Anti-counterfeiting element transfer material, its manufacturing method and application

Through the combination of coextruded film technology and adhesive layer, the stability and integrity of existing anti-counterfeiting element transfer materials in manufacturing and use are solved, and efficient and economical anti-counterfeiting element transfer and protection effects are achieved.

CN114514107BActive Publication Date: 2024-11-01GIESECKE & DEVRIENT CURRENCY TECHNOLOGY GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202080070529.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-10-08
Filing Date
2020-10-01
Publication Date
2024-11-01
Estimated Expiration
2040-10-01

AI Technical Summary

Technical Problem

Existing anti-counterfeiting element transfer materials require more processes and materials to be used in the manufacturing process, and it is difficult to ensure the stability and integrity of anti-counterfeiting elements, especially when the flow of valuable items such as banknotes is prone to tear or damage.

Method used

Using co-extruded film technology, a plastic film/plastic layer composite made of materials such as polyethylene terephthalate (PET) and polyethylene naphthalate (PEN) combined with adhesive layer , forming a temporary carrier and anti-counterfeiting element layer composite that is easy to separate, pre-cut the anti-counterfeiting element profile shape, and forming a high-adhesion or low-adhesion plastic layer on the carrier substrate to reduce material loss and improve stability.

Benefits of technology

It has achieved the reduction of process and material use, enhanced the stability and integrity of anti-counterfeiting components, prevented mechanical and chemical damage to valuable items such as banknotes during the flow process, and ensured effective protection and bonding of anti-counterfeiting components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114514107B_ABST
    Figure CN114514107B_ABST
Patent Text Reader

Abstract

The present invention relates to a security element transfer material, comprising: a security element layer composite, the security element layer composite having a plurality of layers, including at least one characteristic layer; and a temporary carrier, the temporary carrier being detachably connected to a visible layer of the security element layer composite, wherein the temporary carrier has a carrier substrate, i.e. a plastic film, and the carrier substrate is provided with a plastic layer produced by coextrusion.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to an anti-counterfeiting element transfer material, which has a transfer material arranged on a temporary carrier and can be separated from the temporary carrier. The invention relates to a method for producing a security element layer composite and an application of a security element transfer material for providing security for a valuable object, in particular a valuable document.

[0002] Valuable articles, such as branded goods or valuable documents, especially banknotes, are usually provided with security elements, which realize the inspection of the authenticity of valuable articles and are used as protection against unauthorized copying at the same time. The security elements used for this purpose are usually not provided individually, but in the form of a transfer tape with a plurality of security elements designed as transfer elements. The feature of the transfer tape is that the security element is prepared on a carrier layer, wherein the order of the layers of the transfer element is usually opposite to the order of the layers on the article to be protected afterwards. During the transfer, the carrier layer is usually peeled off (abgezogen) from the layer structure of the security element. On the side opposite to the carrier layer direction, the transfer tape has an adhesive layer usually made of a heat-sealing adhesive or a heat-sealing lacquer, which melts when the security element is transferred and the security element is bonded to the article to be secured. The transfer tape is placed on the article with a heat-sealing adhesive layer and is pressed by a heated transfer punch or a transfer roller and is transferred to the article with the contour shape of the heated transfer punch. Transfer elements, transfer belts and the transfer of transfer elements to a target substrate are described, for example, in EP 0 420 261 B1 and WO 2005 / 108108 A2.

[0003] Instead of forming the transfer element by the transfer punch during the transfer process, each individual transfer element can also be prefabricated on the transfer belt to be present in the desired contour shape. The prefabrication of the separated individual security elements is suitable, for example, in the following case, that the security element has a layer structure, which makes it difficult to accurately cut the entire layer structure during the transfer process. This is, for example, the following case, that the layer structure of the security element to be transferred contains a permanent carrier substrate, such as a plastic film. The carrier substrate inside the layer structure of the security element is suitable in the following case, that the security element must be particularly stably designed, that is, for example, the security element must be self-supporting, because the security element should be used to close the through-opening in the article that needs to be secured. Here, according to the size of the article and the opening that needs to be closed, higher requirements may be placed on the stability of the security element. For example, the banknote is subjected to higher stress, touched, bent and may be in moisture during its circulation time. The security element must withstand these stresses like the banknote paper itself, because otherwise there will be a risk that the through-opening in the banknote will be exposed after a certain circulation time.

[0004] The security element whose layer structure includes a stable carrier substrate, usually a plastic film, must exist as a pre-manufactured individual element on the transfer material, which means that the contour shape of the security element must be pre-cut in the security element material in advance. Pre-cutting can be performed, for example, by means of a laser. The problem arising here is that the cutting depth must be controlled very accurately so as to cut off the complete layer structure of the security element on the one hand, but on the other hand not to damage the carrier material that is detached during the transfer. Plastic film is usually used as a carrier material. Although plastic film has a high tear strength, it has a low resistance to continued tearing strength (Weiterreiβwiderstand). If the plastic film is cut, it is almost inevitable that the security element transfer material present as a continuous material is torn at some locations during the transfer process of the security element to the valuable item. It is also necessary to consider that the layer structure to be cut or the carrier film that cannot be cut is a material with a thickness in the micrometer range. The security element layer structure usually has a thickness in the range of about 20μm to 30μm, and the carrier film usually has a thickness in the range of 10μm to 20μm. The problem with the precision required here is that the cutting process must be carried out in such a way that the security element layer composite is completely severed, but the cutting process must be stopped in such a timely manner that the carrier film is not cut at any point. However, due to the partially cut carrier film, the security element transfer material loses stability and can even tear, so that accurate and frictionless application of the security element from the continuous material to the product to be protected can no longer be ensured.

