Vaporization device, substrate processing device, cleaning method, and method for manufacturing semiconductor device

The dual heating system controls the temperature of liquid raw materials, solves the problem of unstable gas supply, and achieves the stability of gasified gas supply and the rapid recovery of temperature, ensuring the continuity of the reaction process.

CN113496918BActive Publication Date: 2024-11-19KOKUSAI DENKI KK
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110294265.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-03-19
Filing Date
2021-03-18
Publication Date
2024-11-19
Estimated Expiration
2041-03-18

AI Technical Summary

Technical Problem

When gas is generated by gasification of liquid raw materials, the gas supply amount is unstable, resulting in a drop in the temperature of liquid raw materials, affecting the gasification amount and the continuity of the reaction process.

Method used

The dual heating system is adopted, and the temperature of the liquid raw materials is controlled separately through the internal heater and the external heater to ensure the stability of the supply flow of the gasified gas.

Benefits of technology

The supply flow of gasification gas is stabilized, the temperature recovery time of liquid raw materials is shortened, and the temperature overshoot and flow rate drop caused by gasification heat is prevented.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113496918B_ABST
    Figure CN113496918B_ABST
Patent Text Reader

Abstract

The present invention relates to a vaporization device, a substrate processing device, a cleaning method, and a method for manufacturing a semiconductor device. A technology capable of stabilizing the supply flow rate of vaporized gas is provided. The vaporization device comprises: a liquid container that stores a liquid raw material; a first heating unit that is immersed in the liquid raw material stored in the liquid container and heats the liquid raw material; a second heating unit that heats the liquid container; a first temperature sensor that is immersed in the liquid raw material stored in the liquid container and measures the temperature of the liquid raw material; a second temperature sensor that measures the temperature of the liquid container; and a control unit that is configured to control the first heating unit based on the temperature of the liquid raw material measured by the first temperature sensor, and to control the second heating unit based on the temperature measured by the second temperature sensor.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a gasification device, a substrate processing device, a cleaning method and a method for manufacturing a semiconductor device. Background Art

[0002] In recent years, with the miniaturization and high density of semiconductor devices, high dielectric constant (High-k) oxide films have begun to be used as gate insulating films. In addition, in order to increase the capacitance of DRAM capacitors, high dielectric constant oxide films have also begun to be used as capacitor insulating films. These high dielectric constant oxide films require film formation at low temperatures, and also require a film formation method with excellent surface flatness, concave filling, step coverage and less foreign matter. Regarding the control of foreign matter, a method of removing the film accumulated on the inner wall of the reaction tube (inside the processing chamber) by gas cleaning without disassembling the reaction tube is generally adopted recently (for example, Patent Document 1).

[0003] Prior art literature

[0004] Patent Literature

[0005] Patent Document 1: International Publication No. 2009 / 037991 Summary of the invention

[0006] Problems to be solved by the invention

[0007] In some cases, a gas obtained by heating a container storing a liquid raw material to vaporize the liquid raw material is used. In this case, if the supply valve to the reaction tube is opened to start supplying the gas, the vaporization amount increases, the vaporization heat is taken away from the liquid raw material, and the liquid temperature decreases, resulting in a decrease in the vaporization amount. That is, when the gas supply is started, the temperature of the liquid raw material decreases due to the vaporization heat, the vaporization amount changes, and the gas supply to the reaction tube cannot be stable.

[0008] An object of the present invention is to provide a technology capable of stabilizing the supply flow rate of a vaporization gas.

[0009] Means for solving problems

[0010] According to one embodiment of the present invention, the following technology is provided, which has:

[0011] A liquid container for storing liquid raw materials;

[0012] a first heating unit immersed in the liquid raw material stored in the liquid container and heating the liquid raw material;

[0013] a second heating unit for heating the liquid container;

[0014] a first temperature sensor immersed in the liquid raw material stored in the liquid container and measuring the temperature of the liquid raw material;

[0015] a second temperature sensor for measuring the temperature of the liquid container; and

[0016] The control unit is configured to control the first heating unit based on the temperature of the liquid raw material measured by the first temperature sensor, and to control the second heating unit based on the temperature measured by the second temperature sensor.

[0017] Effects of the Invention

[0018] It is possible to provide a technology capable of stabilizing the supply flow rate of the vaporization gas. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a schematic diagram of the structure of a vertical processing furnace of a substrate processing apparatus preferably used in one embodiment of the present invention, and shows a processing furnace portion in a vertical cross-sectional view.

[0020] Figure 2 1 is a schematic diagram of a vertical processing furnace of a substrate processing device preferably used in one embodiment of the present invention. Figure 1 The AA line cross-sectional view shows a portion of the processing furnace.

[0021] Figure 3 This is a schematic configuration diagram of a controller of a substrate processing apparatus preferably used in one embodiment of the present invention, and is a diagram showing a control system of the controller in the form of a block diagram.

[0022] Figure 4 This is a schematic diagram of the configuration of a vaporization device included in a substrate processing apparatus preferably used in one embodiment of the present invention.

[0023] Figure 5 This is a diagram showing an example of the set temperature of the heater of the vaporizer in one embodiment of the present invention.

[0024] Figure 6 This is a diagram showing the stability of the liquid temperature of the liquid container in one embodiment of the present invention.

[0025] Figure 7 This is a film formation timing chart when film formation is performed on a wafer according to one embodiment of the present invention.

[0026] Figure 8 It is a schematic configuration diagram of a gasification device in a modified example.

[0027] Description of Reference Numerals

[0028] 10…Substrate processing device

[0029] 60…Gasification device

[0030] 121…Controller (control unit)

[0031] 200…Wafer (substrate)

[0032] 201…Processing Room

[0033] 600…Liquid container

[0034] 610…Internal heater (first heating section)

[0035] 620…External heater (second heating unit)

[0036] 630…1st temperature sensor

[0037] 640…2nd temperature sensor DETAILED DESCRIPTION

[0038] <One embodiment of the present invention>

[0039] Below, refer to Figure 1 to Figure 6 A substrate processing apparatus according to an embodiment of the present invention will be described.

[0040] (1) Composition of treatment furnace

[0041] The processing furnace 202 included in the substrate processing apparatus 10 has a heater 207 as a heating unit (heating mechanism, heating system). The heater 207 has a cylindrical shape and is vertically installed by being supported by a heater base.

[0042] A reaction tube 203 constituting a reaction container (processing container) is arranged concentrically with the heater 207 on the inner side of the heater 207. The reaction tube 203 is made of a heat-resistant material (such as quartz (SiO2), silicon carbide (SiC), etc.) and is formed into a cylindrical shape with a closed upper end and an open lower end. A manifold (inlet flange) 209 is arranged concentrically with the reaction tube 203 below the reaction tube 203. The manifold 209 is made of a metal such as stainless steel (SUS) and is formed into a cylindrical shape with an upper end and a lower end open. An O-ring 220a as a sealing member is provided between the upper end of the manifold 209 and the reaction tube 203. By supporting the manifold 209 on the heater base, the reaction tube 203 is vertically installed. A processing chamber 201 for processing a substrate is formed in the hollow portion of the tube of the processing container.

