A stretching die capable of rapid demoulding and a stretching method thereof

By designing a quick demoulding structure and automated drive system in the drawing mold, the problem of difficult demoulding of the existing drawing mold is solved, production efficiency and product quality are improved, and the cost of replacing parts is reduced.

CN115055573BActive Publication Date: 2024-10-18ZHEJIANG DAOHE MASCH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202210799194.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-06
Publication Date
2024-10-18
Estimated Expiration
2042-07-06

AI Technical Summary

Technical Problem

During the production process of the existing drawing mold, the product tightly fits the punch, causing difficulty in demoulding and reducing production efficiency.

Method used

A drawing die that can be quickly demoulded is designed. It adopts the structure of base, punch core and concave die. Through the cooperation of blank holder and stamping knife, the plate can be fixed, punched and stretched, and driven to reset. Automatic demoulding; the stamping knife and stamping plate are detachable, and designs such as inclined sections and sliders improve cutting force and movement stability, reducing replacement costs.

Benefits of technology

It achieves rapid automatic demoulding of products, improves production efficiency, ensures product quality, and reduces the cost of replacing parts.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115055573B_ABST
    Figure CN115055573B_ABST
Patent Text Reader

Abstract

The present invention relates to a stretching die capable of rapid demoulding and a stretching method thereof, which comprises a base, a male mold core and a female mold arranged in sequence from bottom to top, wherein the male mold core is arranged on one side of the base, a blank holder ring for placing a sheet is arranged on the outer side of the male mold core, the blank holder ring is sleeved on the outer side of the male mold core, and the blank holder ring can be slidably matched with the male mold core, a concave cavity matching the male mold core is formed on the side of the female mold facing the male mold core, the concave cavity and the male mold core form a stretching cavity, a punching knife is arranged in the concave cavity, and punching holes matching the punching knife are opened through the male mold core and the base; in the initial state, the male mold core does not pass over the blank holder ring, and the male mold core and the female mold are driven to close the mold to stretch the sheet. The stretching die of the present invention can realize punching and stretching of the sheet, and can realize rapid demoulding of the stretched product, thereby improving production efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of stretching dies, in particular to a stretching die capable of rapid demoulding and a stretching method thereof. Background Art

[0002] Stretching is an important forming method for sheet metal. In conventional stretching dies, the characteristics are that the die is in the upper die part and the punch is fixed on the lower die base. The current stretching dies produce products that fit tightly on the punch and are difficult to demould, resulting in low production efficiency.

[0003] Therefore, how to achieve stretching of the product and rapid demoulding of the product is a technical problem that needs to be solved urgently in this field. Summary of the invention

[0004] In order to solve the above technical problems, the present invention provides a stretching die capable of rapid demoulding and a stretching method thereof.

[0005] In the first aspect, the present invention provides a stretching die capable of rapid demoulding, which adopts the following technical solution:

[0006] A stretching die capable of rapid demoulding comprises a base, a punch core and a die which are arranged in sequence from bottom to top, the punch core being arranged on one side of the base, a blank holder ring for placing a sheet material being arranged on the outer side of the punch core, the blank holder ring being sleeved on the outer side of the punch core, and the blank holder ring being slidably matched with the punch core, a concave cavity matched with the punch core being formed on the side of the die facing the punch core, the concave cavity and the punch core forming a stretching cavity, a punching knife being arranged in the concave cavity, a punching hole matched with the punching knife being penetrated through the punch core and the base; in an initial state, the punch core does not pass over the blank holder ring, the punch core and the die are driven to close the mold to stretch the sheet material.

[0007] By adopting the above-mentioned technical scheme, after the blank holder and the die are fixed to the sheet, the punch core and the die are driven to close the mold, the sheet is punched and stretched, and the punching waste automatically falls from under the punching hole. Afterwards, the die and the punch core are driven to reset, the product abuts against the blank holder, and the product is automatically demoulded, thereby improving the production efficiency of the product.

[0008] A further technical solution of the present invention is that the punching knife is provided with an inclined cutting surface for cutting the plate.

