A method for evaluating the wear performance of railway fastener pads on sleepers

By using fastener pads and sleeper samples for pin disc friction and wear tests, the problem of complex and low efficiency of the evaluation process of the wear performance of railway fastener pads on rail sleepers in the prior art is solved, and more efficient wear performance evaluation is achieved .

CN114279880BActive Publication Date: 2024-11-01RAILWAY CONSTR RES INST OF CHINA ACAD OF RAILWAY SCI CO LTD +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111652258.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-30
Publication Date
2024-11-01
Estimated Expiration
2041-12-30

AI Technical Summary

Technical Problem

When evaluating the wear performance of railway fastener pads on rail sleepers, the workpiece is complicated, the operation is inconvenient, the test cycle is long, and the test efficiency is inefficient.

Method used

The fastener pad sample and prefabricated sleeper sample are used for pin disc friction and wear tests, which simulate the contact pressure and rotation times in actual use scenarios, and the sample loss quality and wear depth are obtained through the wear test to judge the wear performance.

Benefits of technology

It reduces the complexity of the tooling process, shortens the test cycle, improves the testing efficiency, and realizes the operability of quantitative evaluation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114279880B_ABST
    Figure CN114279880B_ABST
Patent Text Reader

Abstract

The present application discloses a method for evaluating the wear performance of railway fastener pads on sleepers, and belongs to the field of rail transit technology. The present application mainly includes: a sample loading process, in which the fastener pad sample and the sleeper sample are respectively fixed on the upper rotating disk and the lower fixed disk of the friction and wear testing machine, and a predetermined pressure is applied to the upper rotating disk; a wear test process, in which the friction and wear testing machine is used to drive the fastener pad sample to rotate a first preset number of times to obtain a worn fastener pad sample; and the pin-disc friction and wear testing machine is continued to be used to drive the worn fastener pad sample to rotate a second preset number of times to obtain a worn sleeper sample; a result evaluation process, based on the loss mass of the worn fastener pad sample and the worn sleeper sample, and / or the wear depth of the worn fastener pad sample and the worn sleeper sample, the evaluation is performed. The present application can reduce the complexity of tooling in the test process, shorten the test cycle, improve the operability of quantitative evaluation, and improve test efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of rail transit technology, and in particular to a method for evaluating the wear performance of a railway fastener pad on a sleeper. Background Art

[0002] In heavy-duty railways and passenger-freight railways, the train axles are heavy and the transport volume is high, so the wheel-rail dynamics are correspondingly enhanced. As key components in the track system, the loads borne by fasteners and sleepers increase accordingly. Especially in small radius curves and steep slopes, the stress state of sleepers and fasteners is even worse. The fastener pad and the sleeper bearing surface will move relative to each other under the wheel-rail dynamics. Figure 1 When the fastener pad itself has high hardness and high contact stress with the sleeper, the fastener pad will cause wear on the sleeper rail surface during the relative movement between the fastener pad and the sleeper rail surface. Figure 2 As shown. It will not only cause structural damage to the sleeper and reduce its service life, but also change the preset rail bottom slope of the sleeper bearing surface, causing the corresponding line gauge to expand and the wheel-rail profile matching position to change, affecting the running state of the train. At the same time, the fastener pad itself will also wear out, resulting in the failure of the fastener pad, such as Figure 3 shown.

[0003] In the prior art, when evaluating the wear performance of fastener pads on sleepers, actual sleepers and fastener pads are used to carry out tests, which not only has complicated tooling and inconvenient operation, but also has a long test cycle and low test efficiency. Summary of the invention

[0004] In response to the problems existing in the prior art, the present application mainly provides a method for evaluating the wear performance of railway fastener pads on sleepers, and uses fastener pad samples and sleeper samples instead of actual sleepers and fastener pads to carry out wear performance tests, thereby reducing the complexity of tooling in the testing process, shortening the test cycle, and improving test efficiency.