[0043] The processing chamber 201 is configured to accommodate wafers 200 as substrates in a horizontal posture and arranged in a plurality of stages in the vertical direction using a wafer boat 217 to be described later.

[0044] The nozzles 410, 420, and 430 are installed in the processing chamber 201 so as to penetrate the side wall of the manifold 209. The nozzles 410, 420, and 430 are connected to the gas supply pipes 310, 320, and 330, respectively.

[0045] Mass flow controllers (MFCs) 512, 522, 523 as flow controllers (flow control units) and valves 314, 324, 334 as opening and closing valves are provided in order from the upstream side on the gas supply pipes 310, 320, 330. Gas supply pipes 510, 520, 530 for supplying inert gas are connected to the gas supply pipes 310, 320, 330 on the downstream side of the valves 314, 324, 334. MFCs 512, 522, 523 as flow controllers (flow control units) and valves 514, 524, 534 as opening and closing valves are provided in order from the upstream side on the gas supply pipes 510, 520, 530.

[0046] The nozzles 410, 420, and 430 are configured as L-shaped nozzles, and the horizontal portions thereof are provided so as to penetrate the side wall of the manifold 209. The vertical portions of the nozzles 410, 420, and 430 are provided in an annular space formed between the inner wall of the reaction tube 203 and the wafer 200 so as to stand upright (above the arrangement direction of the wafers 200) along the inner wall of the reaction tube 203 (i.e., stand upright from one end side of the wafer arrangement region toward the other end side). That is, the nozzles 410, 420, and 430 are provided in a region horizontally surrounding the wafer arrangement region on the side of the wafer arrangement region where the wafers 200 are arranged so as to stand upright along the wafer arrangement region.

[0047] Gas supply ports 410a, 420a, 430a for supplying gas are arranged on the side of the nozzles 410, 420, 430 in a manner corresponding to the substrate arrangement area where the wafers 200 are arranged along the arrangement direction of the wafers 200. The gas supply ports 410a, 420a, 430a are opened toward the center of the reaction tube 203. The gas supply ports 410a, 420a, 430a are provided in plurality in the range from the bottom to the top of the reaction tube 203, each having the same opening area and arranged at the same opening interval. It should be noted that the gas supply ports 410a, 420a, 430a are not limited to the above-mentioned manner. For example, the opening area may be gradually increased from the bottom to the top of the reaction tube 203. Thus, the flow rate of the gas supplied from the gas supply ports 410a, 420a, 430a can be made uniform.

[0048] As a processing gas, a raw material gas is supplied from a gas supply pipe 310 to the processing chamber 201 via MFC 312, valve 314, and nozzle 410. As the raw material gas, for example, a metal-containing gas containing aluminum (Al) as a metal element, that is, trimethylaluminum (Al(CH3)3, abbreviated as: TMA) as an aluminum-containing raw material (Al-containing raw material gas, Al-containing gas) is used. TMA is an organic raw material, which is an alkyl aluminum with an alkyl group bonded to Al as a ligand.

[0049] The raw material gas is a raw material in a gaseous state, for example, a gas raw material in a gaseous state at normal temperature and pressure, a gas obtained by gasifying a liquid raw material in a liquid state at normal temperature and pressure, or the like.

[0050] When a raw material gas that self-decomposes at a predetermined temperature is supplied from the gas supply pipe 310, the raw material gas supply system is mainly composed of the gas supply pipe 310, the MFC 312 and the valve 314. It is also conceivable that the nozzle 410 is included in the raw material gas supply system. The raw material gas supply system can also be referred to as a raw material supply system. When a metal-containing gas is supplied from the gas supply pipe 310, the raw material gas supply system can also be referred to as a metal-containing gas supply system.

[0051] When an Al-containing raw material (Al-containing raw material gas, Al-containing gas) is used as the metal-containing gas, the metal-containing gas supply system can also be referred to as an Al-containing raw material (Al-containing raw material gas, Al-containing gas) supply system. When TMA is used as the Al-containing raw material, the Al-containing raw material supply system can also be referred to as a TMA supply system.

[0052] When the reaction gas (reactant) is supplied from the gas supply pipe 320, the reaction gas supply system (reactant supply system) is mainly composed of the gas supply pipe 320, the MFC 322, and the valve 324. It is also possible to consider including the nozzle 420 in the reaction gas supply system. When an oxygen-containing gas (oxidizing gas, oxidant) is supplied as the reaction gas, the reaction gas supply system can also be called an oxygen-containing gas (oxidizing gas, oxidant) supply system. When O3 is used as the oxygen-containing gas, the oxygen-containing gas supply system can also be called an O3 supply system. When the reaction gas is allowed to flow in from the nozzle 420, the nozzle 420 can also be called a reaction gas nozzle.

[0053] As a processing gas, a cleaning gas (etching gas) is supplied from a gas supply pipe 330 into the processing chamber 201 via an MFC 332, a valve 334, and a nozzle 430. As the cleaning gas, for example, one or more gases selected from the group consisting of hydrogen chloride (HCl), silicon tetrachloride (SiCl4), thionyl chloride (SOCl2), boron tribromide (BBr3), silicon tetrabromide (SiBr4), and bromine (Br2) are used.

[0054] In addition, when the inert gas is supplied from the gas supply pipes 510 , 520 , 530 to the processing chamber 201 via the MFCs 512 , 522 , 532 , the valves 514 , 524 , 534 , and the nozzles 410 , 420 , 430 , for example, N 2 gas is used.

[0055] The inert gas supply system is mainly composed of the gas supply pipes 510 , 520 , 530 , the MFCs 512 , 522 , 532 , and the valves 514 , 524 , 534 .

[0056] On the other hand, one end of an exhaust pipe 231 as an exhaust flow path for exhausting the atmosphere of the processing chamber 201 is connected to the wall surface of the manifold 209. A pressure sensor 245 as a pressure detector (pressure detection unit) for detecting the pressure of the processing chamber 201 and an APC (Auto Pressure Controller) valve 243 as an exhaust valve (pressure regulating unit) are installed on the exhaust pipe 231, and a vacuum pump 246 as a vacuum exhaust device is installed at the end of the exhaust pipe 231.

[0057] The APC valve 243 is a valve configured in such a manner that the processing chamber 201 can be vacuum-exhausted and vacuum-exhausted stopped by opening and closing the valve while the vacuum pump 246 is in operation, and the pressure of the processing chamber 201 can be adjusted by adjusting the valve opening based on the pressure information detected by the pressure sensor 245 while the vacuum pump 246 is in operation. The exhaust system is mainly composed of the exhaust pipe 231, the APC valve 243, and the pressure sensor 245. It is also conceivable to include the vacuum pump 246 in the exhaust system. The exhaust pipe 231 is not limited to the case where it is provided on the reaction tube 203, and can also be provided on the manifold 209 like the nozzles 410, 420, and 430.

