Method for manufacturing welded components

By making optical marks on the cutting edges of the welded components and evaluating the location of the weld, the problem of labor-consuming and time-consuming inspection of the existing welding quality is solved, rapid and economical weld monitoring and correction are achieved, and the quality and production of welded components are improved. efficiency.

CN114633057BActive Publication Date: 2024-12-03BENTELER AUTOMOBILTECHNIK GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111540599.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-12-16
Filing Date
2021-12-16
Publication Date
2024-12-03
Estimated Expiration
2041-12-16

AI Technical Summary

Technical Problem

The quality detection methods of existing welded components are laborious and time-consuming and costly. Especially by evaluating weld unevenness through microphoto analysis, it is difficult to quickly identify and correct defects during the production process, resulting in the quality of the welded components not meeting the standards.

Method used

When making a welded member, weld position monitoring is achieved by making multiple optical marks on the cutting edges of the component section and evaluating the position of the mark with respect to the weld during or after the welding process, so as to quickly identify and correct the weld seam Defects, improve welding quality.

Benefits of technology

Through visual inspection of optical marking, the position and quality of welds can be quickly and reliably evaluated, the waste rate is reduced, the inspection cost is reduced, and the quality and production efficiency of welded components can be improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114633057B_ABST
    Figure CN114633057B_ABST
Patent Text Reader

Abstract

When producing a welded component (1), a first component section (7) having a first cut edge (8) and a second component section (9) having a second cut edge (10) are produced. The first cut edge (8) and the second cut edge (10) are positioned relative to each other and the first component section (7) and the second component section (9) are joined in a material-locking manner via a weld seam (16). According to the invention, before producing the weld seam (16), a plurality of markings (11, 12) are produced parallel to the first cut edge (8) and / or parallel to the second cut edge (10) at a distance (x) from the cut edges (8, 10). During or after producing the weld seam (16), the position of the weld seam (16) is monitored by evaluating the position of the markings (11, 12) relative to the weld seam (16).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for manufacturing a welded component. Background Art

[0002] Welding is a method for producing welded components in a defined form and is one of the most important and widely used joining methods. Welding is the use of heat and pressure to connect components in an inseparable material-locking manner with or without welding additives. In the case of joint welding, the components are joined to form a welded component by a weld seam at the weld joint. Several welded parts form a welded assembly, and several welded assemblies form a welded structure.

[0003] Components or component sections are connected to one another by welding in such a way that they meet the requirements imposed on them with regard to their expected service life. For this purpose, the welded connection must meet the required quality standards and quality properties. These are closely related to the quality standards and quality properties required of the respective component in use. If the inhomogeneities of the weld seam produced during or after welding are tolerable for the use of the welded component, then it can be assumed that sufficient quality has been achieved. If they are no longer acceptable, then the inhomogeneities are referred to as connection defects and the welded component is scrapped.

[0004] The area where welded parts are joined together is called a weld joint. There are various types of connections, which differ essentially by the structural arrangement of the workpieces or their end faces. Different types of welds are used depending on the type of connection. There are butt welds and fillet welds.

[0005] In the case of a butt joint, the workpieces or component sections to be connected lie in one plane. These workpieces or component sections may have different shapes at their ends and thus determine the shape of the weld. In the case of an I-weld, the weld and the ends of the component sections are straight. In the case of a V-weld, the end faces of the component sections are beveled. The V-weld tapers towards the root.

[0006] In butt joints, the position of the weld seam has a decisive influence on functionally relevant weld seam parameters such as burn-through (or welding flame penetration). The distance between the surface of the base material melted by welding and the original surface of the base material is called penetration. If the weld seam is located off-center (eccentric), it is very likely that a weld seam with a small burn-through will result. The welding result may therefore be unsuitable. Usually, an evaluation of weld seam parameters such as burn-through or lateral penetration length is carried out after a production batch has been completed, in particular by making microscopic sections and evaluating the micrographs. If a systematic defect occurs that is related to the weld seam position, it can only be determined after the analysis and evaluation of the microscopic sections that the entire production batch does not meet the quality standards and is rejected. The current practice of evaluating welded components by making micrographs is relatively costly and time-consuming.

