Wafer reconstruction method for chips with bumps and bare dies without bumps
By forming metal columns on the carrier plate and welding chips, the problem of difficult to control the ball removal process in the prior art is solved, and higher packaging reliability and yield are achieved.
Patent Information
- Application Number
- CN202210645550.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-06-09
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2042-06-09
AI Technical Summary
In the existing wafer reconstruction process, the ball removal process with bump chips is difficult to control, which can easily cause solder ball residue or overetching, affecting the packaging reliability and yield.
Using a method of reconstructing a disk with a bump chip and a bare core without bump core, a metal column is formed by sputtering a seed layer on the carrier plate and coating a photoresist layer, and the chip is welded by underfill, and then Resin encapsulation and carrier plate peeling were performed, and finally the wafer was obtained by debonding.
It effectively reduces the uncertainty of the ball removal process, improves the reliability of packaging, and improves the yield and yield of the product.
Smart Images

Figure CN115020248B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of integrated circuit packaging, in particular to a wafer reconstruction method for a chip with bumps and a bare core without bumps. Background Art
[0002] 2.5D and 3D integration processes are currently the main development direction of integrated circuits. They are valued by the industry for their excellent high-frequency characteristics, ability to reduce transmission delays, reduce noise, small package size, and high thermal expansion reliability, and have a wide range of applications.
[0003] The existing wafer reconstruction process mainly reconstructs bare chips without bumps. If the incoming chip has bumps, the bumps need to be removed before the wafer reconstruction process can be carried out. The current existing ball removal process uses a wet process to etch away the bumps with an etching solution. The process window of the ball removal process is difficult to control, which can easily cause solder ball residue or pad damage caused by over-etching. In addition, most chip surfaces are covered with a PI passivation layer that is not easy to remove, which has a great impact on subsequent processes. Using such a process, there are many high risks in the process and it will affect the reliability of the entire circuit. Summary of the invention
[0004] The purpose of the present invention is to overcome the deficiencies in the prior art and provide a wafer reconstruction method for chips with bumps and bare cores without bumps, which can improve the reliability of packaging and increase the product yield and yield.
[0005] According to the technical solution provided by the present invention, the wafer reconstruction method of the chip with bumps and the bare die without bumps comprises the following steps:
[0006] S1, providing a first carrier, sputtering a seed layer on the front side of the first carrier, and coating a photoresist layer on the seed layer;
[0007] S2, patterning the photoresist layer to form deep holes and cutting path marks;
[0008] S3, filling metal pillars in the deep holes and cutting paths patterned in the photoresist layer, wherein the front surface of the metal pillars is lower than the front surface of the photoresist layer;
[0009] S4, removing the photoresist layer and the seed layer outside the metal pillar to expose a portion of the front surface of the first carrier;
[0010] S5, laminating the front surface of the first carrier board with a film material to form a laminating layer, wherein the laminating layer covers the metal column;
[0011] S6, thinning the front side of the laminated layer until the metal pillar is exposed;
[0012] S7, soldering the bumped chip to the metal pillar using an underfill and an underfill method;
[0013] S8, encapsulating the surface on which the chip with bumps is welded with a first resin material;
[0014] S9, peeling off the first carrier plate;
[0015] S10, cutting into chip units along the cutting path;
[0016] S11, providing a second carrier and a bare die without bumps, firstly pasting a bonding film on the front side of the second carrier, and then pasting the chip unit and the bare die without bumps onto the bonding film through their back sides;
[0017] S12, encapsulating the chip unit and the bare core without bumps with a second resin material;
[0018] S13, removing the second carrier plate by debonding the bonding film, and obtaining wafers with bumped chips and bare cores without bumps.
[0019] Preferably, the thickness of the first carrier is less than or equal to 1 mm, and the material of the first carrier is silicon, glass or resin; the thickness of the seed layer is greater than or equal to 100 nm, and the material of the seed layer is Ni, Cu, Au or Cr; the thickness of the photoresist layer is greater than or equal to 65 μm, and the material of the photoresist layer is a polymer material including polyimide, vinyl resin, epoxy resin or polyparaxylene.
[0020] Preferably, the height of the metal column is greater than or equal to 50 μm, and the material of the metal column is Ni, Cu, Au or Cr.
[0021] Preferably, the lamination layer is a CBF film or an ABF film.
[0022] Preferably, in step S7, the bottom filling method is a capillary filling method, a preformed bottom filling method or a non-flow bottom filling method.
[0023] Preferably, the first resin material is made of a solid molding compound or a liquid molding compound containing resin and SiO2 particles.
[0024] Preferably, the thickness of the second carrier is less than or equal to 1 mm, and the material of the second carrier is silicon, glass or resin.
[0025] Preferably, the second resin material is made of a solid molding compound or a liquid molding compound containing resin and SiO2 particles.