[0005] In order to achieve the above-mentioned purpose, a technical solution adopted in the present application is to provide a method for evaluating the wear performance of a railway fastener pad on a sleeper, which comprises:

[0006] During the sample loading process, the fastener pad sample and the prefabricated sleeper sample are respectively fixed on the upper rotating disk and the lower fixed disk of the pin-disc friction and wear testing machine, and a predetermined pressure is applied to the upper rotating disk so that the contact pressure between the fastener pad sample and the sleeper sample is equal to the contact pressure between the fastener pad and the sleeper in the actual use scenario; during the wear test process, the pin-disc friction and wear testing machine is used to drive the fastener pad sample to rotate relative to the sleeper sample for a first preset number of times at a preset speed to obtain a worn fastener pad sample; and the pin-disc friction and wear testing machine is continued to be used to drive the worn fastener pad sample to rotate relative to the sleeper sample for a second preset number of times at a preset speed to obtain a worn sleeper sample; during the result evaluation process, according to the loss mass of the worn fastener pad sample and the worn sleeper sample, and / or the wear depth of the worn fastener pad sample and the worn sleeper sample, it is judged whether the wear performance of the fastener pad sample on the sleeper sample meets the requirements; wherein, the material of the sleeper sample is the same as that of the actual sleeper, and the fastener pad sample is the same as that of the fastener pad.

[0007] The technical solution of the present application can achieve the beneficial effect of: providing a method for evaluating the wear performance of railway fastener pads on sleepers. The present application method uses a fastener pad sample and a sleeper sample to form a pin-disc friction pair for relative rotation friction test, rather than the actual sleeper and fastener pad to carry out wear performance test, thereby reducing the complexity of tooling in the test process, shortening the test cycle, improving the operability of quantitative evaluation, and improving test efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0008] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, a brief introduction will be given below to the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.

[0009] Figure 1 It is a schematic diagram of the relative displacement between the fastener pad and the sleeper in the actual environment;

[0010] Figure 2 It is a schematic diagram of the wear of the sleeper bearing surface in the actual environment;

[0011] Figure 3 It is a schematic diagram of fastener pad wear in actual environment;

[0012] Figure 4 It is a schematic diagram of the prior art using actual fastener pads and actual sleepers to conduct wear performance tests;

[0013] Figure 5It is a flow chart of a specific implementation method of a method for evaluating the wear performance of a railway fastener pad on a sleeper in the present application;

[0014] Figure 6 It is a schematic diagram of a sleeper sample in a specific example of a method for evaluating the wear performance of a railway fastener pad on a sleeper in the present application;

[0015] Figure 7 It is a schematic diagram of a fastener pad in a specific example of a method for evaluating the wear performance of a railway fastener pad on a sleeper in the present application;

[0016] Figure 8 It is a schematic diagram of the installation of a fastener pad sample and a sleeper sample in a specific embodiment of a method for evaluating the wear performance of a railway fastener pad on a sleeper in the present application;

[0017] Fig. 9 It is a schematic diagram of friction force and friction coefficient obtained in a specific embodiment of a method for evaluating the wear performance of a railway fastener pad on a sleeper in the present application.

[0018] The above drawings show clear embodiments of the present disclosure, which will be described in more detail below. These drawings and text descriptions are not intended to limit the scope of the present disclosure in any way, but to illustrate the concepts of the present disclosure to those skilled in the art by referring to specific embodiments. DETAILED DESCRIPTION

[0019] The preferred embodiments of the present application are described in detail below in conjunction with the accompanying drawings so that the advantages and features of the present application can be more easily understood by those skilled in the art, thereby making a clearer and more definite definition of the protection scope of the present application.

[0020] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the statement "include..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.

[0021] In heavy-duty railways and passenger-freight railways, the train axles are heavy and the transport volume is high, so the wheel-rail dynamics are correspondingly enhanced. As key components in the track system, the loads borne by fasteners and sleepers increase accordingly. Especially in small radius curves and steep slopes, the stress state of sleepers and fasteners is even worse. The fastener pad and the sleeper bearing surface will move relative to each other under the wheel-rail dynamics. Figure 1 When the fastener pad itself has high hardness and high contact stress with the sleeper, the fastener pad will cause wear on the sleeper rail surface during the relative movement between the fastener pad and the sleeper rail surface. Figure 2 As shown. It will not only cause structural damage to the sleeper and reduce its service life, but also change the preset rail bottom slope of the sleeper bearing surface, causing the corresponding line gauge to expand and the wheel-rail profile matching position to change, affecting the running state of the train. At the same time, the fastener pad itself will also wear out, resulting in the failure of the fastener pad, such as Figure 3 shown.

