Radiation detector with butted absorber tiles without dead zones
The use of smaller tiles with filled gaps in radiation detectors addresses production challenges and blind areas, facilitating efficient and effective large-area detector manufacturing.
Patent Information
- Application Number
- CN202210326248.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2021-03-30
- Filing Date
- 2022-03-30
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2042-03-30
AI Technical Summary
The production of large-area radiation detectors for X-rays and gamma rays is hindered by the need for high pressures and complex handling of brittle materials, leading to high costs and the presence of blind areas due to gaps between tiles, which are difficult to eliminate.
A detector design with smaller tiles and gaps filled with a semiconductor or perovskite material, allowing for easier manufacturing and eliminating blind areas by contributing to the imaging signal.
Enables efficient production of large-area detectors with reduced blind areas and improved imaging capabilities by using smaller tiles and filling gaps with semiconductor or perovskite materials.
Smart Images

Figure CN115144888B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a detector for electromagnetic radiation, the detector comprising: a first pixelated electrode layer, the first pixelated electrode layer comprising a plurality of electrode pixels; a first layer, the first layer comprising a plurality of tiles, the plurality of tiles comprising a material that absorbs and converts electromagnetic radiation; and a second electrode layer. The invention also relates to a method for producing a detector for electromagnetic radiation, the method comprising: providing a first pixelated electrode layer comprising a plurality of electrode pixels; applying a plurality of tiles comprising a material that absorbs and converts electromagnetic radiation on the first pixelated electrode layer; and applying a second electrode layer on the first layer. Background Art
[0002] The project in this application has received funding from the European Union's Horizon 2020 research and innovation programme under grant agreement number 871336.
[0003] Detectors for X-rays and / or gamma radiation have a wide variety of applications, for example in medical diagnostics. Thus, the detection of radiation can be based on direct conversion or indirect conversion. For direct conversion, particles are excited in the absorption layer, resulting in the formation of electron-hole pairs, which may travel due to the applied electric field. For indirect conversion, the radiation excites the scintillating material, which results in the formation of photons. The photons can then be converted into electric charges in a photon detector, which can be detected again by applying an electric field. Another detection method is to use a hybrid organic detector as disclosed, for example, in EP 20155403.7, in which the problem of adhesion of the absorption layer on the substrate is solved.
[0004] However, another problem in producing detectors for X-rays and / or gamma radiation, in particular X-ray detectors and in particular those using, for example, soft sintered layers comprising or even consisting of perovskites, is the production of absorber layers, for example for direct conversion, since this requires relatively high pressures in the range of about 100 MPa. 2 For a small area of 10x10cm, this pressure is equivalent to a weight of about 4 tons. As the area increases, the necessary weight increases in a quadratic function. 2 For a detector with an effective area of 20x20cm, a weight of about 102 tons is required; for a detector with an effective area of 20x20cm 2 For a detector with an effective area of 40x40cm, a weight of about 408 tons is required; and for a detector with an effective area of 40x40cm 2 For the effective area of the detector, a weight of approximately 1600 tons is required. Figure 1 This relationship is shown in Figure 1In Fig. 1, assuming a square radiation detector, the increase in weight w with the lateral dimension s of the detector area can be seen at a pressure of 100 MPa.
[0005] Although there are hydraulic presses that can apply such weights, they are very large and expensive. Furthermore, the tools needed for producing the absorber plates / tiles, for example using soft sintering of powders (e.g. perovskite powders), are also very expensive as the size increases, since the plates / tiles need to be produced with plane parallelism between them. Furthermore, the handling of the tiles may become increasingly complex as the size increases, since the material of the absorber layer may be very brittle, as is the case, for example, if the material of the absorber layer is perovskite. And for other materials, such as silicon, cadmium tellurite or selenium, producing large areas is usually accompanied by high costs.
[0006] On the other hand, detectors for electromagnetic radiation - especially X-ray and / or gamma ray detectors - usually require the size of the object to be imaged due to insufficient optics. In addition to the above, the production of large-area radiation detectors is another technical challenge. When using crystalline materials such as CdTe or CdZnTe or Si, the size limitation is the size of the wafer.
[0007] Furthermore, the geometric requirements required in computed tomography, such as curved surfaces, are not easily achieved using rigid materials like silicon or glass as backplanes (e.g. for ASICs (Application Specific Integrated Circuits) or interposers), as is the case for conversion layers (e.g. CdTe or GOS). These technical issues are usually addressed using tiles in total modular units (e.g. in computed tomography) and tiles for CMOS backplanes for flat panel X-ray detectors such as Teledyne Dalsa.
[0008] exist Figure 2 and Figure 3 The use of tiles is schematically illustrated in a comparison of two detectors in the form of large-area direct conversion radiation detectors in the prior art.
[0009] exist Figure 2In the invention, a classical method for a detector is described, which detector has: a first pixelated electrode layer 1, which is optionally on a suitable substrate in the form of an active matrix backplane substrate, the substrate being, for example, glass or silicon with a-Si, IGZO (indium gallium zinc oxide) or a CMOS TFT circuit system, the first pixelated electrode layer 1 also including a bottom electrode for each pixel on the bottom; a first layer 2, which includes a material that absorbs and converts electromagnetic radiation (hereinafter also referred to as a radiation conversion layer), the first layer 2 including, on its top, a semiconductor such as CdTe, a-Se, Si, GaAs, Ge, HgI2, PbO, a semiconductor perovskite or other material; and a second electrode layer 3, which is on top of the first layer 2, the second electrode layer 3 also being referred to as a top electrode.
[0010] exist Figure 3 In FIG. 1 , a so-called docking method is shown, in which a dead zone in the form of a gap 4 is present. Figure 2 Between the two detector components in the embodiment of the present invention, the gap 4 can not only separate the two first layers 2 in the form of mosaics, but also separate the two first pixelated electrode layers 1 and the two second electrode layers 3.
[0011] exist Figure 2 In a classical representation of, as for example in a-Se flat panel detectors for mammography applications, the first layer 2 as absorber layer is respectively larger than or equal to the pixelated area in the first pixelated electrode layer 1 of the backplane. Figure 3 In the docking method used in, for example, a CMOS flat panel X-ray detector, the first layer 2 as an absorber layer is respectively larger than or equal to the pixelated area in the first pixelated electrode layer 1 of the CMOS backplane; however, at the 1st, 2nd or 3rd side of the CMOS tile, the pixelated area and the absorber layer are coincident and extend all the way to the edge of the tile. Between the docked tiles, there is always a dead area in the form of a gap 4 between the tiles, which does not provide imaging signals.
[0012] Therefore, the disadvantage of using tiles or modular units of a CMOS backplane is that the area between the tiles is insensitive and therefore represents a blind area that cannot be imaged. For flat-panel X-ray detectors, the dead zone can be reduced to just one row or column of the detector, which can be seen as a row or column with no signal (defect) in the raw image. However, this requires great attention to precision when applying the tiles. Until now, the blind area could only be reduced, not eliminated.
[0013] In state-of-the-art detectors, the blind areas are interpolated by software. However, this is very difficult to manage as it requires a pixel size P gFor flat panel X-ray detectors of the prior art, the pixel size P g The range of Å is typically between and including 50 μm and 300 μm.
[0014] Therefore, there remains a need for a detector for electromagnetic radiation which can be easily produced and which avoids the problems associated with blind areas between tiles for absorbing radiation.
[0015] The inventors have discovered that the use of even smaller tiles for absorbing and converting electromagnetic radiation in a detector for electromagnetic radiation and their use on a backplane not only enables easier manufacturing, but can also lead to enhanced imaging when the gaps between the tiles are appropriately filled with materials that contribute to the signal in the underlying pixels. Summary of the invention
[0016] In a first aspect, the invention relates to a detector for electromagnetic radiation, in particular an X-ray detector and / or a gamma-ray detector, comprising:
[0017] - a first pixelated electrode layer comprising a plurality of electrode pixels,
[0018] a first layer comprising a plurality of tiles comprising a material that absorbs and converts electromagnetic radiation, wherein the first layer comprises gaps between the tiles, wherein the gaps are filled with a material comprising at least a first semiconductor and / or at least a first perovskite, and
[0019] - A second electrode layer.
