A demulsifier with corrosion inhibition performance and its synthesis method
Through the polymerization reaction of imidazole cyclopolyoxypropylene polyoxyethylene polyether with propylene oxide and ethylene oxide, a demulsifier with corrosion inhibition properties is prepared, which solves the problem of single performance and insufficient anti-corrosion effect of crude oil demulsifiers in the existing technology. It solves the best problem and achieves rapid demulsification and efficient anti-corrosion effects.
Patent Information
- Application Number
- CN202210613408.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-05-23
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-05-23
AI Technical Summary
When faced with crude oil emulsions with complex composition and high salinity, existing crude oil demulsifiers have single performance, are difficult to effectively prevent equipment corrosion and scaling, and have insufficient bactericidal and corrosion inhibition properties.
Develop an imidazole cyclic polyoxypropylene polyoxyethylene polyether, and prepare a demulsifier with corrosion inhibition properties through polymerization reaction with propylene oxide and ethylene oxide, combined with the imidazoline structure to enhance the protective effect on the metal surface. And it is well compounded with alcohols and other bactericides and scale inhibitors.
It achieves rapid demulsification and dehydration, improves the separation efficiency and water quality of crude oil emulsion, and forms a protective film on the metal surface through the imidazole ring structure, which significantly enhances the anti-corrosion performance of the equipment.
Smart Images

Figure FDA0004987348800000011 
Figure FDA0004987348800000012 
Figure FDA0004987348800000013
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of crude oil demulsification, and particularly relates to a demulsifier with corrosion inhibition performance, and further discloses a synthesis method thereof. Background Art
[0002] With the continuous deepening of oil production, enhanced oil recovery methods are becoming more and more widely used. The composition of crude oil produced fluids is also becoming increasingly complex. The increase in water and inorganic salts in crude oil emulsions makes the emulsions more stable and increases the difficulty of crude oil demulsification. If crude oil in this state is collected and refined without treatment, it is easy to cause equipment corrosion, scaling, and tower impact during the crude oil refining process, resulting in danger and economic losses. Currently, the main methods for crude oil demulsification include: electrical demulsification, gravity sedimentation, ultrasonic demulsification, centrifugal demulsification, membrane demulsification, microwave demulsification, biological demulsification, and chemical demulsification. Among them, chemical demulsification is the most commonly used crude oil demulsification method. It mainly adds demulsifiers to the crude oil emulsion to change the properties of the oil-water interface, reduce the interfacial film strength, and turn the emulsion from stable to unstable, ultimately achieving the effect of oil-water separation.
[0003] Demulsifiers are surfactants that separate the oil and water in crude oil emulsions. They do this by displacing the emulsion's stabilizing membrane, disrupting it and achieving oil-water separation, ensuring the water content of the crude oil meets specified requirements for export. Currently, there are numerous types of demulsifiers, which can be categorized by surfactant type: cationic, anionic, and nonionic. Cationic demulsifiers, primarily quaternary ammonium salts, form positively charged ions when dissolved in water. These demulsifiers are generally effective against common thin oils and are less effective against heavy oils. Anionic demulsifiers, primarily carboxylates, sulfonates, and sulfates, form negatively charged ions when dissolved in water. These demulsifiers are significantly affected by salinity. Nonionic demulsifiers, which have neither positive nor negative charge when dissolved in water, primarily include phenolic resin polyoxypropylene polyoxyethylene ethers, polyol polyoxypropylene polyoxyethylene ethers, and organic amine polyoxypropylene polyoxyethylene ethers. These demulsifiers are currently the most universal, most resistant to interference, and most widely used.
