Sensor package and method for installing the sensor package

By arranging a resin part and an adhesive layer on the base material, and utilizing the curing technology of the adhesive bonding layer, the problems of bonding position deviation and reduced sensitivity of the FBG sensor are solved, and a simple installation and high-durability package are achieved. Designed for outdoor use.

CN114424028BActive Publication Date: 2024-10-25NITTO DENKO CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202080065103.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-09-17
Filing Date
2020-09-16
Publication Date
2024-10-25
Estimated Expiration
2040-09-16

AI Technical Summary

Technical Problem

When an adhesive is used to attach the FBG sensor to a structure, positional deviation is likely to occur during the curing process of the adhesive, resulting in reduced sensor sensitivity. Especially when operating in unstable locations, the installation becomes complicated and the durability is insufficient.

Method used

A resin part and an adhesive layer are provided on the base material, and the FBG sensor is firmly bonded to the target object through the curing of the adhesive layer, and the combined structure of the resin part and the adhesive layer is used for temporary fixation and protection. Ensures accurate sensor installation and high durability.

Benefits of technology

It realizes the simple installation and positioning of the FBG sensor, maintains high sensitivity, and provides a high-durability package suitable for outdoor use, simplifying the operation process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114424028B_ABST
    Figure CN114424028B_ABST
Patent Text Reader

Abstract

The present invention relates to a sensor package that is attached to a target object, the sensor package comprising: a first substrate; an FBG sensor; a resin portion and a first adhesive layer located on the first substrate; and an adhesive layer, the adhesive layer being located on a surface of the resin portion that is opposite to the first substrate, the FBG sensor being held by the resin portion.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a sensor package and a method for installing the sensor package. Background Art

[0002] Conventionally, a sensor is used which is installed on a target object and measures physical changes such as vibration and strain of the target object and various information.

[0003] For example, Patent Document 1 describes a sensor module in which a sensor device is incorporated in a packaging member and an adhesive sheet is attached to the packaging member in order to reduce fluctuations in output characteristics of a sensor that monitors a state of a structure.

[0004] Patent document 2 describes a strain gauge comprising: a micro-adhesive sheet having a micro-adhesive / peelable surface on one side of a base sheet; and a strain gauge element formed by patterning a strain gauge element material by photolithography and provided on the adhesive / peelable surface of the micro-adhesive sheet.

[0005] Furthermore, Patent Document 3 describes a curable adhesive sheet that can easily bond a deformation converter to an adherend and that can allow the deformation converter to accurately detect deformation of the adherend.

[0006] Prior art literature

[0007] Patent Literature

[0008] Patent Document 1: Japanese Patent Application Publication No. 2016-194441

[0009] Patent Document 2: Japanese Patent Application Publication No. 2009-300096

[0010] Patent Document 3: Japanese Patent No. 6449795 Summary of the invention

[0011] Problem that the invention aims to solve

[0012] When attaching sensors such as FBG sensors to structures using adhesives, it takes time for the adhesive to cure, so there is a concern that the sensor attachment position may shift, and when using adhesives, the sensitivity of the sensor may be significantly reduced. Therefore, a sensor package with excellent workability is required that can be installed more easily without significantly reducing sensitivity even when working at high places, in places where scaffolding is unstable, or when the user is working with gloves.

[0013] Furthermore, the mounted sensor device is required to have high durability to withstand outdoor use, but conventional sensor packages still have room for improvement.

[0014] In view of the above problems, an object of the present invention is to provide a sensor package that can be easily installed and positioned without significantly reducing the sensitivity of the FBG sensor and has excellent workability. Another object is to provide a sensor package that is highly durable and suitable for outdoor use.

[0015] Solutions for solving problems

[0016] The inventors of the present invention have repeatedly conducted careful research and have come up with the idea that a resin portion holding the FBG sensor and an adhesive layer are provided on a substrate, and the adhesive layer is used to temporarily fix the sensor package body when it is attached to a target object. In addition, the inventors of the present invention have come to the conclusion that it is important to firmly adhere the resin portion holding the FBG sensor to the target object using an adhesive layer in order to prevent a significant decrease in the sensitivity of the FBG sensor.

[0017] In order to solve the above problems and achieve the object, the present invention has the following configurations.

[0018] [1]

[0019] A sensor package is attached to a target object, and the sensor package comprises:

[0020] The first substrate;

[0021] FBG sensor;

[0022] a resin portion and a first adhesive layer located on the first substrate; and

[0023] an adhesive layer, the adhesive layer being located on the surface of the resin portion that is opposite to the first substrate,

[0024] The FBG sensor is held by the resin portion.

[0025] [2]

[0026] The sensor package according to [1], wherein the adhesive layer is cured at room temperature.

[0027] 〔3〕

[0028] The sensor package according to [1] or [2], wherein the adhesive layer is cured by a curing agent.

[0029] [4]

[0030] The sensor package according to any one of [1] to [3], wherein at least a portion of the entire periphery of the resin portion holding the FBG sensor except for a surface on the adhesive bonding layer side is covered with the first adhesive layer.

[0031] 〔5〕

[0032] The sensor package according to any one of [1] to [4], wherein the first adhesive layer has an opening penetrating in the thickness direction.

[0033] The resin portion is provided so as to fill a gap between the FBG sensor disposed in the opening and the opening, thereby holding the FBG sensor.

[0034] [6]

[0035] The sensor package according to any one of [1] to [5], wherein surfaces of the first pressure-sensitive adhesive layer and the adhesive bonding layer that are attached to the target object are protected by a first release sheet.

[0036] 〔7〕

[0037] The sensor package according to any one of [1] to [6], wherein the first substrate is transparent or translucent.

[0038] 〔8〕

[0039] The sensor package according to any one of [1] to [7], further comprising a second adhesive layer and a second substrate in this order on a surface of the first substrate opposite to a surface on the first adhesive layer side.

[0040] 〔9〕

[0041] The sensor package according to [8], wherein the second substrate is a weather-resistant substrate.

[0042] 〔10〕

[0043] The sensor package according to [8] or [9], wherein a second release sheet is provided in a portion between the first substrate and the second adhesive layer, and the second release sheet has an extension portion extending and exposed from the second adhesive layer in a surface extension direction of the second release sheet.

[0044]

[11]

[0045] A method for installing a sensor package, which is the method for installing a sensor package as described in any one of [1] to

[10] ,

[0046] The adhesive layer in the sensor package is cured by a curing agent.

[0047] The installation method comprises:

[0048] The step of applying the curing agent to at least one of the adhesive layer and the target object; and

[0049] A step of attaching the sensor package to the target object via the adhesive layer.

[0050]

[12]

[0051] A method for installing a sensor package, which is the method for installing a sensor package as described in any one of [1] to

[10] ,

[0052] The adhesive layer in the sensor package is cured by a curing agent.

[0053] The installation method comprises:

[0054] The step of applying the curing agent to the adhesive layer;

[0055] The step of applying the curing agent to the target object; and

[0056] A step of attaching the sensor package to the target object such that the curing agent applied to the adhesive layer contacts the curing agent applied to the target object.

[0057] 〔13〕

[0058] A method for mounting a sensor package, comprising mounting the sensor package described in any one of [1] to [3] on a sensor package of a target object.

[0059] The surfaces of the first adhesive layer and the adhesive bonding layer in the sensor package that are attached to the target object are protected by a first release sheet.

[0060] The sensor package comprises, in order, the first substrate, the second adhesive layer, and the second substrate on a surface of the first adhesive layer opposite to the surface to be attached to the target object.

[0061] A second release sheet is provided at a portion between the first substrate and the second adhesive layer, wherein the second release sheet has an extension portion extending from the second adhesive layer and exposed in a surface extension direction of the second release sheet.

[0062] The installation method comprises: peeling off the first peeling sheet and applying a curing agent to the adhesive layer;

[0063] A step of attaching the release surface of the sensor package from which the first release sheet has been peeled off to the target object;

[0064] The second release sheet is peeled off, and the release surface of the second adhesive layer from which the second release sheet has been peeled off is attached to the first substrate.

[0065]

[14]

[0066] A kit comprising the sensor package according to any one of [1] to

[10] and a curing agent.

[0067] Effects of the Invention

[0068] The sensor package of one embodiment of the present invention can be easily mounted and positioned without significantly reducing the sensitivity of the FBG sensor, and has excellent workability. In addition, it has excellent durability and is suitable for outdoor use. BRIEF DESCRIPTION OF THE DRAWINGS

[0069] Figure 1 A schematic diagram of a configuration example of a sensor package.

[0070] Figure 2 for Figure 1 Schematic II cross-sectional view.

[0071] Figure 3 for Figure 1 Schematic II-II cross-sectional view.

[0072] Figure 4 A schematic diagram of a configuration example of a sensor package.

[0073] Figure 5 for Figure 4 Schematic III-III cross-sectional view.

[0074] Figure 6 for Figure 4 Schematic IV-IV cross-sectional view.

[0075] Figure 7 A cross-sectional schematic diagram of a configuration example of a sensor package.

[0076] Figure 8 A cross-sectional schematic diagram of a configuration example of a sensor package.

[0077] Fig. 9 A cross-sectional schematic diagram of a configuration example of a sensor package.

[0078] Fig.10 A cross-sectional schematic diagram of a configuration example of a sensor package.

[0079] Fig.11 (a) to (f) are schematic cross-sectional views for explaining a manufacturing example of a sensor package.

[0080] Fig.12 (a) to (f) are schematic diagrams for explaining a manufacturing example of a sensor package.

[0081] Fig.13(a) to (c) are schematic cross-sectional views for explaining a manufacturing example of a sensor package.

[0082] Fig.14 (a) to (d) are schematic diagrams for explaining a manufacturing example of a sensor package. DETAILED DESCRIPTION

[0083] Hereinafter, embodiments of the present invention will be described in detail.

