Method for forming semiconductor structure
By forming the first core layer and the side wall in semiconductor manufacturing, using side wall self-alignment etching to form openings and adjusting the spacing of the conductive layers, the problem of insufficient lithography resolution in the prior art is solved, and the performance of the semiconductor structure is improved and electrical properties.
Patent Information
- Application Number
- CN202010725642.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-07-24
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2040-07-24
AI Technical Summary
In the existing semiconductor manufacturing process, insufficient lithography resolution leads to a spacing deviation during the pattern transfer process, affecting the performance of the final semiconductor structure.
By forming the first core layer and the side wall on the layer to be etched, the initial and second openings are formed by self-aligning etching of the side walls, the spacing of the conductive layers is adjusted, and the controllability of the spacing of the conductive layers is achieved, and the same thickness is used Side wall material to reduce electrical performance deviation.
The performance of semiconductor structure is improved, and through controllable conductive layer spacing and electrical performance, it meets design requirements and reduces the spacing deviation of metal wires.
Smart Images

Figure CN113972167B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor manufacturing, and in particular to a method for forming a semiconductor structure. Background Art
[0002] As circuit integration increases and scale increases, the size of unit devices in the circuit continues to shrink, and the requirements for integrated circuit manufacturing processes continue to increase. For example, critical dimensions continue to decrease, and chip manufacturing has increasingly higher requirements for lithography resolution.
[0003] In the process of manufacturing semiconductor devices, the pattern on the mask is usually transferred to the substrate by using a photolithography process. The photolithography process includes: providing a substrate; forming a photoresist on the semiconductor substrate; exposing and developing the photoresist to form a patterned photoresist so that the pattern on the mask is transferred to the photoresist; etching the substrate using the patterned photoresist as a mask so that the pattern on the photoresist is transferred to the substrate; and removing the photoresist.
[0004] However, there are still problems with the pattern transfer process in the prior art. Summary of the invention
[0005] The technical problem solved by the present invention is to provide a method for forming a semiconductor structure to improve the performance of the finally formed semiconductor structure.
[0006] To solve the above problems, the present invention provides a method for forming a semiconductor structure, comprising: providing a layer to be etched, the layer to be etched comprising a plurality of first regions, a second region and a third region arranged in parallel along a first direction, the second region being adjacent to the first region and the third region respectively; forming a first core layer extending along a second direction on the first region, the first direction being perpendicular to the second direction; forming a first sidewall on the sidewall of the first core layer; forming a sacrificial layer covering a portion of the first sidewall on the layer to be etched, the sacrificial layer having a plurality of initial first openings therein, the initial first openings being located on the second region, and the initial first openings extending along the second direction, and a portion of the initial first openings exposing a portion of the first sidewall on the second region; removing the first sidewall exposed by the initial first opening to form a first opening; forming a second sidewall in the first opening; forming a plurality of second openings in the sacrificial layer, the second openings exposing a portion of one or both of the first sidewall and a portion of the second sidewall.
[0007] Optionally, the method for forming the first core layer includes: forming a first core material layer on the layer to be etched; forming a first patterned layer on the first core material layer, the first patterned layer having a first patterned opening exposing a portion of the first core material layer; etching the first core material layer using the first patterned layer as a mask until the top surface of the layer to be etched is exposed, thereby forming the first core layer.
[0008] Optionally, the method for forming the first side wall includes: forming a first side wall material layer on the side wall and top surface of the first core layer and the top surface of the layer to be etched; etching the first side wall material layer until the first core layer and the top surface of the layer to be etched are exposed to form the first side wall.
[0009] Optionally, the formation process of the first spacer material layer includes an atomic layer deposition process.
[0010] Optionally, the method for forming the sacrificial layer and the initial first opening includes: forming a second core layer on the second region, the second core layer extending along the second direction, and the second core layer covering a portion of the first side wall; forming an initial sacrificial layer on the layer to be etched, the initial sacrificial layer covering the first side wall and the first core layer; back etching the initial sacrificial layer until the top surface of the first side wall and the first core layer are exposed to form the sacrificial layer; after forming the sacrificial layer, removing the second core layer to form the initial first opening.
