Pad structure and preparation method thereof and semiconductor device

By designing the pad structure of multi-layer metal layer and dielectric layer, combined with the floating well layer, the problem that the pad structure in high-speed chips is difficult to take into account both parasitic effects and reliability, and the effect of reducing parasitic capacitance and improving packaging reliability is achieved. .

CN113130427BActive Publication Date: 2024-11-12MICROTERA SEMICON (GUANGZHOU) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201911406374.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-12-31
Publication Date
2024-11-12
Estimated Expiration
2039-12-31

AI Technical Summary

Technical Problem

The existing chip packaging pad structure is difficult to take into account both parasitic effects and reliability, especially in high-speed chips, parasitic parameters have a great impact on circuit performance, and the reliability of packaging PAD is a basic requirement for mature mass production.

Method used

A pad structure including a bottom metal layer, a middle metal layer, a top metal layer and a dielectric layer is designed, and each metal layer is connected through conductive vias, and an insulating layer and pad opening are provided on the top metal layer, and the bottom metal layer is provided. Separated conductive regions to reduce area, and a floating well layer is formed on the semiconductor substrate to reduce parasitic capacitance.

Benefits of technology

It realizes the consideration of parasitic effects and reliability in high-speed chip packaging, reduces the parasitic capacitance of the pad structure, improves the reliability and performance of the chip packaging, and is suitable for high-speed chips such as optical communication transimpedance amplifiers and limiting amplifiers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113130427B_ABST
    Figure CN113130427B_ABST
Patent Text Reader

Abstract

The present invention provides a pad structure and a preparation method thereof and a semiconductor device, wherein the pad structure includes a bottom metal layer including a plurality of separated conductive areas; a middle metal layer formed on the bottom metal layer, wherein the middle metal layer and the bottom metal layer are connected via an intermediate conductive via; a top metal layer formed on the middle metal layer, wherein the middle metal layer and the top metal layer are connected via a top conductive via; a top insulating layer disposed on the top metal layer, wherein a pad opening is provided in the top insulating layer to expose the upper surface of the top metal layer; wherein the area of ​​the top metal layer is greater than the area of ​​the middle metal layer, and the projection of the pad opening on the plane where the middle metal layer is located surrounds the middle metal layer. The pad structure of the present invention can be applied to a high-speed chip packaging PAD structure, and can take into account both parasitic effects and reliability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of analog integrated circuit packaging design, and in particular relates to a pad structure and a preparation method thereof and a semiconductor device. Background Art

[0002] Conventional chip package pads (PADs) are generally square and have two structures: one is to use only the top layer of Metal, and the other is to use all from the bottom Metal1 to the top layer of Meta. The former has less parasitics, and the latter has higher reliability.

[0003] For high-speed chips, parasitic parameters have a great impact on circuit (chip) performance, especially input / output PADs, and we hope to reduce parasitic effects as much as possible; on the other hand, the reliability of packaged PADs is a basic requirement for mature chip mass production. Taking both performance and reliability into account has always been a difficult problem in PAD design. Summary of the invention

[0004] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a pad structure and a preparation method thereof and a semiconductor device that can take both parasitic effects and reliability into consideration.

[0005] To achieve the above objectives and other related objectives, the present invention provides a pad structure, the pad structure comprising:

[0006] a bottom metal layer including a plurality of separate conductive regions;

[0007] A middle metal layer is formed on the bottom metal layer, and the middle metal layer is connected to the bottom metal layer through an intermediate conductive via;

[0008] A top metal layer is formed on the middle metal layer, and the middle metal layer is connected to the top metal layer through a top conductive via;

[0009] A top insulating layer is disposed on the top metal layer, wherein a pad opening is formed in the top insulating layer to expose the interior of the upper surface of the top metal layer;

[0010] A dielectric layer, wherein the dielectric layer is respectively disposed in the gaps between the conductive regions of the bottom metal layer, the gap between the top metal layer and the middle metal layer, and the gap between the middle metal layer and the bottom metal layer;

[0011] The area of ​​the top metal layer is respectively larger than the area of ​​the middle metal layer and the area of ​​the bottom metal layer, and the projection of the pad opening on the plane where the middle metal layer is located surrounds the middle metal layer.

[0012] In one embodiment, the bottom metal layer includes at least one sub-bottom metal layer, and each sub-bottom metal layer includes a plurality of separated sub-conductive regions; when the bottom metal layer includes two or more bottom metal layers, the sub-conductive regions at corresponding positions in two adjacent sub-bottom metal layers are connected by a first conductive through-hole.

[0013] In one embodiment, the middle metal layer includes at least one sub-middle metal layer, the sub-middle metal layer includes a plurality of separate conductive regions, and the conductive regions of the bottom metal layer correspond to the conductive regions of the middle metal layer.

[0014] In one embodiment, an area of ​​the bottom metal layer is smaller than an area of ​​the middle metal layer.

[0015] In one embodiment, a spacing between the middle conductive vias, the top conductive vias, or the sub-conductive vias is greater than or equal to twice the diameter of each conductive via.

[0016] In one embodiment, the plurality of conductive regions of the bottom metal layer are disposed along edges of the middle metal layer.

[0017] In one embodiment, the middle metal layer comprises a square metal layer, and four vertices of the square metal layer fall on the edge line of the projection of the pad opening on the plane where the middle metal layer is located.

[0018] In one embodiment, the bottom metal layer includes four conductive regions, and the four conductive regions are respectively located at four vertex corners of the middle metal layer.

[0019] In one embodiment, the middle metal layer includes at least two sub-middle metal layers, and two adjacent sub-middle metal layers are connected via a second conductive via.

[0020] In one embodiment, the top metal layer includes at least two sub-top metal layers, and two adjacent sub-top metal layers are connected via a third conductive via.

[0021] In one embodiment, a projection of the third conductive via on the plane where the middle metal layer is located is located outside the middle metal layer.

[0022] In one embodiment, the position of the middle conductive via corresponds to the position of the conductive region of the bottom metal layer.

[0023] In one embodiment, the top insulating layer includes a top passivation layer and a top dielectric layer located between the top passivation layer and the top metal layer; and the pad opening penetrates the top passivation layer and the top dielectric layer.

[0024] In one embodiment, the top metal layer includes an octagon, a quadrilateral or a circle; the pad opening includes an octagon, a square or a circle; and the middle metal layer includes an octagon, a square or a circle.

[0025] In one embodiment, the pad structure further includes a semiconductor substrate, a doped region is formed on the surface of the semiconductor substrate close to the bottom metal layer, the doped region serves as a floating well layer, and the floating well layer is isolated from the bottom metal layer by the dielectric layer.

[0026] In one embodiment, a projection of the top metal layer on a plane where the floating well layer is located is located inside the floating well layer.

[0027] In one embodiment, the floating well layer and the semiconductor substrate have different conductivity types.

[0028] In order to achieve the above-mentioned object and other related objects, the present invention also provides a method for preparing a pad structure, characterized in that the preparation method comprises:

[0029] forming a bottom metal layer including a plurality of isolated conductive regions;

[0030] forming a first dielectric layer and a middle metal layer on the bottom metal layer in sequence, wherein a middle conductive via connecting the middle metal layer and the bottom metal layer is formed in the first dielectric layer;

[0031] forming a second dielectric layer and a top metal layer on the middle metal layer in sequence, wherein a top conductive via connecting the middle metal layer and the top metal layer is formed in the second dielectric layer;

[0032] forming a top insulating layer on the top metal layer;

[0033] A pad opening is formed in the top insulating layer to expose the upper surface of the top metal layer;

[0034] The area of ​​the top metal layer is respectively larger than the area of ​​the middle metal layer and the area of ​​the bottom metal layer, and the projection of the pad opening on the plane where the middle metal layer is located surrounds the middle metal layer.

[0035] In one embodiment, the step of forming the bottom metal layer comprises:

[0036] At least one sub-bottom metal layer is formed in sequence, wherein each sub-bottom metal layer includes a plurality of separated sub-conductive regions; and when the bottom metal layer includes two or more bottom metal layers, the sub-conductive regions at corresponding positions in two adjacent sub-bottom metal layers are connected by a first conductive through-hole.

[0037] In one embodiment, the middle metal layer includes at least one sub-middle metal layer, the sub-middle metal layer includes a plurality of separate conductive regions, and the conductive regions of the bottom metal layer correspond to the conductive regions of the middle metal layer.

[0038] In one embodiment, an area of ​​the bottom metal layer is smaller than an area of ​​the middle metal layer.

[0039] In one embodiment, a spacing between the middle conductive vias, the top conductive vias, or the sub-conductive vias is greater than or equal to twice the diameter of each conductive via.

