An organic compound containing xanthone and triazine structure and its application

By using organic compounds containing xanthone and triazine structures in OLED devices, the problem of efficiency and life lag of TADF materials in OLED devices is solved, achieving higher efficiency and longer life, especially at high temperatures. It is stable under various conditions and has broad industrial application prospects.

CN114249715BActive Publication Date: 2024-10-11JIANGSU SUNERA TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011023672.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-09-25
Publication Date
2024-10-11
Estimated Expiration
2040-09-25

AI Technical Summary

Technical Problem

The efficiency and lifespan of existing TADF materials lag behind in the commercialization process of OLED devices, making it difficult to meet industry needs.

Method used

Organic compounds containing xanthone and triazine structures are used as light-emitting layer materials. By optimizing the device structure, the efficiency and life of the OLED device are improved, especially the stability under high temperature conditions.

Benefits of technology

It effectively improves the current efficiency, power efficiency and external quantum efficiency of OLED devices, significantly increases the device life, especially the stability and life at high temperatures, and has good industrialization prospects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114249715B_ABST
    Figure CN114249715B_ABST
Patent Text Reader

Abstract

The invention discloses an organic compound containing a structure of xanthone and triazine, belonging to the field of semiconductor technology; the structure of the organic compound is shown in general formula (1); the compound of the invention contains a structure of xanthone and triazine, has a high glass transition temperature and molecular thermal stability, suitable HOMO, LUMO energy levels and T1 energy levels, high chemical bond energy and excited state reorganization energy, and high carrier mobility, and can effectively improve the efficiency of OLED devices through device structure optimization, reduce the voltage of OLED devices, and improve the life of OLED devices, especially improve the high temperature life of OLED devices.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of organic photoelectric materials, and relates to an organic compound containing xanthone and triazine structures and use thereof as an organic light-emitting functional material, and an organic electroluminescent device having a light-emitting layer containing such a structural material. Background Art

[0002] Organic light emitting diode (OLED) device technology can be used to manufacture new display products as well as new lighting products. It is expected to replace existing liquid crystal displays and fluorescent lighting, and has a wide range of applications. OLED light-emitting devices are like sandwich structures, including electrode material films and organic functional materials sandwiched between different electrode film layers. Various functional materials are superimposed on each other according to their uses to form OLED light-emitting devices. As a current device, when voltage is applied to the electrodes at both ends of the OLED light-emitting device and the electric field acts on the positive and negative charges in the organic layer functional material film layer, the positive and negative charges are further compounded in the light-emitting layer, generating OLED electroluminescence.

[0003] The development and use of OLED light-emitting layer materials have gone through three major stages. The first stage is mainly based on the fluorescent luminescence mechanism, the second stage is mainly based on the phosphorescent luminescence mechanism, and the third stage uses TADF materials as light-emitting layer materials, effectively utilizing triplet excitons to improve the luminescence efficiency of the device. TADF materials have been developed to date and have a wide range of applications in the light-emitting layer. They have controllable structures, stable properties, low prices, and do not require precious metals. They have broad application prospects in the field of OLEDs.

[0004] As far as the actual needs of the current OLED display lighting industry are concerned, the development of TADF materials is far from enough, and a lot of manpower and material resources are still needed to solve the problem of lagging efficiency and lifespan development encountered in the commercialization process of such materials. Summary of the invention

[0005] In view of the problems existing in the prior art, the present invention provides an organic compound containing a xanthone combined with a triazine structure and its application. The compound of the present invention contains a structure of xanthone connected to a triazine, has a high glass transition temperature and molecular thermal stability, suitable HOMO, LUMO energy levels and T1 energy levels, high chemical bond energy and excited state reorganization energy, and high carrier mobility, and can effectively improve the efficiency of OLED devices through device structure optimization, reduce the voltage of OLED devices, and improve the life of OLED devices, especially improve the high temperature life of OLED devices.