[0020] Furthermore, in a second aspect, the present invention relates to a method for producing a detector for electromagnetic radiation, in particular an X-ray detector and / or a gamma-ray detector, the method comprising:
[0021] - providing a first pixelated electrode layer comprising a plurality of electrode pixels,
[0022] - optionally, applying a second layer on the first pixelated electrode layer, wherein the second layer is an adhesion promoting layer, preferably wherein the second layer comprises at least a second semiconductor and / or conductor and / or a third perovskite,
[0023] - applying a plurality of tiles comprising a material that absorbs and converts electromagnetic radiation on the first pixelated electrode layer or on the optional second layer, wherein gaps are formed between the tiles,
[0024] - applying a material comprising at least a first semiconductor and / or at least a first perovskite in the gap until the gap is filled, wherein the tiles and the filled gap form a first layer, and
[0025] - Applying a second electrode layer on the first layer.
[0026] Other aspects and embodiments of the present invention are disclosed in the technical solution of the present invention and can be obtained from the following description, drawings and examples, but are not limited thereto. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The accompanying drawings shall illustrate embodiments of the invention and convey a further understanding of the embodiments. In conjunction with the description, the accompanying drawings serve as an illustration of the concepts and principles of the invention. Other embodiments and many of the stated advantages can be derived with respect to the accompanying drawings. The elements in the accompanying drawings are not necessarily to scale with each other. Unless otherwise stated, the same reference numerals are used in the figures of the accompanying drawings to represent the same, functionally equivalent, and equivalent features and components.
[0028] Figure 1 The pressing weight required to produce a tile of absorbent material at a pressure of 100 MPa for square radiation detectors with different detector areas is shown.
[0029] Figure 2 and Figure 3 A detector for electromagnetic radiation according to the prior art is schematically shown.
[0030] exist Figure 4 and Figure 5 In FIG. 1 , the filling of gaps between tiles in a detector for electromagnetic radiation of the present invention is schematically depicted.
[0031] Figure 6 Two alternatives for a back plate in a detector of electromagnetic radiation according to the invention are schematically shown.
[0032] exist Figure 7 and Figure 8 as well as Fig. 9 and Fig.10 In FIG. 1 , the filling of gaps between tiles in a detector for electromagnetic radiation with different backplates according to the invention is schematically depicted.
[0033] Figures 11 to 14 The steps in the method of the present invention are schematically shown.
[0034] Figures 15 to 17 The filling of a gap by the method of the invention is schematically illustrated. DETAILED DESCRIPTION
[0035] Unless otherwise defined, technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention belongs.
[0036] Unless stated otherwise or clear from the context, amounts in the present invention are given in wt %.
[0037] In this disclosure, reference to a conductive material refers to an electrically conductive material unless expressly stated otherwise.
[0038] Before describing the present invention in exemplary detail, it should be understood that the present invention is not limited to the specific components of the processing steps of the method described herein, because such a method can be changed. It should also be understood that the terms used herein are only for the purpose of describing specific embodiments, and are not intended to be limiting. It must be noted that, as used in the specification and the appended claims, the singular forms of "one", "an" and "the" include singular referents and / or plural referents, unless otherwise clearly indicated in the context. For example, the term "one" as used herein can be understood as a single entity or the meaning of "one or more" entities. It should also be understood that, unless otherwise clearly indicated in the context, the plural form includes singular referents and / or plural referents. In addition, it should be understood that, given the range of parameters defined by numerical values, these ranges are considered to include these limiting values.
[0039] A first aspect of the invention relates to a detector for electromagnetic radiation, in particular an X-ray and / or gamma ray detector, the detector for electromagnetic radiation comprising:
[0040] - a first pixelated electrode layer comprising a plurality of electrode pixels,
[0041] a first layer comprising a plurality of tiles comprising a material that absorbs and converts electromagnetic radiation, wherein the first layer comprises gaps between the tiles, wherein the gaps are filled with a material comprising at least a first semiconductor and / or at least a first perovskite, and
[0042] - A second electrode layer.
[0043] In particular, the first layer is arranged between the first pixelated electrode layer and the second electrode layer.
[0044] In particular, the detector may detect X-rays and / or gamma radiation, but preferably at least detects X-rays or in particular detects X-rays, ie the detector is an X-ray detector according to certain embodiments.
[0045] In the detector, the first pixelated electrode layer comprising a plurality of electrode pixels is not particularly limited. The number of electrode pixels is not particularly limited, but is at least 2. According to some embodiments, the number of electrode pixels (respective pixels) in each row is between 2 and 10,000 and includes 2 and 10,000, for example, between 2 and 1,000 and includes 2 and 1,000, for example, between 2 and 100 and includes 2 and 100. For example, a square detector, this results in the number of electrode pixels being, for example, 2×2 to 10,000×10,000, for example, 3,000×4,000. The first pixelated electrode layer includes at least 2 pixels, i.e., 2 or more, for example, 3, 4, 5, 6, 7, 8, 9, 10 or more. The electrode pixels may be appropriately electrically contacted. Neither the pixel size nor the material of the electrode pixels are particularly limited, and the pixel size and material of those electrode pixels applied in the detector for electromagnetic radiation may be appropriately applied. The electrode pixels may have square electrode pixels with a spacing of 98 μm, but may also have any other size. The material of the electrode pixel is not particularly limited, and may include a conductive metal oxide, a conductive polymer, and / or a metal, the material being used to detect, for example, electrons or holes generated in the first layer.
[0046] The first pixelated electrode layer may include a substrate on which the electrode pixels may be appropriately arranged. The substrate, which may also be referred to as a backplane, is not particularly limited and may be made of materials such as glass, silicon, plastic, etc. In order to contact the electrode pixels, there may be transistors and / or electrical connections for each individual pixel, the transistors being made, for example, of a-Si, IGZO or CMOS-based technology, etc. The backplane may also include a lower electrode, a passivation layer, for example comprising oxide and / or nitride, an optional anchor structure / grid, etc.
[0047] In addition, the second electrode layer is not particularly limited. The second electrode layer may include a conductive material, such as a conductive metal oxide, a conductive polymer and / or a metal. According to some embodiments, the second electrode layer may be arranged in a plane. According to some embodiments, the second electrode layer is at least partially permeable or even completely permeable to electromagnetic radiation to be detected, such as X-rays (wavelength ≥ 10pm and <10nm) and / or gamma radiation (wavelength <10pm). For example, the second electrode layer may include indium tin oxide (ITO), aluminum zinc oxide (aluminum-doped zinc oxide, AZO), antimony tin oxide (ATO) and / or fluorine tin oxide (FTO) as electrode materials, or the second electrode layer may be composed of indium tin oxide (ITO), aluminum zinc oxide (aluminum-doped zinc oxide, AZO), antimony tin oxide (ATO) and / or fluorine tin oxide (FTO).
[0048] In the detector, the corresponding electrode can be connected appropriately as anode or cathode.
[0049] According to certain embodiments, a surface layer such as glass and / or encapsulation may be disposed on the second electrode layer opposite to the first layer for protection, which is not particularly limited. The surface layer may be appropriately formed in the method of the present invention.
[0050] Furthermore, the first layer comprises a plurality of tiles comprising a material that absorbs and converts electromagnetic radiation, wherein the first layer comprises gaps between the tiles - without being particularly limited as long as the gaps are filled with a material comprising at least a first semiconductor and / or at least a first perovskite.
[0051] In particular, in the present detector, the first layer consists only of tiles and filled gaps.
[0052] The tiles comprising the material absorbing and converting electromagnetic radiation in the first layer are not particularly limited. These tiles can be regular, for example square or rectangular in shape, but can also have any other shape, or can also be irregular. According to some embodiments, these tiles are square so that they can be arranged regularly and as close as possible so that the spaces between the gaps can be minimized.