[0009] By adopting the above technical solution, the top of the inclined cut surface is in contact with the plate in advance, applying a larger cutting force to the plate, thereby facilitating cutting of the plate.

[0010] A further technical solution of the present invention is that the punching knife is detachably arranged in the die through bolts.

[0011] By adopting the above technical solution, it is easy to replace the punching knife, ensure the quality of product stretching, and reduce replacement costs.

[0012] A further technical solution of the present invention is that a groove is opened on the punch core, a stamping plate is arranged on the punch core and is located in the groove, the stamping knife can pass through the stamping plate, the stamping plate is detachably arranged on the punch core by a countersunk bolt, and the side of the stamping plate away from the groove is coplanar with the surface of the punch core.

[0013] By adopting the above technical solution, it is easy to replace the stamping plate on the punch core, thereby ensuring the quality of product stretching and reducing replacement costs.

[0014] A further technical solution of the present invention is that a sliding block is provided on the punch core, and a sliding groove which is slidably matched with the sliding block is provided on the pressure ring.

[0015] By adopting the above technical solution, the sliding cooperation between the punch core and the pressure ring improves the stability of the punch core movement and ensures the quality of product stretching.

[0016] A further technical solution of the present invention is that a first weight-reducing groove is provided on one side of the male mold core that is in contact with the base.

[0017] By adopting the above technical solution, the first weight-reducing groove reduces the weight of the punch core, thereby reducing the cost of the punch core and improving the heat dissipation performance of the punch core.

[0018] A further technical solution of the present invention is that a second weight-reducing groove is provided on the outside of the die.

[0019] By adopting the above technical solution, the second weight-reducing groove reduces the weight of the die, thereby reducing the cost of the die and improving the heat dissipation performance of the die.

[0020] In a second aspect, the present invention provides a stretching method for a stretching die capable of rapid demoulding, which adopts the following technical solution:

[0021] A stretching method for a stretching die capable of rapid demoulding comprises the following steps:

[0022] Step 1: first place the drawing die on the hydraulic press, adjust the position of the push rod, adjust the pressure parameters of the hydraulic press, then lift the punch core to be flush with the top of the blank holder, and place the sheet on the blank holder;

[0023] Step 2: The die is driven to push downward, and the die presses the sheet onto the blank holder to fix the position of the sheet;

[0024] Step 3: The hydraulic press drives the punch core to move upward and starts stretching. When the punch core and the die are closed, the sheet metal stretching is completed.

[0025] Step 4: After the stretching is completed, the concave mold returns, the punch core returns, the product is automatically demoulded, and after the product is taken out, the next stretching is carried out.

[0026] A further technical solution of the present invention is that the hydraulic press controls the flow of hydraulic oil by adjusting the valve switch to adjust the pressure to adapt to the speed of movement of the plate during stretching.

[0027] A further technical solution of the present invention is that the plate is a cold-rolled plate, and a plastic film is laid on the cold-rolled plate.

[0028] In summary, the present invention includes the following beneficial technical effects:

[0029] 1. After the blank holder and the die are fixed to the sheet, the punch core is driven to close the die, the sheet is punched and stretched, and the punching waste automatically falls from the punching hole. After that, the die and the punch core are driven to reset, the product abuts against the blank holder, and the product is automatically demoulded, which improves the production efficiency of the product;

[0030] 2. The top of the inclined cut surface on the punching knife is in contact with the plate in advance, exerting a greater cutting force on the plate, making it easier to cut the plate; the punching knife and punching plate can be replaced to ensure the quality of product stretching and reduce replacement costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 is a schematic structural diagram of an embodiment of the present invention;

[0032] Figure 2 is a cross-sectional schematic diagram of an embodiment of the present invention;

[0033] Figure 3 Schematic diagram of the structure of the punching knife and the die in the embodiment of the present invention;

[0034] Figure 4 is a schematic diagram of the structure of a punching knife in an embodiment of the present invention;

[0035] Figure 5 Schematic diagram of the structure of the punch plate and the punch core in the embodiment of the present invention;

[0036] Figure 6 2 is a schematic structural diagram of a male mold core in an embodiment of the present invention;

[0037] Figure 7 2 is a schematic diagram of the structure of the blank holder in an embodiment of the present invention;

[0038] Figure 8 It is a structural schematic diagram of a base in an embodiment of the present invention.

