Wind turbine rotor blade manufacturing
By using thermal management technology of phase change materials in the manufacturing of wind turbine rotor blades, the problem of difficult heat management in the existing technology is solved, achieving more stable blade manufacturing and a more efficient production process.
Patent Information
- Application Number
- CN202110850448.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-07-27
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2041-07-27
AI Technical Summary
The complex manufacturing methods of existing wind turbine rotor blades make it difficult to manage the heat of the resin material during the cross-linking reaction, which may lead to incomplete curing or damage to auxiliary equipment, and the stability of the blades cannot be guaranteed.
Phase change materials are used to set different states in specific areas to absorb or release heat and adjust the heat distribution in the cross-linking reaction. By setting the phase change material on the surface of the fiber material and utilizing its thermal management capabilities during the cross-linking reaction, the resin is ensured. Complete cure and blade stability.
The manufacturing process is simplified, time is reduced, the stability of the rotor blades is improved, damage to auxiliary equipment is avoided, and the hardness and strength of the blades are ensured.
Smart Images

Figure CN113977986B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method of manufacturing a rotor blade for a wind turbine. Background Art
[0002] A conventional wind turbine comprises a wind turbine tower, a nacelle mounted on top of the tower, wherein a rotor is rotatably supported within the nacelle, where a plurality of rotor blades are mounted. Once the rotor rotates, a coupled generator generates electrical energy that is supplied to a grid.
[0003] Rotor blades for conventional turbines can have a considerable length, for example between 30 and 100 meters. Conventionally, rotor blades are manufactured by cross-linking resins in which fiber materials are embedded. During the cross-linking reaction of the resin material or in order to start the cross-linking reaction, heating is performed. For the one-piece blade manufacturing method, heating is only possible from the outside. The heating necessary for internal curing (i.e. cross-linking the resin) is mainly generated by the exotherm from the curing reaction.
[0004] Overheating in resin-rich areas and thick laminates as well as insufficient heating at the contact of prefabricated parts and infused laminates can both lead to problems in completed rotor blades. In particular, too little heat during the crosslinking reaction can lead to a locally low (incomplete) degree of crosslinking of the resin, which can require a subsequent post-curing step. On the other hand, overheating can damage auxiliary equipment and, in the worst case, can lead to burns on the blade and can cause fires in auxiliary equipment such as mandrels.
[0005] Mandrels and their use in the casting of blades have been described in EP 1 310 351 , US 2011 / 0274553, US 8 919 754 and for example EP 2 897 791 .
[0006] Document WO 03 / 000623A1 discloses a method and apparatus for casting molten material using a phase change material. In which the phase change material is heated above its melting point, the mold is filled with the mold material and excess material is held in a funnel device. The latent heat of fusion of the phase change material heats the funnel device as the phase change material changes from liquid to solid and prevents the material in the funnel device from solidifying as the material in the mold solidifies and shrinks, thereby allowing the material in the funnel device to be fed into the mold and fill any voids created by the shrinkage of the solidified material.
[0007] Conventionally, thermal management during the manufacture of wind turbine blades has been performed by varying the layup of reinforcements or auxiliary materials. Resin-rich areas are usually avoided in design to avoid overheating. Thin sections that tend to not cure completely are covered with additional layers of glass or auxiliary materials to increase the layer thickness and generate more heat release. If this is not possible, the curing time must be extended or the blade must be post-cured locally using a heating blanket or as a whole in an oven.
[0008] Therefore, conventional manufacturing methods are cumbersome and complicated, and result in the design of the resin material taking into account the amount of heat generated during the curing reaction. However, as a result, the stability problem of the rotor blade may not be optimally considered.
[0009] Therefore, there is a need for a method of manufacturing a rotor blade for a wind turbine, wherein the method is simplified, requires less time, and is able to ensure the required stability of the manufactured rotor blade. Furthermore, auxiliary equipment used during manufacturing may not be damaged during manufacturing, so that the auxiliary equipment may be used again to manufacture further rotor blades. Summary of the invention
[0010] This need is met by a method according to the invention for manufacturing a rotor blade for a wind turbine. Advantageous embodiments of the invention are described by preferred embodiments.
[0011] According to an embodiment of the present invention, a method for manufacturing a rotor blade for a wind turbine is provided, the method comprising: placing a fiber material on a shape forming surface (for example, provided by a mold); setting a phase change material (also referred to as PCM) in a first state at at least one predetermined first region (specifically in thermal contact with the fiber material), and / or setting a phase change material in a second state at at least one predetermined second region (specifically in thermal contact with the fiber material); embedding / impregnating the fiber material to be in thermal contact with the phase change material at the first region and / or the second region with a resin; during a cross-linking reaction for cross-linking the resin: absorbing heat generated in the resin by the phase change material at the first region; and / or releasing heat from the phase change material toward the resin at the second region.
[0012] The method can be performed partially manually and partially automatically after starting the crosslinking reaction. The fiber material can, for example, include a glass fiber material and / or a carbon fiber material or any other type of fiber material. The fiber material is then impregnated or embedded with a resin that can be in a fluid state before starting or completing the crosslinking reaction. When fully cured, after completing the crosslinking reaction, the fiber material can be firmly connected to the already crosslinked solidified resin. Thereby, the fiber material is used as a reinforcement to provide a rigid and strong rotor blade surface.
