Ring part deformation correction method and system

Through the three-dimensional dimensional measurement of the casing-like annular parts and the finite element simulation model combined with the correction method of the curved mold and multi-point loading tooling, the problem of low deformation correction accuracy of the annular parts in the existing technology has been solved, and high-quality and accurate deformation correction has been achieved. correction effect.

CN114818172BActive Publication Date: 2024-10-01TSINGHUA UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210334178.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-03-31
Publication Date
2024-10-01
Estimated Expiration
2042-03-31

AI Technical Summary

Technical Problem

It is difficult to achieve high-quality and precise deformation correction of casing-like annular parts with existing technology, especially in the case of multi-directional deformation and complex shapes. There are problems of low accuracy and high difficulty.

Method used

Obtain the deformation distribution law by measuring the three-dimensional dimensional profile of the parts to be processed, establish a finite element simulation model, use curved surface molds of different sizes to perform the first correction, and perform the second correction through multi-point loading tooling until the deformation meets the preset range requirements. .

Benefits of technology

It achieves high-quality and precise correction of casing-like annular parts, improves the correction accuracy, avoids microscopic or macroscopic damage to the material, and ensures the dimensional stability of the parts.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114818172B_ABST
    Figure CN114818172B_ABST
Patent Text Reader

Abstract

The present invention provides a method and system for correcting deformation of an annular part, wherein the method comprises: measuring the three-dimensional dimensional profile of the part to be processed, obtaining the first deformation distribution law of the part to be processed; based on the first deformation distribution law, establishing a finite element simulation model, and using curved surface molds of different sizes to perform a first correction on the part to be processed; obtaining the second deformation distribution law of the part to be processed after the first correction; based on the second deformation distribution law, using a multi-point loading tooling to perform a second correction on the part to be processed, until the deformation amount of the part to be processed meets the preset range requirements. The above invention can realize efficient and safe correction of parts.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of part deformation correction, and more specifically, to a method and system for correcting annular part deformation. Background Art

[0002] In the manufacturing process of parts, when parts have been finished but still have deformation, or when finished spare parts in stock or installed parts are deformed due to the release of residual stress, the problem can only be solved by deformation correction.

[0003] The fundamental principle of existing deformation correction is to make the deformed parts undergo reverse plastic deformation and eliminate the original deformation after unloading and rebound. However, since once the material undergoes plastic deformation, there will be risks of microscopic or macroscopic damage, the correction work must avoid these risks and control the correction plastic strain to the minimum.

[0004] At present, most of the correction research is aimed at one-dimensional deformation problems, and research on two-dimensional deformation is rarely seen, especially the three-dimensional safety correction of annular parts is even more lacking. It can be seen that casing parts are generally rotating bodies, and deformation may be multi-directional. In addition, the casing inner bore, stop size and shape will affect the blade tip clearance or fit quality. Therefore, the correction of casing parts requires high correction accuracy, but the current correction scheme is difficult to achieve high-quality and accurate correction of casing parts. Summary of the invention

[0005] In view of the above problems, an object of the present invention is to provide a method and system for correcting deformation of annular parts, so as to solve the problems of low accuracy and great difficulty in the existing correction of deformation of annular parts of casings.

[0006] The annular part deformation correction method provided by the present invention comprises: measuring the three-dimensional size profile of the part to be processed to obtain the first deformation distribution law of the part to be processed; based on the first deformation distribution law, establishing a finite element simulation model, and using curved surface molds of different sizes to perform a first correction on the part to be processed; obtaining the second deformation distribution law of the part to be processed after the first correction; based on the second deformation distribution law, using a multi-point loading tooling to perform a second correction on the part to be processed until the deformation amount of the part to be processed meets the preset range requirements.

[0007] In addition, the preferred technical solution is to measure the three-dimensional dimensional contour of the part to be processed, and the step of obtaining the first deformation distribution law of the part to be processed includes: using a three-dimensional coordinate measuring machine to measure the three-dimensional dimensional contour of the part to be processed to obtain the three-dimensional size of the part to be processed; based on the three-dimensional size and the preset ideal size and allowable deviation range, determine the first deformation distribution law.

[0008] In addition, the preferred technical solution is that the curved surface mold includes matching inner and outer molds, and the steps of performing a first correction on the part to be processed using curved surface molds of different sizes include: determining the mold correction amount and the shapes and sizes of the inner and outer molds according to the first deformation distribution law; performing a first correction on the part to be processed based on the correction amount and the inner and outer molds, and obtaining the deformation distribution law of the part to be processed after the first correction; adjusting the mold correction amount based on the deformation distribution law of the part to be processed after the first correction, and performing a second first correction based on the adjusted new mold correction amount; and looping the above steps until the deformation amount of the part to be processed meets the first preset range requirements.

[0009] In addition, the preferred technical solution is that based on the second deformation distribution law, a multi-point loading tool is used to perform a second correction on the part to be processed until the deformation of the part to be processed meets the requirements of a preset range. The steps include: based on the second deformation distribution law, determining the positions of deformation points of the part to be processed that are ranked in front of a preset number of deformation points; and performing reverse deformation correction on the deformation points one by one based on the multi-point loading tool.

