MEMS structure and forming method thereof, integrated chip

By using a composite spring structure of monocrystalline silicon and polycrystalline silicon in a MEMS device, and using polycrystalline silicon layers with different crystal orientations to stop crack propagation, the fracture problem of composite springs under bending stress in the existing technology is solved, and the durability and durability of the device are improved. reliability.

CN113044800BActive Publication Date: 2024-10-15TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 17 Cites 0 Cited by

Patent Information

Application Number
CN202011265692.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-03-23
Filing Date
2020-11-13
Publication Date
2024-10-15
Estimated Expiration
2040-11-13

AI Technical Summary

Technical Problem

The composite springs of existing MEMS devices are prone to fracture under bending stress, leading to device failure. In addition, the difference in crystal orientation between the spring layers of single-crystalline silicon and polycrystalline silicon causes cracks to propagate during bending, affecting the durability and reliability of the device.

Method used

Adopting a composite spring structure, which includes a first spring layer made of monocrystalline silicon and a second spring layer made of polycrystalline silicon, both with different crystal orientations, to increase the bending stress that the spring can withstand before breaking, and Crack propagation is stopped by the second spring layer.

Benefits of technology

The mechanical strength, durability and reliability of MEMS devices are improved, and the service life of the devices is extended.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113044800B_ABST
    Figure CN113044800B_ABST
Patent Text Reader

Abstract

Various embodiments of the present invention are directed to a micro-electromechanical system (MEMS) structure including a composite spring. A first substrate is located below a second substrate. A third substrate is located above the second substrate. The first substrate, the second substrate, and the third substrate at least partially define a cavity. The second substrate includes a movable block located in the cavity and between the first substrate and the third substrate. The composite spring extends from a peripheral area of ​​the second substrate to the movable block. The composite spring is configured to suspend the movable block in the cavity. The composite spring includes a first spring layer and a second spring layer, the first spring layer includes a first crystal orientation, and the second spring layer includes a second crystal orientation different from the first crystal orientation. Embodiments of the present invention also relate to a method for forming a MEMS structure and an integrated chip.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present invention relate to a MEMS structure and a method for forming the same, and an integrated chip. Background Art

[0002] Micro-electro-mechanical systems (MEMS) are technologies that integrate miniaturized mechanical and electro-mechanical components on an integrated chip. MEMS devices are usually manufactured using micro-fabrication techniques. In recent years, MEMS devices have found a wide range of applications. For example, MEMS devices are found in mobile phones (e.g., accelerometers, gyroscopes, digital compasses, etc.), pressure sensors, microfluidic components (e.g., valves, pumps), optical switches (e.g., mirrors), etc. Summary of the invention

[0003] An embodiment of the present invention provides a micro-electromechanical system (MEMS) structure, comprising: a first substrate; a second substrate located on the first substrate; a third substrate located on the second substrate, wherein the first substrate, the second substrate and the third substrate at least partially define a cavity, and wherein the second substrate comprises a movable block located in the cavity and between the first substrate and the third substrate; and a composite spring extending from a peripheral area of ​​the second substrate to the movable block, wherein the composite spring is configured to suspend the movable block in the cavity, and wherein the composite spring comprises a first spring layer and a second spring layer, the first spring layer comprising a first crystal orientation, and the second spring layer comprising a second crystal orientation different from the first crystal orientation.

[0004] Another embodiment of the present invention provides an integrated chip, comprising: a micro-electromechanical system (MEMS) substrate, comprising an anchoring structure and a movable element arranged adjacent to the anchoring structure; a carrier substrate, located below the micro-electromechanical system substrate, wherein the micro-electromechanical system substrate and the carrier substrate at least partially define a cavity, and the movable element is located in the cavity; and a composite spring, extending continuously from the anchoring structure to the movable element, wherein the composite spring comprises a first spring layer and a second spring layer, the first spring layer comprises single crystal silicon, and the second spring layer comprises polycrystalline silicon.

[0005] Yet another embodiment of the present invention provides a method for forming a micro-electromechanical system (MEMS) structure, comprising: providing a micro-electromechanical system substrate comprising single crystal silicon; forming a polysilicon layer within the micro-electromechanical system substrate; bonding the micro-electromechanical system substrate to a carrier substrate; and patterning the micro-electromechanical system substrate to depict a composite spring of the micro-electromechanical system substrate and a movable mass of the micro-electromechanical system substrate, wherein the composite spring comprises a first spring layer and a second spring layer, the first spring layer comprising at least a section of the micro-electromechanical system substrate, the second spring layer comprising a polysilicon layer, wherein the composite spring extends continuously from a peripheral area of ​​the micro-electromechanical system substrate to the movable mass. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] The invention can be best understood from the following detailed description when read in conjunction with the accompanying drawings. It should be noted that, in accordance with standard practice in the industry, the various components are not drawn to scale. In fact, the dimensions of the various components may be arbitrarily increased or reduced for clarity of discussion.

[0007] Figure 1 Cross-sectional views of some embodiments of a micro-electromechanical system (MEMS) structure including a composite spring and a movable mass within a cavity are shown.

[0008] Figure 2 Shown along Figure 1 The line A-A' in Figure 1 Some examples of top views of MEMS structures.

[0009] FIG. 3A to FIG. 3K Shows Figure 2 Top views of various alternative embodiments of portions of a composite spring.

[0010] Figure 4A Cross-sectional views of some embodiments of a MEMS structure including a composite spring and a movable mass within a cavity are shown.

[0011] Figure 4B Shown along Figure 4A The line A-A' in Figure 4A Some examples of top views of MEMS structures.

[0012] FIG. 5A to FIG. 5F Shows Figure 4B Top views of various alternative embodiments of portions of a composite spring.

[0013] Fig. 6A Cross-sectional views of some embodiments of a MEMS structure are shown that includes a composite spring structure and a movable mass within a cavity.

[0014] Figure 6B Shown along Fig. 6A The line A-A' in Fig. 6A Some examples of top views of MEMS structures.

[0015] 7A to 7H Shows Figure 6B Top views of various alternative embodiments of portions of a composite spring.

[0016] Fig. 8A Cross-sectional views of some embodiments of a MEMS structure are shown that includes a composite spring structure and a movable mass within a cavity.

[0017] Figure 8B Shown along Fig. 8A The line A-A' in Fig. 8A Some examples of top views of MEMS structures.

[0018] 9A to 9F Shows Figure 8B Top views of various alternative embodiments of portions of a composite spring.

[0019] Fig. 10A Cross-sectional views of some embodiments of a MEMS structure are shown that includes a composite spring structure and a movable mass within a cavity.

[0020] Fig. 10B Shown along Fig. 10A The line A-A' in Fig. 10A Some examples of top views of MEMS structures.

[0021] FIG. 11A to FIG. 11F Shows Fig. 10B Top views of various alternative embodiments of portions of a composite spring.

[0022] Fig.12 Cross-sectional views of some embodiments of an integrated circuit (IC) having a MEMS structure including a composite spring and a movable mass within a cavity are shown, wherein the MEMS structure is located above an application specific integrated circuit (ASIC) substrate.

[0023] Figures 13 to 20 Various views of some embodiments of a first method of forming a MEMS structure including a composite spring and a movable mass within a cavity are shown.

[0024] Figures 21 to 28 Various views of some embodiments of a second method of forming a MEMS structure including a composite spring and a movable mass within a cavity are shown.

[0025] Figures 29 to 39 Various views of some embodiments of a third method of forming a MEMS structure including a composite spring and a movable mass within a cavity are shown.

[0026] Figures 40 to 49 Various views of some embodiments of a fourth method of forming a MEMS structure including a composite spring and a movable mass within a cavity are shown.

[0027] Figures 50 to 60 Various views of some embodiments of a fifth method of forming a MEMS structure including a composite spring and a movable mass within a cavity are shown.

[0028] Fig.61 A method is shown in flow chart form that illustrates some embodiments for forming a MEMS structure including a composite spring and a movable mass within a cavity. DETAILED DESCRIPTION

[0029] The present invention provides many different embodiments or examples for realizing different features of the present invention. Specific examples of components and arrangements are described below to simplify the present invention. Of course, these are only examples and are not intended to be limiting. For example, in the following description, forming a first component above or on a second component may include an embodiment in which the first component and the second component are directly contacted, and may also include an embodiment in which an additional component may be formed between the first component and the second component so that the first component and the second component may not be in direct contact. In addition, the present invention may repeat reference numbers and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself indicate the relationship between the various embodiments and / or configurations discussed.

[0030] Additionally, for ease of description, spatially relative terms such as "below," "beneath," "lower," "above," "upper," etc. may be used herein to describe the relationship of one element or component to another element or component as illustrated in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or during operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein should likewise be interpreted accordingly.

[0031] A micro-electromechanical system (MEMS) device may include a MEMS substrate. The MEMS substrate includes one or more springs and a movable mass disposed in a cavity. The MEMS substrate may be disposed between a carrier substrate and a cover substrate so that the cavity is defined between the carrier substrate and the cover substrate. The movable mass is attached to a peripheral region of the MEMS substrate by a spring so that the spring is configured to suspend the movable mass in the cavity. During operation of the MEMS device, the movable mass deflects in proportion to an external stimulus such as motion or sound waves applied to the movable mass, so that the external stimulus can be quantified by measuring the deflection. The spring is configured to provide motion to the movable mass so that they can be stretched and / or compressed from the peripheral region of the MEMS substrate. Therefore, the deflection of the movable mass can be measured by a change in capacitance between a movable sensing electrode disposed on the movable mass and a fixed sensing electrode adjacent to the movable sensing electrode.

[0032] Each spring may include a single continuous material extending from a peripheral region of the MEMS substrate to the movable mass. For example, the single continuous material may be polycrystalline silicon. In such an embodiment, when the movable mass deflects in response to an external stimulus, the spring bends. With the aid of a spring comprising polycrystalline silicon, the spring may be relatively thin (e.g., less than about 30 microns), so that the stress induced on the spring by bending is high. This may cause the spring to break, thereby causing device failure. In another example, the single continuous material may be silicon (e.g., single crystal silicon, single crystal silicon, etc.). With the aid of a spring comprising single crystal silicon, the spring may be relatively thick (e.g., greater than 30 microns), so that the spring may withstand a high degree of bending stress before breaking. However, since single crystal silicon includes a single uniform crystal orientation (e.g., a 100 crystal orientation), if a small crack is generated on the surface of the spring, the crack will propagate through the lattice of the spring. This may cause the spring to break, thereby causing device failure.