[0005] The security element transfer material of the known form of WO 2010 / 031543 A1 is a continuous material, wherein the layer security element is pre-cut in the desired contour shape, and the pre-cut element can be transferred to the product to be protected without the risk of tearing the carrier material. The security element transfer material is a continuous material, especially a band with a length of several hundred meters and a width of several millimeters / centimeter to several meters. The security element transfer material has a security element layer composite, that is, a real security element material and a temporary carrier, that is, a material of "storing" security elements. The temporary carrier is based on a carrier layer composite, and the carrier layer composite is composed of the first and second temporary carrier substrates that are inseparable and bonded by means of an adhesive layer. The security element layer composite is directly connected to the temporary carrier or is connected by means of a release layer. The release layer is designed in a conventional manner and makes it easier to separate the security element from the temporary carrier during the transfer process to the valuable article. The temporary carrier is on the side of the security element layer composite facing the observer after transferring the security element. The name "temporary" carrier substrate represents that these carrier substrates are not the components of the security element differently from the "permanent" carrier substrate. The design of the temporary carrier as a carrier layer composite avoids the influence of the stability of the temporary carrier due to the temporary carrier being cut when cutting the contour shape of the security element. Similar results cannot be achieved simply by designing the only temporary carrier film to be thicker, because the plastic film has a lower resistance to continued tearing, that is, even if the film is only cut very slightly, the film will easily continue to tear and may break completely. In the case of a carrier layer composite composed of the first and second temporary carrier substrates bonded inseparably by means of an adhesive layer, it is different that even if one of the temporary carrier substrates is completely cut, the other temporary carrier substrate (or other multiple temporary carrier substrates if necessary) usually remains undamaged and is correspondingly stable. In addition, the adhesive also forms an additional "buffer zone" between the temporary carrier substrates.

[0006] The method described in WO 2010 / 031543 A1 is to remove the edge (entgittern) of the patch film before applying. For this reason, the shape of the patch is punched into the layer to be transferred by a die, that is, the layer is perforated by the die. When removing the edge, these layers are peeled off in the area outside the patch, and these layers remain on the carrier film in the patch area. It is thus ensured that the patch has a clean edge after applying. However, the method described in WO 2010 / 031543 A1 has the disadvantages of the number of required processes and high material usage.

[0007] The technical problem to be solved by the present invention is to provide a security element transfer material which is improved compared with the prior art and whose production requires fewer steps and reduced material usage.

[0008] This technical problem is solved in an alternative way through the following technical solution. SUMMARY OF THE INVENTION

[0010] 1. (First aspect of the present invention) An anti-counterfeiting element transfer material, comprising

[0011] a security element layer composite having a plurality of layers, including at least a first adhesive layer, a feature layer and a visible layer, wherein the visible layer is the layer facing the observer after the first security element (34) has been transferred to the valuable article, and

[0012] a temporary carrier which is detachably connected to the visible layer of the security-element layer composite,

[0013] It is characterized in that

[0014] - the temporary carrier has at least one first temporary carrier substrate (4), ie a plastic film; and

[0015] The visible layer of the security-element layer composite is present in the form of a plastic layer which is produced by coextrusion on the first temporary carrier substrate (4) and has low adhesion to the first temporary carrier substrate (4).

[0016] 2. (Preferred design scheme) The security element transfer material according to item 1 is characterized in that the first temporary carrier substrate (4) is a polyethylene terephthalate (PET) film, and the visible layer of the security element layer composite in the form of a plastic layer with low adhesion ability on the first temporary carrier substrate (4) produced by co-extrusion on the first temporary carrier substrate (4) is a polyethylene naphthalate (PEN) layer.

[0017] 3. (Preferred design scheme) The anti-counterfeiting element transfer material according to item 1 or 2 is characterized in that the temporary carrier has a carrier layer composite, which is composed of a first temporary carrier substrate (4) and a second temporary carrier substrate (2), and the first temporary carrier substrate and the second temporary carrier substrate are respectively plastic films and are inseparably bonded by means of an adhesive layer (3).

[0018] 4. (Preferred design) The security element transfer material according to any one of items 1 to 3, characterized in that the contour shape of the security element is pre-cut in the security element layer composite.

[0019] 5. (Preferred design scheme) The security element transfer material as described in item 4 of the referenced item 3 is characterized in that the contour shape of the security element is pre-cut in the security element layer composite, wherein the incision (11) partially or completely cuts off the first temporary carrier substrate (4) when necessary and partially or completely cuts off the adhesive layer (3) when necessary, but the incision does not enter the second temporary carrier substrate (2), so that the temporary carrier can be detached as a complete carrier layer composite.

[0020] 6. (Preferred design scheme) The security element transfer material as described in item 4 or 5 is characterized in that the layer composite material outside the contour shape of the security element is removed from the security element layer composite, so that the security element transfer material has gaps in the security element layer composite, while the temporary carrier does not have gaps.

[0021] 7. (Preferred design) The security element transfer material according to any one of items 1 to 4, characterized in that the feature layer comprises an embossing lacquer layer and a metallized part or a colored thin-film element.

[0022] 8. (Second aspect of the present invention) An anti-counterfeiting element transfer material having

[0023] - a security element layer composite having a plurality of layers, including at least one adhesive layer, a feature layer and a permanent carrier substrate (24), wherein the feature layer is equal to the visible layer and the visible layer is the layer facing the observer after the security element has been transferred to the valuable article, and

[0024] a temporary carrier which is detachably connected to the visible layer of the security-element layer composite,

[0025] It is characterized in that

[0026] The temporary carrier has a carrier substrate (18), ie a plastic film, and has a plastic layer (19) produced on the carrier substrate (18) by coextrusion, which has a high adhesion to the carrier substrate (18); and

[0027] The visible layer of the security element layer composite is detachably connected to the plastic layer ( 19 ) produced by coextrusion on the carrier substrate ( 18 ).