[0006] An organic compound containing a xanthone and a triazine structure, wherein the structure of the organic compound is shown in the general formula (1)

[0007]

[0008] Z represents CR;

[0009] L1 and L2 are independently a single bond, a substituted or unsubstituted C 6-30 arylene, substituted or unsubstituted C 2-30 One of the heteroaryl groups;

[0010] Ar represents C 6-30 The aromatic group, C 2-30 A heteroaryl group, a structure represented by the general formula (2) or the general formula (3):

[0011]

[0012] X represents an oxygen atom, a sulfur atom, N-R1 or C(R2)(R3);

[0013] Each occurrence of R is the same or different and represents a hydrogen atom, a halogen atom, a deuterium atom, a cyano group, a C 1-10 Alkyl, C 6-30 The aromatic group, C 2-30 Two adjacent R groups on the same aromatic ring can also be bonded to form a substituted or unsubstituted C 2-30 Heteroaryl, substituted or unsubstituted C 6-30 Any of the aromatic groups of

[0014] R1, R2, and R3 are independently represented by C 1-10 Alkyl or C 6-30 R2 and R3 can also be connected to form a 4-membered, 5-membered or 6-membered ring;

[0015] The substituents for the substituent groups are selected from deuterium, tritium, hydroxyl, cyano, amine, C 1-10 Alkyl, deuterium or tritium substituted C 1-10 Alkyl, C 6-30 Aryl, deuterium or tritium substituted C 6-30 The aromatic group, C 2-30 heteroaryl, deuterium or tritium substituted C 2-30 Any one of the heteroaryl groups.

[0016] In a preferred embodiment, L1 and L2 are independently represented by a single bond, a substituted or unsubstituted phenylene, a substituted or unsubstituted biphenylene, a substituted or unsubstituted terphenylene, a substituted or unsubstituted naphthylene, a substituted or unsubstituted phenanthrenylene, a substituted or unsubstituted triphenylene, a substituted or unsubstituted pyridylene, a substituted or unsubstituted pyrimidylene, a substituted or unsubstituted quinolylene, a substituted or unsubstituted imidazolylene, a substituted or unsubstituted thiazolylene, a substituted or unsubstituted furanylene, a substituted or unsubstituted benzimidazolylene, a substituted or unsubstituted benzophenanthrylene, furanyl, substituted or unsubstituted benzothiazolyl, substituted or unsubstituted carbazolyl, substituted or unsubstituted phenylenecarbazolyl, substituted or unsubstituted dibenzofuranyl; the substituent for the substituted group is selected from any one of deuterium, tritium, methyl, ethyl, propyl, isopropyl, n-butyl, isobutyl, sec-butyl, tert-butyl, pentyl, phenyl, diphenyl, terphenyl, naphthyl, phenanthrenyl, triphenylene, pyridyl, pyrimidinyl, quinolyl, imidazolyl, thiazolyl, furanyl, benzimidazolyl, benzofuranyl, benzothiazolyl, carbazolyl, phenylcarbazolyl, and dibenzofuranyl.

[0017] In a preferred embodiment, the general formula (2) is specifically represented by any one of the following structures:

[0018]

[0019] The general formula (3) shown is represented by any of the following structures:

[0020]

[0021] In a preferred embodiment, the structure of the compound is as shown in any one of the general formulas (I-1) to (I-4):

[0022]

[0023] Wherein L1 and L2 are each independently represented by a single bond, a phenylene group or a biphenylene group;

[0024] Wherein Ar represents a hydrogen atom, a phenyl group, a biphenyl group, a naphthyl group, or a structure represented by the general formula (2) or the general formula (3).

[0025] In a preferred embodiment, the specific structure of the compound is any one of the following structures:

[0026]

[0027]

[0028]

[0029]

[0030]

[0031] An organic electroluminescent device comprises an anode and a cathode, and an organic light-emitting functional layer therebetween, wherein the organic light-emitting functional layer contains the organic compound.

[0032] In a preferred embodiment, the main material of the organic light-emitting functional layer contains the organic compound.

[0033] In a preferred embodiment, the guest material of the organic light-emitting functional layer contains the organic compound.

[0034] Compared with the prior art, the beneficial technical effects of the present invention are:

[0035] The compound of the present invention contains a combination of xanthone connected to triazine, so that the molecule has a suitable LUMO energy level and a degree of conjugated delocalization of the extended acceptor fragment, which not only has a stronger electron transmission ability, but also can effectively reduce the local aggregation of electrons in the process of transmitting electrons, enhance the stability of the structure, and thus effectively improve the life of the device. In addition, the carbon-nitrogen connection of carbazole with the acceptor structure in the structure makes the material have a certain hole bearing capacity. The material of the present invention, as an electronic type main body in the main body of the light-emitting layer, has a certain hole bearing capacity on the basis of mainly transmitting electrons, and can also effectively improve the life of the device.

