A method for preparing aerosol generating matrix rod with high porosity by spraying
Through spray sizing technology, only the binder is sprayed on the top of the tobacco particles in heated cigarettes, which solves the problems of poor fixation and low porosity of bulk smoking particles, and achieves high porosity and smooth aerosol release.
Patent Information
- Application Number
- CN202111447294.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-30
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2041-11-30
AI Technical Summary
In the existing heating cigarette preparation method, the bulk smoke particles cannot be fixed, resulting in low production efficiency and high defective rate. In addition, too much binder leads to low porosity and high smoking resistance, and uneven dispersion of the binder leads to smoke generation. Particles are scattered, affecting aerosol release.
Using the spray sizing method, the binder is evenly sprayed on the top of the tobacco particles to ensure that only the top is glued, and the bottom and sides are not glued. An aerosol-generating matrix rod with high porosity is formed through spray preparation to ensure that the tobacco particles are Adhesive and smooth aerosol release.
It achieves high porosity and axial ventilation of the cigarette core rod, reduces the suction resistance, and ensures the aerosol release effect and production efficiency.
Smart Images

Figure CN114098148B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of heat-not-burn cigarettes, and in particular to a method for preparing an aerosol-generating matrix rod with high porosity by spraying. Background Art
[0002] As consumers pay more attention to health issues and demand more personalized experience in cigarette products, the tobacco industry continues to respond to the upgrading of consumer demand and develop various smoking products with reduced tar and harm. Among them, heated cigarettes are different from traditional cigarette products in that they are heated in a way that satisfies consumers' sensory needs for cigarette products while providing a healthier smoking experience.
[0003] The smoking material of granular heated cigarettes is bulk smoking particles. In the prior art, since the bulk smoking particles cannot be fixed, they must be filled into the outer tube by filling, and the particles need to be fixed on both sides of the smoking particle segment by means of sealing paper and sealing parts, resulting in low production efficiency and high defective rate.
[0004] First, on this basis, the present invention bonds the bulk smoke particles together with an adhesive to form a cylindrical cigarette core rod, and then after the cigarette core rod is wrapped with cigarette paper, it is used alone as an aerosol generating matrix rod, and then it is combined with other components to produce an aerosol generating product through a filling, rolling or compounding process. Since this smoking segment is already an integral cylindrical cigarette core rod, there will be no problem of smoke particles falling and scattering, so there is no need to set sealing films or blocking parts on both sides of the smoking segment. In addition, it is not limited to the filling form to combine it with other components to produce an aerosol generating product.
[0005] At present, the method of preparing a cylindrical cigarette core rod by bonding scattered smoke particles with hot melt adhesive is to directly put the scattered tobacco particles into a blender, add a large amount of adhesive into the blender, and then stir and mix them evenly, then extrude and cool them. The problems with the cigarette core rod prepared by this method are: 1. Since a large amount of adhesive is added during the stirring process, after cooling, there is adhesive in the gaps between adjacent tobacco particles in the cigarette core rod, which leads to low porosity of the cigarette core rod, small axial air permeability, and large suction resistance; 2. If less adhesive is added directly during the stirring and mixing process in order to avoid the first problem, it will lead to uneven dispersion of the adhesive, and there will be no adjacent tobacco particles with adhesive on the surface, resulting in the problem of failure to bond, and the problem of scattered smoke particles; 3. Another more critical problem is that the addition of a large amount of adhesive will also result in a large amount of adhesive being applied to the surface of each tobacco particle, thereby seriously affecting the release of aerosol after the tobacco particles are heated. In fact, in essence, the purpose of gluing is only to allow the scattered tobacco particles to bond, but it is not hoped that the places where the tobacco particles are not bonded are also glued, which affects the aerosol release.
[0006] Therefore, how to ensure that the surface where tobacco particles are bonded to each other has adhesive, while the surface where they are not bonded has no hot melt adhesive, is the key to ensuring the porosity and smoke volume of the cigarette core rod.
