Calculation method for distribution of wear depth of debris flow channel
Through a coupled wear depth calculation method that comprehensively considers erosion, corrosion, and freeze-thaw cycles, and using stochastic process theory, the problem of wear depth distribution evaluation of debris flow guide troughs is solved, and the wear and failure time of the guide troughs is accurately estimated. , improving the practicality of project construction and maintenance.
Patent Information
- Application Number
- CN202210193626.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-02-28
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-02-28
AI Technical Summary
The existing technology is difficult to accurately assess the distribution of wear depth of debris flow drainage channels, and cannot effectively support the wear and maintenance of debris flow drainage channels.
A coupling wear depth calculation method that comprehensively considers erosion, corrosion, and freeze-thaw cycles is used. Through linear superposition and random process theory, the wear depth distribution function at any time is solved to estimate the coupling wear failure time of the guide groove.
It provides a more accurate wear depth distribution analysis, which is consistent with the actual situation, improves the practical significance of engineering construction and maintenance, and is more effective than the traditional model.
Smart Images

Figure CN114357805B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of wear analysis of a debris flow drainage channel, and in particular to a distribution calculation method for wear depth of a debris flow drainage channel. Background Art
[0002] The abrasion of debris flow on the flow wall is not a simple mechanical collision and friction between liquid slurry and solid particles on the wall, but a very complex result of two-phase flow coupling. Debris flow drainage channels are effective in discharging flood water, but are not friendly to solid particles of debris flow, which can cause siltation, block bridge holes, flood culverts, and scour and erode the bottom of the channel.
[0003] In recent years, scholars have done a lot of work on the factors affecting the abrasion of debris flows, the mechanism of abrasion, and measures to prevent and control abrasion. With the continuous deepening of research, hundreds of debris flow prevention projects have been widely used along highways, railways, and mines, and have effectively reduced the damage of debris flows to facilities along the lines. However, most drainage chutes are difficult to withstand the strong impact and abrasion of debris flows.
[0004] At present, although there are many studies on the wear of debris flow drainage guide channels, there is a lack of effective analytical methods for the analysis of the wear depth of the drainage guide channels. It is difficult to accurately evaluate the distribution of the wear depth of the drainage guide channels and cannot provide strong technical support for the wear maintenance of debris flow drainage guide channels. Therefore, there is an urgent need for a method to calculate the wear depth distribution of debris flow drainage guide channels by comprehensively considering multiple influencing factors. Summary of the invention
[0005] In view of this, the purpose of the present invention is to overcome the defects in the prior art and provide a distribution calculation method for the wear depth of debris flow drainage grooves, which can solve the distribution function of the coupled wear depth at any time, thereby estimating the time of coupled wear failure of the drainage grooves, which is more practical for existing engineering construction and maintenance work.
[0006] The method for calculating the distribution of wear depth of a debris flow drainage channel of the present invention comprises the following steps:
[0007] S1. Determine the wear depth δ1 of the row guide groove under erosion and abrasion;
[0008] S2. Determine the wear depth δ2 of the row guide groove under corrosion;
[0009] S3. Determine the wear depth δ3 of the row guide groove under the action of freeze-thaw cycles;
[0010] S4. Linearly superimpose the wear depth δ1, wear depth δ2 and wear depth δ3 to obtain the coupled wear depth δ under the combined action of erosion and abrasion, corrosion and freeze-thaw cycles:
[0011] δ=Aδ1+Bδ2+Cδ3+D;
[0012] Among them, A, B, and C are coupling wear correction coefficients; D is the coupling wear correction constant;
[0013] S5. Consider the wear process of debris flow as a random process and calculate the distribution function of the coupled wear depth δ.
[0014] Furthermore, the wear depth δ1 of the row guide groove is determined according to the following formula:
[0015]
[0016] Where, ζ is the anti-abrasion coefficient of the row guide groove; p a is the abrasive force acting on a certain section of the drainage groove; v is the average velocity of the debris flow; t is the cumulative wear time; b is the width of the drainage groove.