[0010] In addition, the preferred technical solution is that the step of performing reverse deformation correction on the deformation points one by one based on the multi-point loading tooling includes: using a finite element simulation model to perform function fitting on the correction amount of the deformation point and the corresponding maximum deformation amount to determine the correction deformation curve; based on the correction deformation curve, determining the actual deformation amount of the deformation point; based on the multi-point loading tooling and the actual deformation amount, performing reverse deformation correction on the deformation points one by one.

[0011] In addition, a preferred technical solution is that the correction deformation curve includes a correction deformation curve 1 when extruding from the outside to the inside, and a correction deformation curve 2 when extruding from the inside to the outside; wherein the expression of the correction deformation curve 1 is:

[0012]

[0013] The expression of the correction deformation curve 2 is:

[0014]

[0015] Wherein, x represents the correction amount, y1 and y2 represent the deformation amounts, a1 and b1 represent the fitting coefficients of the correction deformation curve 1, and a2 and b2 represent the fitting coefficients of the correction deformation curve 2.

[0016] In addition, a preferred technical solution is that the multi-point loading tooling includes a driving device and a cylindrical pressing head arranged at the end of the driving device.

[0017] In addition, a preferred technical solution is that the cylindrical pressing head is an elastic-plastic body.

[0018] In addition, a preferred technical solution is that the parts to be processed include casing ring parts.

[0019] According to another aspect of the present invention, a ring-shaped part deformation correction system is provided, comprising: a first deformation distribution law acquisition unit, used to measure the three-dimensional dimensional contour of the part to be processed, and obtain the first deformation distribution law of the part to be processed; a first correction unit, used to establish a finite element simulation model based on the first deformation distribution law, and perform a first correction on the part to be processed using curved surface molds of different sizes; a second deformation distribution law acquisition unit, used to obtain a second deformation distribution law of the part to be processed after the first correction; and a second correction unit, used to perform a second correction on the part to be processed using a multi-point loading tooling based on the second deformation distribution law, until the deformation amount of the part to be processed meets the preset range requirements.

[0020] By using the above-mentioned annular part deformation correction method and system, the three-dimensional dimensional contour of the part to be processed is first measured to obtain the first deformation distribution law of the part to be processed, and then based on the first deformation distribution law, a finite element simulation model is established, and the first correction is performed on the part to be processed using curved surface molds of different sizes; then the second deformation distribution law of the part to be processed after the first correction is obtained, and based on the second deformation distribution law, a second correction is performed on the part to be processed using a multi-point loading tooling until the deformation amount of the part to be processed meets the preset range requirements, the correction accuracy is high, and high-quality correction of casing-type annular parts can be achieved.

[0021] In order to achieve the above and related purposes, one or more aspects of the present invention include the features that will be described in detail later. The following description and the accompanying drawings describe some exemplary aspects of the present invention in detail. However, these aspects indicate only some of the various ways in which the principles of the present invention can be used. In addition, the present invention is intended to include all these aspects and their equivalents. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] By referring to the following description in conjunction with the accompanying drawings, and with a more comprehensive understanding of the present invention, other objects and results of the present invention will become more apparent and easy to understand. In the accompanying drawings:

[0023] Figure 1 is a flow chart of a method for correcting deformation of an annular part according to an embodiment of the present invention;

[0024] Figure 2-1 A coordinate system diagram of a part to be processed according to an embodiment of the present invention;

[0025] Figure 2-2 is a schematic diagram of the xoy cross-sectional deformation of a part to be processed according to an embodiment of the present invention;

[0026] Figure 3 for Figure 2-2Schematic diagram of the size of the part after correction;

[0027] Figure 4 for Figure 2-2 Schematic diagram of local deformation in area A;

[0028] Figure 5 for Figure 2-2 Schematic diagram of local deformation correction in area A;

[0029] Figure 6 for Figure 2-2 The coordinate expression of the size of area A at different stages;

[0030] Figure 7 A schematic diagram of the evolution of elastic-plastic deformation of a part during calibration according to an embodiment of the present invention;

[0031] Figure 8 A comparison diagram of the ideal size and deformed size of a part according to an embodiment of the present invention;

[0032] Fig. 9 is a distribution regularity diagram of two original deformations along the circumference according to an embodiment of the present invention;

[0033] Fig.10 A deformation curve diagram of a part correction according to an embodiment of the present invention;

[0034] Fig.11 is a deformation distribution diagram of a part after correction according to an embodiment of the present invention;

[0035] Fig.12 A schematic diagram of a multi-point loading fixture simulation model according to an embodiment of the present invention;

[0036] Fig.13 4 is a block diagram of a system for correcting deformation of an annular part according to an embodiment of the present invention.