[0007] In order to solve the above problems, the present invention is proposed. Summary of the invention
[0008] The present invention adopts a spraying gluing method, and the adhesive is directly sprayed evenly to the top of the tobacco particles from a spray head on the top of the tobacco particles, so that it can be ensured that only the top of the tobacco particles is glued, while the bottom and side surfaces are not glued. On the basis of achieving adhesion, the release of aerosols after the tobacco particles are heated is guaranteed, and the smoke volume and the axial ventilation volume and porosity of the cigarette core rod are guaranteed.
[0009] The first aspect of the present invention provides a method for preparing an aerosol generating matrix rod having a high porosity by spraying, characterized in that it comprises the following steps:
[0010] (1) taking tobacco particles and spreading them on a sizing plate so that at least a portion of the sizing plate contains at least two layers of tobacco particles;
[0011] (2) spraying the adhesive evenly onto the top of the tobacco particles through a spray head above the sizing plate, so that the top of the surface tobacco particles are sizing, while the bottom tobacco particles are not sizing;
[0012] (3) Finally, the sized tobacco particles and the unsized tobacco particles are mixed evenly and extruded, and after cooling, they are wrapped with anti-seepage / thermal conductive paper to obtain an aerosol generating matrix rod, wherein the gaps between the tobacco particles in the aerosol generating matrix rod form an air flow channel axially penetrating the aerosol generating matrix rod.
[0013] Preferably, the mass ratio of tobacco particles to binder is 2:1-10:1, more preferably, the mass ratio of tobacco particles to binder is 3:1.
[0014] Preferably, in step (1), at least 70-100% of the area on the sizing board contains at least two layers of tobacco particles, and more preferably, at least 90% of the area on the sizing board contains at least two layers of tobacco particles.
[0015] Preferably, in step (2), the area of the top of the tobacco particles coated with glue accounts for 20-40% of the surface area of the tobacco particles. That is, the sized tobacco particles are only coated with glue on the top, and the sides and bottom are not coated with glue.
[0016] Preferably, in step (3), the mass ratio of the unsized tobacco particles to the sized tobacco particles is 1:1-5:1, and more preferably, the mass ratio of the unsized tobacco particles to the sized tobacco particles is 3:1.
[0017] Preferably, the porosity of the aerosol generating matrix rod is 40-80%, and more preferably, the porosity of the aerosol generating matrix rod is 80%.
[0018] Preferably, the axial suction resistance of the aerosol generating matrix rod is 5-40 Pa / mm, and more preferably, the axial suction resistance of the aerosol generating matrix rod is 10 Pa / mm.
[0019] Preferably, the weight of the anti-seepage / thermal conductive paper is 30-70 g / m 2 More preferably, the weight of the anti-seepage / thermal conductive paper is 60 g / m 2 .
[0020] Preferably, the particle size of the tobacco particles is 8-60 meshes, more preferably, the particle size of the tobacco particles is 20-30 meshes.
[0021] Preferably, the binder is selected from but not limited to chitosan, hydroxyethylated composite modified ethyl cellulose, guar gum, carboxymethyl cellulose, starches, modified starches, plant celluloses, microcrystalline cellulose, hydroxyethyl cellulose, hydroxyethyl methyl cellulose.
[0022] The second aspect of the present invention provides an aerosol generating matrix rod with high porosity prepared by the method for preparing an aerosol generating matrix rod with high porosity by spraying as described in the first aspect of the present invention.
[0023] The anti-seepage / thermal conductive paper of the present invention has an anti-seepage / thermal conductive layer with anti-seepage or thermal conductive function, and the anti-seepage / thermal conductive layer includes a waterproof layer and / or an oil-proof layer and / or a thermal conductive layer;
[0024] The waterproof layer is made of alkyl ketene dimer AKD, cationic rosin glue or iron-free aluminum sulfate mixed, paraffin material; the oil-proof layer is made of fluorocarbon organic matter, modified starch, AKD and paraffin mixture, AKD and modified starch mixture material. The heat-conducting layer is selected from but not limited to the aluminum foil layer, which is added to the inner wall of the cigarette paper tube by pasting; the aluminum foil layer can play the role of waterproof and / or oil-proof, and at the same time, the aluminum foil layer also has the role of heat conduction and heat preservation, so that the smoking material on the inner wall of the cigarette is evenly heated.