[0017] Furthermore, the wear depth δ2 of the row guide groove is determined according to the following formula:
[0018]
[0019] Among them, x0 is the current corrosion depth of the drainage channel concrete; t0 is the current corrosion time of the drainage channel concrete; and t is the action time of the corrosive medium.
[0020] Furthermore, the wear depth δ3 of the row guide groove is determined according to the following formula:
[0021] δ3=rt
[0022] Among them, r is the annual spalling rate; t is the freeze-thaw cycle time.
[0023] Furthermore, the wear process of debris flow is regarded as a random process, and the distribution function of the coupled wear depth δ is calculated, which includes:
[0024] S51. Derivative the coupling wear depth δ with respect to time to obtain the coupling wear depth rate
[0025]
[0026] in,
[0027] S52. Introduce a stationary normal random process X(t) with a median of 1, so that the coupled wear depth rate Becomes the following formula:
[0028]
[0029] S53. Taking the mean square integral of equation (2), we get the following equation:
[0030]
[0031] Among them, δ(t) is the wear amount at time t;
[0032] S54. Order F δ (x) and F w (x) represent the distribution functions of δ(t) and W(t), respectively, then we have the following formula:
[0033]
[0034] S55. Analyze the distribution characteristics of the function W(t) to obtain the distribution function F of the function W(t) w (x);
[0035] S56. Determine the distribution function F w Substituting (x) into equation (4), we can obtain the distribution function F of the coupling wear depth δ δ (x).
[0036] Further, the step S55 specifically includes:
[0037] a. Determine the mean μ of W(t) w :
[0038]
[0039] Among them, μ x is the mean of the stationary normal random process X(t);
[0040] b. Determine the variance of W(t)
[0041]
[0042] Among them, cov[X(τ1), X(τ2)] is the autocorrelation function of X(t), which represents the statistical correlation of wear at the two time states of τ1 and τ2;
[0043] c. Assuming that the autocorrelation function cov[X(τ1), X(τ2)] of X(t) is an exponential decay function of the time difference τ2-τ1, then:
[0044]
[0045] in, is the variance of the stationary normal random process X(t); α is a parameter with a value between 0 and infinity;
[0046] d. Substitute (7) into (6) to obtain the variance of W(t) for:
[0047]
[0048] e. The mean and variance of W(t) are taken as the distribution characteristics of W(t), and the distribution of the coupled wear depth is assumed to obtain the distribution function of W(t).
[0049] The beneficial effects of the present invention are as follows: a method for calculating the distribution of wear depth of a debris flow drain guide groove disclosed in the present invention introduces random process theory into the wear and destruction process of the debris flow drain guide groove, regards the wear phenomenon of the debris flow as a random process, randomizes the calculation model of coupled wear of the debris flow drain guide groove, and uses mathematical methods to solve the distribution function of the coupled wear depth at any time, thereby estimating the time when the coupled wear of the drain guide groove fails. Compared with traditional calculation models, the results are more in line with the actual situation and have more practical significance for existing engineering construction and maintenance work. BRIEF DESCRIPTION OF THE DRAWINGS
[0050] The present invention will be further described below in conjunction with the accompanying drawings and embodiments:
[0051] Figure 1 It is a schematic diagram of the method flow of the present invention;
[0052] Figure 2 It is a curve schematic diagram of the coupling wear depth changing with time of the present invention;
[0053] Figure 3 It is a schematic diagram of a curve showing the coupling wear depth rate changing with time according to the present invention;
[0054] Figure 4 This is a schematic diagram of a random curve of coupling wear depth in the first year of the present invention;
[0055] Figure 5 This is a schematic diagram of the probability density of coupling wear depth in the first year of the present invention;
[0056] Figure 6 It is a schematic diagram of a random curve of coupling wear depth in the third year of the present invention;
[0057] Figure 7 This is a schematic diagram of the probability density of coupling wear depth in the third year of the present invention;
[0058] Figure 8 A schematic diagram of the probability density of the time required for the coupling wear depth to reach 30 mm according to the present invention;
[0059] Fig. 9 It is a schematic diagram of the distribution function of the time required for the coupling wear depth to reach 30 mm according to the present invention;
[0060] Fig.10 A schematic diagram of the probability density of the time required for the coupling wear depth to reach 80 mm according to the present invention;
[0061] Fig.11 It is a schematic diagram of the distribution function of the time required for the coupling wear depth to reach 80 mm according to the present invention. DETAILED DESCRIPTION
[0062] The present invention is further described below in conjunction with the accompanying drawings, as shown in the drawings:
[0063] The method for calculating the distribution of wear depth of a debris flow drainage channel of the present invention comprises the following steps:
[0064] S1. Determine the wear depth δ1 of the row guide groove under erosion and abrasion;
[0065] S2. Determine the wear depth δ2 of the row guide groove under corrosion;
[0066] S3. Determine the wear depth δ3 of the row guide groove under the action of freeze-thaw cycles;
[0067] S4. Linearly superimpose the wear depth δ1, wear depth δ2 and wear depth δ3 to obtain the coupled wear depth δ under the combined action of erosion and abrasion, corrosion and freeze-thaw cycles:
[0068] δ=Aδ1+Bδ2+Cδ3+D;
[0069] Among them, A, B, and C are coupling wear correction coefficients; D is the coupling wear correction constant;
[0070] S5. Consider the wear process of debris flow as a random process and calculate the distribution function of the coupled wear depth δ.