[0084] It should be noted that, in the following drawings, the same symbols are sometimes used to describe components and parts that play the same role, and repeated descriptions are omitted or simplified. In addition, the embodiments described in the drawings are schematically illustrated to clearly describe the present invention, and may not accurately represent the size or scale of the actual product.

[0085] 〔Sensor package〕

[0086] The sensor package of an embodiment of the present invention is a sensor package attached to a target object, comprising: a first substrate; an FBG sensor; a resin portion and a first adhesive layer located on the aforementioned first substrate; and an adhesive bonding layer located on a surface of the aforementioned resin portion that is on the opposite side to the aforementioned first substrate, wherein the aforementioned FBG sensor is held by the aforementioned resin portion.

[0087] (First Embodiment)

[0088] Figure 1 FIG. 1 is a schematic diagram of a sensor package 100 according to a first embodiment of the present invention. Figure 2 for Figure 1 Schematic II cross-sectional view. Figure 3 for Figure 1 Schematic II-II cross-sectional view.

[0089] Figures 1 to 3 The sensor package 100 shown comprises: a first substrate 20; a FBG (Fiber Bragg Grating) sensor 10 attached to a target object; a resin portion 12 and a first adhesive layer 11 located on the first substrate 20; and an adhesive bonding layer 14 located on the surface of the resin portion 12 on the opposite side to the first substrate 20, and the FBG sensor 10 is held by the resin portion 12.

[0090] In the sensor package 100, at least a portion of the entire periphery of the resin portion 12 holding the FBG sensor 10 except for the surface on the adhesive layer side may be covered with the first adhesive layer 11. Figures 1 to 3 In the illustrated sensor package 100 , the surface on which the adhesive layer 14 is provided is the surface to be attached to the target object.

[0091] The FBG sensor 10 is formed by engraving a periodic diffraction grating on the core of the optical fiber 15 , and the detection signal of the FBG sensor 10 is output to the outside of the sensor package 100 . In addition, the optical fiber 15 may be covered with a covering material 13 .

[0092] The material of the covering material 13 is not particularly limited, and examples thereof include metal materials such as metal coatings, and resin materials such as polyimide, silicone, nylon, acrylic, and vinyl chloride. The covering material 13 may be a resin coating material obtained by coating the optical fiber 15 with a resin, or a sheath material, etc. The covering material 13 may be a single layer or multiple layers.

[0093] The first adhesive layer 11 is provided on the first substrate. By providing the first adhesive layer 11, when the sensor package is placed on the target object, the first adhesive layer 11 can be used for temporary fixation, and the adhesive layer can be firmly bonded by curing, which is excellent in workability. In addition, the first adhesive layer 11 eliminates the gap between the sensor package 100 and the target object, and the durability is excellent, so it is also possible to prevent the intrusion of external air and moisture into the FBG sensor 10.

[0094] The first adhesive layer preferably covers at least a portion of the entire periphery of the resin portion holding the FBG sensor, except for the surface attached to the target object side. This is because when the FBG sensor detects information from the target object, if there is an adhesive layer between the FBG sensor and the target object, the adhesive layer will mitigate the resulting deformation, thereby significantly reducing the detection sensitivity.

[0095] The first adhesive layer 11 may be formed of a plurality of adhesive layers. Figures 1 to 3 As shown, the first adhesive layer 11a and the first adhesive layer 11b are stacked, or as shown in FIG. Figures 4 to 6 As shown, the first adhesive layer 11c and the first adhesive layer 11d are placed opposite to each other. The thickness of the first adhesive layer 11a and the first adhesive layer 11b may be the same or different, and when different, one of them may be thicker.

[0096] When the covering material 13 is provided on the optical fiber 15, the first adhesive layer 11a and the first adhesive layer 11b may be provided with cuts at positions corresponding to the covering material 13, depending on the thickness thereof. By providing the cuts, the sensor package can be mounted on the target object with almost no gap between the first adhesive layer 11 and the target object, and the intrusion of external air and moisture into the FBG sensor 10 can be prevented, thereby achieving excellent durability.

[0097] When the maximum diameter of the covering material 13 (the outer diameter of the covering material 13 including the optical fiber 15) is smaller than the thickness of the first adhesive layer 11, there is no need to provide an incision in the first adhesive layer 11. The covering material 13 is buried in the first adhesive layer 11, which can prevent the intrusion of external air and moisture and has excellent durability.

[0098] When the covering material 13 is provided on the optical fiber 15 , the thickness of the first adhesive layer 11 is preferably the same as the maximum diameter (outer diameter) of the covering material 13 , or larger than the maximum diameter.

[0099] The outer diameter of the optical fiber is preferably 0.125 mm.

[0100] The thickness of the covering material 13 covering the optical fiber 15 is not particularly limited, but is usually 10 μm to 1 mm.

[0101] For example, an optical fiber having an outer diameter of 0.125 mm may be covered with a resin covering material, and the outer diameter of the covering material including the optical fiber is preferably set to 0.15 to 1 mm.

[0102] The first adhesive layer 11 may have an opening (hereinafter sometimes simply referred to as an opening) penetrating in the thickness direction.

[0103] When the FBG sensor is arranged in the opening and the gap between the FBG sensor and the opening is filled with the resin part, the FBG sensor does not contact the first adhesive layer, making it easier to obtain accurate information about the target object. Furthermore, by arranging the FBG sensor in the opening, the position of the FBG sensor can be visually confirmed, making it easier to position the sensor during installation.

[0104] The shape of the opening is not particularly limited, and may be circular, elliptical, polygonal, square, or rectangular.

[0105] The resin portion 12 is located on the first base material and serves to hold the FBG sensor 10 .

[0106] The FBG sensor 10 is preferably protected by the resin portion 12 so as not to be exposed to the outside air. The FBG sensor 10 may be embedded in the resin portion 12, or a portion of the FBG sensor 10 may be exposed from the resin portion 12. However, it is preferred that the entire periphery of the FBG sensor 10, except for the wiring, is embedded in the resin portion 12. When the entire periphery of the FBG sensor 10, except for the wiring, is embedded in the resin portion 12, the FBG sensor 10 detects information of the target object through the resin portion 12.

[0107] Alternatively, at least a portion of the entire periphery of the resin portion 12 excluding the surface to be attached to the target object may be covered with the first adhesive layer 11 .

[0108] When the first adhesive layer 11 has an opening penetrating in the thickness direction, the resin portion 12 may be provided to fill a gap between the FBG sensor 10 disposed in the opening and the opening to hold the FBG sensor 10 .

[0109] In order to improve the detection sensitivity of the FBG sensor 10, the resin portion 12 is preferably formed so that the surface of the resin portion 12 opposite to the first substrate and the surface (attachment surface) of the first adhesive layer 11 opposite to the first substrate are flush with each other.

[0110] The resin portion 12 and the first adhesive layer 11 are located on the first substrate 20, and the sensor package 100 includes an adhesive layer 14 located on the surface of the resin portion 12 that is opposite to the first substrate 20. Figures 1 to 3 As shown, the adhesive layer 14 can be provided in such a manner that when the sensor package 100 is attached to the target object, the resin portion 12 is attached to the target object via the adhesive layer 14. Thus, the FBG sensor 10 held by the resin portion 12 is attached to the target object via the resin portion 12 and the adhesive layer 14. That is, the FBG sensor 10 detects information of the target object not via the first adhesive layer 11 but via the resin portion 12 and the adhesive layer 14, thereby preventing a significant decrease in sensitivity.

[0111] (Second Embodiment)

[0112] In the second embodiment, the same components as those in the above-described embodiment are denoted by the same reference numerals, and detailed description thereof will be omitted.

[0113] Figure 4 FIG. 2 is a schematic diagram of a sensor package 200 according to a second embodiment of the present invention. Figure 5 for Figure 4 Schematic III-III cross-sectional view. Figure 6 for Figure 4 Schematic IV-IV cross-sectional view.

[0114] Figure 4 The sensor package 200 shown is Figure 1 The modified example of the sensor package 100 shown in FIG. Figure 1 The thickness of the first adhesive layer 11 is set to be approximately the same as the maximum diameter (thickness) of the covering material 13. The thickness of the first adhesive layer 11 may be larger than the maximum diameter of the covering material 13.

[0115] like Figures 4 to 6As shown, the sensor package 200 can make the first adhesive layer 11c and the first adhesive layer 11d of the shape formed by cutting the first adhesive layer 11 at the position corresponding to the covering material 13 dock with the covering material 13, thereby configuring the FBG sensor 10 in the opening portion of the first adhesive layer 11 and being held by the resin portion 12.

[0116] The thicknesses of the first adhesive layer 11 c and the first adhesive layer 11 d may be the same or different, but are preferably the same.

[0117] It should be noted that, in addition to the first adhesive layer 11c and the first adhesive layer 11d, a further Figure 1 The first adhesive layer 11a is formed in the first adhesive layer 11.

[0118] (Third Embodiment)

[0119] In the third embodiment, the same components as those in the above-described embodiment are denoted by the same reference numerals, and detailed description thereof will be omitted.

[0120] Figure 7 FIG. 4 is a schematic cross-sectional view of a sensor package 300 according to a third embodiment of the present invention.

[0121] Figure 7 The sensor package 300 shown is Figure 1 The modified example of the sensor package 100 shown in FIG. Figure 1 This is an embodiment in which the first adhesive layer 11 is provided as one layer.

[0122] The FBG sensor 10 in the sensor package 300 may be formed on an optical fiber 15, and the optical fiber 15 has a covering material 13. Figure 7 As shown, the optical fiber 15 with the FBG sensor 10 in the sensor package 300 may be arranged so that the cover material 13 is in contact with the first base material 20 .

[0123] (Fourth Embodiment)

[0124] In the fourth embodiment, the same components as those in the above-described embodiment are denoted by the same reference numerals, and detailed description thereof will be omitted.

[0125] Figure 8 FIG. 4 is a schematic cross-sectional view of a sensor package 400 according to a fourth embodiment of the present invention.

