A preparation method and application of flexible pressure sensor
By using a combination of MWCNTs/PDMS electrode layer and BaTiO3/PDMS dielectric layer in a flexible pressure sensor, constructing a microstructure and combining it with a neural network model, the problem of insufficient sensitivity and stability in the existing technology is solved, and the detection of human movement is realized. Efficient recognition of status has application potential in human-computer interaction and health monitoring.
Patent Information
- Application Number
- CN202111156003.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-09-30
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2041-09-30
AI Technical Summary
Existing flexible pressure sensors have problems with insufficient sensitivity and stability in human body motion status recognition. In particular, they cannot effectively measure static pressure and are greatly affected by environmental factors, which affects the real-time detection effect.
A flexible capacitive pressure sensor based on MWCNTs/PDMS electrode layer and BaTiO3/PDMS dielectric layer is used. By constructing a microstructure and increasing the dielectric constant, a "sandwich" structure is designed and combined with a neural network model to identify human body motion status.
The sensitivity and response speed of the sensor are improved, and it can effectively monitor human physiological activity information, such as respiratory signals and joint movements, and realize the recognition of motion states such as sitting still, standing still, walking, and running. It has great potential in human-computer interaction and health monitoring. Huge application potential.
Smart Images

Figure CN113855004B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of human body motion state recognition, and in particular to a preparation method and application of a flexible pressure sensor. Background Art
[0002] Human motion state detection and recognition technology has been widely used in different fields such as medical treatment, human-computer interaction and home life. Current human motion detection research can usually be divided into two ways: one is human motion state recognition based on video and image processing technology, and the other is human motion state recognition based on wearable devices. With the rapid development of flexible electronic technology, the emergence of flexible sensors has provided a new idea for human motion state detection. Unlike traditional rigid sensors, flexible sensors can adapt to complex detection environments, and have the advantages of small size and light weight. They can well adapt to the requirements of human motion monitoring and will not cause great obstacles to human activities. Although there have been reports on the application of flexible sensors in the field of motion state recognition, the recognition effect is still limited by key factors such as sensor sensitivity and stability. Therefore, it is of certain significance and value to design a flexible sensor with superior performance that can be well applied to human motion state detection. There are many types of flexible pressure sensors, and their sensing mechanisms are mainly divided into three categories: piezoresistive, piezoelectric and capacitive. Due to its unique sensing principle, piezoelectric sensors have the advantages of high sensitivity and fast response speed, but they cannot effectively measure static pressure; piezoresistive sensors have the advantages of easy data collection, simple production, and stable performance, but the sensing material is easily affected by environmental factors, and piezoresistive sensors are greatly affected by the viscoelasticity of flexible materials, which easily produces large hysteresis, affecting the real-time detection effect; in comparison, capacitive sensors have low power consumption, high sensitivity, low hysteresis, fast response time, and good perception of tiny stresses, which can meet the actual needs of human motion detection. At present, the main way to improve the performance of capacitive sensors is to construct microstructures in the dielectric layer and electrode layer, and maximize the sensitivity of the capacitance change when the dielectric layer and electrode layer are compressed and deformed through the design of microstructures, and performance optimization can be sought from the combination of constructing microstructures in the electrode layer and improving the dielectric constant. Summary of the invention
[0003] In view of the above problems existing in the prior art, the present invention proposes a preparation method and application of a flexible pressure sensor, which has a reasonable design, overcomes the shortcomings of the prior art, and has good effects.
[0004] In order to achieve the above-mentioned invention objective 1, the present invention adopts the following technical solution:
[0005] A method for preparing a flexible pressure sensor comprises the following steps:
[0006] First, the MWCNTs solution is sprayed onto the surface of 80-grit sandpaper flat on a glass plate. After heating and drying, a layer of dry MWCNTs is deposited on the sandpaper surface. The PDMS solution is poured on the surface and evenly coated by spin coating. The PDMS solution penetrates into the MWCNTs layer due to gravity. After heating and curing, the PDMS solution solidifies to form a PDMS film. The PDMS film is peeled off to obtain a PDMS / MWCNTs electrode layer.