[0011] Optionally, the process of etching back the initial sacrificial layer includes: one or more combinations of a wet etching process and a dry etching process.
[0012] Optionally, the method for forming the second core layer includes: forming a second core material layer on the layer to be etched; forming a second patterned layer on the second core material layer, the second patterned layer having a second patterned opening exposing a portion of the second core material layer; etching the second core material layer using the second patterned layer as a mask until the top surface of the layer to be etched is exposed, thereby forming the second core layer.
[0013] Optionally, the material of the second core layer includes: organic material, silicon oxide or amorphous carbon.
[0014] Optionally, the material of the first core layer includes: one or more combinations of polycrystalline silicon, amorphous silicon, silicon oxide, silicon nitride and amorphous carbon.
[0015] Optionally, the first side wall and the second side wall have the same thickness.
[0016] Optionally, the first side wall and the second side wall are made of the same material.
[0017] Optionally, materials of the first spacer and the second spacer include: one or more combinations of silicon oxide, silicon nitride, aluminum oxide, aluminum nitride, titanium nitride and titanium oxide.
[0018] Optionally, the material of the sacrificial layer includes: spin-on silicon oxide, metal oxide, polysilicon or amorphous silicon.
[0019] Optionally, after forming the second opening, the method further includes: removing the first core layer and forming a plurality of third openings in the sacrificial layer.
[0020] Optionally, the layer to be etched includes: a substrate and a first mask layer located on the substrate.
[0021] Optionally, after removing the first core layer, the method further includes: etching the first mask layer using the sacrificial layer, the first sidewall and the second sidewall as masks to form a plurality of transition grooves in the first mask layer.
[0022] Optionally, after forming the plurality of transition grooves, the method further includes: etching the substrate using the first mask layer as a mask to form a plurality of target grooves in the substrate.
[0023] Optionally, after forming the plurality of target grooves, the method further includes: forming conductive layers in the plurality of target grooves respectively.
[0024] Optionally, the material of the conductive layer includes: one or more combinations of copper, aluminum, tungsten, cobalt, tantalum, tantalum nitride, titanium, titanium nitride, ruthenium, ruthenium nitride and graphene.
[0025] Optionally, the material of the first mask layer includes: one or more combinations of titanium nitride, tungsten carbide, silicon oxide, silicon oxycarbide and silicon oxycarbonitride.
[0026] Optionally, the layer to be etched further includes: an underlying hard mask layer, wherein the underlying hard mask layer is located on the substrate, and the first mask layer is located on the underlying hard mask layer.
[0027] Optionally, the material of the bottom hard mask layer includes one or more combinations of silicon oxide, titanium nitride, tungsten carbide, silicon carbide, silicon carbide nitride, silicon oxycarbide, aluminum oxide and aluminum nitride.
[0028] Compared with the prior art, the technical solution of the present invention has the following advantages:
[0029] In the technical solution of the present invention, a first core layer is formed on the first region, and the first core layer defines the position of the subsequent third opening. A first sidewall is formed on the first core layer, and the initial first opening and the second opening are formed by self-aligned etching of the first sidewall, thereby reducing the position deviation of the initial first opening and the second opening relative to the third opening. By adjusting the thickness of the first sidewall and the second sidewall, the spacing between the conductive layers formed subsequently is adjusted, so that the spacing between the conductive layers can be controlled to meet the requirements of the final electrical structure, thereby improving the performance of the final semiconductor structure.
[0030] Furthermore, the first sidewall spacer and the second sidewall spacer have the same thickness. By setting the first sidewall spacer and the second sidewall spacer to have the same thickness, the spacing between the conductive layers formed subsequently is also the same, which reduces the deviation of the electrical performance between the conductive layers, thereby improving the performance of the semiconductor structure finally formed. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figures 1 to 3 The invention is a schematic diagram of a method for forming a semiconductor structure;
[0032] Figures 4 to 20 It is a schematic structural diagram of each step of an embodiment of a method for forming a semiconductor structure of the present invention. DETAILED DESCRIPTION
[0033] As described in the background art, there are still problems with the pattern transfer process in the prior art, which will be described in detail below with reference to the accompanying drawings.