[0126] Figure 8 The sensor package 400 is shown as Figure 1 The modified example of the sensor package 100 shown in FIG. Figure 1 This is an embodiment in which the first adhesive layer 11 is provided as one layer.

[0127] The FBG sensor 10 in the sensor package 400 is formed on an optical fiber 15, and the optical fiber 15 has a covering material 13. Figure 8 As shown, the optical fiber 15 with the FBG sensor 10 in the sensor package 400 may be arranged in such a manner that the covering material 13 is in contact with the adhesive layer 14 .

[0128] (Fifth Embodiment)

[0129] In the fifth embodiment, the same components as those in the above-described embodiment are denoted by the same reference numerals, and detailed description thereof will be omitted.

[0130] Fig. 9 It is a schematic cross-sectional view of a configuration example of a sensor package according to a fifth embodiment of the present invention.

[0131] like Fig. 9 As shown, the sensor package 500 may include the second adhesive layer 16 and the second base material 17 in this order on the surface of the first base material 20 opposite to the surface on the first adhesive layer 11 side.

[0132] In addition, the sensor package 500 may include a second release sheet 19 at a portion between the first substrate 20 and the second adhesive layer 16. By including the second release sheet 19 at a portion between the first substrate 20 and the second adhesive layer 16, the second substrate 17 can be stacked on the first substrate 20 at any time. After the sensor package 500 is attached to the target object, if the second release sheet 19 is peeled off and the second substrate 17 is stacked on the first substrate 20, the FBG sensor 10 can be easily seen during attachment, positioning becomes easy, and workability is excellent.

[0133] The second release sheet 19 may also be provided with a split portion (Japanese: back cut). The split portion is formed by introducing a cutting line on the surface of the second release sheet 19 on the opposite side of the contact surface with the adhesive layer. The shape of the cutting line may be a straight line, a curved line such as a wave, or a combination thereof. In addition, the cutting line may be a solid line, a dotted line, or a combination thereof. By providing the split portion at the second release sheet 19, the second release sheet 19 can be easily removed.

[0134] In addition, the sensor package 500 may include a second release sheet 19 at a portion between the first substrate 20 and the second adhesive layer 16, wherein the second release sheet 19 has an extension portion extending from the second adhesive layer 16 and exposed in the surface extension direction of the second release sheet 19. When the second release sheet 19 has an extension portion, the extension portion becomes a gripping portion, thereby obtaining a sensor package with excellent operability. There is no particular limitation on the shape of the extension portion, and any appropriate shape may be adopted as required. Specific examples of the visual shape of the extension portion include a quadrilateral (including a trapezoid), a semi-elliptical shape, and the like. In addition, the end of the extension portion may also be a waveform, and the like. The length of the extension portion in the peeling direction is preferably 1 mm to 30 mm, and more preferably 5 mm to 20 mm. When the length of the extension portion in the peeling direction is within such a range, excellent peeling operability is obtained, and a sensor package with good operability can be obtained.

[0135] Next, a method for manufacturing the sensor package according to the embodiment of the present invention will be described.

[0136] [Method for manufacturing sensor package]

[0137] The manufacturing method of the sensor package according to the embodiment of the present invention includes: a step of providing a first adhesive layer 11 on a first substrate 20, a step of providing an FBG sensor 10 embedded in a resin portion 12, and a step of providing an adhesive bonding layer 14 located on a surface of the resin portion 12 on the opposite side to the first substrate 20.

[0138] In the step of providing the first adhesive layer 11, the first adhesive layer 11 may be directly formed on the first substrate by coating and curing the adhesive composition, or a preformed adhesive layer may be attached. When the first adhesive layer 11 is composed of a plurality of adhesive layers, the step of providing the first adhesive layer 11 may be performed in a plurality of steps.

[0139] For example, Figures 1 to 3 In the case of the sensor package 100 shown, the first adhesive layer 11 a may be disposed on the first substrate, and then the FBG sensor 10 may be disposed, and then the first adhesive layer 11 b may be disposed.

[0140] The FBG sensor 10 can be Figures 1 to 3 As shown in FIG. 1 , the adhesive layer 11 is disposed in the opening of the first adhesive layer 11 .

[0141] The optical fiber 15 with the FBG sensor 10 may be covered with the covering material 13. When the optical fiber 15 with the FBG sensor 10 is covered with the covering material 13, at least one of the first adhesive layer 11a and the first adhesive layer 11b may be cut at positions corresponding to the optical fiber 15 and the covering material 13.

[0142] The first adhesive layer 11 may be, for example, Figures 4 to 6 When the optical fiber 15 of the FBG sensor 10 is covered with the covering material 13 , at least one of the first adhesive layer 11c and the first adhesive layer 11d may be cut at positions corresponding to the optical fiber 15 and the covering material 13 .

[0143] You can Figure 7 As shown in FIG. 1 , the sensor package 300 is provided with the FBG sensor 10 on the first substrate 20, and then the first adhesive layer 11 and the resin portion are provided. Figure 8 As shown, in the sensor package 400 , the first adhesive layer 11 is provided on the first base material 20 , the FBG sensor 10 is provided, and then the resin portion is provided.

[0144] When the optical fiber 15 with the FBG sensor 10 is covered with the covering material 13 , the first adhesive layer 11 may be provided with a cutout at a position corresponding to the covering material 13 .

[0145] When the maximum diameter of the covering material 13 is smaller than the thickness of the first adhesive layer 11, there is no need to provide a cut in the first adhesive layer 11. The covering material 13 is buried in the first adhesive layer 11, which can prevent the intrusion of external air and moisture and has excellent durability.

[0146] In the step of providing the FBG sensor 10 embedded in the resin portion 12 , the FBG sensor 10 may be provided on the first substrate and then embedded in the resin portion 12 , or the FBG sensor 10 embedded in the resin portion 12 in advance may be provided on the first substrate.

[0147] When the first adhesive layer 11 has an opening, the FBG sensor 10 can be Figures 1 to 3 As shown, the FBG sensor 10 is arranged in the opening of the first adhesive layer 11. In addition, by filling the resin composition forming the resin portion 12 into the opening, the resin portion 12 can be provided in a manner to fill the gap between the FBG sensor arranged in the opening and the opening. Thus, the FBG sensor is embedded and held by the resin portion 12. The FBG sensor 10 embedded in the resin portion 12 in advance can also be placed on the first substrate 20, and at least a portion of the entire periphery of the resin portion 12 except for the surface attached to the target object side can be covered with the first adhesive layer 11.

[0148] In addition, the step of providing the first adhesive layer 11 on the first base material 20 and the step of providing the FBG sensor 10 embedded in the resin portion 12 may be performed simultaneously.

[0149] For example, the first adhesive layer 11b is arranged on an arbitrary peeling film 30, the FBG sensor 10 is placed in an opening portion of the first adhesive layer 11b, and then the first adhesive layer 11a is arranged opposite to the first adhesive layer 11b, and resin is filled into the opening portions of the first adhesive layer 11a and the first adhesive layer 11b and cured to form the resin portion 12, thereby embedding the FBG sensor 10.

[0150] Next, the first substrate 20 is stacked on the side of the first adhesive layer 11a opposite to the first adhesive layer 11b, and the release film 30 is peeled off, thereby simultaneously providing the first adhesive layer 11 and the FBG sensor 10 embedded in the resin portion 12 on the first substrate 20.

[0151] Then, the adhesive layer 14 can be provided on the surface of the resin portion 12 on the opposite side to the first substrate 20 by the step of providing the adhesive layer 14. The adhesive layer 14 can be directly formed by coating and curing the adhesive composition, or the pre-formed adhesive layer 14 can be attached to the resin portion 12.

[0152] The step of providing the adhesive layer 14 may be performed after the FBG sensor 10 is embedded in the resin portion 12 , after the resin portion 12 is disposed on the first substrate 20 , or before the resin portion 12 is disposed on the first substrate 20 .

[0153] like Fig. 9 As shown, the surface of the first pressure-sensitive adhesive layer and the adhesive bonding layer to be attached to the target object may be protected by the first release sheet, or the first release sheet may be attached.

[0154] The sensor package 500 may include the second adhesive layer 16 and the second base material 17 in this order on the surface of the first base material 20 opposite to the surface on the first adhesive layer 11 side.

[0155] Furthermore, the sensor package 500 may include a second release sheet 19 in a portion between the first base material 20 and the second adhesive layer 16 .

[0156] The second release sheet 19 may be laminated on a portion of the surface of the first substrate 20 on the opposite side to the surface on the first adhesive layer 11 side, and the second adhesive layer 16 and the second substrate 17 may be provided on the first substrate 20 and the second release sheet. The second adhesive layer 16 and the second substrate 17 may be formed by coating and curing a material for forming the second adhesive layer 16 or the second substrate 17, or the preformed second adhesive layer 16 and the second substrate may be attached.

[0157] In addition, the second substrate may be a weather-resistant substrate.

[0158] [How to install the sensor package]

[0159] Next, a method of mounting the sensor package according to the present embodiment will be described.

[0160] The sensor package installation method of the present embodiment includes a step of attaching the sensor package to a target object. Before the adhesive layer is cured, the target object and the FBG sensor held by the resin portion are bonded together using the adhesive layer and the first adhesive layer. The target object and the FBG sensor held by the resin portion are firmly bonded together by the curing of the adhesive layer, thereby preventing the sensitivity of the FBG sensor from being significantly reduced.

[0161] When the adhesive layer in the sensor package is cured by a curing agent, a step of bringing the adhesive layer into contact with the curing agent is required. The adhesive layer reacts by contacting with the curing agent. The step of bringing the adhesive layer into contact with the curing agent may include: applying the curing agent to at least one of the adhesive layer and the target object, and attaching the sensor package to the target object via the adhesive layer.