[0033] Therefore, the present invention relates to a MEMS device including a composite spring structure and a movable mass in a cavity, and a related method for forming a MEMS device. For example, a MEMS device includes a MEMS substrate disposed between a carrier substrate and a cover substrate, so that a cavity is defined between the carrier substrate and the cover substrate. The movable mass is suspended in the cavity by a composite spring structure. The composite spring structure may include one or more composite springs, each composite spring extending from a peripheral area of ​​the MEMS substrate to the movable mass. Each composite spring includes a first spring layer and a second spring layer, the first spring layer including a first material (e.g., single crystal silicon), and the second spring layer including a second material different from the first material (e.g., polycrystalline silicon). The first spring layer and the second spring layer are configured to increase the bending stress that the composite spring can withstand before breaking. For example, if a crack occurs on the surface of the first spring layer due to bending stress, the crack can propagate through the first spring layer and stop at the second spring layer. This is partly because the second spring layer, for example, can have a different crystal orientation from the first spring layer. Therefore, the composite spring structure is configured to increase the durability, reliability and performance of the MEMS device.

[0034] Figure 1 A cross-sectional view of some embodiments of a micro-electromechanical system (MEMS) structure 100 including a composite spring 108 and a movable mass 110 located within a cavity 111 is shown.

[0035] The MEMS structure 100 includes a MEMS substrate 106 disposed between a carrier substrate 102 and a cover substrate 116. In some embodiments, the carrier substrate 102 and / or the cover substrate 116 may be, for example, or include a bulk semiconductor substrate (such as a bulk silicon substrate or a silicon-on-insulator (SOI) substrate), a complementary metal oxide semiconductor (CMOS) wafer with integrated circuits (not shown), a wafer with integrated passive devices (not shown), a wafer with a CMOS image sensor (not shown), a wafer with through substrate vias (TSVs), another similar substrate with other semiconductor devices, or any combination of the foregoing. In further embodiments, the MEMS substrate 106 may be, for example, or include single crystal silicon (i.e., single crystalline silicon), intrinsic single crystal silicon, a bulk silicon substrate, an SOI substrate, another suitable semiconductor material, etc. The lower bonding structure 104 is disposed between the carrier substrate 102 and the MEMS substrate 106. The upper bonding structure 114 is disposed between the cover substrate 116 and the MEMS substrate 106. A cavity 111 is defined between the carrier substrate 102 and the cover substrate 116.

[0036] The MEMS structure 100 may be configured, for example, as a motion sensor, a pressure sensor, a microphone, an actuator, or another suitable device. In some embodiments, the MEMS substrate 106 includes a composite spring 108 and a movable mass 110 (e.g., a detection mass) disposed within a cavity 111. The composite spring 108 connects the movable mass 110 to a peripheral region of the MEMS substrate 106 (e.g., to one or more anchor structures defined by the MEMS substrate 106), and suspends the movable mass 110 within the cavity 111 and above the carrier substrate 102. During operation, the movable mass 110 deflects in proportion to an external stimulus (e.g., motion or an acoustic wave) applied to the movable mass 110, such that the external stimulus can be quantified by measuring the deflection. In some embodiments, a movable sensing electrode (not shown) supported by the movable mass 110 and a fixed sensing electrode (not shown) adjacent to the movable sensing electrode are used. 100. The deflection is measured by capacitive coupling between the movable sensing electrodes and the fixed sensing electrodes. In such an embodiment, the MEMS structure 100 can be configured as an actuator, wherein the fixed electrodes and the movable electrodes (not shown) can provide an electrostatic force to move the movable mass 110. The contact electrode 112 is disposed above the peripheral area of ​​the MEMS substrate 106 and can be configured to facilitate measuring the change in capacitance between the movable sensing electrode and the fixed sensing electrode. For example, the contact electrode 112 can be electrically coupled to the movable sensing electrode and / or the fixed sensing electrode. Therefore, the contact electrode 112 can be configured to output a signal including data related to the deflection of the movable mass 110.

[0037] In some embodiments, each of the composite springs 108 includes a composite structure 109. The composite structure 109 includes two or more layers, each layer including semiconductor materials that are different from each other. In some embodiments, the composite structure 109 includes a first spring layer 109a and a second spring layer 109b. The first spring layer 109a may include a first semiconductor material (e.g., silicon, single crystal silicon, single crystal silicon, etc.), and the second spring layer 109b may include a second semiconductor material that is different from the first semiconductor material (e.g., polycrystalline silicon). In some embodiments, the first spring layer 109a is part of the MEMS substrate 106, so that the first spring layer 109a includes the same material as the MEMS substrate 106 and the movable mass 110. In yet other embodiments, for example, the second semiconductor material may be or include polycrystalline silicon, a metal (e.g., polycrystalline metal), another suitable material, or any combination of the foregoing.

[0038] The first semiconductor material may have a first crystal orientation, and the second semiconductor material may have a second crystal orientation different from the first crystal orientation. In some embodiments, the first crystal orientation and the second crystal orientation of the first spring layer 109a and the second spring layer 109b may be described by Miller indices. For example, the first crystal orientation of the first spring layer 109a may be a single crystal orientation that extends continuously on the first spring layer 109a. The single crystal orientation of the first spring layer 109a may be described by Miller indices, which include values ​​(1, 1, 1). In other embodiments, the single crystal orientation of the first spring layer 109a may be described by Miller indices, which include different values, such as (1, 1, 0), (0, 0, 1), (1, 0, 0), (0, 1, 0) or other suitable values. In further embodiments, the first crystal orientation may be a single crystal orientation extending over the first spring layer 109a (e.g., (1, 1, 1)), and the second crystal orientation may include a plurality of different crystal orientations extending over the second spring layer 109b (e.g., (1, 1, 0), (0, 0, 1), (1, 0, 0), (0, 1, 0), and / or another suitable value). In such embodiments, the second crystal orientation may include a first region having an orientation of (1, 0, 0) and a second region having an orientation (1, 1, 0) different from the first region. When the movable mass 110 deflects in response to an external stimulus, the composite spring 108 bends. This may induce stress in the composite structure 109 of the composite spring 108. In some embodiments, the induced stress may induce cracks along the surface of the first spring layer 109a. Due to the uniformity of the crystal lattice of the first spring layer 109a, the cracks may, for example, propagate through the crystal lattice of the first spring layer 109a. However, due to the different second crystal orientation of the second spring layer 109b, the crack may not propagate through the second spring layer 109b, so that the second spring layer 109b acts as a crack stop structure. This can prevent the composite spring 108 from breaking in response to an external stimulus. Therefore, the composite spring 108 including the composite structure 109 can improve the mechanical strength of the composite spring 108. This increases the reliability and durability of the MEMS structure 100.

[0039] In other embodiments, the bending strength of a material may be defined as the stress in the material before the material breaks and / or fractures due to a bending force applied to the material. In some embodiments, the first semiconductor material (e.g., silicon, monocrystalline silicon, monocrystalline silicon, etc.) of the first spring layer 109a has a first bending strength, and the second semiconductor material (e.g., polycrystalline silicon) of the second spring layer 109b has a second bending strength that is different from the first bending strength. Because the composite structure 109 includes the first spring layer 109a and the second spring layer 109b, in some embodiments, the combined bending strength of the composite structure 109 is greater than the first bending strength and greater than the second bending strength. Therefore, the durability of the composite spring 108 is increased, thereby improving the performance of the MEMS structure 100.

[0040] Figure 2 Shown along Figure 1 The line A-A' in Figure 1 Some embodiments of the top view of the MEMS structure 100. In further embodiments, the Figure 2 The top view is taken from line A-A' Figure 1 1 is a cross-sectional view of a MEMS structure 100 .

[0041] like Figure 2 As shown in the top view of FIG. 1 , the movable mass 110 is attached to the peripheral area of ​​the MEMS substrate 106 at the anchoring structure 202 by the composite spring 108. The anchoring structure 202 can be part of the MEMS substrate 106. The contact electrode 112 is adjacent to the anchoring structure 202 and can be electrically coupled to the movable mass 110, for example. The composite spring 108 includes a composite structure 109. In some embodiments, the composite structure 109 includes a first spring layer 109a and a second spring layer 109b. The second spring layer 109b can be spaced laterally between two segments of the first spring layer 109a, for example. In addition, the first spring layer 109a and the second spring layer 109b extend laterally from the anchoring structure 202 to the movable mass 110 continuously. In other embodiments, the first spring layer 109a, the anchoring structure 202 and the movable mass 110 include the same material (e.g., single crystal silicon). In addition, the portion 108s of the composite spring 108 is spaced laterally between the movable mass 110 and the anchoring structure 202.

[0042] FIG. 3A to FIG. 3K Shows Figure 2 1. Top views of some alternative embodiments of segments 108s of a composite spring 108.

[0043] like Figure 3AAs shown in the top view of FIG. 1 , the first spring layer 109a is disposed on the opposite side of the second spring layer 109b. In some embodiments, the width w1 of the first spring layer 109a is, for example, in the range of about 0.5 to 50 microns, about 0.5 to 25 microns, about 25 to 50 microns, or another suitable value. In some embodiments, the width w2 of the second spring layer 109b is, for example, in the range of about 0.1 to 5 microns, about 0.1 to 2.5 microns, about 2.5 to 5 microns, or another suitable value.

[0044] like Figure 3B As shown in the top view of FIG. 1 , the second spring layer 109 b is configured in a grid structure including a plurality of elongated first segments extending in a first direction and a plurality of second segments extending in a second direction orthogonal to the first direction. The elongated first segments are parallel to each other, and the second segments are parallel to each other. In addition, the first spring layer 109 a is laterally disposed between the elongated first segments and the second segments of the second spring layer 109 b.

[0045] like Figure 3C As shown in the top view of FIG. 1 , the first spring layer 109a includes a first plurality of elongated segments, and the second spring layer 109b includes a second plurality of elongated segments that are laterally alternately spaced between the first plurality of elongated segments of the first spring layer 109a.

[0046] like Figure 3D As shown in the top view of , the second spring layer 109b includes a plurality of segments spaced laterally apart over the length of the first spring layer 109a. Each of the segments of the second spring layer 109b extends continuously over the width of the first spring layer 109a. In some embodiments, the segments of the second spring layer 109b are spaced laterally apart from each other by a distance d1, which can be, for example, in the range of about 0.5 to 100 microns, 0.5 to 50 microns, 50 to 100 microns, or another suitable value. In further embodiments, the second spring layer 109b includes two or more segments.

[0047] like Figure 3E 1, the second spring layer 109b includes a plurality of segments spaced laterally apart over the length of the first spring layer 109a. Each of the segments of the second spring layer 109b extends continuously over the width of the first spring layer 109a. In some embodiments, the segments of the second spring layer 109b are spaced laterally apart from each other by a distance d2, which can be, for example, in the range of about 0.1 to 33 microns, 0.1 to 16 microns, 16 to 33 microns, or another suitable value. In further embodiments, the second spring layer 109b includes four or more segments.

