Method for producing an electrode for a storage device for storing electrical energy, use of such an electrode and electrode

Through the solvent-free mixture coating method and the design of fiber-absorbing electrolyte, the problem of solvent removal difficulties in the manufacture of lithium-ion battery electrodes is solved, and the rapid, low-cost manufacturing and efficient ion conductivity of the electrode are achieved.

CN114402458BActive Publication Date: 2024-11-08BAYERISCHE MOTOREN WERKE AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202080064530.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-10-22
Filing Date
2020-09-29
Publication Date
2024-11-08
Estimated Expiration
2040-09-29

AI Technical Summary

Technical Problem

Solvents such as NMP used in the manufacturing process of existing lithium-ion battery electrodes are difficult to completely remove, resulting in insufficient electrode porosity and ion conductivity, and the manufacturing process is complex and costly.

Method used

Using a solvent-free mixture coating method, a heterogeneous mixture of fibers and active materials is used to form a coating on the substrate, and the solvent is removed by evaporation or extrusion process to ensure electrode porosity and fiber absorption of electrolytes to improve ion conductivity.

Benefits of technology

Fast and low-cost manufacturing of electrodes is achieved, drying and recycling steps are avoided, and efficient ion conductivity and environmental sustainability are ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114402458B_ABST
    Figure CN114402458B_ABST
Patent Text Reader

Abstract

The invention relates to a method for producing an electrode (1) of a storage device (12) for storing electrical energy, wherein a substrate (5) is coated with at least one active material (3) for storing electrical energy. A mixture (2) is provided, which comprises the active material (3) and fibers (4) (step S1). The substrate (5) is coated with the mixture (2), which does not contain a solvent which contains the fibers (4) and which is at least largely discharged from the mixture (2) after the coating of the substrate (5), wherein, by coating the substrate (5) with the mixture (2), a coating (6) with the active material (3) and the fibers (4) is formed on the substrate (5) from the mixture (2) (step S2).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for producing an electrode for storing electrical energy, in particular for a motor vehicle, and also to the use of such an electrode and to an electrode. Background Art

[0002] JP2002279994A discloses a battery having a negative electrode.

[0003] In addition, the hyperlink "http: / / www.google.de / url?sa=t&rct=j&q=&esrc=s&source=web&cd=3&ved=2ahUKEwjGz_P4zZPhAhUNZVAKHZMUC_MQFjACegQIAxAC&url=http%3A%2F%2Fwww.theses.fr%2F2012GRENI043.pdf&usg=AOvVaw2E3-UgrowlKdrLlt4AawO8" published by Lara Jabbour et al. on October 2, 2019 can be queried. The publication discloses a method in which an aqueous slurry containing graphite and microfibrillated cellulose as a solid phase is cast into a mold and then water is evaporated from the slurry. This results in a porous film made of graphite and microfibrillated cellulose which is used to prepare electrodes for lithium-ion batteries. Summary of the invention

[0004] The object of the present invention is to provide a method for producing an electrode for storing electrical energy, in particular for a motor vehicle, the use of such an electrode and an electrode which can be produced in a particularly advantageous manner.

[0005] According to the invention, this object is achieved by a method having the features of the invention, by a use having the features of the invention and by an electrode having the features of the invention.

[0006] A first aspect of the invention relates to a method for producing an electrode of a storage device for storing electrical energy, in particular electric current, in particular for a motor vehicle. In the method, the substrate of the electrode is coated with at least one active material for storing electrical energy. The active material may, for example, include lithium and / or graphite and / or nickel and is used in particular to store electrical energy by means of or in a storage device, in particular electrically and / or electrostatically, wherein the storage device is, for example, a primary cell. In particular, the storage device may be a battery, in particular a lithium-ion battery, or a storage cell, in particular a storage cell, and in this case, for example, a lithium-ion cell, so that the active material may in particular include at least lithium. In addition, for example, the active material is used to discharge the electrical energy stored in or by means of the storage device from the storage device, that is to say to be conducted from the storage device and, for example, supplied to at least one electrical consumer.

[0007] Preferably, the substrate consists of a material different from the storage material. In particular, the substrate can consist of a metallic and / or electrically conductive material, in particular copper or aluminum. The substrate is preferably a solid, wherein the substrate can be designed as a film, in particular a metal foil, or as a metal sheet. In particular, the substrate can be used as a current collector, which is also called a current collector or a current tap or a current collector.

