Extreme ultraviolet light mask and method for manufacturing the same
By using a multi-layer absorber layer in an extreme ultraviolet mask, including an oxide layer as an isolation body, the carbon pollution problem is solved, key dimensional consistency is improved, and multiple structures are defined on semiconductor components, achieving better Extreme UV mask performance.
Patent Information
- Application Number
- CN202011388345.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-01-17
- Filing Date
- 2020-12-01
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2040-12-01
AI Technical Summary
Extreme UV masks are susceptible to hydrocarbon contamination during exposure, resulting in key dimension shifts and inconsistencies in the wafer, affecting the performance of semiconductor components.
A multi-layer absorbing layer is employed, including at least one oxide layer as a separator to reduce the reaction of the hydrocarbon with the metal cover layer and to define the structure of the semiconductor element by etching to form features. The multilayer absorbing layer includes a first metal oxide layer, a metal nitride layer and a second metal oxide layer, and a hard mask layer and a photoresist are used during the etching to define and transfer patterns.
It effectively avoids carbon pollution, improves the key dimensional consistency of features, improves the performance of extreme ultraviolet masks, and defines multiple structures on semiconductor components.
Smart Images

Figure CN113138528B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a mask used in an extreme ultra violet (EUV) lithography process and a method for manufacturing the mask. Background Art
[0002] Optical lithography can be performed in a variety of different ways. One example of an optical lithography process is extreme ultraviolet lithography (EUV). EUV lithography is based on exposure using a portion of the electromagnetic spectrum with a wavelength of 10 to 15 nanometers.
[0003] In one example, an EUV mask can be used to define the structure of multiple layers in a substrate. The EUV mask can be reflective. Thus, by selectively removing the absorbent layer to reveal a portion of a lower mirrored volume overlying the substrate, a pattern on the EUV mask can be defined. Summary of the invention
[0004] One aspect of the present disclosure is to provide an extreme ultraviolet mask. The mask includes a substrate, a multi-layer mirror layer formed on the substrate, a metal cap layer formed on the multi-layer mirror layer, and a multi-layer absorber layer. The multi-layer absorber layer includes at least one oxide layer formed on the multi-layer mirror layer. The multi-layer absorber layer includes a plurality of features etched into the multi-layer absorber layer to define a plurality of structures on a semiconductor device.
[0005] Another aspect of the present disclosure is to provide an EUV mask, the mask comprising a substrate, a multi-layer mirror layer formed on the substrate, a metal cap layer formed on the multi-layer mirror layer, and an oxide-containing absorber layer formed on the multi-layer mirror layer. The oxide-containing absorber layer comprises a plurality of features etched into the multi-layer absorber layer to define a plurality of structures on a semiconductor device.
[0006] Another aspect of the present disclosure is to provide a method for manufacturing an EUV photomask. First, a multi-layer absorption layer including at least one oxide layer is deposited on a multi-layer mirror layer; then, a plurality of features are defined in the multi-layer mirror layer through the steps of exposing, baking, and developing a photoresist coated on a hard mask layer; and then, the multi-layer absorption layer is etched to form features in the multi-layer absorption layer to define a plurality of structures on a semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] The present disclosure is better understood by reading the following detailed description in conjunction with the accompanying drawings. It should be noted that, as is standard practice in the industry, many features are not drawn to scale. In fact, for the sake of clarity of discussion, the dimensions of many features may be arbitrarily scaled.
[0008] Figure 1is a schematic cross-sectional view of an extreme ultraviolet (EUV) mask according to at least one embodiment of the present disclosure;
[0009] Figure 2 is a cross-sectional schematic diagram illustrating an EUV mask having multiple absorption layers according to at least one embodiment of the present disclosure;
[0010] Figure 3 is a flow chart illustrating a method for forming an EUV mask according to at least one embodiment of the present disclosure;
[0011] FIG. 4A to FIG. 4J is a partial cross-sectional schematic diagram illustrating an EUV mask at various manufacturing sites according to at least one embodiment of the present disclosure;
[0012] Figure 5 is a schematic diagram of an EUV lithography system using an EUV mask in the present disclosure.
[0013]
Explanation of symbols
[0014] 10: Optical lithography system
[0015] 12: Radiation Source
[0016] 14: Illuminator
[0017] 16: Photomask base
[0018] 20: Projection optical box
[0019] 22: Semiconductor substrate
[0020] 24: Substrate base
[0021] 100: Extreme Ultraviolet Photomask
[0022] 102: Base material
[0023] 104: Multiple mirror layers
[0024] 106: Metal Covering
[0025] 108: Multiple absorption layers
[0026] 1101-110 n :feature
[0027] 112: High refractive index material
[0028] 114: Low refractive index material
[0029] 116: First metal oxide layer
[0030] 118: Metal nitride layer
[0031] 119: Second metal oxide layer
[0032] 120: Hard mask layer
[0033] 122: Photoresist
[0034] 1241-124 n :feature
[0035] 150: Tantalum boride or chromium nitride layer
[0036] 300: Methods 302, 304, 306, 308, 310, 312, 314, 316,
[0038] 318, 320: Operation
[0039] 40: Extreme ultraviolet light DETAILED DESCRIPTION
[0040] The following disclosure provides many different embodiments or examples to implement different features of the subject matter of the application. The specific examples of components and arrangements described below are intended to simplify the disclosure. These are of course only examples and are not intended to be limiting. For example, the size of the components is not limited to the disclosed ranges or values, but may depend on process conditions and / or desired characteristics of the device. Furthermore, the description of a first feature formed on or above a second feature includes embodiments in which the first feature and the second feature are in direct contact, and also includes embodiments in which other features are formed between the first feature and the second feature, so that the first feature and the second feature are not in direct contact. In addition, the disclosure repeats reference values and / or letters in various examples. The purpose of this repetition is to simplify and clarify the description and does not indicate a relationship between the various discussed embodiments and / or configurations.