[0022] The prior art, such as the method proposed by the American Railway Engineering and Road Maintenance Association (AREMA), includes: (1) applying a test load to the rail head at an angle of 27.5° to the vertical direction, such as Figure 4 As shown, a certain proportion of vertical and lateral load components can be applied to the rail at the same time. In this test, the vertical load is 32,500 pounds (about 144.6 kN) and the lateral load is 16,900 pounds (about 75.2 kN); (2) Before assembling the test fixture, clean the test sleeper bearing surface to ensure that there is no debris when assembling the fasteners; (3) Measure the thickness and static stiffness of each pad at two locations inside and outside the pad; (4) Sprinkle clean dry sand on the bearing surface, assemble the fasteners, and measure the track gauge after installation; (5) Arrange displacement sensors on the rail head and rail bottom. Measure its vertical and lateral displacement relative to the sleeper; (6) Set up a dry ice box and a drip trough around the rail section to ensure that the pad maintains a constant temperature and that the pad and sleeper contact surface remain moist; (7) Perform fatigue tests at least 3 million times at a loading frequency of 2.5 Hz or until failure; (8) Before the damage test is completed, the assembly of the rail fasteners should be checked and photographed for record; (9) After the test is completed, remove the fastener system, re-measure the thickness, static stiffness and gauge expansion of the rail pad, and check the damage of the rail bearing surface and each fastener component. Not only is the tooling complex and the large size inconvenient to operate. In addition, the test is conducted at a frequency of 2.5 Hz, and it takes about 14 days to conduct 3 million tests. In addition, the relative displacement between the sleeper and the fastener pad is small in this test method. After 3 million loadings, the wear of the sleeper is small. Conventional wear test methods such as weighing are difficult to measure and evaluate the wear of the sleeper. If calculated based on the annual transportation volume of a typical heavy-load railway, the number of wheels passing through in a year is more than 15 million. Although increasing the number of loading times can increase the amount of wear, it will also greatly extend the test cycle and reduce the test efficiency.

[0023] This application uses sleeper and pad material samples instead of finished product samples in the original method to carry out tests, and uses pin-disc rotary loading instead of the original reciprocating loading, which accelerates the wear rate and shortens the test cycle; quantitatively describes the wear of pads and sleepers, and proposes corresponding wear assessment standards, and evaluates the friction and wear performance of railway fastener pads on sleepers from the two perspectives of pad wear and sleeper wear.

[0024] The technical solution of the present application is described in detail below with specific embodiments in combination with the accompanying drawings. The following specific embodiments can be combined with each other, and the same or similar concepts or processes may not be described in detail in some embodiments.

[0025] Figure 5 A specific implementation of a method for evaluating the wear performance of a railway fastener pad on a sleeper according to the present application is shown.

[0026] exist Figure 5 In the specific embodiment shown, the method for evaluating the wear performance of the railway fastener pad on the sleeper of the present application includes: a sample loading process S501, respectively fixing the fastener pad sample and the prefabricated sleeper sample on the upper rotating disk and the lower fixed disk of the pin-disc friction and wear testing machine, and applying a predetermined pressure to the upper rotating disk so that the contact pressure between the fastener pad sample and the sleeper sample is equal to the contact pressure between the fastener pad and the sleeper in the actual use scenario; a wear test process S502, using the pin-disc friction and wear testing machine to drive the fastener pad sample to rotate relative to the sleeper sample at a preset speed The worn fastener pad sample is obtained for a first preset number of times; and the pin-on-disc friction and wear testing machine is continued to be used to drive the worn fastener pad sample to rotate relative to the sleeper sample at a preset speed for a second preset number of times to obtain the worn sleeper sample; in the result evaluation process S503, according to the loss mass of the worn fastener pad sample and the worn sleeper sample, and / or the wear depth of the worn fastener pad sample and the worn sleeper sample, it is judged whether the wear performance of the fastener pad sample on the sleeper sample meets the requirements; wherein, the material of the sleeper sample is the same as that of the actual sleeper, and the fastener pad sample is the same as the material of the fastener pad.

