Semiconductor light receiving element
By using a doped semiconductor layer in the semiconductor light-receiving element and adjusting the contact mode of the metal electrode, the problems of manufacturing difficulty and increased contact resistance caused by the reduced width of the ring electrode are solved, and higher sensitivity and speed performance are achieved.
Patent Information
- Application Number
- CN202080027577.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-04-09
- Filing Date
- 2020-04-07
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2040-04-07
AI Technical Summary
It is difficult to balance the improvement of light sensitivity and working speed of existing semiconductor light-receiving elements. In particular, the reduced width of the ring electrode leads to a reduction in manufacturing process margin and an increase in contact resistance, making it difficult to achieve high-speed and high-sensitivity operation.
Use a semiconductor layer doped with the first impurity and the second impurity to adjust the band gap energy of the light absorption layer, and make contact with the side of the metal electrode and the doped semiconductor layer to ensure that the side of the electrode is parallel to the growth direction, increasing the manufacturing process margin and reduce contact resistance.
It is possible to increase the working speed without sacrificing the light-receiving sensitivity, increase the process margin and reduce the contact resistance, and improve the high-speed and high-sensitivity performance of the semiconductor light-receiving element.
Smart Images

Figure CN113678266B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a semiconductor light-receiving element (photodiode (PD)), and more particularly to a semiconductor light-receiving element having a higher speed and a higher sensitivity. Background Art
[0002] Semiconductor photodetectors convert incident optical signals into electrical signals and are widely used in optical receivers in optical communications and optical mixers for millimeter-wave oscillators.
[0003] The performance of semiconductor photodetectors is often discussed in terms of light sensitivity and operating speed. This is because the sensitivity and operating speed of semiconductor photodetectors are basically in a trade-off relationship. When designing semiconductor photodetectors, the sensitivity and operating speed are optimized according to their intended use.
[0004] The sensitivity and operating speed of a semiconductor light-receiving element are in a trade-off relationship, which is mainly related to the thickness of the light-absorbing layer and the operating area.
[0005] Regarding the thickness of the light absorbing layer, the greater the thickness, the longer the distance (optical path length) that the signal light passes through the light absorbing layer when the signal light enters the semiconductor light receiving element. On the other hand, the electrons and holes (carriers) generated in the light absorbing layer need to travel a longer distance before reaching the electrode. Therefore, the greater the thickness of the light absorbing layer, the higher the light sensitivity, but the lower the operating speed.
[0006] On the other hand, regarding the working area, the larger the working area, the easier it is for the incident light to be optically coupled in the semiconductor photosensitive element. The general technology is: when the signal light is incident on the semiconductor photosensitive element, a lens is used to focus the incident light, so that lossless optical coupling is achieved as much as possible even for semiconductor photosensitive elements with a small working area. However, in actual applications, even with a lens, the spot size of the incident light can only be reduced to about 10μm. The light signal irradiated outside the working surface is not converted into an electrical signal, so it becomes a loss from the perspective of light receiving sensitivity, causing a decrease in sensitivity. On the other hand, from the perspective of operating speed, the smaller the working area, the lower the capacity of the element. Therefore, the speed limit based on the RC time constant is relaxed, and the semiconductor photosensitive element can operate at a higher speed.
[0007] As mentioned above, in order to realize a semiconductor light-receiving element with high light-receiving sensitivity and high-speed operation, the following design is required: lengthening the optical path length of the signal light in the element, and maximizing the area for receiving signal light while reducing the working area. Figure 1 As shown in FIG. 1 , a light receiving element including, for example, an electrode 106 and a reflector 105 having a ring shape when viewed from above, on an upper portion of the element has been proposed (Non-Patent Document 1).
[0008] exist Figure 1 The structure of the semiconductor light-receiving element 100 shown has a layer structure in which a contact layer 102 containing p-type InP, a light-absorbing layer 103 containing undoped InGaAs (indium gallium arsenic), and a contact layer 104 containing n-type InP are stacked in this order on an InP (indium phosphide) substrate 101. In addition, the semiconductor light-receiving element 100 has the following multi-level mesa structure: the uppermost contact layer 104 containing n-type InP is processed into the smallest mesa, and then, in the order of the light-absorbing layer 103 containing undoped InGaAs and the contact layer 102 containing p-type InP, the outer shape gradually increases in stages. A reflector 105 and a ring-shaped electrode 106 are formed on the upper part of the n-type contact layer 104, and an electrode 106 is formed on the side of the reflector 105. Figure 1 In the structure of the semiconductor light receiving element 100 shown, the signal light is incident from the back side of the InP substrate 101 of the semiconductor light receiving element 100 and is reflected by the reflector 105 on the upper part of the element. Therefore, the signal light reciprocates in the light absorbing layer 103 (2-pass structure), thereby increasing the optical path length and improving the light receiving sensitivity. On the other hand, the ring-shaped electrode 106 (upper electrode) for extracting current is formed into a ring shape surrounding the reflector 105.