[0007] Inspection of the quality of welds is very important. Various destructive or non-destructive inspection methods are known. In addition to optical inspection, there are various surface inspection methods for welds, such as magnetic particle inspection, dye penetrant inspection, ultrasonic inspection or fluoroscopy (X-ray) and inspection using image processing systems or laser profile sensors.

[0008] DE 10 2008 058 187 A1 describes a method and a device for non-destructively determining the quality of a weld seam.

[0009] A method for welding seam determination is known from DE 43 12 241 A1.

[0010] Furthermore, EP 1 245 923 A2 discloses a method and a device for edge tracking and edge detection during welded connections.

[0011] However, conventional optical or visual measurements of the weld surface and evaluation of its homogeneity can only yield inadequate conclusions about the weld depth. Destructive tests such as microscopic photo analysis are laborious and time-consuming. Similar statements also apply to magnetic particle testing, ultrasonic testing or penetrant testing. Testing using image processing systems or laser profile sensors requires expensive instrumentation. Summary of the invention

[0012] Starting from the prior art, the object of the invention is to provide a method for producing a welded component with improved welding results and a reasonable monitoring of the weld seam position which can be integrated into the production process.

[0013] According to the invention, this object is achieved by a method for producing a welded component according to the invention, wherein a first component section having a first cut edge and a second component section having a second cut edge are produced, the first cut edge and the second cut edge are then positioned relative to each other, and the first component section and the second component section are materially joined together by a weld, and before producing the weld, a plurality of marks are produced parallel to the first cut edge and / or parallel to the second cut edge at a distance from the cut edge, wherein the marks are produced simultaneously with producing the cut edges, and during or after producing the weld, the position of the weld is monitored by evaluating the position of the marks relative to the weld.

[0014] When producing a welded component, a first component section having a first cut edge and a second component section having a second cut edge are produced. This is achieved by cutting a weldable sheet material, in particular a steel sheet. To produce the welded connection, the first cut edge and the second cut edge are positioned relative to each other and the first component section is joined to the second component section in a material-locking manner by a weld seam.

[0015] According to the invention, before making the weld, a plurality of marks are made parallel to the first cut edge and / or parallel to the second cut edge at a distance from the cut edge. In order to make a material-locked connection between component sections, these component sections are connected via a weld. During or after making the weld, the position of the weld is monitored by evaluating the position of the marks relative to the weld. In this way, already during making the weld, but in particular also shortly after making the weld, the weld position can be reliably evaluated, and therefore important conclusions about the quality of the weld can be drawn. This is achieved immediately or shortly after making the weld, so that defective weld structures / patterns can be quickly identified. In this way, the manufacturing process can be directly intervened and corrective measures can be taken. The invention makes it possible to quickly evaluate the welding process parameters and the weld or welded component during the manufacturing process without destructive testing. The manufactured component is of high quality. The scrap of the manufacturing process can be reduced.

[0016] In particular, these are optical markings which are visually recognizable and enable visual inspection at the end of or during the production of the weld seam.

[0017] The invention enables improved visual monitoring or testing of weld seams and thus of the welded components produced. By identifying and evaluating the position of the weld seam relative to the marking, the course of the weld seam, in particular the weld seam center and any offset, can be reliably checked, so that conclusions can be drawn directly about the weld depth or penetration. This is achieved without expensive measuring stations and in a short time. Qualitative conclusions about the quality of the welded joint can be drawn by externally evaluating the weld seam and the weld seam position, more precisely by purely visual inspection or testing.

[0018] The process of producing or manufacturing welded components, in particular in the case of components whose component sections are joined to one another via butt joints, provides the possibility of introducing additional features in the form of markings parallel to the cut edges, in particular when cutting the sheet metal blanks to be joined along the cut edges. The position of the markings relative to the weld seam allows conclusions to be drawn about the position of the weld seam in the joint without the need for destructive testing. In this way, conclusions can be drawn about the weld seam even before the production of the micrograph and the welding parameters can be corrected if necessary.