[0028] 9. (Preferred design scheme) The anti-counterfeiting element transfer material as described in item 8 is characterized in that the carrier substrate (18) of the temporary carrier is a polyethylene terephthalate (PET) film, and the plastic layer (19) produced on the carrier substrate (18) by co-extrusion and having a high adhesion ability on the carrier substrate (18) is a polyethylene naphthalate (PEN) layer mixed with polyethylene terephthalate (PET).

[0029] 10. (Preferred design scheme) The security element transfer material according to one of items 8 or 9 is characterized in that the contour shape of the security element is pre-cut in the security element layer composite, wherein the incision partially or completely cuts off the plastic layer (19) with high adhesion on the carrier substrate (18) produced by coextrusion on the carrier substrate (18), but the incision does not enter the carrier substrate (18) of the temporary carrier, so that the temporary carrier can be detached as a complete carrier layer composite.

[0030] 11. (Preferred design scheme) The security element transfer material as described in Item 10 is characterized in that the layer composite material outside the contour shape of the security element is removed from the security element layer composite, so that the security element transfer material has gaps in the security element layer composite, while the temporary carrier does not have gaps.

[0031] 12. (Preferred design) The security element transfer material according to any one of items 8 to 11, characterized in that the feature layer comprises an embossing lacquer layer and a metallized part or a colored thin-film element.

[0032] 13. (Preferred design scheme) The security element transfer material according to item 7 or 12 is characterized in that the colored thin layer element is a thin layer element with angle-dependent color (farbkippend, or color inclination), and the thin layer element conveys different color impressions to the observer at different observation angles, or the colored thin layer element is a translucent thin layer element, and the thin layer element conveys different color impressions to the observer when observed with reflected light and when observed with transmitted light.

[0033] 14. (Third aspect of the present invention) A use of the security element transfer material according to any one of items 1 to 13 for providing security for valuable items, especially valuable documents, having a security element.

[0034] 15. (Preferred design) The application according to item 14 of one of the referenced items 8 to 13, characterized in that the valuable item is a valuable document having a through opening (37), and the security element is applied in such a way that the security element covers the through opening (37).

[0035] 16. (Fourth aspect of the present invention) A method for producing a security element transfer material according to any one of items 1 to 13, comprising:

[0036] - providing a carrier substrate, ie a plastic film, which is provided with a plastic layer produced by coextrusion; and

[0037] Arranging at least one adhesive layer and the security element layer composite with the feature layer on the plastic layer produced by coextrusion.

[0038] 17. (Preferred embodiment) The method according to item 16 of one of items 1 to 7, wherein the plastic layer produced on the carrier substrate by coextrusion has low adhesion to the carrier substrate.

[0039] 18. (Preferred embodiment) The method according to item 16 of one of items 8 to 12, wherein the plastic layer produced on the carrier substrate by coextrusion has a high adhesion to the carrier substrate. DETAILED DESCRIPTION OF THE INVENTION

[0041] According to the invention, viewing with reflected light is illuminating the value document from one side and observing the value document from the same side. Thus, for example, viewing with reflected light occurs when the front side of the value document is illuminated and the front side of the value document is also observed.

[0042] According to the invention, viewing with transmitted light is illuminating the value document from one side and observing the value document from a different side, in particular from opposite sides. Thus, for example, viewing with transmitted light occurs when the back side of the value document is illuminated and the front side of the value document is observed. Thus, light appears through the value document.

[0043] The valuable document according to the invention can be, for example, a banknote or an identity document, but can also be a stock certificate, a certificate, a stamp, a check, an admission ticket, a ticket, an airline ticket, an identity card or a visa sticker, etc., as well as a label, a seal, a packaging or other elements. Therefore, the simplified name "valuable document" always includes the above-mentioned types of documents below. The term valuable document also includes security papers for the production of banknotes. The term banknotes especially includes paper banknotes, polymer banknotes or film composite banknotes.

[0044] The transfer element, ie the security element to be transferred, can be in particular a transfer patch or a transfer label or a transfer strip or a transfer line. The invention is described in the following detailed description based on the example of a transfer patch and should therefore not be construed as being limited to a patch.

[0045] Here, the term functional layer is also used instead of the term characteristic layer. A functional layer can be a single (functional) layer or a plurality of (functional) layers.

[0046] The security element transfer material according to the invention comprises a carrier substrate, i.e. a plastic film provided with a plastic layer produced by coextrusion. Depending on the materials used for the plastic film on the one hand and for the plastic layer on the other hand, a plastic film / plastic layer arrangement can be produced which selectively or easily delaminates highly or has reliable adhesion and is thus able to prevent delamination at the interface between the plastic film and the plastic layer. Here, the term "delamination" means shedding, i.e. the separation of layers from each other within a composite or laminate. The plastic film / plastic layer arrangement used according to the invention is a coextruded film, i.e. a coextruded film, and therefore a composite film consisting of a plurality of layers, in which a variety of properties of different film materials are combined. Using a polyester film, such as polyethylene terephthalate (PET) as a carrier substrate and combining a plastic layer based on a heterogeneous plastic material, such as pure polyethylene naphthalate (PEN), applied to the carrier substrate by coextrusion, produces a plastic film / plastic layer composite film that is easily delaminated. Pure polyethylene naphthalate (PEN) has poor adhesion to polyethylene terephthalate (PET) and leads to insufficient anchoring of the plastic layer coextruded onto the carrier substrate. However, the use of a polyester film, such as polyethylene terephthalate (PET) as a carrier substrate in combination with a plastic layer based on polyethylene naphthalate (PEN) with a certain amount of polyethylene terephthalate (PET) mixed therein, applied to the carrier substrate by coextrusion, results in a stable plastic film / plastic layer composite film that is protected against delamination.