[0036] The chemical bonds within the molecules of the compound of the present invention all have relatively high bond energy, which can effectively inhibit the decomposition of the molecules under the action of electric field and light, thereby improving the stability of the device.

[0037] After the compound of the present invention is used as an organic electroluminescent functional layer material in an OLED device, the current efficiency, power efficiency and external quantum efficiency of the device are greatly improved; at the same time, the device life is significantly improved, and it has a good application effect in OLED light-emitting devices and has a good industrialization prospect. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 This is a schematic diagram of the structure of an OLED device in which the materials listed in the present invention are applied;

[0039] Among them, 1 is a transparent substrate layer, 2 is an anode layer, 3 is a hole injection layer, 4 is a hole transport layer, 5 is an electron blocking layer, 6 is a light-emitting layer, 7 is a hole blocking layer, 8 is an electron transport layer, 9 is an electron injection layer, 10 is a cathode layer, and 11 is a covering layer. DETAILED DESCRIPTION

[0040] definition

[0041] The C used in this article6-30 Aryl refers to a monovalent group including a carbocyclic aromatic system having 6 to 30 carbon atoms as ring atoms. 6-30 The arylene group refers to a divalent group including a carbocyclic aromatic system having 6 to 30 carbon atoms as ring atoms. 6-30 Non-limiting examples of aryl groups may include phenyl, biphenyl, phenanthrenyl, terphenyl, naphthyl, and the like. 6-30 Non-limiting examples of the arylene group may include phenylene, biphenylene, phenanthrenyl, terphenylene, naphthylene, and the like. 6-30 Aryl and / or C 6-30 When the arylene group includes two or more rings, these rings may be fused to each other.

[0042] The C used in this article 2-30 Heteroaryl, C 2-30 Heteroaryl, heteroaryl with 5 to 30 ring atoms refers to a monovalent group including a carbocyclic aromatic system having at least one heteroatom selected from N, O, P and S and 2 to 30 carbon atoms as ring atoms. The 5-3 yuan heteroaryl used herein refers to a divalent group including a carbocyclic aromatic system having at least one heteroatom selected from N, O, P and S and 3 to 30 carbon atoms as ring atoms. Non-limiting examples of 5-30 yuan heteroaryl can include pyridyl, dibenzofuranyl, benzoxazolyl, bisbenzoxazolyl, carbazolyl, N-phenylcarbazolyl, etc. Non-limiting examples of 5-30 yuan heteroaryl can include divalent groups of the above groups. When 5-30 yuan heteroaryl and 5-30 yuan heteroaryl include two or more rings, these rings can be fused to each other.

[0043] The C used in this article 1-10 The alkyl group refers to a monovalent group including a straight or branched chain alkyl group having 1 to 10 carbon atoms. 1-10 Non-limiting examples of alkyl groups may include methyl, ethyl, propyl, isopropyl, tert-butyl, pentyl.

[0044] I. Synthesis Example

[0045] The raw materials involved in the synthesis examples of the present invention were purchased from China Energy Conservation Wanrun Co., Ltd.

[0046] Example 1 Synthesis of Compound 1

[0047]

[0048] In a three-necked flask, under the protection of nitrogen, add 0.01 mol of intermediate 1 and 0.012 mol of raw material 2-1, 150 mL of toluene, stir evenly, add 0.02 mol of K2CO3 aqueous solution, and finally add 5×10 -5mol of Pd(PPh3)4, heated to 120℃ for 24h, cooled to room temperature naturally after the reaction, filtered, and the filtrate was evaporated under reduced pressure (-0.09MPa, 85℃), and passed through a neutral silica gel column to obtain compound 1. Elemental analysis structure (molecular formula C 40 H 24 N4O2): theoretical value C, 81.07; H, 4.08; N, 9.45; test value: C, 81.08; H, 4.07; N, 9.46. LC-MS: theoretical value 592.19, found value 592.75. 1 HNMR(400MHz,Chloroform-d)δ8.24(d,1H),8.02(s,2H),7.97(dd,1H),7.82–7.77(m,1H),7.74(ddd,1H) ,7.64(dd,2H),7.55(d,1H),7.52–7.41(m,5H),7.41–7.32(m,6H),7.19–7.12(m,3H),7.10–7.04(m,1H).