[0162] For example, the process of bringing the adhesive layer into contact with the curing agent may include: the process of applying the curing agent to the adhesive layer, and the process of attaching the sensor package to the aforementioned target object, or it may include the process of applying the curing agent to the target object and the process of attaching the sensor package to the aforementioned target object in a manner that the adhesive layer contacts the applied curing agent.

[0163] In addition, the process of bringing the adhesive layer into contact with the curing agent may include: a process of applying the curing agent to the adhesive layer, a process of applying the aforementioned curing agent to a target object, and a process of attaching the sensor package to the aforementioned target object in a manner such that the curing agent applied to the adhesive layer contacts the curing agent applied to the target object.

[0164] Furthermore, the adhesive layer and the curing agent may be heated as necessary. The heating temperature is, for example, preferably 50° C. or higher, more preferably 70° C. or higher, and, for example, preferably 130° C. or lower, more preferably 110° C. or lower.

[0165] The reaction temperature is preferably room temperature, which is a temperature at which the heating (for example, heating at 50° C. or higher) for reacting the adhesive layer with the curing agent is not performed, for example, less than 50° C., preferably 40° C. or lower, and for example, 10° C. or higher, preferably 20° C. or higher.

[0166] When the reaction temperature is room temperature, heating for reacting the adhesive layer and the curing agent is not required, and the sensor package can be bonded to the target object more easily, which is excellent in workability.

[0167] The reaction time is, for example, 1 hour or more, preferably 12 hours or more, and, for example, 96 hours or less, preferably 48 hours or less.

[0168] Thereby, the adhesive layer is cured to form a cured layer. It is preferred that the adhesive layer is cured at room temperature.

[0169] The cured layer allows the target object and the FBG sensor held by the resin portion to be firmly bonded together, thereby preventing a significant decrease in the sensitivity of the FBG sensor.

[0170] The shear adhesive strength of the cured layer is, for example, 0.1 MPa or more, preferably 0.4 MPa or more, more preferably 0.6 MPa or more, further preferably 0.7 MPa or more, particularly preferably 1.0 MPa or more, most preferably 2.3 MPa or more, further preferably 2.5 MPa or more, further preferably 3.5 MPa or more.

[0171] When the shear adhesive strength of the cured layer is not less than the above lower limit, the adhesive layer has excellent adhesiveness, and the target object and the FBG sensor held by the resin portion can be reliably bonded to each other.

[0172] The shear bonding strength of the solidified layer is measured by the following method. That is, the adhesive layer is clamped between two polyethylene terephthalate films that have been peeled off, one polyethylene terephthalate film is peeled off from the adhesive layer, the peeled adhesive layer is arranged on the first slate board, and then the other polyethylene terephthalate film is peeled off from the adhesive layer. Separately, a curing agent is arranged on the second slate board. Next, the adhesive layer and the curing agent are brought into contact in a manner that they are clamped by the first slate board and the second slate board, and are left for 24 hours to form a solidified layer. Thereafter, the first slate board and the second slate board are stretched in the shear direction at a speed of 5 mm / minute, and the strength when the two slate boards are peeled off is determined as the shear bonding strength.

[0173] In another embodiment of a sensor package installation method, the first adhesive layer and the surface of the aforementioned adhesive layer attached to the aforementioned target object are protected by a first release sheet, the sensor package comprises a first substrate, a second adhesive layer and a second substrate in sequence on the surface of the first adhesive layer on the opposite side to the surface attached to the target object, a second release sheet is provided on a portion between the first substrate and the aforementioned second adhesive layer, the second release sheet has an extension portion extending and exposed from the second adhesive layer along a surface extension direction of the second release sheet, the installation method comprises: a step of peeling off the aforementioned first release sheet to allow a curing agent to contact the aforementioned adhesive layer; a step of attaching the release surface of the aforementioned sensor package from which the aforementioned first release sheet has been peeled off to the aforementioned target object; and a step of peeling off the aforementioned second release sheet and attaching the release surface of the aforementioned second adhesive layer from which the aforementioned second release sheet has been peeled off to the aforementioned first substrate.

[0174] The step of bringing the adhesive layer into contact with the curing agent is the same as described above.

[0175] like Fig. 9 As shown, the sensor package has a second release sheet at a portion between the first substrate and the second adhesive layer, so that when the release surface from which the first release sheet has been peeled off is attached to a target object, the FBG sensor held by the resin portion can be visually observed. Therefore, positioning of the FBG sensor when attached to the target object becomes easy, and workability is excellent.

[0176] Next, the second release sheet is peeled off and the release surface of the second adhesive layer is attached to the first substrate. Fig.10 As shown, the second adhesive layer and the second substrate are sequentially stacked on the surface of the first substrate opposite to the resin portion. Thus, the first adhesive layer, the FBG sensor, the resin portion, and the first substrate are protected by the second adhesive layer and the second substrate, thereby improving the weather resistance of the sensor package.

[0177] [Kit including sensor package and curing agent]

[0178] The sensor package according to the embodiment of the present invention may be made into a set together with a curing agent. That is, the set according to the embodiment of the present invention includes the sensor package according to the embodiment of the present invention and a curing agent.

[0179] The sensor package and the curing agent in the kit according to the embodiment of the present invention have the same meanings as the sensor package and the curing agent described above, and the preferred embodiments are also the same.

[0180] According to the kit of the embodiment of the present invention, the sensor package and the target object can be bonded easily and firmly, the workability is excellent, and a significant decrease in the sensitivity of the FBG sensor can be prevented.

[0181] Next, materials and the like constituting the sensor package according to the embodiment of the present invention will be described.

[0182] [First base material]

[0183] As the first substrate, various substrates can be preferably used. As the first substrate, for example, resin film, paper, cloth, rubber film, foam film, metal foil, their composites, laminates, etc. can be used. Among them, from the viewpoint of adhesion and appearance, a film substrate containing a resin film is preferred. It is also advantageous to contain a resin film from the viewpoints of dimensional stability, thickness accuracy, processability, tensile strength, etc. As examples of resin films, polyolefin resin films such as PE, PP, and ethylene-propylene copolymers; polyester resin films such as PET, polybutylene terephthalate, and polyethylene naphthalate; vinyl chloride resin films; vinyl acetate resin films; polyimide resin films; polyamide resin films; fluorine resin films; cellophane; etc. As appropriate examples, resin films formed by PE, PP, and PET can be cited.

[0184] Among the resin films, polyester films are more preferred, and PET films are more preferred. The film substrate may have a single-layer structure or a multilayer structure having two or three or more layers.

[0185] The first substrate is preferably transparent or translucent.

[0186] In order to accurately obtain information of the target object, the installation position of the FBG sensor is important when the sensor package is installed on the target object. By making the first substrate transparent or translucent, the position of the FBG sensor in the sensor package can be grasped, so positioning when installing on the target object becomes easy and workability is excellent.

[0187] Specifically, the first substrate preferably has a total light transmittance of 80% or more (eg, 90% or more, typically 95% or more) and preferably has a haze value of 10% or less (eg, 5% or less).

[0188] From the viewpoint of ensuring the strength of the first substrate for functioning as a support body in the sensor package, the thickness of the first substrate is preferably 5 μm or more, more preferably 10 μm or more. In addition, from the viewpoint of achieving appropriate flexibility of the sensor package, the thickness of the first substrate is preferably 300 μm or less, more preferably 200 μm or less.

[0189] [First adhesive layer]

[0190] The first adhesive layer may be composed of an adhesive, and the adhesive is preferably a pressure-sensitive adhesive.

[0191] As the adhesive (adhesive composition) constituting the first adhesive layer, for example, one or a combination of two or more of a rubber adhesive, an acrylic adhesive, a vinyl alkyl ether adhesive, a silicone adhesive, a polyester adhesive, a polyamide adhesive, a urethane adhesive, a fluorine adhesive, a styrene-diene block copolymer adhesive, an epoxy adhesive, etc. can be used. In addition, a light-curing adhesive (ultraviolet curing adhesive, etc.) can also be used as the adhesive.

[0192] The thickness of the first adhesive layer is preferably 50 μm or more, more preferably 100 μm or more, and even more preferably 300 μm or more, and is preferably 2 mm or less, more preferably 1.5 mm or less, and even more preferably 1 mm or less.

[0193] When preparing the adhesive composition, when a curing reaction based on heat or active energy rays is used, it is preferred that the adhesive composition contain a polymerization initiator such as a thermal polymerization initiator or a photopolymerization initiator. As the polymerization initiator, a photopolymerization initiator can be appropriately used from the advantage of being able to shorten the polymerization time. The polymerization initiator can be used alone or in combination of two or more.

[0194] The first adhesive layer may also have a bubble structure. The "bubble structure" may be a structure having a gas component, and may be a "bubble" formed only by a gas component without a shell, or a "hollow microsphere" having a structure in which a gas component such as glass microbubbles is sealed in a shell.

[0195] The first adhesive layer (or adhesive composition) may contain suitable additives according to the purpose of the adhesive sheet. Such additives include, for example, crosslinking agents (e.g., polyisocyanate crosslinking agents, silicone crosslinking agents, epoxy crosslinking agents, alkyl etherified melamine crosslinking agents, etc.), tackifiers (e.g., tackifiers that are solid, semi-solid or liquid at room temperature, including rosin derivative resins, polyterpene resins, petroleum resins, oil-soluble phenolic resins, etc.), plasticizers, fillers, antioxidants, antioxidants, colorants (pigments, dyes, etc.), etc.

[0196] The adhesive composition forming the first adhesive layer can be prepared by mixing the monomer components (e.g., (meth) alkyl acrylate, etc.) forming the above-mentioned base polymer, hollow microspheres as required, a polymerization initiator, various additives, etc. by a known method. In addition, a part of the monomer components can be polymerized as required for viscosity adjustment, etc.