[0071] In this embodiment, the debris flow is a typical multiphase flow with coupled solid, liquid and gas anomalies, which can be approximated as a two-phase fluid composed of homogeneous debris flow slurry and homogeneous solid particles. The abrasion mechanism of this fluid on the drainage trough structure can be approximated as the slurry abrasion mechanism and the solid particle abrasion mechanism.
[0072] (1) Slurry abrasion: The abrasion process of debris flow slurry on the concrete surface of the drainage channel can be divided into two stages. In the first stage, the abrasion starts from the mortar on the concrete surface. As the surface mortar is gradually abraded away, the coarse aggregate continues to expose the surface. At this time, the mortar and the coarse aggregate jointly bear the abrasive effect of the debris flow slurry. In the second stage, due to the different wear resistance of the mortar and the coarse aggregate, the coarse aggregate with better wear resistance gradually protrudes, and the cement mortar is abraded to form pits. At this time, the abrasive force of the debris flow is mainly borne by the protruding coarse aggregate. As the abrasion continues, when the abrasive force of the debris flow slurry on the coarse aggregate is greater than the force that fixes the coarse aggregate on the matrix, the coarse aggregate detaches from the matrix and is washed away, the mortar is subjected to abrasion, and the abrasion process returns to the first stage. The two stages are repeated, causing the abrasion depth to increase continuously.
[0073] (2) Solid impact and cutting: There are a large number of poorly sorted solid particles in the debris flow, which move along the bottom of the drainage channel under the influence of the debris flow slurry, and then impact, cut and abrade the uneven concrete wall. Generally speaking, the larger the solid ratio of the debris flow slurry, the more coarse particles, the worse the roundness of the solid phase particles, and the faster the particle movement speed, the stronger the impact and abrasion of the solid phase particles on the bottom of the drainage channel.
[0074] The abrasive force and abrasive amount of debris flow are comprehensively analyzed from the perspective of slurry abrasion and solid phase cutting, and the state equation of the abrasive amount of concrete on the wall of the drainage channel is obtained as follows:
[0075] δ1=f(P a ,v,,σ a ,H a )
[0076] By deduction, the wear depth δ1 of the guide groove under erosion and abrasion is obtained:
[0077]
[0078] Where ζ is the anti-abrasion coefficient of the row guide groove, in m 3 / KN;p a is the abrasive force acting on a certain section of the drainage channel, in kN / m; v is the average velocity of the debris flow, in m / s; t is the accumulated wear time, in s ; b is the width of the row guide groove, in m.
[0079] In this embodiment, under normal circumstances, the degradation effect of environmental corrosive media on the structure is a gradual process. The impact of the environment on the structure can be divided into two categories, one is the impact of the natural environment, and the other is the impact of the use environment. The impact of the natural environment is mainly the erosion of the structure by the corrosive media in the natural environment. In addition to the impact of the corrosive media existing in nature itself, it also includes the adverse effects of environmental pollution caused by modern industrial development on the structure or the aggravation of corrosion, such as the formation of "acid rain", the increase in atmospheric temperature, and the increase in carbon dioxide content.