[0026] In step S13, the debonding method is high temperature debonding, laser debonding or chemical corrosion debonding.
[0027] The present invention can effectively reduce the process problems caused by the uncertainty of the deballing process and the influence of the PI passivation layer on the subsequent processes, greatly improve the reliability of the package, and improve the product yield and yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 Schematic diagram of a first carrier coated with a photoresist layer and a sputtering layer.
[0029] Figure 2 It is a schematic diagram of the photoresist layer on the surface of the first carrier after patterning.
[0030] Figure 3 It is a schematic diagram after the surface of the first carrier is filled with metal.
[0031] Figure 4 It is a schematic diagram of the first carrier board after removing the redundant photoresist layer and seed layer from the surface.
[0032] Figure 5 It is a schematic diagram of the surface of the first carrier after lamination.
[0033] Figure 6 This is a schematic diagram of the first carrier board after the surface is thinned to reveal the metal pillars.
[0034] Figure 7 It is a schematic diagram of a first carrier board after the chip with bumps is welded on the surface and the bottom is filled.
[0035] Figure 8 It is a schematic diagram of the chip encapsulation on the surface of the first carrier.
[0036] Fig. 9 It is a schematic diagram after the first carrier is peeled off.
[0037] Fig.10 It is a schematic diagram of the chip unit after the bumped chip is divided into individual chips after encapsulation.
[0038] Fig.11 It is a schematic diagram of mounting a chip unit and a bare die without bumps on a second carrier board with a bonding film.
[0039] Fig.12 It is a schematic diagram of the chip unit and the bare core without bumps after encapsulation.
[0040] Fig.13 It is a schematic diagram of a chip unit and a bare die reconstructed wafer without bumps. DETAILED DESCRIPTION
[0041] The following is a further detailed description of a wafer reconstruction method for a chip with bumps and a bare die without bumps proposed by the present invention in conjunction with the accompanying drawings and specific embodiments. The features of the present invention will become clearer according to the following description and claims. It should be noted that the accompanying drawings are all in a very simplified form and are not in precise proportions, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.
[0042] A wafer reconstruction method for a chip with bumps and a bare die without bumps, the method comprising the following steps:
[0043] S1. Provide a first carrier 101, sputter a seed layer 102 on the front side of the first carrier 101, and coat a photoresist layer 103 on the seed layer 102; the first carrier 101 can be made of silicon, glass, and resin materials including wafer-level and board-level materials, the thickness of the first carrier 101 is 0.5-1.0 mm, the seed layer 102 can be made of materials including Ni, Cu, Au, and Cr, the thickness of the seed layer 102 is greater than or equal to 100 nm, the thickness of the photoresist layer 103 is greater than or equal to 65 μm, and the material of the photoresist layer 103 is a polymer material including polyimide, vinyl resin, epoxy resin, or polyparaxylene, such as Figure 1 As shown;
[0044] S2, patterning the photoresist layer 103 to form deep holes and cutting road marks, such as Figure 2 As shown;
[0045] S3, filling metal pillars 104 in the patterned deep holes and cutting paths of the photoresist layer 103, the front side of the metal pillars 104 is lower than the front side of the photoresist layer 103, the metal pillars 104 can be made of materials including Ni, Cu, Au, Cr, and the height of the metal pillars 104 is greater than or equal to 50 μm, such as Figure 3 As shown;
[0046] S4, removing the photoresist layer 103 and the seed layer 102 outside the metal pillar 104 to expose a portion of the front surface of the first carrier 101, such as Figure 4 As shown;
[0047] S5, laminating the front surface of the first carrier 101 with a film material to form a laminating layer 105, wherein the laminating layer 105 covers the metal column 104, and the laminating layer 105 can be a resin polymer material including a CBF film and an ABF film, such as Figure 5 As shown;
[0048] S6, thinning the front surface of the laminate layer 105 until the metal pillar 104 is exposed, such as Figure 6 As shown;
[0049] S7, the chip with bumps 106 is welded to the metal pillar 104 by using the bottom filler 107 and the bottom filling method, and the bottom filling method may include a capillary filling method, a preformed bottom filling method and a non-flow bottom filling method, such as Figure 7 As shown;
[0050] S8, encapsulating the surface of the chip 106 with bumps welded thereon with a first resin material 108, wherein the resin material 108 may be a solid molding material or a liquid molding material containing resin and SiO2 particles, such as Figure 8 As shown;
[0051] S9, peeling off the first carrier plate 101, as shown in FIG. Fig. 9 As shown;
[0052] S10, cutting into chip units 109 along the cutting path, such as Fig.10 As shown;
[0053] S11, providing a second carrier 110 and a bare core 112 without bumps, firstly pasting a bonding film 111 on the front side of the second carrier 110, and then pasting the chip unit 109 and the bare core 112 without bumps on the bonding film 111 through their front sides, wherein the second carrier 110 may be made of a material including silicon, glass and resin material, and the thickness of the second carrier 110 is 0.5-1.0 mm, such as Fig.11 As shown;
[0054] S12, encapsulating the chip unit 109 and the bare core 112 without bumps with a second resin material 113, wherein the second resin material 113 may be a solid molding material or a liquid molding material containing resin and SiO2 particles, such as Fig.12 As shown;
[0055] S13, removing the second carrier 110 by debonding the bonding film 111, and obtaining a wafer with a bump chip and a wafer with a bare die without a bump, and the debonding method is high temperature debonding, laser debonding or chemical corrosion debonding, such as Fig.13 shown.