[0058] A sealing cover 219 as a furnace port cover that can hermetically seal the lower end opening of the manifold 209 is provided below the manifold 209. The sealing cover 219 is formed of a metal such as SUS and is formed in a disc shape. An O-ring 220 as a sealing member that abuts against the lower end of the manifold 209 is provided on the upper surface of the sealing cover 219. A rotating mechanism 267 that rotates a wafer boat 217 described later is provided on the side of the processing chamber 201 opposite to the sealing cover 219. The rotating shaft 255 of the rotating mechanism 267 passes through the sealing cover 219 and is connected to the wafer boat 217.

[0059] The sealing cover 219 is configured to be able to be raised and lowered in the vertical direction by a wafer boat elevator 115 as an elevating mechanism vertically provided outside the reaction tube 203. The wafer boat elevator 115 is configured to be able to carry the wafer boat 217 into and out of the processing chamber 201 by raising and lowering the sealing cover 219. The wafer boat elevator 115 is configured as a transport device (transport mechanism) that transports the wafer boat 217, i.e., the wafer 200 into and out of the processing chamber 201.

[0060] The wafer boat 217 as a substrate support is configured to support a plurality of wafers 200, for example, 25 to 200 wafers 200, in a horizontal posture and in a state where the centers are aligned with each other in a vertical direction and in multiple stages, that is, arranged at intervals. A top plate 215 is provided on the top of the wafer boat 217. The wafer boat 217 and the top plate 215 are made of a heat-resistant material such as quartz or SiC. A heat insulation plate 218 made of a heat-resistant material such as quartz or SiC is supported in a horizontal posture in multiple stages in a heat insulation area at the bottom of the wafer boat 217.

[0061] In addition, if Figure 2 As shown, a temperature sensor 263 as a temperature detector is arranged in the processing chamber 201. The temperature of the processing chamber 201 is set to a desired temperature distribution by adjusting the power supply to the heater 207 based on the temperature information detected by the temperature sensor 263. The temperature sensor 263 is provided along the inner wall of the reaction tube 203 in the same manner as the nozzles 410 and 420.

[0062] like Figure 3 As shown, the controller 121 as a control unit (control mechanism) is configured in the form of a computer having a CPU (Central Processing Unit) 121a, a RAM (Random Access Memory) 121b, a storage device 121c, and an I / O port 121d. The RAM 121b, the storage device 121c, and the I / O port 121d are configured to be able to exchange data with the CPU 121a via an internal bus. The controller 121 is connected to an input / output device 122 such as a touch panel.

[0063] The storage device 121c is composed of, for example, a flash memory, an HDD (Hard Disk Drive), etc. A control program for controlling the temperature of a liquid raw material, a control program for controlling the operation of a substrate processing device, a process recipe recording the steps, conditions, etc. of a method for manufacturing a semiconductor device described later, etc., is stored in a readable manner in the storage device 121c. The process recipe is a combination of methods that enable the controller 121 to execute each process (step) in the method for manufacturing a semiconductor device described later and obtain a specified result, and functions as a program. Hereinafter, the process recipe, control program, etc. are also referred to as programs. When the term program is used in this specification, it includes a case where only a process recipe alone is included, a case where only a control program alone is included, or a case where a combination of a process recipe and a control program is included. RAM121b is configured as a memory area (work area) that temporarily holds programs, data, etc. read by CPU121a.

[0064] The I / O port 121d is connected to at least any one of the above-mentioned MFC312, 322, 332, 512, 522, 532, valves 314, 324, 334, 344, 514, 524, 534, pressure sensor 245, APC valve 243, vacuum pump 246, heater 207, temperature sensor 263, rotating mechanism 267, wafer boat elevator 115, internal heater 610, external heater 620, first temperature sensor 630, second temperature sensor 640, etc.

[0065] It should be noted that the control unit (not shown) for controlling the internal heater 610 and the external heater 620 may be independently configured from the controller 121 for controlling the substrate processing apparatus 10, wherein the internal heater 610 and the external heater 620 are provided in the liquid container 600 of the vaporization apparatus 60 described later. In the case of an independent configuration, the control unit (not shown) for controlling the internal heater 610 and the external heater 620 may be configured to be connected to the controller 121 for controlling the substrate processing apparatus 10.

[0066] The control unit (not shown) that controls the internal heater 610 and the external heater 620 may be connected to at least one of the first temperature sensor 630 , the second temperature sensor 640 , the internal heater 610 , and the external heater 620 .

[0067] The CPU 121 a is configured to read a control program from the storage device 121 c and execute the control program, and to read a recipe from the storage device 121 c in response to input of an operation command from the input / output device 122 or the like. CPU 121a is configured to control, according to the contents of the read process, the flow rate regulation actions of various gases performed by MFC 312, 322, 332, 512, 522, 532, the opening and closing actions of valves 314, 324, 334, 514, 524, 534, the opening and closing actions of APC valve 243 and the pressure regulation actions of APC valve 243 based on pressure sensor 245, the temperature regulation actions of heater 207 based on temperature sensor 263, the starting and stopping of vacuum pump 246, the rotation and rotation speed regulation actions of wafer boat 217 performed by rotating mechanism 267, the lifting and lowering actions of wafer boat 217 performed by wafer boat elevator 115, the storage actions of wafer 200 into wafer boat 217, the temperature regulation actions of liquid raw materials by internal heater 610 based on first temperature sensor 630 and external heater 620 based on second temperature sensor 640, etc.

[0068] The controller 121 can be constructed by installing the above-mentioned program stored in an external storage device (for example, a magnetic disk such as a magnetic tape, a floppy disk, a hard disk, an optical disk such as a CD, a DVD, an optical magnetic disk such as an MO, a USB memory, a semiconductor memory such as a memory card) 123 into a computer. The storage device 121c and the external storage device 123 are configured as a computer-readable recording medium. Hereinafter, they are also referred to as recording media. In this specification, the recording medium may include only a storage device 121c monomer, only an external storage device 123 monomer, or both. It should be noted that the provision of the program to the computer may also be carried out without using the external storage device 123 and using communication means such as the Internet and dedicated lines.

[0069] (2) Composition of the gasification device

[0070] Next, use Figure 4 A gasification device for storing a liquid raw material and generating a process gas by gasifying the liquid raw material is described.

[0071] like Figure 4As shown, the liquid container 600 is provided with a gas supply pipe 330 (which supplies, for example, a cleaning gas as a processing gas into the processing chamber 201) and a gas supply pipe 650 for supplying a liquid raw material of the cleaning gas into the liquid container 600. As the liquid raw material of the cleaning gas, for example, SiCl4 liquid is stored in the liquid container 600, and the cleaning gas vaporized by vapor draw enters the gas supply pipe 330 and is supplied to the processing chamber 201 via the gas supply pipe 330, MFC332, and valve 334. Thus, the film attached to the processing chamber 201 is etched, and the processing chamber 201 is cleaned. The liquid container 600 is cylindrical and the cross-sectional area inside the container is the same, and its material is a metal material such as SUS.