[0013] Placing the fiber material on the shape forming surface can, for example, be performed partially manually. Thereby, the fiber material can be provided in multiple pieces, such as pads or webs having a size of, for example, between 30×50 cm and, for example, 1 m×3 m. The shape forming surface can, for example, be complementary in shape to a pressure surface or a suction surface of a rotor blade to be manufactured. The shape forming surface can be substantially completely covered with the fiber material, in particular so that the fiber material covers the shape forming surface substantially uniformly, so that the thickness of the fiber material is substantially constant across the shape forming surface. In other embodiments, the thickness or amount of fiber material placed on specific areas of the shape forming surface can vary depending on the strength requirements expected in different areas of the wind turbine blade.
[0014] Phase change material can include materials that can exist in at least two states (i.e., first state and second state). The transition from the first state to the second state can, for example, occur when heat is supplied to the phase change material in the first state. The transition of the phase change material from the second state to the first state can, for example, occur when heat is released from the phase change material in the second state. The phase change material can include one or more other states. For example, the transition from the first state to the second state or from the second state to the first state may include or may not include the transition between one or more other intermediate states. The phase change material in the first state and / or the second state can be a liquid or solid state. In order to set the phase change material to the first state or the second state, corresponding preparation steps can also be performed, wherein the phase change material is heated or cooled so that the phase change material is set to the first state or the second state.
[0015] By placing the phase change material in the corresponding state directly onto the fiber material (or onto the plastic sheet covering the fiber material) that has been placed on the shape forming surface, the phase change material can be arranged at the at least one predetermined first area in the first state or at the at least one predetermined second area in the second state. In other embodiments, the phase change material (in the first state or the second state) can be attached to an auxiliary device, specifically a filling body or a mandrel, which can be placed as a whole onto the fiber material on the shape forming surface. Thereby, one or more filling bodies can be covered by a plastic sheet.
[0016] The predetermined first area and the predetermined second area can be determined based on an analysis or simulation or estimation of the thermal behavior of the entire system during the cross-linking reaction, the system comprising resin, fiber material and additional reinforcement structure within the rotor blade. For example, the predetermined first area can be an area where a relatively thick layer or a large amount of resin is present, and the at least one predetermined second area can be an area where a relatively small amount of resin is present or the resin has a relatively small thickness or contacts other structures that do not participate in the cross-linking reaction. The phase change material in the first state is arranged in the at least one predetermined first area and the phase change material in the second state is arranged in the at least one predetermined second area. It can be performed, for example, in a single step, wherein a filling body and possibly another filling body having a phase change material in the first state installed at a specific area and a phase change material in the second state installed at other areas are placed on the fiber material on the shape forming surface.
[0017] The resin may, for example, contain epoxy resin or acrylic resin or any other type of resin capable of undergoing a cross-linking reaction in which the molecules in the resin are cross-linked to form covalent bonds or other bonds. The fiber material may be impregnated with the resin when the resin is in a liquid state. After cross-linking or curing the resin, the resin will be in a solid state embedded in or surrounding the fiber material. When the phase change material at the first region and / or the second region contacts the resin, the phase change material at the first region may absorb the heat generated in the resin at the first region and may release the heat to the resin at the second region. The fiber material and / or the resin need not directly contact the phase change material, but thermally contact the phase change material. For example, a plastic foil or sheet may be between the phase change material and the resin / fiber material. Thus, vacuum-assisted manufacturing (e.g., vacuum-assisted resin transfer molding (VARTM)) is supported, wherein the resin is introduced into a sealed mold (particularly formed by a shape forming surface and another shape forming surface) and is vacuum-drawn to impregnate all fiber materials disposed in the sealed mold. The resin may, for example, be introduced from a section that eventually forms the root of the rotor blade and may be drawn toward the tip of the rotor blade. In other embodiments, multiple entry ports may be provided to introduce resin into the sealed mold body, and one or more suction ports may be provided to cause the resin to flow through the sealed mold and thereby substantially saturate the entire fiber material placed within the sealed mold.
[0018] By having the phase change material disposed in the first state at the predetermined first region, heat generated in the resin is advantageously absorbed. Thus, overheating can be avoided. When the phase change material in the second state is disposed at the predetermined second region, heat can advantageously be released from the phase change material to the resin to accelerate the cross-linking reaction compared to the case where the phase change material in the second state is not present.
[0019] According to an embodiment of the present invention, the first state allows absorption of heat (for example, transformation into a second state) and includes a solid phase of a phase change material, in particular a crystalline phase or a first crystalline phase, wherein the second state allows release of heat (for example, transformation into a first state) and includes a liquid phase or a second crystalline phase of the phase change material.