Claims
1. A wafer reconstruction method for a chip with bumps and a bare die without bumps, characterized in that The method comprises the following steps: S1, providing a first carrier (101), sputtering a seed layer (102) on the front surface of the first carrier (101), and coating a photoresist layer (103) on the seed layer (102); S2, patterning the photoresist layer (103) to form deep holes and cutting path marks; S3, filling metal pillars (104) in the patterned deep holes and cutting paths of the photoresist layer (103), wherein the front surface of the metal pillars (104) is lower than the front surface of the photoresist layer (103); S4, removing the photoresist layer (103) and the seed layer (102) outside the metal pillar (104), exposing a portion of the front surface of the first carrier board (101); S5, laminating the front surface of the first carrier board (101) with a film material to form a laminating layer (105), wherein the laminating layer (105) covers the metal column (104); S6, thinning the front surface of the laminated layer (105) until the metal pillar (104) is exposed; S7, using an underfill material (107) to weld the bumped chip (106) to the metal pillar (104) by underfilling; S8, encapsulating the surface on which the chip with bumps (106) is welded with a first resin material (108); S9, peeling off the first carrier plate (101); S10, cutting into chip units along the cutting path (109); S11, providing a second carrier (110) and a bare core without bumps (112), firstly laminating a bonding film (111) on the front side of the second carrier (110), and then laminating the chip unit (109) and the bare core without bumps (112) onto the bonding film (111) through their front sides; S12, encapsulating the chip unit (109) and the bare core (112) without bumps with a second resin material (113); S13, removing the second carrier board (110) by debonding the bonding film (111), thereby obtaining wafers of chips with bumps and bare chips without bumps.
2. The wafer reconstruction method of the chip with bumps and the bare die without bumps as claimed in claim 1, characterized in that: The thickness of the first carrier plate (101) is less than or equal to 1 mm, and the material of the first carrier plate (101) is silicon, glass or resin; the thickness of the seed layer (102) is greater than or equal to 100 nm, and the material of the seed layer (102) is Ni, Cu, Au or Cr; the thickness of the photoresist layer (103) is greater than or equal to 65 μm, and the material of the photoresist layer (103) is a polymer material including polyimide, vinyl resin, epoxy resin or polyparaxylene.
3. The wafer reconstruction method of the chip with bumps and the bare die without bumps as claimed in claim 1, characterized in that: The height of the metal column (104) is greater than or equal to 50 μm, and the material of the metal column (104) is Ni, Cu, Au or Cr.
4. The wafer reconstruction method of the chip with bumps and the bare die without bumps as claimed in claim 1, characterized in that: The lamination layer (105) is a CBF film or an ABF film.
5. The wafer reconstruction method of the chip with bumps and the bare die without bumps as claimed in claim 1, characterized in that: In step S7, the bottom filling method is a capillary filling method, a preformed bottom filling method or a no-flow bottom filling method.
6. The wafer reconstruction method of the chip with bumps and the bare die without bumps as claimed in claim 1, characterized in that: The material of the first resin material (108) is a solid molding material or a liquid molding material containing resin and SiO2 particles.
7. The wafer reconstruction method of the chip with bumps and the bare die without bumps as claimed in claim 1, characterized in that: The thickness of the second carrier plate (110) is less than or equal to 1 mm, and the material of the second carrier plate (110) is silicon, glass or resin.
8. The wafer reconstruction method of the chip with bumps and the bare die without bumps as claimed in claim 1, characterized in that: The material of the second resin material (113) is a solid molding material or a liquid molding material containing resin and SiO2 particles.
9. The wafer reconstruction method of the chip with bumps and the bare die without bumps as claimed in claim 1, characterized in that: In step S13, the debonding method is high temperature debonding, laser debonding or chemical corrosion debonding.
Citation Information
Patent Citations
Resin type wafer-level fan-out integrated packaging method and structure
CN110911291A
Method for preparing multi-size micro convex points on multiple chips
CN114093779A