[0040] In one embodiment, the plurality of conductive regions of the bottom metal layer are disposed along edges of the middle metal layer.

[0041] In one embodiment, the middle metal layer comprises a square metal layer, and four vertices of the square metal layer fall on the edge line of the projection of the pad opening on the plane where the middle metal layer is located.

[0042] In one embodiment, the bottom metal layer includes four conductive regions, and the four conductive regions are respectively located at four vertex corners of the middle metal layer.

[0043] In one embodiment, the step of forming the middle metal layer includes:

[0044] At least two sub-middle metal layers are sequentially formed on the first dielectric layer, and two adjacent sub-middle metal layers are connected via a second conductive through hole.

[0045] In one embodiment, the step of forming the top metal layer comprises:

[0046] At least two sub-top metal layers are sequentially formed on the second dielectric layer, and two adjacent sub-top metal layers are connected via a third conductive through hole.

[0047] In one embodiment, a projection of the third conductive via on the plane where the middle metal layer is located is located outside the middle metal layer.

[0048] In one embodiment, the position of the middle conductive via corresponds to the position of the conductive region of the bottom metal layer.

[0049] In one embodiment, the step of forming a top insulating layer on the top metal layer comprises:

[0050] forming a top dielectric layer on the top metal layer;

[0051] forming a top passivation layer in the top dielectric layer;

[0052] Wherein, the pad opening penetrates the top passivation layer and the top dielectric layer.

[0053] In one embodiment, the top metal layer includes an octagon, a quadrilateral or a circle; the pad opening includes an octagon, a square or a circle; and the middle metal layer includes an octagon, a square or a circle.

[0054] In one embodiment, the bottom metal layer is formed on a semiconductor substrate, and the step of forming a bottom metal layer includes:

[0055] A doped region is formed on the surface of the semiconductor substrate close to the bottom metal layer, and the doped region serves as a floating well layer;

[0056] forming a third dielectric layer on the floating well layer,

[0057] The bottom metal layer is formed on the third dielectric layer.

[0058] In one embodiment, a projection of the top metal layer on a plane where the floating well layer is located is located inside the floating well layer.

[0059] In one embodiment, the floating well layer and the semiconductor substrate have different conductivity types.

[0060] The present invention also provides a semiconductor device using any one of the pad structures described above.

[0061] The pad structure of the present invention can be applied to the PAD structure of high-speed chip packaging, taking into account both parasitic effects and reliability, not only ensuring the reliability of the PAD during chip packaging and wiring, but also greatly reducing the parasitic effects caused by the use of a full-layer metal PAD, and can be applied to high-speed chips, such as optical communication transimpedance amplifiers, limiting amplifiers, clock recovery circuits, laser diode drivers, etc.

[0062] The pad structure of the present invention can effectively reduce the parasitic capacitance between each metal layer in the pad structure and the semiconductor substrate by arranging a floating gate layer in the semiconductor substrate below the pad structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0063] Figure 1 A top view of a pad structure of the present invention is shown (only various metal layers are shown).

[0064] Figure 2 Display as Figure 1 Schematic diagram of the cross section at AA in the middle.

[0065] Figure 3 A top view of another pad structure of the present invention is shown (only the metal layers are shown).

[0066] Figure 4 Display as Figure 3 Schematic diagram of the cross section at BB.

[0067] Figure 5 Shown is a top view of the third pad structure of the present invention (only showing the metal layers).

[0068] Figure 6 Display as Figure 5 Schematic diagram of the cross section at CC.

[0069] Figure 7 A top view of a fourth pad structure of the present invention is shown (only the metal layers and the floating well layer are shown).

[0070] Figure 8 Display as Figure 7 Schematic diagram of the cross section at DD in the middle.

[0071] Fig. 9 It is a schematic diagram showing the simulation of the frequency characteristics of the pad structure of the present invention and the existing pad structure.

[0072] Fig.10 Shown is a schematic flow chart of a method for preparing a pad structure of the present invention.

[0073] Component number description

[0074] 1 Semiconductor substrate

[0075] 2 Top dielectric layer

[0076] 3 Top passivation layer

[0077] 4 Pad opening

[0078] 5 Dielectric layer

[0079] 6 Floating Well Layer

[0080] VIA1, VIA2, ..., VIA n-1 Conductive vias

[0081] M1, M2, M n Metal layer

[0082] Steps S10~S50,S11~S14,S31,S32 DETAILED DESCRIPTION

[0083] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention. For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional view showing the device structure will not be partially enlarged according to the general proportion, and the schematic diagram is only an example, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional dimensions of length, width and depth should be included.

[0084] For the convenience of description, spatial relational terms such as "under", "below", "below", "below", "above", "on", etc. may be used here to describe the relationship between one element or feature shown in the drawings and other elements or features. It will be understood that these spatial relational terms are intended to include other directions of the device in use or operation, in addition to the directions depicted in the drawings. In addition, when a layer is referred to as being "between" two layers, it may be the only layer between the two layers, or there may be one or more layers between them. In the context of the present application, the structure described as a first feature "above" a second feature may include an embodiment in which the first and second features are formed in direct contact, and may also include an embodiment in which another feature is formed between the first and second features, so that the first and second features may not be in direct contact. It should be noted that the illustrations provided in this embodiment only illustrate the basic concept of the present invention in a schematic manner, so the illustrations only show the components related to the present invention rather than being drawn according to the number, shape and size of the components in actual implementation. The form, quantity and proportion of each component in actual implementation may be a random change, and the component layout form may also be more complicated.

[0085] Conventional chip package pads (PADs) are generally square and have two structures: one is to use only the top layer of Metal (TM-PAD), and the other is to use all the Metal from Metal1 to the top layer (M1-M6 PAD). The former structure has relatively small parasitics, and the latter structure has relatively high reliability. For high-speed chips, parasitic parameters have a greater impact on circuit (chip) performance, especially input / output PADs. It is hoped that parasitic effects can be reduced as much as possible. On the other hand, the reliability of the package PAD is a basic requirement for the mature mass production of chips. Therefore, the two existing package pad structures cannot take into account both performance and reliability. Based on this, the embodiments of the present invention provide a pad structure and a preparation method thereof that can take into account both performance and reliability. The technical solution of the present invention will be explained below in conjunction with specific embodiments.

[0086] It should be noted that in the specification and the drawings, the symbol “n " stands for the topmost level metal layer in the chip, while "M n-1 " represents a metal layer lower than the top metal layer, and so on, wherein n is greater than or equal to 3, for example, between 3-10. The symbol "VIA" represents a through hole connecting two adjacent metal layers, for example, VIA3 represents a through hole connecting M3 to M4. In the present invention, the wire bonding hereinafter is also called Wire Bonding (pressure welding, also known as binding, bonding, wire bonding), which refers to the use of metal wires (gold wires, aluminum wires, etc.) to complete the connection of the internal interconnection wiring of the solid-state circuit in the microelectronic device by using heat pressing or ultrasonic energy, that is, the connection between the chip and the circuit or lead frame.

[0087] It should be noted that the parasitic capacitance of the pad PAD is composed of the parasitic capacitance of each metal layer of the PAD to the semiconductor substrate 1 and the mutual coupling capacitance between different metal layers, wherein, since the metal layers of the pad PAD are interconnected through conductive through-holes, this is equivalent to the two substrates of the coupling capacitor being in a short-circuit relationship, and the coupling capacitor does not work correctly, and the coupling capacitor has basically no effect on the output signal of the pad PAD; and the parasitic capacitance of the metal layer to the semiconductor substrate 1 is equivalent to the metal layers of the pad PAD being the upper plate, and the semiconductor substrate 1 being the lower plate, and the semiconductor substrate is connected to the "ground" by default in the CMOS process, that is, the parasitic capacitance of the metal layer to the semiconductor substrate 1 is working normally, which will have a greater impact on the output signal of the pad PAD.

[0088] Embodiment 1

[0089] Figure 1 and Figure 2 The top view and the side view of a pad structure of the present invention are respectively shown. Figure 1 Schematic diagram of the cross section at AA in the figure. Figure 1 and Figure 2 The pad structure includes multiple metal layers (M1, M2..., M n ), a multilayer dielectric layer 5 and conductive vias (VIA1, VIA2, . . . , VIA2) respectively disposed between adjacent metal layers n-1 ), and a top insulating layer arranged on the upper surface of the top metal layer. The multi-layer metal layer includes a bottom metal layer, a middle metal layer and a top metal layer formed in sequence from bottom to top, and the top insulating layer is formed with an opening exposing the top metal layer as a pad opening 4, wherein the area of ​​the top metal layer is respectively larger than the area of ​​the middle metal layer and the area of ​​the bottom metal layer; the bottom metal layer, the middle metal layer and the top metal layer each include at least one metal layer, which can be adjusted as needed. As an example, Figure 1 and Figure 2Given that the top metal layer contains two metal layers M n-1 and M n as a demonstration Figure 3 and Figure 4 Given that the top metal layer contains a metal layer M n As an example, Figure 5 and Figure 6 The top metal layer contains three metal layers M n-2 、M n-1 and M n or more. The structures of the three examples are similar. Figure 1 and Figure 2 To illustrate the technical solution of the present invention.