[0049] The synthesis methods of Examples 2-19 are similar to those of Example 1, except that different intermediates and raw materials are used. The specific intermediates, raw materials and test results used are shown in Table 1 below.

[0050] Table 1

[0051]

[0052]

[0053]

[0054] The NMR of the synthesized materials in the synthesis example table is shown in Table 2 below:

[0055] Table 2

[0056]

[0057] The specific steps for synthesizing the intermediate bodies involved in Table 1 are as follows:

[0058] Synthesis of intermediate 1

[0059]

[0060] In a three-necked flask, under the protection of nitrogen, add 0.01 mol of raw material 1-1, 0.012 mol of raw material 1-2, and 150 mL of toluene and stir to mix. After stirring evenly, add 0.02 mol of K2CO3 aqueous solution, and finally add 5×10 -5mol of Pd(PPh3)4, heated to 120℃ for 24h. After the reaction, naturally cooled to room temperature, filtered, and the filtrate was subjected to reduced pressure rotary evaporation (-0.09MPa, 85℃), and passed through a neutral silica gel column to obtain intermediate 1.

[0061] Synthesis of intermediate 3

[0062]

[0063] In a three-necked flask, under the protection of nitrogen, add 0.01 mol of raw material 3-1, 0.012 mol of raw material 3-2, 150 mL of toluene, stir and mix, add 0.03 mol of sodium tert-butoxide, 5×10 -5 mol of palladium acetate, heated to 120°C, reacted for 24 hours; cooled naturally to room temperature, filtered, the filtrate was subjected to vacuum rotary evaporation (-0.09 MPa, 85°C), and passed through a neutral silica gel column to obtain the target product intermediate 3;

[0064] Synthesis of intermediate 6

[0065]

[0066] In a three-necked flask, under the protection of nitrogen, add 0.012 mol of raw material 6-1, 0.012 mol of raw material 6-2, and 150 mL of toluene, stir and mix, add 0.02 mol of potassium carbonate aqueous solution after stirring evenly, and finally add 5×10 -5 mol of Pd(PPh3)4, heated to 120℃ for 24h, cooled naturally to room temperature, filtered, and the filtrate was subjected to vacuum rotary evaporation (-0.09MPa, 85℃), and passed through a neutral silica gel column to obtain intermediate 6-1;

[0067] In a three-necked flask, under the protection of nitrogen, add 0.012 mol of intermediate 6-1, 0.012 mol of raw material 6-3, and 150 mL of toluene, stir and mix, add 0.02 mol of potassium carbonate aqueous solution after stirring evenly, and finally add 5×10 -5 mol of Pd(PPh3)4, heated to 120℃ for 24h, cooled naturally to room temperature, filtered, and the filtrate was subjected to vacuum rotary evaporation (-0.09MPa, 85℃), and passed through a neutral silica gel column to obtain intermediate 6;

[0068] Synthesis of intermediate 9

[0069]

[0070] In a three-necked flask, under the protection of nitrogen, add 0.012 mol of raw material 9-1, 0.012 mol of raw material 9-2, and 150 mL of toluene and stir to mix. After stirring evenly, add 0.02 mol of potassium carbonate aqueous solution, and finally add 5×10 -5 mol of Pd(PPh3)4, heated to 120℃ for 24h, cooled naturally to room temperature, filtered, and the filtrate was subjected to vacuum rotary evaporation (-0.09MPa, 85℃), and passed through a neutral silica gel column to obtain intermediate 9-1;

[0071] In a three-necked flask, add 0.012 mol of intermediate 9-1, 0.01 mol of raw material 9-3, and 150 mL of toluene under nitrogen protection, stir evenly, then add 0.03 mol of cesium carbonate, 5×10 -5 mol of palladium acetate, heated to 120°C, reacted for 24 hours, and after the reaction was completed, naturally cooled to room temperature, filtered, and the filtrate was subjected to reduced pressure rotary evaporation (-0.09 MPa, 85°C), and passed through a neutral silica gel column to obtain compound intermediate 9;

[0072] The synthesis steps of intermediates 2, 5, and 11 are similar to the synthesis method of intermediate 6, except that different raw materials are used; the synthesis steps of intermediates 4 and 10 are similar to the synthesis steps of intermediate 3, except that different raw materials are used. The synthesis steps of intermediates 7 and 8 are similar to the synthesis steps of intermediate 9, except that different raw materials are used. The raw materials required for the specific synthesis of the intermediates are shown in Table 3 below.