[0039] Explanation of the reference numerals in the accompanying drawings: 1. Base; 2. Punch core; 21. Groove; 22. Slider; 23. First weight-reducing groove; 3. Die; 31. Concave cavity; 32. Second weight-reducing groove; 4. Pressure ring; 41. Slide groove; 5. Punching knife; 51. Inclined section; 6. Punching hole; 7. Punching plate. DETAILED DESCRIPTION

[0040] The following is combined with Figure 1-8 The present invention is further described in detail.

[0041] The embodiment of the invention discloses a drawing die capable of rapid demoulding and a drawing method thereof.

[0042] like Figure 1 and Figure 2 As shown, the drawing die that can be quickly demolded includes a base 1, a punch core 2, a die 3 and a pressure ring 4.

[0043] Among them, the base 1, the male mold core 2 and the female mold 3 are arranged in sequence from bottom to top, the base 1 is fixed to the bottom surface of the male mold core 2, and the bottom surface of the female mold 3 is formed with a concave cavity 31 adapted to the male mold core 2, and a stretching cavity of the stretched product is formed when the male mold core 2 and the female mold 3 are molded together. A punching knife 5 is installed in the concave cavity 31 of the female mold 3, and a punching hole 6 adapted to the punching knife 5 is opened through the male mold core 2 and the base 1 from top to bottom.

[0044] The blank holder 4 is sleeved on the outer side of the male mold core 2, and the blank holder 4 can slide and cooperate with the male mold core 2. The position of the blank holder 4 is fixed, and the sheet is placed on the blank holder 4, and the bottom periphery of the female mold 3 coincides with the top periphery of the blank holder 4.

[0045] In the initial state, the punch core 2 does not go over the blank holder 4, the sheet is placed on the top surface of the blank holder 4, and the die 3 is controlled by the drive to move downward to press the sheet onto the blank holder 4. After that, the punch core 2 is controlled by the drive to move upward, the punch core 2 and the die 3 are closed to punch and stretch the sheet, and the punching waste automatically falls from the punching hole 6. Finally, the die 3 and the punch core 2 are reset by the drive, the product abuts against the blank holder 4, and the product is automatically demolded to improve the production efficiency of the product.

[0046] like Figure 1 and Figure 3 As shown, in the present invention, the die 3 is in the shape of a rectangular parallelepiped as a whole, and a second weight-reducing groove 32 is provided on the surface of the die 3, and the second weight-reducing groove 32 is located on the peripheral side of the die 3 and on the side of the die 3 away from the cavity 31. The second weight-reducing groove 32 reduces the weight of the die 3, reduces the cost of the die 3, and improves the heat dissipation performance of the die 3.

[0047] In addition, the punching knife 5 will be worn during operation. When the punching knife 5 is greatly worn, the quality of the stretched product will be unqualified. At this time, in order to ensure the quality of the stretched product, the punching knife 5 needs to be replaced.

[0048] In order to reduce the cost of replacing the punching knife 5, the punching knife 5 is separately arranged from the die 3, and two through holes are opened in the middle of the punching knife 5. Bolts pass through the through holes and cooperate with the threads of the die 3 to detachably fix the punching knife 5 in the concave cavity 31 of the die 3.

[0049] like Figure 4 As shown, in addition, the punching knife 5 is integrally formed with an inclined cutting surface 51 for cutting the plate, and the top of the inclined cutting surface 51 is in contact with the plate in advance, exerting a greater cutting force on the plate, making it easier to cut the plate.