[0090] See also Figure 1 and Figure 2 In this embodiment, the top metal layer includes two metal layers, the middle metal layer includes one metal layer, and the remaining metal layers are used as the structure of the bottom metal layer to illustrate the technical solution of the present invention. Specifically, the bottom metal layer (corresponding to Figure 2 The metal layer M n-3 , ..., M2, M1, as the respective sub-bottom metal layers of the bottom metal layer) can be formed on a semiconductor substrate 1, for example, the bottom metal layer includes a plurality of separated conductive areas; the middle metal layer (corresponding to Figure 2 The metal layer M n-2 , as a sub-middle metal layer of the middle metal layer) is formed on the bottom metal layer, and the middle metal layer and the bottom metal layer are connected by an intermediate conductive via (corresponding to Figure 2 Conductive vias in n-3 ) connection; the top metal layer (corresponding to Figure 2 The metal layer M n-1 and M n , respectively serving as the respective sub-top metal layers of the top metal layer) are formed on the middle metal layer, and the middle metal layer and the top metal layer are connected by top conductive vias (corresponding to Figure 2 Conductive vias in n-2 ) connection; the dielectric layer 5 is respectively filled in the gaps between the conductive areas of the bottom metal layer, the gaps between the top metal layer and the middle metal layer, and the gaps between the middle metal layer and the bottom metal layer; wherein the area of ​​the top metal layer is respectively larger than the area of ​​the middle metal layer and the area of ​​the bottom metal layer; the projection of the pad opening 4 on the plane where the middle metal layer is located surrounds the middle metal layer. The pad structure of this embodiment adopts a top metal layer (metal layer M n 、M n-1 ), and the middle metal layer (metal layer Mn-2 ) can basically meet the reliability requirements of the pad, and in order to reduce the parasitic capacitance, the bottom metal layer adopts a separated conductive area structure to reduce the area of ​​the bottom metal layer as much as possible, thereby reducing the parasitic capacitance of the pad structure to meet the performance requirements of high-speed chips. In addition, the separated conductive area structure can facilitate the setting of the conductive area of ​​the separated bottom metal layer at the edge of the middle metal layer to avoid the wire bonding position, effectively avoiding the damage of the pad structure during wire bonding. The pad structure can be applied to high-speed chips such as optical communication transimpedance amplifiers, limiting amplifiers, clock recovery circuits, and laser diode drivers.

[0091] See also Figure 2 As shown, the pad structure of the present embodiment can be arranged on a semiconductor substrate 1, and one or more active devices can be formed on the substrate 1. The active devices can be transistors, diodes and other known active devices, and the passive devices can be resistors, capacitors and inductors and other various known passive devices. The substrate is connected to the pad of the present invention to form a semiconductor device, but the substrate 1 does not have a key impact on the pad structure of the present invention, so it will not be repeated here.

[0092] See also Figure 1 and Figure 2 In order to improve the overall structural strength of the pad structure, the dielectric layer 5 is filled in the gaps between the conductive areas of the bottom metal layer, the gaps between the top metal layer and the middle metal layer, and the gaps between the middle metal layer and the bottom metal layer. The dielectric layer 5 is composed of an interlayer dielectric layer formed in the gaps inside each metal layer and between adjacent metal layers. The interlayer dielectric layer between two adjacent metal layers is formed with a corresponding conductive through hole VIA for interconnection. As an example, the dielectric layer 5 is gradually formed in the above-mentioned gaps during the preparation of the pad structure, as described in detail in the pad structure preparation method section below. As an example, the material of the dielectric layer 5 and the top dielectric layer 2 to be introduced below includes, but is not limited to, silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, low dielectric constant or ultra low dielectric constant (ultra low-k, ULK) materials (such as organic (such as aromatic hydrocarbons (SiLK)) or inorganic (such as hydrogen-containing silicate (HSQ)) materials), or any combination of the above materials. In a specific example, the material of the dielectric layer 5 can be, for example, the material of the dielectric layer 5.

[0093] See also Figure 1and Figure 2 In order to form a pad opening 4 on the top metal layer, the top insulating layer includes a top passivation layer 3 and a top dielectric layer 2 located between the top passivation layer 3 and the top metal layer, that is, the top dielectric layer 2 is first formed on the top metal layer, and then the top passivation layer 3 is formed on the top dielectric layer 2, and then the pad opening 4 is formed on the top passivation layer 3 and the top dielectric layer 2 by etching, and the pad opening 4 penetrates the top passivation layer 3 and the top dielectric layer 2 to expose the upper surface of the top metal layer, and the bottom surface of the pad opening 4 is located within the upper surface of the top metal layer. As an example, the material of the top dielectric layer 2 is described above, which will not be repeated here; the material of the top passivation layer 3 includes but is not limited to silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, polyimide, or any combination of the above materials or similar substances.

[0094] See also Figure 1 and Figure 2 Since there will be great stress during wire bonding, a larger metal layer area can reduce such stress and improve the reliability of the PAD. In order to reduce parasitic capacitance, the area of ​​the metal layer needs to be reduced as much as possible. Therefore, in this embodiment, in order to improve the reliability of the packaged PAD and take into account the parasitic effect, the top metal layer includes metal layers M, ... n and metal layer M n-1 , respectively as the sub-top metal layers of the top metal layer, and the two adjacent sub-top metal layers are connected by a third conductive via (corresponding to Figure 2 Conductive vias in n-1 )connect.

[0095] In this embodiment, a top metal layer (metal layer M) is used. n 、M n-1 ), and the middle metal layer (metal layer M n-2 ) with a larger area of ​​three metal layers, the reliability requirements of the pad can be basically met. In order to reduce the parasitic capacitance, the bottom metal layer adopts a separated conductive area structure to reduce the area of ​​the bottom metal layer as much as possible, thereby reducing the parasitic capacitance of the pad structure to meet the performance requirements of high-speed chips.

[0096] See also Figure 1 and Figure 2 The bottom metal layer includes a stacked structure consisting of a sub-bottom metal layer and a first conductive via alternately formed. Specifically, the bottom metal layer includes a plurality of sub-bottom metal layers (metal layer M n-3 to M1) and a plurality of first conductive vias (conductive vias VIA) formed between two adjacent sub-bottom metal layers. n-4As an example, the bottom metal layer includes several sub-bottom metal layers, which are marked as M1, M2, ..., M from bottom to top. n-3 The first conductive vias are VIA1, VIA2, ..., VIA from bottom to top. n-4 ; Each sub-bottom metal layer includes a number of separate sub-conductive areas, the sub-conductive areas in each sub-bottom metal layer correspond to each other one by one, and the sub-conductive areas at corresponding positions in two adjacent sub-bottom metal layers are respectively connected by a number of separate first conductive through holes, thereby forming a number of separate conductive areas. The specific formation method is detailed in the preparation method section below and will not be repeated here.

[0097] See also Figure 1 and Figure 2 In this embodiment, the intermediate conductive layer (metal layer M n-2 ) is larger than the area of ​​the above-mentioned sub-bottom metal layers (metal layer M n-3 to M1), and the intermediate metal layer is a whole; in other embodiments, the intermediate conductive layer (metal layer M n-2 ) can also be equal to the area of ​​each of the above-mentioned sub-bottom metal layers (metal layer M n-3 to M1), the middle metal layer (metal layer M n-2 ) can also be configured to include a plurality of discrete conductive regions, wherein the conductive region of the bottom metal layer corresponds to the conductive region of the middle metal layer, so as to facilitate the interconnection between the upper and lower layers. It should be noted that, although in the present invention, the middle metal layer includes a metal layer M n-2 However, it can be understood that, in other examples, the middle metal layer can also adopt multiple metal layers, which are respectively used as sub-middle metal layers of the middle metal layer, and adjacent sub-middle metal layers are connected through second conductive through holes.