[0008] The storage device is used, in particular in the fully manufactured state of the storage device, for example in a motor vehicle, preferably in the form of a car, in particular a passenger car, or for the motor vehicle, in order to store and provide electrical energy, by means of which the motor vehicle can be driven electrically, in particular purely electrically. The motor vehicle is thus, for example, in the form of a hybrid vehicle or an electric vehicle, in particular a battery electric vehicle (BEV).

[0009] In order to be able to produce the electrode and thus the storage device in a particularly advantageous manner overall, the method according to the invention provides for a mixture to be provided which contains the active material and, in particular, the fibers which are formed separately from the active material. The mixture is therefore preferably a heterogeneous mixture, in particular a heterogeneous substance mixture, which has the fibers as a first substance, in particular as a first solid material, and the active material as a second substance, in particular as a second solid material.

[0010] Furthermore, in the method according to the invention, it is provided that the substrate is coated with a mixture, wherein the mixture does not contain a solvent which holds the fibers and which at least for the most part is discharged from the mixture after the coating of the substrate. In other words, the mixture is solvent-free. In particular, it is to be understood that the mixture does not include, has or contains a solvent which holds the fibers and which at least for the most part is discharged or discharged from the mixture after the coating of the substrate. By coating the substrate with the mixture, a coating with active material and fibers is formed on the substrate, that is to say produced, from the mixture. As described above or according to the above definition, since the mixture is solvent-free, no removal of the solvent from the mixture occurs in the method. As a result, the electrode can be produced particularly time-efficiently and cost-effectively.

[0011] The present invention is based on the knowledge that N-methylpyrrolidone (NMP) is usually used as a solvent for coatings, especially for cathodes or positive electrodes for lithium-ion batteries. The present invention now makes it possible to avoid NMP and produce electrodes without NMP or without other solvents, which are at least largely discharged from the mixture after the substrate is coated with the mixture. It is usually provided that a paste with NMP is used as a solvent for electrode coatings, especially for cathode coatings. For anode coatings, it is conceivable to use water as a solvent. Due to the stability of the active material relative to water, the use of water as a solvent cannot be problem-free for cathode coatings. The basic advantage of using a solvent that is at least largely discharged or removed from the mixture after coating the substrate is that it results in an advantageous porosity of the coating or electrode. Due to the porosity, the electrode or coating has pores in which a preferably liquid electrolyte can be accommodated, especially in the fully manufactured state of the storage device. In particular, the electrolyte can, in particular, completely fill the pores, wherein an advantageous ion conductivity can be achieved by accommodating the electrolyte through the pores. The porosity is produced in particular by removing the solvent from the mixture or the coating at least to a large extent, in particular completely, after coating the substrate, in particular in a targeted manner, in particular by evaporation, that is to say by an evaporation process which follows the coating, that is to say the coating process, within the scope of which the substrate is coated with the mixture.

[0012] The solvent-free production of the electrode allows a particularly time-efficient and cost-effective production of the electrode, since, for example, a drying or evaporation step, i.e. a working step in which the solvent is at least largely, in particular completely, removed from the mixture, as well as a step for recovering the solvent removed at least largely from the mixture, can be avoided. Purification can also be omitted. In addition, the electrode can be produced in an environmentally sustainable manner, since solvents that are disadvantageous for this, such as, in particular, NMP, can be omitted.

[0013] However, if the solvent, which is at least largely removed from the mixture or from the coating after the substrate is applied, is now omitted, the porosity of the coating or electrode cannot be produced by evaporating, drying or removing the solvent from the mixture. In this regard, however, favorable ion conductivity can be ensured by using fibers, especially in the fully manufactured state of the storage device.

[0014] It has proven to be particularly advantageous here if, after coating the substrate with the mixture, the coating is brought into contact with an electrolyte, in particular a liquid electrolyte, which is at least partially absorbed, in particular drawn in, by or through the fibers. In other words, the fibers absorb the electrolyte instead of the previously described pores, in particular at least a portion of the electrolyte is drawn in through the fibers. This ensures particularly advantageous ion conductivity.