[0080] In nature, structural materials will gradually age over time, which will reduce the strength and performance of the materials. Some active materials in the structure will react slowly with other components, which will change the chemical composition of the materials. The expansion pressure generated by the products will cause the structure to be damaged. The alkali-aggregate reaction of concrete is such an internal reaction.
[0081] The debris flow drainage channel is also affected by environmental factors. The corrosive media in the natural environment, such as carbon dioxide and sulfate, will corrode the concrete structure of the drainage channel. There are mainly two types of corrosion: concrete carbonization and sulfate corrosion.
[0082] 1) Concrete carbonization: Carbon dioxide from the air, soil or groundwater penetrates into the concrete and reacts with the alkaline substances in the concrete, causing the concrete to carbonize. As the alkalinity of the concrete decreases, the passivation film on the surface of the steel bars that has been formed is destroyed, and the steel bars are corroded in the presence of oxygen and water.
[0083] 2) Sulfate corrosion: Sulfate corrosion is one of the most widespread and common forms of chemical corrosion in concrete. In the natural environment, sulfates are often present in groundwater, especially when the proportion of clay in the soil is high. Sulfates react chemically with calcium hydroxide and calcium aluminate hydrate in cement to produce gypsum and calcium sulfoaluminate, which expand in volume and cause concrete to disintegrate. Sulfates not only corrode reinforced concrete components buried in the soil or in contact with the soil, but also often corrode concrete components on the ground.
[0084] Based on Fick's law, by analyzing the diffusion and migration of corrosive media in concrete, and after a series of derivations, the wear depth δ2 of the drainage groove under corrosion is obtained:
[0085]
[0086] Among them, x0 is the current corrosion depth of the drainage channel concrete; t0 is the current corrosion time of the drainage channel concrete; and t is the action time of the corrosive medium.
[0087] In the present embodiment, concrete is a porous body composed of cement mortar and coarse aggregate, and when mixing concrete, excess free water is retained in these interconnected capillaries. In cold regions, when the temperature drops below 0°, the free water freezes and expands, causing a certain degree of damage to the internal structure of the concrete. With the alternating changes in temperature, the free water inside the concrete is also constantly freezing and melting, and this process gradually accumulates the internal damage of the concrete. When the damage accumulates to a certain extent, the concrete is destroyed. In cold regions, the freeze-thaw cycle of concrete is one of the main reasons for the premature destruction of roads and bridges, and for the debris flow drainage structure built in cold regions, the freeze-thaw cycle damage acts together with the erosion and corrosion, showing different destruction characteristics from the single freeze-thaw or erosion, accelerating the deterioration process of the concrete.
[0088] Then under the action of freeze-thaw cycles, the wear depth of the drain groove δ3 is:
[0089] δ3=rt
[0090] Among them, r is the annual spalling rate; t is the freeze-thaw cycle duration. Since the annual spalling rate of the surface concrete is related to the concrete parameters during the freeze-thaw cycle, the annual spalling rate is determined according to the following formula:
[0091] r=C1C2C3a -0.7 (f cu +8) -1.4
[0092] Where: r is the annual spalling rate (mm / a), C1 is the curing time coefficient, Where d is the curing time (days); C2 is the environmental impact coefficient, which is between 20 and 40; C3 is the mineral additive impact coefficient, Where P s P b P f are the mixing ratios of silica fume, slag and fly ash (%); a is the air content of concrete (%), f cu is the compressive strength of concrete (MPa).
[0093] In this embodiment, in step S4, during the abrasion process of the debris flow drainage structure, there are often complex interactions between the three abrasion mechanisms of erosion and abrasion, corrosion, and freeze-thaw cycles. For example, corrosive abrasion will be more severe in the case of both corrosion and erosion and abrasion, because when erosion and abrasion take away the corrosion layer on the wall of the drainage structure and expose the fresh wall, corrosive abrasion will more easily act on the next layer, and the corrosion and peeling will continue to repeat; at the same time, the erosion and abrasion process brings acid, alkali, salt and other material bases for corrosion, and puts the drainage structure in a dry-wet alternating state, aggravating the degree of corrosion. In the cold winter environment in the area where the debris flow drainage structure is located, the freeze-thaw cycle also accelerates the continued expansion of the abrasion depth. Therefore, when erosion and abrasion, corrosion and freeze-thaw cycles exist at the same time, the abrasion of the prevention and control structure is further aggravated. The combined effects of erosion and abrasion, corrosion and freeze-thaw cycles are more serious than when a single effect exists.