[0197] As a specific example of the preparation method, for example, the following steps can be cited. (i) The monomer components (for example, (meth) alkyl acrylate, other comonomers) and polymerization initiators (for example, photopolymerization initiators) used to form the base polymer are mixed to prepare a monomer mixture, (ii) the monomer mixture is subjected to a polymerization reaction corresponding to the type of polymerization initiator (for example, ultraviolet polymerization), and a composition (slurry) in which only a portion of the monomer components are polymerized is prepared. Then, (iii) hollow microspheres, fluorine-based surfactants, and other additives are mixed in the obtained slurry as needed. Furthermore, in the case of containing bubbles, (iv) bubbles are introduced into the compound obtained in (iii) and mixed, thereby obtaining an adhesive composition. It should be noted that the preparation method of the adhesive composition is not limited to this, for example, it can also be a preparation method in which fluorine-based surfactants and hollow microspheres are pre-mixed into the monomer mixture when preparing the aforementioned slurry.

[0198] The first adhesive layer can be formed by a known or even customary method. For example, the first adhesive layer is formed by applying the above-mentioned adhesive composition on the first substrate, and the first adhesive layer is cured (for example, cured by heat, cured by active energy rays) and dried as required. Among them, as mentioned above, curing based on irradiation with active energy rays is preferred.

[0199] Alternatively, the pressure-sensitive adhesive composition may be applied to a supporting substrate, cured and dried to produce a pressure-sensitive adhesive sheet, and then bonded to a first substrate, and the supporting substrate may be peeled off to produce a first pressure-sensitive adhesive layer.

[0200] As the pressure-sensitive adhesive sheet, commercially available products may be used. For example, “HYPERJOINT H7004, H7008, H7012, H8008, H9008” (substrate-less double-sided pressure-sensitive adhesive sheet) manufactured by Nitto Denko Corporation may be used.

[0201] 〔Resin Department〕

[0202] The resin portion is preferably transparent or translucent. By making the resin portion transparent or translucent, the position of the FBG sensor held by the resin portion can be more accurately grasped, and positioning when mounted on a target object becomes easy.

[0203] The initial tensile elastic modulus of the resin portion at 25°C is preferably 1.0×10 8 Pa or more, more preferably 5.0×10 8 Pa or more, more preferably 1.0×10 9 Pa or above.

[0204] The thickness of the resin portion is preferably 200 μm or more, more preferably 400 μm or more, and even more preferably 800 μm or more, and is preferably 3 mm or less, more preferably 2 mm or less, and even more preferably 1.5 mm or less.

[0205] The resin portion can be formed by a resin composition. The resin composition can contain a curable resin or a thermoplastic resin, and preferably contains a resin that cures at room temperature. By appropriately combining a curable resin and a curing agent, a resin that cures at room temperature can be made. As curable resins, for example, epoxy resins, phenolic resins, amino resins, unsaturated polyester resins, polyurethane resins, silicone resins, and thermosetting polyimide resins can be cited, preferably epoxy resins. Epoxy resins tend to have a low content of ionic impurities that may cause degradation of the FBG sensor, and are therefore preferred as curable resins in the resin portion. The resin composition may contain one curable resin, or may contain two or more curable resins.

[0206] As a curing agent for making the epoxy resin curable at room temperature, an amine curing agent, an imidazole curing agent, a thiol curing agent, or the like is preferable.

[0207] As epoxy resin, for example, bifunctional epoxy resins and multifunctional epoxy resins such as bisphenol A type epoxy resin, bisphenol F type epoxy resin, bisphenol S type epoxy resin, brominated bisphenol A type epoxy resin, hydrogenated bisphenol A type epoxy resin, bisphenol AF type epoxy resin, biphenyl type epoxy resin, naphthalene type epoxy resin, fluorene type epoxy resin, phenol novolac type epoxy resin, o-cresol novolac type epoxy resin, trihydroxyphenylmethane type epoxy resin, and tetraphenol ethane type epoxy resin can be cited. As epoxy resin, hydantoin type epoxy resin, triglycidyl isocyanurate type epoxy resin, and glycidylamine type epoxy resin can also be cited. In addition, the resin portion can contain one epoxy resin, or two or more epoxy resins.

[0208] The epoxy resin may be a commercially available product. For example, "jER828, bisphenol A type epoxy resin" (viscosity at 25° C.: 12 to 15 Ps·s) manufactured by Mitsubishi Chemical Corporation may be used.

[0209] A commercially available curing agent may be used, for example, "ST-12, modified aliphatic polyamine" (viscosity at 25° C.: 1650 to 3300 mPa·s) manufactured by Mitsubishi Chemical Corporation may be used.

[0210] The content of the curable resin in the resin portion is preferably 5 to 60% by mass, more preferably 10 to 50% by mass, from the viewpoint of appropriately curing the resin portion.

[0211] [Adhesive layer]

[0212] The adhesive layer of this embodiment is located on the surface of the resin portion that is opposite to the first substrate. Thus, the FBG sensor protected by the resin portion is attached to the target object by the adhesive layer.

[0213] The adhesive layer of this embodiment bonds the target object and the FBG sensor held by the resin portion before the adhesive layer is cured. The adhesive layer is cured to firmly bond the target object and the FBG sensor held by the resin portion, thereby preventing a significant decrease in sensitivity of the FBG sensor.

[0214] In order to detect information from the target object at a high level and prevent the sensitivity of the FBG sensor from being greatly reduced, the elastic modulus of the cured layer formed on the adhesive layer by curing is preferably 1.0×10 8 Pa or more, more preferably 3.0×10 8 Pa or more, more preferably 5.0×10 8 Pa or above.

[0215] The adhesive layer is a layer (sheet) that is cured by contacting and reacting with a curing agent, and has a generally flat plate shape extending in a plane direction (a direction perpendicular to the thickness direction) and having a flat front and back surface. The curing agent that cures the adhesive layer will be described later.

[0216] The adhesive layer is formed in a layer form from an adhesive component.

[0217] The adhesive component is not particularly limited as long as it is a main component of a two-component adhesive capable of forming a layer, and examples thereof include organic silicon compounds, polyol compounds such as polypropylene glycol, urethane resins, epoxy resins, etc. The adhesive component preferably contains epoxy resin as a main component. Thus, the FBG sensor and the resin portion can be bonded to the target object simply and firmly.

[0218] Examples of the epoxy resin include bisphenol-based epoxy resins such as bisphenol A epoxy resin, bisphenol F epoxy resin, bisphenol S epoxy resin, and hydrogenated bisphenol A epoxy resin, naphthalene epoxy resins, biphenyl epoxy resins, dicyclic epoxy resins, alicyclic epoxy resins, triglycidyl isocyanurate epoxy resins, hydantoin epoxy resins, glycidyl ether epoxy resins, and glycidyl amino epoxy resins.

[0219] As the epoxy resin, preferably, a bisphenol epoxy resin is used. The epoxy resin may be used alone or in combination of two or more.

[0220] The epoxy resin can be in any form of liquid, semi-solid and solid at room temperature, and preferably the use of a semi-solid epoxy resin alone and a combination of a liquid epoxy resin and a solid epoxy resin can be mentioned. Thus, a viscous layered adhesive layer can be reliably formed by the adhesive component.

[0221] The epoxy resin that is liquid at room temperature is specifically liquid at 25° C. The viscosity of the liquid epoxy resin at 25° C. is, for example, 30 Pa·s or more, preferably 80 Pa·s or more, for example, 500 Pa·s or less, preferably 300 Pa·s or less.

[0222] Specifically, the epoxy resin that is solid at room temperature is solid at 25° C. The softening point of the solid epoxy resin is, for example, 70° C. or higher, and preferably 75° C. or higher.

[0223] The blending ratio of the liquid epoxy resin to the solid epoxy resin (liquid epoxy resin / solid epoxy resin (mass ratio)) is, for example, 1.0 or more, preferably 1.5 or more, and for example, 4.0 or less, preferably 3.0 or less.

[0224] When the mixing ratio of the liquid epoxy resin to the solid epoxy resin is above the lower limit, the viscosity of the adhesive component can be reduced to prevent uneven coating, thereby obtaining a uniform adhesive layer. When the mixing ratio of the liquid epoxy resin to the solid epoxy resin is below the upper limit, a sticky layered adhesive layer can be obtained.

[0225] The blending ratio of the epoxy resin is set to a ratio in which the epoxy resin is the main component in the adhesive component. Specifically, it is, for example, 70% by mass or more, preferably 75% by mass or more, more preferably 80% by mass or more, further preferably 90% by mass or more, and for example, 100% by mass or less, relative to the adhesive component.

[0226] It is preferred that the adhesive component is composed of only the epoxy resin, that is, the blending ratio of the epoxy resin to the adhesive component is 100% by mass.

[0227] An acrylic polymer may be blended into the adhesive component as needed, thereby increasing the cohesive force of the adhesive component.

[0228] The acrylic polymer is obtained by reacting a monomer component containing a (meth)acrylate. The (meth)acrylate is an alkyl methacrylate and / or an alkyl acrylate, and specifically, methyl (meth)acrylate, ethyl (meth)acrylate, propyl (meth)acrylate, isopropyl (meth)acrylate, butyl (meth)acrylate, isobutyl (meth)acrylate, sec-butyl (meth)acrylate, tert-butyl (meth)acrylate, n-butyl (meth)acrylate, pentyl (meth)acrylate, isopentyl (meth)acrylate, hexyl (meth)acrylate, heptyl (meth)acrylate, octyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, (meth)acrylate) (meth)acrylates having an alkyl group having 1 to 20 carbon atoms, such as isooctyl (meth)acrylate, nonyl (meth)acrylate, isononyl (meth)acrylate, decyl (meth)acrylate, isodecyl (meth)acrylate, undecyl (meth)acrylate, dodecyl (meth)acrylate, tridecyl (meth)acrylate, tetradecyl (meth)acrylate, pentadecyl (meth)acrylate, hexadecyl (meth)acrylate, heptadecyl (meth)acrylate, octadecyl (meth)acrylate, nonadecyl (meth)acrylate, eicosyl (meth)acrylate, and the like.