[0041] Furthermore, spatially relative terms, such as "beneath," "below," "lower," "above," "upper," etc., are used to facilitate description of the relationship of an element or feature illustrated in the drawings to other elements or features. Spatially relative terms encompass different orientations of the device in use or operation in addition to the orientation depicted in the drawings. The device may be otherwise oriented (rotated 90 degrees or at other orientations), and the spatially relative descriptors used herein may be interpreted so.
[0042] The advanced lithography processes, methods, and materials described in the present disclosure may be used in a variety of applications including fin-type field effect transistors (FETs). For example, fins may be patterned to create relatively close gaps between features, and the disclosure is suitable for use therein. In addition, spacers used to form fins of fin-type field effect transistors may be processed according to the above disclosure.
[0043] The present disclosure relates to various embodiments that can prevent carbon contamination of EUV masks. Carbon contamination has a negative impact on the critical dimensions of features formed in the absorber and capping layers of the EUV mask. For example, some metal capping layers may have many free radicals that can react with hydrocarbons near the surface of the EUV mask during the exposure process. During the exposure process, the hydrocarbons near the surface of the EUV mask break due to the high energy during the exposure. The carbon grown on the metal layer will cause problems with the critical dimensions of the wafer.
[0044] The present disclosure generally provides a multi-layer absorber or a multi-layer capping layer in an EUV mask. At least one layer in the EUV mask includes an oxide. The oxide can act as an insulator to minimize the reaction of the absorber layer with hydrocarbons or carbon during wafer exposure.
[0045] Figure 1 An EUV mask 100 is shown according to an embodiment of the present disclosure. The mask 100 includes a substrate 102, a multi-layer (ML) mirror layer 104, a metal cap layer 106, and a multi-layer absorber layer 108. In one embodiment, the substrate 102 is a low temperature expansion material (LTEM) deposited on a layer 150. The layer 150 is a tantalum boride (TaB) layer or a chromium nitride (CrN) layer. The substrate 102 has a low defect level and a smooth surface. The substrate 102 can be glass, a glass-ceramic material, or silicon.
[0046] In one embodiment, the multi-layer mirror layer 104 may include alternating layers of a high refractive index material 112 and a low refractive index material 114. In one example, the high refractive index material 112 may be molybdenum (Mo) and the low refractive index material 114 may be silicon (Si). However, it should be noted that any type of material may be used. In one embodiment, 40 pairs of high refractive index material 112 and low refractive index material 114 may be formed on the substrate 102. However, it should be noted that the alternating layers in the multi-layer mirror layer 104 may be extended to any number of pairs.
[0047] The thickness of the high refractive index material 112 and the low refractive index material 114 may be a function of the selected wavelength of the illumination light and the incident angle of the illumination light. In one embodiment, the thickness of the high refractive index material 112 and the low refractive index material 114 is selected to maximize the constructive interference of the EUV light reflected at the respective interfaces and minimize the total absorption of the EUV light.
[0048] In one embodiment, the thickness of the high refractive index material 112 and the low refractive index material 114 is approximately one-quarter of the wavelength of the irradiated light. For example, assuming the wavelength is 10 nanometers (nm), the thickness of the high refractive index material 112 and the low refractive index material 114 are approximately 2.5 nanometers respectively. In one embodiment, the thickness of the high refractive index material 112 and the low refractive index material 114 may be different.
[0049] In one embodiment, a metal capping layer 106 may be deposited on the topmost layer of the multi-layer mirror layer 104. The metal capping layer 106 may prevent the high refractive index material 112 (e.g., molybdenum) from being oxidized by contact with the environment. In one embodiment, the metal capping layer 106 includes ruthenium (Ru) or ruthenium dioxide (RuO2). The metal capping layer 106 is deposited to a thickness of about 2.5 to 5.5 nanometers. In one embodiment, the metal capping layer 106 is deposited to a thickness of about 3.5 nanometers.
[0050] In one embodiment, the multi-layer absorber layer 108 may include multiple layers, including an absorber layer containing an oxide. In other words, at least one layer of the multi-layer absorber layer 108 contains an oxide. The oxide may act as an insulator to prevent carbon contamination. For example, the oxide may minimize the reaction of the multi-layer absorber layer 108 with hydrocarbons or carbon, which are generated during the printing of the multi-layer absorber layer 108. Hydrocarbons may contaminate the cover layer and affect the critical dimensions of the wafer. Further details of the different layers are shown in FIG. Figure 2 It is described in detail below.