[0004] In recent years, demulsifiers used in oilfield applications have mostly been formulated, primarily focusing on demulsifier performance. Other secondary properties, such as bactericidal and corrosion-inhibiting properties, are still met through compounding. However, the agents typically used to achieve these properties are ionic, which, when combined with demulsifiers, can have a significant impact on the final demulsification performance. Therefore, developing a multi-performance demulsifier has significant implications for its application. Summary of the Invention
[0005] Therefore, the technical problem to be solved by the present invention is to provide an imidazole ring polyoxypropylene polyoxyethylene polyether, an intermediate for synthesizing the imidazole ring polyoxypropylene polyoxyethylene polyether and a synthesis method;
[0006] The second technical problem to be solved by the present invention is to provide a demulsifier with corrosion inhibition performance. The demulsifier has a new structure, which gives the demulsifier certain corrosion inhibition performance, enhances the protection of pipelines and storage tanks, and overcomes the problem of single performance of demulsifier products in the prior art.
[0007] In order to solve the above technical problems, the present invention provides an imidazole ring polyoxypropylene polyoxyethylene polyether having a structure shown in the following formula (I):
[0008]
[0009] Wherein, x is an integer from 0 to 2;
[0010] R1 is selected from substituted or unsubstituted C2-C 20 Saturated fatty chain, substituted or unsubstituted monounsaturated fatty chain, substituted or unsubstituted polyunsaturated fatty chain, or a mixture of at least two of the above fatty chains;
[0011] R2 is a polyoxypropylene polyoxyethylene segment having the structure shown in the following formula (II):
[0012]
[0013] Among them, m=30-44, n=14-24.
[0014] Optionally, the R1 is selected from C 16 H 32 、C 16 H 33 、C 17 H 34 、C 17 H 35 、C 18 H 36 or C 18 H 37 One or more mixed chain structures.
[0015] The present invention also discloses an intermediate for preparing the imidazole polyoxypropylene polyoxyethylene polyether, wherein the intermediate has a structure shown in the following formula (M):
[0016]
[0017] Wherein, x is an integer from 0 to 2;
[0018] R1 is selected from substituted or unsubstituted C2-C 20Saturated fatty chain, substituted or unsubstituted monounsaturated fatty chain, substituted or unsubstituted polyunsaturated fatty chain, or a mixed chain of at least two of the above fatty chains.
[0019] The present invention also discloses a method for preparing the intermediate, comprising the steps of slowly adding an organic amine to a mixed solution containing an organic acid and a water-carrying agent and carrying out a heat-insulating reaction, and further comprising the steps of heating under reflux for dehydration and vacuum removal of the water-carrying agent to obtain the desired intermediate.
[0020] Specifically, the preparation method of the intermediate is:
[0021] The organic amine includes at least one of ethylenediamine, diethylenetriamine, triethylenetetramine or tetraethylenepentamine, preferably tetraethylenepentamine;
[0022] The organic acid is selected from at least one of oleic acid, linoleic acid, palmitic acid, arachidic acid, linolenic acid or stearic acid, preferably oleic acid;
[0023] The water-carrying agent includes at least one of toluene, xylene, trimethylbenzene, 120# solvent oil, 150# solvent oil or 200# solvent oil.
[0024] Specifically, the preparation method of the intermediate is:
[0025] The molar ratio of the organic acid to the organic amine is 1:0.5-2, preferably 1 mol:0.8-1.2 mol;
[0026] The amount of the water-carrying agent used accounts for 20-90 wt% of the total amount of the reaction substrate, and the preferred amount is 40 wt%.
[0027] The present invention also discloses a method for preparing the imidazole cyclopolyoxypropylene polyoxyethylene polyether, comprising the steps of polymerizing the intermediate with propylene oxide and ethylene oxide;
[0028] The molar ratio of the intermediate to the propylene oxide and ethylene oxide is 1:20-200:20-240, and the preferred molar ratio is 1:60-90:30-50.
[0029] The invention also discloses the use of the imidazole ring polyoxypropylene polyoxyethylene polyether in preparing a demulsifier with corrosion inhibition performance.
[0030] The invention also discloses a demulsifier with corrosion inhibition performance, comprising the imidazole polyoxypropylene polyoxyethylene polyether.
[0031] Specifically, the demulsifier further includes a solvent;
[0032] The solvent includes at least one of methanol, ethanol or water.
[0033] The invention also discloses the application of the demulsifier with corrosion inhibition performance in demulsifying crude oil in oil fields.