[0098] As an example, the sizes of the sub-conductive areas at the corresponding positions in each sub-bottom metal layer are basically the same (of course, there may be differences), so as to use the same Mask to save production costs. In other examples, the sizes of the sub-conductive areas at the corresponding positions in each sub-bottom metal layer may also be different. As an example, each first conductive via (conductive vias VIA1, VIA2, ..., VIA n-4) have basically the same aperture, and in other examples, there may also be differences, which can be made using the same Mask. As an example, several sub-conductive areas of the sub-bottom metal layer M1 are electrically connected to several sub-conductive areas of the sub-bottom metal layer M2 through several first conductive vias VIA1 (blocks), that is, each first conductive via VIA1 (block) corresponds to a sub-conductive area of ​​the sub-bottom metal layer M1 and a sub-conductive area of ​​the sub-bottom metal layer M2, that is, the number of first conductive vias VIA1 (blocks) between the sub-bottom metal layer M1 and the sub-bottom metal layer M2 is the same as the number of sub-conductive areas in the sub-bottom metal layer M1 / the number of sub-conductive areas in the sub-bottom metal layer M2, and each first conductive via VIA1 (block) contains several conductive channels arranged at intervals; similarly, several sub-conductive areas of the sub-bottom metal layer M2 are electrically connected to several sub-conductive areas of the sub-bottom metal layer M3 through several first conductive vias VIA2 (blocks); the sub-bottom metal layer M n-4 The plurality of sub-conductive regions are connected through a plurality of first conductive vias VIA n-4 (Block) and the sub-bottom metal layer M n-3 Several sub-conductive regions are electrically connected.

[0099] In this embodiment, each metal layer M1, M2, ..., M n The material of the conductive vias VIA1, VIA2 to VIA n-1 The material may include, for example, one of conductive materials such as copper, aluminum, tungsten or copper-aluminum alloy.

[0100] See also Figure 1 and Figure 2 , each of the first conductive vias (conductive vias VIA1, VIA2, ..., or VIA n-4 ), the middle conductive via (conductive via VIA n-3 ), the top conductive via (conductive via VIA n-2 ), the third conductive via (conductive via VIA n-1 ) include multiple independent blocks, distributed at the edge of the upper and lower metal layers, so as to ensure the strength of the middle position of the dielectric layer between the upper and lower metal layers. Figure 1 and Figure 2 In the embodiment, since the conductive areas of the bottom metal layer are connected along the middle metal layer M n-2 The edge of the third conductive via (conductive via VIA n-2 ) corresponds to the position of each conductive area in the bottom metal layer, and the intermediate conductive via (conductive via VIA n-3) corresponds to the position of each conductive area in the bottom metal layer one by one, that is, each first conductive via (conductive vias VIA1, VIA2, ..., VIA n-4 ), and the intermediate conductive via (conductive via VIA n-3 ) are located on the same vertical line and are respectively located in the middle metal layer M n-2 The first top conductive through hole VIA n-1 In the middle metal layer M n-2 The projection on the plane is located at the middle metal layer M n-2 outside of the.

[0101] It should be noted that each conductive via VIA adopts Figure 1 and Figure 2 The design in is to increase the strength of the pad, improve the success rate of product package pad bonding, and reduce tape-out; this is because the conductive via VIA is conductive, generally made of metal materials, such as tungsten, which is relatively soft, and is formed in the dielectric layer 5 (such as silicon dioxide). The more conductive vias VIA are formed in the dielectric layer, the less dielectric layer 5 will be below the pad opening 4 (Pad opening), which is equivalent to reducing the strength of the dielectric layer below the pad opening 4, which is not conducive to bonding. The present application makes improvements in two aspects. On the one hand, when bonding, it will directly hit the metal layer at a deeper position below the pad opening 4, such as the middle metal layer (metal layer M n-2 ) in the bottom metal layer below, such as metal layer M2 or even M1, causing tape-out, and during wire bonding, it is generally located at the center of Padopending. Based on this, each conductive via VIA can be placed around the pad opening 4 to avoid the wire bonding position, effectively avoiding the damage of the pad structure during wire bonding; on the other hand, even if each conductive via VIA is set at an edge position, each conductive via VIA will cause the strength of the dielectric layer 5 nearby to be reduced. Therefore, between two adjacent metal layers, on the basis of ensuring electrical connection, the number of conductive channels in each conductive channel (block) should be minimized, thereby reducing the influence of the conductive channel on the strength of the nearby dielectric layer 5, avoiding PAD splitting, and improving the success rate of wire bonding.

[0102] For example, the number of conductive channels in a unit area can be reduced by increasing the spacing between the conductive vias VIA of each layer. Due to the manufacturing process, in a PAD structure composed of multiple metal layers, the spacing between the conductive vias VIA between the metal layers is generally selected to be equal to the size of VIA. In this embodiment, by changing the existing manufacturing process, the conductive vias VIA1, VIA2, ..., VIA n-1The spacing between the conductive vias is greater than or equal to twice the aperture of each conductive via, so as to reduce the PAD separation caused by the stress during package bonding and further improve the reliability of the pad structure. As an example, the spacing between the conductive vias is greater than or equal to three times the aperture of each conductive via. This is because the metal layer area of ​​the PAD is generally large, and if the conductive vias VIA are too dense, the metal layer will be more brittle and relatively easier to rot, so the conductive vias VIA between the metal layers should be sparse.

[0103] In this example, see Figure 1 and Figure 2 In order to ensure sufficient contact area for bonding during wire bonding to increase reliability, the top metal layer (metal layer M n and metal layer M n-1 ) can adopt a (regular) octagon, and in other embodiments, other shapes such as a quadrilateral, hexagon, circle, etc. can also be adopted. The octagon can increase the area of ​​the pad opening 4 while also helping to reduce the difficulty of layout design and manufacturing process. In the layout design and manufacturing process, angles such as 0°, 45°, 90°, and 135° are easier to achieve; the pad opening 4 also adopts an octagon, and in other embodiments, other shapes such as a quadrilateral, hexagon, circle, etc. can also be adopted; the middle metal layer adopts a (regular) quadrilateral, and in other embodiments, other shapes such as an octagon, hexagon, circle, etc. can also be adopted. As an example, in order to obtain the largest area, the middle metal layer can be a square, and the four vertices of the square fall on the edge of the projection of the pad opening 4 on the plane where the middle metal layer is located. The bottom metal layer includes four conductive areas (it can also include more conductive areas), and the four conductive areas are respectively located at the four vertex positions of the middle metal layer of the square. In some examples, the four conductive areas can also be set at other positions on the edge of the square. In other examples, the four conductive areas can also be set at any other position of the middle metal layer. As an example, the critical dimension CD (corresponding to Figure 2 The horizontal direction data in the figure are as follows: the CD of the pad opening 4 is between 65-75 μm, for example, 70 μm, and the first top metal layer M n and the second top metal layer M n-1 The CD of the middle metal layer M is between 70-78 μm, for example 74 μm. n-2 The CD is between 45-55μm, for example, 50μm; M n-3 -M1’s CD is between 7μm-13μm, for example 11μm, VIA1-VIA n-2 The CD is between 0.22 and 0.30 μm, for example, 0.26 μm, VIA n-1The CD is between 0.32 and 0.40 μm, for example, 0.36 μm. Fig. 9 The frequency characteristic simulation diagram of the pad structure corresponding to this example includes 6 metal layers (n=6) and the two existing pad structures, and Table 1 is a performance comparison table of applying the metal pad including 6 metal layers to the 10Gbps transimpedance amplifier (TIA).

[0104] Table 1

[0105] Conventional TM-PAD Conventional M1-M6 PAD This embodiment PAD reliability Poor very good better Parasitic capacitance (fF) Better (30fF) Poor (80fF) Better (40fF) 10G TIA Bandwidth (GHz) 10.47 7.94 10

[0106] It can be seen from the above figure that under the same process, the conventional M1-M6 PAD packaging has the best reliability, the TM-PAD packaging has the worst reliability, and the PAD structure of this embodiment is in the middle and can meet the reliability requirements. In terms of parasitic capacitance, the parasitic capacitance values ​​of the conventional TM-PAD, M1-M6 PAD and the PAD of this embodiment are 30fF, 80fF and 40fF respectively; correspondingly, Figure 3 The bandwidths of the 10Gbps TIA under the conventional TM-PAD, M1-M6 PAD and new PAD packages are 10.47GHz, 10GHz and 7.94GHz respectively. It can be seen that although the PAD package of this embodiment is not optimal in terms of reliability and parasitic effects, it can achieve the optimal solution while taking both into account, and is an excellent solution for high-speed chip PAD packaging.

[0107] Embodiment 2

[0108] In this embodiment, different from the pad structure in Embodiment 1, when the top metal layer of the pad structure includes multiple metal layers, some or all of the metal layers constituting the top metal layer have different shapes and / or areas, such as a gradient area design.