[0051] In one embodiment, the multi-layer absorber layer 108 includes features 1101-110n (hereinafter, individually referred to as features 110 or collectively referred to as features 110). Features 110 may be etched into the multi-layer absorber layer 108. Features 110 define regions where extreme ultraviolet light can penetrate into the multi-layer mirror layer 104 to define structures on the semiconductor device.
[0052] As described above, some metal capping layers carry many free radicals that can react with hydrocarbons near the EUV mask surface during the EUV exposure process. The hydrocarbons may break into carbon. Aliphatic hydrocarbons or aromatic hydrocarbons may be deposited directly on the metal capping layer 106. Carbon or hydrocarbons on the metal capping layer 106 may cause problems with the critical dimension (CD) of the feature. For example, contamination with carbon or hydrocarbons causes CD shifts, including close trends or changes in CD uniformity. These problems have a negative impact on the performance of the EUV mask 110.
[0053] The present disclosure provides a multi-layer absorber layer 108 including an oxide to eliminate carbon contamination and improve CD uniformity in the feature 110. The single or multiple oxide layers in the multi-layer absorber layer 108 can act as an insulator and not react with carbon or hydrocarbons during EUV exposure. The oxide can also prevent carbon or hydrocarbons from reacting with free radicals in the metal cap layer 106.
[0054] Figure 2 More details are shown regarding the multi-layer absorber layer 108 in the EUV photomask 100 . Figure 2 The EUV mask 100 shown includes Figure 1 The EUV mask 100 shown has the same multiple layers and is manufactured in the same manner as Figure 1 The EUV mask 100 shown is the same. For example: Figure 2 The EUV mask 100 shown includes a substrate 102, a multi-layer mirror layer 104, a metal cap layer 106, and a multi-layer absorber layer 108 on a tantalum boride (TaB) layer 150. The dimensions of the multi-layer mirror layer 104 and the metal cap layer 106 are similar to those described above. Figure 1 The dimensions are similar.
[0055] In one embodiment, the multi-layer absorber layer 108 may be an oxide-based absorber layer, which includes a first metal oxide layer 116, a metal nitride layer 118, and a second metal oxide layer 119. The metal nitride layer 118 is between the first metal oxide layer 116 and the second metal oxide layer 119. In one embodiment, the material of the first metal oxide layer 116 and the material of the second metal oxide layer 119 may be the same. In one embodiment, the material of the first metal oxide layer 116 and the material of the second metal oxide layer 119 may also be different.
[0056] In one embodiment, the thickness of the metal nitride layer 118 is thicker than the first metal oxide layer 116 and the second metal oxide layer 119. In one embodiment, the thickness of the first metal oxide layer 116 is approximately equal to the thickness of the second metal oxide layer 119.
[0057] In particular, these oxide layers are part of the absorber layer, rather than being formed as a separate buffer layer as described in other EUV masks and methods. In addition, the multi-layer absorber layer 108 includes a metal oxide layer surrounding a metal nitride in the multi-layer absorber layer 108, or located on both sides or opposite sides of the metal nitride layer.
[0058] In one embodiment, the thickness of the first metal oxide layer 116 is about 0 to 5.5 nanometers, depending on the material of the first metal oxide layer 116. In one embodiment, the first metal oxide material includes tantalum boron oxide (TaBO). The tantalum boron oxide is deposited to a thickness of about 0 to 2 nanometers.
[0059] In one embodiment, the first metal oxide layer 116 includes tantalum pentoxide (Ta2O5). The tantalum pentoxide is deposited to a thickness of about 1 to 2 nanometers.
[0060] In one embodiment, the first metal oxide layer 116 includes ruthenium dioxide (RuO2), which is deposited to a thickness of about 0 to 5.5 nanometers.
[0061] In one embodiment, the first metal oxide layer 116 includes niobium ruthenium oxide (RuNbO). The niobium ruthenium oxide may have a niobium content greater than 20 atomic percent. The niobium ruthenium oxide is deposited to a thickness of about 0 to 5.5 nanometers.
[0062] In one embodiment, the first metal oxide layer 116 includes niobium pentoxide (Nb2O5). The niobium pentoxide is deposited to a thickness of about 0 to 5.5 nanometers.
[0063] In some embodiments, the metal capping layer 106 is optional depending on the material, for example, the metal capping layer 106 includes ruthenium dioxide, ruthenium niobium oxide, or niobium pentoxide.
[0064] In one example, the metal nitride layer 118 includes tantalum boron nitride (TaBN). The TaBN is deposited to a thickness between 60 and 75 nanometers. In one example, the TaBN is deposited to a thickness between 66 and 67 nanometers.
[0065] In one embodiment, when the first metal oxide layer 116 includes tantalum boron oxide, the thickness of the tantalum boron oxide is about 1 to 2 nanometers, and this thickness allows a small amount of tantalum boron oxide to remain on the metal cap layer 106 during the etching of the multi-layer absorber layer 108. For example, after etching the multi-layer absorber layer 108, less than 1 nanometer of tantalum boron oxide remains on the metal cap layer 106. The residual thickness of the tantalum boron oxide can be reduced by reducing the over-etching time of the metal nitride layer 118 by about 30%.