[0037] The same reference numerals throughout the drawings indicate similar or corresponding features or functions. DETAILED DESCRIPTION

[0038] In the following description, for the purpose of illustration, in order to provide a comprehensive understanding of one or more embodiments, many specific details are set forth. However, it is apparent that these embodiments may also be implemented without these specific details. In other examples, for ease of describing one or more embodiments, known structures and devices are shown in the form of block diagrams.

[0039] In the description of the present invention, it is to be understood that the terms “center”, “longitudinal”, “lateral”, “length”, “width”, “thickness”, “up”, “down”, “front”, “back”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inside”, “outside”, “clockwise”, “counterclockwise”, “axial”, “radial”, “circumferential”, etc., indicating orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0040] To describe the annular part deformation correction method and system of the present invention in detail, specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings.

[0041] Figure 1 The schematic flow of the annular part deformation correction method according to the present invention is shown.

[0042] like Figure 1 As shown, the annular part deformation correction method according to the embodiment of the present invention mainly includes:

[0043] S100: measuring the three-dimensional dimension profile of the part to be processed to obtain a first deformation distribution law of the part to be processed.

[0044] Specifically, in the process of measuring the three-dimensional dimensional contour of the part to be processed and obtaining the first deformation distribution law of the part to be processed, the three-dimensional dimensional contour of the part to be processed can be measured using a three-dimensional coordinate measuring machine to obtain the three-dimensional size of the part to be processed; then, based on the three-dimensional size and the preset ideal size and allowable deviation range, the first deformation distribution law is determined.

[0045] As a specific example, Figure 2-1 and Figure 2-2 The three-dimensional coordinate diagram of the part to be processed and the xoy cross-sectional deformation schematic diagram according to an embodiment of the present invention are respectively shown; Figure 3 Shows Figure 2-2 A schematic diagram of the dimensions of the part after correction.

[0046] like Figure 2-1 , Figure 2-2 and Figure 3 As shown in the figure, the center of the circle is taken as the reference point, and the distance between the deformed part and the center of the circle is expressed as D A (θ) indicates that the ideal part size is R0 and the upper deviation circle radius is R max , the radius of the lower deviation circle is R min , the distance between the part and the center of the circle after correction is D B (θ) represents, then the correction deformation is D A(θ)-D B (θ); If you want to accurately correct the parts, you need to analyze the deformation distribution characteristics of the parts. Figure 2-2 The A area in the figure is analyzed as a local deformation unit. The deformation position can be approximately regarded as a circular arc. The distance between each point of the circular arc and the center of the part is D. A (θ), and then reverse deformation correction is performed. Within the arc range D A (θ)>R max , the minimum correction deformation at each point is D A (θ)-R max , the maximum correction deformation is D A (θ)-R min .according to Figure 3 The deformation characteristics of the part shown in can be divided into N parts. The deformation characteristics of each part can be regarded as arcs of different curvatures. The deformation of the entire part can be corrected by analysis and correction in the same way.

[0047] Among them, Figure 2-2 Take the local deformation of region A in the figure as an example to illustrate. Figure 4 The black solid line is the shape of the deformed part, the gray solid line is the ideal part size shape with a radius of R0, and the dotted line is the allowable deviation range of the part size. When the deformed part size exceeds the part size deviation range, the part needs to be corrected so that the corrected part size is within the deviation range to meet the part size design requirements. Figure 5 Shown are two dimensional shapes with maximum deformation and minimum deformation under deformation correction.

[0048] Further, Figure 6 The coordinate expression of the size of the A area of ​​the part at different stages is shown, such as Figure 6 It can be seen that when the angle is π, the deformation is the largest, and it needs to be corrected so that the allowable deviation range of the part after correction is: -Δε0<part deformation<Δε0, in order to meet the deviation requirements. Therefore, the correction deformation should meet Δε min <Deformation correction amount<Δε max . Since the parts undergo elastic-plastic deformation during the deformation correction process, the greater the correction deformation at the deformation position of the parts, the more severe the plastic deformation will be. Under different correction deformation amounts, the stress generated during correction and the springback deformation of the parts after unloading are different. In order to analyze the deformation law of parts, the relationship between the stress and strain in the correction process and the correction amount, deformation amount and springback amount can be analyzed through the elastic-plastic theory. The correction deformation and springback amount occurring at the correction position of the parts under different correction amounts can also be obtained through finite element simulation or experiments, and then the empirical formula is fitted to establish a quantitative relationship between the two.

[0049] Assuming that the deformation of the part during calibration is pure bending elastic-plastic deformation, Figure 7 (a) is the initial state of the part, assuming that the stress at each position is zero. The radius of curvature of the arc in the deformation area before correction is known to be R A , the radius of curvature of the arc in the deformed area after correction is R B . The schematic diagram of deformation evolution during the correction process is shown in Figure 7 As shown, Q represents the elastic deformation area, and its stress range is 0-σ s , P represents the plastic deformation area, and its stress range is σ s -σ b , the yield strain is ε s . Figure 7 (a) shows the initial state of the part, and then the part is corrected for reverse bending deformation. Figure 7 (b) The deformation of the upper and lower surfaces of the part is the largest, and it will enter the plastic deformation state first, while the middle area is still in the elastic deformation stage. The stress and strain corresponding to the deformation state at this time are as follows: Figure 7 (c) Figure 7 As shown in (d), the radius of curvature of the part after springback deformation is reduced compared to the radius of curvature during bending deformation, but it has not returned to its original state.

