AI Technical Summary
然而,传统构筑异质界面采用外延生长方法,构建过程中,需要精确控制衬底的晶体面和外延界面,此过程工序繁杂,产量低,阻碍了其在工业生产中的发展
[0019]1、此过渡金属异质结构电催化产氢催化剂制备方法通过简单的熔融和高温分解的方法可控的构筑异质结构材料,此材料在碱性条件下,表现出优异的电催化产氢性能。
Smart Images

Figure CN115058736B_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of preparation of electrocatalytic hydrogen production catalysts, and in particular relates to a method for preparing a transition metal heterostructure electrocatalytic hydrogen production catalyst. Background Art
[0002] Energy and environment are the most important issues involved in the sustainable development of human society. 80% of the world's energy demand comes from fossil fuels, which will eventually lead to the depletion of fossil fuels, and their use will also lead to serious environmental pollution. The gradual shift from fossil fuels to sustainable development and pollution-free non-fossil energy is an inevitable trend of development. Hydrogen is one of the ideal clean energy sources and an important chemical raw material, which has received widespread attention from countries around the world. Hydrogen production by water electrolysis is an important means to achieve industrial and cheap production of hydrogen. Water electrolysis includes two reaction processes: hydrogen evolution reaction (HER) and oxygen evolution reaction (OER). The development of cheap, efficient and stable electrocatalysts is an important guarantee for the electrolysis of water to move towards more extensive industrial applications of hydrogen production, and it is also a goal that the majority of scientific researchers need to overcome. Although the electrocatalytic activity of precious metal electrocatalysts Pt, IrOx, and RuOx is very high, their poor stability and high cost hinder their practical application in industrial production. Many efficient HER catalysts (including alloy materials, transition metal borides, carbides, nitrides, oxides, phosphides, sulfides and single-atom catalysts) have been developed. Although a large number of HER electrocatalysts have been reported, these catalysts still have problems with poor activity and stability, and there is still a certain gap with commercial Pt / C catalysts. Therefore, for future large-scale production, low-cost, efficient and durable electrocatalysts based on non-precious metals that are abundant on the earth must be developed.
[0003] The work reported so far shows that interface engineering has become one of the most effective methods to improve electrocatalytic activity, selectivity and stability. However, the traditional construction of heterogeneous interfaces uses epitaxial growth methods. During the construction process, the crystal surface of the substrate and the epitaxial interface need to be precisely controlled. This process is complicated and has low yield, which hinders its development in industrial production. Therefore, it is still a big challenge to construct heterogeneous structure electrocatalysts with rich interfaces by means of interface engineering. To this end, the present invention proposes a method for preparing a transition metal heterostructure electrocatalytic hydrogen production catalyst. Summary of the invention
[0004] In order to solve the problems existing in the prior art, the present invention provides a method for preparing a transition metal heterostructure electrocatalytic hydrogen production catalyst. The method for preparing a transition metal heterostructure electrocatalytic hydrogen production catalyst is reasonably designed, and a heterostructure material can be controllably constructed by a simple melting and high-temperature decomposition method. This material exhibits excellent electrocatalytic hydrogen production performance under alkaline conditions. The method is simple, easy to operate, and can be used for large-scale industrial production. The prepared catalyst has high activity, good stability, excellent electrocatalytic performance, and high economic benefits.
[0005] In order to achieve the above object, the present invention is implemented by the following technical scheme: a method for preparing a transition metal heterostructure electrocatalytic hydrogen production catalyst, comprising the following steps:
[0006] Step 1: Preparation of graphene oxide by Hummer method;
[0007] Step 2: Mixing, drying and melting urea, ethylenediamine and transition metal salt;
[0008] Step 3: The melt-cooled mixture is subjected to high-temperature decomposition to prepare a heterogeneous structure.
[0009] Furthermore, the step 1 is specifically as follows:
[0010] ①: Add a certain amount of 98% H2SO4 to a 1000ml beaker, then add graphite, then add a certain amount of KMnO4, stir in an ice salt bath, and then stir at room temperature;
[0011] ②: After freeze-drying the product, disperse it in water at a certain concentration, sonicate it, and freeze-dry it to obtain graphene oxide;
[0012] ③: Take 100-300 mg-GO and put it into 50 mL of distilled water, and disperse it by ultrasonic for 1-3 hours.