[0007] S2, preparing a sensor dielectric layer;
[0008] BaTiO3 accounts for 30% of the mass of BaTiO 3 The mixed solution of / PDMS was spin-coated on a smooth glass sheet. After the spin coating was completed, the sample was placed in a vacuum drying oven and heated at 70 °C for 3 h to form a solidified composite film. Finally, the composite film was peeled off from the surface of the smooth glass sheet to obtain BaTiO 3 / PDMS dielectric layer;
[0009] S3, packaging sensor;
[0010] The PDMS / MWCNTs electrode layer was cut into strips with a width of 1 cm and a length of 4 cm. 3 / PDMS dielectric layer is cut into squares of 1.5cm long and 1.5cm wide. The structure of the sensor adopts a "sandwich" structure. The upper and lower layers are electrode layers, and the middle layer is a dielectric layer. The three-layer structure is sealed and bonded using a single-sided adhesive PI film, and the flexible pressure sensor is completed.
[0011] Furthermore, in S1, the preparation method of the MWCNTs solution is: dispersing multi-walled carbon nanotubes with a purity of 95%, a length of 10-30m, and a carboxyl content of 2.0wt% in anhydrous ethanol, manually stirring for 10 minutes, and further dispersing the multi-walled carbon nanotubes using high-frequency ultrasound for 30 minutes to obtain a multi-walled carbon nanotube / ethanol dispersion with a mass fraction of 1wt%, keeping the dispersion solution still for 12 hours, removing the bottom precipitate, and retaining the supernatant, which is the MWCNTs solution.
[0012] Furthermore, in S1, the preparation method of the PDMS solution is: mixing the PDMS main agent and the curing agent in a ratio of 15:1 and stirring for 30 minutes, and then treating in a vacuum state for 30 minutes to remove bubbles in the solution.
[0013] Furthermore, in S1 and S2, the spin coating speed is 400 rpm and the spin coating time is 40 s.
[0014] Further, in S3, a PI film with a thickness of 50 um is selected.
[0015] In order to achieve the above-mentioned invention objective 2, the present invention adopts the following technical solution:
[0016] A method for identifying human motion state, using a flexible pressure sensor prepared by the preparation method described above, wherein three flexible pressure sensors are provided, and one end of a wire is fixed to the surface of an electrode layer using a copper foil conductive tape, and the other end of the wire is connected to the same circuit board, wherein the circuit board includes a capacitance acquisition module, a microcontroller module, a switch module, and a power supply module, and the microcontroller module transmits the collected sensor signal to a computer via Bluetooth;
[0017] The following steps are involved:
[0018] S1. Obtain original sample data;
[0019] Three flexible pressure sensors are fixed on the chest, elbow and knee joints of the human body respectively, and the collected breathing signals, elbow bending signals and knee bending signals are used as original sample data;
[0020] S2, denoising, sample division and feature extraction are performed on the original sample data to obtain a sample set;
[0021] The wavelet threshold denoising method is used to denoise the original sample data;
[0022] The feature extraction method is time domain feature extraction. The time domain features include maximum value, minimum value, average value, root mean square and variance. Each group of sample sets contains 15 feature parameters.
[0023] S3. Determine the structure of the neural network model, where the neural network model includes an input layer, a hidden layer, and an output layer;
[0024] S4, using the Levenberg-Marguardt algorithm to train the neural network model based on the sample set, when the mean square error reaches the optimum, the neural network model is determined as the final neural network model;
[0025] S5. Identify the human body's motion state based on the final neural network model.
[0026] Furthermore, in S3, the number of neuron nodes in the input layer is 15, and the 15-dimensional input vector constitutes 15 eigenvalues of a set of training data in sequence; the number of neuron nodes in the hidden layer is 7; the number of neuron nodes in the output layer is 1, and different motion states are represented by outputs 1, 2, 3, and 4, respectively, output 1 represents a sitting state, output 2 represents a standing state, output 3 represents a walking state, and output 4 represents a running state.