[0072] In addition, the liquid container 600 is provided with: an internal heater 610 as a first heating device (first heating unit) which is immersed in the liquid raw material and heats the liquid raw material; a first temperature sensor 630 (for example, a thermocouple) which is immersed in the liquid raw material to control the internal heater 610 and measures the temperature of the liquid raw material; and a second temperature sensor 640 (for example, a thermocouple) which measures the temperature of the outer wall of the liquid container 600 to control the external heater 620 described later. The internal heater 610 is connected to a power source (not shown) and the temperature of the internal heater 610 is adjusted by feedback control such as PID based on the measured temperature obtained by the first temperature sensor 630 so that the measured temperature obtained by the first temperature sensor 630 (that is, the measured temperature of the liquid raw material) reaches a predetermined temperature. It should be noted that the second temperature sensor 640 can be provided in the heat insulating cloth of the external heater 620 or can be provided in direct contact with the outer wall of the liquid container 600.

[0073] The liquid container 600 is covered by an external heater (e.g., a sleeve heater) 620 as a second heating device (a second heating unit) for heating the liquid container 600 and the liquid raw material therein. The external heater 620 is connected to a power source, etc. (not shown), and the temperature of the external heater 620 is adjusted based on the measured temperature obtained by the second temperature sensor 640 so that the measured temperature obtained by the second temperature sensor 640 (i.e., the measured temperature of the outer wall of the liquid container 600) reaches a predetermined temperature. Since the external heater 620 heats the liquid through the heat insulating cloth (not shown) of the external heater 620 and the liquid container 600, the liquid raw material is heated by heating the liquid in accordance with the temperature sensor 640. Figure 5 By performing temperature control in the manner shown in FIG. 1 so as to achieve a temperature (second temperature) higher than the temperature (first temperature) of the internal heater 610, stable liquid temperature control can be achieved. Figure 5In the figure, "RT" is the room temperature. For example, when the electric power of the internal heater 610 is controlled so that the temperature measured by the first temperature sensor 630 (TCin) reaches 100°C, the electric power of the external heater 620 can be controlled so that the temperature measured by the second temperature sensor 640 (J / H TC) reaches about 102°C.

[0074] An example of the operation of the vaporization device 60 is described. When the cleaning gas is supplied from the liquid container 600 to the processing chamber 201 via the supply pipe 330, the MFC 332, the valve 334, and the nozzle 430, the temperature of the liquid raw material in the liquid container 600 is measured using the first temperature sensor 630, and the temperature of the outer wall of the liquid container 600 heated by the external heater 620 is measured using the second temperature sensor 640. It should be noted that the temperature of the liquid raw material at this time is in a state of rapid temperature drop due to the heat of vaporization. The temperature (supply power) of the internal heater 610 is adjusted based on the temperature of the liquid raw material measured by the first temperature sensor 630 so that the temperature of the liquid raw material reaches a predetermined temperature, and the temperature (supply power) of the external heater 620 is adjusted based on the temperature of the outer wall of the liquid container 600 measured by the second temperature sensor 640 so that the temperature of the outer wall of the liquid container 600 reaches a predetermined temperature. Therefore, by heating the liquid raw material with the internal heater 610 and the external heater 620, the temperature drop of the liquid raw material, which drops sharply after the start of the clean gas supply, can be suppressed, and the temperature can be raised to a predetermined temperature in a short time. In addition, by suppressing the drop in the temperature of the liquid raw material, the overshoot amount of the temperature of the liquid raw material caused by heating can be suppressed. For example, Figure 6 The time (t) from the start of liquid vaporization supply (A) to the stable recovery of the liquid temperature (set temperature ±1%) (B) is shortened from the conventional 60 minutes to within 5 minutes.

[0075] By adopting such a configuration to independently control the internal heater 610 and the external heater 620, the responsiveness and stability of the liquid temperature of the liquid raw material become good, and the liquid raw material can be restored to a predetermined temperature range in a short time. In addition, since the liquid raw material can be raised to a predetermined temperature in a short time, it is possible to prevent the saturated vapor pressure from decreasing due to the temperature drop of the liquid raw material caused by the heat of vaporization when the cleaning gas is supplied, and the vapor pressure required for the liquid raw material can be ensured, thereby preventing the flow rate of the cleaning gas from decreasing.

[0076] According to the vaporization device of this embodiment, the cross-sectional area of ​​the liquid container 600 is set to A (cm 2), the generated gas flow rate (supply gas flow rate) is set to Q (slm), for example, A = 250 (cm 2 ) when the temperature of the liquid raw material is heated to 100°C, a gas flow rate of 6 (slm) or more can be stably supplied. That is, Q / A ≥ 2.4 (%), as shown in the region of Q / A>2 (%), even under the condition that the temperature drop of the liquid raw material at the start of gasification is large, a stable supply of the gasification gas can be achieved. Specifically, even when the first temperature and the second temperature are set to the specified values ​​that satisfy Q / A>2 (%), a stable supply of the gasification gas can be achieved. The gasification device of this embodiment can also be applied in the region of Q / A≤2 (%), but since the temperature drop of the liquid raw material at the start of gasification is small, the gasification device of this embodiment is suitable for application in the region of Q / A>2 (%).

[0077] The vaporization temperature depends on the desired amount of vaporization. The higher the vaporization temperature, the greater the amount of vaporization. It should be noted that if the vaporization temperature is too high, thermal decomposition of the raw material will occur, so it is desirable that the vaporization temperature is lower than the temperature at which thermal decomposition of the raw material occurs. In the case of film-forming raw material gas, such a large flow rate (more than 5 slm) is usually not required, but in the case of clean raw material gas, in order to increase the pressure rise rate in the furnace, that is, in order to increase the concentration of the clean raw material gas to increase the etching amount in each cycle, it is required to supply it at a large flow rate. Therefore, the gasification device of the present invention that can supply a large flow rate of gasification gas of more than 5 slm can be more suitable for the supply of clean raw material gas.

[0078] In addition, although the vaporization device is described as a vaporization device for cleaning gas, it can also be used as a vaporization device for raw material gas or reaction gas as a process gas other than the cleaning gas.

[0079] (3) Substrate processing step

[0080] Next, as one of the steps of manufacturing the semiconductor device (device) of this embodiment, an example of a method of forming a film on a substrate using the above-mentioned substrate processing apparatus 10 to manufacture a semiconductor device (device) is described. In the following description, the operations of the various components constituting the substrate processing apparatus 10 are controlled by the controller 121.

[0081] It should be noted that the term "wafer" is used in this specification to mean "the wafer itself" or "a stack (assembly) of a wafer and predetermined layers, films, etc. formed on its surface" (i.e., a wafer is referred to as a wafer when the predetermined layers, films, etc. formed on the surface are included). In addition, the term "surface of the wafer" is used in this specification to mean "the surface (exposed surface) of the wafer itself" or "the surface of the predetermined layers, films, etc. formed on the wafer, i.e., the outermost surface of the wafer as a stack". It should be noted that the term "substrate" is used in this specification to mean the same as the term "wafer".

[0082] use Figure 7 The sequence of forming a film on a wafer 200 using the substrate processing apparatus 10 is described. In this embodiment, a processing chamber 201 in which a plurality of wafers 200 are stored in a stacked state is heated at a predetermined temperature. In addition, the following steps are performed a predetermined number of times (n times): a raw material gas supply step of supplying TMA gas from the gas supply port 410a of the nozzle 410 to the processing chamber 201 as a raw material gas; and a reactive gas supply step of supplying a reactive gas from the gas supply port 420a of the nozzle 420. Thus, an aluminum oxide film (AlO film) is formed on the wafer 200 as a film containing Al and O.