[0025] Preferably, the waterproof layer and / or oil-proof layer is coated on the inner wall of the cigarette paper tube by spraying.
[0026] During the storage of cigarettes, the moisture in the smoking material seeps to the outside of the cigarette paper tube, causing yellow spots, so it is necessary to add a waterproof layer to the inner wall of the cigarette paper tube filled with the smoking material. The waterproof layer is made of alkyl ketene dimer AKD, cationic rosin glue or iron-free aluminum sulfate mixed with paraffin material, which can prevent the moisture in the smoking material from seeping to the outside of the cigarette paper tube.
[0027] Similarly, smoking materials will be added with smoking agents, flavors and fragrances. During long-term storage, the smoking agents in the smoking materials will carry the flavors and fragrances to penetrate the outer side of the paper tube, resulting in yellow spots and affecting the appearance of the paper tube. Since the smoking agents are oily, it is necessary to add an oil-proof layer to the inner wall of the cigarette paper tube filled with smoking materials. The oil-proof layer uses a mixture of fluorocarbon organic matter, modified starch, AKD and paraffin, and a mixture of AKD and modified starch, which can prevent the smoking agents in the smoking materials from carrying flavors and fragrances to penetrate the outer wall of the paper tube and prevent the generation of yellow spots.
[0028] Compared with the prior art, the present invention has the following beneficial effects:
[0029] 1. The present invention adopts a spraying gluing method, and the adhesive is directly sprayed from the spray head on the top of the tobacco particles evenly to the top of the tobacco particles, so that it can be ensured that only the top of the tobacco particles is glued, while the bottom and side surfaces are not glued, and the area of the top of the tobacco particles glued accounts for 20-40% of the surface area of the tobacco particles. After stirring evenly, at least one of the two adjacent tobacco particles has glue on the partial surface area, and bonding can be achieved. Similarly, since the bottom and side surfaces of the tobacco particles are not glued, the release of aerosol after the tobacco particles are heated can be well guaranteed to ensure the amount of smoke.
[0030] 2. The tobacco particles of the present invention are directly spread on the sizing plate, and are not spread thinly on the sizing plate, but at least part of the area on the sizing plate contains at least two layers of tobacco particles. This further ensures that only part of the surface of some tobacco particles is glued. In essence, during the bonding process, when two tobacco particles are in contact, as long as there is glue on one of the surfaces, the two can be bonded, without the need for both particles to have glue on them. This can avoid the adhesive in the gap formed between the two particles after bonding, blocking the pores after cooling, and ensure the axial ventilation and porosity of the cigarette core rod. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 Schematic diagram of the spray sizing process in the process of preparing aerosol generating matrix rods with high porosity by spraying;
[0032] Figure 2 Schematic diagram of the high-porosity aerosol generating matrix rod structure.
[0033] The names of the figure labels in the figure description are: 1-gluing plate, 2-spraying device, 3-sprayed hot melt adhesive, 4-tobacco particles, 5-aerosol generating matrix rod, 6-air flow channel, 41-glued tobacco particles, 42-unglued tobacco particles. DETAILED DESCRIPTION
[0034] The present invention is further described in detail below in conjunction with the embodiments and drawings. The embodiments are only intended to illustrate the present invention, but not to limit the present invention.
[0035] Comparative Example 1
[0036] Directly put the scattered tobacco particles into the blender, add a large amount of binder into the blender, then stir and mix evenly, extrude and cool.
[0037] The surface of the smoke-generating particles in the aerosol generating matrix rod finally obtained is almost 100% coated with glue, the porosity is less than 30% after measurement, and the axial suction resistance is as high as 100 Pa / mm.