[0020] The phase change material may have a melting temperature between 50°C and 100°C, specifically between 60°C and 80°C, specifically about substantially 70°C. The phase change material may comprise an organic (carbonaceous) material, such as a material obtained from petroleum, plants or animals. The phase change material may comprise hydrocarbons, primarily paraffins and / or lipids, but also one or more sugar alcohols. For example, paraffins may contain 31 carbons, paraffins may contain 32 carbons, or paraffins may contain 33 carbons, which may have a melting temperature between 60°C and 80°C. The phase change material may also comprise stearic acid, acrylic acid, dinitrotoluene, phenylacetic acid, or a combination of the above materials, for example. The phase change material may comprise an inorganic material, such as a salt hydrate, which may typically use natural salts from the ocean or a mineral deposit, or may be a pre-byproduct of other processes. A third type of phase change material that may be used is a solid to solid phase change material, such as Na2SiO3*5H2O having a melting temperature of 72°C. The phase change material may comprise one or more organic components and one or more inorganic components, in particular alkanes and / or inorganic salts and / or sodium acetate. The material may be provided in a plurality of pockets or pouches, such as plastic bags. Thus, the method may be performed using conventionally available materials. When the melting temperature is, for example, between 60° C. and 80° C., the curing reaction or cross-linking reaction required for forming the rotor blade may be advantageously supported.
[0021] According to an embodiment of the invention, the shape forming surface is provided by the first mould and defines the shape of the suction side or the pressure side of the rotor blade.
[0022] The first mold may include a shape forming surface that is substantially complementary to the suction side or pressure side of the remanufactured rotor blade. A second mold having another shape forming surface may further be used to define the pressure side or suction side of the rotor blade. The second mold may be placed onto the (circumferential) edge of the first mold so that the first mold and the second mold contact each other at the respective edges. The edges of the first mold and the second mold may then be connected and sealed, wherein the filling body and the other filling body are encapsulated together with the fibers and the phase change material at the predetermined area. Subsequently, a resin may be introduced into the sealed mold formed by the first mold portion and the second mold portion. In addition, the cross-linking reaction may be initiated by supplying or generating heat from outside the mold.
[0023] According to an embodiment of the present invention, the method further includes: arranging a filling body, specifically a filling body comprising a flexible foam, at the fibrous material on the shape forming surface, wherein the phase change material is arranged to be close to and / or at least partially embedded in the filling body and / or at least partially adhered to the filling body; specifically, the fibrous material is arranged at least partially around the filling body.
[0024] The filling body may also be referred to as a mandrel, which may also be used in conventional manufacturing methods. However, the filling body according to this embodiment of the present invention is prepared to receive a phase change material in a first state and / or a second state at one or more predetermined areas, so that the corresponding phase change material is (reversibly) connected to the filling body. When the phase change material is attached or connected to the filling body in some way, the phase change material can be easily arranged at a predetermined first area and / or a predetermined second area, and it is ensured that the phase change material remains at those predetermined first areas and / or predetermined second areas during any one manufacturing step without displacement. The filling body can basically fill the half of the internal space of the rotor blade to be manufactured that does not include the space required for resin and fiber material. The filling body and another filling body (mentioned below) can be covered by a plastic foil or sheet, so that the phase change material arranged close to and / or attached to the filling body and / or another filling body is surrounded by the plastic foil. The filling body can advantageously fill the part of the rotor blade to be manufactured that is not expected to be filled with resin.
[0025] According to an embodiment of the invention the filling body (or covering plastic sheet) contacts an inner part of the fiber material and / or resin substantially forming the suction side or pressure side half and / or forming the leading edge or trailing edge of the rotor blade.
[0026] When the filling body contacts the inner part of the fiber material and / or resin forming only half of the suction side or pressure side of the wind turbine, advantageously, a reinforcement structure comprising resin and fiber material can be manufactured and arranged to connect the suction surface inner part and the pressure surface inner part of the rotor blade. Thereby, the rotor blade can be reinforced as required.
[0027] According to an embodiment of the present invention, the method further includes: arranging another filling body at the fiber material on the shape forming surface, wherein the phase change material is arranged to be close to and / or at least partially embedded in the other filling body and / or at least partially adhered to the other filling body; arranging the fiber material at least partially around the other filling body.
[0028] The filling body and / or the further filling body may be provided by an integrally formed structure or may in other embodiments be provided by a plurality of filling body parts. When the filling body and / or the further filling body are provided as an integrally formed structure, it may be simplified to withdraw the filling body and the further filling body from a complete rotor blade, for example from a root end section from the interior of a manufactured rotor blade.
[0029] According to an embodiment of the present invention, a further filling body (or a plastic covering sheet) contacts an inner part of the fiber material and / or resin which basically forms half of the pressure side or suction side and / or forms the trailing edge or leading edge of the rotor blade, wherein specifically by the filling body and the further filling body as well as the fiber material and the resin, substantially the entire inner space of the rotor blade is filled.
[0030] The filling body and the further filling body are not in direct contact with each other within the rotor blade to be manufactured. The filling body and / or the further filling body may both comprise planar outer surfaces facing each other within the rotor blade to be manufactured. The planar surfaces may be substantially approximately perpendicular to the suction surface and the pressure surface. In the interface or gap between the two planar surfaces of the filling body and the further filling body, a reinforcing structure may be formed, also referred to as a reinforcing web, which comprises one or more precast parts and other parts manufactured by cross-linking a resin embedded in a fiber material, the cross-linking occurring during the same reaction as when manufacturing the suction surface and the pressure surface and the leading edge and the trailing edge by cross-linking a resin impregnated into the fiber material.