[0050] In the present invention, the punching blade 5 is cylindrical in shape, and the inclined section 51 is arranged to be inclined to one side along the middle of the punching blade 5. Of course, the punching blade 5 can also be in the shape of a cube, a hexagonal prism, an octagonal prism, or the like.

[0051] like Figure 5 As shown, the punching knife 5 cooperates with the punching hole 6 on the punch core 2. During the stretching process of the plate, the plate is punched. The punching process will cause certain damage to the punching part on the surface of the punch core 2, affecting the quality of the stretched product. At this time, in order to ensure the quality of the stretched product, the punch core 2 needs to be replaced, which causes a great waste.

[0052] In order to avoid this situation, a groove 21 coaxial with the punching hole 6 is provided on the top of the punch core 2, and a punching plate 7 located in the groove 21 is installed on the top of the punch core 2. The punching plate 7 is annular, and the punching knife 5 is adapted to the punching plate 7, and the punching knife 5 can pass through the punching plate 7. A countersunk hole is provided on the punching plate 7, and a countersunk bolt passes through the countersunk hole and is threadedly matched with the punch core 2, so that the punching plate 7 is detachably fixed to the punch core 2, and the side of the punching plate 7 away from the groove 21 is coplanar with the surface of the punch core 2. By replacing the punching plate 7, the replacement cost is reduced and the quality of the stretched product is guaranteed.

[0053] like Figure 6 As shown, in addition, a first weight-reducing groove 23 is provided on one side of the male mold core 2 that is in contact with the base 1 . The first weight-reducing groove 23 reduces the weight of the male mold core 2 , thereby reducing the cost of the male mold core 2 and improving the heat dissipation performance of the male mold core 2 .

[0054] like Figure 6 and Figure 7As shown, a slider 22 is integrally formed on one side of the male mold core 2, and there are two sliders 22, which are located at both ends of one side of the male mold core 2. A slide groove 41 is provided on the inner side of the blank holder 4 to slide with the slider 22. The sliding cooperation between the slider 22 and the slide groove 41 improves the stability of the movement of the male mold core 2 and ensures the quality of product stretching.

[0055] like Figure 8 As shown, in the present invention, the base 1 includes a rectangular plate, which is detachably fixed to the punch core 2, a rectangular frame plate is welded to the side of the rectangular plate facing away from the punch core 2, and four ear plates are welded at the four corners of the rectangular frame plate.

[0056] The embodiment of the present invention also discloses a stretching method of a stretching die capable of rapid demoulding.

[0057] A stretching method for a stretching die capable of rapid demoulding comprises the following steps:

[0058] Step 1: first place the stretching die on the hydraulic press, adjust the position of the push rod, adjust the pressure parameters of the hydraulic press, then lift the punch core 2 to be flush with the top of the blank holder 4, and place the sheet on the blank holder 4.

[0059] Step 2: The die 3 is pushed downward by the drive of the oil cylinder, so that the die 3 presses the plate onto the blank holder 4 to fix the position of the plate;

[0060] Step three, the hydraulic press drives the punch core 2 to move upward and starts stretching. When the punch core 2 and the die 3 are closed until the punch core 2 and the die 3 are in contact with each other to ensure that the sheet material in the stretching cavity formed by the punch core 2 and the die 3 does not flow, the stretching is completed.

[0061] Step 4: After the stretching is completed, the concave mold 3 returns, the convex mold core 2 returns, the product is automatically demoulded, and after the product is taken out, the next stretching is carried out.

[0062] In the present invention, the hydraulic press controls the flow of hydraulic oil by adjusting the valve switch to adjust the pressure to adjust the speed of material movement during stretching so as to effectively control the depth. The upward speed of the hydraulic press is adjusted so that the sheet material can be fed evenly according to the shape of the punch during stretching.

[0063] In the present invention, the plate is a cold-rolled plate, and a plastic film is laid on the cold-rolled plate.