[0050] If the part undergoes such uneven elastic-plastic deformation during the correction process, the part will rebound when the external load is removed. The material in the elastic deformation zone Q has a tendency to recover to the initial state of the part, while the zero stress state of the material in the plastic deformation zone P of the part is to rebound to ε r The springback strain is ε sp Therefore, the deformation of the two regions Q and P cannot be coordinated during the springback process. At the beginning of the deformation release, when the materials on the upper and lower surfaces of the part complete the springback deformation, they are already in a zero stress state, while the internal materials are still in a deformed state and have a tendency to continue to deform. At this time, the deformation is further released, the material on the upper surface will be compressed, and the material on the lower surface will be stretched. Assuming that the final strain inside the part is ε B Therefore, the materials at different positions inside the part will produce different degrees of tensile or compressive strain ε RS It cannot be fully recovered and is eventually stored inside the part as internal stress, which forms residual stress σ RS .

[0051] like Figure 7 As shown, the strain ε at different positions of the part during calibration C , the stress σ at different positions during correction C , the strain ε at different positions of the part after correction B, when the material rebounds to the zero stress state, the theoretical rebound strain ε sp =σ C / E, the plastic strain ε produced by the material relative to its initial zero strain state r =ε C -ε sp However, in the actual correction deformation, the material at different positions of the part undergoes non-uniform deformation, and the deformation of the two regions Q and P cannot be coordinated during the springback process, causing the final material to spring back to ε B When the self-equilibrium state is reached, the actual rebound strain is ε' sp =ε C -ε B The residual elastic strain stored in the material is ε RS =ε B -ε r .

[0052] From this, the residual stress introduced by the correction can be calculated:

[0053] σ RS =E×ε RS (1)

[0054] σ RS =E×(ε B -ε r ) (2)

[0055] σ RS =E×(ε B -(ε C -ε sp )) (3)

[0056] σ RS =E×(ε B -(ε C -σ C / E)) (4)

[0057] Among them, ε in the formula B , ε C and σ C It can be calculated from the dimensional changes before and after the part is corrected.

[0058] Assume that the radius corresponding to the neutral layer position of the workpiece before correction is R A0 , whose arc length is L A0 The radius of the part at different positions before correction is R A , the arc length corresponding to this radius position is L A The radius of the part at different positions during calibration is R C , the arc length corresponding to this radius position is L C , the radius corresponding to the neutral layer position is R c0The radius of the part at different positions after correction is R B , the arc length corresponding to this radius position is L B , the radius corresponding to the neutral layer position is R B0 Since the length of the neutral layer remains unchanged at different stages, then:

[0059] L A0 =θ A ×R A0 =θ C ×R C0 =θ B ×R B0 (5)

[0060] Strain ε at different positions of the part during calibration C The distribution law is:

[0061]

[0062] Strain ε at different positions of the positive and negative parts B Distribution pattern:

[0063]

[0064] Among them, θ A is the radian of the microelement before correction, θ C is the arc of the microelement in the correction, θ B is the arc of the microelement after correction. According to the critical strain value of plastic deformation ε s The critical position of the part reaching plastic deformation during bending deformation can be obtained. When the material enters the plastic deformation zone:

[0065] |ε C |≥ε s (8)

[0066] Substituting formula (6) into formula (8), we can obtain:

[0067]

[0068] When calculating the deformation, it is necessary to ensure that the analysis is done at the same position before and after correction, so ΔR = R A -R A0 =R C -R C0 .but:

[0069]

[0070]

[0071]

[0072] It can be concluded that, under certain correction conditions, R A0 and R C0 When constant, the larger ΔR is, the greater the deformation of the material is, and the easier it is to undergo plastic deformation. For a specific material, the stress-strain curve can be found in the material manual. Assume that the functional relationship between stress and strain is:

[0073] σ C =f(ε C ) (13)

[0074] The strain energy density function can be written as:

[0075]

[0076] The total strain energy function of the corrected part can be written as:

[0077]

[0078] From the above analysis, it can be seen that the correction deformation directly affects the magnitude of the residual stress introduced by the correction, and the residual stress directly represents the magnitude of the introduced strain energy. The greater the correction deformation during the correction process, the greater the probability of plastic damage on the surface of the part after correction. The greater the correction deformation, the greater the residual stress introduced, and therefore the greater the strain energy. The greater the strain energy inside an object, the more unstable the current state of the object, and the easier it is to deform. The greater the residual stress, the greater the deformation caused by the release of the residual stress over time, and the less conducive it is to the dimensional stability of the part. Therefore, under the condition of meeting the part size requirements, the correction technology with the minimum correction amount as the optimization target is the safest.

