A layout structure for improving the surge capability of a discharge tube

By adopting an improved layout structure in the discharge tube and using the design of multiple short-circuit holes and PN junctions, the initial opening area is maximized, which solves the problem of slow conduction speed of the large-page discharge tube, resulting in concentrated burning of current, and significantly improves surge Ability and tolerance.

CN114171515BActive Publication Date: 2024-11-29ANHUI FUXIN MICROELECTRONICS CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202111444182.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-11-30
Publication Date
2024-11-29
Estimated Expiration
2041-11-30

AI Technical Summary

Technical Problem

When the large-panel discharge tube is turned on, due to the small initial conduction area and slow conduction speed, it is easy to form local current concentration, causing the device to overheat and burn, affecting normal use.

Method used

Adopt an improved layout structure, including boron region, adjustment region and emission region. The adjustment region is divided into two parts, the emission region is divided into two parts, and a plurality of short-circuit holes are formed at the edge of the boron region, and PN junction is formed through phosphorus ion implantation. , the length of the adjustment area is adapted to the length of the transmit area to maximize the initial opening area and surge capacity.

Benefits of technology

The di/dt resistance and surge capability of the discharge tube is significantly improved, preventing burn failure caused by the concentration of current at the moment of opening. The surge current that can pass through the 8/20μs waveform is 1.4 times that of the conventional layout structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114171515B_ABST
    Figure CN114171515B_ABST
Patent Text Reader

Abstract

The present invention discloses a layout structure for improving the surge capacity of a discharge tube, comprising a boron region, wherein an adjustment region and an emission region are provided on the boron region, wherein the adjustment region is divided into an adjustment region 1 and an adjustment region 2, wherein the emission region is divided into an emission region 1 and an emission region 2, wherein a plurality of short-circuit holes 1 are provided on the emission region 1, wherein a plurality of short-circuit holes 2 are provided on the emission region 2, wherein the adjustment region 1 is located between the emission region 1 and the emission region 2, and wherein the adjustment region 2 is located at the edge of the boron region adjacent to the emission region 1. The layout structure of the present invention reduces the distance from the adjustment region to the emission region, has a large initial opening area, and will not form local current concentration at the moment of opening to cause overheating and burning. Compared with a traditional single emission region layout structure, the di / dt tolerance and surge capacity of the present invention are significantly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of semiconductor protection devices, and in particular to a layout structure for improving the surge capability of a discharge tube. Background Art

[0002] The discharge tube is a common protective device. Figure 1 This is a conventional large-format discharge tube layout. Its working principle is: when the external voltage reaches the breakdown voltage of the device, the PN junction in the body breaks down to generate a large number of carriers, causing the device to enter the on state, thereby achieving the purpose of discharging current.

[0003] In order to improve the dv / dt tolerance of the discharge tube and prevent false start-up caused by displacement current, the layout structure of the discharge tube will introduce a cathode short-circuit point. When the discharge tube containing the cathode short-circuit point is turned on, not all areas are turned on at the same time. The emission area close to the breakdown PN junction on the layout will be turned on first, and the emission area far from the breakdown PN junction will be turned on later. The discharge tube with a smaller layout has a small flow area and is less affected by this effect. However, for a discharge tube with a large layout, if the surge current passing through the discharge tube is large, due to the small initial conduction area and slow conduction speed, it is easy to form local current concentration, causing the device to overheat and burn, seriously affecting the normal use of the device.

[0004] Therefore, it is necessary to improve the di / dt tolerance of large-format discharge tubes by optimizing the layout structure and thus improve the surge capability. Summary of the invention

[0005] The purpose of the present invention is to provide a layout structure for improving the surge capacity of a discharge tube, so as to improve the di / dt tolerance of a large-format discharge tube, thereby improving the surge capacity and preventing current concentration from occurring at the moment of opening, resulting in burnout and failure.

[0006] The purpose of the present invention can be achieved through the following technical solutions:

[0007] A layout structure for improving the surge capability of a discharge tube, comprising a boron region, wherein an adjustment region and an emission region are provided on the boron region;

[0008] The adjustment area is divided into adjustment area 1 and adjustment area 2;

[0009] The emitting area is divided into an emitting area 1 and an emitting area 2, the emitting area 1 is provided with a plurality of short-circuit holes 1, and the emitting area 2 is provided with a plurality of short-circuit holes 2;

[0010] The adjustment area 1 is located between the emission area 1 and the emission area 2, and the adjustment area 2 is located at the edge of the boron area and adjacent to the emission area 1.