[0053] In the present detector, the size of the blocks in the first layer is not particularly limited. According to some embodiments, the size of the blocks is 1×1 cm 2 Up to 50×50cm 2 In the range of 5×5 cm, preferably, the size of the puzzle piece is 5×5 cm 2 Up to 50×50cm 2 Between and including 5×5cm 2 and 50×50cm 2 Preferably, the size of the puzzle is 10×10 cm 2 Up to 50×50cm 2 Between and including 10×10cm 2 and 50×50cm 2. With these dimensions, good manufacturing of the tiles is guaranteed, while good conversion in the absorption layer is achieved and the application of filling material in the gap can be easily carried out. In particular, with such dimensions, soft sintering of the tiles, in particular in the case where the tiles comprise a second perovskite, is possible and the tiles can be easily attached. In particular, the smaller size of the tiles also enables the use of smaller presses and tools to manufacture the tiles. Compared to the prior art in EP20155403.7, in which the surface of the absorption layer is greater than or at least equal to the effective area of the pixelated electrode layer (corresponding backplane), in particular, the present detector has tiles of a size smaller than the size of the first pixelated electrode layer, so that a large number of tiles, i.e. at least two tiles, are necessary to cover the entire surface of the first pixelated electrode layer. If there are only two tiles, there is only one gap.
[0054] According to certain embodiments, the number of tiles in the first layer is between 2 and 1000 and includes 2 and 1000, preferably, the number of tiles in the first layer is between 2 and 100 and includes 2 and 100, and more preferably, the number of tiles in the first layer is between 2 and 50 and includes 2 and 50.
[0055] According to certain embodiments, the tilt angle between tiles of two adjacent tiles in the first layer is between 0° and 5° inclusive. This enables good filling of the gap.
[0056] In addition, the thickness of the patch is not particularly limited and may be, for example, between 10 μm and 10,000 μm, preferably, the thickness of the patch may be between 50 μm and 3,000 μm, more preferably, the thickness of the patch may be between 100 μm and 1,500 μm, for example, the thickness of the patch may be between 100 μm and 1,000 μm, inclusive.
[0057] According to certain embodiments, the gaps between the tiles are completely filled, so that no blind areas remain, i.e. areas that are insensitive and therefore do not contribute to the image. However, it is not excluded that a small amount of gaps are not completely filled, e.g. in case another layer, e.g. an intermediate layer, is arranged on top of the first layer. In such a case, less than 10 vol%, preferably less than 5 vol%, in particular less than 1 vol% of the gaps may not be filled. If all gaps are filled, the thickness of the material in the gaps is preferably substantially the same as the thickness of the tiles.
[0058] According to some embodiments, the gap size g between tiles depends on the pixel pitch P g According to certain embodiments, the following applies:
[0059] P g / 100≤g≤P g *1000; preferably, P g / 10≤g≤P g *100; more preferably, P g ≤g≤P g *10
[0060] According to certain embodiments, the gaps between tiles have a width of 0.1 pixel pitches to 50 pixel pitches, wherein the length of the pixel pitches is between and including 10 μm and 1000 μm.
[0061] According to the present invention, the gaps between the tiles are filled with a material comprising at least a first semiconductor and / or at least a first perovskite, for example in fluid form, as a paste or as a solid. After recrystallization (when using, for example, a liquefied perovskite), solvent removal (for example, when using a paste), etc., a layer comprising at least a first semiconductor and / or at least a first perovskite remains, which layer can contribute to the signal in the pixel below. According to certain embodiments, it is ensured that the material comprising at least a first semiconductor and / or at least a first perovskite completely fills the gap, for example, using a liquefied perovskite and / or a paste to completely fill the gap. This is equivalent to (metaphorically) applying a caulking mortar between the tiles, especially deep in the gap.
[0062] If the first semiconductor and / or at least the first perovskite is included, the material comprising at least the first semiconductor and / or at least the first perovskite in the gap is not particularly limited. According to certain embodiments, the material comprising at least the first semiconductor and / or at least the first perovskite in the gap is essentially composed of (meaning that at least 95wt%, at least 99wt% or even 99.9wt% of the material is at least the first semiconductor and / or the first perovskite) or even consists of at least the first semiconductor and / or the first perovskite. According to certain embodiments, the material comprising at least the first semiconductor and / or at least the first perovskite in the gap only comprises the first semiconductor and / or the first perovskite, but does not exclude the first semiconductor and / or the first perovskite from being present as a mixture of the first semiconductor and / or the first perovskite. In addition to the first semiconductor and / or the first perovskite, additional materials such as binders may also be included, however, relative to the material comprising at least the first semiconductor and / or the at least first perovskite, the amount of the additional material is up to 30wt%, preferably up to 30wt%, further preferably up to 10wt%, even more preferably up to 5wt%.
[0063] The material in the gap includes at least one first semiconductor and / or at least one first perovskite. The first semiconductor and / or the first perovskite may be the same as the material that absorbs and converts electromagnetic radiation or may be different. According to some embodiments, the material including at least the first semiconductor and / or at least the first perovskite is the same as the material that absorbs and converts electromagnetic radiation.
[0064] Since some perovskites are also semiconductors, there is also an overlap between possible materials for the first semiconductor and the first perovskite. According to certain embodiments, the gap is filled with a material comprising at least the first perovskite, which is particularly advantageous when the material that absorbs and converts electromagnetic radiation comprises a second perovskite, which may be the same as the first perovskite or may be different.
[0065] The first semiconductor is not particularly limited and may include at least one of the following: mercury (II) iodide (HgI2), lead (II) iodide (PbI2), bismuth triiodide (BiI3), thallium bromide (TlBr), lead oxide (II) (PbO), cadmium telluride (CdTe), cadmium zinc telluride (CdZnTe), amorphous selenium (a-Se), gallium arsenide (GaAs) and / or silicon (Si). However, an organic-inorganic semiconductor perovskite may also be a semiconductor and thus may also be considered as a first semiconductor, but according to certain embodiments, the organic-inorganic semiconductor perovskite is not included.
[0066] In addition, the first perovskite is not particularly limited and may include any organic perovskite, inorganic perovskite and / or organic-inorganic perovskite and mixtures thereof. For example, suitable perovskites are described in WO 2014045021 A1, and reference is made to the document WO 2014045021 A1 regarding perovskites. The perovskite may have an ABX structure, such as an ABX3 structure, having one or more A cations, one or more B cations and one or more anions X, in particular, the A cations, B cations and anions X are selected from chalcogenides and / or halides, in particular halides, wherein,
[0067] The A cation and the B cation may be organic and / or inorganic - in particular, A is an organic cation selected from alkyl, aryl, aralkyl, alkylaryl, alkenyl and / or alkynyl ammonium groups (i.e. having one, two, three or four identical or different residues, including organic residues and H, in the ammonium group), for example having 1 to 60 carbon atoms; in particular, B is an inorganic cation, in particular selected from cations (in particular divalent cations) of metals such as Ca, Sr, Cd, Cu, Ni, Mn, Fe, Co, Pd, Ge, Sn, Pb and lanthanides such as Yb, Gd, Eu, suitable chalcogenides include oxides, sulfides, selenides, tellurides; and
[0068] Suitable halides include, for example, F - , Cl - Br - ,I - , especially Cl - Br - ,I - .