[0064] The implementation principle of the embodiment of the present invention is:

[0065] In the present invention, after the pressure ring 4 and the die 3 fix the plate, the punch core 2 and the die 3 are driven to close the mold, the plate is punched and stretched, and the punching waste automatically falls from under the punching hole. Afterwards, the die 3 and the punch core 2 are driven to reset, the product abuts on the pressure ring 4, and the product is automatically demoulded, thereby improving the production efficiency of the product; the top of the inclined cut surface 51 on the punching knife 5 is in contact with the plate in advance, and a larger cutting force is applied to the plate, which is convenient for cutting the plate; the punching knife 5 and the punching plate 7 are replaceable to ensure the quality of product stretching and reduce replacement costs.

[0066] The above are all preferred embodiments of the present invention, and are not intended to limit the protection scope of the present invention. Therefore, any equivalent changes made based on the structure, shape, and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A stretching die that can be quickly demoulded. Features: The invention comprises a base (1), a male mold core (2) and a female mold (3) which are arranged in sequence from bottom to top, wherein the male mold core (2) is arranged on one side of the base (1), and a blank holder (4) for placing a plate is arranged on the outer side of the male mold core (2), and the blank holder (4) is sleeved on the outer side of the male mold core (2), and the blank holder (4) can be slidably matched with the male mold core (2), and the female mold (3) is formed with a side facing the male mold core (2) to be in contact with the male mold core. The core (2) is provided with a concave cavity (31) adapted to the die, the concave cavity (31) and the convex core (2) form a stretching cavity, a punching knife (5) is arranged in the concave cavity (31), and a punching hole (6) adapted to the punching knife (5) is provided through the convex core (2) and the base (1); in an initial state, the convex core (2) does not pass over the blank holder (4), the convex core (2) and the concave die (3) are driven to close the mold, and the sheet is stretched; The punching knife (5) is provided with an inclined cutting surface (51) for cutting the plate; The punching knife (5) is detachably arranged in the die (3) by means of bolts; The punch core (2) is provided with a groove (21), and the punch core (2) is provided with a stamping plate (7) located in the groove (21); the stamping knife (5) can pass through the stamping plate (7); the stamping plate (7) is detachably arranged on the punch core (2) by means of a countersunk bolt, and the side of the stamping plate (7) away from the groove (21) is coplanar with the surface of the punch core (2).

2. A drawing die capable of rapid demoulding according to claim 1, Features: The male mold core (2) is provided with a slider (22), and the pressure ring (4) is provided with a slide groove (41) that is slidably matched with the slider (22).

3. A drawing die capable of rapid demoulding according to claim 1, Features: A first weight-reducing groove (23) is provided on one side of the male mold core (2) that abuts against the base (1).

4. A drawing die capable of rapid demoulding according to claim 1, Features: A second weight-reducing groove (32) is provided on the outside of the concave mold (3).

5. A stretching method for a stretching die capable of rapid demoulding according to claim 1, Features: The following steps are included: Step 1: first place the drawing die on the hydraulic press, adjust the position of the push rod, adjust the pressure parameters of the hydraulic press, then lift the punch core (2) to be flush with the top of the blank holder (4), and place the sheet on the blank holder (4); Step 2: The die (3) is driven to be ejected downward, and the die (3) presses the plate onto the blank holder (4) to fix the position of the plate; Step 3: The hydraulic press drives the punch core (2) to move upwards and starts stretching. When the punch core (2) and the die (3) are closed, the sheet stretching is completed. Step 4: After the stretching is completed, the concave mold (3) returns, the convex mold core (2) returns, the product is automatically demoulded, and after the product is taken out, the next stretching is carried out.

6. According to the stretching method of a stretching die capable of rapid demoulding as described in claim 5, the hydraulic press controls the flow of hydraulic oil by adjusting the valve switch to adjust the pressure to adapt to the speed of movement of the plate during stretching.

7. A stretching method for a stretching die capable of rapid demoulding according to claim 5, Features: The plate is a cold-rolled plate, on which a plastic film is laid.

Citation Information

Patent Citations

  • Stretching method for preventing stretching piece from being broken

    CN113560414A

  • A mould that is used for shaping to plough a machine walking wheel sideboard a little

    CN207463946U