[0079] Specifically, in the first calibration process, the deformation of a simple titanium alloy ring casing is used as an example for calibration analysis. From the material manual, it is known that the yield stress of titanium alloy TC4 is 867MPa and the strength limit is 940MPa. First, the three-dimensional dimension profile of the deformed casing is measured using a three-dimensional coordinate measuring machine to obtain the deformation distribution law of the casing. Figure 8 The figure shows the comparison between the ideal size and the deformed size of the receiver parts. The gray solid is the ideal shape of the part, with an outer radius Router of 114.5mm, an inner radius Rinner of 112.5mm, a wall thickness of 2mm, and a height L of 113mm. During the processing, the part is deformed due to the release of residual stress. The deformation cloud is the shape of the part after deformation. The maximum deformation of the part is 0.100mm, and it is required to be reduced to 0.020mm after correction.

[0080] Depend on Figure 8 It can be seen that the deformation of the part is most severe on the upper end surface, so the deformation of the upper end surface is corrected. The distribution law of the original deformation of the upper end surface of the receiver along the circumference is that the maximum deformation is 0.100mm. Fig. 9 As shown in the distribution pattern of the original deformation of the receiver along the circumference, the deformation of the parts after correction is required to be within 0.020mm, and the positions where the deformation of the parts exceeds 0.02mm need to be reversed. The angle ranges are 0°~39.7°, 51.3°~129.7°, 141.3°~219.7°, 231.3°~309.7°, and 321.3°~360°. Therefore, the positions of the loading points should be concentrated within this angle range during the multi-point loading correction process.

[0081] Next, through finite element simulation, two correction tools, multi-point loading fixture and curved surface mold, are used to correct the deformation of the parts. The multi-point loading correction scheme uses displacement control to perform reverse deformation correction. First, the deformation characteristics of the parts are analyzed to find the position of the maximum deformation point, and the maximum deformation position is reversely deformed. Then, the characteristics of the corrected parts are analyzed to find the position of the maximum deformation point under the current deformation state, and the maximum deformation position is reversely deformed. Repeat the above process and perform corrections repeatedly until the shape and size of the corrected parts meet the design requirements. The curved surface mold also uses displacement control to perform reverse deformation correction on the parts. The upper end face of the curved surface mold is elliptical, and the lower end face is circular. The radial difference between the cross-sectional elliptical size of the curved surface mold and the cross-sectional size of the corresponding position of the casing part is the reverse deformation correction amount.

[0082] S200: Based on the first deformation distribution law, a finite element simulation model is established, and a first correction is performed on the part to be processed using curved surface molds of different sizes.

[0083] Among them, the curved surface mold includes an adaptive inner mold and an outer mold, and the step of performing a first correction on the part to be processed using curved surface molds of different sizes includes: determining the mold correction amount and the shapes and sizes of the inner mold and the outer mold according to the first deformation distribution law; performing a first correction on the part to be processed based on the correction amount and the inner mold and the outer mold, and obtaining the deformation distribution law of the part to be processed after the first correction; adjusting the mold correction amount based on the deformation distribution law of the part to be processed after the first correction, and performing a second first correction based on the adjusted new mold correction amount; and repeating the above steps until the deformation amount of the part to be processed meets the first preset range requirements.

[0084] Specifically, according to Fig. 9As shown, the maximum deformation position is at 0° (360°), 90°, 180° and 270°, and the corresponding deformation amounts are -0.1mm, 0.1mm, -0.1mm and 0.1mm respectively. That is, during correction, the mold curvature radius of the part at the 0° and 180° positions should be smaller than the radius of the part, and the mold should perform compression deformation correction on the part from the inside to the outside. On the contrary, the mold curvature radius at the 90° and 270° positions of the part should be larger than the radius of the part, and the mold should perform deformation correction on the part from the outside to the inside. Therefore, the shape of the curved mold used should have a gradually increasing curvature radius from 0° to 90°, and then gradually decrease from 90° to 180°. The same is true for the change of the mold curvature radius from 180° to 360°. According to the change of the mold curvature radius, the cross-sectional shape of the curved mold is selected as an ellipse, and then a finite element model is established to correct the deformation of the casing.

[0085] The curved mold shape is established so that the upper end surface is elliptical and the lower end surface is circular, and then displacement control is used to perform safety correction on the parts. The outer ellipse size of the upper end surface of the receiver: the major semi-axis a 外 , short semi-axis b 外 , inner ellipse size: major semi-axis a 内 , short semi-axis b 内 . Let the maximum correction amount of the curved surface mold in the X-axis and Y-axis directions be x. During the correction process, the displacement of the outer mold in the X-axis direction is x, and the displacement of the inner mold in the Y-axis direction is x. Then the short semi-axis of the inner diameter of the ellipse on the upper end face of the external correction curved surface mold in the X direction is a 外-x The major semi-axis of the ellipse outer diameter of the upper end surface of the internal correction curved mold in the Y direction is b 内+x In order to prevent the radial spacing between the inner and outer molds at the same position of the casing from being smaller than the casing wall thickness during the correction process, so that the inner and outer surfaces of the casing are completely fitted with the inner and outer correction molds at the same time and extrusion deformation occurs, the long semi-axis of the elliptical inner diameter of the upper end face of the external correction curved mold in the Y direction should be slightly larger than b 外+x The short semi-axis of the elliptical outer diameter of the upper end surface of the internal correction curved mold in the X direction is slightly smaller than a 内-x The circular size of the lower end surface of the curved mold, the inner mold radius should be smaller than the inner radius of the receiver, and the outer mold radius should be larger than the outer radius of the receiver.