[0048] like Figure 3F and Figure 3G109a. As shown in the top view of , the second spring layer 109b includes a plurality of inclined segments spaced laterally apart over the length of the first spring layer 109a. The inclined segments of the second spring layer 109b extend over the width of the first spring layer 109a. In some embodiments, the angle θ is defined between a substantially straight line 301 and the sidewalls of each inclined segment of the second spring layer 109b. The substantially straight line 301 can be aligned with the sidewalls of the first spring layer 109a. In further embodiments, the angle θ is in the range of about 1 degree to 89 degrees, about 1 degree to 45 degrees, about 45 degrees to 89 degrees, or another suitable value.

[0049] like Figure 3H 1 , the second spring layer 109b includes a plurality of inclined segments spaced laterally apart over the length of the first spring layer 109a. Each inclined segment includes a first portion disposed along a first sidewall of the first spring layer 109a and a second portion disposed along a second sidewall of the first spring layer 109a. A substantially straight line 301 is disposed along the center of the width of the first spring layer 109a. The first portion and the second portion of each inclined segment of the second spring layer 109b are inclined from the substantially straight line 301 at an angle θ. In some embodiments, the angle θ is in a range of about 1 degree to 89 degrees, about 1 degree to 45 degrees, about 45 degrees to 89 degrees, or another suitable value.

[0050] like Fig. 3I and Figure 3J As shown in the top view of FIG. 1 , the second spring layer 109b includes a first plurality of inclined segments and a second plurality of inclined segments. The first plurality of inclined segments are arranged along a first sidewall of the first spring layer 109a, and the second plurality of inclined segments are arranged along a second sidewall of the first spring layer 109a opposite to the first sidewall.

[0051] like Figure 3K As shown in the top view of FIG. 1 , the second spring layer 109b includes a first plurality of inclined segments, a second plurality of inclined segments, and an elongated segment. The first plurality of inclined segments are arranged along a first side wall of the first spring layer 109a, and the second plurality of inclined segments are arranged along a second side wall of the first spring layer 109a opposite to the first side wall. The elongated segment of the second spring layer 109b is arranged at the center of the width of the first spring layer 109a and extends continuously along the length of the first spring layer 109a, so that the first plurality of inclined segments and the second plurality of inclined segments extend from the elongated segment to the opposite side wall of the first spring layer 109a.

[0052] Although FIG. 3A to FIG. 3K Each of the Figure 2 Different variations of the segments 108s of the composite spring 108, it should be understood that FIG. 3A to FIG. 3K Each of the segments 108s shown in the layout may be connected from a corresponding anchor structure 202 to Figure 2The movable mass 110 extends continuously across the entire length and / or width of each composite spring 108 .

[0053] Figure 4A and Figure 4B Shown according to Figure 1 and Figure 2 Various views of some embodiments of some alternative embodiments of the MEMS structure 100 and some embodiments of the MEMS structure 400 . Figure 4A Some embodiments of a cross-sectional view of a MEMS structure 400 are shown, and Figure 4B Some embodiments of a top view of a MEMS structure 400 are shown. Figure 4A Shown along Figure 4B The top view of some embodiments of the MEMS structure 400 is taken along line AA'. Figure 4B Shown along Figure 4A The cross-sectional view is a top view of some embodiments of the MEMS structure 400 taken along line AA′.

[0054] like Figure 4A and Figure 4B As shown, the composite structure 109 of the composite spring 108 includes a first spring layer 109a and a second spring layer 109b. Figure 4A In the cross-sectional view of FIG. 1 , the first spring layer 109a is laterally spaced apart between the elongated sections of the second spring layer 109b such that the second spring layer 109b is disposed on opposite sides of the first spring layer 109a.

[0055] FIG. 5A to FIG. 5F Shows Figure 4B 1. Top views of some alternative embodiments of segments 108s of a composite spring 108.

[0056] like Figure 5A As shown in the top view of FIG. 1 , the second spring layer 109 b is disposed on opposite side walls of the first spring layer 109 a. The second spring layer 109 b extends continuously and laterally along the opposite side walls of the first spring layer 109 a.

[0057] like Figure 5B As shown in the top view of , the second spring layer 109b is arranged along the opposite sidewalls of the first spring layer 109a. In some embodiments, the second spring layer 109b is laterally offset from the central region of the first spring layer 109a by a non-zero distance, so that the second spring layer 109b is discontinuous on the central region of the first spring layer 109a.

[0058] like Figure 5C As shown in the top view of FIG. 1 , the second spring layer 109b is disposed along opposite side walls of the first spring layer 109a such that the side walls of the central segment of the first spring layer 109a are aligned with the outer side walls of the second spring layer 109b.

[0059] Figure 5D The top view shows Figure 5A An alternative embodiment of a segment 108s of a composite spring 108 is provided, wherein a plurality of openings 502 are disposed within the first spring layer 109a. In further embodiments, the center of each opening 502 is aligned with the center of the width of the first spring layer 109a. In addition, the second spring layer 109b laterally surrounds each opening 502. In some embodiments, the width w3 of each opening 502 is, for example, in the range of about 0.5 to 100 microns, about 0.5 to 50 microns, about 50 to 100 microns, or other suitable values. Figure 5D As shown, each opening 502 has a square and / or rectangular shape, however, the openings 502 may have other shapes, such as circular and / or oval.

[0060] Figure 5E The top view shows Figure 5B An alternative embodiment of a segment 108s of a composite spring 108, wherein the opening 502 is arranged in a central region of the first spring layer 109a. In addition, the second spring layer 109b continuously surrounds the opening 502 laterally.

[0061] Fig. 5F The top view shows Figure 5C An alternative embodiment of the portion 108s of the composite spring 108, wherein the opening 502 is disposed within a central section of the first spring layer 109a. In addition, the second spring layer 109b continuously surrounds the opening 502 laterally.

[0062] Although FIG. 5A to FIG. 5F Each of the Figure 4B The different variations of the segments 108s of the composite spring 108, however, it should be understood that FIG. 5A to FIG. 5F Each of the segments 108s shown in the layout may be from a corresponding anchor structure 202 to Figure 4B The movable mass 110 extends continuously across the entire length and / or width of each composite spring 108 .

[0063] Fig. 6A and Figure 6B Shown according to Figure 1 and Figure 2 Various views of some embodiments of MEMS structure 600 of some alternative embodiments of MEMS structure 100 . Fig. 6A Some embodiments of a cross-sectional view of a MEMS structure 600 are shown, and Figure 6B Some embodiments of a top view of a MEMS structure 600 are shown. Fig. 6A Shown along Figure 6B The top view of some embodiments of the MEMS structure 600 is taken along line AA'. In addition, Figure 6BShown along Fig. 6A The cross-sectional view is a top view of some embodiments of the MEMS structure 600 taken along line AA′.

[0064] like Fig. 6A and Figure 6B As shown, the composite structure 109 includes a first spring layer 109a, a second spring layer 109b, and a third spring layer 109c. In some embodiments, the third spring layer 109c is arranged along the opposite sidewalls of the first spring layer 109a. In further embodiments, the third spring layer 109c extends laterally from the corresponding anchoring structure 202 to the movable block 110 continuously. In various embodiments, the third spring layer 109c includes a third semiconductor material different from the first semiconductor material of the first spring layer 109a and the second semiconductor material of the second spring layer 109b. In further embodiments, the third semiconductor material may be, for example, or include amorphous silicon, amorphous silicon dioxide, a metal (e.g., such as an amorphous metal material), a polymer, another suitable material, or any combination of the foregoing. Therefore, the third semiconductor material may have an amorphous structure different from the first crystal orientation of the first semiconductor material and the second crystal orientation of the second semiconductor material. For example, the amorphous structure may include a continuous random network of atoms in the third spring layer 109c. Therefore, in some embodiments, the third spring layer 109c has an amorphous structure. Because the amorphous structure is different from the first crystal orientation and the second crystal orientation, stress-induced cracks formed on the first spring layer 109a and / or the second spring layer 109b and / or propagated through the first spring layer 109a and / or the second spring layer 109b may not propagate through the third spring layer 109c. This can prevent the composite spring 108 from breaking in response to an external stimulus. Therefore, the composite structure 109 including the first spring layer 109a, the second spring layer 109b, and the third spring layer 109c can increase the mechanical strength of the composite spring 108. This increases the reliability and durability of the MEMS structure 600.

[0065] In a further embodiment, the third spring layer 109c includes a third bending strength that is different from the first bending strength of the first spring layer 109a and different from the second bending strength of the second spring layer 109b. Because the composite structure 109 includes the first spring layer 109a, the second spring layer 109b, and the third spring layer 109c, in some embodiments, the combined bending strength of the composite structure 109 is greater than the first bending strength, greater than the second bending strength, and greater than the third bending strength. Therefore, the durability of the composite spring 108 is increased, thereby enhancing the performance of the MEMS structure 100. In yet another embodiment, at least one spring layer of the composite structure 109 may be, for example, or include a metal, an organic polymer, or another material having a different crystal structure from other spring layers within the composite structure 109. In some embodiments, if at least one spring layer of the composite structure 109 includes a metal, the metal may be deposited by, for example, electroplating, chemical plating, or other suitable deposition or growth processes. This may result in an enhanced bending strength of the composite structure 109.

[0066] 7A to 7H Shows Figure 6B 1. Top views of some alternative embodiments of segments 108s of a composite spring 108.

[0067] 7A to 7H The top view shows FIG. 3A to FIG. 3E , Figure 3H , Fig. 3I and Figure 3K 108 s of the composite spring 108 of the top view of the embodiment of the present invention, wherein the third spring layer 109 c is disposed along the opposite outer sidewalls of the first spring layer 109 a. In some embodiments, the width w4 of the third spring layer 109 c is, for example, in the range of about 0.1 to 2 microns, 0.1 to 1 micron, about 1 to 2 microns, or another suitable value.

[0068] Although 7A to 7H Each of the Figure 6B Different variations of the segments 108s of the composite spring 108 will be appreciated. 7A to 7H Each of the illustrated arrangements of segments 108s may be configured to extend from a corresponding anchor structure 202 to Figure 6B The movable mass 110 extends continuously across the entire length and / or width of each composite spring 108 .

[0069] Fig. 8A and Figure 8B Shown according to Figure 4A and Figure 4B Various views of some embodiments of MEMS structure 800 of some alternative embodiments of MEMS structure 400 . Fig. 8A Some embodiments of a cross-sectional view of a MEMS structure 800 are shown, and Figure 8B Some embodiments of a top view of a MEMS structure 800 are shown. Fig. 8A Shown along Figure 8B The top view of some embodiments of the MEMS structure 800 is taken along line AA'. In addition, Figure 8B Shown along Fig. 8A The cross-sectional view is a top view of some embodiments of the MEMS structure 800 taken along line AA′.

[0070] like Fig. 8A and Figure 8B As shown, the composite structure 109 of the composite spring 108 includes a first spring layer 109a, a second spring layer 109b and a third spring layer 109c, wherein the third spring layer 109c is disposed along an opposite outer side wall of the second spring layer 109b.