[0027] The present invention has the following beneficial effects:
[0028] The present invention designs a MWCNTs / PDMS electrode with microstructures embedded on the surface and BaTiO 3 / PDMS dielectric layer, effectively improving the sensitivity and response speed of the sensor, and determining the mass ratio of 30% BaTiO 3 / PDMS hybrid film can effectively improve the dielectric constant of the sensor;
[0029] The present invention designs a human motion state recognition method based on the flexible sensor, and uses a multi-layer recognition data model to realize the recognition of four motion states: sitting, standing, walking, and running. The sensor can effectively monitor human physiological activity information, such as breathing signals and jumping joint movements, and can play a huge role in the field of wearable motion detection. This method provides a new idea for the field of human motion recognition and has great application potential in human-computer interaction and health monitoring. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 This is a flow chart of electrode layer preparation in one embodiment of the present invention;
[0031] Figure 2 A flow chart of dielectric layer preparation in one embodiment of the present invention;
[0032] Figure 3 This is a schematic diagram of the structure of a flexible pressure sensor in an embodiment of the present invention;
[0033] Figure 4 A pressure-capacitance variation curve of a sensor in one embodiment of the present invention;
[0034] Figure 5 A graph showing a respiratory signal acquisition curve of a sensor in one embodiment of the present invention;
[0035] Figure 6 It is a curve graph of elbow joint bending acquisition by a sensor in one embodiment of the present invention;
[0036] Figure 7 A curve diagram of knee joint bending acquisition by a sensor in one embodiment of the present invention;
[0037] Figure 8 A flow chart of a method for identifying human motion in one embodiment of the present invention;
[0038] Fig. 9 This is a comparison diagram of the sensor signal before and after denoising in one embodiment of the present invention; DETAILED DESCRIPTION
[0039] The specific implementation of the present invention is further described below in conjunction with the accompanying drawings and specific embodiments:
[0040] A method for preparing a flexible pressure sensor comprises the following steps:
[0041] S1, preparing the sensor microstructure electrode layer;
[0042] First, spray the MWCNTs solution onto the surface of 80-grit sandpaper flat on a glass plate. After heating and drying, a layer of dry MWCNTs is deposited on the sandpaper surface. Pour the PDMS solution onto the surface and spread it evenly by spin coating. Set the spin coating speed to 400 rpm and the spin coating time to 40 seconds. After heating and curing, the PDMS solution solidifies and the MWCNTs layer is firmly locked. The PDMS film is peeled off to obtain the PDMS / MWCNTs electrode layer. Since the sandpaper surface has an uneven microstructure, the PDMS / MWCNTs electrode layer will also present a microstructure with the opposite properties of the uneven sandpaper surface. The preparation process is as follows: Figure 1 As shown in the figure, since the thickness of the MWCNTs layer is much lower than that of the PDMS layer, the MWCNTs layer will hardly affect the elastic properties of the PDMS layer, thus ensuring that the microstructure electrode has excellent stability, stretchability and low production cost.
[0043] Specifically, the preparation method of the MWCNTs solution is as follows: multi-walled carbon nanotubes with a purity of 95%, a length of 10-30m, and a carboxyl content of 2.0wt% are dispersed in anhydrous ethanol, and after manual stirring for 10 minutes, high-frequency ultrasound is used to further disperse the multi-walled carbon nanotubes for 30 minutes to reduce the occurrence of agglomeration of the multi-walled carbon nanotubes in the dispersion to obtain a multi-walled carbon nanotube / ethanol dispersion with a mass fraction of 1wt%. After the dispersion solution is kept static for 12 hours, the bottom precipitate is removed and the supernatant is retained, which is the MWCNTs solution.
[0044] Specifically, the preparation method of the PDMS solution is: mixing the PDMS main agent and the curing agent at a ratio of 15:1 and stirring for 30 minutes, and then treating under a vacuum state for 30 minutes to remove bubbles in the solution.
[0045] S2, preparing a sensor dielectric layer;
[0046] BaTiO 3 BaTiO with a mass percentage of 30% 3 The mixed solution of / PDMS was spin-coated on a smooth glass sheet, and the spin-coating speed was set to 400 rpm and the spin-coating time was 40 s. After the spin-coating was completed, the sample was placed in a vacuum drying oven and heated at 70 °C for 3 h to solidify the composite film. Finally, the composite film was peeled off from the surface of the smooth glass sheet to obtain BaTiO 3 / PDMS dielectric layer; the preparation process is as follows Figure 2 shown.