[0069] Suitable examples of perovskites as the first perovskite include, for example, MAPbI3(CH3NH3PbI3), MAPbBr3(CH3NH3PbBr3), FAPbI3(HC(NH2)2PbI3), MAPbICl2(CH3NH3PbICl2), FAPbBr3(HC(NH2)2PbBr3), EAPbI3(CH3CH2NH3PbI3), PAPbI3(CH3CH2CH2NH3PbI3), BA2PbI4((CH3CH2CH2CH2NH3)2PbI4), PMA2PbI4((C6H5CH2NH3)2PbI4), PEA2PbI4((C6H5CH2NH3)2PbI4), 6H5CH2CH2NH3)2PbI4), EAPbBr3 (CH3CH2NH3PbBr3), PAPbBr3 (CH3CH2CH2NH3PbBr3); their other mixed halides; inorganic-organic perovskites with mixtures of A-cations and halides X (X=Cl, Br, I), such as MAFAPbX3 (MA=CH3NH3, FA=HC(NH2)2), MAGAPbX3 (GA=guanidine salt), BAPAPbX3 (BA=CH3CH2CH2CH2NH3, PA=CH3CH2CH2NH3), etc.; organic halogenated mixtures, in which halogens can be partially replaced by other halogens, such as formula I 3-x Cl x or Br 3-x Cl x Halides, such as MAPbI 3-x Cl x or CH3NH3PbBr 3-x Cl x; organic and / or inorganic perovskites, wherein Pb is at least partially or even completely replaced by Sn, Cu, Ni, Bi, Co, Fe, Mn, Cr, Cd, Ge and / or Yb and / or mixtures thereof; inorganic perovskites and mixtures thereof such as CsPbX3, wherein X=Cl, Br and / or I, and mixtures thereof (e.g., CsPbBr3, CsPbI3, CsPbCl3); Cs3Bi2X9, wherein X=Cl, B r and / or I, and mixtures thereof; Cs3Sb2X, wherein X=Cl, Br and / or I, and mixtures thereof; Cs2AgBiX6, wherein X=Cl, Br and / or I, and mixtures thereof; Rb3Bi2X9, wherein X=Cl, Br and / or I, and mixtures thereof; Rb3Sb2X9, wherein X=Cl, Br and / or I, and mixtures thereof; CsSnI3; etc.; and mixtures of these perovskites.
[0070] In particular, the first perovskite can be applied as a liquefied perovskite and as a hardened paste or as a powder, and / or the first semiconductor can be applied as a paste and / or as a powder. If the material is applied as a paste or as a powder, suitable additives can be included, such as at least a solvent and / or at least a binder.
[0071] For example, it is possible to liquefy the first perovskite using methylamine (MA) gas, in particular in the case of methylammonium ions in the first perovskite. This process is described, for example, in the following documents: EP 20155403.7 or Li, C., S. Pang, H. Xu and G. Cui, "Methylamine gas based synthesis and healing process toward upscaling of perovskite solar cells: Progress and perspective", Solar RRL, 1 (9), 1700076 (2017), wherein reference is made to these two documents regarding the liquefaction of perovskite using methylamine gas. Due to the MA gas, once the MA gas is no longer present in the atmosphere, the perovskite can be liquefied and subsequently recrystallized, for example with a changed morphology. After removing the methylamine gas, the perovskite can therefore be recrystallized in the gap using the present method, and the perovskite is respectively present in the detector in a recrystallized form. In particular, in such a case, it is preferred that the first perovskite includes an alkylammonium cation, wherein the alkyl group has 1 to 4 carbon atoms, particularly a methylammonium cation.
[0072] In such a case, it is also possible to fill a precursor, such as lead iodide of a perovskite, as described, for example, in EP 3304611 B1, and then crystallize it.
[0073] For the application of the paste, at least one first semiconductor and / or at least one first perovskite may be present in the form of particles, which may be suitably mixed with at least one binder and / or at least one solvent. To this end, particles, for example in the form of a powder, may be dispersed in a suitable solvent, optionally with the addition of at least one binder. Pastes suitable for application are described, for example, in US 20120181440 A1 and EP 3376260 A1.
[0074] In the paste, the size of the particles is not particularly limited, and for example as measured by sieve analysis or laser diffraction, the size of the particles can be, for example, between 0.01 μm and 600 μm and within the range of 0.01 μm and 600 μm (i.e. also covering quantum dots and / or nanocrystals), the size of the particles is, for example, between 1 μm and 300 μm and within the range of 1 μm and 300 μm.
[0075] If the paste contains at least one binder, the binder is not particularly limited and can be selected from suitable polymer resins such as polyvinyl butyral (PVB) resins, acrylic resins, phenoxy resins, polyester resins, polyvinyl formal resins, polyamide resins, polystyrene resins, polycarbonate resins, polyvinyl acetate resins, polyurethane resins, epoxy resins, polyimide resins, polyvinyl alcohol resins, polyethylene resins, polyester resins, polycarbonate resins, and any mixtures thereof. The amount of the binder can be appropriately set based on, for example, the binder, and the amount of the binder can be in a range of equal to or less than 30 wt %, in a range of equal to or less than 20 wt %, and / or in a range of greater than 1 wt %, for example, greater than 2 wt %, based on the total amount of the paste.
[0076] If the paste contains a solvent, the solvent is not particularly limited and can be appropriately selected, for example, from the following list according to the binder: dipropylene glycol monomethyl ether (DPGME), butyl cellosolve (BC), γ-butyrolactone, N-methyl-2-pyrrolidone, N,N-dimethylformamide, butyl cellosolve acetate (BCeA), KOCOSOL, butyl cellosolve (BC), ethyl 3-ethoxypropionate (EEP) and mixtures thereof. If a solvent is contained, the amount of the solvent can be in the range of 1 wt% to 60 wt%, for example, in the range of 2 wt% to 50 wt%, for example, in the range of 3 wt% to 40 wt%, based on the total mass of the paste. In addition, the paste may also include additives such as dispersants, defoamers and leveling agents.
[0077] As described above with respect to the paste, in the case where the material comprising at least one first semiconductor and / or at least one first perovskite in the gap is applied as a powder, the material may be applied only as a powder of particles of at least one first semiconductor and / or at least one first perovskite, wherein the size of the particles is, for example, between 0.01 μm and 600 μm and including 0.01 μm and 600 μm, and the size of the particles is, for example, between 1 μm and 300 μm and including 1 μm and 300 μm. In such a case, the powder may be merely filled, but may also be compacted, bonded together using a suitable resin, etc.
[0078] According to certain embodiments, the material in the gap is filled as a recrystallized liquefied perovskite and / or as a paste comprising at least one first semiconductor and / or at least one first perovskite.
[0079] In the tiles of the first layer, the material that absorbs and converts electromagnetic radiation is not particularly limited.
[0080] For example, the material absorbing and converting electromagnetic radiation may comprise or even consist of a scintillator, for example for detecting gamma radiation, the scintillator being selected from the list comprising: CsI:Tl - thallium-doped cesium iodide, terbium-doped gadolinium oxysulfide, barium fluoride (BaF2), bismuth germanate (BGO), beryllium fluoride (BeF3), quantum dots, scintillating perovskite nanocrystals (the perovskite being selected from those described with respect to the first perovskite), etc. Alternatively or additionally, the material absorbing and converting electromagnetic radiation may comprise or even consist of a second semiconductor, which may be the same as or different from the first semiconductor. Such a second semiconductor is not particularly limited and may include at least one of: mercury (II) iodide (HgI2), lead (II) iodide (PbI2), bismuth triiodide (BiI3), thallium bromide (TlBr), lead oxide (II) (PbO), cadmium telluride (CdTe), cadmium zinc telluride (CdZnTe), amorphous selenium (a-Se), gallium arsenide (GaAs) and / or silicon (Si).
[0081] According to certain embodiments, the tiles in the first layer include at least a second perovskite as a material that absorbs and converts electromagnetic radiation, or the tiles in the first layer may even consist of a second perovskite as a material that absorbs and converts electromagnetic radiation. The second perovskite may be the same as the first perovskite, or may be different from the first perovskite. According to certain embodiments, the second perovskite is the same as the first perovskite. As the first perovskite, the second perovskite is not particularly limited and may include any organic perovskite, inorganic perovskite and / or organic-inorganic perovskite and mixtures thereof. For example, suitable perovskites are described in WO2014045021 A1, and reference is made to WO 2014045021 A1 regarding perovskites. The perovskite may have an ABX structure, such as an ABX3 structure, having one or more A cations, one or more B cations and one or more anions X, in particular, the A cations, B cations and anions X are selected from chalcogenides and / or halides, in particular halides, wherein,
[0082] The A cation and the B cation may be organic and / or inorganic - in particular, A is an organic cation selected from, for example, alkyl, aryl, aralkyl, alkylaryl, alkenyl, alkynyl groups having 1 to 20 carbon atoms; in particular, B is an inorganic cation, in particular selected from cations (in particular divalent cations) of metals such as Ca, Sr, Cd, Cu, Ni, Mn, Fe, Co, Pd, Ge, Sn, Pb and lanthanides such as Yb, Gd, Eu,
[0083] Suitable chalcogenides include oxides, sulfides, selenides, tellurides, and
[0084] Suitable halides include, for example, F - , Cl - Br - ,I - , especially Cl - Br - ,I - .