[0009] The ring-shaped electrode 106 is typically formed of a stacked structure of Ti (lower layer) / Pt (middle layer) / Au (upper layer) from the viewpoint of ohmic contact with the contact layer 102, heat resistance, and adhesion. On the other hand, the reflector 105 is formed of Au to increase reflectivity.
[0010] Prior art literature
[0011] Non-patent literature
[0012] Non-patent literature 1: E. Yagyu et al., “Recent advances in AlInAs Avalanche Photodiodes,” in Proc. OFC 2007, OThG 2. Summary of the invention
[0013] Problems to be solved by the invention
[0014] exist Figure 1 In the case where incident light is irradiated to the annular electrode 106 , the reflectivity of the contact layer 104 including the semiconductor and the metal of the annular electrode is lower than that of the reflector 105 , so the light receiving sensitivity is reduced compared to the case where the light is reflected by the mirror portion.
[0015] Therefore, in a semiconductor light-receiving element having a certain working area, in order to maximize the light-receiving area, the electrode width of the ring electrode must be reduced. However, in order to reduce the width of the ring-shaped electrode 106, the process margin of photolithography in the element manufacturing process must be reduced, and manufacturing becomes difficult in practical applications. In addition, there is the following problem: since the contact area between the ring-shaped electrode (metal electrode) 106 and the semiconductor contact layer 104 also becomes smaller, the contact resistance increases, and according to the limitation based on the RC time constant, it is impossible to foresee the expected degree of increase in the working speed.
[0016] In addition, as described in the background technology, in a vertically incident semiconductor light-receiving element, increasing its light-receiving area is necessary to improve the sensitivity as a light receiver. Therefore, the electrode on the upper part of the element adopts a ring-shaped electrode shape. However, there are the following problems: when the element diameter is reduced for high speed, the width of the ring needs to be reduced, and it becomes difficult to ensure the process margin. In addition, the contact resistance increases, resulting in difficulty in high-speed and high-sensitivity operation.
[0017] Solutions for solving problems
[0018] In view of the above problems in the prior art, the present invention increases the margin of the manufacturing process in the semiconductor light-receiving element, thereby achieving high-speed operation without sacrificing the light-receiving sensitivity.
[0019] One embodiment of the semiconductor light-receiving element of the present invention comprises: a semiconductor layer doped with a first impurity; a semiconductor light-absorbing layer, on the semiconductor layer doped with the first impurity, adjusting the band gap energy by absorbing incident light; a semiconductor layer doped with a second impurity, on the semiconductor light-absorbing layer; and a metal electrode, in contact with the side surface of the semiconductor layer doped with the second impurity, wherein the semiconductor light-receiving element is characterized in that the side surface of the metal electrode is a surface parallel to the growth direction of the semiconductor layer doped with the second impurity. It should be noted that when the first impurity is a P-type impurity, the second impurity is an n-type impurity; when the first impurity is an n-type impurity, the second impurity is a P-type impurity.
[0020] Effects of the Invention
[0021] The present invention has the effect of increasing the margin of the manufacturing process and achieving high-speed operation without sacrificing light sensitivity. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 A diagram showing a conventional semiconductor light-receiving element.
[0023] Figure 2 A diagram showing a semiconductor light-receiving element according to a first embodiment of the present invention.
[0024] Figure 3 It is a figure which shows the manufacturing process of the semiconductor light-receiving element which concerns on 1st Embodiment of this invention.
[0025] Figure 4 It is a figure which shows the manufacturing process of the semiconductor light-receiving element which concerns on 1st Embodiment of this invention.
[0026] Figure 5 It is a figure which shows the manufacturing process of the semiconductor light-receiving element which concerns on 1st Embodiment of this invention.
[0027] Figure 6 A diagram showing a semiconductor light-receiving element according to a second embodiment of the present invention.
[0028] Figure 7 A diagram showing a semiconductor light-receiving element according to a third embodiment of the present invention. DETAILED DESCRIPTION
[0029] The semiconductor light-receiving element of the embodiment of the present invention is described in detail below using the accompanying drawings. However, it should be understood by those skilled in the art that the present invention is not limited to the contents of the embodiments shown below, and various changes can be made to the scheme and details without departing from the purpose of the invention disclosed in this specification, etc. It should be noted that in the structure of the invention described below, the same symbol is used for the same part or the part with the same function, and its repeated description is sometimes omitted.