[0027] The method of the present application utilizes a pin-disc friction pair composed of a fastener pad specimen and a sleeper specimen to conduct a relative rotational friction test, rather than conducting a wear performance test on actual sleepers and fastener pads, thereby reducing the complexity of tooling in the test process, shortening the test cycle, improving the operability of quantitative evaluation, and improving test efficiency.

[0028] The sample loading process S501 represents the process of respectively fixing the fastener pad sample and the prefabricated sleeper sample on the upper rotating disk and the lower fixed disk of the pin-disc friction and wear testing machine, and applying a predetermined pressure to the upper rotating disk so that the contact pressure between the fastener pad sample and the sleeper sample is equal to the contact pressure between the fastener pad and the sleeper in the actual use scenario. This can facilitate the simulation of the relative position and force conditions of the fastener pad and the sleeper in reality, thereby facilitating subsequent friction and wear tests.

[0029] In an optional specific embodiment of the present application, the sleeper sample is obtained through a sample preparation process, and the sleeper sample having the same strength as the actual sleeper is prepared using the same concrete mix ratio and steel bar configuration as the actual sleeper, for example, a sleeper sample with a strength grade of C60. Specifically, the sleeper sample should be able to prevent surface defects such as cracking, no pores, skin staining, and roughness during the rotational friction test.

[0030] In an optional specific embodiment of the present application, the sample preparation process includes trial-making the fastener pad sample using the same material as the actual fastener pad.

[0031] In an optional specific embodiment of the present application, the fastener pad sample is obtained by cutting the sample from the actual fastener pad. Cutting the sample directly from the actual fastener pad can ensure the consistency of the sample and the actual pad process, and avoid wear performance differences caused by inconsistent processes.

[0032] Optionally, the sleeper specimen can be a regular octagonal flat plate, which is convenient for fixing the sleeper specimen on the pin-disc friction and wear testing machine and avoids the problem that the quadrilateral specimen is easily damaged and lost at the corners. Figure 6 shown.

[0033] In an optional specific embodiment of the present application, the sample preparation process further includes trial-producing the fastener pad sample. Optionally, the fastener pad sample is trial-produced into a hexahedral long pin, the width dimension of which is consistent with the pad thickness, for example, the width and thickness dimensions are 10mm*10mm, and the structure is as follows: Figure 7 shown.

[0034] In an optional specific embodiment of the present application, the number of the above-mentioned fastener pad samples is multiple, and each fastener pad sample can perform a rotational friction motion relative to the sleeper sample along the same trajectory. Using multiple fastener pad samples to perform a rotational friction motion relative to the sleeper sample once is equivalent to performing a rotational friction motion on one sleeper sample multiple times, which increases the amount of wear caused by the fastener pad samples on the sleeper sample and improves the operability of quantitative evaluation.

[0035] In an optional specific example of the present application, the first friction pair includes three fastener pad samples. After being loaded using a pin-on-disc friction and wear tester, the three fastener pad samples are evenly distributed at 120°. Figure 8 shown.

[0036] In an optional specific embodiment of the present application, the rotation radius of the center point of the fastener pad sample relative to the sleeper sample is not greater than a first preset radius, and preferably, the rotation radius is not greater than 30 mm.

[0037] Specifically, the larger the rotation radius of the rotational friction of the center point of the fastener pad sample relative to the sleeper sample, the higher the requirement on the motor, so the rotation radius should not be too large.

[0038] In an optional specific embodiment of the present application, the rotation radius of the center point of the fastener pad sample relative to the sleeper sample is not less than the second preset radius. Preferably, the rotation radius is not less than 15 mm. Specifically, when there are multiple fastener pad samples, if the rotation radius is too small, it is impossible to load the multiple fastener pad samples.

[0039] S502 represents the process of using a pin-on-disc friction and wear testing machine to drive the fastener plate sample to rotate relative to the sleeper sample at a preset speed for a first preset number of times to obtain a worn fastener plate sample; and continuing to use the pin-on-disc friction and wear testing machine to drive the worn fastener plate sample to rotate relative to the sleeper sample at a preset speed for a second preset number of times to obtain a worn sleeper sample. This process can efficiently test the friction performance of the fastener plate material, and facilitates the assessment of whether the fastener plate material meets the wear performance requirements.

