Display panel and method for manufacturing display panel

By using charged ion scanning technology to expose potential dark spots and repair them in the manufacturing process of OLED display panels, the problem of untimely exposure of dark spots and risk-free pixels becoming dark spots in the prior art is solved, and product yield and reliability are improved. Reduced manufacturing costs.

CN114709356BActive Publication Date: 2024-11-26SHENZHEN CHINA STAR OPTOELECTRONICS SEMICON DISPLAY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210458420.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-27
Publication Date
2024-11-26
Estimated Expiration
2042-04-27

AI Technical Summary

Technical Problem

It is difficult for existing OLED display panels to expose potential dark spots early during the manufacturing process, resulting in product yield and reliability affected. The general reverse voltage repair method can easily turn risk-free pixels into dark spots, increasing manufacturing costs.

Method used

After forming the driving circuit layer, anode and cathode on the substrate, charged ion scanning technology (such as electron beam or plasma scanning) is used to expose potential dark spots and release excess charge after the scan is completed to repair dark spots and avoid risk-free pixels Turns into a dark spot.

Benefits of technology

It improves the yield and reliability of OLED display panels, saves repair production capacity, reduces manufacturing costs, and avoids the risk of risk-free pixels becoming dark spots.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114709356B_ABST
    Figure CN114709356B_ABST
Patent Text Reader

Abstract

The embodiments of the present application provide a display panel and a method for manufacturing the display panel. By performing charged ion scanning on the substrate, not only can potential dark spots be exposed, but also the problem of anode and cathode breakdown will not occur. This can avoid turning pixels that do not have potential dark spot risks into dark spots, thereby improving the yield and reliability of the product, saving repair capacity, and reducing manufacturing costs.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display technology, and in particular to a display panel and a method for manufacturing the display panel. Background Art

[0002] At present, the market maturity of medium and large-sized organic light emitting diode (OLED) display panels is increasing, and the market share is also increasing. However, the current prices of OLED TVs or monitors remain high. One reason is that the material cost of OLED is higher than that of liquid crystal display panels (LCD). Another reason is that the OLED manufacturing process is relatively complex and it is difficult to improve the yield. The dark spot problem is one of the most important keys to improving the yield of OLED.

[0003] like Figure 1 As shown, in the pixel without particles and anode protrusions, the film thickness uniformity of the anode 11 and the cathode 13 is good, the charge distribution is relatively uniform, and the problem of cathode and cathode breakdown will not occur. One of the main reasons for dark spots is: Figure 2 The particles 14 with larger particle sizes in the light-emitting layer 12 shown in the figure cause a potential leakage path between the cathode 13 and the anode 11. Another major cause of dark spots is: Figure 3 The anode protrusion 110 shown causes a potential leakage path between the cathode 13 and the anode 11. When the potential leakage path is turned on, the current can be concentrated at the potential leakage path position and flow from the anode to the cathode, resulting in no electron-hole recombination in the OLED light-emitting device, and the OLED light-emitting device cannot emit light, thereby forming a dark spot. Some dark spots will not be discovered immediately during the lighting test phase after manufacturing is completed, but will only appear after a period of time, or even after a period of use in the hands of the end user, which has a relatively serious impact on product yield and reliability. Therefore, it is necessary to expose the dark spots as early as possible during the product manufacturing process.

[0004] The current common method is to apply reverse voltage to the pixels. By applying a certain voltage, pixels with particle or anode protrusion problems will have some potential leakage paths between the anodes, and the anode and cathode will be broken down due to the voltage difference, thereby exposing the hidden dark spots in advance. However, the process of applying voltage is to put pressure on all pixels on the entire surface, which can easily turn some pixels that do not have potential dark spot risks into dark spots, resulting in excessive repair, waste of repair capacity, and increased manufacturing costs.

[0005] In summary, the existing method of exposing potential dark spots is to apply reverse voltage to all pixels of the display panel, which may cause pixels without potential dark spot risk to become dark spots. Therefore, it is necessary to provide a display panel and a method for manufacturing the display panel to improve this defect. Summary of the invention

[0006] The embodiments of the present application provide a display panel and a method for manufacturing the display panel, which can not only expose potential dark spots, but also prevent pixels that have no potential dark spot risks from becoming dark spots, thereby improving the yield and reliability of the product, saving repair capacity, and reducing manufacturing costs.