[0031] According to an embodiment of the present invention, the method further includes: forming a reinforced web that ultimately connects the suction side and the pressure side inside the complete rotor blade by: arranging a precast web portion in the root section between the filling body and another filling body; arranging a fiber material in the center-to-tip section between the filling body and another filling body; impregnating the fiber material in the center-to-tip section, between the filling body and another filling body with a resin and cross-linking.
[0032] The reinforcing web may connect the interior of the pressure surface of the rotor blade with the interior of the suction surface inside the complete rotor blade to strengthen the rotor blade. The precast web portion may be a solid reinforcement structure (e.g. a laminate) that has been fully cured and cross-linked. The precast web portion may be placed in the root section between the planar surface of the filling body and the other filling body. The fiber material may also be placed onto or between the planar surface of the filling body and the other filling body. The fiber material may be placed in any remaining free space between the planar surface of the filling body and the other filling body, i.e. not only in the center to tip section but also in the root region between the root end of the rotor blade to be connected and the precast web portion.
[0033] According to an embodiment of the present invention, the filling body includes at least one first installation area for receiving and / or installing a phase change material in a first state, specifically a first groove, and / or the filling body includes at least one second installation area for receiving and / or installing a phase change material in a second state, specifically a second groove, and / or another filling body includes at least one other first installation area for receiving and / or installing a phase change material in a first state, specifically another first groove, and / or another filling body includes at least one other second installation area for receiving and / or installing a phase change material in a second state, specifically another second groove.
[0034] The filling body and the further filling body can have a first mounting area and / or a second mounting area, for example by cutting or removing material from the filling body at the corresponding mounting areas. The phase change material can be placed in and also attached or attached to the groove. Thus, one or more different attachment methods and devices can be used, such as rubber bands, tapes, adhesives or simply by using a plastic foil to cover the groove filled with the phase change material in the corresponding state. The corresponding first and second mounting areas can be shaped and / or selected and / or positioned so that, when the filling body and / or the further filling body is placed on the fiber material on the shape forming surface, the phase change material in the first state is placed at a predetermined first area and the phase change material in the second state is arranged at a predetermined second area, which area is relative to the area of the rotor blade to be manufactured.
[0035] According to an embodiment of the invention, the first mounting area is located at, at and / or near at least one of: the fiber material and the resin that eventually forms at least a central portion of the reinforcing web; the fiber material and the resin that eventually forms at least a central portion of the pressure side and / or suction side of the rotor blade.
[0036] The first mounting area can be, for example, close to the corresponding planar surface portion (surface) of the filling body and the other filling body. The space between the planar surface of the filling body and the planar surface of the other filling body can form a part of the reinforcing web. In this area, a large amount of heat is expected to be generated during the cross-linking reaction. Therefore, when the phase change material in the first state is installed at the first mounting area, this incoming heat is advantageously absorbed by the phase change material in the first state. In addition, also in the area where there is resin to ultimately form the pressure side and / or suction side, it is expected that during cross-linking, excess heat is generated, which can be advantageously absorbed by the phase change material in the first state arranged in the first mounting area.
[0037] According to an embodiment of the present invention, the second mounting area is located at and / or near at least one of the following: a tip side end portion of a precast web portion in a central portion of the blade, specifically extending from an inner portion of the blade on the suction side to an inner portion of the blade on the pressure side; a root end of a filler body and / or another filler body.
[0038] At the tip side end of the precast web portion and at the root ends of the filling body and the other filling body, it is expected that during the cross-linking reaction, if the phase change material in the second state is not placed at the second installation area, there will be relatively cold areas, which will delay the cross-linking reaction.
[0039] According to an embodiment of the present invention, the first installation area and / or the second installation area of a filling body and / or another filling body allows the phase change material to be reversibly installed at the corresponding filling body, specifically using elastic material and / or tape for installation, wherein the phase change material is contained in at least one bag, specifically in multiple bags.
[0040] When the phase change material is reversibly mounted at the filling body and / or at the further filling body, the phase change material can advantageously be used again for the manufacture of another rotor blade after the crosslinking reaction has been completed and the filling body and the further filling body have been removed from the interior of the manufactured rotor blade. However, since the phase change material has been transformed from the first state into the second state and from the second state into the first state, respectively, during the previous crosslinking reaction, the phase change material should be set to the state required for a specific installation area before it is used for another manufacture of another rotor blade. For example, the phase change material can be exchanged from the corresponding first installation area to the corresponding second installation area and vice versa.
[0041] According to an embodiment of the present invention, the method further includes: setting another shape forming surface on which the fiber material is placed onto the filling body and / or another filling body; sealing / connecting the (e.g. circumferential) edge of the shape forming surface to / with the (e.g. circumferential) edge of the other shape forming surface, thereby encapsulating the filling body and / or another filling body and the fiber material on the shape forming surface and the other shape forming surface and the fiber material surrounding the filling body and / or another filling body; supplying resin to the encapsulated fiber material, specifically using vacuum-assisted supply, wherein the other shape forming surface specifically defines the shape of the pressure side or suction side of the rotor blade; specifically further includes: heating from the outside to start and / or accompany the cross-linking reaction of the resin.
[0042] Thus, the method may be characterized as a one-shot method, wherein substantially or essentially the entire rotor blade is manufactured by one single cross-linking reaction and the rotor blade is manufactured by a single mold formed by connecting a shape forming surface and another shape forming surface and sealing them.