[0085] Suitable examples of perovskites as the second perovskite include, for example, MAPbI3(CH3NH3PbI3), MAPbBr3(CH3NH3PbBr3), FAPbI3(HC(NH2)2PbI3), MAPbICl2(CH3NH3PbICl2), FAPbBr3(HC(NH2)2PbBr3), EAPbI3(CH3CH2NH3PbI3), PAPbI3(CH3CH2CH2NH3PbI3), BA2PbI4((CH3CH2CH2CH2NH3)2PbI4), PMA2PbI4((C6H5CH2NH3)2PbI4), PEA2PbI4((C6H5CH2NH3)2PbI4), 6H5CH2CH2NH3)2PbI4), EAPbBr3 (CH3CH2NH3PbBr3), PAPbBr3 (CH3CH2CH2NH3PbBr3); their other mixed halides; inorganic-organic perovskites with mixtures of A-cations and halides X (X=Cl, Br, I), such as MAFAPbX3 (MA=CH3NH3, FA=HC(NH2)2), MAGAPbX3 (GA=guanidine salt), BAPAPbX3 (BA=CH3CH2CH2CH2NH3, PA=CH3CH2CH2NH3), etc.; organic halogenated mixtures, in which halogens can be partially replaced by other halogens, such as formula I 3-x Cl x or Br 3-x Cl x Halides, such as MAPbI 3-x Cl x or CH3NH3PbBr 3-x Cl x ; organic and / or inorganic perovskites, wherein Pb is at least partially or even completely replaced by Sn, Cu, Ni, Bi, Co, Fe, Mn, Cr, Cd, Ge and / or Yb and / or mixtures thereof; inorganic perovskites and mixtures thereof, such as CsPbX3, wherein X=Cl, Br and / or I, and mixtures thereof (e.g., CsPbBr3, CsPbI3, CsPbCl3); Cs3Bi2X9, wherein X=Cl, B r and / or I, and mixtures thereof; Cs3Sb2X, wherein X=Cl, Br and / or I, and mixtures thereof; Cs2AgBiX6, wherein X=Cl, Br and / or I, and mixtures thereof; Rb3Bi2X9, wherein X=Cl, Br and / or I, and mixtures thereof; Rb3Sb2X9, wherein X=Cl, Br and / or I, and mixtures thereof; CsSnI3; etc.; and mixtures of these perovskites.
[0086] If the second perovskite and the first perovskite are used and are identical, the material in the patch can nevertheless still be distinguished from the material in the gap due to the manufacturing process. Differences, for example regarding grain size, grain boundaries, density, porosity, etc., can be found in the morphology of the individual layers at the location of the patch and in the gap. Thus, even if the same material is used, for example regarding morphology and / or interior, the material in the patch and the gap can be clearly distinguished due to differences in their production. Thus, even if the same chemical material is used, the electrical signal (and corresponding sensitivity) may be different when comparing the material in the patch and the gap due to differences in morphology, etc.
[0087] According to some embodiments, the detector further comprises at least one intermediate layer between the first pixelated electrode layer and the first layer and / or between the first layer and the second electrode layer. The intermediate layer is a layer that can be used as an electron transport layer (corresponding hole blocking layer (HBL)) or a hole transport layer (corresponding electron blocking layer (EBL)). The various layers can be appropriately arranged according to the charge of the various electrodes (corresponding electrode layers). The material and thickness of any intermediate layer are not particularly limited.
[0088] An exemplary electron transport layer (HBL) may include one or more of the following materials, for example, with ≥30 wt%, ≥50 wt%, or ≥70 wt%, relative to the electron transport layer; consist essentially of one or more of these materials (e.g., with ≥90 wt%, ≥95 wt%, or ≥99 wt%, relative to the electron transport layer); or even consist of at least one of these materials (wherein the following list is not exhaustive and also includes mixtures of these materials as well as heterogeneous mixtures, such as binary mixtures, ternary mixtures, quaternary mixtures, etc.):
[0089] Fullerene derivatives, such as C60 PCBM ([6,6]-phenyl C61 butyric acid methyl ester), C70 PCBM ([6,6]-phenyl C71 butyric acid methyl ester), bis-C60 PCBM (bis-[6,6]-phenyl C61 butyric acid methyl ester), C60 oQDM (o-quinodimethane C60 monoadduct), bis-C60-oQDM (o-quinodimethane C60 bisadduct), ICMA (indene C60 monoadduct), ICBA (indene C60 bisadduct), fullerol (C60(OH)44); and other acceptors, including polymers and small molecules, such as dithienoindanediyl compounds, such as 3,9-bis(2-methylene-(3-(1,1-dicyanomethylene)-indanone))-5, 5,11,11-Tetrakis(4-hexylphenyl)-dithienyl[2,3-d:2',3'-d']-s-indenadiene[1,2-b:5,6-b']dithienyl (ITIC), IT-M (ITIC-M; 3,9-bis(2-methylene-((3-(1,1-dicyanomethylene)-6 / 7-methyl)-indanone))-5,5,11,11-tetrakis(4-hexylphenyl)-dithienyl[2,3-d:2',3'-d']-s-indenadiene[1,2-b:5,6-b']dithienyl (ITIC), IT-M ,3'-d']-s-indan[1,2-b:5,6-b']dithiophene), IT-DM (ITIC-DM; 3,9-bis(2-methylene-((3-(1,1-dicyanomethylidene)-6,7-dimethyl)-indanone))-5,5,11,11-tetra(4-hexylphenyl)-dithieno[2,3-d:2',3'-d']-s-indan[1,2-b:5,6-b']dithiophene) and IDTBR ((5Z,5'Z)-5,5'-((7,7'-(4,4,9,9-tetraoctyl-4,9-dihydro-s-indeno[1,2-b:5,6-b']dithiophene-2,7-diyl)bis(benzo[c][1,2,5]thiadiazole-7,4-diyl))bis(methylene))bis(3-ethylthiazoline-2,4-dione)); perylene diimide-based compounds such as TPB (tert-butylpyridine, C9H 13N), SdiPDI-Se (a perylene diimide derivative modified by inserting a selenophene unit at the bay position), NIDCS-HO ((2E,2'E)-3,3'-(2,5-bis(hexyloxy)-1,4-phenylene)bis(2-(5-(4-(N-(2-ethylhexyl)-1,8-naphthyl)-2-thiophene)acrylonitrile)); diketopyrrolopyrrole-based compounds such as DPP6 (dipeptidyl aminopeptidase-like protein 6), 6,6'-(benzo[c][1,2 ,5]thiadiazole-4,7-diylbis([2,2'-bithiophene]-5',5-diyl))bis(2,5-bis(2-ethylhexyl)-3-(thiophene-2-yl)-2,5-dihydropyrrolo[3,4-c]pyrrole-1,4-dione)(DTDfBT(DPP)2), 6,6',6",6"'-(9,9'-spirobi[fluorene]-2,2',7,7'-tetrayltetra(thiophene-5,2-diyl))tetra(2,5-bis(2-ethylhexyl)-3-(5- PFN (poly[(9,9-bis(3'-(N,N-dimethylamino)propyl)-2,7-fluorene)-alt-2,7-(9,9-dioctylfluorene)]), PFN-OX (poly[9,9-bis(60-(N,N-diethylamino)propyl)-fluorene-alt-9,9-bis-(3-ethyl(oxetane-3-ethoxy)-hexane)]) [(N,N'-bis(2-decyl-tetradecyl)-3,4,9,10-perylene diimide-1,7-diyl)]-alt-(dithieno[3,2-b:2',3'-d]thiophene-2,6-diyl)}), TPBi (1,3,5-tri(N-phenylbenzimidazol-2-yl)benzene); metal oxides, such as TiOx, SnOx, IGZO, etc.