[0071] 9A to 9F Shows Figure 8B Top views of some alternative embodiments of the segments 108s of the composite spring 108. For example, 9A to 9F The top view shows FIG. 5A to FIG. 5F Various optional embodiments of the segment 108s of the composite spring 108 are shown in top view, wherein the third spring layer 109c is disposed along the opposite outer side wall of the second spring layer 109b and / or along the opposite outer side wall of the first spring layer 109a. In some embodiments, Fig. 9A The top view shows Figure 5A An alternative embodiment of the segment 108s of the composite spring 108. In a further embodiment, FIG. 9B to FIG. 9D The top view shows Figure 5B Various optional embodiments of the segments 108s of the composite spring 108. In further embodiments, Fig.9E The top view shows Figure 5C An alternative embodiment of the segment 108s of the composite spring 108. In various embodiments, Fig.9F The top view shows Figure 5D An alternative embodiment of the segment 108s of the composite spring 108 is shown, wherein the third spring layer 109c laterally surrounds each opening 502, and the third spring layer 109c is disposed along opposing outer sidewalls of the second spring layer 109b.

[0072] Although 9A to 9F Each of the Figure 8B Different variations of the segments 108s of the composite spring 108 will be appreciated. 9A to 9F Each of the illustrated arrangements of segments 108s may be configured to extend from a corresponding anchor structure 202 to Figure 8B The movable mass 110 extends continuously across the entire length and / or width of each composite spring 108 .

[0073] Fig. 10A and Fig. 10B Shown according to Fig. 8A and Figure 8B Various views of some embodiments of some alternative embodiments of MEMS structure 800 and some embodiments of MEMS structure 1000 . Fig. 10A Some embodiments of cross-sectional views of MEMS structures 1000 are shown, and Fig. 10B Some embodiments of a top view of a MEMS structure 1000 are shown. Fig. 10A Shown along Fig. 10B A cross-sectional view of some embodiments of the MEMS structure 1000 taken along line AA'. In addition, Fig. 10B Shown along Fig. 10A A top view of some embodiments of the MEMS structure 1000 taken along line AA′.

[0074] like Fig. 10A and Fig. 10B As shown, the composite structure 109 of the composite spring 108 includes a first spring layer 109a, a second spring layer 109b, and a third spring layer 109c. In some embodiments, the middle segment of the third spring layer 109c is transversely disposed between a first pair of segments of the first spring layer 109a, the first pair of segments of the first spring layer 109a is disposed between a pair of segments of the second spring layer 109b, the pair of segments of the second spring layer 109b is disposed between a second pair of segments of the first spring layer 109a, and the second pair of segments of the first spring layer 109a is disposed between an outer pair of segments of the third spring layer 109c.

[0075] FIG. 11A to FIG. 11F Shows Fig. 10B 1. Top views of some alternative embodiments of segments 108s of a composite spring 108.

[0076] like Fig.11A As shown in the top view of FIG. 1 , the first spring layer 109 a , the second spring layer 109 b and the third spring layer 109 c respectively include a plurality of segments alternately adjacent to each other.

[0077] like Fig. 11B As shown in the top view of FIG. 1 , the third spring layer 109c is omitted. In addition, the first spring layer 109a and the second spring layer 109b respectively include a plurality of segments alternately stacked adjacent to each other.

[0078] like Fig. 11CAs shown in the top view of , each of the second spring layer 109b and the third spring layer 109c includes a plurality of inclined segments arranged in the first spring layer 109a. Therefore, the first spring layer 109a laterally surrounds the inclined segments of the second spring layer 109b, and laterally surrounds the inclined segments of the third spring layer 109c. The plurality of inclined segments of the third spring layer 109c are aligned with the center of the width of the first spring layer 109a, and a pair of inclined segments of the second spring layer 109b are arranged on the opposite sides of each inclined segment of the third spring layer 109c. In addition, the third spring layer 109c includes an outer segment arranged along the opposite sidewalls of the first spring layer 109a.

[0079] Fig.11D Shows the corresponding Fig. 11C A top view of an alternative embodiment of a top view of a top view, wherein the plurality of inclined segments of the second spring layer 109b are aligned with the center of the width of the first spring layer 109a, and a pair of inclined segments of the third spring layer 109c are disposed on opposite sides of each inclined segment of the second spring layer 109b.

[0080] Fig.11E Shows the corresponding Fig.11A 109 a , the second spring layer 109 b , and the third spring layer 109 c respectively include a plurality of segments alternately adjacent to each other.

[0081] like Fig.11F As shown in the top view of , the third spring layer 109c extends continuously laterally along the opposite side walls of the first spring layer 109a, and includes a plurality of inclined protrusions extending from the opposite side walls of the first spring layer 109a. In addition, the second spring layer 109b includes a plurality of inclined sections arranged between adjacent pairs of inclined protrusions of the third spring layer 109c.

[0082] Although FIG. 11A to FIG. 11F Each of the Fig. 10B The different variations of the segments 108s of the composite spring 108, however, it should be understood that FIG. 11A to FIG. 11F Each of the illustrated arrangements of segments 108s may be configured to extend from a corresponding anchor structure 202 to a Fig. 10B The movable mass 110 extends continuously across the entire length and / or width of each composite spring 108 .

[0083] Fig.12 A cross-sectional view of some embodiments of an integrated circuit (IC) 1200 having a MEMS substrate 106 disposed between a carrier substrate 102 and an application specific integrated circuit (ASIC) structure 1202 is illustrated.

[0084] In some embodiments, the ASIC structure 1202 includes an interconnect structure 1208 located on an ASIC substrate 1204. In some embodiments, the ASIC substrate 1204 may be, for example, or include a bulk silicon substrate, an SOI substrate, or other suitable substrate material. In further embodiments, a plurality of semiconductor devices 1206 are disposed within and / or above the ASIC substrate 1204. The semiconductor devices 1206 may be configured as transistors. Thus, in some embodiments, each of the semiconductor devices 1206 includes a gate structure 1214 located on the ASIC substrate 1204 and a source / drain region 1212 disposed within the ASIC substrate 1204 and disposed on opposite sides of the gate structure 1214. In further embodiments, the gate structure 1214 includes a gate electrode located on a gate dielectric layer.

[0085] The interconnect structure 1208 includes an interconnect dielectric structure 1210, a plurality of conductive lines 1218, and a plurality of conductive vias 1216. The conductive vias 1216 and the conductive lines 1218 are disposed within the interconnect dielectric structure 1210 and are configured to electrically couple the semiconductor device 1206 to other devices (not shown) disposed within the IC 1200. For example, the conductive vias 1216 and the conductive lines 1218 may electrically couple the contact electrodes 112 to the semiconductor device 1206 so that a capacitance change due to a deflection of the movable mass 110 may be accessed at the semiconductor device 1206. In some embodiments, the conductive vias 1216 and / or the conductive lines 1218 may be, for example, respectively, or include copper, aluminum, titanium nitride, tantalum nitride, or any combination of the foregoing. In further embodiments, the interconnect dielectric structure 1210 may be, for example, or include silicon dioxide, a low-k dielectric material, an extremely low-k dielectric material, another suitable dielectric material, or any combination of the foregoing.

[0086] In some embodiments, Fig.12 Shows Figure 1 An alternative embodiment in which the cover substrate 116 is replaced by an ASIC structure 1202. It should be understood that the ASIC structure 1202 may replace Figure 4A , Fig. 6A , Fig. 8A and / or Fig. 10A The MEMS structure is covered by substrate 116 .

[0087] Figures 13 to 20 Various views of some embodiments of a first method of forming a MEMS structure according to the present invention, the MEMS structure including a composite spring and a movable mass within a cavity. Figures 13 to 20 The various views shown should be understood that Figures 13 to 20 The structure shown is not limited to the first method, but can be independently independent of this method. Figures 13 to 20Described as a series of actions, it should be understood that these actions are not limited thereto, the order of the actions can be changed in other embodiments, and the disclosed method is also applicable to other structures. In other embodiments, some actions shown and / or described can be omitted in whole or in part.

[0088] like Fig.13 As shown in the cross-sectional view of , a MEMS substrate 106 is provided, and then the MEMS substrate 106 is patterned to define a plurality of openings 1302 in the MEMS substrate 106. In some embodiments, the MEMS substrate 106 may be, for example, or include single crystal silicon (i.e., single crystal silicon), intrinsic single crystal silicon, a bulk silicon substrate, an SOI substrate, another suitable semiconductor material, etc. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106; performing an etching process according to the mask layer to define the openings 1302; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a deep reactive ion etching (DRIE) process.

[0089] like Fig.14 As shown in the cross-sectional view of FIG. 1 , a polysilicon layer 1402 is formed over the MEMS substrate 106 to fill the opening ( Fig.13 1302). In some embodiments, the polysilicon layer 1402 may be, for example, or include polysilicon, intrinsic polysilicon, doped polysilicon, another material, etc. In further embodiments, the polysilicon layer 1402 includes a different material than the MEMS substrate 106. In yet other embodiments, the polysilicon layer 1402 may be deposited by, for example, a chemical vapor deposition (CVD) process, a physical vapor deposition (PVD) process, an atomic layer deposition (ALD) process, or other suitable growth or deposition process.

[0090] like Fig.15 As shown in the cross-sectional view of the polysilicon layer ( Fig.14 A planarization process (eg, a chemical mechanical planarization process (CMP)) is performed until the front side 106 f of the MEMS substrate 106 is reached, thereby forming a second spring layer 109 b in the MEMS substrate 106 .

[0091] like Fig.16As shown in the cross-sectional view of , a carrier substrate 102 and a lower bonding structure 104 are provided. Subsequently, the front side 106f of the MEMS substrate 106 is bonded to the lower bonding structure 104. In some embodiments, the bonding process may be, for example, a fusion bonding process, a hybrid bonding process, or another suitable bonding process. In some embodiments, the carrier substrate 102 may be, for example, or include a bulk substrate (e.g., a bulk silicon substrate), a single crystal silicon substrate, a silicon on insulator (SOI) substrate, or some other suitable substrate. In further embodiments, the lower bonding structure 104 may be, for example, or include an oxide (such as silicon dioxide) or another suitable material.

[0092] like Fig.17 As shown in the cross-sectional view of FIG. 1 , a thinning process is performed on the MEMS substrate 106 to reduce the initial thickness Ti of the MEMS substrate 106 to a thickness Ts. In some embodiments, the thinning process is performed by a mechanical grinding process, a CMP process, some other thinning process, or any combination of the foregoing. For example, the thinning process can be performed entirely by a mechanical grinding process.

[0093] like Fig.18 As shown in the cross-sectional view of FIG, a contact electrode 112 is formed over the MEMS substrate 106. In some embodiments, the process for forming the contact electrode 112 may include: depositing (e.g., by CVD, PVD, sputtering, electroplating, chemical plating, etc.) a conductive layer over the MEMS substrate 106; forming a mask layer (not shown) over the conductive layer; patterning the conductive layer according to the mask layer to define the contact electrode 112; and performing a removal process to remove the mask layer. In some embodiments, the contact electrode 112 may be, for example, or include aluminum, copper, titanium, another suitable conductive material, or any combination of the foregoing.