[0073] Table 3

[0074]

[0075]

[0076] II Basic physical property test

[0077] The compounds of the present invention are used in light-emitting devices and can be used as light-emitting layer materials. The compounds prepared in the above embodiments of the present invention were tested for energy level, thermal stability and spectrum, and the test results are shown in Table 4:

[0078] Table 4

[0079] Compound HOMO LUMO Eg T1 Tg(℃) 1 6.12 3.08 3.04 2.8 131.8 5 6.13 3.16 2.97 2.73 133.1 20 6.05 3.01 3.04 2.79 136.1 46 6.21 3.1 3.11 2.96 141.3 49 6.12 3.14 2.98 2.85 142.7 57 6.05 2.98 3.07 2.82 138.6 72 6.07 3.17 2.9 2.74 134.4 86 6.04 2.96 3.08 2.79 133.3 91 6 3.11 2.89 2.84 136.1 101 6.06 3.04 3.02 2.71 143.2 110 6.01 3.19 2.82 2.99 137.3 122 6.18 3.19 2.99 2.98 144.9 137 6.04 2.91 3.13 2.86 130.9 139 6.09 2.93 3.16 2.88 146.8 REF-1 6.18 2.87 3.31 2.76 150 REF-2 6.23 2.95 3.28 2.75 139.2 REF-3 6.15 2.99 3.16 2.77 141.2 REF-4 6.18 3.06 3.12 2.79 136.5

[0080] Note: The triplet energy level T1 is tested by Horiba's Fluorolog-3 series fluorescence spectrometer, and the material testing conditions are 2*10 -5mol / L toluene solution; the highest occupied molecular orbital HOMO energy level is tested by ionization energy test system (IPS-3) in atmospheric environment; Eg is tested by double beam UV-visible spectrophotometer (model: TU-1901); glass transition temperature Tg is measured by differential scanning calorimetry (DSC, DSC204F1 differential scanning calorimeter of NETZSCH, Germany) with a heating rate of 10℃ / min.

[0081] It can be seen from the data in the above table that the organic compound of the present invention has a suitable energy level and a suitable triplet energy, and can be applied to the light-emitting layer of an OLED device as a main body.

[0082] III. Device Preparation Example

[0083] The following describes in detail the application effect of the OLED material synthesized by the present invention in the device through device examples 1-28 and device comparative examples 1-8. The device examples 2-28 of the present invention and device comparative examples 1-8 are completely identical in manufacturing process to device example 1, and the same substrate material and electrode material are used, and the film thickness of the electrode material is also the same, except that the light-emitting layer material in the device is replaced.

[0084] Device Example 1

[0085] like Figure 1As shown, the transparent substrate layer 1 is a transparent PI film, and the anode layer 2 (ITO (15nm) / Ag (150nm) / ITO (15nm)) is washed, that is, the cleaning agent washing (SemiClean M-L20), pure water washing, drying, and then ultraviolet-ozone washing are performed in sequence to remove organic residues on the surface of the anode layer. On the anode layer 2 after the above washing, HT-1 and P-1 are evaporated as the hole injection layer 3 using a vacuum evaporation device, with a film thickness of 10nm, and the mass ratio of HT-1 to P-1 is 97:3. Then HT-1 is evaporated as the hole transport layer 4 with a thickness of 130nm. EB-1 is then evaporated as the electron blocking layer 5 with a thickness of 40nm. After the above-mentioned electron blocking layer material is evaporated, the light-emitting layer 6 of the OLED light-emitting device is manufactured, and its structure includes the compound 1 used in the OLED light-emitting layer 6 as the main material, GD-1 as the doping material, the doping ratio of the doping material is 6% (mass ratio), and the light-emitting layer film thickness is 40nm. After the above-mentioned light-emitting layer 6, HB-1 was vacuum-deposited with a film thickness of 5 nm, which was the hole blocking layer 7. After the above-mentioned hole blocking layer 7, ET-1 and Liq were vacuum-deposited with a mass ratio of ET-1 to Liq of 1:1 and a film thickness of 35 nm, which was the electron transport layer 8. On the electron transport layer 8, a Yb layer with a film thickness of 1 nm was made by a vacuum evaporation device, which was the electron injection layer 9. On the electron injection layer 9, a Mg:Ag electrode layer with a film thickness of 15 nm was made by a vacuum evaporation device, and the mass ratio of Mg to Ag was 1:9, which was used as the cathode layer 10. On the cathode layer 10, CP-1 was vacuum-deposited as the CPL layer 11 with a thickness of 70 nm.