[0047] The plastic film / plastic layer composite film that is easily delaminated is used in the security element transfer material according to the first aspect of the present invention, which is explained in more detail in the following description:

[0048] The security element transfer material comprises a temporary carrier substrate, i.e. a plastic film, and a security element layer composite, wherein the security element layer composite has a plastic layer with low adhesion on the temporary carrier substrate produced by coextrusion, a characteristic layer and an adhesive layer suitable for bonding the transfer element to the valuable article. The temporary carrier substrate is, for example, a polyester film, such as a polyethylene terephthalate (PET) film. The plastic layer with low adhesion on the temporary carrier substrate produced by coextrusion can be suitably based on polyethylene naphthalate (PEN). By using a coextruded film, a security element transfer material with a significantly thinner total thickness can be obtained compared to the security element transfer materials known in the prior art. This is possible because the coextruded plastic layer can be produced very thinly, especially with a thickness of less than 1 μm. The coextruded plastic layer suitably has a layer thickness in the range of 2 to 4 μm.

[0049] The security element transfer material according to the first aspect of the present invention is particularly suitable for realizing a thin, patch-like security element, which is applied to a security paper or a polymer substrate such as a polymer banknote, wherein the security paper or the polymer substrate is covered by the security element over the entire surface in the area where the security element is arranged thereon (i.e., the security paper or the polymer substrate preferably does not have a recessed portion covered by the security element in the area where the security element is arranged thereon).

[0050] When bonding the transfer element to the valuable article, a release or separation is achieved within the security element transfer material according to the first aspect of the invention at the interface between the plastic film and the plastic layer produced thereon by coextrusion.

[0051] Since the coextruded plastic layer is present as the outermost layer at the top in the patch-like security element applied to security paper or a polymer substrate such as a polymer banknote, extremely good protection of the sensitive security element layer composite can be achieved against mechanical damage during banknote circulation or against chemical damage by solvents, etc.

[0052] In the simplest case, the temporary carrier of the security element transfer material according to the first aspect of the present invention can be in the form of a separate plastic film, for example a polyethylene terephthalate (PET) film. According to a preferred embodiment, the temporary carrier can also be based on a carrier layer composite imitating WO 2010 / 031543 A1, which has a first and a second temporary carrier substrate that are inseparable and bonded by an adhesive layer.

[0053] Furthermore, the contour shape of the security element can be precut into the security element layer composite.

[0054] A plastic film / plastic layer composite film capable of preventing delamination is used in the anti-counterfeiting element transfer material according to the second aspect of the present invention, which is described in more detail in the following description:

[0055] The security element transfer material comprises a plastic film as a temporary carrier substrate, which is provided with a plastic layer produced by coextrusion and having a high adhesion ability on the plastic film. The security element transfer material also comprises a security element layer composite, which has a characteristic layer, a permanent carrier substrate and an adhesive layer suitable for bonding the transfer element to the valuable article. The plastic film of the temporary carrier substrate is, for example, a polyester film, such as a polyethylene terephthalate (PET) film. The plastic layer with a high adhesion ability produced by coextrusion is, for example, based on polyethylene naphthalate (PEN) mixed with a certain amount of polyethylene terephthalate (PET).

[0056] The security element transfer material according to the second aspect of the invention is particularly suitable for realizing a patch-like security element that covers a recess in a value document.

[0057] When bonding the transfer element to the valuable article, release or separation occurs within the security element transfer material according to the second aspect of the invention at the interface between the plastic layer produced by coextrusion and the security element layer composite arranged thereon.

[0058] Compared to the security element transfer materials known in the prior art, the security element transfer material according to the second aspect of the invention is advantageous because it is possible to avoid excessive penetration of the punch knife or the laser radiation in the step of cutting the contour shape of the security element into the security element layer composite. In addition, compared to the security element transfer material known from WO 2010 / 031543A1, the structure of the security element transfer material according to the second aspect of the invention is advantageous because fewer working steps and bonding steps are required during the manufacturing process and the film can be omitted.

[0059] The following description is in basic form and relates to the security element transfer material according to the first aspect of the present invention and the security element transfer material according to the second aspect of the present invention:

[0060] Suitable feature layers or functional layers provide optically variable security features, such as embossed holograms, micromirror elements, subwavelength structures, etc. Optically variable security features are usually produced by embossing lacquers, such as UV embossing lacquers, with microstructures embossed therein and metallization present at least in certain areas. Other layers are usually present, such as protective lacquers or primers, to which a heat-sealing lacquer layer is finally attached. The heat-sealing lacquer layer can actually also consist of multiple layers of different lacquers.

[0061] During application or final application, the patch is heated as usual, wherein the heat-sealing lacquer melts and adheres to the (value document) substrate. The (value document) substrate can be, for example, a paper substrate or a polymer substrate or a paper / polymer composite substrate. Here, the heating can be carried out regionally (i.e. in an area slightly larger than the patch itself) or over the entire surface. If the temporary carrier is then separated from the (value document) substrate, the functional layer remains in the patch area on the (value document) substrate, because the heat-sealing lacquer ensures that the adhesion to the paper is stronger than the adhesion between the temporary carrier and the functional layer.

[0062] Other preferred implementation variants:

[0063] Functional layer or feature layer:

[0064] For example, micromirrors, holographic structures, subwavelength structures or (for example embedded) microlenses can be introduced into the functional layer. Microlenses can be present in particular in combination with microimages designed in a separate plane and in this way produce optically variable security features in the form of so-called moiré magnifiers, mode mappers, tilted images, etc. For example, security features based on microlenses combined with microimages are known from WO 2006 / 087138 A1.

[0065] Micromirrors, holographic structures, etc. are usually coated with a metallization which is present at least in certain areas and which can consist of metals such as Al or Ag, high-refractive-index coatings such as ZnS or TiO. 2 , or a three-layer system with farbkippend (or color tilt), i.e., reflector / dielectric / absorber (e.g., Al / SiO 2 / Cr structure).

[0066] Adhesive layers, especially heat seal lacquers:

[0067] It is important for the heat seal lacquer that it must ultimately ensure the desired bond when applied by pressure and, if necessary, elevated temperature. The heat seal lacquer can be melted and / or activated by heat. It can also be provided that the heat seal lacquer is subsequently reprocessed (recrosslinked), for example, by UV radiation.