[0094] like Fig.19A The cross-sectional view and Fig.19B As shown in the top view of FIG. 1 , the MEMS substrate 106 is patterned to define the movable mass 110, the composite spring 108, and the first spring layer 109a of the composite structure 109. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106 and the contact electrode 112; performing an etching process according to the mask layer to define the movable mass 110, the composite spring 108, and the first spring layer 109a; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0095] Fig.19B Shown along with Fig.19A The line A-A' intercepts Fig.19A Some embodiments of the cross-sectional views correspond to top views. Fig.19BThe layout of the composite spring 108 extending from the corresponding anchor structure 202 to the movable mass 110 is shown. In a further embodiment, Fig.19A The patterning process of the cross-sectional view of the anchor structure 202 can further define the anchor structure 202. In further embodiments, each of the first spring layer 109a and the second spring layer 109b can be formed and / or defined such that the top view layout of the composite structure 109 corresponds to FIG. 3A to FIG. 3K Any top view.

[0096] like Fig. 20 As shown in the cross-sectional view of , a covering substrate 116 and an upper bonding structure 114 are provided. Subsequently, the covering substrate 116 is bonded to the MEMS substrate 106 through the upper bonding structure 114. In some embodiments, the bonding process may be, for example, a fusion bonding process, a hybrid bonding process, or another suitable bonding process. In a further embodiment, the covering substrate 116 may, for example, be or include a bulk semiconductor substrate (such as a bulk silicon substrate), a silicon-on-insulator (SOI) substrate, or another suitable substrate material. In a further embodiment, the upper bonding structure 114 may, for example, be or include an oxide (such as silicon dioxide) or another suitable dielectric material. In some embodiments, after forming the covering substrate 116, the contact electrode 112 may be electrically connected to another integrated chip (not shown) through one or more bonding structures (not shown), and one or more TSVs (not shown) extending through the covering substrate 116 to contact the contact electrode 112 or another suitable method and / or structure may be used to couple the contact electrode 112 to another integrated chip (not shown).

[0097] Figures 21 to 28 Various views of some embodiments of a second method of forming a MEMS structure according to the present invention, the MEMS structure including a composite spring and a movable mass within a cavity. Figures 21 to 28 The various views shown should be understood that Figures 21 to 28 The structure shown is not limited to the second method, but can be independently independent of this method. Figures 21 to 28 Described as a series of actions, it will be understood that these actions are not limited thereto, the order of actions can be changed in other embodiments, and the disclosed method is also applicable to other structures. In other embodiments, some actions shown and / or described may be omitted in whole or in part.

[0098] like Fig.21As shown in the cross-sectional view of , a MEMS substrate 106 is provided, and then the MEMS substrate 106 is patterned to define a plurality of openings 2102 in the MEMS substrate 106. In some embodiments, the MEMS substrate 106 may be, for example, or include single crystal silicon (i.e., single crystal silicon), intrinsic single crystal silicon, a bulk silicon substrate, an SOI substrate, another suitable semiconductor material, etc. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106; performing an etching process according to the mask layer to define the openings 2102; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0099] like Fig. 22 As shown in the cross-sectional view of FIG. 1 , a polysilicon layer 2202 is formed over the MEMS substrate 106 to fill the opening ( Fig.21 In some embodiments, the polysilicon layer 2202 may be, for example, or include polysilicon, intrinsic polysilicon, doped polysilicon, another suitable material, etc. In further embodiments, the polysilicon layer 2202 includes a material different from the MEMS substrate 106. In still other embodiments, the polysilicon layer 2202 may be deposited by, for example, a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process.

[0100] like Fig.23 As shown in the cross-sectional view of the polysilicon layer ( Fig. 22 A planarization process (eg, a CMP process) is performed on the MEMS substrate 106 until the front side 106 f of the MEMS substrate 106 is reached, thereby forming a second spring layer 109 b in the MEMS substrate 106 .

[0101] like Fig.24 As shown in the cross-sectional view of FIG, a carrier substrate 102 and a lower bonding structure 104 are provided. Subsequently, the front side 106f of the MEMS substrate 106 is bonded to the lower bonding structure 104. In some embodiments, the bonding process may be, for example, a fusion bonding process, a hybrid bonding process, or another suitable bonding process. In some embodiments, the carrier substrate 102 may be, for example, or include a bulk substrate (e.g., a bulk silicon substrate), a silicon substrate, an SOI substrate, or some other suitable substrate. In further embodiments, the lower bonding structure 104 may be, for example, or include an oxide (such as silicon dioxide) or another suitable material.

[0102] like Fig.25As shown in the cross-sectional view of FIG. 1 , a thinning process is performed on the MEMS substrate 106 to reduce the initial thickness Ti of the MEMS substrate 106 to a thickness Ts. In some embodiments, the thinning process is performed by a mechanical grinding process, a CMP process, some other thinning process, or any combination of the foregoing. For example, the thinning process can be performed entirely by a mechanical grinding process.

[0103] like Fig.26 As shown in the cross-sectional view of FIG, a contact electrode 112 is formed over the MEMS substrate 106. In some embodiments, the process for forming the contact electrode 112 may include: depositing (e.g., by CVD, PVD, sputtering, electroplating, chemical plating, etc.) a conductive layer over the MEMS substrate 106; forming a mask layer (not shown) over the conductive layer; patterning the conductive layer according to the mask layer to define the contact electrode 112; and performing a removal process to remove the mask layer. In some embodiments, the contact electrode 112 may be, for example, or include aluminum, copper, titanium, another suitable conductive material, or any combination of the foregoing.

[0104] like Fig.27A The cross-sectional view and Fig.27B As shown in the top view of FIG. 1 , the MEMS substrate 106 is patterned to define the movable mass 110, the composite spring 108, and the first spring layer 109a of the composite structure 109. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106 and the contact electrode 112; and performing an etching process according to the mask layer to define the movable mass 110, the composite spring 108, and the first spring layer 109a; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0105] Fig.27B Shown along with Fig.27A The line A-A' intercepts Fig.27A Some embodiments of the cross-sectional views correspond to top views. Fig.27B The layout of the composite spring 108 extending from the corresponding anchor structure 202 to the movable mass 110 is shown. In a further embodiment, Fig.27A The patterning process of the cross-sectional view of the anchor structure 202 can further define the anchor structure 202. In further embodiments, each of the first spring layer 109a and the second spring layer 109b can be formed and / or defined such that the top view layout of the composite structure 109 corresponds to FIG. 5A to FIG. 5F Any top view.

[0106] like Fig.28As shown in the cross-sectional view of FIG, a covering substrate 116 and an upper bonding structure 114 are provided. Subsequently, the covering substrate 116 is bonded to the MEMS substrate 106 through the upper bonding structure 114. In some embodiments, the bonding process may be, for example, a fusion bonding process, a hybrid bonding process, or another suitable bonding process. In further embodiments, the covering substrate 116 may be, for example, or include a bulk semiconductor substrate (such as a bulk silicon substrate), a silicon-on-insulator (SOI) substrate, or another suitable substrate material. In further embodiments, the upper bonding structure 114 may be, for example, or include an oxide (such as silicon dioxide) or another suitable dielectric material.

[0107] Figures 29 to 39 Various views of some embodiments of a third method of forming a MEMS structure according to the present invention, the MEMS structure including a composite spring and a movable mass within a cavity. Figures 29 to 39 The various views shown will allow one to understand that Figures 29 to 39 The structure shown is not limited to the third method, but can be independently independent of this method. Figures 29 to 39 Described as a series of actions, it will be understood that these actions are limited to this, the order of actions can be changed in other embodiments, and the disclosed method is also applicable to other structures. In other embodiments, some actions shown and / or described can be omitted completely or partially.

[0108] like Fig.29 As shown in the cross-sectional view of , a MEMS substrate 106 is provided, and then the MEMS substrate 106 is patterned to define a plurality of openings 2902 in the MEMS substrate 106. In some embodiments, the MEMS substrate 106 may be, for example, or include single crystal silicon (i.e., single crystal silicon), intrinsic single crystal silicon, a bulk silicon substrate, an SOI substrate, another suitable semiconductor material, etc. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106; performing an etching process according to the mask layer to define the openings 2902; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0109] In addition, each opening 2902 can be formed to have a height h1. In some embodiments, the height h1 can be, for example, in the range of about 25 to 200 microns, in the range of about 5 to 500 microns, in the range of about 0.5 to 100 microns, in the range of about 0.5 to 50 microns, in the range of about 50 to 100 microns, or less than about 5 microns. It will be understood that other values ​​of the height h1 are also within the scope of the present invention.

[0110] like Fig.30As shown in the cross-sectional view of FIG. 1 , a dielectric layer 3002 is formed over the MEMS substrate 106 to fill the opening ( Fig.29 2902). In some embodiments, the dielectric layer 3002 may be or include, for example, amorphous silicon, amorphous silicon dioxide, etc. In further embodiments, the dielectric layer 3002 includes a material different from the MEMS substrate 106. In still other embodiments, the dielectric layer 3002 may be deposited by, for example, a CVD process, a PVD process, thermal oxidation, or other suitable growth or deposition process.

[0111] like Fig.31 As shown in the cross-sectional view of the dielectric layer ( Fig.30 A planarization process (eg, a CMP process) is performed until the front side 106 f of the MEMS substrate 106 is reached, thereby forming a third spring layer 109 c in the MEMS substrate 106 .

[0112] like Fig.32 As shown in the cross-sectional view of , the MEMS substrate 106 is patterned to define a plurality of openings 3202 within the MEMS substrate 106. In some embodiments, each opening 3202 is laterally spaced apart between adjacent segments of the third spring layer 109c. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106; performing an etching process based on the mask layer to define the openings 3202; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0113] In addition, each opening 3202 can be formed to have a height h2. In some embodiments, the height h2 can be, for example, in the range of about 25 to 200 microns, in the range of about 5 to 500 microns, in the range of about 0.5 to 100 microns, in the range of about 0.5 to 50 microns, in the range of about 50 to 100 microns, or less than about 5 microns. It should be understood that other values ​​of the height h2 are also within the scope of the present invention.

[0114] like Fig.33 As shown in the cross-sectional view of FIG. 1 , a polysilicon layer 3302 is formed over the MEMS substrate 106 to fill the opening ( Fig.32 3202). In some embodiments, the polysilicon layer 3302 may be, for example, or include polysilicon, intrinsic polysilicon, doped polysilicon, another material, etc. In further embodiments, the polysilicon layer 3302 includes a material different from the MEMS substrate 106 and / or different from the third spring layer 109c. In yet other embodiments, the polysilicon layer 3302 may be deposited by, for example, a CVD process, a PVD process, an ALD process, or another suitable growth or deposition process.

