A local volume-increasing casting wheel mold
By designing the partially expanded casting wheel mold, including the innovative structure and cooling design of the top mold, lower mold and side mold, the problem of low efficiency and low yield of low-pressure cast wheel products has been solved, and efficient, stable casting production and high quality have been achieved. Finished product.
Patent Information
- Application Number
- CN202111592728.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-24
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2041-12-24
AI Technical Summary
Due to the limited size of the center gate of low-pressure cast wheel products, the efficiency and yield of small-gate products are low, and the profit margin is not high. It is difficult to effectively improve the existing technology.
Design a partially expanded casting wheel mold, including a top mold, a lower mold and a side mold. A shunt is embedded in the center of the top mold, and the upper and lower gate sleeves are set from top to bottom in the center of the bottom mold. The intermediate pipe is connected and the shunt is made of The three-piece structure and double cooling channels, as well as the optimized bolt column shape, improve the heat and feeding capacity of the gate area.
The efficiency and yield of small gate products have been significantly improved to 15 pieces/hour and 95%, ensuring the profit margin of the product. Through simple structural design, the castings can be quickly and stably solidified and high-quality finished products can be achieved.
Smart Images

Figure CN114433791B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of casting, and in particular to a local volume-enhanced casting wheel mould. Background Art
[0002] The car is an outstanding creation of the industrial development of human society. Whether it is traditional fuel-driven or the emerging electric and hydrogen-driven, it is the wheels that always support human travel. In recent years, technological progress has brought about a variety of wheel manufacturing technologies, such as mixed extrusion, semi-solid casting, multi-directional forging, etc., which can be roughly divided into three categories, namely, one, casting molding process; two, plastic molding process; three, stacking molding process, such as 3D printing. Among them, the low-pressure casting process is widely used due to its cost-effectiveness. Most low-pressure castings adopt the center pouring method, and the size of the center gate is often limited by the product shape of the automobile OEM and cannot be changed. This is very unfavorable for the production of large-size and small-gate wheel products. Since the gate cannot provide sufficient shrinkage compensation capacity, the die-casting efficiency and yield rate will be greatly reduced. Taking a 19-inch φ50 gate as an example, the efficiency is only 10 pieces / hour, and the yield rate is only 80%, resulting in an extremely low profit margin for the product. To this end, a low-pressure casting riser local capacity expansion mold structure was specially designed, combined with new processes and mold ideas for verification, which increased the efficiency and yield of small-gate products to 15 pieces / hour and 95%, ensuring the profit margin of this type of product. Summary of the invention
[0003] In view of this, the present invention aims to propose a partially increased capacity casting wheel mold, which can increase the efficiency and yield of small gate products to 15 pieces / hour and 95%, so that the profit margin of such products is guaranteed. To achieve the above purpose, the technical solution of the present invention is implemented as follows:
[0004] A local volume increase casting wheel mold comprises a top mold, a bottom mold and a side mold, wherein a diverter is embedded in the center of the top mold, and an upper gate sleeve and a lower gate sleeve are arranged in sequence from top to bottom at the center of the bottom mold, wherein the lower gate sleeve is connected to an intermediate tube, and the diverter comprises an upper diverter, a middle diverter and a lower diverter which are connected in sequence from top to bottom.
[0005] In some embodiments, the upper splitter and the middle splitter are fixedly connected by welding, and the middle splitter and the lower splitter are fixedly connected by welding.
[0006] In some embodiments, the upper splitter and the middle splitter are fixedly connected by screwing, and the middle splitter and the lower splitter are fixedly connected by screwing.
[0007] In some embodiments, an intermediate tube is disposed between the lower gate bushing and the riser tube.
[0008] In some embodiments, the lower gate sleeve is disposed between the upper gate sleeve and the middle tube.
[0009] In some embodiments, a second cooling air hole is opened in the upper splitter, and a second cooling air duct is arranged in the second cooling air hole.
[0010] In some embodiments, a first cooling air hole is opened in the middle of the middle splitter, and a first cooling air duct is arranged in the first cooling air hole.
[0011] Compared with the prior art, the local volume-increasing casting wheel mold of the present invention has the following advantages:
[0012] The mold structure of the present invention is simple, and through a variety of innovative designs, the volume of aluminum liquid in the pouring area and the mold temperature are significantly increased, so that the casting can be solidified quickly and stably in sequence, achieving the purpose of improving product quality and yield rate. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings:
[0014] Figure 1 The figure is a front view of a partially expanded casting wheel mold according to the present invention.