[0068] Carrier substrate, especially carrier film:

[0069] Preferably, a thicker film is used as the carrier film, for example a 19 μm thick polyethylene terephthalate (PET) film. It must be ensured that the carrier film does not tear after the patch is applied to the (value document) substrate. According to a variant, a separate carrier film is not used as the carrier film, but a laminated composite consisting of two films, as is known from WO 2010 / 031543 A1 (for example a 12 μm thick film and a 19 μm thick film, which are bonded to one another): during the punching process, only one of the two films is then punched out, while the second film remains intact. A punched film alone tears more easily than a laminated composite, since a "first tear" of the film requires greater force than further tearing.

[0070] Applying the transfer patch to the (value document) substrate:

[0071] For better transfer, it may be advantageous to peel the carrier film off the rest of the layer composite using a sharp edge (or a wedge).

[0072] Other preferred parameters:

[0073] The functional layer preferably comprises an embossing lacquer, the total thickness of which is usually in the range from 2 μm to 7 μm. Depending on the type of structure, typical embossing depths may be in the range from 100 nm to 3.5 μm, for example.

[0074] The total thickness of the patch without the carrier film is preferably below 50 μm, more preferably below 30 μm and especially preferably below 20 μm.

[0075] - Typical patch dimensions are eg 5 mm to 35 mm wide and eg 5 mm to 70 mm high.

[0076] - The patch shape can be chosen arbitrarily. An oval shape is usually easier to apply than, for example, a rectangle. A serrated edge can sometimes be advantageous.

[0077] Other principles:

[0078] The embossed structures that can be used according to the invention are embossed in particular in embossing lacquers. In the context of the present application, the expression "optically variable effect" also includes, in addition to holograms, diffraction structures similar to holograms, i.e. structures which, for example, do not produce a defined image but rather a blurred colored impression. The expression "optically variable effect" also includes diffraction patterns, structures with an angle-dependent color effect, kinoforms, structures with a microlens effect, structures with an isotropic or anisotropic scattering effect or with other interference effects, subwavelength structures, moth-eye structures, microlens structures and microstructures for moiré magnifiers or pattern mappers, micromirror structures and microprismatic structures.

[0079] Preferred reflective embossed structures include, for example, a multilayer structure having interference capability, which has

[0080] - a reflective layer (especially a metallic reflective layer);

[0081] - a semi-transparent (mirror) layer (especially selected from Al, Ag, Ni, Cr, Cu, Au and alloys of one or more of the aforementioned elements); and

[0082] - a dielectric layer arranged between the reflective layer and the semi-transparent (mirror) layer,

[0083] Among them, the color of the multilayer structure changes with the change of observation angle.

[0084] It is feasible to produce a first appearance of a multilayer structure with interference ability, which can be identified when observing the front side with reflected light, and to produce a second appearance of a multilayer structure with interference ability, which can be identified when observing the front side with transmitted light, for example, by a recessed portion in a reflective layer and / or a semi-transparent layer. Such film anti-counterfeiting elements with different reflected light / transmitted light appearances are known from WO 2009 / 149831 A2. For example, a semi-transparent layer can have a large number of recessed portions arranged in a grid shape, which form a symbol, an image or a pattern as a whole. The pattern produced in this way is visible in reflected light and disappears in transmitted light. Alternatively and / or additionally, different reflected light / transmitted light appearances of the multilayer structure can be achieved by combining the multilayer structure with a convex structure, in particular a diffractive convex structure, a micro-optical convex structure or a sub-λ structure.

[0085] Other preferred reflective embossing structures for example include a multilayer structure with two semi-transparent layers and a dielectric layer arranged between the two semi-transparent layers, wherein the multilayer structure has different hues when observed with reflected light and when observed with transmitted light on the one hand, especially presents a golden hue when observed with reflected light, and presents a blue hue when observed with transmitted light. These two different hues are especially complementary colors. This multilayer structure is especially based on two semi-transparent mirror layers and a dielectric layer arranged between the two semi-transparent mirror layers. This multilayer structure that presents a golden hue when observed with reflected light and a blue hue when observed with transmitted light is for example known from WO 2011 / 082761 A1. Metals selected from alloys of Al, Ag, Ni, Cr, Cu, Au and one or more of the above elements are particularly suitable as semi-transparent mirror layers, wherein Al or Ag are preferably used as semi-transparent mirror layers, and Al is particularly preferred. A suitable multilayer structure with two semi-transparent mirror layers and a dielectric layer arranged between the two semi-transparent mirror layers preferably has the following specific characteristics:

[0086] - two semi-transparent mirror layers are preferably selected from Al or Ag; the dielectric layer is especially SiO 2 layer;

[0087] In the case where each of the two semitransparent mirror layers is based on Al, the corresponding preferred layer thickness is in the range from 5 nm to 20 nm, particularly preferably in the range from 10 nm to 14 nm; the dielectric SiO 2 The layer preferably has a layer thickness in the range of 50 nm to 450 nm, more preferably in the range of 80 nm to 260 nm, wherein, in particular to provide a gold / blue color change, the ranges of 80 nm to 100 nm and 220 nm to 240 nm are particularly preferred;

[0088] - In the case of two semitransparent mirror layers each based on Ag, the corresponding preferred layer thickness is in the range of 15 nm to 25 nm; the dielectric SiO 2 The layer preferably has a layer thickness in the range of 50 nm to 450 nm, more preferably in the range of 80 nm to 260 nm, wherein, in particular to provide a gold / blue color change, the ranges of 80 nm to 100 nm and 220 nm to 240 nm are particularly preferred.