[0115] like Fig.34 As shown in the cross-sectional view of the polysilicon layer ( Fig.33 A planarization process (eg, a CMP process) is performed on the MEMS substrate 106 until the front side 106 f of the MEMS substrate 106 is reached, thereby forming a second spring layer 109 b in the MEMS substrate 106 .

[0116] like Fig.35 As shown in the cross-sectional view of FIG, a carrier substrate 102 and a lower bonding structure 104 are provided. Subsequently, the front side 106f of the MEMS substrate 106 is bonded to the lower bonding structure 104. In some embodiments, the bonding process may be, for example, a fusion bonding process, a hybrid bonding process, or another suitable bonding process. In some embodiments, the carrier substrate 102 may be, for example, or include a bulk substrate (e.g., a bulk silicon substrate), a single crystal silicon substrate, an SOI substrate, or some other suitable substrate. In further embodiments, the lower bonding structure 104 may be, for example, or include an oxide (such as silicon dioxide) or another suitable material.

[0117] like Fig.36 As shown in the cross-sectional view of , a thinning process is performed on the MEMS substrate 106 to reduce the initial thickness Ti of the MEMS substrate 106 to a thickness Ts. In some embodiments, the thickness Ts may be, for example, in the range of about 25 to 200 microns, or in the range of about 5 to 500 microns. It will be understood that other values ​​of the thickness Ts are also within the scope of the present invention. In some embodiments, the thinning process is performed by a mechanical grinding process, a CMP process, some other thinning process, or any combination of the foregoing. For example, the thinning process may be performed entirely by a mechanical grinding process. Therefore, in some embodiments, the thickness of the second spring layer 109b may be, for example, in the range of about 25 to 200 microns, in the range of about 5 to 500 microns, or another suitable thickness value. In addition, in some embodiments, the thickness of the third spring layer 109c may be, for example, in the range of about 25 to 200 microns, in the range of about 5 to 500 microns, or another suitable thickness value.

[0118] like Fig.37 As shown in the cross-sectional view of FIG, a contact electrode 112 is formed over the MEMS substrate 106. In some embodiments, the process for forming the contact electrode 112 may include: depositing (e.g., by CVD, PVD, sputtering, electroplating, chemical plating, etc.) a conductive layer over the MEMS substrate 106; forming a mask layer (not shown) over the conductive layer; patterning the conductive layer according to the mask layer to define the contact electrode 112; and performing a removal process to remove the mask layer. In some embodiments, the contact electrode 112 may be, for example, or include aluminum, copper, titanium, another suitable conductive material, or any combination of the foregoing.

[0119] like Fig.38A The cross-sectional view and Fig.38B As shown in the top view of FIG. 1 , the MEMS substrate 106 is patterned to define the movable mass 110, the composite spring 108, and the first spring layer 109a of the composite structure 109. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106 and the contact electrode 112; performing an etching process according to the mask layer to define the movable mass 110, the composite spring 108, and the first spring layer 109a; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0120] Fig.38B Shown along with Fig.38A The line A-A' intercepts Fig.38A Some embodiments of the cross-sectional views correspond to top views. Fig.38B The layout of the composite spring 108 extending from the corresponding anchor structure 202 to the movable mass 110 is shown. In a further embodiment, Fig.38A The patterning process of the cross-sectional view of the anchor structure 202 can further define the anchor structure 202. In further embodiments, each of the first spring layer 109a, the second spring layer 109b, and the third spring layer 109c can be formed and / or defined such that the top view layout of the composite structure 109 corresponds to 7A to 7H Any top view.

[0121] like Fig.39 As shown in the cross-sectional view of , a covering substrate 116 and an upper bonding structure 114 are provided. Subsequently, the covering substrate 116 is bonded to the MEMS substrate 106 through the upper bonding structure 114. In some embodiments, the bonding process may be, for example, a fusion bonding process, a hybrid bonding process, or another suitable bonding process. In some embodiments, the bonding process may, for example, define a cavity 111 between the carrier substrate 102 and the covering substrate 116, so that the cavity 111 has a first gas pressure. In a further embodiment, the covering substrate 116 may, for example, be or include a bulk semiconductor substrate (such as a bulk silicon substrate) or an SOI substrate. In a further embodiment, the upper bonding structure 114 may, for example, be or include an oxide (such as silicon dioxide) or another suitable dielectric material.

[0122] Figures 40 to 49 Various views of some embodiments of a fourth method for forming a MEMS structure according to the present invention, the MEMS structure including a composite spring and a movable mass within a cavity. Figures 40 to 49 The various views shown should be understood that Figures 40 to 49 The structure shown in is not limited to the fourth method, but can be independently independent of this method. Figures 40 to 49 Described as a series of actions, it will be understood that these actions are not limited thereto, the order of actions can be changed in other embodiments, and the disclosed method is also applicable to other structures. In other embodiments, some actions shown and / or described may be omitted in whole or in part.

[0123] like Fig.40 As shown in the cross-sectional view of , a MEMS substrate 106 is provided, and the MEMS substrate 106 is patterned to define a plurality of openings 4002 in the MEMS substrate 106. In some embodiments, the MEMS substrate 106 may be, for example, or include single crystal silicon (i.e., single crystal silicon), intrinsic single crystal silicon, a bulk silicon substrate, an SOI substrate, another suitable semiconductor material, etc. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106; performing an etching process according to the mask layer to define the openings 4002; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0124] like Fig.41 As shown in the cross-sectional view of FIG. 4 , a polysilicon layer 4102 is formed over the MEMS substrate 106 to line the opening 4002. In some embodiments, the polysilicon layer 4102 may be, for example, or include polysilicon, intrinsic polysilicon, doped polysilicon, another material, etc. In further embodiments, the polysilicon layer 4102 includes a different material than the MEMS substrate 106. In yet other embodiments, the polysilicon layer 4102 may be deposited by, for example, a CVD process, a PVD process, or another suitable growth or deposition process.

[0125] like Fig.42 As shown in the cross-sectional view of FIG. 1 , a dielectric layer 4202 is formed over the MEMS substrate 106 and the polysilicon layer 4102 to fill the opening ( Fig.41 4002). In some embodiments, dielectric layer 4202 may be or include, for example, amorphous silicon, amorphous silicon dioxide, another material, etc. In further embodiments, dielectric layer 4202 includes a material different from MEMS substrate 106 and / or different from polysilicon layer 4102. In yet other embodiments, dielectric layer 4202 may be deposited by, for example, a CVD process, a PVD process, an ALD process, thermal oxidation, or other suitable growth or deposition process.

[0126] like Fig.43 As shown in the cross-sectional view of the dielectric layer ( Fig.42 4202) performs a patterning process to define the third spring layer 109c. In some embodiments, the patterned dielectric layer ( Fig.424204) includes performing a wet etching process, a dry etching process, another suitable etching process, or any combination of the foregoing.

[0127] like Fig.44 As shown in the cross-sectional view of FIG. 4 , a planarization process (eg, a CMP process) is performed on the polysilicon layer 4102 until reaching the front side 106 f of the MEMS substrate 106 , thereby removing at least a portion of the polysilicon layer 4102 .

[0128] like Fig.45 As shown in the cross-sectional view of , a carrier substrate 102 and a lower bonding structure 104 are provided. Subsequently, the front side 106f of the MEMS substrate 106 is bonded to the lower bonding structure 104. In some embodiments, the bonding process may be, for example, a fusion bonding process, a hybrid bonding process, or another suitable bonding process. In some embodiments, the carrier substrate 102 may be, for example, or include a bulk substrate (e.g., a bulk silicon substrate), a single crystal silicon substrate, an SOI substrate, or some other suitable substrate. In further embodiments, the lower bonding structure 104 may be, for example, or include an oxide (such as silicon dioxide) or another suitable material.

[0129] like Fig.46 As shown in the cross-sectional view of FIG. 1 , a thinning process is performed on the MEMS substrate 106 to reduce the initial thickness Ti of the MEMS substrate 106 to a thickness Ts. In some embodiments, the thinning process is performed by a mechanical grinding process, a CMP process, some other thinning process, or any combination of the foregoing. For example, the thinning process can be performed entirely by a mechanical grinding process. In further embodiments, the thinning process removes at least a portion of the polysilicon layer 4102.

[0130] like Fig.47 As shown in the cross-sectional view of FIG, a contact electrode 112 is formed over the MEMS substrate 106. In some embodiments, the process for forming the contact electrode 112 may include: depositing (e.g., by CVD, PVD, sputtering, electroplating, chemical plating, etc.) a conductive layer over the MEMS substrate 106; forming a mask layer (not shown) over the conductive layer; patterning the conductive layer according to the mask layer to define the contact electrode 112; and performing a removal process to remove the mask layer. In some embodiments, the contact electrode 112 may be, for example, or include aluminum, copper, titanium, another suitable conductive material, or any combination of the foregoing.

[0131] like Fig.48A The cross-sectional view and Fig.48B As shown in the top view, the patterned MEMS substrate 106 and the polysilicon layer ( Fig.474102), thereby defining the movable mass 110, the composite spring 108, and the first spring layer 109a and the second spring layer 109b of the composite structure 109. In some embodiments, the patterned MEMS substrate 106 and the polysilicon layer ( Fig.47 4102) includes: forming a mask layer (not shown) over the MEMS substrate 106 and the contact electrode 112; performing an etching process according to the mask layer to define the movable mass 110, the composite spring 108, the first spring layer 109a and the second spring layer 109b; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0132] Fig.48B Shown along with Fig.48A The line A-A' intercepts Fig.48A Some embodiments of the cross-sectional views correspond to top views. Fig.48B The layout of the composite spring 108 extending from the corresponding anchor structure 202 to the movable mass 110 is shown. In a further embodiment, Fig.48A The patterning process of the cross-sectional view of the anchor structure 202 can further define the anchor structure 202. In further embodiments, each of the first spring layer 109a, the second spring layer 109b, and the third spring layer 109c can be formed and / or defined such that the top view layout of the composite structure 109 corresponds to 9A to 9F Any top view.

[0133] like Fig.49 As shown in the cross-sectional view of , a covering substrate 116 and an upper bonding structure 114 are provided. Subsequently, the covering substrate 116 is bonded to the MEMS substrate 106 through the upper bonding structure 114. In some embodiments, the bonding process may be, for example, a fusion bonding process, a hybrid bonding process, or another suitable bonding process. In some embodiments, the bonding process may, for example, define a cavity 111 between the carrier substrate 102 and the covering substrate 116, so that the cavity 111 has a first gas pressure. In a further embodiment, the covering substrate 116 may, for example, be or include a bulk semiconductor substrate (such as a bulk silicon substrate) or an SOI substrate. In a further embodiment, the upper bonding structure 114 may, for example, be or include an oxide (such as silicon dioxide) or another suitable dielectric material.