[0047] S3, packaging sensor;
[0048] The PDMS / MWCNTs electrode layer was cut into strips with a width of 1 cm and a length of 4 cm. 3 / PDMS dielectric layer is cut into a square with a length of 1.5cm and a width of 1.5cm. The structure of the sensor adopts a "sandwich" structure, with the upper and lower layers being electrode layers and the middle layer being a dielectric layer. A 50um thick, single-sided adhesive PI film is used to seal the three-layer structure. The structural diagram of the sensor is shown in the figure. Figure 3 As shown. The flexible pressure sensor is prepared.
[0049] The flexible pressure sensor prepared according to the above preparation method is tested:
[0050] The sensor was fixed on the base of the digital push-pull force gauge, pressure was applied and the capacitance change corresponding to different pressures was recorded. Figure 4 The pressure-capacitance curve. The piecewise linear fitting analysis shows that within the pressure range of 0-120Pa, the sensitivity of the sensor is 2.39kPa -1 , in the pressure range of 0.27-2.68kPa, the sensitivity of the sensor is 0.23kPa -1 , within the pressure range of 3.25-9.45kPa, the sensitivity of the sensor is 0.08kPa -1 , within the pressure range of 10.73-28.73kPa, the sensitivity of the sensor is 0.02kPa-1.
[0051] Signal acquisition is performed on the flexible pressure sensor prepared according to the above preparation method:
[0052] The multi-channel sensor signal acquisition system is used to collect data on breathing signals, elbow flexion signals, and knee flexion signals. The acquisition results are shown in the figure below. Figure 5 As shown. Figure 5 It can be seen that the sensor responds more accurately to the three breathing states of normal breathing, deep breathing, and rapid breathing. The breathing intensity during deep breathing is stronger than normal breathing, while rapid breathing has a higher breathing frequency, and the depth of inhalation during rapid breathing is similar to deep breathing, but the exhalation is not thorough enough. The real-time acquisition changes of the sensor capacitance value have a good mapping with the actual breathing situation, which is consistent with the actual situation. Figure 6 , 7They represent the capacitance value response of the sensor to the bending state of the elbow joint and the knee joint. The elbow joint is a smaller joint, and the sensor also bends more when the elbow joint is bent, so a larger capacitance value change will occur; the knee joint is a larger joint, and even if the knee joint is bent at a larger angle, the capacitance value response is slightly lower than when the elbow joint is bent due to the smaller size of the sensor. The test curve results also prove that the sensor can effectively respond to different joint motion signals.
[0053] Therefore, three sensors will be used to collect breathing signals, elbow joint and knee joint bending signals respectively to realize the identification of four typical movement states of human body: sitting, standing, walking and running.
[0054] A method for identifying human motion status, the design flow chart is as follows Figure 8 As shown, three flexible pressure sensors prepared according to the above preparation method are used, and one end of the wire is fixed on the surface of the electrode layer using copper foil conductive tape, and the other end of the wire is connected to the same circuit board. The circuit board includes a capacitance acquisition module, a microcontroller module, a switch module and a power module. The power supply voltage of the circuit board is 303V. The microcontroller module transmits the collected sensor signal to the computer end. The key to programming development is IAR software;
[0055] The following steps are involved:
[0056] S1. Obtain original sample data;
[0057] Three flexible pressure sensors were fixed on the chest, elbow and knee joints of the human body. The experimenters kept sitting, standing, walking and running for 1 minute each, and repeated 15 times in total. Considering that the breathing frequency range is about 0.15-0.4Hz, and taking into account the movement frequency of the elbow and knee joints, the sensor signal acquisition frequency was set to 5Hz to avoid introducing too much noise. The three sets of data collected, namely the breathing signal, elbow bending signal and knee bending signal, were used as the original sample data;
[0058] S2, denoising, sample division and feature extraction are performed on the original sample data to obtain a sample set;
[0059] Specifically, due to the limitations of the environment and experimental conditions during the signal acquisition process, various noise signals are inevitably mixed in the signal. Fig. 9 It can be seen from the thinner curves that the breathing signals, elbow and knee bending signals collected by the sensor are interfered by noise to a certain extent. The wavelet threshold denoising method is selected to denoise the collected sensor signals. Fig. 9The thicker curve in the middle shows the denoising effect of the breathing signal in a partial static state. It is not difficult to see that the noise in the signal is successfully removed, the denoised signal has good smoothness and can better retain the original change trend and characteristics of the signal.