[0034] Since the spacing limit of a single mask often cannot meet the precision requirements when forming metal line grooves with small spacing, a two-step patterning process is usually used, among which the LELE (Litho-Etch-Litho-Etch) process is a more common one among the existing multiple two-step patterning process methods. Figure 1 As shown) is split into two parts (as Figure 2 and Figure 3 As shown in the figure, a portion of the pattern is then produced through the lithography and etching steps. However, the lithography, etching and deposition processes will produce EPE (Edge Placement Error), which will lead to vertical alignment deviation between layers, and thus the spacing between the metal lines finally formed will also be biased. Since the alignment deviation caused by this step-by-step etching is uncontrollable, the spacing between the metal lines finally formed is also uncontrollable, which will cause the spacing between the metal lines to be inconsistent with the design requirements, affecting the performance of the semiconductor device finally formed.
[0035] On this basis, the present invention provides a method for forming a semiconductor structure, wherein the position of the subsequent fourth opening is defined by a first core layer located on the first region. A first sidewall is formed on the first core layer, and the initial first opening is formed by self-aligned etching of the first sidewall, thereby reducing the position deviation of the initial first opening relative to the fourth opening. By adjusting the thickness of the second sidewall, the spacing between the subsequently formed conductive layers is adjusted, so that the spacing between the conductive layers can be controlled to meet the requirements of the final electrical structure, thereby improving the performance of the final semiconductor structure.
[0036] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0037] Figures 4 to 20 It is a structural schematic diagram of a formation process of a semiconductor structure according to an embodiment of the present invention.
[0038] Please refer to Figure 4 , providing a layer to be etched.
[0039] In this embodiment, the layer to be etched includes: a substrate 200 and a first mask layer 202 located on the substrate 200 .
[0040] In this embodiment, the material of the substrate 200 is a low-K sacrificial layer (K is less than or equal to 3.9); in other embodiments, the material of the substrate 200 includes silicon oxide.
[0041] The material of the first mask layer 202 includes: one or more combinations of titanium nitride, tungsten carbide, silicon oxide, silicon oxycarbide and silicon oxycarbonitride. In this embodiment, the material of the first mask layer 202 is silicon oxycarbide.
[0042] In this embodiment, the layer to be etched further includes: an underlying hard mask layer 201 , the underlying hard mask layer 201 is located on the substrate 200 , and the first mask layer 202 is located on the underlying hard mask layer 201 .
[0043] The function of the bottom hard mask layer 201 is that the bottom hard mask layer 201 can be used as a stop layer for the subsequent planarization of the conductive film; the material of the bottom hard mask layer 201 is a hard mask material, so when etching is performed subsequently to form each target groove, the etching loss of the bottom hard mask layer 201 is small, so in the process of transferring the pattern in the bottom hard mask layer 201 to the substrate 200, the stability of the pattern transfer is relatively high.
[0044] The bottom hard mask layer 201 may be a single-layer structure or a multi-layer structure, and the material of the bottom hard mask layer 201 includes one or more combinations of silicon oxide, titanium nitride, tungsten carbide, silicon carbide, silicon carbide nitride, silicon oxycarbide, aluminum oxide or aluminum nitride. In this embodiment, the material of the bottom hard mask layer 201 is titanium nitride.
[0045] Please refer to Figure 5 and Figure 6 , Figure 6 yes Figure 5 In the cross-sectional schematic diagram along line AA, the layer to be etched includes a plurality of first regions I, a second region II and a third region III arranged in parallel along a first direction X, the second region II is adjacent to the first region I and the third region III, respectively, and a first core layer 203 extending along a second direction Y is formed on the first region I, and the first direction X is perpendicular to the second direction Y.
[0046] In this embodiment, the regions not marked with the first region I, the second region II, and the third region III are considered to be other regions where the first conductive layer or the second conductive layer is not formed.
[0047] In this embodiment, the first core layer 203 is used to define the position of the third opening to be formed subsequently.