[0134] Figures 50 to 60 Various views of some embodiments of a fifth method for forming a MEMS structure according to the present invention, the MEMS structure including a composite spring and a movable mass within a cavity. Figures 50 to 60 The various views shown will allow one to understand that Figures 50 to 60The structure shown in is not limited to the fifth method, but can be independently independent of this method. Figures 50 to 60 Described as a series of actions, it will be understood that these actions are not limited thereto, the order of actions can be changed in other embodiments, and the disclosed method is also applicable to other structures. In other embodiments, some actions shown and / or described may be omitted in whole or in part.

[0135] like Fig.50 As shown in the cross-sectional view of , a MEMS substrate 106 is provided, and then the MEMS substrate 106 is patterned to define a plurality of openings 5002 in the MEMS substrate 106. In some embodiments, the MEMS substrate 106 may be, for example, or include single crystal silicon (i.e., single crystal silicon), intrinsic single crystal silicon, a bulk silicon substrate, an SOI substrate, another suitable semiconductor material, etc. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106; performing an etching process according to the mask layer to define the openings 5002; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0136] like Fig.51 As shown in the cross-sectional view of FIG. 1 , a dielectric layer 5102 is formed over the MEMS substrate 106 to fill the opening ( Fig.50 In some embodiments, the dielectric layer 5102 may be or include, for example, amorphous silicon, amorphous silicon dioxide, etc. In further embodiments, the dielectric layer 5102 includes a material different from the MEMS substrate 106. In still other embodiments, the dielectric layer 5102 may be deposited by, for example, a CVD process, a PVD process, thermal oxidation, or other suitable growth or deposition process.

[0137] like Fig.52 As shown in the cross-sectional view of the dielectric layer ( Fig.51 A planarization process (eg, a CMP process) is performed on the MEMS substrate 102 until the front side 106f of the MEMS substrate 106 is reached, thereby forming a third spring layer 109c in the MEMS substrate 106.

[0138] like Fig.53As shown in the cross-sectional view of , the MEMS substrate 106 is patterned to define a plurality of openings 5302 within the MEMS substrate 106. In some embodiments, each opening 5302 is laterally spaced apart between adjacent segments of the third spring layer 109c. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106; performing an etching process based on the mask layer to define the openings 5302; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0139] like Fig.54 As shown in the cross-sectional view of FIG. 1 , a polysilicon layer 5402 is formed over the MEMS substrate 106 to fill the opening ( Fig.53 5302). In some embodiments, the polysilicon layer 5402 may be, for example, or include polysilicon, intrinsic polysilicon, doped polysilicon, etc. In further embodiments, the polysilicon layer 5402 includes a material different from the MEMS substrate 106 and / or different from the third spring layer 109c. In still other embodiments, the polysilicon layer 5402 may be deposited by, for example, a CVD process, a PVD process, an ALD process, or another suitable growth or deposition process.

[0140] like Fig.55 As shown in the cross-sectional view of the polysilicon layer ( Fig.54 A planarization process (eg, a CMP process) is performed on the MEMS substrate 106 until the front side 106 f of the MEMS substrate 106 is reached, thereby forming a second spring layer 109 b in the MEMS substrate 106 .

[0141] like Fig.56 As shown in the cross-sectional view of , a carrier substrate 102 and a lower bonding structure 104 are provided. Subsequently, the front side 106f of the MEMS substrate 106 is bonded to the lower bonding structure 104. In some embodiments, the bonding process may be, for example, a fusion bonding process, a hybrid bonding process, or another suitable bonding process. In some embodiments, the carrier substrate 102 may be, for example, or include a bulk substrate (e.g., a bulk silicon substrate), a single crystal silicon substrate, an SOI substrate, or some other suitable substrate. In further embodiments, the lower bonding structure 104 may be, for example, or include an oxide (such as silicon dioxide) or another suitable material.

[0142] like Fig.57 As shown in the cross-sectional view of FIG. 1 , a thinning process is performed on the MEMS substrate 106 to reduce the initial thickness Ti of the MEMS substrate 106 to a thickness Ts. In some embodiments, the thinning process is performed by a mechanical grinding process, a CMP process, some other thinning process, or any combination of the foregoing. For example, the thinning process can be performed entirely by a mechanical grinding process.

[0143] like Fig.58 As shown in the cross-sectional view of FIG, a contact electrode 112 is formed over the MEMS substrate 106. In some embodiments, the process for forming the contact electrode 112 may include: depositing (e.g., by CVD, PVD, sputtering, electroplating, chemical plating, etc.) a conductive layer over the MEMS substrate 106; forming a mask layer (not shown) over the conductive layer; patterning the conductive layer according to the mask layer to define the contact electrode 112; and performing a removal process to remove the mask layer. In some embodiments, the contact electrode 112 may be, for example, or include aluminum, copper, titanium, another suitable conductive material, or any combination of the foregoing.

[0144] like Fig.59A The cross-sectional view and Fig.59B As shown in the top view of FIG. 1 , the MEMS substrate 106 is patterned to define the movable mass 110, the composite spring 108, and the first spring layer 109a of the composite structure 109. In some embodiments, patterning the MEMS substrate 106 includes: forming a mask layer (not shown) over the MEMS substrate 106 and the contact electrode 112; performing an etching process according to the mask layer to define the movable mass 110, the composite spring 108, and the first spring layer 109a; and performing a removal process to remove the mask layer. In some embodiments, the etching process includes performing a dry etching process, such as a plasma etching process and / or a DRIE process.

[0145] Fig.59B Shown along with Fig.59A The line A-A' intercepts Fig.59A Some embodiments of the cross-sectional views correspond to top views. Fig.59B 2 shows a layout of composite springs 108 extending from respective anchoring structures 202 to movable mass 110. In other embodiments, Fig.59A The patterning process of the cross-sectional view of the anchor structure 202 can further define the anchor structure 202. In further embodiments, each of the first spring layer 109a, the second spring layer 109b, and the third spring layer 109c can be formed and / or defined such that the top view layout of the composite structure 109 corresponds to FIG. 11A to FIG. 11F Any top view.

[0146] like Fig.60As shown in the cross-sectional view of , a covering substrate 116 and an upper bonding structure 114 are provided. Subsequently, the covering substrate 116 is bonded to the MEMS substrate 106 through the upper bonding structure 114. In some embodiments, the bonding process may be, for example, a fusion bonding process, a hybrid bonding process, or another suitable bonding process. In some embodiments, the bonding process may, for example, define a cavity 111 between the carrier substrate 102 and the covering substrate 116, so that the cavity 111 has a first gas pressure. In a further embodiment, the covering substrate 116 may, for example, be or include a bulk semiconductor substrate (such as a bulk silicon substrate) or an SOI substrate. In a further embodiment, the upper bonding structure 114 may, for example, be or include an oxide (such as silicon dioxide) or another suitable dielectric material.

[0147] Fig.61 A method 6100 of forming a MEMS structure including a composite spring and a movable mass within a cavity according to the present invention is shown. Although method 6100 is shown and / or described as a series of actions or events, it should be understood that the method is not limited to the order or actions shown. Therefore, in some embodiments, the actions can be performed in an order different from the order shown, and / or the actions can be performed simultaneously. In addition, in some embodiments, the actions or events shown can be subdivided into multiple actions or events, which can be performed at separate times or simultaneously with other actions or sub-actions. In some embodiments, some of the actions or events shown can be omitted, and other actions or events not shown can be included.

[0148] A micro-electromechanical system (MEMS) substrate is provided at act 6102. The MEMS substrate includes, for example, single crystal silicon (ie, single crystalline silicon) or another suitable semiconductor material. Fig.13 , Fig.21 , Fig.29 , Fig.40 and Fig.50 Cross-sectional views corresponding to various embodiments of action 6102 are shown.

[0149] At act 6104a, the MEMS substrate is patterned to form a plurality of openings within the MEMS substrate. Fig.13 and Fig.21 Cross-sectional views corresponding to various embodiments of action 6104a are shown.

[0150] At activity 6104b, a polysilicon layer is formed over the MEMS substrate and within the opening. Fig.14 and Fig. 22 Cross-sectional views corresponding to various embodiments of action 6104b are shown.

[0151] At activity 6104c, a planarization process is performed on the polysilicon layer, thereby defining a second spring layer in the MEMS substrate. Fig.15 and Fig.23 Cross-sectional views corresponding to various embodiments of action 6104c are shown.

[0152] At act 6106a, the MEMS substrate is patterned to form a plurality of openings within the MEMS substrate. Fig.29 , Fig.40 and Fig.50 Cross-sectional views corresponding to various embodiments of action 6106a are shown.

[0153] At activity 6106b, a dielectric layer is formed over the MEMS substrate and within the opening. Fig.30 , Fig.42 and Fig.51 Cross-sectional views corresponding to various embodiments of action 6106b are shown.

[0154] At activity 6106c, a planarization process or a patterning process is performed on the dielectric layer to define a third spring layer in the MEMS substrate. Fig.31 , Fig.43 and Fig.52 Cross-sectional views corresponding to various embodiments of action 6106c are shown.

[0155] At action 6106d, a polysilicon layer is formed over and within the MEMS substrate. Fig.33 , Fig.41 and Fig.54 Cross-sectional views corresponding to various embodiments of action 6106d are shown.

[0156] At activity 6106e, a planarization process or a patterning process is performed on the polysilicon layer to define a second spring layer in the MEMS substrate, the second spring layer being laterally adjacent to the third spring layer. Fig.34 , Fig.44 and Fig.48A and Fig.55 Cross-sectional views corresponding to various embodiments of action 6106e are shown.

[0157] At act 6108, the MEMS substrate is bonded to a carrier substrate. Fig.16 , Fig.24 , Fig.35 , Fig.45 and Fig.56 Cross-sectional views corresponding to various embodiments of action 6108 are shown.

[0158] At act 6110, a thinning process is performed on the MEMS substrate. Fig.17 , Fig.25 , Fig.36 , Fig.46 and Fig.57Cross-sectional views corresponding to various embodiments of action 6110 are shown.

[0159] At action 6112, an etching process is performed on the MEMS substrate to define a movable mass, a composite spring, and a first spring layer. The first spring layer is part of the MEMS substrate. In addition, each composite spring includes a composite structure that includes a first spring layer, a second spring layer, and / or a third spring layer. FIG. 19A to FIG. 19B , FIG. 27A to FIG. 27B , FIG. 38A to FIG. 38B , FIG. 48A to FIG. 48B and FIG. 59A to FIG. 59B Various views corresponding to various embodiments of action 6112 are shown.

[0160] At act 6114, the MEMS substrate is bonded to the cover substrate, thereby defining a cavity between the carrier substrate and the cover substrate. A movable mass and a composite spring are disposed within the cavity. Fig. 20 , Fig.28 , Fig.39 , Fig.49 and Fig.60 Cross-sectional views corresponding to various embodiments of action 6114 are shown.