[0030] [First embodiment]
[0031] A first embodiment of the present invention will be described. This embodiment is a basic embodiment of the present invention.
[0032] Figure 2 This is a cross-sectional view of a semiconductor light-receiving element 200 for explaining the first embodiment. In this embodiment, the semiconductor light-receiving element 200 has a layer structure in which a contact layer 202 containing p-type InP, a light-absorbing layer 203 containing undoped InGaAs, and a contact layer 204 containing n-type InP are stacked in this order on an InP substrate 201. In addition, the semiconductor light-receiving element 200 has a multi-level mesa structure as follows: the uppermost contact layer 204 containing n-type InP is processed into the smallest mesa, and then, in the order of the light-absorbing layer 203 containing undoped InGaAs and the contact layer 202 containing p-type InP, the outer shape gradually increases.
[0033] A reflective mirror film 205 is formed on the upper portion of the n-type contact layer 204 , and a metal electrode 206 is formed on the side surface of the n-type contact layer to be in electrical contact with the side surface of the contact layer 204 containing n-type InP.
[0034] That is, the light-receiving element of the first embodiment comprises: a contact layer 202 (a semiconductor layer doped with impurities in a manner to become P-type), a light-absorbing layer 203 on the contact layer 202 (a semiconductor light-absorbing layer that adjusts the band gap energy by absorbing incident light), a contact layer 204 on the light-absorbing layer 203 (a semiconductor layer doped with impurities in a manner to become N-type), and a metal electrode 206 connected to the side surface of the contact layer 204. The semiconductor light-receiving element is characterized in that the side surface of the metal electrode 206 is a surface parallel to the growth direction of the contact layer 204.
[0035] The working principle of the light receiving element in this embodiment is described. After the electrons generated by excitation in the light absorption layer 203 containing undoped InGaAs reach the n-type contact layer 204, they move to the metal electrode 206 as majority carriers. Here, in the case where the mirror film 205 is formed of metal, the electrons can also move to the mirror film 205 containing metal. However, in general, the mirror film 205 requires a low reflectivity at the semiconductor / mirror interface, and there is no need to make special efforts to reduce the contact resistance at the interface. Even if it is assumed that the impedance of the mirror / semiconductor interface becomes larger, it is sufficient as long as the contact resistance at the semiconductor / metal electrode can be reduced.
[0036] The manufacturing method of this embodiment is described. Figure 3 As shown, first, a contact layer 202 containing p-type InP, a light absorbing layer 203 containing undoped InGaAs, and a contact layer 204 containing n-type InP are epitaxially grown in this order on a semi-insulating InP substrate 201 using the MOCVD method (metal organic chemical vapor deposition method). After crystal growth, the n-type contact layer 204 becomes the smallest terrace, and then, in the order of the light absorbing layer 203 containing undoped InGaAs and the contact layer 202 containing p-type InP, photolithography and etching are performed in sequence. Next, as shown in FIG. Figure 3 As shown in FIG. 1 , a mirror film 205 containing metal having the same size as the n-type contact layer 204 is formed by sputtering using a photoresist 307 formed by photolithography. Figure 4As shown, the photoresist is peeled off to form an annular gap with the n-type contact layer 204 as the center and the outer periphery of the n-type contact layer 204 as its inner diameter, and the photoresist 407 is patterned again by photolithography. At this time, the pattern is formed in a manner such that the outer diameter of the annular gap is about 3 to 5 μm larger than the n-type contact layer 204, and the metal electrode 206 is formed in the annular gap portion by evaporation. If the metal electrode 206 is a layer structure of Ti / Pt / Au, for example, it is possible to reduce the contact resistance and ensure a high adhesion strength with the semiconductor. In addition, in the formation of the metal electrode, if the evaporation is performed while the wafer is rotating, the metal can be formed more uniformly on the side of the n-type contact layer 204.
[0037] Furthermore, the mirror film 205 and the metal electrode 206 shown in this embodiment will not destroy the intended characteristics even if they are in contact. This is because the electrons generated in the semiconductor light-receiving element 200 can be taken out to the external circuit from the contact layer 204 containing n-type InP via the metal electrode 206 and then via the mirror film 205 and the metal electrode 206, and if the mirror and the electrode are made of metal, their impedance is smaller than that of the semiconductor, so they will not affect the impedance of the semiconductor light-receiving element 200 as a whole.