[0094] Because there are complex interactions among various wear factors, in order to simplify the problem, the calculation formula for the coupled wear depth is obtained by linear superposition, and the coupled wear coefficient is added to reflect the interaction of various wear factors to make the formula more reasonable.
[0095] That is, the coupling wear depth is:
[0096] Among them, A, B, and C are coupling wear correction coefficients; D is the coupling wear correction constant; and t is time. By substituting the actual calculation parameters of the debris flow drainage project into the above coupling wear depth calculation model, the instantiation values of A, B, C, and D can be obtained.
[0097] In this embodiment, the wear process of the debris flow is regarded as a random process, and the distribution function of the coupled wear depth δ is calculated, which specifically includes:
[0098] S51. Derivative the coupling wear depth δ with respect to time to obtain the coupling wear depth rate
[0099]
[0100] in,
[0101] In this embodiment, the The D1 is a derivative constant.
[0102] S52. The main reason for the failure of debris flow drainage channel is excessive wear, that is, the life and reliability of debris flow drainage channel depend to a large extent on the wear condition, and the wear process is the result of the coupling of multiple factors and is dynamic and random. In order to describe the dispersion of coupled wear statistics, a stationary normal random process X(t) with a median of 1 is introduced, so that the coupled wear depth rate Becomes the following formula:
[0103]
[0104] S53. Set the random variable δ(t) for the coupling wear depth δ. Since it is difficult to calculate the analytical solution of the distribution function of the random variable δ(t), the second moment approximation method is used to simulate the actual distribution with a specific distribution that conforms to these low-order cumulants to obtain a result that meets certain accuracy requirements. According to the estimated values of the mean and standard deviation of the random variable δ(t), a suitable function is selected to fit the distribution function of δ(t); the specific operations are as follows:
[0105] Taking the mean square integral of formula (2), we get the following formula:
[0106]
[0107] Among them, δ(t) is the wear amount at time t, and δ(t) represents a random variable;
[0108] S54. Order W(t) is an integral used to describe a normal random process, expressed as F δ (x) and F w (x) represent the distribution functions of δ(t) and W(t), respectively, then we have the following formula:
[0109]
[0110] S55. Analyze the distribution characteristics of the function W(t) to obtain the distribution function F of the function W(t) w (x);
[0111] S56. Determine the distribution function F w Substituting (x) into equation (4), we can obtain the distribution function F of the coupling wear depth δ δ (x).
[0112] In this embodiment, the step S55 specifically includes:
[0113] a. Determine the mean μ of W(t) w :
[0114]
[0115] Among them, μ x is the mean of the stationary normal random process X(t);
[0116] b. Determine the variance of W(t)
[0117]
[0118] Among them, cov[X(τ1), X(τ2)] is the autocorrelation function of X(t), which represents the statistical correlation of wear at the two time states of τ1 and τ2;
[0119] c. Assuming that the autocorrelation function cov[X(τ1), X(τ2)] of X(t) is an exponential decay function of the time difference τ2-τ1, then:
[0120]
[0121] in, is the variance of the stationary normal random process X(t); α is a parameter with a value between 0 and infinity; when α approaches 0, X(t) is a random variable, and when α approaches infinity, X(t) is a white noise process; the true value of α is obtained through experiments. Generally speaking, α takes a value between 0 and infinity.