[0066] In one embodiment, the second metal oxide layer 119 comprises tantalum phosphite. The tantalum borate oxide is deposited to a thickness of about 1 to 5 nanometers. In one embodiment, the tantalum borate oxide is deposited to a thickness of about 2 nanometers.
[0067] In one embodiment, the feature 110 is etched into the metal nitride layer 118 of the multi-layer absorber layer 108 by an optical lithography process, wherein the optical lithography process is followed by a main etch and an over-etch process. For example: a hard mask is deposited on the multi-layer absorber layer 108, and a photoresist is spin-coated onto the hard mask. The feature 110 is defined using an electron beam writer or a laser beam writer. The portion of the photoresist not covered by the patterned mask can be exposed and developed using a radiation light source or an ultraviolet light source. The pattern is transferred to the hard mask, and the feature 110 is etched into the multi-layer absorber layer 108. The hard mask, the remaining photoresist, and the patterned mask are removed. FIG. 4A to FIG. 4J In one embodiment, the main etching and over-etching processes can be performed by ion etching or dry etching in various gas environments.
[0068] In one embodiment, the main etching process is performed by ion etching for about 30 to 50 seconds (s), using a source power of about 100 to 500 watts (W), a bias power of about 5 to 30 W, and a pressure of about 1 to 3 mTorr. The ion etching is performed in an environment of 50 to 150 cubic centimeters per second (sccm) of chlorine and 10 to 100 sccm of helium. In one embodiment, the main etching process is performed by ion etching for about 35 s, using a source power of about 300 W, a bias power of about 15 W, and a pressure of about 2 mTorr. The ion etching is performed in an environment of 100 sccm of chlorine and 60 sccm of helium. It should be noted that the above is an example of a value or range that can be applied to etching the multi-layer absorption layer 108.
[0069] In one embodiment, the overetch is performed by ion etching for about 30% of the main etch process time. Similar ranges of source power, bias power, pressure, chlorine gas, and helium gas flow rates for the main etch process time may be applied to the overetch.
[0070] In one embodiment, the feature 110 is etched into the metal nitride layer 118 of the multi-layer absorber layer 108 by pulsed source power. In other words, the source power is turned on and off in a pulsed manner to etch the feature 110 into the multi-layer absorber layer 108.
[0071] Figure 3 3 is a flow chart of a method 300 for forming an EUV mask according to at least one embodiment of the present disclosure. The method 300 may be performed using one or more different machines in a manufacturing plant under the control of a regulator or a manufacturer.
[0072] When method 300 is described and illustrated below as a series of actions or events, it should be understood that the order shown in these actions or events should not be interpreted in a restrictive sense. For example, in addition to being illustrated and / or described herein, some actions may occur in a different order and / or simultaneously with other actions or events. In addition, not all of the illustrated actions need to be used to implement one or more embodiments or aspects described herein. Further, one or more operations described herein may be completed in one or more separate actions and / or stages.
[0073] The method 300 starts at block 302. At block 304, the method 300 deposits a multi-layer absorber layer on the multi-layer mirror layer. The multi-layer absorber layer includes an oxide or at least one oxide layer to avoid carbon contamination, which negatively affects the critical dimensions of features formed in the multi-layer absorber layer. The multi-layer absorber layer includes a first metal oxide layer, a metal nitride layer, and a second metal oxide layer.
[0074] At block 306, method 300 deposits a hard mask layer on the multi-layer absorber layer. The hard mask layer can serve as an etch endpoint when subsequently removing the photoresist layer. The hard mask layer can be a metal oxynitride. In one embodiment, the hard mask layer is chromium oxynitride (CrON), chromium nitride (CrN), chromium oxynitride carbon (CrOCN), and the like. The hard mask layer is deposited to a thickness of about 3 to 10 nanometers.
[0075] At block 308, method 300 deposits photoresist on the hard mask layer. The photoresist is spin coated onto the hard mask layer. The photoresist is a radiation sensitive layer and is coated onto the hard mask layer. The photoresist is deposited to a thickness of about 100 to 1000 nanometers.
[0076] In block 310, method 300 performs the steps of exposure, post-exposure baking, and photoresist development. For example, an electron beam writer or a laser beam writer is used to define a pattern on the photoresist. The photoresist may then be post-processed by post-exposure baking and development steps.
[0077] After the photoresist is developed, the critical dimensions of the features in the photoresist can be measured. After the measurements, the features in the photoresist are transferred to the multi-layer absorber layer using the following blocks in method 300.
[0078] At block 312, method 300 performs hard mask etching. For example, features developed into the photoresist may define portions of the hard mask layer to be etched. Then, the selected portions of the hard mask layer are etched. In one embodiment, dry etching, wet etching, or a combination of both may be used to perform the etching step.
[0079] At block 314, method 300 removes the photoresist and then measures the critical dimensions of the features etched into the portion of the multi-layer absorber layer. In one embodiment, any form of measurement method or metrology instrument may be used to measure the critical dimensions. For example, a critical dimension scanning electron microscope (CD-SEM) may be used.