[0038] In this case, if Figure 5 As shown, it is not necessary to form an annular gap by photoresist, and the electrode 506 can be formed by patterning the photoresist 507 to form a circular gap centered on the n-type contact layer 204. In the case of this shape, the process margin of the photolithography process can be further increased compared to the photoresist pattern forming the annular gap.
[0039] For example, consider a semiconductor light-receiving element having a circular mesa shape with an n-type contact layer 204 having a diameter of 10 μm. Figure 1 When the width of the annular electrode 106 is 2 μm, the diameter of the mirror formed is 6 μm, and the effective light receiving diameter is only 6 μm. On the other hand, in the semiconductor light receiving element shown in this embodiment, a light receiving diameter of 10 μm can be obtained.
[0040] As described above, according to the semiconductor light receiving element of this embodiment, even if the mesa diameter of the light receiving element is reduced for speed increase, a larger light receiving diameter can be obtained, and a high-speed and high-sensitivity light receiving element can be realized while increasing the process margin.
[0041] In the semiconductor light receiving element 200 of the embodiment 1, the ring-shaped electrode (metal electrode) 206 is electrically contacted with the side surface of the n-type contact layer 204 , thereby forming the metal electrode without reducing the area of the upper surface of the mirror film 205 .
[0042] It should be noted that an electrode (not shown) for electrical connection is provided at the end of the P-type contact layer 202 in contact with the light absorbing layer 203 .
[0043] [Second Embodiment]
[0044] Figure 6 The cross-sectional structure diagram of the semiconductor light-receiving element 600 of the second embodiment is illustrated. This embodiment has the following structure: In the first embodiment, the semiconductor layer (light-absorbing layer 203 containing InGaAs) adjacent to the contact layer 204 containing n-type InP and the metal electrode 206 in contact with the contact layer 204 containing n-type InP are isolated by the insulating film 607. The semiconductor light-receiving element 600 of the second embodiment is characterized in that the metal electrode 206 and the light-absorbing layer 203 containing InGaAs are not in contact with each other on a surface perpendicular to the growth direction, and the metal electrode 206 is in contact with the contact layer (semiconductor layer) 204 containing n-type InP on a surface parallel to the growth direction.
[0045] Here, in the second embodiment, an insulating film 607 using SiO2 is deposited on the upper surface of the light absorption layer 203 containing InGaAs which is a layer adjacent to the contact layer 204 containing n-type InP, and the expansion of the parasitic capacitance in the metal electrode accompanied by the thickness is suppressed by isolating the InGaAs light absorption layer 203 and the metal electrode 206 in contact with the contact layer 204 containing n-type InP.
[0046] As a method for manufacturing a semiconductor light-receiving element of this embodiment, after forming a mesa of an n-type contact layer 204 by the same process as that shown in Embodiment 1, an insulating film such as SiO2 is formed on the entire surface of a wafer by sputtering. Thereafter, photolithography is performed in such a manner that a portion other than the mesa formed by the contact layer 204 containing n-type InP is covered with a resist, and the insulating film is dry-etched in this pattern to form an insulating film 607. Thereafter, a mirror film 205 containing a metal and a metal electrode 206 may be formed in the same manner as in Embodiment 1.
[0047] As described above, according to this embodiment, even if the mesa diameter of the light receiving element is reduced for speed increase, a larger light receiving diameter can be obtained, and a high-speed and high-sensitivity light receiving element can be realized while increasing the process margin.
[0048] [Third Embodiment]
[0049] like Figure 7As shown, the third embodiment is a semiconductor light receiving element 700, in which an insulating film 707 is further formed between the mirror film 205 composed of metal and the contact layer 204 containing n-type InP as a semiconductor contact layer in the structure shown in the second embodiment. The semiconductor light receiving element 700 of the third embodiment has a structure in which the mirror film 205 containing metal and the contact layer (semiconductor layer) 204 in contact with the metal electrode 206 are not in contact.
[0050] The insulating film 707 may be, for example, silicon nitride SiN. Silicon nitride SiN has good adhesion to both semiconductors and metals without sacrificing optical properties. Although the electrical contact from the contact layer 204 containing a mesa-shaped semiconductor to the mirror film 205 containing a metal is lost, the electrons in the semiconductor light-receiving element 700 are taken out via the metal electrode 206 in contact with the side of the contact layer 204 containing n-type InP, as in the previous embodiments.