[0122] d. Substitute (7) into (6) to obtain the variance of W(t) for:
[0123]
[0124] e. Take the mean and variance of W(t) as the distribution characteristics of W(t), and use the distribution of the coupled wear depth to make an assumption to obtain the distribution function of W(t). Through the distribution function of W(t) given above, the distribution function F of the coupled wear depth δ can be obtained: δ (x);
[0125] Assuming that W(t) obeys normal distribution, the distribution function of the coupling wear depth δ at time t is:
[0126]
[0127] Through the above analysis, we can get Figure 2-11 The analysis results are shown. The present invention introduces random process theory into the wear and damage process of debris flow drain grooves, regards the wear phenomenon of debris flow as a random process, randomizes the calculation model of coupled wear of debris flow drain grooves, and uses mathematical methods to solve the distribution function of coupled wear depth at any time, thereby estimating the time of coupled wear failure of drain grooves. Compared with traditional calculation models, the results are more in line with reality and more practical for existing engineering construction and maintenance work.
[0128] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the purpose and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.
Claims
1. A method for calculating the distribution of wear depth of debris flow channel. Features: The steps include: S1. Determine the wear depth δ of the guide groove under erosion and abrasion 1 ; S2. Determine the wear depth δ of the row guide groove under corrosion 2 ; S3. Determine the wear depth δ of the row guide groove under the action of freeze-thaw cycles 3 ; S4. Wear depth δ 1 , wear depth δ 2 and wear depth δ 3 Linear superposition is performed to obtain the coupled wear depth δ under the combined action of erosion and abrasion, corrosion and freeze-thaw cycles: δ=Aδ 1 +Bδ 2 +Cδ 3 +D; Among them, A, B, and C are coupling wear correction coefficients; D is the coupling wear correction constant; S5. Treat the wear process of debris flow as a random process and calculate the distribution function of the coupled wear depth δ, including: S51. Derivative the coupling wear depth δ with respect to time to obtain the coupling wear depth rate in, S52. Introduce a stationary normal random process X(t) with a median of 1, so that the coupled wear depth rate Becomes the following formula: S53. Taking the mean square integral of equation (2), we get the following equation: Among them, δ(t) is the wear amount at time t; S54. Order F δ (x) and F w (x) represent the distribution functions of δ(t) and W(t), respectively, then we have the following formula: S55. Analyze the distribution characteristics of the function W(t) to obtain the distribution function F of the function W(t) w (x); The step S55 specifically includes: a. Determine the mean μ of W(t) w : Among them, μ x is the mean of the stationary normal random process X(t); b. Determine the variance of W(t) Among them, cov[X(τ 1 ), X(τ 2 )] is the autocorrelation function of X(t), indicating τ 1 , τ 2 Statistical correlation of wear on two time states; c. Assume that the autocorrelation function cov[X(τ 1 ), X(τ 2 )] is the time difference τ 2 -τ 1 The exponential decay function of is: in, is the variance of the stationary normal random process X(t); α is a parameter with a value between 0 and infinity; d. Substitute (7) into (6) to obtain the variance of W(t) for: e. Taking the mean and variance of W(t) as the distribution characteristics of W(t), and assuming that the coupling wear depth obeys the distribution, the distribution function of W(t) is obtained; S56. Determine the distribution function F w Substituting (x) into equation (4), we can obtain the distribution function F of the coupling wear depth δ δ (x).
2. The method for calculating the distribution of wear depth of debris flow drainage channel according to claim 1, Features: The wear depth δ of the row guide groove is determined according to the following formula: 1 : Where, ζ is the anti-abrasion coefficient of the row guide groove; p a is the abrasive force acting on a certain section of the drainage groove; v is the average velocity of the debris flow; t is the cumulative wear time; b is the width of the drainage groove.
3. The method for calculating the distribution of wear depth of debris flow drainage channel according to claim 1, Features: The wear depth δ of the row guide groove is determined according to the following formula: 2 : Among them, x 0 is the current corrosion depth of the drainage channel concrete; t 0 is the current corrosion time of the drainage channel concrete; t is the action time of the corrosive medium.
4. The method for calculating the distribution of wear depth of debris flow drainage channel according to claim 1, Features: The wear depth δ of the row guide groove is determined according to the following formula: 3 : d 3 =rt Among them, r is the annual spalling rate; t is the freeze-thaw cycle time.
Citation Information
Patent Citations
Concrete microstructure chloride ion erosion model based on natural environment effect of cold region
CN114861496A