[0011] As a further solution of the present invention: the length of the adjustment zone 1 is adapted to the lengths of the emission zone 1 and the emission zone 2.

[0012] As a further solution of the present invention: the length of the adjustment zone 2 is adapted to the length of the emission zone 1.

[0013] As a further solution of the present invention: the adjustment region 1 forms a first PN junction with the boron region.

[0014] As a further solution of the present invention: the second adjustment region and the boron region form a second PN junction.

[0015] As a further solution of the present invention: the adjustment area 1 and the adjustment area 2 are formed simultaneously by ion implantation.

[0016] As a further solution of the present invention: the implanted element is phosphorus, the implantation dose is 8e13-9e14, and the implantation energy is 60-120keV.

[0017] Beneficial effects of the present invention:

[0018] In the layout structure of the present invention, the emitter area is divided into two parts, the emitter area one and the emitter area two. The adjustment area one is located between the emitter area one and the emitter area two, and the adjustment area two is located at the edge of the boron area close to the emitter area one. That is, when breakdown occurs, the hole current of the first PN junction can flow to the emitter area one and the emitter area two at the same time, and the length of the adjustment area one is equivalent to the lengths of the emitter area one and the emitter area two. In a short time, the opening area of ​​the emitter area one and the emitter area two can reach a large area. At the same time, the hole current of the second PN junction will flow to the part of the emitter area one where no current has flowed yet, which further increases the opening area of ​​the emitter area one, maximizes the initial opening area, and greatly improves the di / dt tolerance and surge capability, effectively preventing current concentration at the moment of opening and causing burning failure. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The present invention will be further described below in conjunction with the accompanying drawings.

[0020] Figure 1 It is a schematic diagram of the structure of a conventional large-format discharge tube layout;

[0021] Figure 2 The present invention is a schematic structural diagram of a layout for improving the surge capability of a discharge tube.

[0022] In the figure: 1, boron region; 2, emitter region 1; 3, adjustment region 1; 4, emitter region 2; 5, adjustment region 2; 6, short-circuit hole 1; 7, short-circuit hole 2; 8, first PN junction; 9, second PN junction. DETAILED DESCRIPTION

[0023] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0024] See also Figure 2 As shown, the present invention is a layout structure for improving the surge capability of a discharge tube, an adjustment area and an emission area are provided on the boron area 1, the adjustment area is divided into an adjustment area 13 and an adjustment area 25, the emission area is divided into an emission area 12 and an emission area 24, a plurality of short-circuit holes 16 are provided on the emission area 12, a plurality of short-circuit holes 27 are provided on the emission area 24, the adjustment area 13 is located between the emission area 12 and the emission area 24, the adjustment area 25 is located at the edge of the boron area 1 adjacent to the emission area 12, the length of the adjustment area 13 is matched with the length of the emission area 12 and the emission area 24, the length of the adjustment area 25 is matched with the length of the emission area 12, the adjustment area 13 forms a first PN junction 8 with the boron area 1, and the adjustment area 25 forms a second PN junction 9 with the boron area 1.

[0025] When in use, the emitter region 1 2, the adjustment region 1 3, the emitter region 2 4, and the adjustment region 2 5 are phosphorus regions, and the emitter region 1 2 and the emitter region 2 4 form an emitter junction with the boron region 1;

[0026] By adjusting the surface concentration of the adjustment area and the junction depth of the first PN junction 8 and the second PN junction 9, the breakdown voltage can be precisely controlled. When the external voltage reaches the breakdown voltage of the first PN junction 8 (the breakdown voltages of the first PN junction 8 and the second PN junction 9 are the same), the first PN junction 8 and the second PN junction 9 undergo avalanche breakdown at the same time, generating a large number of carriers, and the hole current flows through the boron region 1 to the short-circuit hole 1 6 and the short-circuit hole 2 7. When the voltage drop generated by the hole current in the boron region 1 reaches the turn-on voltage of the emitter junction, the emitter junction is forward biased, and a large number of electrons are injected from the emitter region 1 2 and the emitter region 2 4 into the boron region 1, and the discharge tube enters the on state;