[0034] The imidazole ring polyoxypropylene polyoxyethylene polyether of the present invention has an imidazole ring as its main structure while retaining four active hydrogen atoms that can continue to react with propylene oxide and ethylene oxide to generate a multi-branched polyether structure containing an imidazoline structure. This demulsifier incorporates an imidazoline structure while maintaining a multi-branched structure. The multi-branched structure ensures the demulsifier's demulsification performance, enabling demulsification and dehydration of crude oil with high dehydration speed and high-quality dewatered water. Furthermore, the adsorption of nitrogen atoms on the imidazole ring structure imparts the demulsifier with certain corrosion inhibition properties, allowing it to form a protective film on metal surfaces to prevent corrosion from crude oil emulsions.
[0035] The demulsifier with corrosion inhibition performance of the present invention has good compounding performance and can be compounded and dissolved with alcohols and / or water to form a clear and transparent solution. It also has good compatibility with products such as imidazoline quaternary ammonium salts, quaternary ammonium salt bactericides, and polymer scale inhibitors, and can be compounded arbitrarily according to formulation requirements.
[0036] The preparation method of the demulsifier with corrosion inhibition performance of the present invention uses organic acid and organic amine as main raw materials, undergoes amidation reaction and cyclization reaction in a water-carrying agent to obtain an intermediate containing an imidazoline structure, and then undergoes a common alkoxylation reaction with propylene oxide and ethylene oxide. The entire reaction process is simple and reliable, has low requirements on equipment, and is easy to control product quality without the occurrence of phenomena such as explosion and gelation.
[0037] In the preparation method of the demulsifier with corrosion inhibition performance of the present invention, oleic acid is preferably used as the organic acid, and tetraethylenepentamine is used as the organic amine. Oleic acid has a carbon chain length of 18 carbon atoms, which acts as a hydrophobic agent, facilitates film formation on the metal surface, and enhances the protective effect. Tetraethylenepentamine itself has a multi-branched structure and has multiple groups that can be alkoxylated. The multi-branched structure enhances the diffusion of the demulsifier in the crude oil emulsion, accelerates the coalescence speed of water droplets and the separation efficiency, and improves the dehydration speed and the quality of the dehydrated water. DETAILED DESCRIPTION
[0038] In the following examples of the present invention, if specific experimental steps or conditions are not specified, the procedures or conditions of conventional experimental steps described in the literature in the field can be followed. The reagents or instruments used, if the manufacturer is not specified, are all conventional reagents that can be obtained commercially.
[0039] Example 1
[0040] The imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment has the structural formula shown below:
[0041]
[0042] Among them, m=30, n=14.
[0043] The preparation method of the imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment comprises the following steps:
[0044] (1) At room temperature, 315 kg of 120# solvent oil and 282 kg of oleic acid were added to the reactor, and the temperature was raised to 100°C and stirred thoroughly until the state was uniform; 189 kg of tetraethylene pentamine was slowly added dropwise at 100°C, and the addition time was controlled to be 60 min. After the addition was completed, the reaction was kept at 100°C for 30 min, and then the temperature was slowly raised to reflux for dehydration, with a gradient of 10°C. When no water was removed from the receiver, the temperature was raised to the next stage, and finally the temperature was raised to 200°C-210°C, and the reaction was kept at this temperature for 2 h until no water was removed, and then the vacuum was slowly opened and the solvent was removed under vacuum, and the temperature was lowered to 70°C to discharge the material to obtain the intermediate M1;
[0045] (2) Take 100 kg of the above intermediate M1 and put it into a high-temperature and high-pressure reactor, heat it to 125 ° C, vacuum treat it for 30 minutes, then slowly introduce 1600 kg of propylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it to 120 ° C-125 ° C, continue to slowly introduce 560 kg of ethylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the system pressure drops to -0.1 MPa, cool it and discharge it, and the desired demulsifier dry agent is obtained, which is recorded as M-PE1.
[0046] Example 2
[0047] The imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment has the structural formula shown below:
[0048]
[0049] Among them, m=30, n=24.