[0019] One embodiment of the marking that is advantageous in practice provides that the marking is formed by an indentation, in particular an indentation, in the surface of the component section. The indentation can be a few tenths of a millimeter deep. Such an indentation or indentation preferably has a rounded contour, so that no or no disadvantageous incision effects occur in the component due to the marking.

[0020] In principle, it is sufficient to arrange the optical marking parallel to only one cut edge. It is particularly suitable to arrange the markings in parallel along the first cut edge and along the second cut edge. These markings are arranged at a certain distance from the cut edge. The distance is measured on the upper side of the component section perpendicular to the longitudinal axis of the cut edge. The size of the distance between the markings in a row along a cut edge is preferably the same. The distance between each marking and the adjacent cut edge is also the same. The markings in a row along the first cut edge and the markings in a row along the second cut edge are designed to be symmetrical with respect to the joint line or the weld groove.

[0021] A simple approach provides for an optical evaluation of the weld seam directly during the production process. This can be done visually (if necessary with the aid of measuring tools). Preferably, the weld seam or welded component is subsequently evaluated when the material has essentially cooled down. In the case of mass-produced welded components, templates (or gauges) suitable for this purpose can be used for testing. These templates are designed specifically for the components and weld seams to be evaluated and facilitate or improve optical or visual manual testing in a short time.

[0022] In principle, optoelectronic assistance or detection and position monitoring is of course also possible.

[0023] Within the scope of the invention, the information obtained from the weld seam position monitoring can also be used for weld seam guidance during the welding process. In such a system, the markings are detected optically and continuously compared with indicators or targets in order to ensure the desired weld quality even in large quantities. Additional evaluation features such as the position, size and shape of the weld seam and the speed during the welding process can be incorporated into this system.

[0024] The invention makes it possible to detect defects and reliably monitor the weld seam in a simple manner. When defects or tolerances occur, a corresponding reaction can be made in a short time and deviations can be noted or corrected in time.

[0025] Particularly advantageously, when producing the cut edge, the marking is produced simultaneously. In particular, the marking is placed in the component surface along the cut edge of the component section directly in parallel with the cutting process.

[0026] However, in principle it is also possible to produce the marking before or after producing the cut edge.

[0027] The time of making the mark depends on the geometry of the welded component to be produced and the direction of the shearing edge. The time of making the mark is advantageously integrated into the production process of the welded component.

[0028] It is preferably provided that the component or its component body is formed from one or more sheet metal blanks.

[0029] The welded component or the component body of this component can be made of a metal plate. Such a component is for example an integral pipe body, wherein a steel sheet blank is formed into a pipe and welded together along the cut edges positioned mutually by a butt joint.

[0030] The component or its component body can also be formed from a plurality of cut-to-size and optionally preformed metal sheets (for example two half shells).

[0031] The method according to the invention for producing welded components is particularly suitable for producing motor vehicle components such as longitudinally welded tubes, cross members or torsional profiles, as well as steering arm components, motor vehicle pillars or floor beams which are formed and / or assembled from sheet metal blanks. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] The present invention is described in detail below with the aid of the accompanying drawings.

[0033] Figure 1 The cutting edge production on two component sections is shown in a simplified technical manner;

[0034] Figure 2 Two component sections positioned relative to each other before the welding process;

[0035] Figure 3 Component sections that are joined together by a weld seam;

[0036] Figure 4 Two component sections with properly completed welds;

[0037] Figure 5 Two component sections with defective welds;

[0038] Figure 6for Figure 4 A top view of two component sections and a weld seam shown in the accompanying drawings;

[0039] Figure 7 for Figure 5 A top view of two component sections and a weld seam shown in the accompanying drawings;

[0040] Figure 8 is a perspective view of a welded component made according to the present invention within a welded assembly, and

[0041] Fig. 9 for Figure 8 A vertical cross section of a twisted profile is shown in the accompanying drawings. DETAILED DESCRIPTION

[0042] exist Figure 8 1 shows a welded component 1 in the form of a torsion profile, produced according to the invention, of a combined control arm axle 2. A trailing arm 5, 6 (trailing control arm or trailing arm) is welded to each end 3, 4 of the torsion profile 1. Fig. 9 A vertical cross section of a twisted profile 1 is shown.