[0043] According to an embodiment of the present invention, during the cross-linking reaction, the phase change material at the at least one first region is at least partially transformed from the first phase to the second phase, and / or during the cross-linking reaction, the phase change material at the at least one second region is at least partially transformed from the second phase to the first phase.
[0044] Thus, the phase change material can provide additional heat for the cross-linking reaction where it is needed, and can absorb heat at specific areas where heat absorption is needed.
[0045] According to an embodiment of the present invention, the method further includes: after completing the cross-linking reaction: removing the filling body and / or another filling body from the interior of the rotor blade and removing the solidified resin from the root portion; disassembling the phase change material at least in one first area and / or at least in one second area from the filling body and / or another filling body; in order to manufacture another rotor blade: installing the phase change material obtained from the second area at the first area; and / or installing the phase change material obtained from the first area at the second area.
[0046] Additionally or alternatively, the corresponding phase change material zones removed from the first region and / or the second region may additionally be analyzed for their corresponding state and, based on the analysis, may also be prepared to be in a desired state, after which the phase change material is installed at the corresponding first mounting region and / or the second mounting region for preparing the next rotor blade.
[0047] Embodiments of the present invention allow for improved manufacturing of wind turbine blades, wherein the stiffness or strength of the rotor blade and the quality of the cross-linked resin and fiber material can be improved. By introducing a phase change material (PCM) in critical areas, for example into or at or near a forming body, in particular a mandrel, both extremes during the cross-linking reaction, i.e. undercooled temperatures and overheated temperatures, can be compensated. Excess energy in overheated areas can be absorbed by the PCM. By, for example, exchanging a PCM pack from an overheated position to a heat-deficient position, the stored energy can be used to heat areas with too low a temperature when producing the next rotor blade.
[0048] Phase change materials can have the ability to balance temperature extremes or store energy via a transition from one phase to another. The most common phase transition can be a melting / crystallization transition. Melting is an endothermic phase transition so that it absorbs energy and can help remove excess energy. Reverse solidification and crystallization can release equal amounts of energy. A special case is a supercooled liquid, which does not spontaneously crystallize below the melting point, but remains liquid until an external trigger initiates crystallization.
[0049] The PCM that can be used in embodiments of the present invention should provide special properties to be suitable for use in the proposed method. Specifically, it should be suitable for being placed near or at a filler body or mandrel and attached to it. The melting temperature can be, for example, about 70°C or in the range of from 60°C to 80°C. The PCM can ideally crystallize in a solvent or diluent to form a sol (form) that is still flexible and flowable. In order to transfer excess energy from hot spots to cold spots, the PCM can ideally be stable like a supercooled liquid. Candidate materials for the PCM can be pure organic compounds or mixtures thereof, for example medium-chain length, chain alkanes or organic or inorganic salts, such as sodium acetate.
[0050] The PCM packets can be placed in bags in or at the fill body, close to the surface of the fill body (mandrel). Advantageously, they need to be easily accessible to remove the PCM after each curing cycle.
[0051] In an embodiment of the present invention, the PCM is provided, for example, in a package, and does not need to be connected to the outside, and does not require cables or controls. The process is energy neutral, and by storing excess heat in the PCM, the excess heat is transferred to where the heat is needed. Compared to other solutions, the complexity is greatly reduced and the investment cost is minimal.
[0052] By using embodiments of the present invention, the cycle time for manufacturing multiple wind turbine blades can be reduced to result in faster curing of sensitive areas of the blades. At the same time, the integrity of the blades can be enhanced and hardness can be ensured because overheating and too fast curing can be avoided.
[0053] The aspects defined above and further aspects of the invention are apparent from the examples of embodiment to be described hereinafter and are explained with reference to the examples of embodiment.The invention will be described in more detail hereinafter with reference to examples of embodiment, but the invention is not limited to these examples. BRIEF DESCRIPTION OF THE DRAWINGS
[0054] Embodiments of the invention will now be described with reference to the accompanying drawings. The invention is not limited to the embodiments shown or described.
[0055] Figure 1 schematically illustrates a front cross-sectional view of a wind turbine rotor blade during manufacture according to an embodiment of the present invention;
[0056] Figure 2 The side cross-sectional view schematically shows Figure 1 The wind turbine blade shown in ;
[0057] Figure 3 and Figure 4 A graph showing temperature distribution according to the prior art and an embodiment according to the present invention is illustrated. DETAILED DESCRIPTION
[0058] The illustrations in the drawings are schematic. It should be noted that in different drawings, similar or identical elements in structure and / or function have the same reference numerals or reference numerals that differ only in the first digit. The description of an element not described in one embodiment can be obtained from the description of this element with respect to another embodiment.
[0059] Figure 1 and Figure 2 A wind turbine rotor blade 1 is schematically shown during manufacture, in a cross-sectional front view and a cross-sectional side view, respectively, including a manufacturing apparatus. Thus, during normal operation the complete rotor blade 1 will rotate about an axis of rotation 3 which is substantially perpendicular to the Figure 1 drawing plane. Figure 2 A wind turbine blade 1 is shown in a cross-sectional side view, wherein the rotation axis 3 is Figure 2 is oriented substantially vertically. Figure 2 As can be seen in FIG. 1 , the first mould part 5 is placed on the ground 7 (or on a support). The first mould part 5 comprises a shape forming surface 9 which is complementary to or defines a suction surface or a pressure surface of the rotor blade 1 to be manufactured.