[0050] The preparation method of the imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment comprises the following steps:
[0051] (1) At room temperature, 315 kg of 150# solvent oil and 282 kg of oleic acid were added to the reactor, and the temperature was raised to 100°C and stirred until the state was uniform; at 100°C, 189 kg of tetraethylene pentamine was slowly added dropwise, and the addition time was controlled to be 60 min. After the addition was completed, the reaction was kept at 100°C for 30 min, and then the temperature was slowly raised to reflux for dehydration, with a gradient of 10°C. When no water was removed from the receiver, the temperature was raised to the next stage, and finally the temperature was raised to 200°C-210°C. The reaction was kept at this temperature for 2 h until no water was removed, and then the vacuum was slowly opened and the solvent was removed under vacuum. The temperature was lowered to 70°C, and the material was discharged to obtain the intermediate M2;
[0052] (2) Take 100 kg of intermediate M2 and put it into a high-temperature and high-pressure reactor, heat it to 125 ° C, vacuum treat it for 30 minutes, then slowly introduce 1600 kg of propylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it to 120 ° C-125 ° C, continue to slowly introduce 960 kg of ethylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it down and discharge the materials, and the desired demulsifier dry agent is obtained, which is recorded as M-PE2.
[0053] Example 3
[0054] The imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment has the structural formula shown below:
[0055]
[0056] Among them, m=44, n=14.
[0057] The preparation method of the imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment comprises the following steps:
[0058] (1) Add 315 kg of 200# solvent oil and 282 kg of oleic acid to the reactor at room temperature, heat to 100°C and stir until the state is uniform; slowly add 189 kg of tetraethylene pentamine dropwise at 100°C, control the dropwise addition time to 60 min, keep the temperature at 100°C for 30 min after the dropwise addition is completed, then slowly heat and reflux for dehydration, with a gradient of 10°C. When no water is removed from the receiver, start heating to the next stage, finally heat to 200°C-210°C, keep the temperature for 2 h until no water is removed, then slowly open the vacuum, vacuum desolventize until the solvent is completely removed, cool to 70°C, and discharge the material to obtain intermediate M3;
[0059] (2) Take 100 kg of initiator M3 and put it into a high-temperature and high-pressure reactor, heat it to 125 ° C, vacuum treat it for 30 minutes, then slowly introduce 2350 kg of propylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it to 120 ° C-125 ° C, continue to slowly introduce 560 kg of ethylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it and discharge it to obtain a demulsifier dry agent, which is recorded as M-PE3.
[0060] Example 4
[0061] The imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment has the structural formula shown below:
[0062]
[0063] Among them, m=44, n=24.
[0064] The preparation method of the imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment comprises the following steps:
[0065] (1) Add 315 kg of 120# solvent oil and 282 kg of oleic acid to the reactor at room temperature, heat to 100°C and stir until the state is uniform; slowly add 189 kg of tetraethylene pentamine dropwise at 100°C, control the dropwise addition time to 60 min, keep the temperature at 100°C for 30 min after the dropwise addition is completed, then slowly heat and reflux for dehydration, with a gradient of 10°C. When no water is removed from the receiver, start heating to the next stage, finally heat to 200°C-210°C, keep the temperature for 2 h until no water is removed, then slowly open the vacuum, vacuum desolventize until the solvent is completely removed, cool to 70°C, and discharge the material to obtain intermediate M4;
[0066] (2) Take 100 kg of initiator M4 and put it into a high-temperature and high-pressure reactor, heat it to 125 ° C, vacuum treat it for 30 minutes, then slowly introduce 2350 kg of propylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it to 120 ° C-125 ° C, continue to slowly introduce 960 kg of ethylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it and discharge it to obtain a demulsifier dry agent, which is recorded as M-PE4.
[0067] Example 5
[0068] The imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment has the structural formula shown below:
[0069]
[0070] Among them, m=38, n=20.