[0007] The present application provides a method for manufacturing a display panel, including:

[0008] A driving circuit layer, an anode, a light-emitting layer and a cathode are sequentially formed on the substrate;

[0009] Scanning the substrate with charged ions to expose potential dark spots; and

[0010] The dark spots are repaired.

[0011] According to an embodiment of the present application, the charged ion scanning on the substrate is performed by electron beam scanning or plasma scanning.

[0012] According to an embodiment of the present application, the method for manufacturing the display panel further includes:

[0013] After the scanning is finished, the probe connected to the ground wire is connected to the test terminal on the substrate to release the excess charge.

[0014] According to an embodiment of the present application, the step of forming the anode includes:

[0015] forming a first anode material layer on the driving circuit layer;

[0016] forming a second anode material layer on the first anode material layer; and

[0017] forming a third anode material layer on the second anode material layer;

[0018] The first anode material layer, the second anode material layer and the third anode material layer constitute the anode, the first anode material layer and the third anode material layer are both made of transparent conductive oxides, and the second anode material layer is made of metal.

[0019] According to an embodiment of the present application, the transparent conductive oxide is indium tin oxide or indium zinc oxide, and the material of the second anode material layer is silver.

[0020] According to an embodiment of the present application, the material of the first anode material layer is the same as the material of the third anode material layer.

[0021] According to an embodiment of the present application, the thickness of the second anode material layer is greater than the thickness of the first anode material layer and the thickness of the third anode material layer.

[0022] According to one embodiment of the present application, the thickness of the first anode material layer is greater than or equal to 100 μm and less than or equal to 200 μm, the thickness of the second anode material layer is greater than or equal to 1000 μm and less than or equal to 2000 μm, and the thickness of the third anode material layer is greater than or equal to 100 μm and less than or equal to 200 μm.

[0023] According to an embodiment of the present application, the material of the cathode is a mixture of magnesium and silver; or the cathode is a stacked structure of silver and transparent conductive oxide.

[0024] According to the method for manufacturing a display panel provided in the above embodiment of the present application, an embodiment of the present application further provides a display panel, and the display panel is manufactured by the method for manufacturing a display panel provided in the above embodiment.

[0025] Beneficial effects of the embodiments of the present application: The embodiments of the present application provide a display panel and a method for manufacturing a display panel, wherein the method for manufacturing a display panel is used to manufacture the display panel, and after a driving circuit layer, an anode, a light-emitting layer and a cathode are sequentially formed on a substrate, the substrate is subjected to charged ion scanning, and pixels with particles or anode protrusions are more likely to accumulate charge at more protruding positions due to the tip discharge characteristics, and when the charge accumulates to a certain amount, the local potential difference causes the cathode and anode to break down, causing a short circuit between the cathode and the anode, exposing potential dark spots; pixels without particles and anode protrusions, due to the better uniformity of the film thickness of the anode and cathode, the charge distribution is more uniform, and the problem of cathode and anode breakdown will not occur, thereby avoiding pixels with no potential dark spot risk from becoming dark spots, thereby not only improving the product yield and reliability, but also saving repair capacity and reducing manufacturing costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] In order to more clearly illustrate the technical solutions in the embodiments or the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0027] Figure 1 is a schematic diagram of a normal pixel in the related art;

[0028] Figure 2 A schematic diagram of an abnormal pixel containing particles in the related art;

[0029] Figure 3 A schematic diagram of an abnormal pixel with an anode protrusion in the related art;

[0030] Figure 4 A flowchart of a method for manufacturing a display panel provided in an embodiment of the present application;

[0031] Figure 5a to Figure 5c A schematic diagram of the process structure of a method for manufacturing a display panel provided in an embodiment of the present application;

[0032] Figure 6 A schematic diagram of the structure of the anode provided in an embodiment of the present application. DETAILED DESCRIPTION

[0033] The following descriptions of the embodiments are made with reference to the attached drawings to illustrate specific embodiments that the present application may be implemented in. The directional terms mentioned in the present application, such as [up], [down], [front], [back], [left], [right], [inside], [outside], [side], etc., are only with reference to the directions of the attached drawings. Therefore, the directional terms used are used to illustrate and understand the present application, rather than to limit the present application. In the drawings, units with similar structures are represented by the same reference numerals.

[0034] The present application is further described below in conjunction with the accompanying drawings and specific embodiments.