[0048] In this embodiment, the method for forming the first core layer 203 includes: forming a first core material layer (not shown) on the layer to be etched; forming a first patterned layer (not shown) on the first core material layer, the first patterned layer having a first patterned opening (not shown) exposing a portion of the first core material layer; etching the first core material layer using the first patterned layer as a mask until the top surface of the layer to be etched is exposed, thereby forming the first core layer 203.
[0049] The material of the first core layer 203 includes: one or more combinations of polysilicon, amorphous silicon, silicon oxide, silicon nitride and amorphous carbon. In this embodiment, the material of the first core layer 203 is amorphous carbon.
[0050] Please refer to Figure 7 , Figure 7 and Figure 6 In accordance with the viewing direction, a first sidewall 204 is formed on the sidewall of the first core layer 203.
[0051] In this embodiment, the method for forming the first side wall 204 includes: forming a first side wall material layer (not shown) on the side wall and top surface of the first core layer 203 and the top surface of the layer to be etched; etching the first side wall material layer until the first core layer 203 and the top surface of the layer to be etched are exposed to form the first side wall 204.
[0052] In this embodiment, the process of forming the first spacer material layer includes an atomic layer deposition process.
[0053] The material of the first sidewall spacer 204 includes: one or more combinations of silicon oxide, silicon nitride, aluminum oxide, aluminum nitride, titanium nitride and titanium oxide. In this embodiment, the material of the first sidewall spacer 204 is aluminum nitride.
[0054] In this embodiment, after forming the first sidewall 204, the method further includes: forming a sacrificial layer covering a portion of the first sidewall 204 on the layer to be etched, wherein the sacrificial layer has a plurality of initial first openings, the initial first openings are located on the second region II, and the initial first openings extend along the second direction Y, and a portion of the initial first openings exposes a portion of the first sidewall 204 of the second region II. For a specific formation process, please refer to Figures 8 to 11 .
[0055] Please refer to Figure 8 and Fig. 9 , Fig. 9 yes Figure 8 In the cross-sectional diagram along line BB, a second core layer 205 is formed on the second region II. The second core layer 205 extends along the second direction Y, and the second core layer 205 covers a portion of the first sidewall 204 .
[0056] In this embodiment, the method for forming the second core layer 205 includes: forming a second core material layer (not shown) on the layer to be etched; forming a second patterned layer (not shown) on the second core material layer, the second patterned layer having a second patterned opening (not shown) exposing a portion of the second core material layer; etching the second core material layer using the second patterned layer as a mask until the top surface of the layer to be etched is exposed, thereby forming the second core layer 205.
[0057] In this embodiment, the material of the second core layer 205 is different from that of the first core layer 203 , in order to avoid etching damage to the first core layer 203 when the second core layer 205 is subsequently removed.
[0058] The material of the second core layer 205 includes: organic material, silicon oxide or amorphous carbon. In this embodiment, the second core layer 205 is made of silicon oxide.
[0059] Please refer to Fig.10 , Fig.10 and Fig. 9 In accordance with the viewing direction, an initial sacrificial layer (not shown) is formed on the layer to be etched, and the initial sacrificial layer covers the first side wall 204 and the first core layer 203; the initial sacrificial layer is back-etched until the top surfaces of the first side wall 204 and the first core layer 204 are exposed to form the sacrificial layer 206.
[0060] The material of the sacrificial layer 206 includes: spin-on silicon oxide, metal oxide, polysilicon or amorphous silicon. In this embodiment, the material of the sacrificial layer 208 is polysilicon.
[0061] The process of etching back the initial sacrificial layer includes: one or more combinations of a wet etching process and a dry etching process. In this embodiment, the process of etching back the initial sacrificial layer adopts a wet etching process.
[0062] Please refer to Fig.11 After forming the sacrificial layer 206 , the second core layer 205 is removed to form the initial first opening 207 .
[0063] Since the material of the second core layer 205 is different from that of the sacrificial layer 206, the first sidewall 204 and the first core layer 203, the second core layer 205 can be removed by self-alignment between different materials, thereby reducing the position deviation of the initial first opening 207 relative to the subsequently formed third opening.