[0071] The preparation method of the imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment comprises the following steps:
[0072] (1) Add 315 kg of xylene and 282 kg of oleic acid to the reactor at room temperature, heat to 100 ° C and stir until the state is uniform. Slowly add 189 kg of tetraethylene pentamine dropwise at 100 ° C, and control the dropwise addition time to 60 minutes. After the dropwise addition is completed, keep the temperature at 100 ° C for 30 minutes, then slowly increase the temperature and reflux for dehydration, with a gradient of 10 ° C. When no water is released from the receiver, start to increase the temperature to the next stage, and finally increase the temperature to 200 ° C - 210 ° C, keep the temperature for 2 hours until no water is released, then slowly open the vacuum, vacuum desolventize until the solvent is completely removed, cool to 70 ° C and discharge to obtain intermediate M5;
[0073] (2) Take 100 kg of intermediate M5 and put it into a high-temperature and high-pressure reactor, heat it to 125 ° C, vacuum treat it for 30 minutes, then slowly introduce 2030 kg of propylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it to 120 ° C-125 ° C, continue to slowly introduce 800 kg of ethylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it and discharge it to obtain a demulsifier dry agent, which is recorded as M-PE5.
[0074] Example 6
[0075] The imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment has the structural formula shown below:
[0076]
[0077] Among them, m=38, n=20.
[0078] The preparation method of the imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment comprises the following steps:
[0079] (1) Add 315 kg of xylene and 282 kg of oleic acid to the reactor at room temperature, heat to 100 ° C and stir until the state is uniform. Slowly add 146 kg of triethylenetetramine dropwise at 100 ° C, and control the dropwise addition time to 60 minutes. After the dropwise addition is completed, keep the temperature at 100 ° C for 30 minutes, then slowly increase the temperature and reflux for dehydration, with a gradient of 10 ° C. When no water is released from the receiver, start heating to the next stage, and finally increase the temperature to 200 ° C - 210 ° C, keep the temperature for 2 hours until no water is released, then slowly open the vacuum, vacuum desolventize until the solvent is completely removed, cool to 70 ° C and discharge to obtain intermediate M6;
[0080] (2) Take 100 kg of intermediate M6 and put it into a high-temperature and high-pressure reactor, heat it to 125 ° C, vacuum treat it for 30 minutes, then slowly introduce 1690 kg of propylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it to 120 ° C-125 ° C, continue to slowly introduce 670 kg of ethylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it and discharge it to obtain a demulsifier dry agent, which is recorded as M-PE6.
[0081] Example 7
[0082] The imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment has the structural formula shown below:
[0083]
[0084] Among them, m=38, n=20.
[0085] The preparation method of the imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment comprises the following steps:
[0086] (1) Add 315 kg of xylene and 282 kg of oleic acid to the reactor at room temperature, heat to 100 ° C and stir until the state is uniform. Slowly add 103 kg of diethylenetriamine dropwise at 100 ° C, and control the dropwise addition time to 60 minutes. After the dropwise addition is completed, keep the temperature at 100 ° C for 30 minutes, then slowly increase the temperature and reflux for dehydration, with a gradient of 10 ° C. When no water is released from the receiver, start heating to the next stage, and finally increase the temperature to 200 ° C - 210 ° C, keep the temperature for 2 hours until no water is released, then slowly open the vacuum, vacuum desolventize until the solvent is completely removed, cool to 70 ° C and discharge to obtain intermediate M7;
[0087] (2) Take 100 kg of intermediate M7 and put it into a high-temperature and high-pressure reactor, heat it to 125 ° C, vacuum treat it for 30 minutes, then slowly introduce 1260 kg of propylene oxide. After the feeding is completed, heat it to 130 ° C, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it to 120 ° C-125 ° C, continue to slowly introduce 500 kg of ethylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it and discharge it to obtain a demulsifier dry agent, which is recorded as M-PE7.
[0088] Example 8
[0089] The imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment has the structural formula shown below:
[0090]
[0091] Among them, m=38, n=20.