[0027] During the start-up process, the hole current first flows to the short-circuit hole close to the adjustment area, which is the fundamental reason for the local concentration of current during the start-up process. In the layout structure of the present scheme for improving the surge capacity of the discharge tube, the emission area is divided into two parts: emission area 1 2 and emission area 2 4. The adjustment area 1 3 is located between the emission area 1 2 and the emission area 2 4, and the adjustment area 2 5 is located at the edge of the boron area 1 close to the emission area 1 2. When breakdown occurs, the hole current of the first PN junction 8 can flow to the emission area 1 2 and the emission area 2 4 at the same time, and the length of the adjustment area 1 3 is equivalent to the length of the emission area 1 2 and the emission area 2 4, so in a short time, the opening area of ​​the emission area 1 2 and the emission area 2 4 can reach a large size. At the same time, the hole current of the second PN junction 9 will flow to the part of the emission area 2 where no current has flowed yet, which further increases the opening area of ​​the emission area 2, maximizes the initial opening area, and greatly improves the di / dt tolerance and surge capacity.

[0028] After tape-out verification, the surge current that the discharge tube using the layout structure of the present invention can pass under the 8 / 20μs waveform is Figure 1 The layout structure shown is 1.4 times that of the discharge tube with the conventional layout structure. In summary, the layout structure provided by the present invention can significantly improve the surge capacity of the discharge tube.

[0029] Among them, the forward and reverse breakdown voltages of the discharge tube using the layout structure in this case are 28-32V.

[0030] The adjustment area 1 3 and the adjustment area 2 5 are formed simultaneously by ion implantation, the implanted element is phosphorus, the implantation dose is 8e13-9e14, and the implantation energy is 60-120keV.

[0031] A manufacturing process of a layout structure for improving the surge capability of a discharge tube comprises the following steps:

[0032] Step 1: Substrate material

[0033] N-type silicon single crystal, resistivity ρ: 30~60Ω·cm, thickness: 230~300μm, double-sided polishing;

[0034] Step 2: Oxidation

[0035] Oxidation temperature 900-1300℃, t=5-10h, oxide layer thickness Tox=1-2μm;

[0036] Step 3: Adjusting the area lithography

[0037] Adopting adjustment area photomask;

[0038] Step 4: Ion Implantation

[0039] Phosphorus is implanted on both sides, the implant dose is 8e13-9e14, the implant energy is 60-120keV, the post-implantation junction temperature is 1100-1300℃, and the junction time is 30-50h;

[0040] Step 5: Boron Diffusion

[0041] S1: Pre-deposition

[0042] T = 900-1100 ° C, t = 1-4h;

[0043] S2: Re-diffusion

[0044] T=1100-1300℃, t=10h-20h, X j =20μm-40μm;

[0045] Step 6: Emission Area Lithography

[0046] Using an emission region photomask;

[0047] Step 7: Phosphorus Diffusion

[0048] S1: Pre-deposition

[0049] T = 900-1100 ° C, t = 1h-2h;

[0050] S2: Re-diffusion

[0051] T = 1000-1200 ° C, t = 1h-4h, X j =10-20μm;

[0052] Step 8: Groove Lithography

[0053] Use slotted version;

[0054] Step 9: Countertop Corrosion

[0055] The etching solution is a mixed solution of nitric acid, hydrofluoric acid and glacial acetic acid, the etching temperature is 5-15°C, the etching time is 3-8min, and the groove depth is 50-70μm;

[0056] Step 10: Passivation

[0057] Use glass passivation and burn glass powder;

[0058] Step 11: Deposition of LTO

[0059] Deposition temperature 400-500℃, deposition time 10-50min, LTO thickness 1000-3000A o ;

[0060] Step 12: Lead hole lithography

[0061] Adopt lead hole version;

[0062] Step 13: Aluminum Steaming

[0063] Aluminum layer thickness δ = 1-4 μm;

[0064] Step 14: Aluminum reverse engraving

[0065] Use metal reverse engraving;

[0066] Step 15: Aluminum Alloy

[0067] Alloy temperature 300-500℃, time 30-90min;

[0068] Step 16: Steaming Ti-Ni-Ag

[0069] Total thickness of Ti-Ni-Ag 1-4μm;

[0070] Step 17: Ti-Ni-Ag reverse etching

[0071] Metal reverse engraving is used.