[0043] In order to make Figure 8 and 9 In the welded component 1 shown in FIG. 1 , a sheet metal blank is prepared. The sheet metal blank corresponds to the unfolded state of the component 1 to be manufactured. When the sheet metal blank is cut, a first component section 7 having a first trimmed edge 8 and a second component section 9 having a second trimmed edge 10 are manufactured.

[0044] With the help of Figure 1 The production of a sheet metal blank is schematically illustrated. When the sheet metal blank is cut, a plurality of optical markings 11, 12 are respectively produced in the surface 13 of the sheet metal blank or of the first component section 7 and the second component section 9 parallel to the first cut edge 8 and parallel to the second cut edge 10 and at a distance x from the cut edge 8 or 10. The markings 11, 12 are formed by indentations 14, in particular embossments, in the surface 13 of the respective component section 7, 9. Figure 1 A shearing and punching die is schematically shown in FIG. 1 and is labeled with the reference symbol W. The indentation is a few tenths of a millimeter deep. The spacing x is measured transversely to the longitudinal direction of the cutting edges 8 , 10 and at right angles to the cutting edges 8 , 10 .

[0045] Figure 6 and 7 It is shown that in each first component section 7 and in each second component section 9, a plurality of markings 11, 12 are arranged in a row along the corresponding cutting edge 8, 10 parallel to the cutting edge 8, 10. The size of the spacing l between the markings 11, 12 in a row in the first component section 7 or in the second component section 9 is equal.

[0046] The sheet metal blank is then formed and the first trimmed edge 8 and the second trimmed edge 10 are positioned relative to one another. In the case of a welded component 1 whose geometry is V-shaped in cross section, the sheet metal blank is formed into a slotted tube. The first component section 7 and the second component section 9 have the same thickness d. The first component section 7 and the second component section 9 are located in one plane so that the first trimmed edge 8 and the second trimmed edge 10 abut against one another or are positioned relative to one another with a butt joint 15 (see Figure 2 ).

[0047] The end cut edges 8, 10 extend straight. Such a butt joint 15 is also called an I-joint. The first component section 7 is then joined to the second component section 9 in a material-locking manner by a weld seam 16. This weld seam is designed as a V-shaped weld seam and the weld root formed tapers toward the lower side 17 of the component sections 7, 9.

[0048] Figure 3 The component sections 7, 9 are shown as being materially connected to one another via a weld seam 16. An optical marking 11, 12 is visible to the left and right of the weld seam 16. The weld seam 16 extends along the center of the weld groove between the two component sections 7, 9 (see also Figure 6 ).

[0049] With the help of Figure 4 and 5 The quality features of the weld seam 16 are described. Figure 4 The normal weld position in the center between the component sections 7, 9 is shown. The spacings a1 and a2 are equal, starting from the center line ML extending in the longitudinal direction of the weld 16 to the left in the drawing plane to the adjacent upper edge 18 of the marking 11 arranged in the first component section 7 and to the right to the adjacent upper edge 19 of the marking 12 arranged in the second component section 9. The penetration t is the normal depth. The position of the weld 16 is monitored by evaluating the position of the markings 11, 12 relative to the weld 16, from which reliable conclusions and conclusions about the strength of the penetration t can be drawn. The welded component 1 is normal.