[0035] The embodiment of the present application provides a method for manufacturing a display panel, which can not only expose potential dark spots, but also avoid turning pixels that have no potential dark spot risks into dark spots, thereby improving the yield and reliability of the product, saving repair capacity, and reducing manufacturing costs.

[0036] Combination Figure 4 to Figure 5c As shown, Figure 4 A flowchart of a method for manufacturing a display panel provided in an embodiment of the present application, Figure 5a to Figure 5c The present invention provides a schematic diagram of a process structure of a method for manufacturing a display panel according to an embodiment of the present invention. The method for manufacturing a display panel includes:

[0037] Step S10 : forming a driving circuit layer 21 , an anode 22 , a light emitting layer 23 and a cathode 24 in sequence on the substrate 20 .

[0038] The substrate 20 may be a flexible substrate made of a transparent flexible material, and the flexible material may include but is not limited to flexible transparent organic materials such as polyimide. The substrate 20 may also be made of a transparent and hard inorganic material, for example, the substrate 20 may be a glass substrate.

[0039] like Figure 5a As shown, the driving circuit layer 21 is disposed on one side of the substrate 20. The driving circuit layer 21 may be in direct contact with a surface of one side of the substrate 20, or may be in indirect contact with the substrate 20. The driving circuit layer 21 may be formed by overlapping multiple inorganic insulating layers and metal layers, and the metal layers may include but are not limited to gate metal layers, source and drain electrode metal layers, etc. The driving circuit layer 21 may also include a flat layer away from the side of the substrate 20.

[0040] A plurality of anodes 22 are disposed on a side of the driving circuit layer 21 away from the substrate 20 and are distributed in an array on the driving circuit layer 21. The anodes 22 may be directly disposed on a surface of a side of the flat layer in the driving circuit layer 21 away from the substrate 20. The anodes 22 may be electrically connected to a source or drain of a thin film transistor in the driving circuit layer 21.

[0041] The step of forming the anode 22 in step S10 includes: forming a first anode material layer 221 on the driving circuit layer 21 ; forming a second anode material layer 222 on the first anode material layer 221 ; and forming a third anode material layer 223 on the second anode material layer 222 .

[0042] like Figure 6 As shown, Figure 6 This is a schematic diagram of the structure of the anode provided in an embodiment of the present application. The first anode material layer 221 , the second anode material layer 222 , and the third anode material layer 223 constitute the anode 22 .

[0043] Furthermore, the materials of the first anode material layer 221 and the third anode material layer 223 are both transparent conductive oxides, and the material of the second anode material layer 222 is metal.

[0044] Furthermore, the transparent conductive oxide is indium tin oxide (ITO) or indium zinc oxide (IZO), and the material of the second anode material layer 222 is silver.

[0045] The display panel provided in the embodiment of the present application is a top-emitting OLED display panel. The second anode material layer 222 is made of silver with a high reflectivity, which can reflect the light emitted from the light-emitting layer 23 toward the anode 22 side to be emitted from the light-emitting side of the display panel, thereby improving the utilization rate of the light. The first anode material layer 221 and the third anode material layer 223 are both made of transparent conductive oxide, which can protect the second anode material layer 222 on the one hand, prevent the second anode material layer 222 from oxidation or corrosion, and on the other hand, reduce the absorption of light and improve the utilization rate of light.

[0046] In one embodiment, the material of the first anode material layer 221 and the third anode material layer 223 may be the same. For example, the materials of the first anode material layer 221 and the third anode material layer 223 are both indium tin oxide; or, the materials of the first anode material layer 221 and the third anode material layer 223 are both indium zinc oxide.

[0047] In one embodiment, the materials of the first anode material layer 221 and the third anode material layer 223 may also be different. For example, the material of the first anode material layer 221 is indium tin oxide, and the material of the third anode material layer 223 is indium zinc oxide; or, the material of the first anode material layer 221 is indium zinc oxide, and the material of the third anode material layer 223 is indium tin oxide.

[0048] Furthermore, the thickness of the second anode material layer 222 is greater than the thickness of the first anode material layer 221 and the thickness of the third anode material layer 223, so as to avoid a reduction in the transmittance of the first anode material layer 221 and the third anode material layer 223 due to the first anode material layer 221 and the third anode material layer 223 being too thin.

[0049] In one embodiment, the thickness of the first anode material layer 221 is greater than or equal to 100 μm and less than or equal to 200 μm, the thickness of the second anode material layer 222 is greater than or equal to 1000 μm and less than or equal to 2000 μm, and the thickness of the third anode material layer 223 is greater than or equal to 100 μm and less than or equal to 200 μm.