[0109] As an example, the area gradient may include gradually increasing the areas of all or part of the metal layers constituting the top metal layer in a direction from the bottommost metal layer of the top metal layer to the topmost metal layer of the top metal layer.

[0110] As an example, the area gradient may include a gradient in the areas of any several metal layers among the multiple metal layers constituting the top metal layer.

[0111] Specifically, the top metal layer includes M n-1 and M n , where M n-1 Layer in M n As an example, the metal layer M n The area is larger than the metal layer M n-1 The area of ​​the metal layer M nIn Metal M n Layer M n-1 The projection on the plane surrounds the metal layer M n-1 .

[0112] Embodiment 3

[0113] In this embodiment, different from the pad structure in the first or second embodiment, when the middle metal layer of the pad structure includes multiple metal layers, the shapes and / or areas of the metal layers constituting the middle metal layer are different, such as a design with a gradient area.

[0114] As an example, the area gradient may include gradually increasing the areas of all or part of the metal layers constituting the intermediate metal layer in a direction from the lowest metal layer of the intermediate metal layer to the highest metal layer of the intermediate metal layer.

[0115] As an example, the area gradient may include that the areas of any several metal layers among the multiple metal layers constituting the intermediate metal layer exist in a gradient.

[0116] Embodiment 4

[0117] The pad structure described in the first embodiment can effectively reduce the parasitic capacitance of each metal layer to the semiconductor substrate 1 and the coupling capacitance between metal layers. Among these parasitic capacitances, the upper and lower plates of the coupling capacitance (that is, any two metal layers of the pad PAD) are electrically connected to each other, so the coupling capacitance is short-circuited. In other words, the coupling capacitance has no effect on the signal of the pad PAD. As for the parasitic capacitance of each metal layer to the semiconductor substrate 1, the upper plate is the metal layer of the pad PAD, and the lower plate is the semiconductor substrate. In the CMOS process, the semiconductor substrate is connected to the "ground" by default. From the circuit point of view, these parasitic capacitances are working normally and will have a great impact on the output signal of the pad PAD. To this end, this embodiment also introduces a pad structure that can further reduce the parasitic capacitance of each metal layer to the semiconductor substrate 1. Please refer to Figure 7 and Figure 8 .

[0118] See 7 and Figure 8 The top view and the side view of another pad structure of the present invention are respectively shown. Figure 7 Schematic diagram of the cross section at DD in the figure. Figure 7 and Figure 8, which is different from the embodiment, a doped region is formed on the surface of the semiconductor substrate 1 close to the bottom metal layer, and the doped region serves as a floating well layer 6, and the bottom metal layer of the pad PAD is formed on the floating well layer 6 of the semiconductor substrate 1, and the bottom metal layer M1 of the pad PAD is separated from the floating well layer 6 by a dielectric layer 6. As an example, the floating well layer 6 can be formed on the surface of the semiconductor substrate 1 by thermal diffusion or ion implantation. As an example, the projection of the pad PAD in the plane where the floating well layer 6 is located is located inside the floating well layer 6, in other words, the floating well layer 6 surrounds the projection of the pad PAD in the plane where the floating well layer 6 is located, that is, the size of the floating well layer 6 is larger than the area of ​​each metal layer of the pad PAD.

[0119] In this embodiment, the floating well layer 6 and the semiconductor substrate 1 have different conductivity types, one is an electron conductive semiconductor and the other is a hole conductive semiconductor, that is, one is an N-type semiconductor and the other is a P-type semiconductor. In a specific example, the semiconductor substrate 1 is a P-type doped substrate, and the floating well layer 6 is N-type doped, that is, a floating N-well (N-Well) is formed; in another specific example, the semiconductor substrate 1 is an N-type doped substrate, and the floating well layer 6 is P-type doped, that is, a floating P-well (P-Well) is formed.

[0120] It should be noted that by arranging a floating well layer 6 with a larger area than the PAD under the pad PAD, the pad PAD is separated from the semiconductor substrate 1. Although the parasitic capacitance of each metal layer to the semiconductor substrate 1 still exists, the lower plates of these parasitic capacitors become the floating well layer 6, and the floating well layer 6 is floating. From the circuit point of view, the lower plates of these parasitic capacitors (floating well layer 6) have no specific connection, that is, these parasitic capacitors do not work correctly, and therefore have little effect on the output signal of the pad PAD as the upper plate. In other words, by adding a floating well layer 6 under the pad PAD, the effect of the parasitic capacitance of the pad PAD on its output signal can be greatly optimized.

[0121] In this embodiment, the floating well layer 6 may be in the shape of a (regular) octagon. In other embodiments, other shapes such as a quadrilateral, a hexagon, a circle, etc. may also be used. As an example, the shape of the floating well layer 6 and the top metal layer M of the pad PAD are similar. n The shapes of the floating well layer 6 may be the same (for example, the same octagon, quadrilateral, hexagon or circle), or different, but it is necessary to ensure that the size of the floating well layer 6 is larger than the area of ​​each metal layer of the pad PAD.

[0122] The technical solution of setting a floating well layer 6 in the semiconductor substrate 1 and forming a pad PAD on the floating well layer 6 in this embodiment is applicable not only to the pad structures of embodiments 1, 2 and 3, but also to pad structures of other structures, such as the TM-PAD or M1-M6 PAD mentioned above.

[0123] Embodiment 5

[0124] See also Fig.10 The present embodiment discloses a method for preparing a pad structure as described in the first embodiment, characterized in that the preparation method comprises step S10, forming a bottom metal layer including a plurality of separated conductive areas; step S20, sequentially forming a first dielectric layer and a middle metal layer on the bottom metal layer, wherein the first dielectric layer is provided with an intermediate conductive via connecting the middle metal layer and the bottom metal layer; step S30, sequentially forming a second dielectric layer and a top metal layer on the middle metal layer, wherein the second dielectric layer is provided with a top conductive via connecting the middle metal layer and the top metal layer; step S40, forming a top insulating layer on the top metal layer; step S50, opening a pad opening 4 in the top insulating layer to expose the interior of the upper surface of the top metal layer, wherein the area of ​​the top metal layer is respectively larger than the area of ​​the middle metal layer and the area of ​​the bottom metal layer, and the projection of the pad opening 4 on the plane where the middle metal layer is located surrounds the middle metal layer.

[0125] It should be noted that the first dielectric layer, the second dielectric layer, and the bottom interlayer dielectric layer, the middle interlayer dielectric layer, the top interlayer dielectric layer, and the third dielectric layer to be introduced later are collectively used as the dielectric layer 5 in the embodiment, and the dielectric layer 5 can improve the structural strength of the pad structure as a whole. As an example, the material of the dielectric layer 5 and the top dielectric layer 2 to be introduced below includes but is not limited to silicon oxide (silicon oxide), silicon nitride (silicon nitride), silicon carbide (silicon carbide), silicon oxynitride (silicon oxy-nitride), low dielectric constant or ultra low dielectric constant (ultra low-k, ULK) material (such as organic (such as aromatic hydrocarbons (SiLK)) or inorganic (such as hydrogen-containing silicate (HSQ)) material), or any combination of the above materials. In a specific example, the material of the dielectric layer 5 can be, for example, silicon dioxide.

[0126] See also Figure 2As shown, the pad structure of the present embodiment can be arranged on a semiconductor substrate 1, and one or more active devices can be formed on the substrate 1. The active devices can be transistors, diodes and other known active devices, and the passive devices can be resistors, capacitors and inductors and other various known passive devices. The substrate is connected to the pad of the present invention to form a semiconductor device, but the substrate 1 does not have a key impact on the pad structure of the present invention, so it will not be repeated here.

[0127] In step S10, refer to Figure 2 In this embodiment, the step of forming the bottom metal layer includes forming a plurality of sub-bottom metal layers on the semiconductor substrate 1 from bottom to top, wherein each sub-bottom metal layer includes a plurality of separated sub-conductive regions, and the sub-conductive regions at corresponding positions in two adjacent sub-bottom metal layers are connected by a first conductive through hole. As an example, each sub-bottom metal layer (M n-3 , ..., M2, M1) and the middle metal layer (metal M n-2 ), the top metal layer (metal layer M n and metal layer M n-1 ) can be made of, for example, copper, aluminum, or a copper-aluminum alloy or other conductive materials; each of the first conductive vias (conductive vias VIA1, VIA2 to VIA n-4 ), the middle conductive via (conductive via VIA n-3 ) and the top conductive via (conductive via VIA n-2 ) and the third conductive via (conductive via VIA n-1 ) may include conductive materials such as copper, aluminum, tungsten or copper-aluminum alloy.