[0040] Preferably, the rotation radius of the above-mentioned rotational friction test is 21 mm, the above-mentioned first preset number of times is 50,000 times, and the above-mentioned second preset number of times is 8 million times. Specifically, in a typical high-capacity heavy-load railway line, the pads and sleepers will experience a large degree of wear on the sleepers after they have been in service for half a year. The total number of wheels passing through the typical high-capacity heavy-load railway line within half a year is taken as the maximum number of sliding movements, that is, 8 million times. According to the actual measurement results on site, when the train passes, the maximum relative displacement between the pad and the sleeper bearing surface is about 0.8 mm. According to the rotation radius of the pad sample in this test scheme, each rotation of the pad sample is equivalent to about 160 times. Therefore, in actual applications, the distance of 8 million sliding of the fastener pad is equivalent to the distance of 50,000 relative displacements in the above-mentioned rotational friction test. The present application can greatly reduce the time required for the test.

[0041] In an optional specific embodiment of the present application, in the process of using a pin-on-disc friction and wear testing machine to drive the fastener pad sample to rotate relative to the sleeper sample at a preset speed for a first preset number of times to obtain a worn fastener pad sample, the contact surface between the fastener pad sample and the sleeper sample is a dry friction state environment. In order to make the pad achieve the worst wear effect, the friction pair interface is in a dry friction state during the test.

[0042] In an optional specific embodiment of the present application, in the process of continuing to use the pin-on-disc friction and wear tester to drive the worn fastener pad sample to rotate relative to the sleeper sample for a second preset number of times at a preset speed to obtain the worn sleeper sample, the contact surface between the fastener pad sample and the sleeper sample is a water-cooled environment. In order to achieve the worst wear effect on the sleeper and form the effects of water pressure cracking and water drilling during friction, the test is carried out in a water-cooled environment. In addition, the water-cooled environment can cool the pad sample to avoid excessive wear caused by softening.

[0043] In an optional specific embodiment of the present application, during the above-mentioned wear test process, the temperature of the fastener pad sample is monitored. If the temperature of the fastener pad sample is not lower than the preset first temperature threshold, the wear test process is stopped, and the wear test process is continued when the temperature of the fastener pad sample drops to not higher than the preset second temperature threshold. In this way, it is possible to prevent the fastener pad from softening when the temperature is too high, causing deviation in the test results.

[0044] Optionally, the first temperature threshold is 10 degrees Celsius below the softening temperature of the fastener pad material; and the second temperature threshold is room temperature.

[0045] In an optional specific embodiment of the present application, during the above-mentioned wear test, the friction force between the fastener pad sample and the sleeper sample is calculated according to the torque and the turning radius borne by the lower fixed plate, and the friction coefficient between the fastener pad sample and the sleeper sample is obtained according to the friction force and the pressure, such as Fig. 9 As shown, it is convenient to use the friction coefficient to evaluate whether the material of the fastener pad sample can pass the corresponding wear performance assessment.

[0046] In an optional specific embodiment of the present application, the above-mentioned preset rotation speed is adjustable. By setting the rotation speed to be adjustable, a suitable rotation speed can be selected according to the actual test scenario.

[0047] Optionally, the rotation speed of the upper rotating disk can be adjusted within the range of 0.1 to 3000 r / min. The adjustment is based on ensuring that the temperature of the fastener pad specimen is stable within the range of -40 to 70°C during the test, and the test rotation speed is accelerated as much as possible to shorten the test cycle.

[0048] In an optional specific example of the present application, the above-mentioned first friction pair is set up, and 3 pad material samples are tested. The corresponding sleeper wear frequency is also tripled. Assuming that the rotation speed of the upper rotating disk is 3000r / min, the corresponding sleeper wear loading frequency is 150Hz, which is 60 times the loading frequency of 2.5Hz in the prior art, which can greatly reduce the time required for the test.

[0049] The result evaluation process S503 represents the judgment of whether the wear performance of the fastener plate sample on the sleeper sample meets the requirements based on the loss mass of the worn fastener plate sample and the worn sleeper sample, and / or the wear depth of the worn fastener plate sample and the worn sleeper sample; wherein the sleeper sample is made of the same material as the actual sleeper, and the fastener plate sample is made of the same material as the fastener plate, so it is possible to efficiently and accurately judge whether the material of the fastener plate sample can meet the requirements for the wear performance of the sleeper sample.