[0072] The above is a detailed description of an embodiment of the present invention, but the content is only a preferred embodiment of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made within the scope of the present invention should still fall within the scope of the patent coverage of the present invention.

Claims

1. A layout structure for improving the surge capability of a discharge tube, characterized in that: It comprises a boron region (1), wherein an adjustment region and an emission region are formed on the boron region (1); The adjustment area is divided into adjustment area 1 (3) and adjustment area 2 (5); The emitting area is divided into an emitting area 1 (2) and an emitting area 2 (4), the emitting area 1 (2) is provided with a plurality of short-circuit holes 1 (6), and the emitting area 2 (4) is provided with a plurality of short-circuit holes 2 (7); The adjustment region 1 (3) is located between the emission region 1 (2) and the emission region 2 (4), and the adjustment region 2 (5) is located at the edge of the boron region (1) and adjacent to the emission region 1 (2); The length of the adjustment area 1 (3) is equal to the length of the emission area 1 (2) and the emission area 2 (4); The length of the adjustment area 2 (5) is equal to the length of the emission area 1 (2); The adjustment region 1 (3) and the boron region (1) form a first PN junction (8); The second adjustment region (5) and the boron region (1) form a second PN junction (9).

2. A layout structure for improving the surge capability of a discharge tube according to claim 1, characterized in that: The adjustment region 1 (3) and the adjustment region 2 (5) are formed simultaneously by ion implantation.

3. A layout structure for improving the surge capability of a discharge tube according to claim 1, characterized in that: The implanted element is phosphorus, the implantation dose is 8e13-9e14, and the implantation energy is 60-120keV.

4. A manufacturing process of a layout structure for improving the surge capability of a discharge tube as claimed in claim 1, characterized in that: The following steps are involved: Step 1: Substrate material N-type silicon single crystal, resistivity ρ: 30~60Ω·cm, thickness: 230~300μm, double-sided polishing; Step 2: Oxidation Oxidation temperature 900-1300℃, t=5-10h, oxide layer thickness Tox=1-2μm; Step 3: Adjusting the area lithography Adopting adjustment area photomask; Step 4: Ion Implantation Phosphorus is implanted on both sides, the implant dose is 8e13-9e14, the implant energy is 60-120keV, the post-implantation junction temperature is 1100-1300℃, and the junction time is 30-50h; Step 5: Boron Diffusion S1: Pre-deposition T = 900-1100 ° C, t = 1-4h; S2: Re-diffusion T=1100-1300℃、t=10h-20h,X j =20μm-40μm; Step 6: Emission Area Lithography Using an emission region photomask; Step 7: Phosphorus Diffusion S1: Pre-deposition T = 900-1100 ° C, t = 1h-2h; S2: Re-diffusion T=1000-1200℃、t=1h-4h,X j =10-20μm; Step 8: Groove Lithography Use slotted version; Step 9: Countertop Corrosion The etching solution is a mixed solution of nitric acid, hydrofluoric acid and glacial acetic acid, the etching temperature is 5-15°C, the etching time is 3-8min, and the groove depth is 50-70μm; Step 10: Passivation Use glass passivation and burn glass powder; Step 11: Deposition of LTO Deposition temperature 400-500℃, deposition time 10-50min, LTO thickness 1000-3000A o ; Step 12: Lead hole lithography Adopt lead hole version; Step 13: Aluminum Steaming Aluminum layer thickness δ = 1-4 μm; Step 14: Aluminum reverse engraving Use metal reverse engraving; Step 15: Aluminum Alloy Alloy temperature 300-500℃, time 30-90min; Step 16: Steaming Ti-Ni-Ag Ti-Ni-Ag thickness 1-4μm; Step 17: Ti-Ni-Ag reverse etching Metal reverse engraving is used.

Citation Information

Patent Citations

  • Semiconductor device

    CN104916670A

  • Miniature ultra-low capacitance solid discharge tube and manufacturing method thereof

    CN110783399A