[0051] In addition, in this embodiment, the film thickness of the contact layer 204 containing n-type InP, which contacts the metal electrode 206 on the surface horizontal to the growth direction of the semiconductor, is set to 0.3μm. This is to increase the contact area with the metal electrode 206 and reduce the contact resistance. Of course, the thicker the film thickness of the contact layer 204 containing n-type InP, the more effective it is to reduce the contact resistance, but in reality, setting it too thick sometimes destroys the crystal quality of the epitaxial layer. If it is a light-receiving element with an operating frequency band of about 50GHz, as long as the film thickness of the contact layer 204 is at least about 0.3μm, it will not cause a serious process effect of contact resistance.
[0052] Figure 7 2 shows an example of a semiconductor light receiving element 700 having an insulating film 707 and an insulating film 607 as insulating films, but a semiconductor light receiving element having an insulating film 707 as an insulating film and a light absorbing layer 203 in contact with a metal electrode 206 can also be realized.
[0053] As described above, according to this embodiment, even if the mesa diameter of the light receiving element is reduced for speed increase, a larger light receiving diameter can be obtained, and a high-speed and high-sensitivity light receiving element can be realized while increasing the process margin.
[0054] In the first to third embodiments, circular mesa-shaped and ring-shaped electrodes are used as examples for explanation, but the embodiments of the present invention are of course not limited to the shape of the mesa of the semiconductor or the shape of the metal electrode. For example, the shape of the mesa may be a quadrilateral. In addition, as an electrode shape, even if it is formed on a part or multiple parts of the side of the mesa, the generality of the present invention is not lost.
[0055] Furthermore, in the embodiment of the present invention, metal electrodes are formed on surfaces parallel to the growth direction for all the contact layers of the n-type semiconductors, but it is obvious that the contact layers of the p-type semiconductors can also have the same electrode structure.
[0056] Industrial Applicability
[0057] The present invention can be applied to the technical field related to semiconductor light-receiving elements (photodiodes).
[0058] Description of reference numerals:
[0059] 100, 200, 600, 700: semiconductor light receiving element
[0060] 101, 201: InP substrate
[0061] 102, 202: Contact layer
[0062] 103, 203: Light absorption layer
[0063] 104, 204: Contact layer
[0064] 105: Reflector
[0065] 205: Mirror film
[0066] 106: Ring-shaped electrode
[0067] 206: Metal Electrode
[0068] 307, 407, 507: Photoresist
[0069] 607, 707: Insulating film.
Claims
1. A semiconductor light receiving element, comprising: a semiconductor layer doped with a first impurity; a semiconductor light absorbing layer, on the semiconductor layer doped with the first impurity, adjusting the band gap energy by absorbing incident light; a semiconductor layer doped with a second impurity, on the semiconductor light absorbing layer; a mirror film, on the semiconductor layer doped with the second impurity, reflecting the incident light, the mirror film containing metal; as well as a metal electrode in contact with a side surface of the semiconductor layer doped with the second impurity, The semiconductor light-receiving element is characterized in that the side surface of the metal electrode is a surface parallel to the growth direction of the semiconductor layer doped with the second impurity.
2. The semiconductor light receiving element according to claim 1, wherein: The metal electrode in contact with the semiconductor layer doped with the second impurity in a plane parallel to the growth direction of the semiconductor layer doped with the second impurity does not contact with the semiconductor light absorbing layer in a plane perpendicular to the growth direction of the semiconductor layer doped with the second impurity.
3. The semiconductor light-receiving element according to claim 1 or 2, wherein: In the case where the first impurity is a p-type impurity and the second impurity is an n-type impurity, When the first impurity is an n-type impurity, the second impurity is a p-type impurity.
4. The semiconductor light receiving element according to claim 1, wherein: The metal electrode is in contact with the mirror film.
5. The semiconductor light receiving element according to claim 4, characterized in that: The mirror film containing metal is not in contact with the semiconductor layer in contact with the metal electrode.
6. The semiconductor light receiving element according to claim 1, wherein: An insulating layer is formed between the semiconductor light absorbing layer and the metal electrode.
7. The semiconductor light receiving element according to claim 4, characterized in that: An insulating layer is formed between the mirror film and the semiconductor layer doped with the second impurity and in contact with the metal electrode.
8. The semiconductor light receiving element according to claim 1, wherein: The metal electrode includes Ti, Pt and Au.
Citation Information
Patent Citations
Buried-waveguide-type light receiving element and manufacturing method thereof
CN101207162A
Avalanche photodiode used for communication and preparation method thereof
CN106098836A
Light receiving element and its manufacturing method
JP1993275732A
Semiconductor photodetector, its manufacturing method, and light receiving apparatus
JP2007335753A
Light receiving element, semiconductor epitaxial wafer, method for manufacturing the light receiving element, method for manufacturing the semiconductor epitaxial wafer, and detecting device
US20130248821A1