[0128] As an example, the step of forming the bottom metal layer includes:

[0129] Step S11: First, a metal material layer is formed on the semiconductor substrate 1, and then Figure 1 The metal material layer is patterned according to the shape in the figure to form a sub-bottom metal layer (metal layer M1) including a plurality of separated sub-conductive regions;

[0130] Step S12, then forming a bottom interlayer dielectric layer (finally serving as a part of the dielectric layer 5) on the sub-bottom metal layer (metal layer M1), patterning the bottom interlayer dielectric layer to form a plurality of spaced channel holes in the bottom interlayer dielectric layer, the channel holes being divided into a plurality of regions corresponding to the sub-conductive regions of the sub-bottom metal layer M1, filling the channel holes with a conductive material, and performing a planarization process (e.g., chemical mechanical polishing CMP) to form a first conductive via (i.e., conductive via VIA1);

[0131] Step S13, after the planarization process step, continue to form a sub-bottom metal layer (metal layer M2) including a plurality of sub-conductive regions on the structure formed in step S12; it should be understood that the sub-bottom metal layer M2 and the first conductive via VIA1 can be formed separately or by a dual damascene process; the plurality of sub-conductive regions of the sub-bottom metal layer M1 are electrically connected to the plurality of sub-conductive regions of the sub-bottom metal layer M2 through a plurality of first conductive vias VIA1 (blocks), that is, each first conductive via VIA1 (block) corresponds to a sub-conductive region of the sub-bottom metal layer M1 and a sub-conductive region of the sub-bottom metal layer M2, that is, the number of first conductive vias VIA1 (blocks) between the sub-bottom metal layer M1 and the sub-bottom metal layer M2 is the same as the number of sub-conductive regions in the sub-bottom metal layer M1 / the number of sub-conductive regions in the sub-bottom metal layer M2, and each first conductive via VIA1 (block) includes a plurality of conductive channels arranged at intervals;

[0132] Step S14: Repeat steps S12 and S13 until a sub-bottom metal layer M is formed. n-3 , to complete the preparation of the bottom metal layer, the plurality of sub-conductive regions of the sub-bottom metal layer M2 are electrically connected to the plurality of sub-conductive regions of the sub-bottom metal layer M3 through a plurality of first conductive vias VIA2 (blocks); the sub-bottom metal layer M n-4 The plurality of sub-conductive regions are connected through a plurality of first conductive vias VIA n-4 (Block) and the sub-bottom metal layer M n-3 Several sub-conductive regions are electrically connected.

[0133] As an example, in step S10, the sizes of the sub-conductive areas at the corresponding positions in each sub-bottom metal layer are substantially the same (of course, there may be differences), so as to use the same Mask to save production costs. In other examples, the sizes of the sub-conductive areas at the corresponding positions in each sub-bottom metal layer may also be different. As an example, each first conductive via (conductive vias VIA1, VIA2, ..., VIA n-4) have basically the same aperture, and in other examples, there may be differences, which can be produced using the same Mask.

[0134] It should be noted that each conductive via VIA adopts Figure 1 and Figure 2 The design in is to increase the strength of the pad, improve the success rate of product package pad bonding, and reduce tape-out; this is because the conductive via VIA is conductive, generally made of metal materials, such as tungsten, which is relatively soft and is formed in the dielectric layer 5 (such as silicon dioxide). The more conductive vias VIA are formed in the dielectric layer, the less dielectric layer 5 will be below the pad opening 4 (Pad opening), which is equivalent to reducing the strength of the dielectric layer below the pad opening 4, which is not conducive to bonding. We have made improvements in two aspects. On the one hand, when bonding, the metal layer at a deeper position below the pad opening 4 will be directly hit, such as the middle metal layer (metal layer M n-2 ) in the bottom metal layer below, such as metal layer M2 or even M1, to cause wafer taping, and during wire bonding, it is generally located at the center of Pad opening, based on which each conductive via VIA can be placed around the pad opening 4; on the other hand, even if each conductive via VIA is set at an edge position, each conductive via VIA will cause the strength of the dielectric layer 5 nearby to be reduced. Therefore, between two adjacent metal layers, on the basis of ensuring electrical connection, the number of conductive channels in each conductive channel (block) should be minimized as much as possible, thereby reducing the influence of the conductive channel on the strength of the nearby dielectric layer 5 and improving the success rate of wire bonding.

[0135] For example, the number of conductive channels in a unit area can be reduced by increasing the spacing between the conductive vias VIA of each layer. Due to the manufacturing process, in a PAD structure composed of multiple metal layers, the spacing between the conductive vias VIA between the metal layers is generally selected to be equal to the size of VIA. In this embodiment, by changing the existing manufacturing process, the conductive vias VIA1, VIA2, ..., VIA n-1 The spacing between the conductive vias is greater than or equal to twice the aperture of each conductive via, so as to reduce the PAD separation caused by the stress during package bonding and further improve the reliability of the pad structure. As an example, the spacing between the conductive vias is greater than or equal to three times the aperture of each conductive via. This is because the metal layer area of ​​the PAD is generally large, and if the conductive vias VIA are too dense, the metal layer will be more brittle and relatively easier to rot, so the conductive vias VIA between the metal layers should be sparse.

[0136] It should be noted that, in this embodiment, the bottom metal layer adopts a separated conductive area structure in order to reduce the area of ​​the bottom metal layer as much as possible to reduce the parasitic capacitance of the pad structure, and the top metal layer M formed subsequently n 、M n-1 , and the middle metal layer M n-2 After three metal layers with larger areas are formed, the reliability requirements can be basically met. In this way, the pad structure obtained by the preparation method of this embodiment can take into account both reliability and parasitics, and meet the performance requirements of high-speed chips.

[0137] In this example, see Figure 1 and Figure 2 In step S20, a method similar to step S10 for preparing the metal layer and the conductive vias thereunder may be used to prepare the bottom metal layer (sub-bottom metal layer M n-3 ) on the first dielectric layer and the middle metal layer M n-2 , wherein the first dielectric layer is formed with a connection to the middle metal layer M n-2 The topmost sub-bottom metal layer (metal layer M) of the bottom metal layer n-3 ) between the intermediate conductive vias (conductive vias VIA n-3 ). See Figure 1 and Figure 2 In this embodiment, the area of ​​the middle conductive layer (metal layer Mn-2) is larger than the area of ​​each of the above-mentioned sub-bottom metal layers (metal layers Mn-3 to M1), and the middle metal layer (metal layer M n-2 ) is an integral structure, rather than a discrete structure, which is located at the bottom metal layer M n-3 The projection of the plane surrounds the sub-bottom metal layer M n-3 In other embodiments, the middle metal layer (metal layer M n-2 ) can also be configured to include a plurality of discrete conductive regions, wherein the conductive region of the bottom metal layer corresponds to the conductive region of the middle metal layer, so as to facilitate the interconnection between the upper and lower layers. It should be noted that, although in the present invention, the middle metal layer includes a metal layer M n-2 However, it can be understood that, in other examples, the middle metal layer can also adopt multiple metal layers, which are respectively used as sub-middle metal layers of the middle metal layer, and adjacent sub-middle metal layers are connected through second conductive through holes.

[0138] It should be noted that when the middle metal layer of the pad structure includes multiple metal layers, the shapes and / or areas of the metal layers constituting the middle metal layer are different, such as a design with a gradual area change. As an example, the gradual area change may include a direction from the bottom metal layer of the middle metal layer to the top metal layer of the middle metal layer, where the areas of all or part of the metal layers constituting the middle metal layer gradually increase. As an example, the gradual area change may include a gradual change in the areas of any of the multiple metal layers constituting the middle metal layer.

[0139] In this example, see Figure 1 and Figure 2 Since there will be great stress during wire bonding, a larger metal layer area can reduce such stress and improve the reliability of the PAD. In order to reduce parasitic capacitance, the area of ​​the metal layer needs to be reduced as much as possible. Therefore, in this embodiment, in order to improve the reliability of the packaged PAD and take into account the parasitic effect, in step S30, the middle metal layer (metal layer M n-2 ) is formed from bottom to top including metal layers M n-1 and metal layer M n , as a sub-top metal layer of the top metal layer, and formed between the two metal layers M n-1 and M n A top interlayer dielectric layer is formed between the top interlayer dielectric layer, wherein a connecting metal layer M is formed in the top interlayer dielectric layer n-1 and M n The third conductive via (conductive via VIA n-1 ), the metal layer M n-1 and M n As the top metal layer. The specific steps include:

[0140] Step S31: A method similar to the method for preparing the metal layer and the conductive vias thereunder in step S10 may be used to prepare the metal layer and the conductive vias thereunder in the middle metal layer (metal layer M n-2 ) and sequentially forming a second dielectric layer and a metal layer M n-1 , and connected to the metal layer M n-1 and the middle metal layer (metal layer M n-2 ) between the top conductive vias (conductive vias VIA n-2 ); The difference is that the metal layer M n-1 With the top conductive via VIA n-2 The shape and position of the

[0141] Step S32: A method similar to the method for preparing the metal layer and the conductive vias thereunder in step S10 may be used to prepare the metal layer M n-1 The top interlayer dielectric layer and the metal layer M are sequentially formed on n, wherein the top interlayer dielectric layer is formed with a connection to the metal layer M n With metal layer M n-1 Conductive vias n-1 , as the third conductive via, the metal layer M n With metal layer M n-1 The two sub-top metal layers are respectively used as the top metal layer, and the difference is that the metal layer M n With the conductive vias VIA n-1 It should be noted that, in other embodiments, the top metal layer may also include a metal layer (see Figure 3 and Figure 4 ), or three metal layers (see Figure 5 and Figure 6 ), which can be selected based on comprehensive consideration of device performance.