[0092] The preparation method of the imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment comprises the following steps:
[0093] (1) Add 315 kg of 150# solvent oil and 282 kg of oleic acid to the reactor at room temperature, heat to 100°C and stir until the state is uniform. Slowly add 189 kg of tetraethylene pentamine dropwise at 100°C, and control the dropwise addition time to 60 minutes. After the dropwise addition is completed, keep the temperature at 100°C for 30 minutes, then slowly heat up and reflux for dehydration, with a gradient of 10°C. When no water is removed from the receiver, start heating to the next stage, and finally heat up to 200°C-210°C, keep the temperature for 2 hours until no water is removed, then slowly open the vacuum, vacuum desolventize until the solvent is completely removed, cool to 70°C and discharge to obtain intermediate M8;
[0094] (2) Take 100 kg of intermediate M8 and put it into a high-temperature and high-pressure reactor, heat it to 125 ° C, vacuum treat it for 30 minutes, then slowly introduce 2030 kg of propylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it to 120 ° C-125 ° C, continue to slowly introduce 800 kg of ethylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it and discharge it to obtain a demulsifier dry agent, recorded as M-PE8.
[0095] Example 9
[0096] The imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment has the structural formula shown below:
[0097]
[0098] Among them, m=38, n=20.
[0099] The preparation method of the imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment comprises the following steps:
[0100] (1) Add 315 kg of 150# solvent oil and 282 kg of oleic acid to the reactor at room temperature, heat to 100°C and stir until the state is uniform. Slowly add 146 kg of triethylenetetramine dropwise at 100°C, and control the dropwise addition time to 60 minutes. After the dropwise addition is completed, keep the temperature at 100°C for 30 minutes, then slowly heat up and reflux for dehydration, with a gradient of 10°C. When no water is removed from the receiver, start heating to the next stage, and finally heat up to 200°C-210°C, keep the temperature for 2 hours until no water is removed, then slowly open the vacuum, vacuum desolventize until the solvent is completely removed, cool to 70°C and discharge to obtain intermediate M9;
[0101] (2) Take 100 kg of intermediate M9 and put it into a high-temperature and high-pressure reactor, heat it to 125 ° C, vacuum treat it for 30 minutes, then slowly introduce 1690 kg of propylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it to 120 ° C-125 ° C, continue to slowly introduce 670 kg of ethylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it and discharge it to obtain a demulsifier dry agent, which is recorded as M-PE9.
[0102] Example 10
[0103] The imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment has the structural formula shown below:
[0104]
[0105] Among them, m=38, n=20.
[0106] The preparation method of the imidazole polyoxypropylene polyoxyethylene polyether demulsifier described in this embodiment comprises the following steps:
[0107] (1) Add 315 kg of 150# solvent oil and 282 kg of oleic acid to the reactor at room temperature, heat to 100°C and stir until the state is uniform. Slowly add 103 kg of diethylenetriamine dropwise at 100°C, and control the dropwise addition time to 60 minutes. After the dropwise addition is completed, keep the temperature at 100°C for 30 minutes, then slowly heat up and reflux for dehydration, with a gradient of 10°C. When no water is removed from the receiver, start heating to the next stage, and finally heat up to 200°C-210°C, keep the temperature for 2 hours until no water is removed, then slowly open the vacuum, vacuum desolventize until the solvent is completely removed, cool to 70°C and discharge to obtain intermediate M10;
[0108] (2) Take 100 kg of intermediate M10 and put it into a high-temperature and high-pressure reactor, heat it to 125 ° C, vacuum treat it for 30 minutes, then slowly introduce 1260 kg of propylene oxide. After the feeding is completed, heat it to 130 ° C, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it to 120 ° C-125 ° C, continue to slowly introduce 500 kg of ethylene oxide, heat it to 130 ° C after the feeding is completed, keep it warm for 2 hours until the pressure drops to -0.1 MPa, cool it and discharge it to obtain a demulsifier dry agent, which is recorded as M-PE10.