[0050] For example, the thickness of the first anode material layer 221 may be but is not limited to any one of 100μm, 120μm, 140μm, 150μm, 160μm, 180μm or 200μm, etc., the thickness of the second anode material layer 222 may be but is not limited to any one of 1000μm, 1200μm, 1400μm, 1500μm, 1600μm, 1800μm or 2000μm, etc., and the thickness of the third anode material layer 223 may be but is not limited to any one of 100μm, 120μm, 140μm, 150μm, 160μm, 180μm or 200μm, etc.

[0051] In one embodiment, the thickness of the first anode material layer 221 may be equal to or different from the thickness of the third anode material layer 223 .

[0052] like Figure 5aAs shown, the light-emitting layer 23 is arranged on the side of the anode 22 away from the driving circuit layer 21. The light-emitting layer 23 may include a stacked hole injection layer (HIL) 231, a hole transport layer (HTL) 232, an emission layer (EML) 233, and an electron transport layer (ETL) 234. The hole injection layer 231, the hole transport layer 232, and the electron transport layer 234 may be formed by a whole-surface evaporation process, and the emission layer 233 may be formed by an inkjet printing method. The display panel may include a plurality of emission layers 233 distributed in an array, and the material of the emission layer 233 is an organic light-emitting material.

[0053] The cathode 24 is disposed on a side of the light emitting layer 23 away from the anode 22. The material of the cathode 24 may be a mixture of magnesium and silver, or may be a laminated structure formed by stacking silver and a transparent conductive oxide material, for example, the cathode 24 may be a laminated structure of silver / indium zinc oxide, or may be a laminated structure of indium zinc oxide / silver.

[0054] The cathode 24 may be formed by a whole-surface evaporation process. The display panel may include a plurality of pixels distributed in an array in a display area, each pixel may have an organic light emitting diode, and the organic light emitting diode may be composed of an anode 22 , a light emitting layer 23 and a cathode 24 .

[0055] Step S20: performing charged ion scanning on the substrate 20 to expose potential dark spots.

[0056] In one embodiment, the substrate 20 may be scanned with charged ions by electron beam scanning.

[0057] In one embodiment, the substrate 20 may be scanned with charged ions by plasma scanning.

[0058] During the process of charged ion scanning of the substrate 20, the charge will gradually accumulate in the cathode 24. In the pixels without particles or anode protrusions, the thickness uniformity of the cathode 24 and the anode 22 is good, the charge distribution is relatively uniform, and there will be no problem of cathode and anode breakdown. Pixels with particles or anode protrusions will become potential dark spots. Due to the tip discharge characteristics, the more protruding positions are more likely to accumulate voltage. When the charge accumulates to a certain amount, due to the local potential difference, the cathode and anode breakdown occurs, resulting in a short circuit between the cathode 24 and the anode 22, exposing the potential dark spots.

[0059] In the embodiment of the present application, the process of performing charged ion scanning on the substrate 20 in step S20 needs to be performed in a vacuum environment. Figure 5b An inert gas is injected into the vacuum chamber 30 shown, and an ion generator 40 is used to perform charged ion scanning on the substrate 20 by electron beam scanning or plasma scanning. The inert gas may be, but is not limited to, argon.

[0060] It should be noted that if the charged ion scanning is not performed in a vacuum environment, the charged ions will collide with the gas in the air, so that the charged ions that can actually be applied to the surface of the substrate 20 are greatly reduced, and the effect of breaking down the anode and cathode of the potential dark spot cannot be achieved, and the potential dark spot cannot be exposed.

[0061] Step S30: repairing the dark spot.

[0062] In an embodiment of the present application, the pixel generating the dark spot can be cut by a laser to destroy the cathode and the light-emitting layer of the pixel by the laser; or, the entire pixel generating the dark spot can be circularly cut by a laser to prevent it from emitting light normally.

[0063] Furthermore, the method for manufacturing the display panel further includes:

[0064] Step S40: After the scanning is completed, the probe connected to the ground line is connected to the test terminal on the substrate 20 to release the excess charge.

[0065] like Figure 5c As shown, after the scan is completed, the probe 50 connected to the ground line is connected to the test terminal on the substrate 20 to release the accumulated charge on the substrate 20, so as to avoid electrostatic breakdown caused by excessive charge accumulation and damage to the device.