[0060] Specifically, the denoised signal is windowed, that is, the longer data is divided into fixed-length data segments as samples. The window length used in this paper is set to 10s, and the sliding window with 5s increments divides the signal into a series of analysis samples, thereby generating a 5s overlap, and maximizing the use of continuous data streams by signal overlap. The signal sampling frequency of the sensor is 5Hz, that is, every 50 data points is taken as a sample, and a sample is collected every 25 data points. A total of 716 groups of samples in four motion states are obtained, and each group of samples includes 10s of breathing signals, elbow and knee bending signals.
[0061] Specifically, the data feature extraction method is time domain feature extraction, and the time domain features include maximum value, minimum value, average value, root mean square and variance, and each group of sample sets containing 15 feature parameters is obtained;
[0062] S3. Determine the structure of the neural network model. The neural network model includes an input layer, a hidden layer and an output layer. The number of neuron nodes in the input layer is 15, and the 15-dimensional input vector constitutes 15 eigenvalues of a set of training data in sequence. The number of neuron nodes in the hidden layer determines the final effect of the neural network. Too few nodes may lead to poor recognition ability of the network, and too many nodes may lead to low fault tolerance. The number of neurons in the hidden layer is 7. The number of neuron nodes in the output layer is 1, and different motion states are represented by outputs 1, 2, 3, and 4. Output 1 represents a sitting state, output 2 represents a standing state, output 3 represents a walking state, and output 4 represents a running state.
[0063] S4, using the Levenberg-Marguardt algorithm to train the neural network model based on the sample set, when the mean square error reaches the optimum, the neural network model is determined as the final neural network model;
[0064] Specifically, 70% of the samples of the 716 groups for distinguishing four motion states were randomly selected as training sets, 15% of the samples were selected as validation sets, and 15% of the samples were selected as test sets. The training algorithm selected was the Levenberg-Marguardt algorithm, and the mean square error of the three sample sets after 26 training iterations reached the optimal value.
[0065] S5. Identify the human body's motion state based on the final neural network model.
[0066] Test the trained neural network model:
[0067] 100 test samples were taken using the signal acquisition system, including 25 sitting samples, 25 standing samples, 25 walking samples, and 25 running samples. The trained human motion state recognition network was tested for reliability using the samples, and the test results are shown in Table 1. As can be seen from the table, the overall correct recognition rate of the test was 94%, among which the neural network analysis model had the highest recognition rate for sitting and standing, reaching 96%, and the recognition rates for walking and running were 92% respectively. This may be because the movement amplitude of the first two states was extremely low, only including the involuntary slight movement of the joints, and the sensor collected data was relatively stable; while the movement amplitude of the walking and running states was large, the sensor collected signals changed dramatically, and the training samples were not comprehensive enough to cover all possible samples.
[0068] Table 1 Test results of neural network model
[0069]
[0070] Of course, the above description is not a limitation of the present invention, and the present invention is not limited to the above examples. Changes, modifications, additions or substitutions made by technicians in this field within the essential scope of the present invention should also fall within the protection scope of the present invention.