[0109] Comparative Example 1
[0110] This comparative example scheme follows the water-soluble nonionic imidazoline corrosion inhibitor scheme disclosed in Chinese patent document CN103320797B, using imidazoline as an initiator and copolymerizing with ethylene oxide, propylene oxide, and butylene oxide to obtain a water-soluble imidazoline corrosion inhibitor. However, the polyether product synthesized in this scheme is only used as a corrosion inhibitor and does not have demulsification properties. In addition, this scheme uses butylene oxide, which is relatively expensive and highly toxic, and the application of butylene oxide in China has not been fully developed, making it more dangerous.
[0111] Experimental example
[0112] 1. Demulsification experiment
[0113] Experimental object: crude oil emulsion from Changqing Oilfield (water content: 28%, wax content: approximately 12%, viscosity: 50 mPa·s at 50°C, freezing point: approximately 20°C).
[0114] Preparation of demulsifier solution: Take 200 g of the demulsifier dry agent M-PE prepared in each group of examples, add 100 kg of methanol and 100 g of water in sequence, mix well, and obtain a series of demulsifier solutions.
[0115] Experimental method: Referring to the national standard SY / T5281-2018, the bottle test method was used to test the demulsification effect of each group of demulsifiers on the above crude oil emulsion.
[0116] The dosage was 100 ppm except for the blank group, in which no demulsifier solution was added and the emulsion was broken naturally.
[0117] The test temperature was 50°C and the test time was 90 min. The water output at 15 min, 30 min, 60 min and 90 min was recorded and the dehydration rate was calculated.
[0118] For the cleanliness of the water phase, level one means: the extracted water is clear, transparent or milky white; level two means: the extracted water is relatively clear, light yellow; level three means: the extracted water is relatively turbid, yellow or brown; level four means: the extracted water is turbid, dark brown or black.
[0119] The test results are shown in Table 1 below.
[0120] Table 1 Demulsification effect test results of demulsifier
[0121]
[0122] As can be seen from the data in the above table, the demulsifier of the structure of the present invention has good demulsification performance, among which the performance of the imidazole ring polyoxypropylene polyoxyethylene polyether defined in Example 5 and Example 8 is the best; by comparing the data of the schemes in Example 1 and Example 2, it is found that an increase in the ethylene oxide content in the polymer can improve the demulsification efficiency of the product, which is reflected in a fast dehydration speed and a high final dehydration rate; and from a comparison of Example 3 and Example 4, it is found that a reduction in the propylene oxide content can also improve the demulsification performance of the product; comparing Examples 5, 6, and 7 with Examples 8, 9, and 10, it is found that the solvent used in the initiator synthesis stage has no effect on the effect of the final product.
[0123] In summary, the demulsifier of the structure of the present invention has good demulsification performance, and the ratio of propylene oxide to ethylene oxide in Examples 5 and 8 is the best ratio for treating the crude oil emulsion, and the demulsification performance is better.
[0124] 2. Corrosion inhibition experiment
[0125] Experimental object: wastewater from Changqing Oilfield.
[0126] Preparation of demulsifier solution: Take 200 g of the demulsifier dry agent M-PE prepared in each group of examples, add 100 kg of methanol and 100 g of water in sequence, mix well, and obtain a series of demulsifier solutions.
[0127] Experimental method: Refer to Sinopec standard Q / SH CG0040-2021 Technical requirements for corrosion inhibitors for oilfield water treatment to test the corrosion inhibition effect of the demulsifier.
[0128] The test steel sheet is A3 steel sheet, and the product dosage is 30ppm.
[0129] The test temperature was 50±2°C for 7 days, and the corrosion inhibition rate was calculated by the static atmospheric pressure weight loss method.
[0130] The test results are shown in Table 2 below.