[0229] As the (meth)acrylate, preferably, a (meth)acrylate of an alkyl group having 2 to 14 carbon atoms is used, and more preferably, a (meth)acrylate of an alkyl group having 4 to 9 carbon atoms is used.

[0230] The (meth)acrylate may be used alone or in combination of two or more.

[0231] The blending ratio of the (meth)acrylic acid ester is, for example, 70 mass % or more, preferably 80 mass % or more, and for example, 99 mass % or less, preferably 98 mass % or less, based on the monomer components.

[0232] The monomer component may contain a copolymerizable monomer copolymerizable with the (meth)acrylic acid ester.

[0233] Examples of the copolymerizable monomer include carboxyl group-containing monomers such as (meth)acrylic acid, itaconic acid, maleic acid, crotonic acid, and maleic anhydride, or their anhydrides; hydroxyl group-containing (meth)acrylates such as 2-hydroxyethyl (meth)acrylate and 3-hydroxypropyl (meth)acrylate; amide group-containing monomers such as (meth)acrylamide, N,N-dimethyl (meth)acrylamide, N-hydroxymethyl (meth)acrylamide, N-methoxymethyl (meth)acrylamide, and N-butoxymethyl (meth)acrylamide; vinyl esters such as vinyl acetate; aromatic vinyl compounds such as styrene and vinyltoluene; (meth)acrylonitrile; N-(meth)acryloylmorpholine; and N-vinyl-2-pyrrolidone.

[0234] As the copolymerizable monomer, preferably, a carboxyl group-containing monomer and a hydroxyl group-containing (meth)acrylate are mentioned, and more preferably, (meth)acrylic acid and 2-hydroxyethyl (meth)acrylate are mentioned.

[0235] These copolymerizable monomers may be used alone or in combination of two or more thereof. Preferably, a carboxyl group-containing monomer and a hydroxyl group-containing (meth)acrylate are used in combination, and more preferably, a (meth)acrylic acid and 2-hydroxyethyl (meth)acrylate are used in combination.

[0236] The blending ratio of the copolymerizable monomer is, for example, 0.1 parts by mass or more, preferably 0.3 parts by mass or more, and for example, 15 parts by mass or less, preferably 10 parts by mass or less, based on 100 parts by mass of the (meth)acrylate.

[0237] When reacting the monomer components, for example, (meth)acrylate and, if necessary, copolymerizable monomers are blended to prepare the monomer components, which are then prepared by a known polymerization method such as solution polymerization, bulk polymerization, emulsion polymerization, or various radical polymerizations.

[0238] As the polymerization method, solution polymerization is preferably used.

[0239] In solution polymerization, for example, a monomer component and a polymerization initiator are mixed in a solvent to prepare a monomer solution, and then the monomer solution is heated.

[0240] As the solvent, for example, an organic solvent can be cited. As the organic solvent, for example, aromatic solvents such as toluene, benzene, and xylene, ether solvents such as ethyl acetate, ketone solvents such as acetone and methyl ethyl ketone, ester solvents such as ethyl acetate, and amide solvents such as N,N-dimethylformamide can be cited. The solvent can be used alone or in combination of two or more, and preferably an aromatic solvent and an ether solvent can be used in combination. The mixing ratio of the solvent is, for example, 10 parts by mass or more, preferably 50 parts by mass or more, relative to 100 parts by mass of the monomer component, and, for example, 1000 parts by mass or less, preferably 500 parts by mass or less.

[0241] Examples of the polymerization initiator include peroxide-based polymerization initiators and azo-based polymerization initiators.

[0242] Examples of the peroxide-based polymerization initiator include organic peroxides such as peroxycarbonate, ketone peroxide, peroxyketal, hydrogen peroxide, dialkyl peroxide, diacyl peroxide, and peroxyester.

[0243] Examples of the azo polymerization initiator include azo compounds such as 2,2'-azobisisobutyronitrile, 2,2'-azobis(2-methylbutyronitrile), 2,2'-azobis(2,4-dimethylvaleronitrile) and dimethyl 2,2'-azobisisobutyrate.

[0244] As the polymerization initiator, preferably, an azo polymerization initiator is used.

[0245] The mixing ratio of the polymerization initiator is, for example, 0.01 parts by mass or more, preferably 0.05 parts by mass or more, and, for example, 5 parts by mass or less, preferably 3 parts by mass or less, based on 100 parts by mass of the monomer components.

[0246] The heating temperature is, for example, 50° C. or higher and 80° C. or lower, and the heating time is, for example, 1 hour or higher and 24 hours or lower.

[0247] Thus, the monomer components are polymerized to obtain an acrylic polymer solution containing an acrylic polymer.

[0248] The acrylic polymer solution is mixed with the epoxy resin in such a manner that the mixing ratio of the acrylic polymer is, for example, 1 part by mass or more, preferably 2 parts by mass or more, and for example, 50 parts by mass or less, and preferably 30 parts by mass or less, relative to 100 parts by mass of the adhesive component. In addition, the mixing ratio of the acrylic polymer is, for example, 1 part by mass or more, preferably 2 parts by mass or more, and for example, 43 parts by mass or less, and preferably 35 parts by mass or less, relative to 100 parts by mass of the epoxy resin.

[0249] When the blending ratio of the acrylic polymer is not less than the above lower limit, the cohesive force and thus the adhesive force of the pressure-sensitive adhesive component are improved, and the peel adhesive force of the pressure-sensitive adhesive layer can be improved.

[0250] When the blending ratio of the acrylic polymer is not more than the above upper limit, curing is possible.

[0251] A small amount of a curing agent may be blended into the adhesive component. This can increase the cohesive force of the adhesive layer. Examples of the curing agent are described below.

[0252] The mixing ratio of the curing agent is adjusted to a ratio that improves the peeling adhesive strength of the adhesive layer and slightly cures the adhesive component (incompletely cures).

[0253] In order to obtain the adhesive component, for example, an epoxy resin and, if necessary, an acrylic polymer (acrylic polymer solution) and / or a curing agent are mixed, and the mixture is diluted with a solvent as necessary to prepare a varnish.

[0254] The solvent may be any solvent as long as it can dissolve the adhesive component, and examples thereof include the above-mentioned solvents. Preferably, a ketone solvent is used as the solvent.

[0255] The concentration of the adhesive component in the varnish is, for example, 20 mass % or more, preferably 40 mass % or more, and for example, 80 mass % or less, preferably 70 mass % or less.

[0256] When an acrylic polymer is blended into the adhesive component, a crosslinking agent may be blended when the adhesive component is prepared.

[0257] Examples of the crosslinking agent include isocyanate crosslinking agents, aziridine crosslinking agents, epoxy crosslinking agents, and metal chelate crosslinking agents. Preferably, an isocyanate crosslinking agent is used.

[0258] Examples of the isocyanate crosslinking agent include aromatic diisocyanates such as tolylene diisocyanate and xylene diisocyanate, alicyclic diisocyanates such as isophorone diisocyanate, aliphatic diisocyanates such as hexamethylene diisocyanate, and modified products of these isocyanates (specifically, toluene diisocyanate adducts of trimethylolpropane, etc.).

[0259] As the cross-linking agent, preferably, a modified product of isocyanate is used.

[0260] The blending ratio of the crosslinking agent is, for example, 1 part by mass or more, preferably 5 parts by mass or more, and for example, 20 parts by mass or less, preferably 15 parts by mass or less, based on 100 parts by mass of the acrylic polymer.

[0261] Then, as described later, the adhesive layer is formed to a predetermined thickness by applying an adhesive component on the substrate and drying it.

[0262] The thickness of the adhesive layer is, for example, 1 μm or more, preferably 5 μm or more, more preferably 10 μm or more, and, for example, 1000 μm or less, preferably 500 μm or less, more preferably 100 μm or less.

[0263] The curing agent contacts and reacts with the adhesive layer, thereby curing the adhesive layer and forming a curing agent layer (sheet). In this case, it has a generally flat plate shape extending in the plane direction (direction perpendicular to the thickness direction) and having a flat surface and back.

[0264] The curing agent layer is formed in a layer form by a curing component, and the curing component contains a curing agent.

[0265] The curing agent is not particularly limited as long as it is a curing agent for a two-component adhesive. When the adhesive component contains an epoxy resin, examples thereof include epoxy resin curing agents such as imidazole compounds, amine compounds, and amide compounds.

[0266] Examples of the imidazole compound include methylimidazole, 2-ethyl-4-methylimidazole, 1-isobutyl-2-methylimidazole, 1-benzyl-2-methylimidazole, 2-ethyl-4-methylimidazole, ethylimidazole, isopropylimidazole, 2,4-dimethylimidazole, phenylimidazole, undecylimidazole, heptadecylimidazole, 2-phenyl-4-methylimidazole, 2-phenyl-4,5-dihydroxymethylimidazole, and 2-phenyl-4-methyl-5-hydroxymethylimidazole. Preferred examples include 1-isobutyl-2-methylimidazole, 1-benzyl-2-methylimidazole, and 2-ethyl-4-methylimidazole. More preferred examples include 1-isobutyl-2-methylimidazole and 1-benzyl-2-methylimidazole. Further preferred examples include 1-isobutyl-2-methylimidazole.

[0267] Examples of the amine compound include ethylenediamine, propylenediamine, diethylenetriamine, triethylenetetramine, amine adducts thereof, m-phenylenediamine, diaminodiphenylmethane, and diaminodiphenylsulfone.

[0268] Examples of the amide compound include dicyandiamide and polyamide, and preferably dicyandiamide is used.

[0269] As the curing agent, preferably, an imidazole compound is used.

[0270] The curing agent may be used alone or in combination of two or more.