[0161] Therefore, in some embodiments, the present invention relates to a MEMS structure including a MEMS substrate. The MEMS substrate includes a composite spring and a movable mass disposed in a cavity. The composite spring is configured to suspend the movable mass in the cavity and includes a composite structure, the composite structure including two or more spring layers. Each of the two or more spring layers includes a semiconductor material that is different from each other.

[0162] In some embodiments, the present application provides a micro-electromechanical system (MEMS) structure, comprising: a first substrate; a second substrate located on the first substrate; a third substrate located on the second substrate, wherein the first substrate, the second substrate and the third substrate at least partially define a cavity, and wherein the second substrate comprises a movable mass located in the cavity and between the first substrate and the third substrate; and a composite spring extending from a peripheral area of ​​the second substrate to the movable mass, wherein the composite spring is configured to suspend the movable mass in the cavity, and wherein the composite spring comprises a first spring layer and a second spring layer, the first spring layer comprising a first crystal orientation, and the second spring layer comprising a second crystal orientation different from the first crystal orientation.

[0163] In the above MEMS structure, wherein the first spring layer is a segment of the second substrate, so that the second substrate and the movable mass respectively include the first crystal orientation.

[0164] In the above MEMS structure, wherein the first crystal orientation of the first spring layer is a single crystal orientation extending continuously on the first spring layer, and wherein the second crystal orientation of the second spring layer includes a plurality of different crystal orientations.

[0165] In the above MEMS structure, the first spring layer includes a first material, and the second spring layer includes a second material different from the first material.

[0166] In the above MEMS structure, the first spring layer includes a first material, and the second spring layer includes a second material different from the first material, wherein the first material includes single crystal silicon, and the second material includes polycrystalline silicon.

[0167] In the above MEMS structure, the first spring layer is arranged along opposite side walls of the second spring layer.

[0168] In the above MEMS structure, the second spring layer is arranged along opposite side walls of the first spring layer.

[0169] In the above MEMS structure, the composite spring further includes: a third spring layer including an amorphous structure having a different crystal orientation from the first crystal orientation and the second crystal orientation.

[0170] In the above-mentioned MEMS structure, wherein the composite spring further comprises: a third spring layer comprising an amorphous structure having a different crystal orientation from the first crystal orientation and the second crystal orientation, wherein the third spring layer comprises amorphous silicon dioxide, metal or polymer.

[0171] In some embodiments, the present application provides an integrated chip, comprising: a micro-electromechanical system (MEMS) substrate, comprising an anchoring structure and a movable element arranged adjacent to the anchoring structure; a carrier substrate, located below the MEMS substrate, wherein the MEMS substrate and the carrier substrate at least partially define a cavity, and the movable element is located in the cavity; and a composite spring, extending continuously from the anchoring structure to the movable element, wherein the composite spring comprises a first spring layer and a second spring layer, the first spring layer comprises single crystal silicon, and the second spring layer comprises polycrystalline silicon.

[0172] In the above integrated chip, wherein the composite spring further comprises: a third spring layer comprising amorphous material.

[0173] In the above integrated chip, wherein the composite spring further comprises: a third spring layer comprising an amorphous material, wherein the amorphous material comprises amorphous silicon dioxide.

[0174] In the above integrated chip, wherein the composite spring further comprises: a third spring layer comprising an amorphous material, wherein the first spring layer is arranged along the opposite side wall of the second spring layer, wherein the third spring layer is arranged along the opposite side wall of the first spring layer.

[0175] In the above integrated chip, wherein the first spring layer includes a first plurality of segments, and the second spring layer includes a second plurality of segments laterally alternately spaced between the first plurality of segments of the first spring layer.

[0176] In the above integrated chip, the micro-electromechanical system substrate and the movable element respectively include single crystal silicon.

[0177] In some embodiments, the present application provides a method for forming a microelectromechanical system (MEMS) structure, the method comprising: providing a MEMS substrate comprising single crystal silicon; forming a polysilicon layer within the MEMS substrate; bonding the MEMS substrate to a carrier substrate; and patterning the MEMS substrate to depict a composite spring of the MEMS substrate and a movable mass of the MEMS substrate, wherein the composite spring comprises a first spring layer and a second spring layer, the first spring layer comprising at least a segment of the MEMS substrate, the second spring layer comprising a polysilicon layer, wherein the composite spring extends continuously from a peripheral region of the MEMS substrate to the movable mass.

[0178] In the above method, forming the polysilicon layer includes: patterning the micro-electromechanical system substrate to define a plurality of openings within the micro-electromechanical system substrate; depositing the polysilicon layer above the micro-electromechanical system substrate so that the polysilicon layer fills the plurality of openings; and performing a planarization process on the polysilicon layer until reaching the front side of the micro-electromechanical system substrate.

[0179] In the above method, after the micro-electro-mechanical system substrate is bonded to the carrier substrate, a thinning process is performed on the micro-electro-mechanical system substrate until the upper surface of the polysilicon layer is reached.

[0180] In the above method, the method further includes: forming a third spring layer in the micro-electromechanical system substrate, wherein the third spring layer is a part of the composite spring and includes an amorphous material.

[0181] In the above method, patterning the MEMS substrate includes performing a deep reactive ion etching (DRIE) process.

[0182] The present invention summarizes the features of several embodiments so that those skilled in the art can better understand aspects of the present invention. Those skilled in the art should understand that they can easily use the present invention as a substrate to design or modify other processes and structures for implementing the same purpose and / or achieving the same advantages as the embodiments introduced herein. Those skilled in the art should also be aware that this equivalent configuration is not directed away from the spirit and scope of the present invention, and in the case of not directed away from the spirit and scope of the present invention, they can make multiple changes, replacements and changes herein.

Claims

1. A micro-electromechanical system structure, comprising: a first substrate; A second substrate, located on the first substrate; a third substrate positioned above the second substrate, wherein the first substrate, the second substrate, and the third substrate at least partially define a cavity, and wherein the second substrate includes a movable mass positioned in the cavity and between the first substrate and the third substrate; and a composite spring extending from a peripheral region of the second substrate to the movable mass, wherein the composite spring is configured to suspend the movable mass in the cavity, and wherein the composite spring includes a first spring layer and a second spring layer, the first spring layer including a first crystal orientation, the second spring layer including a second crystal orientation different from the first crystal orientation, the first spring layer directly contacting opposite sidewalls of the second spring layer.

2. The micro-electromechanical system structure according to claim 1, wherein: The first spring layer is a segment of the second substrate such that the second substrate and the movable mass respectively comprise the first crystal orientation.

3. The micro-electromechanical system structure according to claim 1, wherein: The first crystal orientation of the first spring layer is a single crystal orientation extending continuously on the first spring layer, and wherein the second crystal orientation of the second spring layer includes a plurality of different crystal orientations.

4. The micro-electromechanical system structure according to claim 1, wherein: The first spring layer includes a first material, and the second spring layer includes a second material different from the first material.

5. The micro-electromechanical system structure according to claim 4, wherein: The first material includes single crystal silicon, and the second material includes polycrystalline silicon.

6. The micro-electromechanical system structure according to claim 1, wherein: The first spring layer is disposed along opposite side walls of the second spring layer.

7. The micro-electromechanical system structure according to claim 1, wherein: The second spring layer is disposed along opposite side walls of the first spring layer.

8. The micro-electromechanical system structure according to claim 1, wherein: The composite spring further comprises: The third spring layer includes an amorphous structure different from the first crystal orientation and the second crystal orientation.

9. The micro-electromechanical system structure according to claim 8, wherein: The third spring layer includes amorphous silicon dioxide, metal or polymer.

10. An integrated chip, comprising: A micro-electromechanical system substrate including an anchoring structure and a movable element disposed adjacent to the anchoring structure; a carrier substrate disposed beneath the MEMS substrate, wherein the MEMS substrate and the carrier substrate at least partially define a cavity, the movable element being disposed within the cavity; and A composite spring continuously extends from the anchoring structure to the movable element, wherein the composite spring comprises a first spring layer and a second spring layer, the first spring layer comprises single crystal silicon, the second spring layer comprises polycrystalline silicon, and the top surface and the bottom surface of the first spring layer are flush with the top surface and the bottom surface of the second spring layer, respectively.

11. The integrated chip according to claim 10, wherein: The composite spring further comprises: The third spring layer includes an amorphous material.

12. The integrated chip according to claim 11, wherein: The amorphous material includes amorphous silicon dioxide.

13. The integrated chip according to claim 11, wherein: The first spring layer is disposed along opposite side walls of the second spring layer, wherein the third spring layer is disposed along opposite side walls of the first spring layer.

14. The integrated chip according to claim 10, wherein: The first spring layer includes a first plurality of segments, and the second spring layer includes a second plurality of segments spaced alternately laterally between the first plurality of segments of the first spring layer.

15. The integrated chip according to claim 10, wherein: The MEMS substrate and the movable element each include single crystal silicon.

16. A method for forming a micro-electromechanical system structure, comprising: Providing a micro-electromechanical system substrate including single crystal silicon; forming a polysilicon layer in the micro-electromechanical system substrate; bonding the MEMS substrate to a carrier substrate; as well as The MEMS substrate is patterned to delineate a composite spring of the MEMS substrate and a movable mass of the MEMS substrate, wherein the composite spring comprises a first spring layer and a second spring layer, the first spring layer comprising at least a segment of the MEMS substrate, the second spring layer comprising a polysilicon layer, wherein the composite spring extends continuously from a peripheral region of the MEMS substrate to the movable mass, and wherein a bottom surface of the first spring layer is coplanar with a bottom surface of the second spring layer.

17. The method according to claim 16, wherein: Forming the polysilicon layer comprises: patterning the MEMS substrate to define a plurality of openings in the MEMS substrate; depositing the polysilicon layer over the MEMS substrate such that the polysilicon layer fills the plurality of openings; and A planarization process is performed on the polysilicon layer until reaching the front side of the MEMS substrate.

18. The method according to claim 16, wherein: After the micro-electromechanical system substrate is bonded to the carrier substrate, a thinning process is performed on the micro-electromechanical system substrate until an upper surface of the polysilicon layer is reached.

19. The method according to claim 16, further comprising: A third spring layer is formed in the MEMS substrate, wherein the third spring layer is part of the composite spring and comprises an amorphous material.

20. The method according to claim 16, wherein: Patterning the MEMS substrate includes performing a deep reactive ion etching process.

Citation Information

Patent Citations

  • A microelectronic mechanical system (MEMS) structure equipped with substrate through holes and a forming method therefore

    CN103224216A

  • Micro-electro mechanical apparatus with interdigitated spring

    CN104016295A

  • MEMS and CMOS integration with low-temperature bonding

    CN105609433A

  • MEMS devices and methods of manufacturing the same

    CN107010592A

  • MEMS Devices and Methods of Forming the Same

    CN107032290A