[0080] At block 316, method 300 completes the etching step of the multi-layer absorber layer. The etching step of the multi-layer absorber layer is performed by ion etching or dry etching. Examples of process parameters for ion etching are provided above. In one embodiment, ion etching can be performed by pulsing source power on and off.
[0081] At block 318, method 300 strips the hard mask layer, which can be selectively etched away from the multi-layer absorber layer. For example, the hard mask layer can be removed by a wet etch or dry etch process. The remaining structure after removing the hard mask layer is the EUV mask with multi-layer absorber layers of the present disclosure. As described above, the multi-layer absorber layer including oxide can avoid carbon contamination. At block 320, method 300 ends.
[0082] FIG. 4A to FIG. 4J are multiple partial cross-sectional views illustrating methods of forming an EUV mask at various manufacturing sites according to at least one embodiment of the present disclosure. Figure 4A First, a substrate 102 is provided. The substrate 102 is a low temperature expansion material (LTEM). Examples of the low temperature expansion material include glass, glass ceramic material, or silicon. The substrate 102 can be deposited on a layer 150. The layer 150 is a tantalum boride layer or a chromium nitride layer.
[0083] exist Figure 4B In the process, a multi-layer mirror layer 104 is deposited or formed on a substrate 102. In one embodiment, the multi-layer mirror layer 104 is formed on the substrate 102 by ion beam deposition (IBD) or direct current (DC) magnetron sputtering.
[0084] The multi-layer mirror layer 104 includes alternating layers of high refractive index material 112 and low refractive index material 114. In one embodiment, the high refractive index material 112 may be molybdenum and the low refractive index material 114 may be silicon.
[0085] The multi-layer mirror layer 104 has between 20 and 60 pairs of high refractive index material 112 and low refractive index material 114. In one embodiment, the multi-layer mirror layer 104 includes 40 pairs of high refractive index material 112 and low refractive index material 114.
[0086] exist Figure 4CIn the embodiment, a metal capping layer 106 is deposited on the multi-layer mirror layer 104. In one embodiment, the metal capping layer 106 can be deposited by an ion beam sputtering process. In one embodiment, the metal capping layer 106 is optional, depending on the material used for the multi-layer absorption layer 108, such as Figure 4D Draw and discuss below.
[0087] In one embodiment, the metal capping layer 106 can prevent the high refractive index material 112 (eg, molybdenum) from being oxidized by contacting the environment. Figure 4D As shown and discussed below, the metal capping layer 106 includes a material having a lower etch rate relative to the multi-layer absorber layer 108. Therefore, the metal capping layer 106 can protect the multi-layer mirror layer 104 when the multi-layer absorber layer 108 is patterned etched.
[0088] In one embodiment, the metal capping layer 106 comprises ruthenium, ruthenium dioxide (RuO2), ruthenium niobium oxide (RuNbO), niobium pentoxide (Nb2O5), and the like. The metal capping layer 106 is deposited to a thickness of about 2.5 to 5.5 nanometers. In one embodiment, the metal capping layer 106 is deposited to a thickness of about 3.5 nanometers.
[0089] exist Figure 4D In the embodiment, a multi-layer absorption layer 108 is formed on the multi-layer mirror layer 104. In some embodiments where a metal cap layer 106 is deposited, the multi-layer absorption layer 108 is formed on the metal cap layer 106.
[0090] In one embodiment, the multi-layer absorber layer 108 includes a first metal oxide layer 116, a metal nitride layer 118, and a second metal oxide layer 109. The layers of the multi-layer absorber layer 108 may be deposited one layer at a time by chemical vapor deposition (CVD) or ion beam sputtering.
[0091] In one embodiment, the first metal oxide layer 116 comprises tantalum boron oxide (TaBO), tantalum pentoxide (Ta2O5), ruthenium dioxide (RuO2), ruthenium niobium oxide (RuNbO), or niobium pentoxide (Nb2O5). When the first metal oxide layer 116 comprises tantalum boron oxide or tantalum pentoxide, the metal capping layer 106 may be deposited. When the first metal oxide layer 116 comprises ruthenium dioxide, ruthenium niobium oxide, or niobium pentoxide, the metal capping layer 106 may be removed, or the deposition process may be skipped. Figure 4C Related process steps.
[0092] In one embodiment, the metal nitride layer 118 includes tantalum boronitride (TaBN). In one embodiment, the second metal oxide layer 119 includes tantalum boron oxide (TaBO).
[0093] As described above, the oxides in the first metal oxide layer 116 and the second metal oxide layer 119 can act as spacers to prevent carbon contamination at the edges and center of features of the multi-layer absorber layer 108. Carbon contamination can negatively impact critical dimensions of features formed in the multi-layer absorber layer 108.
[0094] In addition, when the first metal oxide layer 116 is tantalum boron oxide, the tantalum boron oxide may be deposited to have a desired thickness to reduce the over-etching time. For example, the desired thickness allows a small amount of tantalum boron oxide to remain on the metal capping layer 106. For example, the tantalum boron oxide is deposited to a thickness of about 1 to 2 nanometers, so that less than about 1 nanometer of tantalum boron oxide remains on the metal capping layer 106 after etching the multi-layer absorber layer 108.