[0060] The complete rotor blade 1 has a leading edge 14 and a trailing edge 16 .
[0061] In a first manufacturing step, a fiber material 11 is placed onto the shape forming surface 9. Figure 2 , this is only schematically illustrated for clarity of illustration, depicting a gap between the shape forming surface 9 and the fiber material 11. In reality, the fiber material 11 is placed directly onto the shape forming surface 9 of the first mold part 5. Later during manufacturing, the fiber material 11 will be impregnated with resin, forming a fiber material / resin 13. Later, the mixture of resin and fiber material 13 will be crosslinked or cured so as to solidify, thereby actually forming the pressure side 15 or the suction side 17 of the rotor blade.
[0062] like Figure 1 As can be seen in FIG. 1 , the filling body 19 has been arranged at the fibrous material 11 which has been placed on the shape forming surface 9. The filling body 19 (and the further filling body 25) has the phase change material 21 attached thereto in the first state at the predetermined first regions 23a, 23b, 23c, 23d. The phase change material 21 is also placed at the first region 23b, as shown in FIG. Figure 2Moreover, this PCM 21 in the first state provided at the first area 23b is adhered or attached to the filling body 19 or another filling body 25, which is also provided at the fiber material 11 provided on the shape forming surface 9 of the first mold part 5. For example, the PCM 21 in the first state provided at the first area 23b is adhered or attached to the filling body 19 or another filling body 25, which is also provided at the fiber material 11 provided on the shape forming surface 9 of the first mold part 5. Figure 1 The outer surface of the rotor blade is attached to or received in the grooves in the first filler body 19 and the further filler body 25 at the outer surface above or below the drawing page to be close to the pressure side 15 or the suction side 17 of the rotor blade.
[0063] exist Figure 2 In the embodiment, the filling body 19 and the further filling body 25 are not shown because Figure 2 1 is a cross-sectional view, wherein the cross-section is in the central part, wherein in the complete rotor blade the reinforcing web 27 will be formed. For the sake of clarity, the fiber material 11 and the fiber material impregnated with the resin 13 are shown in FIG. Figure 2 In this central area, it is not shown. Figure 2 The reinforcement web 27 shown in the figure will eventually also comprise fiber material and resin and will also solidify during the cross-linking reaction. Thus, the fiber material / resin of the reinforcement web and the fiber material / resin of the suction side 17 and / or the pressure side 15 will contact the phase change material 21 in the first state at the first predetermined areas 23a and 23b.
[0064] Furthermore, the method comprises placing the phase change material 29 at the predetermined second area 31a, 31b, 31c also in thermal contact with the fiber material 11 and / or the resin and the fiber material. Moreover, the PCM 29 in the second state is placed close to or adhered to or attached to the first filling body 19 and / or the further filling body 25. Figure 1 and Figure 2 As can be seen in FIG. 1 , both the filling body 19 and the further filling body 25 contact an inner portion of the fiber material and / or resin forming the suction side 17 half or the pressure side 15 half of the rotor blade.
[0065] The filling body 19 comprises a planar outer surface 33, which faces a planar outer surface 35 of the other filling body. In these planar surfaces 33, 35, respective grooves are provided to enable the PCM 21 to be arranged in the first state at the first areas 23a and 23d, respectively. Similar grooves are provided in the filling body 19 at a first area 23b of the inner part close to the suction side 17. Similar grooves are provided in the other filling body 25 at a first area 23c of the inner part close to the pressure side 15.
[0066] Furthermore, the filling body 19 and the other filling body 25 include grooves to allow attachment of the PCM 29 in the second state at the predetermined second areas 31 a , 31 b , 31 c .
[0067] The method further includes forming a reinforcing web 27, which eventually connects the suction side 17 and the pressure side 15 of the rotor blade inside the completed rotor blade 1. Thereby, the precast web portion 37 is arranged in the root section 39 between the filling body 19 and the further filling body 25. Furthermore, the fiber material 11 is arranged in the center-to-tip section 41 to be between the filling body 19 and the further filling body 25. Furthermore, the fiber material 11 in the center-to-tip section 41 is impregnated with resin and cross-linked.
[0068] Based on the analysis or simulation of the cross-linking reaction, one or more first areas or second areas to be filled with the PCM in the first state or the second state may be identified. Corresponding mounting areas at the filling body 19 and / or the further filling body 25 may be provided. The PCM may be attached to the filling body and / or the further filling body at the corresponding mounting locations. Figure 1 As can be seen in the figure, the first mounting area 23a is close to the fiber material and resin that will eventually form at least the central part of the reinforcing web 27. Furthermore, the first area 23b is located at a position that will eventually form at least the central part of the pressure side 15 and / or suction side 17 of the rotor blade.
[0069] like Figure 1 As can be seen in Fig. 1 , the second region 31a, 31c is close to the root end 43 of the filling body 19 and / or the further filling body 25. The second region 31b is at the tip end portion of the precast web portion 37 in the central portion of the blade.