[0086] Furthermore, the maximum deformation of the part is obtained by using finite element simulation and using curved molds of different sizes. Function fitting is performed on the relationship between different correction amounts and maximum deformation, and the following is obtained: Fig.10 The corrected deformation curve is shown: Among them, a3 = 1.909 × 10-8, b3 = 10.5, c3 = 8.69 × 10 -3, x represents the correction amount, and y3 represents the deformation amount.

[0087] Depend on Figure 8 It can be seen that the maximum deformation of the receiver is 0.100mm. After correction using the curved mold, the correction amount can be calculated and the initial selection is 4.33mm. A curved mold model is established based on the correction amount, and the shape of the mold on the XY section is also established so that the shape of the upper end face is elliptical and the shape of the lower end face is circular. First, import the corrected curved mold and the part to be corrected into the simulation model, and then adjust the relative position of the mold and the part. The elliptical minor axis direction of the mold in the simulation should correspond to the major axis direction of the part after machining deformation. Only in this way can the part be reversely deformed and extruded during deformation correction, thereby reducing part deformation. When the correction amount is 4.33mm, the deformation of the part is too small.

[0088] Then, after repeated adjustments of the correction amount, it was found that when the correction amount was 4.70 mm, a more ideal correction result could be obtained. The correction deformation of the upper end surface of the receiver at different angles after correction was extracted, and then added to the deformation of the upper end surface of the receiver before correction, the following can be obtained: Fig.11 The deformation distribution after correction is shown. The maximum deformation deviation of the upper end face of the part after the curved mold correction is 0.016mm, which is 84% ​​less than the original deformation of the part. The maximum correction stress during the curved mold correction process when the correction deformation is the largest is 904MPa. After the correction, the maximum correction residual stress and strain position of the part is at the bottom of the receiver, with a maximum correction residual stress value of 219MPa and a maximum correction residual strain value of 0.0048. Compared with the part after multi-point loading correction, the curved mold correction process is completed at one time, and the deformation deviation of the corrected part is smaller, which effectively avoids the stress and strain concentration problem at the loading point position of the part caused by multi-point correction. Moreover, when the correction scheme of the curved mold is adopted, both the correction residual stress after the correction and the maximum correction stress during the correction process are less than the stress results generated by the multi-point loading correction. Therefore, it is safer to adopt the correction scheme of the curved mold.

[0089] S300: Obtaining a second deformation distribution law of the part to be processed after the first correction.

[0090] Among them, after the first correction, if the deformation of the part has met the preset requirements, there is no need to perform a second correction. Otherwise, a rough correction can be performed using a curved mold, and then a local correction can be performed using a multi-point loading tool.

[0091] S400: Based on the second deformation distribution law, a second correction is performed on the part to be processed by using a multi-point loading tooling until the deformation amount of the part to be processed meets the preset range requirement.

[0092] Among them, this step may further include: based on the second deformation distribution law, determining the positions of deformation points of the parts to be processed that are ranked in front of a preset number of deformation amounts; and performing reverse deformation correction on the deformation points one by one based on a multi-point loading tool.

[0093] Furthermore, the step of performing reverse deformation correction on the deformation points one by one based on the multi-point loading tooling includes: using a finite element simulation model to perform function fitting on the correction amount of the deformation point and the corresponding maximum deformation amount to determine a correction deformation curve; based on the correction deformation curve, determining the actual deformation amount of the deformation point; based on the multi-point loading tooling and the actual deformation amount, performing reverse deformation correction on the deformation points one by one.

[0094] The correction deformation curve includes a correction deformation curve 1 when extruding from the outside to the inside, and a correction deformation curve 2 when extruding from the inside to the outside; wherein the expression of the correction deformation curve 1 is:

[0095]

[0096] The expression of the correction deformation curve 2 is:

[0097]

[0098] Wherein, x represents the correction amount, y1 and y2 represent the deformation amounts, a1 and b1 represent the fitting coefficients of the correction deformation curve 1, and a2 and b2 represent the fitting coefficients of the correction deformation curve 2.

[0099] As a specific example, the multi-point loading tooling includes a driving device and a cylindrical pressing head arranged at the end of the driving device; wherein the cylindrical pressing head is an elastic-plastic body.