[0083] (Wafer loading)

[0084] The plurality of wafers 200 are loaded into the processing chamber 201 (wafer boat loading). Specifically, after the plurality of wafers 200 are loaded on the wafer boat 217 (wafer filling), as shown in FIG. Figure 1 As shown, the boat 217 supporting the plurality of wafers 200 is lifted by the boat elevator 115 and carried into the processing chamber 201. In this state, the seal cap 219 is in a state of closing the lower end opening of the manifold 209 via the O-ring 220.

[0085] (Pressure regulation and temperature regulation)

[0086] The vacuum pump 246 is used to perform vacuum exhaust so that the desired pressure (vacuum degree) is achieved in the processing chamber 201. At this time, the pressure in the processing chamber 201 is measured by the pressure sensor 245, and the APC valve 243 is feedback-controlled (pressure regulated) based on the measured pressure information. The vacuum pump 246 is always kept in an operating state at least until the processing of the wafer 200 is completed. In addition, the heater 207 is used to heat so that the processing chamber 201 reaches the desired temperature. At this time, the amount of power supplied to the heater 207 is feedback-controlled based on the temperature information detected by the temperature sensor 263 so that the processing chamber 201 has the desired temperature distribution (temperature regulation). The heating of the processing chamber 201 by the heater 207 is continued at least until the processing of the wafer 200 is completed.

[0087] Furthermore, the wafer boat 217 and the wafers 200 are rotated by the rotation mechanism 267. The rotation of the wafer boat 217 and the wafers 200 by the rotation mechanism 267 is continuously performed at least until the processing of the wafers 200 is completed.

[0088] (Film Forming Process)

[0089] Thereafter, the raw material gas supply step (first gas supply step), the residual gas removal step, the reaction gas supply step (second gas supply step), and the residual gas removal step are sequentially performed a predetermined number of times.

[0090] (Raw material gas supply step)

[0091] The valve 314 is opened to allow the raw material gas (TMA gas) to flow into the gas supply pipe 310. The TMA gas is flow-regulated by the MFC 312 and supplied from the gas supply port 410a of the nozzle 410 to the processing chamber 201. At the same time, the valve 514 is opened to allow the carrier gas (N2 gas) as an inert gas to flow into the gas supply pipe 510. The carrier gas is flow-regulated by the MFC 512 and supplied from the supply port 410a of the nozzle 410 to the processing chamber 201 together with the raw material gas, and is exhausted from the exhaust pipe 231. In addition, in order to prevent the raw material gas from intruding into the nozzle 420 (to prevent backflow), the valve 524 is opened to allow the carrier gas to flow into the gas supply pipe 520. The carrier gas is supplied to the processing chamber 201 via the gas supply pipe 520 and the nozzle 420, and is exhausted from the exhaust pipe 231.

[0092] At this time, the APC valve 243 is appropriately adjusted to set the pressure of the processing chamber 201 to a pressure in the range of, for example, 1 to 1000 Pa, preferably 1 to 100 Pa, and more preferably 10 to 50 Pa.

[0093] The supply flow rate of the TMA gas controlled by MFC312 is set to, for example, a flow rate in the range of 10 to 2000 sccm, preferably 50 to 1000 sccm, and more preferably 100 to 500 sccm. It should be noted that in this specification, when a numerical range is recorded as, for example, 10 to 2000 sccm, it means more than 10 sccm and less than 2000 sccm. That is, the numerical range includes 10 sccm and 2000 sccm. Not only the flow rate, but all the numerical values ​​recorded in this specification such as pressure, time, and temperature are the same.

[0094] The supply flow rate of the carrier gas controlled by the MFC 512 is set to be, for example, within the range of 1 to 30 slm. The supply time of the source gas to the wafer 200 is set to be, for example, within the range of 1 to 60 seconds, preferably 1 to 20 seconds, and more preferably 2 to 15 seconds.

[0095] The heater 207 heats the wafer 200 so that the temperature thereof is within a range of, for example, 200 to 600° C., preferably 350 to 550° C., and more preferably 400 to 550° C.

[0096] TMA gas is supplied to the processing chamber 201 under the above conditions, thereby forming an Al-containing layer on the outermost surface of the wafer 200. The Al-containing layer may contain C and H in addition to Al. The Al-containing layer is formed by physically adsorbing TMA on the outermost surface of the wafer 200, chemically adsorbing a substance obtained by decomposing a part of TMA, or accumulating Al by thermally decomposing TMA. That is, the Al-containing layer may be TMA, an adsorption layer obtained by decomposing a part of TMA (physical adsorption layer, chemical adsorption layer), or an Al accumulation layer (Al layer).

[0097] (Residual gas removal step)

[0098] After the Al-containing layer is formed, the valve 314 is closed to stop the supply of TMA gas. At this time, the APC valve 243 is kept open, and the processing chamber 201 is evacuated by the vacuum pump 246 to remove the raw material gas remaining in the processing chamber 201 that has not reacted or participated in the formation of the Al-containing layer from the processing chamber 201. The supply of carrier gas to the processing chamber 201 is maintained while the valves 514 and 524 are opened.

[0099] (Reaction Gas Supply Step)

[0100] After the residual gas in the processing chamber 201 is removed, the valve 324 is opened to allow the reaction gas (O3 gas) to flow into the gas supply pipe 320. The reaction gas is flow-regulated by the MFC 322, supplied from the supply hole 420a of the nozzle 420 to the wafer 200 in the processing chamber 201, and exhausted from the exhaust pipe 231. That is, the wafer 200 is exposed to the reaction gas.

[0101] At this time, the valve 524 is opened to allow the carrier gas to flow into the gas supply pipe 520. The carrier gas is flow-regulated by the MFC 522, and is supplied to the processing chamber 201 together with the reaction gas, and is exhausted from the exhaust pipe 231. At this time, in order to prevent the reaction gas from invading the nozzle 410 (to prevent backflow), the valve 514 is opened to allow the carrier gas to flow into the gas supply pipe 510. The carrier gas is supplied to the processing chamber 201 via the gas supply pipe 510 and the nozzle 410, and is exhausted from the exhaust pipe 231.

[0102] At this time, the APC valve 243 is appropriately adjusted to set the pressure of the processing chamber 201 to a pressure in the range of, for example, 1 to 1000 Pa. The supply flow rate of the reaction gas controlled by the MFC 322 is set to a flow rate in the range of, for example, 5 to 40 slm, preferably 5 to 30 slm, and more preferably 10 to 20 slm. The time for supplying the reaction gas to the wafer 200 is set to, for example, 1 to 60 seconds. The other processing conditions are set to the same processing conditions as those in the aforementioned raw material gas supply step.

[0103] At this time, the gas flowing into the processing chamber 201 is only the reaction gas and the inactive gas (N2 gas). The reaction gas reacts with at least a portion of the Al-containing layer formed on the wafer 200 in the raw material gas supply process. The Al-containing layer is oxidized to form an aluminum oxide layer (AlO layer) containing Al and O as a metal oxide layer. That is, the Al-containing layer is modified into an AlO layer.

