semiconductor device 100 can be mounted on the assembly substrate 30 without the solder 32 passing through the substrate through hole 10a to leave a void in the substrate through hole 10a.
[0029] Figure 5 2 is a cross-sectional view of a conventional semiconductor device 200 mounted on an assembly substrate 30. The conventional semiconductor device 200 does not provide a third metal layer 24 and is formed by FIG. 4A to FIG. 4CThe method of the steps shown in the figure is formed. That is, the conventional semiconductor device 200 does not provide the third metal layer 24 in and around the substrate through hole 10a. The solder 32 can diffuse on the second metal layer 22 having good wettability to the solder 32 and eventually fill the substrate through hole 10a. The solder 32 invading the substrate through hole 10a repeatedly shrinks and expands according to the change of the ambient temperature, and occasionally causes cracks in the substrate through hole 10a. The third metal layer 24 having less wettability to the solder 32 in and around the substrate through hole 10a according to the present invention can effectively prevent the solder 32 from invading the substrate through hole 10a, which can effectively suppress the degradation of the patch strength of the semiconductor device 100 to the assembly substrate 30.
[0030] The first metal layer 20 preferably has an etching selectivity to the third metal layer 24 so as to ensure that the first metal layer 20 is left during the removal of the third metal layer 24 in the region 10b. For example, the first metal layer 20 has an Au layer on top thereof, and the third metal layer 24 has NiCr, and the etchant for the third metal layer 24 is HCl. This arrangement can show sufficient selectivity to etching the metal layer 24 to the metal layer 20.
[0031] refer to Figure 1B , the substrate 10 is provided with a substrate through hole 10a, and the substrate through hole 10a is covered with a first metal layer 20, a second metal layer 22, and a third metal layer 24 from the inside to the surface of the substrate 10. Compared with the first metal layer 20 and the second metal layer 22, the third metal layer 24 has less wettability to the solder 32, and can effectively prevent the solder 32 from invading the substrate through hole 10a. The invading solder 32 in the substrate through hole 10a occasionally causes cracks due to contraction and expansion according to changes in ambient temperature. The embodiment of the present invention can effectively prevent the solder 32 from invading the substrate through hole 10a.
[0032] The first metal layer 20, the second metal layer 22 and the third metal layer 24 are sequentially formed on the source pad 14, the side of the substrate through hole 10a and the back side 10d of the substrate 10 in the periphery of the substrate through hole 10a. The third metal layer 24 prevents the solder 32 from invading the substrate through hole 10a, which enhances the bonding strength of the semiconductor device 100 on the assembly substrate 30 through the solder 32.
[0033] After the semiconductor chip is cut, the first metal layer 20 remains in the periphery of the back side of the semiconductor chip. Therefore, the solder 32 can be diffused in the periphery of the semiconductor chip, which can enhance the patch strength of the semiconductor chip on the assembly substrate 30. The first metal layer 20 includes Au on its top, and the third metal layer 24 includes Ni or Ti. This arrangement of the first metal layer 20 and the third metal layer 24 can show the etching selectivity of the third metal layer 24 to the first metal layer 20.
[0034] The top of the first metal layer 20 and the second metal layer 22 preferably have the same material as each other. For example, the top of the first metal layer 20 and the second metal layer 22 may be Au, which shows good wettability to the solder 32. The top of the first metal layer 20 may be Au, and the third metal layer 24 may be NiCr. The top of the first metal layer 20 and the second metal layer 22 may be copper (Cu). The third metal layer 24 may be Ti.
[0035] The substrate 10 in the semiconductor device 100 includes a FET type semiconductor active device mainly made of a nitride semiconductor material, which is a semiconductor material containing nitrogen (N), such as gallium nitride (GaN), aluminum gallium nitride (AlGaN), indium gallium nitride (InGaN), indium nitride (InN) and / or aluminum indium gallium nitride (AlInGaN). In addition to the nitride semiconductor material, the substrate 10 may be a semiconductor material containing arsenide (As) such as gallium arsenide (GaAs). The semiconductor device in the semiconductor layer may be other than FET. The substrate 10 may be silicon carbide (SiC), silicon (Si), sapphire (Al2O3), or the like. 2 O 3 )wait.
[0036] While several embodiments and variations of the invention have been described in detail herein, it will be apparent to one of ordinary skill in the art that the disclosure and teachings of this invention will suggest numerous alternative designs to those skilled in the art.
Claims
1. A semiconductor device, comprising: A substrate having a main surface and a secondary surface opposite to the main surface, the main surface having a semiconductor active device disposed therein, the substrate having a through-substrate hole passing through from the secondary surface to the semiconductor active device in the main surface; a base metal layer deposited on the secondary surface and within the substrate through-holes; as well as an additional metal layer on the base metal layer, the additional metal layer having different wettability to solder than the base metal layer, whereby the solder contacts the base metal layer and is repelled by the additional metal layer; wherein the semiconductor device is mounted on the assembly substrate by inserting solder between the secondary surface of the substrate and the assembly substrate, wherein the base metal layer in a portion other than the substrate through hole and the periphery of the substrate through hole is brought into contact with the solder by partially removing the additional metal layer, and There are vacancies in the substrate through-hole.
2. The semiconductor device according to claim 1, The base metal layer includes a first metal layer and a second metal layer, the first metal layer includes a NiCr layer and an Au layer in sequence, and the thickness of each of the NiCr layer and the Au layer is 50nm to 200nm.
3. The semiconductor device according to claim 1, The additional metal layer is an alloy of Ni and Cr with a thickness of 20 nm to 200 nm.
4. The semiconductor device according to claim 1, The additional metal layer is left inside the through-substrate hole and at the periphery of the through-substrate hole, and the width of the additional metal layer left at the periphery of the through-substrate hole is 10 μm.
5. The semiconductor device according to claim 2, The second metal layer is an Au layer deposited with a thickness of 5 μm to 10 μm.
6. A semiconductor device comprising: Semiconductor devices and assembly substrates, The semiconductor device comprises: A substrate having a main surface and a secondary surface opposite to the main surface, the main surface having a semiconductor active device disposed therein, the substrate having a through-substrate hole passing through from the secondary surface to the semiconductor active device in the main surface; A base metal layer deposited on the subsurface and within the substrate through-holes; and an additional metal layer on the base metal layer, the additional metal layer having different wettability to solder than the base metal layer, whereby the solder contacts the base metal layer and is repelled by the additional metal layer; wherein the semiconductor device is mounted on the assembly substrate by inserting solder between the secondary surface of the substrate and the assembly substrate, wherein the base metal layer in a portion other than the substrate through hole and the periphery of the substrate through hole is brought into contact with the solder by partially removing the additional metal layer, and There are vacancies in the substrate through-hole.
Citation Information
Patent Citations
Semiconductor device and manufacturing method of the same
JP2015035495A
Imaging device and optical apparatus
JP2018025680A
Semiconductor device and method of manufacturing same
JP2003045965A
Semiconductor device and its manufacturing method
JP2009033097A
Semiconductor device and its method of manufacturing
JP2010003796A