[0015] In order to be able to produce the electrode particularly time-efficiently and cost-effectively, a further embodiment of the invention provides that the substrate is not coated with a solvent before and after coating the substrate with the mixture. Furthermore, it has proven to be particularly advantageous to use cellulose fibers as the fibers. This allows particularly advantageous ion conductivity to be achieved, since, for example, cellulose fibers can absorb, in particular imbibe, in particular liquid electrolytes particularly well.

[0016] In another design of the present invention, the substrate is coated with the mixture by extrusion. Thus, the substrate can be coated with the mixture in a particularly simple, time-favorable and cost-effective manner and thus be arranged. Within the scope of extrusion, the solid substrate is, for example, transported through or driven through, especially inserted through or pulled through the opening, especially through the nozzle. During the substrate is transported through the opening, the substrate is coated with the mixture in the opening, especially so that during the substrate is transported through the opening, the mixture is applied, especially coated on the substrate, especially on the peripheral surface of the peripheral side of the substrate. Alternatively or additionally, during the substrate is transported through the opening, the mixture is applied to the substrate, especially on the side of the peripheral side before and / or after the opening. By extrusion, for example, the shape of the favorable peripheral side of the electrode or structural element can be realized in a simple, time-favorable and cost-effective manner, and the structural element includes the substrate coated with the mixture. In particular, the shape can be established by limiting the wall area of ​​the opening, especially along the circumferential direction of the opening.

[0017] In order to apply, in particular coat the mixture onto the substrate, in particular onto the outer peripheral surface of the circumference, for example, at least one coating device is used, which can have a nozzle, in particular a wide-slot nozzle. For example, the mixture flows through or through the nozzle and is ejected by means of the nozzle and sprayed onto the substrate, in particular onto the outer peripheral surface of the circumference, and is thereby applied or coated onto the substrate, in particular onto the outer peripheral surface of the circumference.

[0018] Furthermore, it has proven to be particularly advantageous to coat the substrate with the mixture by lamination. During the lamination process, for example, the mixture or the coating is thermally and / or materially bonded to the substrate. Thus, lamination includes, for example, a thermal bonding method and / or a materially bonded bonding method, by means of which the mixture or the coating is thermally and / or materially bonded to the substrate using heat. For this purpose, for example, the substrate and / or the mixture is heated, in particular so that the mixture is applied to the substrate, in particular to the peripheral surface of the peripheral side, in the hot or heated state of the substrate and / or in the hot or heated state of the mixture, whereby, for example, the mixture or the coating is thermally and / or materially bonded to the substrate.

[0019] In order to be able to manufacture the electrodes particularly simply and cost-effectively, it is provided in another embodiment of the invention that the fibers are electrically conductive. The embodiment is based on the idea that the fibers can assume at least one further or additional function. For example, if the fibers are electrically conductive, other conductive additives for electrical conductivity, such as carbon black or carbon nanotubes, can be dispensed with. The further functionalization of the fibers and / or at least one property of the fibers can also be used to achieve a particularly high safety of a storage device, for example, in the form of a battery cell, in particular a storage battery cell.

[0020] In this context, it has proven to be particularly advantageous if the fibers consist of a non-combustible or non-combustible material. In other words, the fibers have fire-retardant properties. The feature that the fibers consist of a non-combustible material is understood in particular to mean that the fibers are non-combustible and have no combustible components or are non-combustible with combustible components, so that the fibers are, for example, in class A1 or A2-s1 according to class d0 of the standard EN 13501-1 for defining combustion properties, or the fibers are, for example, in building material class A1 or A2 according to the standard DIN 4102-1 for defining building material classes. The feature that the fibers consist of a non-flammable material can be understood in particular to mean that the fibers are, for example, in class B, C-s1, d0 or A2, B, C-s2, d0 or A2, B, C-s3, d0 or A2, B, C-s1, d1 or A2, B, C-s1, d2 or A2, B, C-s3, d2 according to the standard EN13501-1 for defining combustion properties, or that the fibers are, for example, in building material class B1 according to the standard DIN4102-1 for defining building material classes. Whenever reference is made to the EN13501-1 standard and the DIN4102-1 standard within the scope of the present disclosure, these standards are to be understood as the EN13501-1 standard and the DIN4102-1 standard in their valid text as of October 9, 2019.

[0021] Alternatively or additionally, it is conceivable that the fibers have a particularly high thermal conductivity, whereby a particularly high thermal conductivity of the fiber-based electrode can be achieved in a particularly simple and cost-effective manner.