[0038] Example 1
[0039] This embodiment is a method for preparing an aerosol generating matrix rod with high porosity by spraying, which comprises the following steps:
[0040] (1) taking tobacco particles and spreading them on a sizing plate 1 so that at least a portion of the sizing plate contains at least two layers of tobacco particles 4;
[0041] (2) spraying the adhesive 3 evenly onto the top of the tobacco particles through a spray head (spraying device) 2 above the glue-applying plate, so that the top of the surface tobacco particles is glued, while the bottom tobacco particles are not glued;
[0042] (3) Finally, the sized tobacco particles 41 and the unsized tobacco particles 42 are mixed evenly and then extruded. After cooling, they are wrapped with anti-seepage / heat-conducting paper to obtain an aerosol generating matrix rod 5.
[0043] The mass ratio of tobacco particles to adhesive is 3:1. In step (1), at least 90% of the area on the sizing plate contains at least two layers of tobacco particles. In step (2), the area of the top of the tobacco particles sizing accounts for 30% of the surface area of the tobacco particles. In other words, the sizing tobacco particles are only sizing on the top, and the sides and bottom are not sizing. In step (3), the mass ratio of unsizing tobacco particles to sizing tobacco particles is 3:1. The gram weight of the anti-seepage / thermal conductive paper is 60g / m 2 The particle size of the tobacco particles is 20-30 meshes. The binder is selected from carboxymethyl cellulose.
[0044] After measurement, the axial suction resistance in the aerosol generating matrix rod finally obtained is 10 Pa / mm. The aerosol generating matrix rod 5 includes an air flow channel axially penetrating the aerosol generating matrix rod 5, and the porosity of the aerosol generating matrix rod 5 is 80%.
Claims
1. A method for preparing an aerosol generating matrix rod having a high porosity by spraying, characterized in that: It includes the following steps: (1) taking tobacco particles and spreading them on a sizing plate so that at least a portion of the sizing plate contains at least two layers of tobacco particles; (2) spraying the adhesive evenly onto the top of the tobacco particles through a spray head above the sizing plate, so that the top of the surface tobacco particles are sizing, while the bottom tobacco particles are not sizing; (3) finally, the sized tobacco particles and the unsized tobacco particles are mixed and extruded, and after cooling, they are wrapped with anti-seepage / heat-conducting paper to obtain an aerosol generating matrix rod, wherein the gaps between the tobacco particles in the aerosol generating matrix rod form an airflow channel axially penetrating the aerosol generating matrix rod; In step (1), at least 70-100% of the area on the sizing plate contains at least two layers of tobacco particles; In step (2), the area of the top of the tobacco particles coated with glue accounts for 20-40% of the surface area of the tobacco particles; The particle size of tobacco particles is 8-60 mesh.
2. The method for preparing an aerosol generating matrix rod having a high porosity by spraying according to claim 1, characterized in that: The mass ratio of tobacco particles to binder is 2:1-10:
1.
3. The method for preparing an aerosol generating matrix rod having a high porosity by spraying according to claim 1, characterized in that: In step (3), the mass ratio of the unsized tobacco particles to the sized tobacco particles is 1:1-5:
1.
4. The method for preparing an aerosol generating matrix rod having a high porosity by spraying according to claim 1, characterized in that: The porosity of the aerosol generating matrix rod is 40-80%.
5. The method for preparing an aerosol generating matrix rod having a high porosity by spraying according to claim 1, characterized in that: The axial suction resistance of the aerosol generating matrix rod is 5-40 Pa / mm.
6. The method for preparing an aerosol generating matrix rod having a high porosity by spraying according to claim 1, characterized in that: The weight of the anti-seepage / thermal conductive paper is 30-70g / m 2 .
7. The method for preparing an aerosol generating matrix rod having a high porosity by spraying according to claim 1, characterized in that: The binder is selected from chitosan, hydroxyethylated composite modified ethyl cellulose, guar gum, carboxymethyl cellulose, starch, modified starch, plant cellulose, microcrystalline cellulose, hydroxyethyl cellulose, and hydroxyethyl methyl cellulose.