[0271] The mixing ratio of the curing agent relative to the curing component is, for example, 10% by mass or more, preferably 30% by mass or more, more preferably 50% by mass or more, further preferably 80% by mass or more, particularly preferably 90% by mass or more, and, for example, 100% by mass or less. When the mixing ratio of the curing agent is above the above lower limit, the adhesiveness of the adhesive layer is excellent.

[0272] It is preferred that the curing component is formed of only the curing agent, that is, the ratio of the curing agent is 100% by mass relative to the curing component.

[0273] A curing accelerator may be blended into the curing component as required.

[0274] Examples of the curing accelerator include urea compounds such as 3-(3,4-dichlorophenyl)-1,1-dimethylurea (DCMU), N'-phenyl-N,N-dimethylurea, and 1,1'-(methyl-m-phenylene)bis(3,3'-dimethylurea); tertiary amine compounds such as triethylenediamine and tri-2,4,6-dimethylaminomethylphenol; phosphorus compounds such as triphenylphosphine, tetraphenylphosphonium tetraphenylborate, and tetra-n-butylphosphonium-o,o-diethyldithiophosphate; quaternary ammonium salt compounds; and organic metal salt compounds. Preferably, a urea compound is used, and more preferably, 3-(3,4-dichlorophenyl)-1,1-dimethylurea is used.

[0275] The curing accelerator may be used alone or in combination of two or more.

[0276] The mixing ratio of the curing accelerator is, for example, 10% by mass or more, preferably 15% by mass or more, more preferably 25% by mass or more, and, for example, 40% by mass or less relative to the curing component. The mixing ratio of the curing accelerator is, for example, 10% by mass or more, preferably 25% by mass or more, and, for example, 60% by mass or less, and preferably 50% by mass or less relative to 100% by mass of the curing agent.

[0277] When preparing the curing component, a curing agent and, if necessary, a curing accelerator are mixed.

[0278] When the curing agent is in a solid state, the curing agent is dissolved in a solvent as necessary to prepare a varnish.

[0279] The solvent may be any solvent as long as it can dissolve the curing component, and examples thereof include the solvents described above.

[0280] The concentration of the curing component in the varnish is, for example, 10 mass % or more, preferably 20 mass % or more, and for example, 90 mass % or less, preferably 50 mass % or less.

[0281] Thus, a curing component was prepared.

[0282] Then, as described later, the curing agent is formed to a predetermined thickness by applying a curing component on the adhesive layer or the substrate and drying it.

[0283] The thickness when the curing agent is applied is, for example, 1 μm or more, preferably 5 μm or more, more preferably 10 μm or more, and, for example, 1000 μm or less, preferably 800 μm or less, more preferably 500 μm or less.

[0284] Then, the adhesive layer is sandwiched between the target object, the FBG sensor, and the resin portion so that the adhesive layer is in contact with the resin portion holding the FBG sensor and the curing agent is in contact with the adhesive layer.

[0285] In the adhesive layer, the adhesive component has pressure-sensitive adhesive properties before curing.

[0286] It should be noted that the pressure-sensitive adhesiveness before curing means that the adhesive component has pressure-sensitive adhesiveness before the adhesive component is completely cured by the reaction between the adhesive component and the curing component, specifically: from before the adhesive component and the curing component are mixed until the adhesive component is completely cured after mixing.

[0287] That is, the adhesive layer containing the adhesive component has pressure-sensitive adhesive properties.

[0288] Specifically, the peel adhesion of the adhesive layer to the aluminum plate is, for example, 0.5 N / 20 mm or more, preferably 1.0 N / 20 mm or more, more preferably 2.0 N / 20 mm or more, further preferably 3.0 N / 20 mm or more, particularly preferably 3.5 N / 20 mm or more, and, for example, 10 N / 20 mm or less.

[0289] When the peel adhesion of the adhesive layer to the aluminum plate is not less than the above lower limit, the adhesive layer has excellent pressure-sensitive adhesiveness, and the FBG sensor and the target object can be bonded and positioned.

[0290] The peel strength of the adhesive layer was determined by laminating the adhesive layer to an aluminum plate and then peeling the adhesive layer from the aluminum plate at 90 degrees at a speed of 300 mm / min.

[0291] Thus, it is preferable that the adhesive layer has pressure-sensitive adhesiveness so that the target object and the FBG sensor are bonded together by the adhesive layer and the first adhesive layer before the adhesive layer is cured. Therefore, reliable positioning of the FBG sensor to the target object becomes easy.

[0292] Thereafter, the adhesive layer reacts with the curing agent to be cured.

[0293] The reaction temperature is, for example, room temperature.

[0294] Furthermore, the adhesive layer and the curing agent may be heated as necessary. The heating temperature is, for example, 50° C. or higher, preferably 70° C. or higher, and, for example, 160° C. or lower, preferably 110° C. or lower.

[0295] The reaction temperature is preferably room temperature, which is a temperature at which the above-mentioned heating (for example, heating at 50° C. or higher) for reacting the adhesive layer with the curing agent is not performed, for example, less than 50° C., preferably 40° C. or lower, and for example, 10° C. or higher, preferably 20° C. or higher.

[0296] When the reaction temperature is room temperature, heating for reacting the adhesive layer with the curing agent is not required, and the FBG sensor 10 can be bonded to the target object more easily. In addition, damage to the FBG sensor 10 due to heating can be prevented.

[0297] The reaction time is, for example, 15 minutes or more, preferably 1 hour or more, more preferably 12 hours or more, and, for example, 96 hours or less, preferably 48 hours or less. Thus, the adhesive layer is cured. Preferably, the adhesive layer is cured at room temperature.

[0298] The thickness of the adhesive layer after curing is, for example, 1 μm or more, preferably 5 μm or more, more preferably 30 μm or more, and, for example, 2000 μm or less, preferably 1000 μm or less, more preferably 500 μm or less, further preferably 100 μm or less.

[0299] The FBG sensor and the resin portion are bonded to the target object using the cured adhesive layer.

[0300] [Second base material]

[0301] The second substrate is preferably a film, preferably a resin film that plays a protective and decorative role. As the second substrate, for example, it can be a weather-resistant film such as a moisture-resistant film, a light-resistant film, a surface protection film such as an appearance film, a decorative film, an anti-damage film, etc. From the viewpoint of outdoor use, it is preferably a weather-resistant film.

[0302] As the resin constituting the resin film, for example, there can be mentioned polyimide, polyethylene (PE), polypropylene (PP), fluorinated ethylene propylene copolymer (FEP), ethylene tetrafluoroethylene copolymer (ETFE), polytetrafluoroethylene (PTFE), polyethylene terephthalate (PET), tetrafluoroethylene-perfluoroalkyl vinyl ether copolymer (PFA), or polyvinylidene fluoride (PVDF), etc., preferably polyvinylidene fluoride (PVDF).

[0303] [Second adhesive layer]

[0304] As the second adhesive layer, any adhesive layer can be used without particular limitation. For example, an adhesive layer using an acrylic acid polymer, a silicone polymer, a polyester, a polyurethane, a polyamide, a polyvinyl ether, a vinyl acetate / vinyl chloride copolymer, a modified polyolefin, an epoxy system, a fluorine system, a natural rubber, a synthetic rubber, and other rubber-based polymers as the base polymer can be appropriately selected. From the aspects of showing appropriate wettability, cohesiveness, and adhesion, as well as excellent weather resistance, heat resistance, etc., an acrylic acid adhesive is preferably used.

[0305] 〔Peel-off sheet〕

[0306] The first release sheet and the second release sheet (separator) for protecting the first and second pressure-sensitive adhesive layers until use will be described.

[0307] As the first release sheet and the second release sheet, conventional release paper can be used without particular limitation. For example, a substrate having a release treatment layer, a low-adhesion substrate formed of a fluorine-based polymer, a low-adhesion substrate formed of a non-polar polymer, etc. can be used.

[0308] Examples of the substrate having a release treatment layer include plastic films and papers that have been surface-treated with a release treatment agent such as a silicone-based, long-chain alkyl-based, fluorine-based, or molybdenum sulfide-based release treatment agent.

[0309] Examples of the fluorine-based polymer of the low-adhesive substrate include polytetrafluoroethylene, polychlorotrifluoroethylene, polyethylene fluoride, polyvinylidene fluoride, tetrafluoroethylene-hexafluoropropylene copolymer, and chlorofluoroethylene-vinylidene fluoride copolymer.

[0310] As the non-polar polymer of the low adhesive substrate formed by the non-polar polymer, for example, olefin resins (such as polyethylene, polypropylene, etc.) can be cited. It should be noted that the release sheet can be formed by a known or even conventional method. In addition, the thickness of the release sheet is not particularly limited.

[0311] 〔Target audience〕

[0312] There are no particular restrictions on the target objects to which the FBG sensor is attached, as long as they can be used as objects for measurement based on the FBG sensor. For example, various structures such as metal products, wood products, plastic products, glass products, buildings (inner and outer walls, floors, and ceilings, roads, railways, bridges, etc.), electronic equipment, and transportation equipment (for example, vehicles such as automobiles, two-wheeled vehicles and railways, and ships, etc.) can be cited.

[0313] Example

[0314] Hereinafter, the present invention will be specifically described by way of Examples, but the present invention is not limited to these Examples.

[0315] [Production of adhesive layer]

[0316] 69 parts by mass of liquid bisphenol A epoxy resin (trade name "jER828", manufactured by Mitsubishi Chemical), 30 parts by mass of solid bisphenol A epoxy resin (trade name "jER1256", manufactured by Mitsubishi Chemical), and 1 part by mass of solid special novolac epoxy resin (trade name "jER157S70", manufactured by Mitsubishi Chemical) were mixed, and methyl ethyl ketone was added for dilution so that the epoxy resin concentration became 65% by mass to prepare a varnish. It was applied to the release-treated surface of a release-treated polyethylene terephthalate film (trade name "Diafoil MRF#38", manufactured by Mitsubishi Resins Co., Ltd.) in a manner such that the thickness after drying became 50 μm, and it was heated at 80°C for 3 minutes to dry it to obtain an adhesive layer. Thereafter, the adhesive layer was brought into contact with another polyethylene terephthalate film in a manner such that the adhesive layer was sandwiched between two polyethylene terephthalate films.