[0022] Finally, it has proven to be particularly advantageous if the mixture also includes a binder provided in addition to the fibers and in addition to the active material, which binder, for example, holds the fibers and / or the active material. In other words, the fibers and / or the active material can be embedded in the binder. The binder ensures an advantageous bonding of the fibers and the active material and, for example, an especially advantageous adhesion of the mixture to the substrate.

[0023] Preferably, a polymer, in particular polyvinylidene fluoride (PVdF), is used as binder.

[0024] The second aspect of the present invention relates to the use of an electrode manufactured by the method according to the first aspect of the present invention, wherein the electrode is used as an electrode, in particular a positive electrode, of a storage device for storing electrical energy. The positive electrode is also referred to as a positive electrode or an electrical positive electrode and is, for example, its cathode when the storage device is discharged. Discharging can be understood as the electrical energy stored in the storage device or stored by means of the storage device being discharged from the storage device or by the storage device and, for example, supplied to an electrical consumer. The advantages and advantageous configurations of the first aspect of the present invention can be regarded as the advantages and advantageous configurations of the second aspect of the present invention, and vice versa. The present invention also relates to the use of an electrode or the use of an electrode manufactured by the method according to the first aspect of the present invention, wherein the electrode is used in one or more of the above-mentioned storage devices of a motor vehicle and is therefore used in a motor vehicle or for a motor vehicle. Electrical energy can be stored by means of or in the storage device, which is used or can be used, for example, to drive the motor vehicle electrically, in particular purely electrically. Here, the aforementioned consumer is, for example, an electric motor, which is operated or can be operated in engine operation and thus as an electric motor by supplying the electric energy stored in the storage device to the electric motor. With the electric motor, the motor vehicle is driven, in particular purely electrically.

[0025] A third aspect of the invention relates to an electrode for a storage device for storing electrical energy, in particular for a motor vehicle. The electrode is produced by means of a method according to the first aspect of the invention. The advantages and advantageous embodiments of the first and second aspects of the invention can be regarded as advantages and advantageous embodiments of the third aspect of the invention, and vice versa. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Further details of the invention are obtained from the following description of preferred embodiments in conjunction with the accompanying drawings.

[0027] Figure 1A flow chart is shown for explaining the method according to the invention for producing an electrode for storing electrical energy, in particular for a motor vehicle; and

[0028] Figure 2 A schematic diagram showing the method is shown.

[0029] In the figures, identical or functionally identical elements are provided with the same reference symbols. DETAILED DESCRIPTION

[0030] In the following text, Figure 1 and Figure 2 A method for producing an electrode 1 of a storage device for storing electrical energy, in particular electrical current, is described. The storage device is used to store electrical energy for a motor vehicle, for example, which is configured as a car, in particular as a sedan. Therefore, the storage device is used in a motor vehicle or is used in a motor vehicle, so that the motor vehicle has a storage device and an electrode 1 in its fully manufactured state. The motor vehicle is a hybrid vehicle or an electric vehicle, in particular a battery electric vehicle, so that the motor vehicle has at least one motor. The motor vehicle can be driven by means of an electric motor, in particular purely electrically. For this purpose, the electric motor is operated in engine operation and thus operates as an electric motor. In order to operate the electric motor in engine operation, the electric motor is supplied with electrical energy, in particular electrical current, stored in the storage device. In order to be able to achieve particularly large electrical power for driving the motor vehicle electrically, in particular purely electrically, the storage device and the motor are preferably configured as high-voltage components, whose corresponding voltage, in particular electrical operating voltage or rated voltage is preferably greater than 50 volts, in particular greater than 60 volts or preferably several hundred volts. The storage device is configured, for example, as a battery, in particular a high-voltage battery. In particular, the storage device can be configured as a lithium-ion battery. The storage device comprises, for example, a plurality of electrically connected battery cells, which are also referred to as storage battery cells and are, for example, configured as lithium-ion battery cells. Electrode 1 is, for example, an electrode of one of the storage battery cells. Electrode 1 is, for example, a component of a positive electrode, also referred to as a positive electrode, of a storage battery cell or a storage device, so that electrode 1 is, for example, the cathode of the storage device or the storage battery cell with respect to the discharge of the storage device or the storage battery cell. When the storage device or the storage battery cell is discharged, the electrical energy stored in the storage device or the storage battery cell is drawn from the storage battery cell or from the storage device and, for example, is supplied to an electric motor. In this case, the storage device or the storage battery cell is, in particular, a galvanic cell.