[0015] Figure 2 The present invention is a schematic diagram of a runner structure of a partially expanded casting wheel mold.
[0016] Figure 3 The present invention is a schematic diagram of a flow divider structure of a local volume-enhanced casting wheel mold.
[0017] Figure 4 The present invention is a schematic diagram of a flow divider structure of a local volume-enhanced casting wheel mold.
[0018] Description of reference numerals:
[0019] 1-middle pipe, 2-lower gate sleeve, 3-upper gate sleeve, 4-insulation groove, 5-bolt column, 6-diverter, 7-lower diverter, 8-middle diverter, 9-upper diverter, 10-first cooling air hole, 11-first cooling air duct, 12-second cooling air hole, 13-second cooling air duct, 14-minimum distance from the inside of the bolt column to the diverter cone, 15-minimum distance from the outside of the bolt column to the cavity, 16-bolt column fillet. DETAILED DESCRIPTION
[0020] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments may be combined with each other.
[0021] The technical solution of the present invention will be clearly and completely described below with reference to the accompanying drawings and in combination with the embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0022] Reference below Figures 1 to 4 The local volume expansion casting wheel mold of the embodiment of the present invention is described in conjunction with the embodiment.
[0023] A new wheel casting mold design includes a bottom mold, a top mold, four side molds, a diverter 6, an intermediate tube 1, a gate upper sleeve 3 and a gate lower sleeve 2. Figure 1 As shown, the manifold 6 is embedded in the center of the top mold, and the gate upper sleeve 3 and gate lower sleeve 2 are placed in the center of the bottom mold from top to bottom, and are usually fixed from the back by a pressure plate. The intermediate pipe 1 is located between the gate lower sleeve 2 and the liquid riser (not shown in the figure). The mold structure is changed, and the intermediate pipe 1 and the gate lower sleeve 2 are designed with an overall expansion design; the manifold or manifold 6 is designed with a three-part structure and double cooling channel control; the gate area upper mold, lower mold, and manifold 6 adopt a new design wall thickness; the casting mold bolt column shape is optimized.
[0024] The novel intermediate tube 1 (intermediate tube) and the ingrowing gate lower sleeve 2 have greatly increased the internal volume by expanding the inner wall through structural changes, so that higher heat can be continuously provided to the gate area of the casting during the same filling and holding time during the die casting process.
[0025] The splitter is different from the traditional splitter in that it has three split parts, upper, middle and lower, which are fixed by welding or bolts, reducing the volume of the cold iron in the center area of the middle flange. The splitter maximizes the cooling function, is equipped with two sets of cooling control, and has a more precise cold zone gate area, reducing the difficulty of sequential solidification.
[0026] The thickness of the lower mold in the gate area is designed to be thinned based on the balance concept according to actual needs, and a circle of heat insulation grooves is processed. On the one hand, the volume of the cold iron in the riser area is reduced, and on the other hand, the influence of the cooling outside the gate on the gate temperature is reduced, thereby increasing the temperature of the gate area.
[0027] The casting bolt column shape achieves the purpose of improving the shrinkage compensation capacity of the gate area by designing the bolt column height, angle, and fillet size.
[0028] In some embodiments, Figure 1As shown, a local volume increase casting wheel mold is composed of an upper mold, a lower mold, two to four movable molds, a diverter 6, an intermediate tube 1, a gate lower sleeve 2 and a gate upper sleeve 3. The technical solution is redesigned in the diverter 6, the gate lower sleeve 2 and the intermediate tube 1, the mold wall thickness, and the bolt column shape.
[0029] The novel intermediate tube 1 is as follows Figure 1 As shown, it is located between the lower sleeve 2 of the gate and the riser pipe in the die-casting furnace (not shown in the figure), the lower opening size is φ70-φ110mm, the upper opening size is φ90-φ110mm, a step is set near the upper opening, the step depth is 25-45mm, the opening size inside the step is φ80-φ100mm, and the internal volume is 1.2-1.5 times that of the traditional solution.
[0030] The new gate lower sleeve 2 is located between the new gate upper sleeve 3 and the intermediate tube 1. The height is determined by the product shape and the mold structure. The lower opening diameter is consistent with the upper opening diameter of the new intermediate tube, which is φ90-φ110mm. The upper opening size is determined by the tail end of the gate upper sleeve 3. The internal volume of the gate lower sleeve 2 is 1.5-2.5 times that of the traditional solution.