[0100] According to the deformation distribution law of the parts, in the multi-point loading correction process, the maximum deformation point positions 0° (360°), 90°, 180° and 270° are firstly subjected to reverse deformation correction, such as Fig.12 As shown in the figure, in order to simplify the multi-point loading correction simulation model of the casing, multiple cylindrical clamping heads are used instead of multi-point loading fixtures to perform reverse deformation correction on the deformation position of the casing. The material model of the casing and the clamping head is an elasto-plastic body. In order to reduce the squeeze damage of the clamping head on the surface of the part during the correction process, aluminum alloy 7075 is selected as the correction clamping head material in the simulation. The part is freely meshed using tetrahedral units, and the unit side length is 1mm. The temperature of the part is 20℃, and the room temperature is set to 20℃. Newton-Raphson is selected as the iterative method, and Sparse is selected as the solver. When the relative deformation of the unit is set to 0.7, the model is meshed again to prevent mesh distortion.

[0101] Among them, finite element simulation is used to obtain the maximum correction deformation of the part under different correction amounts, and then the relationship between different correction amounts and maximum deformation is fitted by function, which is the correction deformation curve when extruding from outside to inside: Where a1 = 1.130 × 10 -4 , b1=8.654, x represents the correction amount, y1 represents the deformation amount; the correction deformation curve when extruding from the inside to the outside is: Where a2 = 9.012 × 10 -4 , b2=6.961, x represents the correction amount, and y2 represents the deformation amount.

[0102] In the specific correction process, the four positions of 0°, 90°, 180° and 270° of the casing can be corrected first. Since the maximum deformation of the casing is 0.100mm, the empirical formula 16 can be used to calculate the initial selection of 2.225mm for the correction amount at the two positions of 0° and 180° when extruding from the outside to the inside. Similarly, the empirical formula 17 can be used to solve the correction amount at the two positions of 90° and 270°. 1.984mm. The simulation results show that when the correction amount at the two positions of 0° and 180° is 2.225mm, the deformation of the part is too small, and when the correction amount at the two positions of 90° and 270° is 1.984mm, the deformation of the part is too large. Then, after repeated adjustments to the correction amount, the correction amount at the two positions of 0° and 180° is 2.473mm, and the correction amount at the two positions of 90° and 270° is 1.881mm, and better correction results can be obtained.

[0103] It can be seen that after correction, the deformation of the part at the four positions of 0°, 90°, 180° and 270° is 0.001mm. However, due to the small deformation influence area of ​​the loading point, there is still a large deformation at the upper end surface of the part, and the deformation distribution law after correction is still symmetrical about the XZ and YZ planes. Therefore, in the following analysis, only the deformation distribution law within the range of 0° to 90° is analyzed. Among them, the positions of 15° and 75° are the positions of maximum deformation after correction, and the maximum deformations are 0.081mm and -0.082mm respectively. Then, the 15° and 75° positions will be selected for the second deformation correction. The same as the first correction and debugging process, the initial correction amount is calculated, and then fine-tuned according to the simulation results. It is found that when the correction amount is 2.104mm and 1.815mm, better correction results can be obtained.

[0104] After the second correction, the maximum correction deformation positions of the parts are at 10°, 25°, 65° and 82°, and the deformations are 0.045mm, 0.048mm, -0.049mm and -0.048mm respectively. Then the third deformation correction is performed for these four points. After correction, it is found that most of the deformation of the parts is controlled within 0.020mm, and only the deformation near 0° and 180° exceeds 0.020mm, and the maximum deformation reaches -0.047mm, so the deformation of the parts needs to be further corrected. According to the results of the fourth correction, the deformation of the parts is all controlled within 0.020mm, and the deformation of the upper end face of the receiver is distributed in a wave-like oscillation along the circumferential direction. From the above simulation results, it can be seen that with the increase of loading points, the cross-sectional shape of the corrected parts is closer to a circle.

[0105] Since the maximum deformation deviation of the upper end surface of the part after multi-point correction and curved mold correction meets the size requirements. However, after multi-point correction, there is an obvious stress concentration phenomenon at the loading point position on the part surface, and the maximum corrected residual stress after correction reaches 453MPa. However, there is no stress and strain concentration phenomenon at the extrusion position of the curved mold and the part surface, and the maximum residual stress value after correction is 219MPa. Compared with multi-point loading correction, the residual stress after correction is improved. Strain energy is proportional to residual stress, so the strain energy introduced after curved mold correction is also small. Compared with the multi-point correction scheme, the correction scheme of curved mold is safer.

[0106] Corresponding to the above-mentioned annular part deformation correction method, the present invention also provides an annular part deformation correction system.