[0031] In a first step S1 of the method, a Figure 2 The mixture 2 shown schematically in particular in FIG. 1 has at least one active material and fibers arranged in addition to the active material. The active material is Figure 2, the active material 3 is particularly schematically shown by a triangle and is marked with 3, while the fibers are also particularly schematically shown by a line and are marked with 4. The fibers 4 are preferably solid and are therefore the first solid material. Alternatively or additionally, the active material 3 is solid and is therefore, for example, the second solid material of the mixture 2. In the second step S2 of the method, the substrate 5 of the electrode 1 is coated with the mixture 2 and thus with the active material 3 and the fibers 4, wherein the mixture 2, in particular before, after and during the coating of the substrate 5, contains no solvent which is at least largely discharged from the mixture 2 after the coating of the substrate 5. Therefore, in this method, the solvent is not discharged at least largely from the mixture 2 after the coating of the substrate 5 with the mixture 2. By coating the substrate 5 with the mixture 2, a coating 6 of the electrode 1 with the active material 3 and the fibers 4 is formed on the substrate 5 from the mixture 2. Therefore, the finished electrode 1 is a structural element which has a substrate 5 and a coating 6 with the active material 3 and the fibers 4 applied to the substrate 5 and in particular attached to the substrate 5. In this case, the base body 5 preferably consists of a metallic and / or electrically conductive material, for example copper or aluminum.

[0032] In order to coat the substrate 5 with the mixture 2, a coating device 7, also referred to as a coating unit, is used. The coating device 7 comprises at least one, in particular annular, opening 8 which is designed, for example, as a nozzle or is a component of such a nozzle. The substrate 5, which is preferably solid and thus designed as a solid, is preferably coated with a coating agent. Figure 2 9 is conveyed in the conveying direction indicated by the arrow 9, in particular at least substantially continuously through the opening 10, which is preferably designed as a through-opening, of the coating device 7. Here, the opening 8 opens into the opening 10 and the mixture 2 flows through it, so that while the substrate 5 is conveyed in the conveying direction through the opening 10 and thus through the coating device 7, the coating device 7 ejects the mixture 2 through the opening 8 and sprays it toward the substrate 5, in particular toward the outer circumferential surface 11 of the substrate 5. As a result, the mixture 2 is applied or coated on the substrate 5, in particular on the outer circumferential surface 11 of the outer circumferential side, thereby forming, that is, producing, the coating 6 on the outer circumferential surface 11 of the outer circumferential side.

[0033] exist Figure 2A storage cell is also schematically shown in FIG and is marked with 12, wherein the storage cell 12 has an electrode 1 in its finished state. The storage cell 12 in its finished state further comprises a cell housing 13, in which an electrolyte 14, in particular a liquid state, is contained. After the substrate 5 is coated with the mixture 2, the electrode 1 is arranged in the housing 13 and is in contact with the electrolyte 14, in particular immersed in the electrolyte 14. This is done, for example, in such a way that the electrode 1 is moved into the housing 13, while the electrolyte 14 is already in the housing 13, or it can be provided that the electrode 1 is first at least partially arranged in the cell housing 13 and then the electrolyte 14 is introduced into the cell housing 13. Afterwards, the coating 6 is in contact with the electrolyte 14, in particular in direct contact, wherein the fibers 4 of the coating 6 receive, in particular absorb, at least a portion of the electrolyte 14. In addition, the electrode 1 can be in contact with the electrolyte 14 before being inserted into the housing 13. The electrode 1 soaked with the electrolyte 14 is then introduced into the housing 13. In other words, the fibers 4 are soaked with the electrolyte 14. This makes it possible to ensure particularly favorable ion conductivity of the electrode 1 or of the storage cell 12 .

[0034] Depend on Figure 2 It can be seen that the base body 5 is coated with the mixture 2, for example, by extrusion. It is also conceivable that the base body 5 is coated with the mixture 2 by lamination. In the context of lamination, for example, the mixture 2 or the coating 6 is thermally and materially bonded to the base body 5, that is to say connected to the base body 5. Preferably, the mixture 2 also has Figure 2 The adhesive 15 , which is particularly schematically indicated by a circle in FIG. 1 , can comprise at least one or exactly one polymer, in particular polyvinyl fluoride.