[0031] The splitter 6 is as Figure 1 Assembled on the top mold as shown, Figure 2 The upper, middle and lower parts are designed as three parts, which are fixed by welding or threaded connection. The lower splitter 7 is made of corrosion-resistant molybdenum alloy, and the middle splitter 8 and the upper splitter 9 are made of stainless steel. The first cooling air hole 10 is φ10mm, and the first cooling air duct 11 is made of φ6mm stainless steel pipe; the outer ring second cooling air hole 12 is evenly distributed, with a diameter of φ8mm, and the second cooling air duct 13 is also φ6mm. The first and second cooling air are controlled separately according to actual needs.
[0032] like Figure 1 The thickness of the lower mold in the gate area is designed to be 15-22 mm according to actual needs, and a circle of heat insulation groove 4 is processed with a diameter of φ4-φ6 mm and a minimum distance of 8-12 mm from the cavity surface.
[0033] The bolt column shape 5 is as follows Figure 3 As shown, by optimizing the height, angle and fillet of the bolt column, the minimum distance 14 from the inner side of the bolt column to the splitter is controlled within 15mm-25mm, and the minimum distance 15 from the outer side of the bolt column to the cavity is controlled within 15mm-25mm. The fillet 16 of the bolt column is set to R2-R5.
[0034] Compared with the prior art, the local volume-increasing casting wheel mold of the present invention has the following advantages:
[0035] 1. The structure is simple, reliable and easy to make.
[0036] 2. It complies with the casting processability of the casting, increases the mold temperature in the riser area, enhances the shrinkage compensation capability, and provides accurate and efficient cooling, thereby reducing the impact of cooling in areas that require cooling on areas that do not require excessive cooling.
[0037] 3. Wide applicability: the new wheel casting mold described in the invention is not limited to wheel hub products, but also applicable to similar cylindrical or similar products. The cooling medium of the upper mold water cooling device can be compressed air, oil, oil gas, cooling water, water mist, or compressed air and water alternately.
[0038] In the description of the present invention, it is necessary to understand that the terms "center", "longitudinal", "lateral", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the protection content of the present invention.
[0039] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0040] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or can communicate with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0041] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A local volume increase casting wheel mold, characterized in that: The invention comprises a top mold, a bottom mold and a side mold, wherein a flow divider (6) is embedded in the center of the top mold, an upper gate sleeve (3) and a lower gate sleeve (2) are arranged in sequence from top to bottom in the center of the bottom mold, the lower gate sleeve (2) is connected to an intermediate tube (1), and the flow divider (6) comprises an upper flow divider (9), a middle flow divider (8) and a lower flow divider (7) which are connected in sequence from top to bottom. The thickness of the lower mold in the gate area is 15-22 mm, and a circle of heat insulation groove (4) is processed, with a diameter of φ4-φ6 mm and a minimum distance of 8-12 mm from the cavity surface. Among them, the minimum distance from the inner side of the bolt column to the splitter is controlled at 15mm-25mm, the minimum distance from the outer side of the bolt column to the cavity is controlled at 15mm-25mm, and the fillet of the bolt column is set to R2-R5. A second cooling air hole (12) is provided in the upper flow divider (9), and a second cooling air duct (13) is provided in the second cooling air hole (12). A first cooling air hole (10) is provided in the middle of the middle flow divider (8), and a first cooling air duct (11) is provided in the first cooling air hole (10). The intermediate tube (1) is located between the lower sleeve (2) of the pouring gate and the liquid riser in the die casting furnace, the lower opening size is φ70-φ110 mm, the upper opening size is φ90-φ110 mm, a step is provided near the upper opening, the step depth is 25-45 mm, and the opening size inside the step is φ80-φ100 mm. The gate lower sleeve (2) is located between the gate upper sleeve (3) and the intermediate tube (1), and the lower opening diameter of the gate lower sleeve (2) is consistent with the upper opening diameter of the intermediate tube (1), which is φ90-φ110 mm.
2. The partially expanded wheel casting mold according to claim 1, characterized in that: The upper section splitter (9) and the middle section splitter (8) are fixedly connected by welding, and the middle section splitter (8) and the lower section splitter (7) are fixedly connected by welding.
3. The partially expanded casting wheel mold according to claim 2, characterized in that: The upper section flow divider (9) and the middle section flow divider (8) are fixedly connected by screw connection, and the middle section flow divider (8) and the lower section flow divider (7) are fixedly connected by screw connection.