[0064] In this embodiment, the process of removing the second core layer 205 adopts a wet etching process; in other embodiments, the process of removing the second core layer 205 may also adopt a dry etching process.
[0065] Please refer to Fig.12 , removing the first sidewall 204 exposed by the initial first opening 207 to form a first opening 208 .
[0066] Since the material of the first sidewall spacer 204 is different from that of the first core layer 203 , the first sidewall spacer 204 exposed by the initial first opening 207 can be removed by utilizing self-alignment between different materials.
[0067] In this embodiment, the process of removing a portion of the first sidewall 204 is a wet etching process; in other embodiments, the process of removing a portion of the first sidewall 204 may also be a dry etching process.
[0068] Please refer to Fig.13 A second sidewall 209 is formed on the sidewall of the first opening 208 .
[0069] In this embodiment, the method for forming the second side wall 209 includes: forming a second side wall material layer (not shown) on the side wall and bottom surface of the first opening 208, and the top surface of the first core layer 203, the first side wall 204 and the sacrificial layer 206; etching back the second side wall material layer until the top surface of the first core layer 203, the first side wall 204 and the sacrificial layer 206, and the bottom surface of the first opening 208 are exposed, so as to form the second side wall 209.
[0070] In this embodiment, the first sidewall 204 and the second sidewall 209 are made of the same material, and the second sidewall 209 is made of aluminum nitride. In other embodiments, the second sidewall and the first sidewall may also be made of different materials.
[0071] In this embodiment, the first sidewall spacer 204 and the second sidewall spacer 209 have the same thickness, and the thickness direction is along the first direction X. By setting the first sidewall spacer 204 and the second sidewall spacer 209 to have the same thickness, the spacing between the conductive layers formed subsequently is also the same, which reduces the deviation of the electrical properties between the conductive layers, thereby improving the performance of the semiconductor structure finally formed.
[0072] In other embodiments, the thicknesses of the first side wall and the second side wall may be different.
[0073] Please refer to Fig.14 A plurality of second openings 210 are formed in the sacrificial layer 206 , and the second openings 210 expose a portion of one or both of the first spacer 204 and a portion of the second spacer 209 .
[0074] In this embodiment, part of the second opening 210 is located on the third region III, and part of the second opening 210 is located on the second region II and the third region III.
[0075] Since the material of the sacrificial layer 206 is different from that of the first side wall 204, the second opening 210 is formed by self-aligned etching of the first side wall 204, or the third opening 210 is formed by self-aligned etching of the first side wall 204 and the second side wall 209, thereby reducing the position deviation of the second opening 210 relative to the subsequently formed third opening.
[0076] The process of forming the second opening 210 in the sacrificial layer 206 includes a wet etching process or a dry etching process. In this embodiment, the process of forming the second opening 210 in the sacrificial layer 206 adopts a wet etching process.
[0077] Please refer to Fig.15 and Fig.16 , Fig.16 yes Fig.15 In the cross-sectional diagram along line CC, the first core layer 203 is removed, and a third opening 211 is formed in the sacrificial layer 206 .
[0078] The first core layer 203 is formed on the first region I, and the position of the subsequent third opening 211 is defined by the first core layer 203. The first sidewall 204 is formed on the first core layer 203, and the initial first opening 207 and the second opening 210 are formed by self-aligned etching using the first sidewall 204, thereby reducing the position deviation of the initial first opening 207 and the second opening 210 relative to the third opening 211. By adjusting the thickness of the first sidewall 204 and the second sidewall 209, the spacing between the subsequently formed conductive layers is adjusted, so that the spacing between the conductive layers can be controlled to meet the requirements of the final electrical structure, thereby improving the performance of the final semiconductor structure.
[0079] Since the first core layer 203 is made of a material different from that of the first sidewall spacer 204 , the second sidewall spacer 209 , and the sacrificial layer 206 , the first core layer 203 can be removed by utilizing self-alignment between different materials.
[0080] The process of removing the first core layer 203 includes a wet etching process or a dry etching process. In this embodiment, the process of removing the first core layer 203 adopts a wet etching process.