[0050] In an optional specific embodiment of the present application, the above-mentioned process of judging whether the wear performance of the fastener plate sample on the sleeper sample meets the requirements based on the loss mass of the worn fastener plate sample and the worn sleeper sample includes: before the sample loading process, weighing the fastener plate sample and the sleeper sample to obtain the original fastener plate sample weight and the original sleeper sample weight; weighing the worn plate sample and the worn sleeper sample to obtain the worn fastener plate sample weight and the worn sleeper sample weight, and subtracting the worn fastener plate sample weight and the worn sleeper sample weight from the original fastener plate sample weight and the original sleeper sample weight to obtain a first weight difference and a second weight difference; if the first weight difference is not greater than the preset first difference threshold, and the second weight difference is not greater than the preset second difference threshold, it is determined that the fastener plate sample has passed the wear performance assessment. The loss mass is obtained by weighing the fastener pad samples and sleeper samples before and after the test and calculating the weight difference. By comparing the loss mass with the corresponding mass loss threshold, it is possible to determine whether the wear performance of the fastener pad sample material can pass the assessment, quantitatively describe the wear amount of the pad and sleeper, and evaluate the friction and wear performance of the railway fastener pad on the sleeper from the two perspectives of pad wear and sleeper wear.

[0051] Optionally, the friction pair needs to be cleaned and dried before each weighing.

[0052] In an optional specific embodiment of the present application, the process of judging whether the wear performance of the fastener pad sample on the sleeper sample meets the requirements based on the wear depth of the worn fastener pad sample and the worn sleeper sample includes measuring the wear depth of the worn fastener pad sample and the wear depth of the worn sleeper sample to obtain a first wear depth and a second wear depth respectively; if the first wear depth is not greater than a preset first wear depth threshold, and the second wear depth is not greater than a preset second wear depth threshold, it is determined that the material of the fastener pad sample passes the wear performance assessment.

[0053] Specifically, due to the uneven quality of concrete, the wear depth is introduced as another parameter of the wear amount.

[0054] Preferably, the first wear depth threshold is 1 mm, and the second wear depth threshold is 2 mm, which provides a standard for wear assessment.

[0055] In an optional specific embodiment of the present application, the above result evaluation process further includes judging whether the wear performance of the fastener pad sample on the sleeper sample meets the requirements based on the friction coefficient and a preset friction coefficient threshold.

[0056] In the several embodiments provided in the present application, it should be understood that the disclosed devices and methods can be implemented in other ways. For example, the device embodiments described above are only schematic. For example, the division of units is only a logical function division. There may be other division methods in actual implementation, such as multiple units or components can be combined or integrated into another system, or some features can be ignored or not executed. Another point is that the mutual coupling or direct coupling or communication connection shown or discussed can be through some interfaces, indirect coupling or communication connection of devices or units, which can be electrical, mechanical or other forms.

[0057] The units described as separate components may or may not be physically separated, and the components shown as units may or may not be physical units, that is, they may be located in one place or distributed on multiple network units. Some or all of the units may be selected according to actual needs to achieve the purpose of the solution of this embodiment.

[0058] The above are merely embodiments of the present application, and are not intended to limit the patent scope of the present application. Any equivalent structural transformations made using the contents of the present application specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present application.

Claims

1. A method for evaluating the wear performance of railway fastener pads on sleepers, characterized in that: include, During the sample loading process, the fastener pad sample and the prefabricated sleeper sample are respectively fixed on the upper rotating disk and the lower fixed disk of the pin-on-disc friction and wear testing machine, and a predetermined pressure is applied to the upper rotating disk so that the contact pressure between the fastener pad sample and the sleeper sample is equal to the contact pressure between the fastener pad and the sleeper in the actual use scenario; During the wear test, the pin-on-disk friction and wear testing machine is used to drive the fastener pad sample to rotate relative to the sleeper sample at a preset speed for a first preset number of times to obtain a worn fastener pad sample; and the pin-on-disk friction and wear testing machine is continued to drive the worn fastener pad sample to rotate relative to the sleeper sample at the preset speed for a second preset number of times to obtain a worn sleeper sample; The result evaluation process is to judge whether the wear performance of the fastener pad sample on the sleeper sample meets the requirements according to the loss mass of the worn fastener pad sample and the worn sleeper sample, and / or the wear depth of the worn fastener pad sample and the worn sleeper sample; The material of the sleeper sample is the same as that of the actual sleeper, and the material of the fastener pad sample is the same as that of the actual fastener pad.