[0142] It should be noted that when the top metal layer of the pad structure includes multiple metal layers, the shapes and / or areas of some or all of the metal layers constituting the top metal layer are different, such as a design with a gradual area change. As an example, the gradual area change may include that the areas of all or part of the metal layers constituting the top metal layer gradually increase in the direction from the bottom metal layer of the top metal layer to the top metal layer of the top metal layer. As an example, the gradual area change may include that the areas of any of the multiple metal layers constituting the top metal layer have a gradual change. In a specific example, taking the structure in which the top metal layer includes Mn-1 and Mn, wherein the Mn-1 layer is under the Mn layer, the area of ​​the metal layer Mn is greater than the area of ​​the metal layer Mn-1, and the projection of the metal layer Mn on the plane where the metal Mn layer Mn-1 is located surrounds the metal layer Mn-1.

[0143] In step S40 and step S50, please refer to Figure 1 and Figure 2 , forming a top dielectric layer 2 on the surface of the structure formed in step S30; forming a top passivation layer 3 in the top dielectric layer 2; and then etching the top dielectric layer 2 and the top passivation layer 3 downward in sequence through an etching process, and stopping the etching at the top metal layer (the first top metal layer M n ) is formed on the surface of the bonding pad opening 4, wherein the bonding pad opening 4 exposes the first top metal layer M n And located in the first top metal layer M n In, get Figure 1 and Figure 2 As an example, the material of the top dielectric layer 2 may be silicon dioxide.

[0144] In this example, see Figure 1 and Figure 2 The first conductive vias (conductive vias VIA1, VIA2, ..., or VIA n-4 ), the middle conductive via (conductive via VIA n-3 ), the top conductive via (conductive via VIA n-2 ), the third conductive via (conductive via VIA n-1 ) include multiple independent blocks, distributed at the edge of the upper and lower metal layers, so as to ensure the strength of the middle position of the dielectric layer between the upper and lower metal layers. Figure 1 and Figure 2 In the embodiment, since the conductive areas of the bottom metal layer are connected along the middle metal layer M n-2 The edge of the third conductive via (conductive via VIA n-2 ) corresponds to the position of each conductive area in the bottom metal layer, and the intermediate conductive via (conductive via VIA n-3 ) corresponds to the position of each conductive area in the bottom metal layer one by one, that is, each first conductive via (conductive vias VIA1, VIA2, ..., VIA n-4 ), and the intermediate conductive via (conductive via VIA n-3 ) are located on the same vertical line and are respectively located in the middle metal layer M n-2 The first top conductive through hole VIA n-1 In the middle metal layer M n-2 The projection on the plane is located at the middle metal layer M n-2 outside of the.

[0145] In this example, see Figure 1 and Figure 2 In order to ensure sufficient contact area for bonding during wire bonding to increase reliability, the top metal layer (metal layer M n and metal layer M n-1) can adopt a (regular) octagon, and in other embodiments, other shapes such as a quadrilateral, hexagon, circle, etc. can also be adopted. The octagon can increase the area of ​​the pad opening 4 while also helping to reduce the difficulty of layout design and manufacturing process. In the layout design and manufacturing process, angles such as 0°, 45°, 90°, and 135° are easier to achieve; the pad opening 4 also adopts an octagon, and in other embodiments, other shapes such as a quadrilateral, hexagon, circle, etc. can also be adopted; the middle metal layer adopts a (regular) quadrilateral, and in other embodiments, other shapes such as an octagon, hexagon, circle, etc. can also be adopted. As an example, in order to obtain the maximum area, the middle metal layer can be a square, and the four vertices of the square fall on the edge lines of the projection of the pad opening 4 on the plane where the middle metal layer is located. The bottom metal layer includes four conductive areas (it may also include more conductive areas), and the four conductive areas are respectively located at the four top corners of the middle metal layer of the square. In some examples, the four conductive areas can also be set at other positions on the edge of the square. In other examples, the four conductive areas can also be set at any other position of the middle metal layer.

[0146] It should be noted that the formation process of the pad structure corresponding to the second embodiment and the third embodiment is similar to that of this embodiment and will not be described in detail here.

[0147] Embodiment 6

[0148] This embodiment also introduces a method for preparing a pad structure in which a floating well layer 6 is formed in a semiconductor substrate 1 at the bottom of a pad PAD, and the parasitic capacitance of each metal layer to the semiconductor substrate 1 is further reduced by the floating well layer 6. The method for preparing the pad structure of this embodiment is basically the same as the method for preparing the pad of the fifth embodiment, except that a floating well layer 6 is formed in the semiconductor substrate 1, the bottom metal layer is formed on the floating well layer 6 in the semiconductor substrate 1, and a dielectric layer (third dielectric layer) is provided between the bottom metal layer and the floating well layer 6 for isolation, while in the fifth embodiment, no floating well layer 6 is formed in the semiconductor substrate 1, and the bottom metal layer is directly formed on the semiconductor substrate 1.

[0149] Specifically, see Figure 7 and Figure 8 For example, a doped region can be formed on the upper surface of the semiconductor substrate 1 by thermal diffusion or ion implantation, and the doped region serves as the floating well layer 6; after the floating well layer 6 is formed, a third dielectric layer (the same material as the dielectric layer 5 mentioned above) is formed above and below the semiconductor substrate 1, and then a bottom metal layer is formed on the third dielectric layer, that is, the pad PAD is formed on the floating well layer 6 of the semiconductor substrate 1, and the bottom metal layer M1 is separated from the floating well layer 6 by the dielectric layer 5 (third dielectric layer).

[0150] In this embodiment, the floating well layer 6 and the semiconductor substrate 1 have opposite conductivity types; one is an electron conductive semiconductor and the other is a hole conductive semiconductor, that is, one is an N-type semiconductor and the other is a P-type semiconductor. In a specific example, the semiconductor substrate 1 is a P-type doped substrate, and the floating well layer 6 is N-type doped, that is, a floating N-well (N-Well) is formed; in another specific example, the semiconductor substrate 1 is an N-type doped substrate, and the floating well layer 6 is P-type doped, that is, a floating P-well (P-Well) is formed.

[0151] See also Figure 7 and 8 In this embodiment, the floating well layer 6 may be in the shape of a (regular) octagon. In other embodiments, other shapes such as a quadrilateral, a hexagon, a circle, etc. may also be used. As an example, the shape of the floating well layer 6 and the top metal layer M of the pad PAD are similar. n The shapes of the floating well layer 6 may be the same (for example, the same octagon, quadrilateral, hexagon or circle), or different, but it is necessary to ensure that the size of the floating well layer 6 is larger than the area of ​​each metal layer of the pad PAD.

[0152] See also Figure 7 and 8 , the projection of the pad PAD formed finally in the plane where the floating well layer 6 is located is located inside the floating well layer 6. In other words, the floating well layer 6 surrounds the projection of the pad PAD in the plane where the floating well layer 6 is located, that is, the size of the floating well layer 6 is respectively larger than the area of ​​each metal layer of the pad PAD. By arranging a floating well layer 6 with a larger area than the PAD under the pad PAD, the pad PAD is separated from the semiconductor substrate 1. Although the parasitic capacitance of each metal layer to the semiconductor substrate 1 still exists, the lower plates of these parasitic capacitors become the floating well layer 6, and the floating well layer 6 is floating. From the circuit point of view, the lower plates of these parasitic capacitors (floating well layer 6) have no specific connection, that is, these parasitic capacitors do not work correctly, and therefore have little effect on the output signal of the pad PAD as the upper plate. In other words, by adding a floating well layer 6 under the pad PAD, the effect of the parasitic capacitance of the pad PAD on its output signal can be greatly optimized.