[0013] Furthermore, the step 2 is specifically as follows:
[0014] ①: Add 2-10g urea and 0.5-1.5ml ethylenediamine to the solution obtained in step 1, stir for 20min, mix well, and adjust the pH of the solution;
[0015] ②: Then add 200-800 mg of ammonium tungstate and 100-200 mg of ammonium molybdate, stir for 30 minutes, and then put it in a 100°C oven to dry;
[0016] ③: After drying, place it in a 170℃ oil bath. After the sample is completely melted, stir it for five minutes and take it out to cool.
[0017] Furthermore, the step three is as follows: placing in a tubular furnace under a nitrogen atmosphere, first raising the temperature to 500°C at 2°C / min, maintaining at 500°C for 10 min, then raising the temperature to 800°C at 5°C / min, maintaining at 800°C for 120 min, and finally cooling naturally.
[0018] Beneficial effects of the present invention:
[0019] 1. The preparation method of this transition metal heterostructure electrocatalytic hydrogen production catalyst can controllably construct a heterostructure material through a simple melting and high-temperature decomposition method. This material exhibits excellent electrocatalytic hydrogen production performance under alkaline conditions.
[0020] 2. The preparation method of this transition metal heterostructure electrocatalytic hydrogen production catalyst is simple in process, easy to operate, and can be carried out on a large scale in industrial production. The prepared catalyst has high activity, good stability, excellent electrocatalytic performance, and high economic benefits. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 SEM of three-dimensional porous graphene for the preparation of a transition metal heterostructure electrocatalytic hydrogen production catalyst Figure 1 ;
[0022] Figure 2 SEM of three-dimensional porous graphene for the preparation of a transition metal heterostructure electrocatalytic hydrogen production catalyst Figure 2 . DETAILED DESCRIPTION
[0023] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.
[0024] See also Figure 1 to Figure 2 The present invention provides a technical solution: a method for preparing a transition metal heterostructure electrocatalytic hydrogen production catalyst, comprising the following steps:
[0025] Step 1: Add a certain amount of 98% H2SO4 to a 1000ml beaker, then add graphite, add a certain amount of KMnO4, stir in an ice salt bath, and then stir at room temperature;
[0026] After freeze-drying the product, it is dispersed in water at a certain concentration, sonicated, and freeze-dried to obtain graphene oxide;
[0027] 100 mg GO was placed in 50 mL of distilled water and ultrasonically dispersed for 3 h;
[0028] Step 2: Then add 10g urea and 1ml ethylenediamine and stir for 20min to mix well and adjust the pH of the solution;
[0029] Then add 800 mg of ammonium tungstate and 200 mg of ammonium molybdate, stir for 30 min, and then dry in an oven at 100°C;
[0030] After drying, put it in a 170℃ oil bath. After the sample is completely melted, stir it for five minutes and take it out to cool.
[0031] Step 3: Then put it into a tubular furnace under a nitrogen atmosphere, first increase the temperature to 500°C at 2°C / min, maintain it at 500°C for 10 minutes, then increase the temperature to 800°C at 5°C / min, maintain it at 800°C for 120 minutes, and finally cool it naturally.
[0032] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. It is obvious to those skilled in the art that the present invention is not limited to the details of the above exemplary embodiments, and the present invention can be implemented in other specific forms without departing from the spirit or basic features of the present invention. Therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive. The scope of the present invention is defined by the attached claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims are included in the present invention. Any figure mark in the claims should not be regarded as limiting the claims involved.
[0033] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
Claims
1. A method for preparing a transition metal heterostructure electrocatalytic hydrogen production catalyst, characterized in that: The following steps are involved: Step 1: Preparation of graphene oxide by Hummer method; Step 2: Mixing, drying and melting urea, ethylenediamine and transition metal salt; Step 3: The melted and cooled mixture is subjected to high temperature decomposition to prepare a heterogeneous structure; The step 1 is specifically as follows: ①: Add a certain amount of 98% H2SO4 to a 1000ml beaker, then add graphite, add a certain amount of KMnO4, stir in an ice salt bath, and then stir at room temperature; ②: After freeze-drying the product, disperse it in water at a certain concentration, sonicate it, and freeze-dry it to obtain graphene oxide; ③: Take 100-300 mg-GO and put it into 50 mL of distilled water, and disperse it by ultrasonic for 1-3 hours; The step 2 is specifically as follows: ①: Add 2-10g urea and 0.5-1.5ml ethylenediamine to the solution obtained in step 1, stir for 20min, mix well, and adjust the pH of the solution; ②: Then add 200-800 mg of ammonium tungstate and 100-200 mg of ammonium molybdate, stir for 30 minutes, and then put it in a 100°C oven to dry; ③: After drying, place it in a 170℃ oil bath. After the sample is completely melted, stir it for five minutes and take it out to cool.