[0095] exist Figure 4E In one embodiment, a hard mask layer 120 is deposited on the multi-layer absorber layer 108. In one embodiment, the hard mask layer 120 is deposited by a chemical vapor deposition process. The hard mask layer 120 can be used as an etching endpoint when the photoresist layer is subsequently removed. The hard mask layer 120 can be a metal oxynitride. In one embodiment, the hard mask layer 120 is chromium oxynitride (CrON) and is deposited to a thickness of about 6 nanometers.
[0096] exist Figure 4F In the embodiment of the present invention, a photoresist 122 is deposited on the hard mask layer 120. The photoresist 122 can be coated on the hard mask layer 120, and then the features are exposed, baked, and developed, thereby transferring the pattern into the multi-layer absorber layer 108.
[0097] exist Figure 4G In the embodiment, the photoresist 122 can be etched to produce features 1241-124n (hereinafter, individually referred to as features 124 or collectively referred to as features 124), Figure 4F In FIG. 1 , feature 124 has been patterned into photoresist 122. Feature 124 corresponds to Fig. 4I Features 110 are shown etched into the multi-layer absorber layer 108, further details of which are discussed below.
[0098] exist Figure 4H In this embodiment, the etching step may successively etch the feature 124 through the hard mask layer 120 into the multi-layer absorber layer 108. In one example, reactive ion etching or dry etching may be used. Figure 4H In one embodiment, reactive ion etching is used and the process parameters are as described above.
[0099] In one embodiment, when feature 124 is partially etched into multi-layer absorber layer 108 , a critical dimension of feature 124 may be measured. If the measured critical dimension of feature 124 meets the expected critical dimension, feature 124 may continue to be etched through multi-layer absorber layer 108 .
[0100] exist Fig. 4I In the embodiment, etching is performed through the multi-layer absorber layer 108 to form features 1101 - 110 n , and a remaining portion of the first metal oxide 116 of the multi-layer absorber layer 108 is on the metal cap layer 106 . Fig. 4I The hard mask layer 120 is shown without the photoresist 122 after the photoresist 122 is removed. When the feature 110 is etched into the multi-layer absorber layer 108, the photoresist 122 is also etched away. In one embodiment, the feature 110 is etched into the multi-layer absorber layer 108 using a reactive ion etching process with pulsed source power.
[0101] In one embodiment, the features 110 are used to define structures in a semiconductor device. For example, the EUV mask 100 can be used to create structures based on the features 110 etched into the multi-layer absorber layer 108. An exemplary optical lithography system for using the EUV mask 100 and a process for creating semiconductor device structures is shown in FIG. Figure 5 , further details will be discussed below.
[0102] exist Figure 4J In accordance with at least one embodiment of the present disclosure, the hard mask layer 120 is stripped to form the final EUV mask 100. The hard mask layer 120 may be selectively etched away from the multi-layer absorber layer 108. For example, the hard mask layer 120 may be removed using a wet etch or dry etch process.
[0103] Figure 5 The schematic diagram of an optical lithography system 10 constructed according to some embodiments of the present disclosure describes how to apply this EUV mask 100 on the optical lithography system 10. The optical lithography system 10 is also generally referred to as a scanner that can be operated to perform a lithography exposure process. In the present embodiment, the optical lithography system 10 is an extreme ultraviolet (EUV) optical lithography system designed to expose a photoresist layer with extreme ultraviolet light (or extreme ultraviolet radiation). The optical lithography system 10 uses a radiation source 12 to generate extreme ultraviolet light 40, for example: extreme ultraviolet light having a wavelength range between about 1 nanometer and about 100 nanometers. In a specific example, the extreme ultraviolet light 40 has a wavelength centered at about 13.5 nanometers. Accordingly, the radiation source 12 is also referred to as an extreme ultraviolet radiation source 12. The extreme ultraviolet radiation source 12 uses a laser-induced plasma (LPP) mechanism to generate extreme ultraviolet radiation, which will be further described later.
[0104] The optical lithography system 10 also employs an illuminator 14. In some embodiments, the illuminator 14 includes various optical reflectors, such as a single mirror or a mirror system including multiple mirrors, to direct the light 40 from the radiation source 12 to the mask base 16, in particular, the EUV mask 100 fixed to the mask base 16.
[0105] The optical lithography system 10 also includes a photomask base 16 configured to fix the EUV photomask 100. In some embodiments, the photomask base 16 includes an electrostatic chuck (e-chuck) to fix the EUV photomask 100. In the present disclosure, the terms mask, photomask, and reticle are used interchangeably. In the present embodiment, the optical lithography system 10 is an EUV photolithography system. The EUV photomask 100 can be manufactured by the method described above.
[0106] The optical lithography system 10 also includes a projection optical module (or projection optical box POB) 20, which can image the pattern of the EUV mask 100 onto a semiconductor substrate 22, which is fixed to a substrate base (or wafer base) 24 of the optical lithography system 10. The projection optical box 20 in the present disclosure includes an optical reflector. The EUV light 40 carrying the image of the pattern defined on the EUV mask 100 is emitted from the EUV mask 100 and is collected by the projection optical box 20. The illuminator 14 and the projection optical box 20 can be collectively referred to as an optical module of the lithography system 10.