[0089] The multilayer structures mentioned make it possible not only to produce translucent functional layers which have a golden hue when viewed in reflected light and a blue hue when viewed in transmitted light, but also, depending on the choice of the layer thickness, in particular of the dielectric layer, to produce other color variations, for example

[0090] - Magenta in reflected light, blue-green in transmitted light;

[0091] -Turquoise in reflected light and orange in transmitted light;

[0092] -Golden in reflected light and bluish-purple in transmitted light;

[0093] -It appears silvery in reflected light and violet in transmitted light.

[0094] Other preferred reflective embossed structures include, for example, a liquid crystal layer which, when viewed in reflected light, displays a different color than when viewed in transmitted light. Alternatively and / or additionally, different reflected light / transmitted light appearances can be achieved by combining a liquid crystal layer with a relief structure, in particular a diffractive relief structure, a micro-optical relief structure or a sub-lambda structure.

[0095] Other preferred reflective embossed structures include, for example, a printed layer with an effect pigment composition which, when viewed in reflected light, exhibits a different color than when viewed in transmitted light, in particular a gold / blue color change, a gold / violet color change, a green-gold / magenta color change, a violet / green color change or a silver / opaque color change. Such print colors are described, for example, in WO 2011 / 064162 A2. Alternatively and / or additionally, different reflected light / transmitted light appearances can be achieved by combining the printed layer with a relief structure, in particular a diffractive relief structure, a micro-optical relief structure or a sub-lambda structure.

[0096] The relief structure forming the diffractive structure is in particular a holographic structure. The size of the structural elements of the diffractive structure is preferably in the order of magnitude of the wavelength of light, more preferably in the range of greater than 100 nm and less than 1 μm, wherein the range of greater than 300 nm and less than 1 μm is particularly preferred.

[0097] The relief structure forming the micromirror arrangement structure is also referred to herein as a micro-optical relief structure. The production of the micro-optical relief structure is known in the prior art (see, for example, WO 2014 / 060089 A2). The size of the structural elements of the micromirror arrangement structure is preferably in a range of greater than 1 μm and less than 40 μm, wherein a range of greater than 1 μm and less than 30 μm is particularly preferred. The size of the structural elements of the micromirror arrangement structure has, for example, a height of no more than 15 μm and a lateral extension of no more than 30 μm. Here, the height and lateral extension of the structural elements of the micromirror arrangement structure are preferably greater than 1 μm.

[0098] Other preferred micro-optical relief structures are known, for example, from WO 2007 / 079857 A1. Here, the reflective microstructure has the form of a mosaic consisting of a plurality of reflective mosaic elements, which are characterized by parameters such as size, contour shape, relief shape, reflectivity and spatial orientation and form a predetermined pattern (Motiv, or theme object) in that different groups of mosaic elements with different characteristic parameters reflect incident light into different spatial regions, and the mosaic elements have lateral dimensions that are below the resolution limit of the human eye.

[0099] Further exemplary embodiments and advantages of the invention are explained below with reference to schematically greatly simplified drawings, which are not shown to scale and proportion in the illustrations of the drawings in order to improve the clarity.

[0100] In the attached picture:

[0101] Figures 1 to 4 An embodiment showing the application of the security element transfer material according to the first aspect of the present invention;

[0102] Figures 5 to 8 An embodiment showing the application of the security element transfer material according to the second aspect of the present invention; and

[0103] Fig. 9 A valuable document, in the example a banknote, is shown which is equipped with two security elements, wherein the security elements are transfer patches which are respectively produced from the security element transfer material according to the first aspect of the invention or from the security element transfer material according to the second aspect of the invention.

[0104] Fig. 9A valuable document is shown, in the example a banknote 33 with a denomination of "20". The paper substrate 36 of the banknote 33 is provided with two security elements, namely a first security element 34 and a second security element 35, which are patches in the example. The first security element 34 is produced by the security element transfer material according to the first aspect of the invention. The paper substrate 36 of the banknote 33 is covered by the first security element 34 over the entire surface in the region of the patch-shaped first security element 34. The other second security element 35 is produced by the security element transfer material according to the second aspect of the invention. The paper substrate 36 of the banknote 33 has a square cutout in the region of the patch-shaped second security element 35, i.e. a through opening 37, which can be obtained, for example, by stamping or by laser cutting. The through opening 37 in the paper substrate 36 is therefore covered or closed on one side by the second security element 35.

[0105] Figures 1 to 4 An example of the use of the security element transfer material according to the first aspect of the invention is shown, which is suitable for providing, for example, Fig. 9 The first anti-counterfeiting element 34 in the form of a patch.

[0106] Figure 1 A first security element transfer material 1 is shown, which comprises a carrier material (=temporary carrier) comprising layers 2, 3 and 4 and an upper material comprising layers 5, 6, 7, 8 and 9. The dashed line AA' shows the surface on which the upper material (i.e. the security element or transfer element to be applied to the value document) is separated from the temporary carrier during the subsequent application of the upper material to the value document.

[0107] The first security element transfer material 1 comprises a coextruded film, i.e. a composite film consisting of a polyethylene terephthalate (PET) film having a thickness of 19 μm, i.e. a first temporary carrier substrate 4, and a plastic layer 5 arranged thereon, the plastic layer 5 being based on a heterogeneous plastic material, in the example being pure polyethylene naphthalate (PEN). The coextruded film having layers 4 and 5 is a plastic film / plastic layer composite film that is easy to delaminate along the imaginary line A-A'. The coextruded film having layers 4 and 5 is then inseparably bonded to another polyethylene terephthalate (PET) film having a thickness of 12 μm, i.e. a second temporary carrier substrate 2, through an adhesive layer 3. Subsequently, a first UV embossing lacquer layer 6 is applied above the plastic layer 5, the first UV embossing lacquer layer being provided with a microstructure and / or a nanostructure (the embossed structure is not shown in the figure). Next, a first metallization portion 7 is provided for the first UV embossing lacquer layer 6, the first metallization portion 7 being formed in the form of a pattern or a symbol. The first metallization 7 contains cutouts that form so-called negative characters. The first metallization 7 can be provided, for example, by a cleaning method known in the prior art, see, for example, EP 1 972 462 A2. A primer layer 8 is then applied over the first metallization 7, which in practice serves as a leveling protective lacquer. Finally, a first adhesive layer 9, i.e. a heat-sealing lacquer layer, suitable for bonding to a value document is applied over the primer layer 8.