[0131] Table 2 Corrosion inhibition effect test results of demulsifier
[0132] product Dosage / ppm Weight loss / g Corrosion inhibition rate blank 0 0.0086 / Example 1 30 0.0049 43.02% Example 2 30 0.0051 40.70% Example 3 30 0.0046 45.51% Example 4 30 0.0061 29.07% Example 5 30 0.0041 52.33% Example 6 30 0.0041 52.33% Example 7 30 0.0043 50.00% Example 8 30 0.0042 51.16% Example 9 30 0.0042 51.16% Example 10 30 0.0042 51.16%
[0133] From the corrosion inhibition experimental data in the above table, it can be seen that the demulsifier of the structure of the present invention has good corrosion inhibition performance. Among them, the demulsifier schemes in Example 5 and Example 8 show good corrosion inhibition performance. At the same time, through comparison of the data of each scheme, it can be found that the demulsifier scheme with a high proportion of ethylene oxide in the embodiment components has a relatively poor sustained release effect. Analysis shows that this is because ethoxylates are hydrophilic and propoxylates are lipophilic. When the proportion of ethylene oxide increases, its water solubility will be enhanced, resulting in the inability to form a stable protective film on the metal surface, thus affecting the corrosion inhibition effect.
[0134] In summary, the demulsifiers with the imidazole ring polyoxypropylene polyoxyethylene polyether structure of the present invention all exhibited the expected corrosion inhibition performance.
[0135] Obviously, the above embodiments are merely examples for clarity of explanation and are not intended to limit the implementation methods. Those skilled in the art will readily appreciate that other variations or modifications based on the above descriptions are possible. It is not necessary and impossible to enumerate all implementation methods here. Obvious variations or modifications arising therefrom remain within the scope of protection of the present invention.
Claims
1. Use of an imidazole ring polyoxypropylene polyoxyethylene polyether having a structure as shown in the following formula (I) for preparing a demulsifier with corrosion inhibition performance; in, x is an integer from 0 to 2; R1 is selected from substituted or unsubstituted C2-C 20 Saturated fatty chain, substituted or unsubstituted monounsaturated fatty chain, substituted or unsubstituted polyunsaturated fatty chain; R2 is a polyoxypropylene polyoxyethylene segment having a structure shown in the following formula (II): Among them, m=30-44, n=14-24.
2. The use according to claim 1, characterized in that The preparation method of the imidazole cyclopolyoxypropylene polyoxyethylene polyether comprises the steps of polymerizing the intermediate with propylene oxide and ethylene oxide; Wherein, the intermediate has a structure shown in the following formula (M): Wherein, x is an integer from 0 to 2; R1 is selected from substituted or unsubstituted C2-C 20 Saturated fatty chain, substituted or unsubstituted monounsaturated fatty chain, substituted or unsubstituted polyunsaturated fatty chain.
3. The use according to claim 1 or 2, characterized in that The R1 is selected from C 16 H 32 , C 16 H 33 , C 17 H 34 , C 17 H 35 , C 18 H 36 or C 18 H 37 One of them.
4. The use according to claim 3, characterized in that The preparation method of the intermediate comprises the steps of slowly dropping an organic amine into a mixed solution containing an organic acid and a water-carrying agent and carrying out a heat preservation reaction, and the steps of heating and refluxing for dehydration and vacuum removing the water-carrying agent to obtain the desired intermediate.
5. The use according to claim 4, characterized in that In the preparation method of the intermediate: The organic amine includes at least one of ethylenediamine, diethylenetriamine, triethylenetetramine or tetraethylenepentamine; The organic acid is selected from at least one of oleic acid, linoleic acid, palmitic acid, arachidic acid, linolenic acid or stearic acid; The water-carrying agent includes at least one of toluene, xylene, trimethylbenzene, 120# solvent oil, 150# solvent oil or 200# solvent oil.
6. The use according to claim 5, characterized in that In the preparation method of the intermediate: The molar ratio of the organic acid to the organic amine is 1:0.5-2; The amount of the water-carrying agent used accounts for 20-90wt% of the total amount of the reaction substrate.
7. The use according to claim 1 or 2, characterized in that: The demulsifier further comprises a solvent; the solvent comprises at least one of methanol, ethanol or water.
Citation Information
Patent Citations
A water-soluble nonionic imidazoline corrosion inhibitor and its preparation method
CN103320797B
Water-soluble non-ionic imidazoline corrosion inhibitor and preparation method thereof
CN103320797A