[0081] Please refer to Fig.17 After removing the first core layer 203 , the first mask layer 202 is etched using the sacrificial layer 206 , the first sidewall 204 and the second sidewall 209 as masks to form a plurality of transition grooves 212 in the first mask layer 202 .
[0082] In this embodiment, the first mask layer 202 is etched by a dry etching process; in other embodiments, the first mask layer may be removed by a wet etching process or a combination of dry etching and wet etching.
[0083] Please refer to Fig.18 After forming the plurality of transition grooves 212 , the substrate 200 is etched using the first mask layer 202 as a mask to form a plurality of target grooves 213 in the substrate 200 .
[0084] In this embodiment, the process of etching the substrate 200 also includes etching the bottom hard mask layer 201 .
[0085] The process of etching the bottom hard mask layer 201 and the substrate 200 using the first mask layer 202 as a mask includes one or a combination of a dry etching process and a wet etching process. In this embodiment, the process of etching the bottom hard mask layer 201 and the substrate 200 adopts a dry etching process and a wet etching process.
[0086] In this embodiment, after forming the target grooves 213, the first mask layer 202 and the bottom hard mask layer 201 are not removed first; in other embodiments, after forming the target grooves, part of the mask layer may be removed first, for example, the first mask layer may be removed first.
[0087] Please refer to Fig.19 and Fig. 20 , Fig. 20 yes Fig.19 In the cross-sectional diagram along line DD, after forming a plurality of target grooves 213 , conductive layers 214 are respectively formed in the plurality of target grooves 213 .
[0088] In this embodiment, the method for forming a conductive layer 214 includes: forming a conductive film (not shown) in a number of the target grooves 213, wherein the conductive film covers the first mask layer 202; planarizing the conductive film, the first mask layer 202 and the bottom hard mask layer 201 until the substrate 200 is exposed, and forming a conductive layer 214 in each of the target grooves 213.
[0089] The material of the conductive layer 214 includes one or more combinations of copper, aluminum, tungsten, cobalt, tantalum, tantalum nitride, titanium, titanium nitride, ruthenium, ruthenium nitride and graphene. In this embodiment, the conductive layer 214 is made of copper and tantalum nitride, and tantalum nitride serves as a barrier layer for copper diffusion.
[0090] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for forming a semiconductor structure, characterized in that: include: Providing a layer to be etched, the layer to be etched comprising a plurality of first regions, a second region and a third region arranged in parallel along a first direction, the second region being adjacent to the first region and the third region respectively; forming a first core layer extending along a second direction on the first region, wherein the first direction is perpendicular to the second direction; forming a first sidewall on a sidewall of the first core layer; Forming a sacrificial layer covering a portion of the first sidewall on the layer to be etched, wherein the sacrificial layer has a plurality of initial first openings, the initial first openings are located on the second region, and the initial first openings extend along the second direction, and a portion of the initial first openings exposes a portion of the first sidewall on the second region; removing the first sidewall exposed by the initial first opening to form a first opening; forming a second side wall in the first opening; A plurality of second openings are formed in the sacrificial layer, wherein the second openings expose one or both of a portion of the first spacer and a portion of the second spacer.
2. The method for forming a semiconductor structure according to claim 1, wherein: The method for forming the first core layer includes: forming a first core material layer on the layer to be etched; forming a first patterned layer on the first core material layer, wherein the first patterned layer has a first patterned opening exposing a portion of the first core material layer; etching the first core material layer using the first patterned layer as a mask until the top surface of the layer to be etched is exposed, thereby forming the first core layer.
3. The method for forming a semiconductor structure according to claim 1, wherein: The method for forming the first side wall includes: forming a first side wall material layer on the side wall and top surface of the first core layer and the top surface of the layer to be etched; etching the first side wall material layer until the first core layer and the top surface of the layer to be etched are exposed to form the first side wall.
4. The method for forming a semiconductor structure according to claim 3, wherein: The formation process of the first spacer material layer includes an atomic layer deposition process.