[0066] The step S40 may be performed after the dark spots are repaired, or after the substrate is scanned with charged ions, which is not limited here.

[0067] According to the method for manufacturing a display panel provided in the above embodiment of the present application, an embodiment of the present application further provides a display panel, and the display panel can be manufactured by the method for manufacturing a display panel provided in the above embodiment.

[0068] Based on the display panel provided in the above embodiments of the present application, the embodiments of the present application also provide an electronic device, which includes the display panel provided in the above embodiments. The electronic device can be a mobile terminal, such as color electronic paper, color electronic book, smart phone, etc. The electronic device can also be a wearable terminal, such as a smart watch, smart bracelet, etc. The electronic device can also be a fixed terminal, such as a color electronic billboard, color electronic poster, etc.

[0069] Beneficial effects of the embodiments of the present application: The embodiments of the present application provide a display panel and a method for manufacturing a display panel, wherein the method for manufacturing a display panel is used to manufacture the display panel, and after a driving circuit layer, an anode, a light-emitting layer and a cathode are sequentially formed on a substrate, the substrate is subjected to charged ion scanning, and pixels with particles or anode protrusions are more likely to accumulate charge at more protruding positions due to the tip discharge characteristics, and when the charge accumulates to a certain amount, the local potential difference causes the cathode and anode to break down, causing a short circuit between the cathode and the anode, exposing potential dark spots; pixels without particles and anode protrusions, due to the better uniformity of the film thickness of the anode and cathode, the charge distribution is more uniform, and the problem of cathode and anode breakdown will not occur, thereby avoiding pixels with no potential dark spot risk from becoming dark spots, thereby not only improving the product yield and reliability, but also saving repair capacity and reducing manufacturing costs.

[0070] In summary, although the present application is disclosed as above with preferred embodiments, the above preferred embodiments are not intended to limit the present application. Ordinary technicians in this field can make various changes and modifications without departing from the spirit and scope of the present application. Therefore, the scope of protection of the present application is based on the scope defined by the claims.

Claims

1. A method for manufacturing a display panel, characterized in that: include: A driving circuit layer, an anode, a light-emitting layer and a cathode are sequentially formed on the substrate; Performing charged ion scanning on the substrate to cause electrostatic breakdown on pixels with particles or anode protrusions, resulting in a short circuit between the anode and the cathode of the pixel, thereby exposing potential dark spots; as well as The dark spots are repaired.

2. The method for manufacturing a display panel according to claim 1, wherein: The charged ion scanning method for the substrate is electron beam scanning or plasma scanning.

3. The method for manufacturing a display panel according to claim 1, wherein: The method for manufacturing the display panel further includes: After the scanning is finished, the probe connected to the ground wire is connected to the test terminal on the substrate to release the excess charge.

4. The method for manufacturing a display panel according to claim 1, wherein: The steps of forming the anode include: forming a first anode material layer on the driving circuit layer; forming a second anode material layer on the first anode material layer; and forming a third anode material layer on the second anode material layer; The first anode material layer, the second anode material layer and the third anode material layer constitute the anode, the first anode material layer and the third anode material layer are both made of transparent conductive oxides, and the second anode material layer is made of metal.

5. The method for manufacturing a display panel according to claim 4, wherein: The transparent conductive oxide is indium tin oxide or indium zinc oxide, and the material of the second anode material layer is silver.

6. The method for manufacturing a display panel according to claim 5, wherein: The material of the first anode material layer is the same as that of the third anode material layer.

7. The method for manufacturing a display panel according to claim 4, wherein: The thickness of the second anode material layer is greater than the thickness of the first anode material layer and the thickness of the third anode material layer.

8. The method for manufacturing a display panel according to claim 7, wherein: The thickness of the first anode material layer is greater than or equal to 100 μm and less than or equal to 200 μm, the thickness of the second anode material layer is greater than or equal to 1000 μm and less than or equal to 2000 μm, and the thickness of the third anode material layer is greater than or equal to 100 μm and less than or equal to 200 μm.

9. The method for manufacturing a display panel according to claim 1, wherein: The cathode material is a mixture of magnesium and silver; or the cathode is a stacked structure of silver and transparent conductive oxide.

10. A display panel, characterized in that: The display panel is manufactured by the method for manufacturing a display panel according to any one of claims 1 to 9.