[0153] The technical solution of setting a floating well layer 6 in the semiconductor substrate 1 and forming a pad PAD on the floating well layer 6 in this embodiment is applicable not only to the pad structures of embodiments 1, 2 and 3, but also to pad structures of other structures, such as the TM-PAD or M1-M6 PAD mentioned above.

[0154] In summary, the pad structure and preparation method of the present invention can be applied to high-speed chip packaging PAD structure, taking into account both parasitic effects and reliability, not only ensuring the reliability of PAD during chip packaging wiring, but also greatly reducing the parasitic effects caused by using a full-layer metal PAD, and can be applied to high-speed chips, such as optical communication transimpedance amplifiers, limiting amplifiers, clock recovery circuits, laser diode drivers, etc.; the pad structure of the present invention can effectively reduce the parasitic capacitance between each metal layer and the semiconductor substrate in the pad structure by setting a floating gate layer in the semiconductor substrate under the pad structure. Therefore, the present invention effectively overcomes the various shortcomings of the prior art and has a high industrial utilization value.

[0155] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A pad structure, characterized in that: The pad structure comprises: A bottom metal layer, comprising a plurality of separated conductive regions, wherein the bottom metal layer comprises three sub-bottom metal layers; A middle metal layer is formed on the bottom metal layer, the middle metal layer is connected to the bottom metal layer through an intermediate conductive through hole, the middle metal layer includes a sub-middle metal layer, the middle metal layer is a square, and the four vertices of the square middle metal layer fall on the edge line of the projection of the pad opening on the plane where the middle metal layer is located, and the bottom metal layer includes four conductive areas, and the four conductive areas are respectively located at the four vertex positions of the square middle metal layer; A top metal layer is formed on the middle metal layer, the middle metal layer is connected to the top metal layer through a top conductive via, the top metal layer includes two sub-top metal layers, and the top metal layer is in a regular octagon; A top insulating layer is disposed on the top metal layer, wherein a pad opening for exposing the upper surface of the top metal layer is provided in the top insulating layer, and the pad opening is in a regular octagon; A dielectric layer, wherein the dielectric layer is respectively disposed in the gaps between the conductive regions of the bottom metal layer, the gap between the top metal layer and the middle metal layer, and the gap between the middle metal layer and the bottom metal layer; Among them, the area of ​​the top metal layer is respectively larger than the area of ​​the middle metal layer and the area of ​​the bottom metal layer, and the projection of the pad opening on the plane where the middle metal layer is located surrounds the middle metal layer; the critical dimensions of the pad opening, the top metal layer and the middle metal layer in the horizontal direction are respectively between 65μm-75μm, between 70μm-78μm and between 45μm-55μm.

2. The pad structure according to claim 1, characterized in that: Each sub-bottom metal layer includes a plurality of separated sub-conductive regions; the sub-conductive regions at corresponding positions in two adjacent sub-bottom metal layers are connected via a first conductive through hole.

3. The pad structure according to claim 1, characterized in that: The sub-middle metal layer includes a plurality of separate conductive regions, and the conductive regions of the bottom metal layer correspond to the conductive regions of the middle metal layer.

4. The pad structure according to claim 1, characterized in that: The spacing between the middle conductive vias or the top conductive vias is greater than or equal to twice the diameter of each conductive via.

5. The pad structure according to claim 2, characterized in that: The spacing between the first conductive through holes is greater than or equal to twice the diameter of each conductive through hole.

6. The pad structure according to claim 1, characterized in that: Two adjacent sub-top metal layers are connected via a third conductive via.

7. The pad structure according to claim 6, characterized in that: The projection of the third conductive via on the plane where the middle metal layer is located is located outside the middle metal layer.

8. The pad structure according to claim 1, characterized in that: The position of the middle conductive via corresponds to the position of the conductive area of ​​the bottom metal layer.

9. The pad structure according to claim 1, characterized in that: The top insulating layer includes a top passivation layer and a top dielectric layer located between the top passivation layer and the top metal layer; The pad opening penetrates the top passivation layer and the top dielectric layer.

10. The pad structure according to any one of claims 1 to 9, characterized in that: The pad structure also includes a semiconductor substrate. A doped region is formed on the surface of the semiconductor substrate close to the bottom metal layer. The doped region serves as a floating well layer, and the floating well layer is isolated from the bottom metal layer by the dielectric layer.

11. The pad structure according to claim 10, characterized in that: The projection of the top metal layer on the plane where the floating well layer is located is located inside the floating well layer.

12. The pad structure according to claim 10, characterized in that: The floating well layer and the semiconductor substrate have different conductivity types.

13. A method for preparing a pad structure, characterized in that: The preparation method comprises: forming a bottom metal layer, comprising a plurality of separated conductive regions, wherein the step of forming the bottom metal layer comprises sequentially forming three sub-bottom metal layers; A first dielectric layer and a middle metal layer are sequentially formed on the bottom metal layer, wherein an intermediate conductive through hole connecting the middle metal layer and the bottom metal layer is formed in the first dielectric layer; the step of forming the middle metal layer comprises: forming a sub-middle metal layer on the first dielectric layer, the middle metal layer is a square, and the four vertices of the square middle metal layer fall on the edge line of the projection of the pad opening on the plane where the middle metal layer is located; the bottom metal layer comprises four conductive areas, and the four conductive areas are respectively located at the four vertex positions of the square middle metal layer; A second dielectric layer and a top metal layer are sequentially formed on the middle metal layer, wherein a top conductive via connecting the middle metal layer and the top metal layer is formed in the second dielectric layer; the step of forming the top metal layer comprises: sequentially forming two layers of sub-top metal layers on the second dielectric layer, wherein the top metal layer is in a regular octagon; forming a top insulating layer on the top metal layer; A pad opening is formed in the top insulating layer to expose the upper surface of the top metal layer, wherein the pad opening is in a regular octagonal shape; Among them, the area of ​​the top metal layer is respectively larger than the area of ​​the middle metal layer and the area of ​​the bottom metal layer, and the projection of the pad opening on the plane where the middle metal layer is located surrounds the middle metal layer; the critical dimensions of the pad opening, the top metal layer and the middle metal layer in the horizontal direction are respectively between 65μm-75μm, between 70μm-78μm and between 45μm-55μm.

14. The method for preparing a pad structure according to claim 13, characterized in that: The step of forming the bottom metal layer comprises: Each sub-bottom metal layer includes a plurality of separated sub-conductive regions; the sub-conductive regions at corresponding positions in two adjacent sub-bottom metal layers are connected via a first conductive through hole.

15. The method for preparing a pad structure according to claim 13, characterized in that: The sub-middle metal layer includes a plurality of separate conductive regions, and the conductive regions of the bottom metal layer correspond to the conductive regions of the middle metal layer.

16. The method for preparing a pad structure according to claim 13, characterized in that: The spacing between the middle conductive vias or the top conductive vias is greater than or equal to twice the diameter of each conductive via.

17. The method for preparing a pad structure according to claim 14, characterized in that: The spacing between the first conductive through holes is greater than or equal to twice the diameter of each conductive through hole.

18. The method for preparing a pad structure according to claim 13, characterized in that: The conductive regions of the bottom metal layer are arranged at the edge of the middle metal layer.

19. The method for preparing a pad structure according to claim 13, characterized in that: The step of forming the top metal layer further includes: Two adjacent sub-top metal layers are connected via a third conductive via.

20. The method for preparing a pad structure according to claim 19, characterized in that: The projection of the third conductive via on the plane where the middle metal layer is located is located outside the middle metal layer.

21. The method for preparing a pad structure according to claim 13, characterized in that: The position of the middle conductive via corresponds to the position of the conductive area of ​​the bottom metal layer.

22. The method for preparing a pad structure according to claim 13, characterized in that: The step of forming a top insulating layer on the top metal layer comprises: forming a top dielectric layer on the top metal layer; forming a top passivation layer in the top dielectric layer; Wherein, the pad opening penetrates the top passivation layer and the top dielectric layer.

23. The method for preparing a pad structure according to any one of claims 13 to 22, characterized in that: The bottom metal layer is formed on a semiconductor substrate, and the step of forming a bottom metal layer includes: A doped region is formed on the surface of the semiconductor substrate close to the bottom metal layer, and the doped region serves as a floating well layer; forming a third dielectric layer on the floating well layer, The bottom metal layer is formed on the third dielectric layer.

24. The method for preparing a pad structure according to claim 23, characterized in that: The projection of the top metal layer on the plane where the floating well layer is located is located inside the floating well layer.

25. The method for preparing a pad structure according to claim 23, characterized in that: The floating well layer and the semiconductor substrate have different conductivity types.

26. A semiconductor device, characterized in that: The semiconductor device comprises the pad structure according to any one of claims 1-12.