5. The method for forming a semiconductor structure according to claim 1, wherein: The method for forming the sacrificial layer and the initial first opening includes: forming a second core layer on the second area, the second core layer extending along the second direction, and the second core layer covering part of the first side wall; forming an initial sacrificial layer on the layer to be etched, the initial sacrificial layer covering the first side wall and the first core layer; etching back the initial sacrificial layer until the top surface of the first side wall and the first core layer are exposed to form the sacrificial layer; after forming the sacrificial layer, removing the second core layer to form the initial first opening.
6. The method for forming a semiconductor structure according to claim 5, wherein: The process of etching back the initial sacrificial layer includes: one or more combinations of a wet etching process and a dry etching process.
7. The method for forming a semiconductor structure according to claim 5, wherein: The method for forming the second core layer includes: forming a second core material layer on the layer to be etched; forming a second patterned layer on the second core material layer, the second patterned layer having a second patterned opening exposing a portion of the second core material layer; etching the second core material layer using the second patterned layer as a mask until the top surface of the layer to be etched is exposed, thereby forming the second core layer.
8. The method for forming a semiconductor structure according to claim 5, wherein: The material of the second core layer includes: organic material, silicon oxide or amorphous carbon.
9. The method for forming a semiconductor structure according to claim 1, wherein: The material of the first core layer includes: one or more combinations of polycrystalline silicon, amorphous silicon, silicon oxide, silicon nitride and amorphous carbon.
10. The method for forming a semiconductor structure according to claim 1, wherein: The first side wall and the second side wall have the same thickness.
11. The method for forming a semiconductor structure according to claim 1, wherein: The first side wall and the second side wall are made of the same material.
12. The method for forming a semiconductor structure according to claim 11, wherein: The materials of the first spacer and the second spacer include: one or more combinations of silicon oxide, silicon nitride, aluminum oxide, aluminum nitride, titanium nitride and titanium oxide.
13. The method for forming a semiconductor structure according to claim 1, wherein: The material of the sacrificial layer includes: spin-on silicon oxide, metal oxide, polysilicon or amorphous silicon.
14. The method for forming a semiconductor structure according to claim 1, wherein: After forming the second opening, the method further includes: removing the first core layer and forming a plurality of third openings in the sacrificial layer.
15. The method for forming a semiconductor structure according to claim 14, wherein: The layer to be etched includes: a substrate and a first mask layer located on the substrate.
16. The method for forming a semiconductor structure according to claim 15, wherein: After removing the first core layer, the method further includes: etching the first mask layer using the sacrificial layer, the first sidewall and the second sidewall as masks to form a plurality of transition grooves in the first mask layer.
17. The method for forming a semiconductor structure according to claim 16, wherein: After forming the plurality of transition grooves, the method further includes: etching the substrate using the first mask layer as a mask to form a plurality of target grooves in the substrate.
18. The method for forming a semiconductor structure according to claim 17, wherein: After forming the plurality of target grooves, the method further includes: forming conductive layers in the plurality of target grooves respectively.
19. The method for forming a semiconductor structure according to claim 18, wherein: The material of the conductive layer includes: one or more combinations of copper, aluminum, tungsten, cobalt, tantalum, tantalum nitride, titanium, titanium nitride, ruthenium, ruthenium nitride and graphene.
20. The method for forming a semiconductor structure according to claim 15, wherein: The material of the first mask layer includes: one or more combinations of titanium nitride, tungsten carbide, silicon oxide, silicon oxycarbide and silicon oxycarbonitride.
21. The method for forming a semiconductor structure according to claim 15, wherein: The layer to be etched further includes: an underlying hard mask layer, wherein the underlying hard mask layer is located on the substrate, and the first mask layer is located on the underlying hard mask layer.
22. The method for forming a semiconductor structure according to claim 21, wherein: The material of the bottom hard mask layer includes one or more combinations of silicon oxide, titanium nitride, tungsten carbide, silicon carbide, silicon carbide nitride, silicon oxycarbide, aluminum oxide and aluminum nitride.
Citation Information
Patent Citations
Semiconductor structure and formation method therefor
CN106952865A
Semiconductor structure and forming method thereof
CN109545684A
Semiconductor structure and forming method thereof
CN109904073A
METHOD OF FABRICATING PHASE-CHANGE MEMORY DEVICE HAVING TiC LAYER
US20100190321A1