[0104] (Residual gas removal step)

[0105] After the AlO layer is formed, the valve 324 is closed to stop the supply of the reaction gas. In addition, the reaction gas and reaction by-products remaining in the processing chamber 201 that have not reacted or participated in the formation of the AlO layer are removed from the processing chamber 201 through the same processing step as the residual gas removal step after the raw material gas supply step.

[0106] The above-described raw gas supply step, residual gas removal step, reaction gas supply step, and residual gas removal step are cycled a predetermined number of times (one or more) in sequence. In this way, an AlO film is formed on the wafer 200 by performing batch processing (performing multiple steps multiple times).

[0107] It should be noted that the batch process is a process of forming an AlO film on the wafer 200 by performing a predetermined number of cycles of a raw material gas supply step, a residual gas removal step, a reaction gas supply step, and a residual gas removal step in sequence. Furthermore, the AlO film is formed on the wafer 200 in one batch.

[0108] (Post-purge and atmospheric pressure recovery)

[0109] Inert gas such as N2 gas is supplied to the processing chamber 201 from the gas supply pipes 510, 520, and 530, respectively, and exhausted from the exhaust pipe 231. The N2 gas acts as a purge gas, whereby the processing chamber 201 is purged with the inert gas, and the gas and by-products remaining in the processing chamber 201 are removed from the processing chamber 201 (post-purge). Thereafter, the atmosphere in the processing chamber 201 is replaced with the inert gas (inert gas replacement), and the pressure in the processing chamber 201 is restored to normal pressure (atmospheric pressure restoration).

[0110] (Wafer removal)

[0111] Thereafter, the sealing cover 219 is lowered by the wafer boat elevator 115, and the lower end of the manifold 209 is opened. Then, the processed wafers 200 are carried out from the lower end of the reaction tube 203 to the outside of the reaction tube 203 while being supported by the wafer boat 217 (wafer boat unloading). Thereafter, the processed wafers 200 are taken out of the wafer boat 217 (wafer taking out).

[0112] Next, a process (cleaning process) of etching a film adhering to the inside of the processing chamber 201 and the like will be described.

[0113] (Jingzhou moved in)

[0114] The wafer boat 217 is loaded into the processing chamber 201 (wafer boat loading) without loading the wafer 200. The wafer boat 217 is lifted by the boat elevator 115 and loaded into the processing chamber 201. In this state, the seal cap 219 closes the lower end opening of the manifold 209 via the O-ring 220.

[0115] (Pressure regulation and temperature regulation)

[0116] The vacuum pump 246 is used to perform vacuum exhaust so that the desired pressure (vacuum degree) is reached in the processing chamber 201. At this time, the pressure in the processing chamber 201 is measured by the pressure sensor 245, and the APC valve 243 is feedback-controlled (pressure regulated) based on the measured pressure information. The vacuum pump 246 is always kept in a working state at least until the processing of the wafer 200 is completed. In addition, the heater 207 is used to heat so that the processing chamber 201 reaches the desired temperature. At this time, the amount of power supplied to the heater 207 is feedback-controlled based on the temperature information detected by the temperature sensor 263 so that the processing chamber 201 has the desired temperature distribution (temperature regulation). The heating of the processing chamber 201 by the heater 207 is continued at least until the etching process is completed.

[0117] (Etching (cleaning) process)

[0118] A step of etching a film attached to the inside of the processing chamber 201 and the like to clean the inside of the processing chamber 201 is performed.

[0119] (Etching Step)

[0120] For example, in a volume of 4L (cross-sectional area 250cm 2 ) in a liquid container 600, by heating the liquid raw material SiCl4 to 100°C, a vaporized gas of SiCl4 is obtained. The valve 334 is opened, and the SiCl4 gas is made to flow from the liquid container 600 into the gas supply pipe 330 as a cleaning gas (etching gas) obtained by vaporization. The SiCl4 gas is flow-regulated by the MFC332, supplied from the gas supply port 430a of the nozzle 430 into the processing chamber 201, and exhausted from the exhaust pipe 231. At the same time, the valve 534 is opened, and an inactive gas such as N2 gas is made to flow into the gas supply pipe 530. The N2 gas flowing into the gas supply pipe 530 is flow-regulated by the MFC532, supplied into the processing chamber 201 together with the SiCl4 gas, and exhausted from the exhaust pipe 231. It should be noted that at this time, in order to prevent the SiCl4 gas from invading the nozzles 410 and 420, the valves 514 and 524 are opened, and the N2 gas is made to flow into the gas supply pipes 510 and 520. N 2 gas is supplied into the processing chamber 201 through the gas supply pipes 310 , 320 and the nozzles 410 , 420 , and is exhausted from the exhaust pipe 231 .

[0121] By supplying the SiCl 4 gas, at least a portion of the AlO film attached to the processing chamber 201 reacts with the SiCl 4 gas and is removed from the processing chamber 201 .

[0122] At this time, the heater 207 is controlled by the controller 121 to heat the processing chamber 201 to a predetermined temperature within the range of, for example, 200 to 800° C., preferably 400 to 650° C., so as to activate the SiCl4 gas. At this time, the APC valve 243 is closed or substantially closed to a degree that does not affect the processing, and the SiCl4 gas is sealed in the processing chamber 201. By sealing the SiCl4 gas, the influence of the above-mentioned reaction delay on the etching can be reduced. In addition, the pressure in the processing chamber 201 is maintained at the first pressure, for example, a predetermined pressure within the range of 1 to 40,000 Pa, preferably 10,000 to 30,000 Pa, and more preferably 20,000 to 30,000 Pa. The supply flow rate of the SiCl4 gas controlled by the MFC332 is set to a flow rate within the range of, for example, 1 to 10 slm, preferably 3 to 8 slm. The time for supplying the SiCl4 gas to the processing chamber 201 (the SiCl4 gas supply time) is set to, for example, a time within the range of 60 to 600 seconds.

[0123] (Residual gas removal step)

[0124] After the SiCl4 gas is supplied to the processing chamber 201 for a predetermined time, the valve 334 is closed to stop the supply of the SiCl4 gas. The APC valve 243 is closed, or the APC valve 243 is opened when it is substantially closed to a degree that does not affect the processing. In addition, the SiCl4 gas remaining in the processing chamber 201 that has not reacted or participated in the removal of the AlO layer is discharged from the processing chamber 201 through the same processing step as the residual gas removal step of the TMA gas supply step.

[0125] (Surface oxidation step)

[0126] The valve 324 is opened to allow the O3 gas to flow into the gas supply pipe 320. The O3 gas is flow-regulated by the MFC 322, supplied from the gas supply port 420a of the nozzle 420 into the processing chamber 201, and exhausted from the exhaust pipe 231. At the same time, the valve 524 is opened to allow an inactive gas such as N2 gas to flow into the gas supply pipe 520. The N2 gas flowing into the gas supply pipe 520 is flow-regulated by the MFC 522, supplied into the processing chamber 201 together with the O3 gas, and exhausted from the exhaust pipe 231. It should be noted that at this time, in order to prevent the O3 gas from invading the nozzles 410 and 430, the valves 514 and 534 are opened to allow the N2 gas to flow into the gas supply pipes 510 and 530. The N2 gas is supplied to the processing chamber 201 via the gas supply pipes 310 and 330 and the nozzles 410 and 430, and exhausted from the exhaust pipe 231.