[0090] An exemplary hole transport layer (EBL) may include one or more of the following materials, for example, with ≥30 wt%, ≥50 wt%, or ≥70 wt%, relative to the hole transport layer; essentially consist of one or more of these materials (for example, with ≥90 wt%, ≥95 wt%, or ≥99 wt%, relative to the hole transport layer); or even consist of at least one of these materials (wherein the following list is not exhaustive and also includes mixtures of these materials as well as isomeric mixtures, such as binary mixtures, ternary mixtures, quaternary mixtures, etc.):
[0091] Poly(3-hexylthiophene-2,5-diyl) (P3HT), poly[2-methoxy-5-(2-ethylhexyloxy)-1,4-phenylenevinylene] (MEH-PPV), poly[2-methoxy-5-(3′,7′-dimethyloctyloxy)-1,4-phenylenevinylene] (MDMO-PPV), CN-PPV, CN-MEH-PPV, other phthalocyanines, poly[(9,9-di-n-octylfluorenyl-2,7-diyl)-alt-(benzo[2,1,3]thiadiazole-4,8-diyl)] (F8BT), polyfluorene (PF), Poly[2,1,3-benzothiadiazole-4,7-diyl[4,4-bis(2-ethylhexyl)-4H-cyclopentadienyl[2,1-b:3,4-b']dithiophene-2,6-diyl]] (PCPDTBT), squarylium cyanine (e.g., symmetric squarylium cyanine or diazolosquarylium cyanine with glycolic acid functionalized hydrazone endcapping), (PTT) (polythieno[3,4-b]thiophene), poly(5,7-bis(4-decyl-2-thienyl)-thieno(3,4-b)dithiazolidine-thiophene-2,5) (PDDTT); diketopyrrolopyrrole-based polymers, such as Poly{2,2′-[(2,5-bis(2-hexyldecyl)-3,6-dioxo-2,3,5,6-tetrahydropyrrolo[3,4-c]pyrrole-1,4-diyl)dithiophene]-5,5′-diyl-alt-thiophene-2,5-diyl}(PDPP3T), Poly[[2,5-bis(2-hexyldecyl-2,3,5,6-tetrahydro-3,6-dioxo-pyrrolo[3,4c]pyrrole-1,4-diyl]-alt-[3′,3″-dimethyl-2,2′:5′,2″-terthiophene]-5,5″-diyl](PMDPP3 T) and poly{2,2′-[(2,5-bis(2-hexyldecyl)-3,6-dioxo-2,3,5,6-tetrahydropyrrolo[3,4-c]pyrrole-1,4-diyl)dithiophene]-5,5′-diyl-terthiophene-2,5-diyl} (PDPP5T), poly[2,6-4,8-di(5-ethylhexylthienyl)benzo[1,2-b;3,4-b]dithiophene-alt-5-dibutyloctyl-3,6-bis(5-bromothien-2-yl)pyrrolo[3,4-c]pyrrole-1,4-dione (PBDTT-DPP);Dithienylsilane-based polymers, such as poly[(4,4-bis(2-ethylhexyl)dithieno[3,2-b:2′,3′-d]siloxane)-2,6-diyl-alt-(4,7-bis(2-thienyl)-2,1,3-benzothiadiazole)-5,5′-diyl] (PSBTBT), 7,7′-(4,4-bis(2-ethylhexyl)-4H-silano[3,2-b:4,5-b′]dithiophene-2,6-diyl)bis(6-fluoro-4-(5′-hexyl-[2,2′-bithiophene]-5-yl)benzo[c][1,2,5]thiadiazole) (p-DTS(FBTTh2), poly[2,7-(9-thiophene)-2,1,3-benzothiadiazole]-5,5′-diyl] (PSBTBT), poly[(4,4-bis(2-ethylhexyl)dithieno[3,2-b:4,5-b′]dithiophene-2,6-diyl)bis(6-fluoro-4-(5′-hexyl-[2,2′-bithiophene]-5-yl)benzo[c][1,2,5]thiadiazole) (p-DTS(FBTTh2), poly[(2,7-(9-thiophene)-2,1,3-benzothiadiazole)-5,5′-diyl] (PSBTBT), poly[(4,4-bis(2-ethylhexyl)dithieno[3,2-b:4,5-b′]dithiophene-2,6-diyl)bis(6-fluoro-4-(5′-hexyl-[2,2′-bithiophene]-5-yl)benzo[c][1,2,5]thiadiazole) (p-DTS(FBTTh2), poly[(2 ,9-dioctyl-dibenzosiloxane)-alt-4,7-bis(thiophen-2-yl)benzo-2,1,3-thiadiazole (PSiFDTBT); benzodithiophene-based polymers, such as poly[4,8-bis[(2-ethylhexyl)oxy]benzo[1,2-b:4,5-b']dithiophene-2,6-diyl-alt-3-fluoro-2-[(2-ethylhexyl)carbonyl]thieno[3,4-b]thiophene-4,6-diyl] (PTB7), poly[(2,6-(4,8-bis(5-(2-ethylhexyl)thiophen-2-yl)-benzo[1,2-b:4,5-b']dithiophene))-alt-(5,5-(1',3'- di-2-thienyl-5',7'-bis(2-ethylhexyl)benzo[1',2'-c:4',5'-c']dithiophene-4,8-dione)))))), poly{2,6'-4,8-di(5-ethylhexylthienyl)benzo[1,2-b;3,4-b]dithiophene-alt-5-dibutyloctyl-3,6-bis(5-bromothien-2-yl)pyrrolo[3,4-c]pyrrole-1,4-dione (PBDTT-DPP), poly[4,8-bis(5-(2-ethylhexyl)thien-2-yl)benzo[1,2-b;4,5-b']dithiophene-2,6-diyl-alt-(4-(2-ethylhexyl)thien-2-yl)benzo[1,2-b;3,4-b]dithiophene-alt-5-dibutyloctyl-3,6-bis(5-bromothien-2-yl)pyrrolo[3,4-c]pyrrole-1,4-dione 4-(2-ethylhexyl)-3-fluorothieno[3,4-b]thiophene-)-2-carboxylate-2-6-diyl)] (PBDTT-FTTE), poly[(4,8-bis-(2-ethylhexyloxy)-benzo(1,2-b:4,5-b′)dithiophene)-2,6-diyl-alt-(4-(2-ethylhexanoyl)-thieno[3,4-b]thiophene-)-2-6-diyl)] (PBDTTT-CF), polybenzothiazol-oxazol(thiophene)-stat-benzodithiophene(thiophene)-8 (PBTZT-stat-BDTT-8), and other polymers, copolymers and small molecules having a maximum absorption between 320 nm and 800 nm;Polytriamine and its derivatives, poly[[2,5-bis(2-octyldodecyl)-2,3,5,6-tetrahydro-3,6-dioxopyrrolo[3,4-c]pyrrole-1,4-diyl]-alt2[[2,2'-(2,5-thiophene)bithieno[3,2-b]thiophene]-5,5'-diyl]](DPP(P)}, polyaniline (PANI), poly[(4,8-bis-(2-ethylhexyloxy)-benzo(1,2-b:4,5-b')bithieno)-2,6-diyl-alt-(4-(2-ethylhexanoyl)-thieno[3,4-b]thiophene)-2-6-diyl)](PBDTTT-C), poly[ N29-heptadecanyl-2,7-carbazole-alt-3,6-bis-(thiophen-5-yl)-2,5-dioctyl-2,5-dihydropyrrolo[3,4-]pyrrole-1,4-dione] (PCBTDPP), poly[[9-(1-octylnonyl)-9H-carbazole-2,7-diyl]-2,5-thiophenediyl-2,1,3-benzothiadiazole-4,7-diyl-2,5-thiophenediyl] (PCDTBT), poly[2,5-bis(2-octyldodecyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione-(E)-1,2-bis(2,2'-bithiophene-5-yl)ethylene] (PDPP DBTE), perfluoro(4-methyl-3,6-dioxo-7-ene)sulfonyl fluoride (PFI), poly(4-styrenesulfonate)-grafted polyaniline (PSS-g-PANI); 2'-butyloctyl-4,6-dibromo-3-fluorothieno[3,4-b]thiophene-2-carboxylate (TT-BO), 3',4'-dichlorobenzyl-4,6-dibromo-3-fluorothieno[3,4-b]thiophene-2-carboxylate (TT-DCB) and 2,6-bis(trimethyltin)-4,8-bis(2-ethylhexyloxy)benzo[1,2-b:4,5-b']dithiophene (BDT-EH) copolymer (PTB-DCB21), N2,N2,N2',N2',N7,N7,N7',N7'-octa(4-methoxyphenyl)-9,9'-spirobi[9H-fluorene]-2,2',7,7'-tetraamine (spiro-OMeTAD), poly[(9,9-dioctylfluorenyl-2,7-diyl)-co-(4,4'-(N-(4-sec-butylphenyl)diphenylamine)] (TFB), N4,N4'-di(naphthalene-1-yl)-N4,N4'-bis(4-vinylphenyl)biphenyl-4,4'-diamine (VNPB), 1,4-bis(4-sulfobutyloxy)benzene and thiophene part (PhNa-1T)); metal oxides, such as NiOx, MoOx, etc. ;
[0092] According to some embodiments, the detector further comprises a second layer between the first pixelated electrode layer and the first layer, wherein the second layer is an adhesion promoting layer. Such a second layer is not particularly limited, as long as such a second layer at least achieves better adhesion between the first pixelated electrode layer and the first layer, or between the first layer and the intermediate layer, or between the first pixelated electrode layer and the intermediate layer, in particular between the first pixelated electrode layer and the first layer, or at least between the first pixelated electrode layer and the tiles of the first layer.