[0317] [Production Example 1]

[0318] The adhesive layer (Nitto Denko, HYPERJOINT H7008) was cut into a size of 50 mm × 30 mm. Fig.12 As shown in (a) of FIG. 1 , the central portion is cut to provide an opening of 20 mm×10 mm, thereby preparing the first adhesive layer 11 a and the first adhesive layer 11 b .

[0319] The first adhesive layer 11b is formed as Fig.11 (a) and Fig.12 As shown in (a), it is arranged on a release film 30 (Diafoil MRF#38 manufactured by Mitsubishi Plastics).

[0320] like Fig.11 (b) and Fig.12 As shown in (b), an optical fiber with an FBG sensor 10 having an outer diameter of 0.125 mm is placed so that the FBG sensor 10 is located in the opening of the first adhesive layer 11b.

[0321] Furthermore, if Fig.11 (c) and Fig.12 As shown in (c), the first adhesive layer 11a is stacked on the first adhesive layer 11b and the optical fiber. At this time, the first adhesive layer 11a is pressed against the first adhesive layer 11b. As a result, the gap between the optical fiber and the first adhesive layer 11a and the first adhesive layer 11b is filled, and the FBG sensor 10 is arranged in the opening of the first adhesive layer 11a and the first adhesive layer 11b.

[0322] Then, if Fig.11 (d) and Fig.12As shown in (d), a resin that cures at room temperature, which is a mixture of epoxy resin (Mitsubishi Chemical, jER828) and curing agent (Mitsubishi Chemical, ST-12) in a mass ratio of 100:50, is filled into the opening, and allowed to stand at room temperature to cure, thereby forming a resin portion 12.

[0323] A PET substrate (Lumirror S-10#188 manufactured by Toray Industries, Inc.) as the first substrate 20 was prepared as follows. Fig.11 (e) and Fig.12 As shown in (e), the first adhesive layer 11a is laminated to produce a laminate.

[0324] The adhesive layer prepared above is cut into pieces of 20 mm×10 mm to prepare an adhesive layer 14. Fig.11 (f) and Fig.12 As shown in (f), the release film 30 is peeled off from the laminate, and the adhesive layer 14 is bonded to the resin portion 12 to manufacture a sensor package.

[0325] [Production Example 2]

[0326] like Fig.13 As shown in (a), the optical fiber 15 with the FBG sensor 10 covered with the covering material 13 having an outer diameter of 0.9 mm is placed on a release film 30 (Diafoil MRF#38 manufactured by Mitsubishi Plastics).

[0327] The adhesive layer (HYPERJOINT H7008 manufactured by Nitto Denko Corporation) was cut into a size of 50 mm × 15 mm. Fig.13 As shown in (b), a portion is further cut out to a size of 20 mm×5 mm to prepare a first adhesive layer 11c and a first adhesive layer 11d in a U-shape.

[0328] like Fig.13 As shown in (b), the cover material 13 is sandwiched between the first adhesive layer 11c and the first adhesive layer 11d in the shape of a "コ" character. At this time, the first adhesive layer 11a and the first adhesive layer 11b are pressed against the release film 30. Thus, the gap between the cover material 13 and the first adhesive layer 11c and the first adhesive layer 11d is filled, and the FBG sensor 10 is arranged in the opening formed by the first adhesive layer 11c and the first adhesive layer 11d.

[0329] Then, if Fig.13 As shown in (c), a resin that cures at room temperature, which is a mixture of epoxy resin (Mitsubishi Chemical, jER828) and curing agent (Mitsubishi Chemical, S-12) in a mass ratio of 100:50, is filled into the opening, left to stand at room temperature to cure, and a resin portion 12 is formed.

[0330] Next, a PET substrate (manufactured by Toray Industries, Ltd., Lumirror S-10#188) serving as the first substrate 20 is laminated on the first adhesive layer 11a to produce a laminate, the peeling film 30 is peeled off from the laminate, and the adhesive layer 14 cut into 20 mm×10 mm is adhered to the resin portion 12 to manufacture a sensor package.

[0331] [Production Example 3]

[0332] A sensor package was manufactured in the same manner as in Manufacturing Example 2 except that the optical fiber with FBG sensor was changed to one covered with a covering material having an outer diameter of 0.155 mm (the outer diameter of the covering material including the optical fiber was 0.155 mm).

[0333] [Production Example 4]

[0334] A sensor package was manufactured in the same manner as in Manufacturing Example 2 except that the optical fiber with FBG sensor was changed to one covered with a covering material having an outer diameter of 1 mm (the outer diameter of the covering material including the optical fiber was 1 mm).

[0335] Industrial Applicability

[0336] The sensor package of the present invention can be easily installed and positioned without significantly reducing the sensitivity of the FBG sensor, and has excellent workability. In addition, it has excellent durability and can be suitable for outdoor use.

[0337] While the present invention has been described in detail and with reference to specific embodiments, it will be apparent to one skilled in the art that various changes and modifications can be made therein without departing from the spirit and scope of the present invention.

[0338] This application is based on the Japanese patent application (Japanese Patent Application No. 2019-168780) filed on September 17, 2019, the contents of which are incorporated into this application as a reference.

[0339] Description of Reference Numerals

[0340] 100, 200, 300, 400, 500 sensor packages

[0341] 10 FBG sensor

[0342] 11, 11a, 11b, 11c, 11d: first adhesive layer

[0343] 12 Resin Department

[0344] 13 Covering material

[0345] 14. Bonding layer

[0346] 15. Fiber Optics

[0347] 16 Second adhesive layer

[0348] 17 Second base material

[0349] 18 1st peeling sheet

[0350] 19 Second peeling sheet

[0351] 20 1st base material

[0352] 30 Peel Film

Claims

1. A sensor package, which is attached to a target object, the sensor package comprising: The first substrate; FBG sensor; a resin portion and a first adhesive layer located on the first substrate; and an adhesive layer, the adhesive layer being located on a surface of the resin portion that is opposite to the first substrate, The first adhesive layer is composed of an adhesive, and the adhesive contains at least one adhesive selected from the group consisting of a rubber adhesive, an acrylic adhesive, a vinyl alkyl ether adhesive, a silicone adhesive, a polyester adhesive, a polyamide adhesive, a urethane adhesive, a fluorine adhesive, a styrene-diene block copolymer adhesive, an epoxy adhesive, and a photocurable adhesive. The resin portion is formed of a resin composition containing at least one resin selected from the group consisting of epoxy resin, phenolic resin, amino resin, unsaturated polyester resin, polyurethane resin, silicone resin and thermosetting polyimide resin, The adhesive layer includes an adhesive component, and the adhesive component includes at least one component selected from the group consisting of an organic silicon compound, a polyol compound, a urethane resin, and an epoxy resin. The FBG sensor is held by the resin portion, At least a portion of the entire periphery of the resin portion holding the FBG sensor except for the surface on the adhesive bonding layer side is covered with the first adhesive layer, The first adhesive layer has an opening that penetrates in the thickness direction. The resin portion is provided so as to fill a gap between the FBG sensor disposed in the opening and the opening, thereby holding the FBG sensor.

2. The sensor package according to claim 1, wherein: The adhesive layer is cured at room temperature.

3. The sensor package according to claim 1 or 2, wherein: The adhesive layer is cured using a curing agent.

4. The sensor package according to claim 1 or 2, wherein: The surfaces of the first pressure-sensitive adhesive layer and the adhesive bonding layer that are to be attached to the target object are protected by a first release sheet.

5. The sensor package according to claim 1 or 2, wherein: The first substrate is transparent or translucent. 6 . The sensor package according to claim 1 , further comprising a second adhesive layer and a second substrate in this order on a surface of the first substrate opposite to a surface on the first adhesive layer side.

7. The sensor package according to claim 6, wherein: The second substrate is a weather-resistant substrate.

8. The sensor package according to claim 6, wherein: A second release sheet is provided at a portion between the first substrate and the second adhesive layer, wherein the second release sheet has an extension portion extending and exposed from the second adhesive layer in a surface extension direction of the second release sheet.

9. A method for mounting a sensor package, which is the method for mounting a sensor package according to any one of claims 1 to 8, The adhesive layer in the sensor package is cured by a curing agent, The installation method comprises: The step of applying the curing agent to at least one of the adhesive layer and the target object; and A step of attaching the sensor package to the target object via the adhesive layer.

10. A method for mounting a sensor package, which is the method for mounting a sensor package according to any one of claims 1 to 8, The adhesive layer in the sensor package is cured by a curing agent, The installation method comprises: The step of applying the curing agent to the adhesive layer; The step of applying the curing agent to the target object; and A step of attaching the sensor package to the target object such that the curing agent applied to the adhesive layer contacts the curing agent applied to the target object.

11. A method for mounting a sensor package, the method comprising mounting the sensor package according to any one of claims 1 to 3 on a target object, The surfaces of the first adhesive layer and the adhesive bonding layer in the sensor package that are attached to the target object are protected by a first release sheet. The sensor package includes, on a surface of the first adhesive layer opposite to a surface to be attached to the target object, the first substrate, the second adhesive layer, and the second substrate in this order. A second release sheet is provided at a portion between the first substrate and the second adhesive layer, wherein the second release sheet has an extension portion extending from the second adhesive layer and exposed in a surface extension direction of the second release sheet. The installation method comprises: The first release sheet is peeled off and a curing agent is applied to the adhesive layer; A step of attaching the release surface of the sensor package from which the first release sheet has been released to the target object; and The second release sheet is peeled off, and the release surface of the second adhesive layer from which the second release sheet has been peeled off is attached to the first substrate. 12 . A kit comprising the sensor package according to claim 1 and a curing agent.