[0127] When the O3 gas is flowed in, the APC valve 243 is appropriately adjusted to set the pressure in the processing chamber 201 to a pressure in the range of, for example, 50 to 1330 Pa. The supply flow rate of the O3 gas controlled by the MFCs 235b and 235c is set to a flow rate in the range of, for example, 5 to 40 slm. The supply time (irradiation time) of the O3 gas is set to a time in the range of, for example, 10 to 600 seconds. At this time, the temperature of the heater 207 is set to the same temperature as in step S101.

[0128] By supplying O3 gas, the surface of the inner wall of the processing chamber 201, the wafer boat 217, etc. is oxidized (treated). In addition, the by-products generated in the etching step are reoxidized. For example, the Al-Cl bond of AlClx is cut, removed in the form of Cl2, and reoxidized to AlO. In addition, the organic matter remaining in the AlO film reacts with the O3 gas and is removed from the processing chamber 201. For example, the carbon (C) remaining in the AlO film reacts with the O3 gas to become COx, which is removed from the processing chamber 201. At this time, there are carbon defects on the outermost surface of the film after COx is detached, and there is a weak bond equilibrium state of Al-O and Al-Al. This state is considered to be a surface equilibrium state suitable for etching.

[0129] (Residual gas removal step)

[0130] After the O3 gas is supplied for a predetermined time, the valve 324 is closed to stop the supply of the O3 gas. In addition, the unreacted O3 gas or the O3 gas reacted with the AlO film remaining in the processing chamber 201 is removed from the processing chamber 201 by the same processing step as the residual gas removal step of the TMA gas supply step.

[0131] (Specified number of implementations)

[0132] The cycle of sequentially performing the above steps is performed once or more (predetermined number of times (m times)), thereby removing the AlO film attached to the processing chamber 201. Preferably, the above cycle is repeated a plurality of times.

[0133] As described above, in the etching (cleaning) process, a cycle including an etching step performed by a cleaning gas and a surface oxidation step performed by an O3 gas is repeated multiple times. Since the gasification start / stop is repeated in each cycle, the liquid temperature of the liquid raw material is prone to frequent changes, and therefore, the temperature control of the present invention with a high temperature recovery speed is more suitable.

[0134] According to the present embodiment, one or more of the following effects are achieved.

[0135] (1) By providing two heaters, namely an internal heater controlled based on the temperature of the liquid raw material (liquid temperature) and an external heater controlled based on the temperature of the liquid container, when a liquid temperature change occurs accompanying vaporization, the recovery time until the liquid temperature stabilizes at a specified temperature or within a specified temperature range can be shortened.

[0136] (2) The internal heater is controlled so that the temperature measured by the first temperature sensor reaches a predetermined first temperature, and the external heater is controlled so that the temperature measured by the second temperature sensor reaches a predetermined second temperature. The second temperature is set to a preset value corresponding to the first temperature. Thus, the liquid temperature control can be performed more stably than when the first temperature and the second temperature are set to the same value.

[0137] [Modifications]

[0138] use Figure 8 A gasification device according to a modified example will be described.

[0139] The liquid container 600 of the modified example is provided with: an internal heater 610 as a first heating device (first heating part) which is immersed in the liquid raw material and heats the liquid raw material; a first temperature sensor 630 which is immersed in the liquid raw material to control the internal heater 610 and measures the temperature of the liquid raw material; and a second temperature sensor 640 which measures the temperature of the outer wall of the liquid container 600 to control the external heater 620. The internal heater 610 is composed of a first internal heater 610a and a second internal heater 610b. The first temperature sensor 630 is composed of a first internal sensor 630a and a second internal sensor 630b. The number of each of the internal heater 610 and the first temperature sensor 630 is not limited to two, and may be three or more. The first internal heater 610a is controlled independently of the second internal heater 610b based on the temperature measured by the first internal sensor 630a so that the temperature measured by the first internal sensor 630a reaches a predetermined first temperature. Furthermore, the second internal heater 610b is controlled independently of the first internal heater 610a based on the temperature measured by the second internal sensor 630b so that the temperature measured by the second internal sensor 630b reaches a predetermined first temperature.

[0140] When the temperature measured by at least one of the first internal sensor 630a and the second internal sensor 630b exceeds the third temperature (upper limit temperature) specified, the controller 121 stops the power supply to the first internal heater 610a and the second internal heater 610b. Thus, when an abnormal value exceeding the upper limit value is measured, abnormal heating can be prevented by stopping the heating. Even when a sensor abnormality or a heater abnormality occurs, temperature stability and safety can be ensured.

[0141] In the above embodiment, an AlO film is exemplified as the high dielectric constant oxide film to be etched, but the invention is not limited thereto. For example, when ZrOy, HfOy, HfSixOy, HfAlxOy, ZrSiOy, ZrAlOy, TixOy, or TaxOy (x and y are integers or decimals greater than 0) is used as the high dielectric constant oxide, the invention can be applied in the same manner. That is, the invention can also be applied to a zirconium oxide film, a hafnium oxide film, a titanium oxide film, a tantalum oxide film, and composite films thereof.

[0142] In addition, in the above-mentioned embodiment, TMA is exemplified as an organic raw material, but it is not limited thereto. If it is an organic compound, other raw materials may also be applied. For example, organic Hf raw materials such as tetrakis(ethylmethylamino)hafnium (Hf[N(CH3)CH2CH3]4, TEMAH) and other organic Al raw materials, organic Si raw materials such as tris(dimethylamino)silane (SiH(N(CH3)2)3, TDMAS), organic Ti raw materials such as tetrakis(dimethylamino)titanium (Ti[N(CH3)2]4, TDMAT), organic Ta raw materials such as penta(dimethylamino)tantalum (Ta(N(CH3)2)5, PDMAT) and the like may also be applied.

[0143] In addition, in the above embodiment, an example of using O3 gas in the film forming process is shown, but it is not limited to this, and other materials can also be used as long as it is an oxygen-containing gas. For example, O2, O2 plasma, H2O, H2O2, N2O, etc. can also be used.

[0144] In the above embodiment, an example is shown in which a liquid raw material of a cleaning gas is stored in the liquid container 600 and vaporized by a vapor draw method without using a carrier gas. However, the present invention can also be applied to a bubbling method using a carrier gas.

[0145] In addition, in the above embodiment, O3 is exemplified as the oxidizing gas used in the surface oxidation step, but the present invention is not limited thereto, and other gases may be used as long as they are oxygen-containing gases and gases containing elements that react with the halogen elements contained in the etching gas. For example, H2O, H2O2, etc. may also be used.