[0070] In the next manufacturing step, the other shape-forming surface 45 of the second mold part 47, on which the fiber material is also placed, is set to the filling body 19 and / or the other filling body 25. Then, the edges 49 and 51 of the shape-forming surface 9 and the other shape-forming surface 45 are connected and sealed in a circumferential manner to enclose the filling body 19 and / or the other filling body 25 and the fiber material 11 and the resin. Then, the resin is supplied into the space enclosed by the shape-forming surface 9 and the other shape-forming surface 45 that is not occupied by the filling bodies 19 and 25.
[0071] Furthermore, the method includes heating the resin from outside the mold formed by the molding parts 5 and 47. Figure 1 and Figure 2In the embodiment, one or more inlet ports and one or more outlet ports for introducing resin are not shown. A heating device is not specifically shown either. By heating, a cross-linking reaction can be started. During the cross-linking reaction, at least partially, the phase change material at the first region 23a, 23b, 23c, 23d can be transformed from the first phase to the second phase and / or the phase change material at the second region 31a, 31b, 31c can be transformed from the second state to the first state.
[0072] After the cross-linking reaction has been completed, the filling body 19 and the further filling body 25 can be removed from the interior of the rotor blade, in particular withdrawn from the root end section 43. The phase change material 21 at the first installation area 23a, 23b, 23c, 23d can be removed and the phase change material 29 initially in the second state can be removed or disassembled from the filling body 19 and the further filling body 25. The state of the respective phase change material 21, 29 can be checked after the cross-linking reaction has been completed. In order to manufacture the next rotor blade, the respective phase change material can be prepared in a defined first state or a defined second state and can be installed at the first area and the second area, respectively. Ideally, a plurality of PCMs initially in the first state and PCMs initially in the second state can simply be exchanged and installed at the filling body and / or the further filling body 19, 25.
[0073] The pre-cast web 37 may, for example, comprise a cured epoxy resin laminate.The filling body 19, 25 may comprise a flexible foam or an elastic foam.
[0074] Figure 3 and Figure 4 The diagram shows the conventional method ( Figure 3 ) and according to an embodiment of the present invention ( Figure 4 ) during manufacturing. The abscissa 53 represents time, while the ordinate 55 represents temperature. Curve 57 shows the temperature distribution of the hot spot. Curve 59 shows the temperature distribution of the thick laminate, curve 61 shows the temperature distribution of the thin laminate, and curve 63 shows the temperature distribution of the overlap of the precast parts.
[0075] As from Figure 4 and Figure 3 can be obtained from the comparison of Figure 1 and Figure 2 When phase change material is used at the region 23a, 23b shown in FIG, the temperature of the hot spot is significantly reduced. In addition, when the phase change material is placed at the second region (eg, second region 31a, 31b, 31c), the precast part overlap as shown by curve 63 has an increased temperature.
[0076] Thus, the temperature decreases in the hot spot area and increases in the cold spot area, thereby enhancing the cross-linking reaction without overheating, thereby avoiding damage to equipment such as the filling body.
[0077] It should be noted that the term "comprising" does not exclude other elements or steps, and "a" or "an" does not exclude a plurality. Moreover, elements associated with different embodiments may be combined. It should also be noted that the reference numerals in the claims should not be interpreted as limiting the scope of the claims.
Claims
1. A method for manufacturing a rotor blade (1) for a wind turbine, the method comprising: placing a fibrous material (11) on a shape forming surface (9); A phase change material (21) in a first state is provided at at least one predetermined first region (23a, 23b), and a phase change material (29) in a second state is provided at at least one predetermined second region (31a, 31b, 31c); impregnating the fiber material (11) to be in thermal contact with the phase change material at the predetermined first region (23a, 23b) and the predetermined second region (31a, 31b, 31c) with a resin (13); During the cross-linking reaction for cross-linking the resin: absorbing heat generated in the resin by the phase change material at the predetermined first region (23a, 23b); and Heat from the phase change material is released toward the resin at the predetermined second region (31a, 31b, 31c).
2. The method of claim 1, wherein the first state allows absorption of heat and comprises a solid phase or a first crystalline phase of a phase change material, The second state allows release of heat and includes a liquid phase or a second crystalline phase of the phase change material.
3. Method according to claim 1 or 2, wherein the shape forming surface is provided by a first mould (5) and defines the shape of the suction side (17) or the pressure side (15) of the rotor blade (1).
4. The method according to claim 1 or 2, further comprising: A filling body (19) is arranged at the fibrous material (11) on the shape forming surface (9), wherein the phase change material is arranged close to and / or at least partially embedded in the filling body (19) and / or at least partially adhered to the filling body.
5. The method according to claim 4, wherein the filling body (19) is in contact with an inner part of a fiber material and / or resin substantially forming a suction side or pressure side half and / or forming a leading edge (14) or a trailing edge (16) of the rotor blade (1).
6. The method according to claim 4, further comprising: A further filling body (25) is arranged at the fibrous material (11) on the shape forming surface (9), wherein the phase change material is arranged close to and / or at least partially embedded in the further filling body (25) and / or at least partially adhered to the further filling body.