Claims
1. A method for preparing a flexible pressure sensor, characterized in that: The following steps are involved: S1, preparing the sensor microstructure electrode layer; First, the MWCNTs solution is sprayed onto the surface of 80-grit sandpaper flat on a glass plate. After heating and drying, a layer of dry MWCNTs is deposited on the sandpaper surface. The PDMS solution is poured on the surface and evenly coated by spin coating. The PDMS solution penetrates into the MWCNTs layer due to gravity. After heating and curing, the PDMS solution solidifies to form a PDMS film. The PDMS film is peeled off to obtain a PDMS / MWCNTs electrode layer. S2, preparing a sensor dielectric layer; A BaTiO3 / PDMS mixed solution with a BaTiO3 mass percentage of 30% was spin-coated on a smooth glass sheet. After the spin coating was completed, the sample was placed in a vacuum drying oven and heated at 70°C for 3 hours to form a solidified composite film. Finally, the composite film was peeled off from the surface of the smooth glass sheet to obtain a BaTiO3 / PDMS dielectric layer. S3, packaging sensor; The PDMS / MWCNTs electrode layer was cut into strips of 1 cm wide and 4 cm long, and the BaTiO3 / PDMS dielectric layer was cut into squares of 1.5 cm long and 1.5 cm wide. The structure of the sensor adopted a "sandwich" structure, with the upper and lower layers being electrode layers and the middle layer being a dielectric layer. The three-layer structure was sealed and bonded using a single-sided adhesive PI film, and the flexible pressure sensor was prepared. In S1, the preparation method of the MWCNTs solution is: multi-walled carbon nanotubes with a purity of 95%, a length of 10-30m, and a carboxyl content of 2.0wt% are dispersed in anhydrous ethanol, and after manual stirring for 10 minutes, high-frequency ultrasound is used to further disperse the multi-walled carbon nanotubes for 30 minutes to obtain a multi-walled carbon nanotube / ethanol dispersion with a mass fraction of 1wt%. After the dispersion solution is kept static for 12 hours, the bottom precipitate is removed and the supernatant is retained, which is the MWCNTs solution.
2. The method for preparing a flexible pressure sensor according to claim 1, characterized in that: In S1, the PDMS solution is prepared by mixing the PDMS main agent and the curing agent at a ratio of 15:1 and stirring for 30 minutes, and then treating the mixture under vacuum for 30 minutes to remove bubbles in the solution.
3. The method for preparing a flexible pressure sensor according to claim 1, characterized in that: In S1 and S2, the spin coating speed was 400 rpm and the spin coating time was 40 s.
4. The method for preparing a flexible pressure sensor according to claim 1, characterized in that: In S3, a PI film with a thickness of 50 um is selected.
5. Application of the flexible pressure sensor prepared by the preparation method according to any one of claims 1 to 4, characterized in that: For human motion state recognition, three flexible pressure sensors are selected. One end of the wire is fixed on the surface of the electrode layer using copper foil conductive tape, and the other end of the wire is connected to the same circuit board. The circuit board includes a capacitance acquisition module, a microcontroller module, a switch module and a power module. The microcontroller module transmits the collected sensor signal to the computer via Bluetooth. The following steps are involved: S1. Obtain original sample data; Three flexible pressure sensors are fixed on the chest, elbow and knee joints of the human body respectively, and the collected breathing signals, elbow bending signals and knee bending signals are used as original sample data; S2, denoising, sample division and feature extraction are performed on the original sample data to obtain a sample set; The wavelet threshold denoising method is used to denoise the original sample data; The feature extraction method is time domain feature extraction. The time domain features include maximum value, minimum value, average value, root mean square and variance. Each group of sample sets contains 15 feature parameters. S3. Determine the structure of the neural network model, wherein the neural network model includes an input layer, a hidden layer, and an output layer; S4, using the Levenberg-Marguardt algorithm to train the neural network model based on the sample set, when the mean square error reaches the optimum, the neural network model is determined as the final neural network model; S5. Identify the human body's motion state based on the final neural network model.
6. The use of the flexible pressure sensor according to claim 5, characterized in that: In S3, the number of neuron nodes in the input layer is 15, and the 15-dimensional input vector constitutes 15 eigenvalues of a set of training data in sequence; the number of neuron nodes in the hidden layer is 7; the number of neuron nodes in the output layer is 1, and different motion states are represented by outputs 1, 2, 3, and 4, respectively, output 1 represents a sitting state, output 2 represents a standing state, output 3 represents a walking state, and output 4 represents a running state.