[0035] Overall, it can be seen that the fibers act as small sponges for accommodating the electrolyte 14. As a result, a solvent-free production process for producing the electrode 1 can be achieved, wherein at the same time sufficient ion conductivity of the electrode 1 can be ensured. Such solvent-free production processes usually result in electrodes with very little porosity or no porosity. However, since the fibers 4 accommodate the electrolyte 14, sufficient accommodation capacity of the electrode 1 in terms of accommodating the electrolyte 14 can be ensured, thereby ensuring a favorable ion conductivity.

[0036] Since the mixture 2 has no solvent, which is at least largely expelled from the mixture 2 after the substrate 5 is coated with the mixture 2, the mixture 2 is solvent-free. This makes it possible to avoid complex work steps, such as drying or filtering, for at least largely removing the solvent from the mixture 2, so that the electrode 1 can be produced particularly time-efficiently and cost-effectively.

[0037] Reference numerals list

[0038] 1 Electrode

[0039] 2 Mixture

[0040] 3 Active Materials

[0041] 4. Fiber

[0042] 5 Matrix

[0043] 6 Coating

[0044] 7 Coating device

[0045] 8 Opening

[0046] 9 Arrow

[0047] 10 Opening

[0048] 11 Outer peripheral surface of the outer peripheral side

[0049] 12 Storage battery cells

[0050] 13 Battery cell housing

[0051] 14 Electrolytes

[0052] S1 First step

[0053] S2 Step 2

Claims

1. A method for producing an electrode (1) for a storage device (12) for storing electrical energy, wherein a substrate (5) is coated with at least one active material (3) for storing electrical energy, It is characterized in that The Method The following steps are involved: - providing a mixture (2) comprising an active material (3) and fibers (4); and - coating a substrate (5) with a mixture (2), the mixture being free of a solvent which contains the fibers (4) and which at least predominantly exits the mixture (2) after the coating of the substrate (5), wherein, by coating the substrate (5) with the mixture (2), a coating (6) having the active material (3) and the fibers (4) is formed on the substrate (5) from the mixture (2), wherein the substrate (5) is coated with the mixture (2) by extrusion and / or lamination, wherein the substrate (5) is not coated with a solvent before and after the coating of the substrate (5) with the mixture (2) by extrusion and / or lamination, thereby avoiding a drying step for the solvent, wherein the fibers absorb the electrolyte instead of the pores produced by the drying of the solvent in the mixture, wherein after coating the substrate (5) with the mixture (2), the coating (6) is brought into contact with an electrolyte (14) which is at least partially absorbed by the fibers (4), wherein the electrode (1) is brought into contact with the electrolyte (14) before it is inserted into the battery cell housing (13), and the electrode (1) wetted with the electrolyte (14) is then introduced into the battery cell housing (13), The fibers (4) are electrically conductive in this case, so that further conductive additives for electrical conductivity are dispensed with.

2. The method according to claim 1, characterized in that Cellulose fibers are used as the fibers (4).

3. The method according to claim 1 or 2, characterized in that: During the extrusion process, the substrate is coated with the mixture within the opening, before the opening and / or after the opening while the substrate is conveyed through the opening, so that the mixture is applied to the circumference of the outer circumference of the substrate; and / or During the lamination process, the mixture is applied to the peripheral surface of the outer circumference of the substrate in a hot or heated state of the substrate and / or in a hot or heated state of the mixture, thereby connecting the mixture or the coating to the substrate thermally and / or materially.

4. The method according to claim 1 or 2, characterized in that: The fibers (4) are made of non-combustible or non-combustible material.

5. The method according to claim 1 or 2, characterized in that: The mixture ( 2 ) also contains a binder ( 15 ).

6. The method according to claim 1 or 2, characterized in that: The electrolyte is a liquid electrolyte.

7. The method according to claim 1 or 2, characterized in that: The electrolyte is at least partially absorbed by the fibers (4).

8. Use of an electrode (1) produced by means of a method according to any one of claims 1 to 7, wherein: The electrode (1) is used as an electrode of a storage device (12) for storing electrical energy.

9. The use according to claim 8, characterized in that: The electrode is a positive electrode.

10. An electrode (1) for a storage device for storing electrical energy, wherein: The electrode ( 1 ) is produced by means of a method according to any of the preceding claims 1 to 7 .