[0050] In such Figure 5 and Figure 7In the case shown, different evaluations of the position monitoring of the weld seam 16 result. The weld seam 16 is arranged eccentrically and extends offset to the right in the plane of the drawing, toward the second component section 9. The distance a1 to the marking 11 in the first component section 7 is greater than the distance a2 to the marking 12 in the second component section 9. The penetration t is not deep enough. The weld bead is offset and deviates from the weld seam center. By evaluating the position of the markings 11, 12 relative to the weld seam 16, it can be visually determined that the weld seam 16 is insufficient and most likely does not meet the required strength, so that the component is at risk of not meeting the requirements for service life. The component is therefore unacceptable and should be rejected. This evaluation is carried out visually, if necessary with the help of a template / gauge designed for this purpose.

[0051] If a weld seam pattern is determined to be unacceptable, the manufacturing process can be intervened quickly. This can be done at short notice before further weld seam inspections (e.g. ultrasonic testing or subsequent evaluation of micrographs) are carried out.

[0052] As in Figure 8 and 9 As can be seen in FIG. 1 , on the finished component 1 , the markings 11 , 12 each extend at a perpendicular distance from the cut edges 8 , 10 or the weld seam 16 extending in the longitudinal direction.

[0053] The externally visible optical markings 11 , 12 also allow the weld seam pattern to be checked during subsequent further processing of the welded component 1 and thus the quality assessment of the welded component 1 to be carried out.

[0054] The information obtained from the position monitoring of the weld seam 16 can be used for automated weld seam guidance of the weld seam 16 during the welding process.

[0055] Reference numerals list

[0056] 1 Component

[0057] 2 Combined tie rod shaft

[0058] 3 1 End

[0059] 4 1 end

[0060] 5 Trailing arm

[0061] 6 Trailing arms

[0062] 7 First component section

[0063] 8. Cutting edge

[0064] 9 Second component section

[0065] 10 Second cutting edge

[0066] 11 Optical marking

[0067] 12 Optical marking

[0068] 13 Surface

[0069] 14 Dent

[0070] 15 Butt joint

[0071] 16 Weld

[0072] 17 Lower side

[0073] 18 8 upper edge

[0074] 19 10 upper edge

[0075] a1 spacing

[0076] a2 spacing

[0077] d Thickness

[0078] Spacing

[0079] t Melt depth

[0080] x Spacing

[0081] ML Centerline

[0082] W Shearing and Punching Dies

Claims

1. A method for producing a welded component (1), wherein a first component section (7) having a first cut edge (8) and a second component section (9) having a second cut edge (10) are produced, wherein: A welding groove is provided between a first component section (7) and a second component section (9), and then a first trimmed edge (8) and a second trimmed edge (10) are positioned relative to each other, and the first component section (7) and the second component section (9) are joined in a material-locking manner via a weld seam (16), characterized in that before producing the weld seam (16), a plurality of marks (11, 12) are produced parallel to the first trimmed edge (8) and / or parallel to the second trimmed edge (10) at a distance (x) from the first trimmed edge (8) and / or the second trimmed edge (10), wherein the marks (11, 12) are produced simultaneously with the production of the first trimmed edge (8) and / or the second trimmed edge (10), and during or after the production of the weld seam (16), the position of the weld seam (16) is monitored by evaluating the position of the marks (11, 12) relative to the weld seam (16).

2. The method according to claim 1, characterized in that: The markings (11, 12) are produced by means of indentations (14) in the surface (13) of the first component section (7) and / or the second component section (9).

3. The method according to claim 1 or 2, characterized in that: The first cut edge (8) of the first component section (7) and the second cut edge (10) of the second component section (9) are positioned relative to each other by means of a butt joint (15).

4. The method according to claim 1 or 2, characterized in that: The component (1) or the component body of the component (1) is formed from a sheet metal blank.

5. The method according to claim 1 or 2, characterized in that: The component (1) or the component body of the component (1) is composed of a plurality of sheet metal blanks.

6. The method according to claim 1 or 2, characterized in that: The information obtained from the position monitoring of the weld seam (16) is used for weld seam guidance during the welding process.

7. The method according to claim 1, characterized in that: The markings (11, 12) are produced by indentations in the surface (13) of the first component section (7) and / or the second component section (9).