[0108] exist Figure 2 The line indicated by the reference numeral "11" in the figure is a cut, which shows how to cut the security element layer composite so as to pre-cut the contour shape of the security element. 2 The laser cuts. As can be seen, the cut 11 enters the plastic film of the temporary carrier, i.e. the first temporary carrier substrate 4. The first temporary carrier substrate 4 is unstable due to the cut 11 and can easily tear at the cut site in the event of slight stretching, which is actually unavoidable during the transfer of the security element.

[0109] The excess material of the security element layer composite is then removed in a so-called "edge removal" step (in accordance with Figure 2 The material outside the cutout 11 in the cross-sectional view of FIG. 1 is removed, thereby forming a void in the security element layer composite. This state is Figure 3 . The plastic layer 5 based on polyethylene naphthalate (PEN) produced by coextrusion and having low adhesion on the first temporary carrier substrate 4 makes it easier to remove excess material. The security elements 14 are located on both sides of the gap. The temporary carrier is indicated by the reference numeral 13. The security elements 14 form islands arranged on the temporary carrier 13 to a certain extent. Figure 3The security element transfer material according to the invention is shown as a continuous strip in which in the width direction there is only one security element 14. In practice the continuous strip can be wider and comprise a plurality of security elements 14 arranged side by side.

[0110] Figure 4 The security element 14 is shown after the transfer of the security element transfer material to the security paper substrate 16. The security element 14 is connected to the security paper substrate 16 of the value document via a first adhesive layer 9. Above the first adhesive layer 9 there is a primer layer 8, followed by a first metallization 7 with cutouts and thus forming a pattern or symbol, and a first UV embossing lacquer layer 6. The plastic layer 5 arranged as the uppermost layer, produced by coextrusion and based on polyethylene naphthalate (PEN), serves as a protective layer. In this way, very good protection of the sensitive security element layer composite can be achieved, for example, against mechanical damage during the circulation of banknotes or against chemical damage by solvents or the like.

[0111] Figures 5 to 8 An example of the use of the security element transfer material according to the second aspect of the invention is shown, which is suitable for providing, for example, Fig. 9 The paper substrate 36 of the banknote 33 has a square through-opening 37 in the region of the second patch-shaped security element 35, which can be obtained, for example, by punching or by laser cutting. The through-opening 37 in the paper substrate 36 is therefore covered or closed on one side by the second security element 35.

[0112] Figure 5 A second security element transfer material 17 is shown, which comprises a carrier material (=temporary carrier) comprising layers 18 and 19 and an upper material comprising layers 20, 21, 22, 23, 24 and 25. The dashed line AA' shows the surface on which the upper material (i.e. the security element or transfer element to be applied to the value document) is separated from the temporary carrier during the subsequent application of the upper material to the value document.

[0113] The second security element transfer material 17 comprises a coextruded film, i.e. a composite film consisting of a polyethylene terephthalate (PET) film (i.e. a carrier substrate 18) having a thickness of 19 μm and a plastic layer 19 arranged thereon, the plastic layer being based on polyethylene naphthalate (PEN) and mixed with a certain amount of polyethylene terephthalate (PET). Layers 18 and 19 form a plastic film / plastic layer composite film that is stable against delamination. Next, a second UV embossing lacquer layer 20 is applied, the second UV embossing lacquer layer being provided with a microstructure and / or a nanostructure (the embossed structure is not shown in the figure). The second UV embossing lacquer layer 20 is then provided with a second metallization 21, which is formed in the form of a pattern or a symbol. The second metallization 21 comprises a blank portion that forms a so-called negative character. The second metallization 21 can be provided, for example, by a cleaning method known in the prior art, for example, see EP 1 972 462 A2. A primer layer 22 is then applied over the second metallization 21, which in practice serves as a leveling protective lacquer. Finally, a permanent carrier substrate 24, i.e. a polyethylene terephthalate (PET) film, and a second adhesive layer 25, i.e. a heat-sealing lacquer layer, suitable for bonding to value documents, are applied over the primer layer 22 by means of a third adhesive layer 23.

[0114] exist Figure 6 The line indicated by the reference numeral "27" in the figure shows how the security element layer composite is cut in order to pre-cut the contour shape of the security element. This can be done by means of a punch or by means of a suitable laser, such as a CO 2 The laser performs the cutting. As can be seen, the cut 27 enters into the plastic layer 19 produced by coextrusion, but not into the plastic film of the temporary carrier, ie the carrier substrate 18 .

[0115] The excess material of the security element layer composite is then removed in a so-called "edge removal" step (in accordance with Figure 6 The material outside the cutout 27 in the cross-sectional view of FIG. 2 is formed, thereby forming a void in the security element layer composite. This state is Figure 7 . A plastic layer 19 produced by coextrusion and based on polyethylene naphthalate (PEN) mixed with polyethylene terephthalate (PET) and having a high adhesion on the carrier substrate 18 serves as a release layer and makes it easier to remove excess material. Security elements 30 are located on both sides of the gap. The temporary carrier is indicated by the reference numeral 29. The security elements 30 form to a certain extent islands arranged on the temporary carrier 29. Figure 7 The security element transfer material according to the invention is shown as a continuous strip in which in the width direction there is only one security element 30. In practice the continuous strip can be wider and comprise a plurality of security elements 30 arranged side by side.