[0146] The process (a program recording the processing steps, processing conditions, etc.) used in the formation of the above-mentioned various thin films is preferably prepared separately (preparing multiple) corresponding to the contents of substrate processing, cleaning processing, etc. (film type, composition ratio, film quality, film thickness, processing steps, processing conditions, etc. of the formed thin film). In addition, when starting substrate processing, cleaning processing, etc., it is preferred to appropriately select an appropriate process, cleaning process, etc. from multiple process, cleaning processes, etc. corresponding to the contents of substrate processing, cleaning processing, etc. Specifically, it is preferred that multiple process, cleaning processes, etc. prepared separately corresponding to the contents of substrate processing, cleaning processing, etc. are pre-stored (installed) in the storage device 121c of the substrate processing device via an electrical communication line and a recording medium (external storage device 123) recording the process, cleaning process, etc. In addition, it is preferred that when starting substrate processing, the CPU 121a of the substrate processing device appropriately selects an appropriate process, cleaning process, etc. from multiple process, cleaning processes, etc. stored in the storage device 121c according to the contents of substrate processing. By configuring in this way, thin films of various film types, composition ratios, film qualities, and film thicknesses can be formed universally and reproducibly by one substrate processing apparatus. In addition, the operator's operating burden (the burden of inputting processing steps, processing conditions, etc.) can be reduced, and substrate processing can be started quickly while avoiding operating errors.

[0147] In addition, the present invention can also be implemented by, for example, changing the process, cleaning process, etc. of an existing substrate processing device. When the process, cleaning process, etc. are changed, the process, cleaning process, etc. of the present invention can be installed in the existing substrate processing device via an electrical communication line or a recording medium recording the process, cleaning process, etc., or the input and output device of the existing substrate processing device can be operated to change the process, cleaning process, etc. of the present invention to the process, cleaning process, etc. of the present invention.

Claims

1. A gasification device, comprising: A liquid container for storing liquid raw materials; a first heating unit immersed in the liquid raw material stored in the liquid container and heating the liquid raw material; a second heating unit for heating the liquid container; a first temperature sensor immersed in the liquid raw material stored in the liquid container and measuring the temperature of the liquid raw material; a second temperature sensor for measuring the temperature of the liquid container; as well as A control unit configured to control the first heating unit based on the temperature of the liquid raw material measured by the first temperature sensor in such a manner that the temperature measured by the first temperature sensor reaches a prescribed first temperature, and to control the second heating unit based on the temperature of the liquid container measured by the second temperature sensor in such a manner that the temperature measured by the second temperature sensor reaches a prescribed second temperature, wherein the second temperature is higher than the first temperature.

2. The gasification device according to claim 1, wherein: The second temperature is set to a preset value corresponding to the first temperature.

3. The gasification device according to claim 1, wherein: The cross-sectional area of ​​the liquid container is Acm 2 , set the generated gas flow rate to Qslm, and set the first temperature and the second temperature so that Q / A>2%.

4. The gasification device according to claim 1, wherein: The first heating unit is composed of at least a first internal heater and a second internal heater, and the first temperature sensor is composed of at least a first internal sensor and a second internal sensor.

5. The gasification device according to claim 4, wherein: The control unit is configured to control the first internal heater based on the temperature measured by the first internal sensor, and to control the second internal heater based on the temperature measured by the second internal sensor.

6. The gasification device according to claim 4 or 5, wherein: The control unit is configured to control the first internal heater and the second internal heater so that the temperature measured by the first internal sensor and the second internal sensor reaches a predetermined first temperature.

7. The gasification device according to claim 4 or 5, wherein: The control unit is configured to stop supplying power to the first internal heater and the second internal heater when a temperature measured by at least one of the first internal sensor and the second internal sensor exceeds a predetermined third temperature.

8. The gasification device according to claim 1, wherein: The liquid stored in the liquid container is a liquid raw material of the cleaning gas.

9. A substrate processing device comprising a processing chamber, a gasification device, a gas supply system and a control unit, The processing chamber processes the substrate; The gasification device comprises: A liquid container storing liquid raw materials, a first heating unit immersed in the liquid raw material stored in the liquid container and heating the liquid raw material; a second heating unit for heating the liquid container, a first temperature sensor immersed in the liquid raw material stored in the liquid container and measuring the temperature of the liquid raw material; and a second temperature sensor for measuring the temperature of the liquid container; The gas supply system supplies the gas obtained by gasifying the liquid raw material by the gasification device to the processing chamber; The control unit is configured to control the first heating unit based on the temperature of the liquid raw material measured by the first temperature sensor in such a manner that the temperature measured by the first temperature sensor reaches a prescribed first temperature, and to control the second heating unit based on the temperature of the liquid container measured by the second temperature sensor in such a manner that the temperature measured by the second temperature sensor reaches a prescribed second temperature, wherein the second temperature is higher than the first temperature.

10. The substrate processing apparatus according to claim 9, wherein: The control unit is configured to be able to control the gas supply system so as to perform a plurality of cycles of supplying and stopping the gas obtained by vaporizing the liquid raw material by the vaporization device.

11. A cleaning method, wherein a gasification device is used, wherein the gasification device has: A liquid container for storing liquid raw materials; a first heating unit immersed in the liquid raw material stored in the liquid container and heating the liquid raw material; a second heating unit for heating the liquid container; a first temperature sensor immersed in the liquid raw material stored in the liquid container and measuring the temperature of the liquid raw material; as well as a second temperature sensor for measuring the temperature of the liquid container, The cleaning method comprises the following steps: A step of controlling the first heating unit based on the temperature of the liquid raw material measured by the first temperature sensor so that the temperature measured by the first temperature sensor reaches a predetermined first temperature, and controlling the second heating unit based on the temperature of the liquid container measured by the second temperature sensor so that the temperature measured by the second temperature sensor reaches a predetermined second temperature, the second temperature being higher than the first temperature, thereby vaporizing the liquid raw material; and A step of supplying a gas obtained by vaporizing the liquid raw material into a processing chamber in which a substrate is processed, thereby cleaning the processing chamber.

12. The cleaning method according to claim 11, wherein: In the cleaning step, a cycle of supplying and stopping the vaporization gas is performed a plurality of times.

13. A method for manufacturing a semiconductor device, comprising the following steps: The process of loading the substrate into the processing chamber; Processing the substrate in the processing chamber; A process of using a vaporizing device to control a first heating unit based on the temperature of a liquid raw material measured by a first temperature sensor so that the temperature measured by the first temperature sensor reaches a predetermined first temperature, and to control a second heating unit based on the temperature of a liquid container measured by a second temperature sensor so that the temperature measured by the second temperature sensor reaches a predetermined second temperature, wherein the second temperature is higher than the first temperature, thereby vaporizing the liquid raw material, wherein the vaporizing device comprises: a liquid container that stores the liquid raw material; the first heating unit that is immersed in the liquid raw material stored in the liquid container and heats the liquid raw material; a second heating unit that heats the liquid container; a first temperature sensor that is immersed in the liquid raw material stored in the liquid container and measures the temperature of the liquid raw material; and a second temperature sensor that measures the temperature of the liquid container; and A step of supplying a gas obtained by vaporizing the liquid raw material into the processing chamber to clean the interior of the processing chamber.

14. The method for manufacturing a semiconductor device according to claim 13, wherein: In the cleaning step, a cycle of supplying and stopping the vaporization gas is performed a plurality of times.