[0086] An organic electroluminescent device 1 is obtained.

[0087]

[0088] After the OLED light-emitting device is completed as described above, the anode and cathode are connected with a known driving circuit, and the voltage, current efficiency, luminescence spectrum and life of the device are measured. The device examples 1-26 and comparative examples 1-8 prepared by the same method are shown in Table 5; the obtained devices have a current of 10 mA / cm 2 Voltage, current efficiency, color and 20mA / cm 2 The test results of LT95 life under the conditions are shown in Table 5.

[0089] Table 5

[0090]

[0091] Note: Voltage, current efficiency and color coordinates are obtained at a current density of 10 mA / cm 2The test was conducted under the following conditions: IVL (current-voltage-luminance) test system (Suzhou Fushida Scientific Instrument Co., Ltd.); the life test system was EAS-62C OLED device life tester from Japan System Technology Co., Ltd.; LT95 refers to the life test under 20mA / cm 2 The time it takes for the device brightness to decay to 95% under the condition of .

[0092] It can be seen from the device data results in Table 5 that, compared with device comparison examples 1-8, the organic light-emitting device of the present invention has a significant improvement in both device efficiency and device life compared with the OLED device of known materials. At the same time, the voltage of the organic light-emitting device of the present invention is lower than that of the OLED device of known materials.

[0093] Furthermore, the OLED device prepared by the present invention has a relatively stable life when working at high temperature, and has a longer high temperature life; device embodiments 15-28 and comparative examples 5-8 were tested for life at 85°C and compared with the life at room temperature, and the results are shown in Table 6.

[0094] Table 6

[0095] serial number Lifespan LT95(Hr) / 25℃ Lifespan LT95(Hr) / 80℃ High temperature life multiplier Device Example 15 231.4 72.3 3.2 Device Example 16 203.9 88.7 2.3 Device Example 17 231.8 100.8 2.3 Device Example 18 209.6 65.5 3.2 Device Example 19 224.5 77.4 2.9 Device Example 20 203.8 65.7 3.1 Device Example 21 213.4 68.8 3.1 Device Example 22 207.3 98.7 2.1 Device Example 23 223.2 74.4 3 Device Example 24 237 112.9 2.1 Device Example 25 225 80.4 2.8 Device Example 26 210.7 78.0 2.7 Device Example 27 217.8 62.2 3.5 Device Example 28 222.5 67.4 3.3 Device Comparison Example 5 102.2 15.7 6.5 Device Comparison Example 6 139.9 26.9 5.2 Device Comparison Example 7 100.3 17.6 5.7 Device Comparison Example 8 117.2 23.0 5.1

[0096] Note: The high temperature life ratio in Table 6 above refers to the ratio of the device life at 25°C to the device life at 80°C; the above device life is at a current density of 20mA / cm 2 Measured under the conditions of .

[0097] As shown in Table 6 above, it can be found that the device using the material of the present application as the electronic body has a longer device life at a higher temperature than the comparative example, and the high temperature life multiple is significantly lower than that of the comparative example, indicating that the device using the material of the present application has better high temperature stability.

[0098] In summary, the above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. An organic compound containing a xanthone and a triazine structure, characterized in that: The structure of the organic compound is:

2. An organic electroluminescent device, comprising an anode and a cathode, and an organic light-emitting functional layer therebetween, characterized in that: The organic light-emitting functional layer contains the organic compound according to claim 1.

3. The organic electroluminescent device according to claim 2, characterized in that: The host material of the organic light-emitting functional layer contains the organic compound according to claim 1.