[0093] The thickness of the second layer is not particularly limited and may be in the range between 100 nm and 1000 μm, for example in the range between 200 nm and 500 μm, for example in the range between 300 nm and 100 μm.
[0094] In some embodiments, the second layer is an anisotropic conductive film (ACF) or anisotropic conductive paste (ACP), however, in some embodiments, the second layer may require additional structured electrodes on the corresponding absorber patch and / or the second layer may require good alignment between the electrodes on the patch and the electrodes in the first pixelated electrode layer, for example on the backplane (substrate).
[0095] According to certain embodiments, the second layer includes at least a second semiconductor and / or conductor and / or a third perovskite.
[0096] According to some embodiments, the second layer includes a conductor, which is not particularly limited, for example in the form of bump bonds. These bump bonds are not particularly limited and can be made of, for example, suitable metals, such as conductive metals, such as Cu, Ag, Pb, Sn, In, etc. and their alloys, and / or these bump bonds can be made in any suitable form, such as in the form of balls, spheres, hemispheres, columns, cylinders, cubes, etc. According to some embodiments, the bump bonds can also be associated with glue, which can be introduced, for example, by a bottom filling process, but it is not excluded that the bump bonds are just surrounded by air, etc.
[0097] According to certain embodiments, the second layer comprises or even consists of a third perovskite, which may be the same or different from the first and / or second perovskite. In such a case, the second layer may be produced as a liquefied perovskite, applied accordingly, and recrystallized and / or applied with a paste and dried, as arranged with respect to the first perovskite. According to certain embodiments, as described above, the second layer is made of a recrystallized perovskite, for example liquefied with MA gas.
[0098] Therefore, the third perovskite is not particularly limited and may include any organic perovskite, inorganic perovskite and / or organic-inorganic perovskite and mixtures thereof. For example, suitable perovskites are described in WO 2014045021 A1, and reference is made to WO 2014045021 A1 regarding perovskites. The perovskite may have an ABX structure, such as an ABX3 structure, having one or more A cations, one or more B cations and one or more anions X, in particular, the A cations, B cations and anions X are selected from chalcogenides and / or halides, in particular halides, wherein,
[0099] The A cation and the B cation may be organic and / or inorganic - in particular, A is an organic cation selected from, for example, alkyl, aryl, aralkyl, alkylaryl, alkenyl, alkynyl groups having 1 to 20 carbon atoms; in particular, B is an inorganic cation, in particular selected from cations (in particular divalent cations) of metals such as Ca, Sr, Cd, Cu, Ni, Mn, Fe, Co, Pd, Ge, Sn, Pb and lanthanides such as Yb, Gd, Eu,
[0100] Suitable chalcogenides include oxides, sulfides, selenides, tellurides; and
[0101] Suitable halides include, for example, F - , Cl - Br - ,I - , especially Cl - Br - ,I - .
[0102] Suitable examples of tertiary perovskites include, for example, MAPbI3(CH3NH3PbI3), MAPbBr3(CH3NH3PbBr3), FAPbI3(HC(NH2)2PbI3), MAPbICl2(CH3NH3PbICl2), FAPbBr3(HC(NH2)2PbBr3), EAPbI3(CH3CH2NH3PbI3), PAPbI3(CH3CH2CH2NH3PbI3), BA2PbI4((CH3CH2CH2CH2NH3)2PbI4), PMA2PbI4((C6H5CH2NH3)2PbI4), PEA2PbI4((C6H5CH2NH3)2PbI4), 6H5CH2CH2NH3)2PbI4), EAPbBr3 (CH3CH2NH3PbBr3), PAPbBr3 (CH3CH2CH2NH3PbBr3); their other mixed halides; inorganic-organic perovskites with mixtures of A-cations and halides X (X=Cl, Br, I), such as MAFAPbX3 (MA=CH3NH3, FA=HC(NH2)2), MAGAPbX3 (GA=guanidine salt), BAPAPbX3 (BA=CH3CH2CH2CH2NH3, PA=CH3CH2CH2NH3), etc.; organic halogenated mixtures in which halogens can be replaced by other halogens (for example, formula I 3-x Cl x or Br 3-x Cl x Halides, such as MAPbI 3-x Cl x or CH3NH3PbBr 3-x Cl x ) is partially replaced; organic and / or inorganic perovskites, wherein Pb is at least partially or even completely replaced by Sn, Cu, Ni, Bi, Co, Fe, Mn, Cr, Cd, Ge and / or Yb and / or mixtures thereof; inorganic perovskites and mixtures thereof, such as CsPbX3, wherein X=Cl, Br and / or I, and mixtures thereof (e.g., CsPbBr3, CsPbI3, CsPbCl3); Cs3Bi2X9, wherein X=Cl, Br and / or I; =Cl, Br and / or I, and mixtures thereof; Cs3Sb2X, wherein X = Cl, Br and / or I, and mixtures thereof; Cs2AgBiX6, wherein X = Cl, Br and / or I, and mixtures thereof; Rb3Bi2X9, wherein X = Cl, Br and / or I, and mixtures thereof; Rb3Sb2X9, wherein X = Cl, Br and / or I, and mixtures thereof; CsSnI3; etc.; and mixtures of perovskites.
[0103] According to some embodiments, the detector for electromagnetic radiation comprises at least one intermediate layer between the first pixelated electrode and the second layer and / or between the second layer and the first layer, wherein the respective intermediate layer may be as described above. According to some embodiments, no intermediate layer exists between the first layer and the second layer.
[0104] According to some embodiments, the second layer is a structured layer including a structure and a material, the material including a second semiconductor and / or a conductor and / or a third perovskite at least filled in and / or surrounding the structure. In such an embodiment, the structure is not particularly limited and may be in the form of a grid, a column, etc. The structure therein is used as an anchoring structure, which can enhance the bonding between the first pixelated electrode layer and the second layer. According to some embodiments, the structure is as high as the other material of the second layer, or the other material, such as the second semiconductor and / or the conductor and / or the third perovskite, exceeds the structure by, for example, at least 10nm, at least 100nm, or even 1μm, or even 10μm, or even 30μm. The grid can be appropriately arranged on, for example, the first pixelated electrode layer for producing the structure using, for example, a resist, laser cutting, welding, etc. Suitable structures are described, for example, in EP 20155403.7, with reference to EP20155403.7 for the structure.