[0107] In this embodiment, the semiconductor substrate 22 is a semiconductor wafer to be patterned, such as a silicon wafer or other types of wafers. In this embodiment, a photoresist layer sensitive to extreme ultraviolet light 40 is coated on the semiconductor substrate 22. The various components described above are integrated together to operate the lithography exposure process.
[0108] The above summary summarizes the features of many embodiments, so that those with ordinary knowledge in the art can better understand the aspects of the present disclosure. Those with ordinary knowledge in the art should understand that other processes and structures can be designed or modified based on the present disclosure to achieve the same purpose and / or achieve the same advantages as the embodiments described. Those with ordinary knowledge in the art should also understand that equivalent structures do not deviate from the spirit and scope of the present disclosure, and various changes, exchanges and substitutions can be made without departing from the spirit and scope of the present disclosure.
[0109] Therefore, the present disclosure is about an EUV mask and a method for forming the same. In one embodiment, the present disclosure is about an EUV mask that can prevent carbon contamination. The mask includes a substrate, a multi-layer mirror layer formed on the substrate, a metal cap layer formed on the multi-layer mirror layer, and a multi-layer absorber layer. The multi-layer absorber layer includes at least one oxide layer formed on the multi-layer absorber layer, and the multi-layer absorber layer includes a plurality of features etched into the multi-layer absorber layer to define a plurality of structures on a semiconductor device. In some embodiments, the substrate includes at least a low temperature expansion material. In some embodiments, the multi-layer absorber layer includes at least a first metal oxide layer, a metal nitride layer, and a second metal oxide layer. In some embodiments, the first metal oxide layer includes at least one of tantalum boron oxide (TaBO), tantalum pentoxide (Ta2O5), ruthenium dioxide (RuO2), ruthenium niobium oxide (RuNbO), or niobium pentoxide (Nb2O5). In some embodiments, the first metal oxide layer includes tantalum boron oxide (TaBO) having a thickness of about 1 to 2 nanometers. In some embodiments, the metal capping layer comprises tantalum boron oxide (TaBO) or tantalum pentoxide (Ta2O5). In some embodiments, the metal capping layer comprises ruthenium or ruthenium dioxide (RuO2). In some embodiments, the thickness of the metal capping layer is about 0 to 4 nanometers. In some embodiments, the metal nitride layer comprises tantalum boron nitride (TaBN). In some embodiments, the second metal oxide layer comprises tantalum boron oxide (TaBO).
[0110] In another embodiment, the present disclosure is directed to an extreme ultraviolet photomask that can prevent carbon contamination. The photomask includes a substrate, a multi-layer mirror layer formed on the substrate, a metal cap layer formed on the multi-layer mirror layer, and an oxide-containing absorber layer formed on the multi-layer mirror layer. The oxide-containing absorber layer includes a plurality of features etched into the multi-layer absorber layer to define a plurality of structures on a semiconductor device. In some embodiments, the metal cap layer includes ruthenium or ruthenium dioxide (RuO2) having a thickness of about 0 to 4 nanometers. In some embodiments, the oxide-containing absorber layer formed on the metal cap layer includes a first tantalum boron oxide (TaBO) layer, a tantalum boron nitride (TaBN) layer, and a second tantalum boron oxide (TaBO) layer. In some embodiments, the oxide-containing absorber layer formed on the metal cap layer includes a tantalum boron oxide (TaBO) layer, a tantalum boron nitride (TaBN) layer, and a tantalum pentoxide (Ta2O5) layer. In some embodiments, the oxide-containing absorber layer comprises a tantalum boron oxide (TaBO) layer, a tantalum boron nitride (TaBN) layer, and a ruthenium dioxide (RuO2) layer. In some embodiments, the oxide-containing absorber layer comprises a tantalum boron oxide (TaBO) layer, a tantalum boron nitride (TaBN) layer, and a niobium ruthenium oxide (RuNbO) layer. In some embodiments, the oxide-containing absorber layer comprises a tantalum boron oxide (TaBO) layer, a tantalum boron nitride (TaBN) layer, and a niobium pentoxide (Nb2O5) layer.
[0111] In another embodiment, the present disclosure is directed to a method for manufacturing an EUV mask that can prevent carbon contamination. First, a multi-layer absorber layer including at least one oxide layer is deposited on the multi-layer mirror layer; then, multiple features are defined in the multi-layer mirror layer through the exposure, baking, and development steps of a photoresist coated on the hard mask layer; then, the multi-layer absorber layer is etched to form features in the multi-layer absorber layer to define multiple structures on the semiconductor device. In some embodiments, the multi-layer absorber layer includes a first metal oxide layer, a tantalum boron nitride (TaBN) layer, and a tantalum boron oxide (TaBO) layer. In some embodiments, the first metal oxide layer includes a material: at least one of tantalum boron oxide (TaBO), tantalum pentoxide (Ta2O5), ruthenium dioxide (RuO2), ruthenium niobium oxide (RuNbO), or niobium pentoxide (Nb2O5).