[0116] Figure 8 The security element 30 is shown after the transfer material from the security element to the security paper substrate 32. The security element 30 is connected to the security paper substrate 32 of the value document via the second adhesive layer 25. In the region of the patch-like security element 30, the paper substrate 32 of the banknote 33 has cutouts, which can be obtained, for example, by punching or by laser cutting. Above the second adhesive layer 25 there is a permanent carrier substrate 24, a third adhesive layer 23, a primer layer 22, followed by a second metallization 21 with cutouts and thus forming a pattern or symbol, and a second UV embossing lacquer layer 20 as the uppermost layer.

Claims

1. An anti-counterfeiting element transfer material, comprising - a security element layer composite having a plurality of layers, including at least one adhesive layer, a feature layer and a visible layer, wherein: The visible layer is the layer that faces the observer after the security element has been transferred to the valuable article, and a temporary carrier which is detachably connected to the visible layer of the security-element layer composite, It is characterized in that - the temporary carrier has at least one first temporary carrier substrate (4), ie a plastic film; and The visible layer of the security-element layer composite is present in the form of a plastic layer which is produced by coextrusion on the first temporary carrier substrate (4) and has low adhesion to the first temporary carrier substrate (4).

2. The anti-counterfeiting element transfer material according to claim 1, characterized in that: The first temporary carrier substrate (4) is a polyethylene terephthalate film, and the visible layer of the security element layer composite, which is in the form of a plastic layer with low adhesion on the first temporary carrier substrate (4) produced by coextrusion on the first temporary carrier substrate (4), is a polyethylene naphthalate layer.

3. The anti-counterfeiting element transfer material according to claim 1, characterized in that: The temporary carrier has a carrier layer composite which consists of a first temporary carrier substrate (4) and a second temporary carrier substrate (2), which are each a plastic film and are inseparably bonded together by means of an adhesive layer (3).

4. The anti-counterfeiting element transfer material according to claim 1, characterized in that: The contour shape of the security element is pre-cut out of the security element layer composite.

5. The security element transfer material (1) according to claim 3, characterized in that: The contour shape of the security element is pre-cut in the security element layer composite, wherein the incision (11) partially or completely cuts through the first temporary carrier substrate (4) and partially or completely cuts through the adhesive layer (3), but the incision does not enter the second temporary carrier substrate (2), so that the temporary carrier can be detached as a complete carrier layer composite.

6. The anti-counterfeiting element transfer material according to claim 4 or 5, characterized in that: The layer composite material that is outside the contour shape of the security element is removed from the security element layer composite, so that the security element transfer material has voids in the security element layer composite, while the temporary carrier has no voids.

7. The anti-counterfeiting element transfer material according to claim 1, characterized in that: The feature layer comprises an embossing lacquer layer and a metallization or a colored thin-film element.

8. An anti-counterfeiting element transfer material having - a security element layer composite having a plurality of layers, including at least one adhesive layer, a feature layer and a permanent carrier substrate (24), wherein: the characteristic layer is equal to the visible layer, and the visible layer is the layer facing the observer after the security element has been transferred to the valuable article, and a temporary carrier which is detachably connected to the visible layer of the security-element layer composite, It is characterized in that The temporary carrier has a carrier substrate (18), ie a plastic film, and has a plastic layer (19) produced on the carrier substrate (18) by coextrusion, which has a high adhesion to the carrier substrate (18); and The visible layer of the security element layer composite is detachably connected to the plastic layer ( 19 ) produced by coextrusion on the carrier substrate ( 18 ).

9. The anti-counterfeiting element transfer material according to claim 8, characterized in that: The carrier substrate (18) of the temporary carrier is a polyethylene terephthalate film, and the plastic layer (19) produced on the carrier substrate (18) by coextrusion and having high adhesion to the carrier substrate (18) is a polyethylene naphthalate layer mixed with polyethylene terephthalate.

10. The anti-counterfeiting element transfer material according to claim 8, characterized in that: The contour shape of the security element is pre-cut out of the security element layer composite.

11. The anti-counterfeiting element transfer material according to claim 8, characterized in that: The contour shape of the security element is pre-cut in the security element layer composite, wherein the cut partially or completely cuts off the plastic layer (19) produced on the carrier substrate (18) by coextrusion and having high adhesion on the carrier substrate (18), but the cut does not enter the carrier substrate (18) of the temporary carrier, so that the temporary carrier can be detached as a complete carrier layer composite.

12. The security element transfer material according to claim 8, characterized in that: The feature layer comprises an embossing lacquer layer and a metallization or a colored thin-film element.

13. The anti-counterfeiting element transfer material according to claim 7 or 12, characterized in that: The colored thin-film element is an angularly variable thin-film element which conveys different color impressions to an observer at different observation angles, or the colored thin-film element is a translucent thin-film element which conveys different color impressions to an observer when observed with reflected light and when observed with transmitted light.

14. Use of the security element transfer material according to any one of claims 1 to 13 for providing security for valuable articles using a security element.

15. Use according to claim 14 as a derivative of one of claims 8 to 13, characterized in that The valuable article is a valuable document having a through-opening (37), and the security element is applied in such a way that it covers the through-opening (37).

16. A method for producing a security element transfer material according to any one of claims 1 to 7, the method comprising - providing a first temporary carrier substrate (4), ie a plastic film, which is provided with a plastic layer produced by coextrusion, wherein The plastic layer produced by coextrusion on the first temporary carrier substrate (4) has low adhesion on the first temporary carrier substrate (4); and Arranging at least one adhesive layer and the security element layer composite with the feature layer on the plastic layer produced by coextrusion.

17. A method for producing a security element transfer material according to any one of claims 8 to 12, the method comprising: - providing a carrier substrate (18), ie a plastic film, which is provided with a plastic layer (19) produced by coextrusion, wherein: The plastic layer (19) produced by coextrusion on the carrier substrate (18) has a high adhesion to the carrier substrate (18); and - at least one adhesive layer and the security element layer composite with the feature layer are arranged on the plastic layer (19) produced by coextrusion.