2. The method for evaluating the wear performance of railway fastener pads on sleepers according to claim 1, characterized in that: In the process of using the pin-on-disc friction and wear testing machine to drive the fastener pad sample to rotate relative to the sleeper sample for a first preset number of times at a preset speed to obtain a worn fastener pad sample, the contact surface between the fastener pad sample and the sleeper sample is in a dry friction state environment; In the process of continuing to use the pin-on-disc friction and wear testing machine to drive the worn fastener plate sample to rotate relative to the sleeper sample at the preset speed for a second preset number of times to obtain the worn sleeper sample, the contact surface between the fastener plate sample and the sleeper sample is a water-cooled environment.

3. The method for evaluating the wear performance of railway fastener pads on sleepers according to claim 1, characterized in that: During the wear test, The temperature of the fastener pad sample is monitored. If the temperature of the fastener pad sample is not lower than a preset first temperature threshold, the wear test process is stopped. The wear test process is continued when the temperature of the fastener pad sample drops to no higher than a preset second temperature threshold.

4. The method for evaluating the wear performance of railway fastener pads on sleepers according to claim 1, characterized in that: During the wear test, the friction force between the fastener plate sample and the sleeper sample is calculated based on the torque and the turning radius borne by the lower fixed plate, and the friction coefficient between the fastener plate sample and the sleeper sample is obtained based on the friction force and the pressure; The result evaluation process further includes judging whether the wear performance of the fastener pad sample on the sleeper sample meets the requirements based on the friction coefficient and a preset friction coefficient threshold.

5. The method for evaluating the wear performance of railway fastener pads on sleepers according to claim 1, characterized in that: The process of judging whether the wear performance of the fastener pad sample on the sleeper sample meets the requirements based on the loss mass of the worn fastener pad sample and the worn sleeper sample includes: Before the sample loading process, the fastener pad sample and the sleeper sample are weighed respectively to obtain the original fastener pad sample weight and the original sleeper sample weight; Weighing the worn fastener plate sample and the worn sleeper sample respectively to obtain the weight of the worn fastener plate sample and the weight of the worn sleeper sample, and subtracting the weight of the worn fastener plate sample and the weight of the worn sleeper sample from the original fastener plate sample weight and the original sleeper sample weight to obtain a first weight difference and a second weight difference; If the first weight difference is not greater than a preset first difference threshold, and the second weight difference is not greater than a preset second difference threshold, it is determined that the material of the fastener backing plate sample passes the wear performance assessment.

6. The method for evaluating the wear performance of railway fastener pads on sleepers according to claim 1, characterized in that: The process of judging whether the wear performance of the fastener plate sample on the sleeper sample meets the requirements according to the wear depth of the worn fastener plate sample and the worn sleeper sample comprises: The wear depth of the worn fastener backing plate sample and the wear depth of the worn sleeper sample are measured respectively to obtain a first wear depth and a second wear depth; If the first wear depth is not greater than a preset first wear depth threshold, and the second wear depth is not greater than a preset second wear depth threshold, it is determined that the material of the fastener pad sample passes the wear performance assessment.

7. The method for evaluating the wear performance of railway fastener pads on sleepers according to claim 1, characterized in that: Also includes, In the sample preparation process, the sleeper sample with the same strength as the actual sleeper is prepared using the same concrete mix ratio and steel bar configuration as the actual sleeper, and the fastener pad sample is cut from the actual fastener pad.

8. The method for evaluating the wear performance of railway fastener pads on sleepers according to claim 1, characterized in that: There are multiple fastener pad samples, and each of the fastener pad samples can perform rotational friction movement relative to the sleeper sample along the same trajectory.

9. The method for evaluating the wear performance of railway fastener pads on sleepers according to claim 1, characterized in that: The rotation radius of the center point of the fastener pad sample relative to the sleeper sample is not greater than the first preset radius and not less than the second preset radius.

10. The method for evaluating the wear performance of railway fastener pads on sleepers according to claim 1, characterized in that: The preset rotation speed is adjustable.