Claims
1. An extreme ultraviolet light mask, characterized in that: Include: a substrate; a multi-layer mirror layer formed on the substrate; a metal capping layer formed on the multi-layer mirror layer; and A multi-layer absorption layer comprises at least one oxide layer formed on the multi-layer mirror layer, wherein the multi-layer absorption layer comprises a plurality of features etched into the multi-layer absorption layer to define a plurality of structures on a semiconductor device, wherein there is an opening between each of the structures, and the multi-layer absorption layer comprises a first metal oxide layer, a metal nitride layer and a second metal oxide layer sequentially arranged on the metal cover layer, wherein the metal cover layer between each of the structures is covered by the first metal oxide layer, and a bottom of the opening is located at a top surface of the first metal oxide layer.
2. The extreme ultraviolet light mask according to claim 1, characterized in that: The substrate at least comprises a low temperature expansion material.
3. The extreme ultraviolet light mask according to claim 1, characterized in that: The first metal oxide layer includes at least one of tantalum boron oxide (TaBO), tantalum pentoxide (Ta2O5), ruthenium dioxide (RuO2), ruthenium niobium oxide (RuNbO), or niobium pentoxide (Nb2O5).
4. The extreme ultraviolet light mask according to claim 3, characterized in that: The first metal oxide layer includes tantalum boron oxide (TaBO) having a thickness of substantially 1 to 2 nanometers.
5. The EUV light mask according to claim 3, characterized in that: The metal capping layer includes tantalum boron oxide (TaBO) or tantalum pentoxide (Ta2O5).
6. The extreme ultraviolet light mask according to claim 5, characterized in that: The metal capping layer includes ruthenium or ruthenium dioxide (RuO2).
7. The extreme ultraviolet light mask according to claim 6, characterized in that: The thickness of the metal capping layer is substantially 0 to 4 nanometers.
8. The EUV light mask according to claim 1, wherein: The metal nitride layer includes tantalum boronitride (TaBN).
9. The EUV light mask according to claim 1, wherein: The second metal oxide layer includes tantalum boron oxide (TaBO).
10. An extreme ultraviolet light mask, characterized in that: Include: a substrate; a multi-layer mirror layer formed on the substrate; a metal capping layer formed on the multi-layer mirror layer; and An oxide-containing absorption layer is formed on the multi-layer mirror layer, wherein the oxide-containing absorption layer includes: a plurality of features etched into the oxide-containing absorption layer to define a plurality of structures on a semiconductor device, the metal capping layer between each of the structures is covered by a bottom layer of the oxide-containing absorption layer, and there is an opening between each of the structures, a bottom of the opening is located at a top surface of the bottom layer of the oxide-containing absorption layer.
11. The extreme ultraviolet light mask according to claim 10, characterized in that: The metal capping layer comprises ruthenium or ruthenium dioxide (RuO2) with a thickness of 0 to 4 nanometers.
12. The extreme ultraviolet light mask according to claim 10, characterized in that: The oxide-containing absorption layer includes a first tantalum boron oxide (TaBO) layer, a tantalum boron nitride (TaBN) layer, and a second tantalum boron oxide (TaBO) layer formed on the metal cap layer.
13. The EUV light mask according to claim 10, wherein: The oxide-containing absorption layer includes a tantalum boron oxide (TaBO) layer, a tantalum boron nitride (TaBN) layer, and a tantalum pentoxide (Ta2O5) layer formed on the metal cap layer.
14. The EUV light mask according to claim 10, wherein: The oxide-containing absorber layer includes a tantalum boron oxide (TaBO) layer, a tantalum boron nitride (TaBN) layer, and a ruthenium dioxide (RuO2) layer.
15. The extreme ultraviolet light mask according to claim 10, characterized in that: The oxide-containing absorber layer includes a tantalum boron monoxide (TaBO) layer, a tantalum boron nitride (TaBN) layer, and a niobium ruthenium monoxide (RuNbO) layer.
16. The EUV light mask according to claim 10, wherein: The oxide-containing absorber layer includes a tantalum boron monoxide (TaBO) layer, a tantalum boron nitride (TaBN) layer, and a niobium pentoxide (Nb2O5) layer.
17. A method for manufacturing an extreme ultraviolet light mask, characterized in that: Include: Depositing a multi-layer absorber layer including at least one oxide layer on a multi-layer mirror layer; Defining features in the multi-layer absorber layer by exposing, baking, and developing a photoresist coated on a hard mask layer; and The multi-layer absorption layer is etched to form the plurality of features in the multi-layer absorption layer to define a plurality of structures on a semiconductor device, each of which has an opening between the structures, wherein the multi-layer absorption layer has a bottom layer and a top layer located on the bottom layer, the bottom layer comprises a metal oxide, and a bottom of the opening is located on a top surface of the bottom layer of the multi-layer absorption layer.
18. The method for manufacturing an extreme ultraviolet light mask according to claim 17, characterized in that: The multi-layer absorber layer includes a first metal oxide layer, a tantalum boronitride (TaBN) layer, and a tantalum boron oxide (TaBO) layer.
19. The method for manufacturing an extreme ultraviolet light mask according to claim 18, characterized in that: The first metal oxide layer includes at least one of the following materials: tantalum boron oxide (TaBO), tantalum pentoxide (Ta2O5), ruthenium dioxide (RuO2), ruthenium niobium oxide (RuNbO), or niobium pentoxide (Nb2O5).