[0107] Specifically, Fig.13 FIG. 2 shows a logic block diagram of a ring-shaped part deformation correction system according to an embodiment of the present invention. Fig.13 As shown, the annular part deformation correction system 100 provided by the present invention comprises:

[0108] A first deformation distribution law acquisition unit 101 is used to measure the three-dimensional size profile of the part to be processed and acquire a first deformation distribution law of the part to be processed;

[0109] A first correction unit 102 is used to establish a finite element simulation model based on a first deformation distribution law, and perform a first correction on the part to be processed using curved surface molds of different sizes;

[0110] A second deformation distribution law acquiring unit 103 is used to acquire a second deformation distribution law of the part to be processed after the first correction;

[0111] The second correction unit 104 is used to perform a second correction on the part to be processed by using a multi-point loading tooling based on the second deformation distribution law, until the deformation amount of the part to be processed meets the preset range requirement.

[0112] It should be noted that the embodiments of the above-mentioned annular part deformation correction system can refer to the description in the embodiment of the annular part deformation correction method, which will not be described in detail here.

[0113] As described above, the annular part deformation correction method and system according to the present invention are described by way of example with reference to the accompanying drawings. However, it should be understood by those skilled in the art that various improvements can be made to the annular part deformation correction method and system proposed by the present invention without departing from the content of the present invention. Therefore, the protection scope of the present invention should be determined by the content of the attached claims.

Claims

1. A method for correcting deformation of an annular part, characterized in that: include: Measuring the three-dimensional size profile of the part to be processed to obtain a first deformation distribution law of the part to be processed; Based on the first deformation distribution law, a finite element simulation model is established, and the part to be processed is first corrected using curved surface molds of different sizes; Obtaining a second deformation distribution law of the part to be processed after the first correction; Based on the second deformation distribution law, a second correction is performed on the part to be processed by using a multi-point loading tool until the deformation amount of the part to be processed meets the preset range requirement; The step of measuring the three-dimensional dimension profile of the part to be processed and obtaining the first deformation distribution law of the part to be processed comprises: Measuring the three-dimensional size profile of the part to be processed by using a three-dimensional measuring machine to obtain the three-dimensional size of the part to be processed; Based on the three-dimensional size and the preset ideal size and the allowable deviation range, the first deformation distribution law is determined; the curved surface mold includes an inner mold and an outer mold that are matched, and the step of performing a first correction on the part to be processed using curved surface molds of different sizes includes: Determining a mold correction amount and shapes and sizes of the inner mold and the outer mold according to the first deformation distribution law; Performing a first correction on the part to be processed based on the correction amount and the inner mold and the outer mold, and obtaining a deformation distribution law of the part to be processed after the first correction; Based on the deformation distribution law of the part to be processed after the first correction, the mold correction amount is adjusted, and a second first correction is performed based on the adjusted new mold correction amount; The above steps are executed cyclically until the deformation of the part to be processed meets the first preset range requirement; the step of performing a second correction on the part to be processed by using a multi-point loading tool based on the second deformation distribution law until the deformation of the part to be processed meets the preset range requirement includes: Based on the second deformation distribution law, determining the positions of deformation points of the to-be-processed part whose deformation amounts are ranked first by a preset number; Based on the multi-point loading tool, the deformation points are corrected in reverse deformation one by one; the step of performing reverse deformation correction on the deformation points one by one based on the multi-point loading tool comprises: Using a finite element simulation model, a function fitting is performed on the correction amount of the deformation point and the corresponding maximum deformation amount to determine a correction deformation curve; Based on the corrected deformation curve, determining the actual deformation amount of the deformation point; Based on the multi-point loading tooling and the actual deformation amount, reverse deformation correction is performed on the deformation points one by one.

2. The method for correcting deformation of an annular part according to claim 1, characterized in that: The correction deformation curve includes a correction deformation curve 1 when extruding from the outside to the inside, and a correction deformation curve 2 when extruding from the inside to the outside; wherein, The expression of the correction deformation curve 1 is: The expression of the correction deformation curve 2 is: in, x Indicates the correction amount, y 1 and y 2 represents the deformation amount, a 1 and b 1 represents the fitting coefficient of the correction deformation curve 1, a 2 and b 2 Represents the fitting coefficient of the correction deformation curve 2.

3. The method for correcting deformation of an annular part according to claim 1, characterized in that: The multi-point loading tooling comprises a driving device and a cylindrical pressing head arranged at the end of the driving device.

4. The method for correcting deformation of an annular part according to claim 3, characterized in that: The cylindrical pressing head is an elastic-plastic body.

5. The method for correcting deformation of an annular part according to claim 1, characterized in that: The parts to be processed include casing ring parts.

6. A ring-shaped part deformation correction system, characterized in that: Used to implement the annular part deformation correction method according to any one of claims 1 to 5, the system comprises: A first deformation distribution law acquisition unit is used to measure the three-dimensional size profile of the part to be processed and acquire a first deformation distribution law of the part to be processed; A first correction unit, used to establish a finite element simulation model based on the first deformation distribution law, and perform a first correction on the part to be processed by using curved surface molds of different sizes; A second deformation distribution law acquisition unit, used for acquiring a second deformation distribution law of the part to be processed after the first correction; The second correction unit is used to perform a second correction on the part to be processed by using a multi-point loading tool based on the second deformation distribution law, until the deformation amount of the part to be processed meets the preset range requirement.