7. The method according to claim 6, wherein the further filling body (25) is in contact with an inner part of the fiber material (11) and / or the resin (13) which substantially forms half of the pressure side (15) or suction side (17) and / or forms the trailing edge (16) or leading edge (14) of the rotor blade (1).
8. The method according to claim 6 or 7, further comprising forming a reinforcing web (27) which eventually connects the suction side (17) and the pressure side (15) of the rotor blade (1) inside the completed rotor blade by: A precast web portion (37) is arranged in a root section (39) between the filling body (19) and the further filling body (25); arranging the fiber material (11) in the center-to-tip section (41) between the filling body (19) and the further filling body (25), The fiber material (11) in the center-to-tip section (41) between the filling body (19) and the other filling body (25) is impregnated with a resin (13) and cross-linked.
9. The method according to claim 8, wherein the filling body (19) comprises at least one predetermined first area (23a, 23b, 23c) for mounting the phase change material (21) in the first state, and / or wherein the filling body comprises at least one predetermined second region (31c, 31b) for mounting the phase change material (29) in the second state, and / or wherein the further filling body (25) comprises at least one further predetermined first region (23b, 23c, 23d) for mounting the phase change material (21) in the first state, and / or The further filling body (25) comprises at least one further predetermined second region (31a, 31b) for mounting the phase change material (29) in the second state.
10. The method according to claim 9, wherein the predetermined first area (23a, 23d, 23b, 23c) is located at and / or near at least one of the following: The fiber material and resin finally form at least the central portion of the reinforcing web (27); The fiber material and the resin ultimately form at least a central portion of the pressure side (15) and / or the suction side (17) of the rotor blade.
11. The method according to claim 10, wherein the predetermined second area (31a, 31c, 31b) is located at and / or near at least one of the following: a tip side end portion of the precast web portion (37) in the central portion of the blade; The root end (43) of the filling body (19) and / or another filling body (25).
12. The method according to claim 11, wherein the predetermined first area and / or the predetermined second area of the filling body and / or the further filling body allows for reversible installation of the phase change material at the respective filling body (19, 25), Wherein the phase change material is contained in at least one bag.
13. The method according to claim 6 or 7, further comprising: providing a further shape-forming surface (45) on which the fiber material (11) is placed, onto the filling body (19) and / or the further filling body (25); connecting an edge (51) of the shape forming surface (9) to an edge (49) of the further shape forming surface (45) so as to enclose the filling body (19) and / or the further filling body (25) and the fibrous material on and / or around the shape forming surface (9) and the further shape forming surface (45); Resin (13) is supplied to the encapsulated fiber material.
14. The method according to claim 1 or 2, wherein the phase change material (21) at the at least one predetermined first region at least partially transforms from the first state to the second state during the cross-linking reaction, and / or wherein the phase change material (29) at the at least one predetermined second region at least partially transforms from the second state to the first state during the cross-linking reaction.
15. The method according to claim 6 or 7, further comprising: After completion of the cross-linking reaction: removing the filling body (19) and / or the further filling body (25) from the interior of the rotor blade and removing the cured resin from the root portion of the rotor blade; Removing the phase change material (21, 29) at least in a predetermined first area and / or at least in a predetermined second area from the filling body and / or the further filling body; To manufacture another rotor blade: installing a phase change material obtained from the predetermined second region at the predetermined first region; and / or A phase change material taken from the predetermined first region is installed at the predetermined second region.
16. The method of claim 2, wherein the solid phase is a crystalline phase.
17. The method of claim 4, wherein the filling body (19) comprises a flexible foam.
18. The method according to claim 4, further comprising: A fibrous material is arranged at least partially around the filling body (19).
19. The method according to claim 6, further comprising: A fibrous material is arranged at least partially around the further filling body (25).
20. The method of claim 7, wherein substantially the entire interior space of the rotor blade is filled by the filling body and the further filling body and the fiber material and the resin.
21. The method according to claim 9, wherein the at least one predetermined first region (23a, 23b, 23c) is a first groove, and / or wherein the at least one predetermined second region (31c, 31b) is a second groove, and / or The at least one further predetermined first region (23b, 23c, 23d) is another first groove, and / or the at least one further predetermined second region (31a, 31b) is another second groove.
22. The method of claim 11, wherein the tip-side end portion extends from a blade inner portion of the suction side to a blade inner portion of the pressure side.
23. The method of claim 12, wherein the phase change material is mounted using an elastic material and / or an adhesive tape.
24. The method of claim 12, wherein the phase change material is contained in a plurality of bags.
25. The method of claim 13, further comprising: Resin (13) is supplied to the encapsulated fiber material with vacuum assistance.
26. The method of claim 13, wherein the another shape forming surface defines a shape of a pressure side or a suction side of the rotor blade.
27. The method of claim 13, further comprising: Heat is applied externally to initiate and / or accompany the cross-linking reaction of the resin.
Citation Information
Patent Citations
Method for manufacturing windmill blades
EP1310351A1
Process for producing wind power plant rotor blades and for producing a mould core therefor
EP2897791A2
Method for Manufacturing a Wind Turbine Rotor Blade and Wind Turbine Rotor Blade
US20110274553A1
Inflatable dorn
US8919754B2
Method and apparatus for casting molten materials using phase-change material
WO2003000623A1