[0105] Figure 4 and Figure 5 It is schematically shown how an exemplary detector may be set up. Figure 4 There is shown an arrangement of two exemplary tiles having a first layer 2 (as described above, a radiation conversion layer including, for example, a semiconductor such as CdTe, a-Se, Si, GaAs, Ge, HgI2, PbO, a semiconducting perovskite or other semiconductor in the tile) between a first pixelated electrode layer 1 (e.g., in the form of an active matrix backplane having a suitable substrate (glass or silicon having, for example, a-Si, IGZO or CMOS TFT circuit system), which also includes a bottom electrode for each pixel) and a second electrode layer 3 (here representing a top electrode), the tiles 2 being separated by a gap 4, which represents a blind spot between the butted radiation conversion tiles in the prior art, and thus again illustrates the problem of the present invention. Figure 5 In the embodiment, the gap 4 is filled with a material including at least a first semiconductor and / or at least a first perovskite 5, for example a recrystallized first perovskite introduced as a liquefied perovskite. Since the material including at least a first semiconductor and / or at least a first perovskite can function as a semiconductor, the material can contribute to image generation. Figure 4 and Figure 5In the figure, it is shown how the problem of the present invention can be demonstrated by docking radiation conversion layer tiles on top of a backplane and filling the gaps between the radiation conversion tiles with, for example, a recrystallized radiation conversion layer (semiconductor), thereby completely eliminating the dead zones between the tiles.
[0106] Figure 6 Possible embodiments of the first pixelated electrode layer 1 are schematically shown. In variant A with an anchored grid structure shown as a view, the first pixelated electrode layer 1 has: a substrate 11, such as glass, silicon and / or plastic; a pixel circuit system 12, such as a thin film transistor as an active matrix drive scheme with a storage capacitor; a pixelated (structured) bottom electrode 13; and a structure 14, which acts as a grid anchoring structure for connection to the radiation detection layer. In variant B without an anchored grid structure, this structure 14 is missing. Therefore, Figure 6 Possible schematic diagrams of a radiation image sensor (eg, an X-ray imager and / or a gamma ray imager) backplate cross-section with and without an anchoring grid structure are shown.
[0107] Figure 7 and Figure 8 Then, the use of the second layer 6 as an adhesion promoting layer is schematically shown. Figure 6 Variant B with substrate 11, pixel circuitry 12 and pixelated bottom electrode 13 is applied to Figure 4 and Figure 5 , i.e., a schematic diagram showing a cross section of a possible radiation image sensor (X-ray imager and / or gamma-ray imager) with a butted direct conversion layer and a semi-dead space between tiles in the first layer 2 (in this figure, a butted conversion layer with two tiles). In this arrangement, since the second layer 6 can be semiconducting and floating, the pixels corresponding to the gaps between the absorber tiles are already able to deliver a signal upon irradiation, so Figure 7 The gap 4 in forms a semi-dead area, because the signal will be low but not zero. Figure 7 and Figure 8 In addition, there is a package 7 for protecting the second electrode layer 3. Figure 5 In the embodiment of the present invention, the interspaces 4 are then filled again with a material comprising at least a first semiconductor and / or at least a first perovskite 5 , for example a recrystallized first perovskite introduced as a liquefied perovskite.
[0108] Fig. 9 and Fig.10 Shows the Figure 6 Variant A is applied to Figure 4 and Figure 5 Detector. Fig. 9 The setting corresponds to Figure 7 Settings, Fig.10 The setting corresponds to Figure 8 The settings, except for structure 14 in Fig. 9 and Fig.10 The two settings in the present invention are present in the second layer 6, so as to further anchor the second layer 6 to the first pixelated electrode layer, thereby achieving better bonding between the second layer 6 and the first pixelated electrode layer.
[0109] Furthermore a detector for electromagnetic radiation, in particular an X-ray detector and / or a gamma-ray detector, of a third aspect is described, the detector comprising:
[0110] - a first pixelated electrode layer comprising a plurality of electrode pixels,
[0111] a first layer comprising a plurality of tiles comprising a material that absorbs and converts electromagnetic radiation, wherein the first layer may comprise gaps between the tiles, and
[0112] - a second electrode layer,
[0113] The detector also includes a second layer between the first pixelated electrode layer and the first layer, wherein the second layer is an adhesion promoting layer, preferably wherein the second layer includes at least a second semiconductor and / or conductor and / or a third perovskite, optionally, the detector for electromagnetic radiation of the third aspect includes at least one intermediate layer between the first pixelated electrode and the second layer and / or between the second layer and the first layer.
[0114] In the detector of the third aspect, the tiles in the first layer may include at least a second perovskite as a material that absorbs and converts electromagnetic radiation.
[0115] The detector of the third aspect may further comprise at least one intermediate layer between the first pixelated electrode and the first layer and / or between the first layer and the second electrode layer, and further comprising other layers (eg encapsulation) as described with respect to the detector of the first aspect.
[0116] In the detector of the third aspect, the second layer may be a structured layer including a structure and a material including a second semiconductor and / or a conductor and / or a third perovskite at least filled in and / or surrounding the structure.
[0117] In the detector of the third aspect, the patch may have a size of 1x1 cm 2 Up to 50x50cm 2 Size within the range.
[0118] In the detector of the third aspect, the optional gaps between tiles have a width of 0.1 pixel pitch to 50 pixel pitch, wherein the length of the pixel pitch is between and including 10 μm and 1000 μm.
[0119] In the detector of the third aspect, the tilt angle between tiles of two adjacent tiles in the first layer is between 0° and 5° inclusive.
[0120] In the detector of the third aspect, the first pixelated electrode layer, the first layer, the tiles included therein, the second electrode layer, the second layer and the intermediate layer and their respective materials and any other layers and materials are as described with respect to the detector of the first aspect. In addition, the other embodiments described with respect to the detector of the first aspect are also applicable to the detector of the third aspect. With such a detector, improved adhesion between the first pixelated electrode layer and the tiles of the first layer is obtained. Therefore, the detector of the third aspect can be manufactured in the same manner as the detector of the first aspect, with the difference that the second layer is applied and the gaps between the tiles in the first layer are not filled.
[0121] In a second aspect, the invention relates to a method of producing a detector for electromagnetic radiation, in particular an X-ray detector and / or a gamma-ray detector, the method comprising:
[0122] - providing a first pixelated electrode layer comprising a plurality of electrode pixels,
[0123] - optionally, applying a second layer on the first pixelated electrode layer, wherein the second layer is an adhesion promoting layer, preferably wherein the second layer comprises at least a second semiconductor and / or conductor and / or a third perovskite,
[0124] - applying a plurality of tiles comprising a material that absorbs and converts electromagnetic radiation on the first pixelated electrode layer or optionally on the second layer, wherein gaps are formed between the tiles,
[0125] - applying a material comprising at least a first semiconductor and / or at least a first perovskite in the gap until the gap is filled, wherein the tiles and the filled gap form a first layer, and
[0126] - Applying a second electrode layer on the first layer.
[0127] In particular, using the present method, the detector for electromagnetic radiation of the present invention can be produced.Therefore, certain embodiments discussed with respect to the present detector for electromagnetic radiation also apply to the present method, and vice versa, the present method also applies to certain embodiments discussed with respect to the present detector for electromagnetic radiation.
[0128] In the present method, the step of providing a first pixelated electrode layer comprising a plurality of electrode pixels is not particularly limited, and the first pixelated electrode layer may be provided as described above with respect to the present detector.
[0129] Furthermore, the step of optionally applying a second layer on the first pixelated electrode layer is not particularly limited, wherein the second layer is an adhesion promoting layer, preferably wherein the second layer comprises at least a second semiconductor and / or conductor and / or a third perovskite. As described above, the second layer can be applied, for example, as a liquefied third perovskite, and recrystallized into a paste and hardened, etc., whereupon the final thickness of the second layer can be in the range between 100 nm and 1000 μm, for example in the range between 200 nm and 500 μm, for example in the range between 300 nm and 100 μm.
[0130] According to some embodiments, applying the second layer comprises: applying a structure; and filling and / or surrounding a material comprising a second semiconductor and / or conductor and / or a third perovskite at least in and / or around the structure. For example, as also described above with respect to the detector, the application of the structure is not particularly limited, and the application of the structure can be accomplished using lithography, welding, laser cutting, atomic layer deposition, etc. When the structure is applied, the structure can then be filled and / or surrounded (for example, when the structure comprises a column) by a material comprising a second semiconductor and / or conductor and / or a third perovskite, for example, by applying a liquefied perovskite and recrystallizing, applying a paste, etc.
[0131] Furthermore, the step of applying a plurality of tiles comprising a material that absorbs and converts electromagnetic radiation on a first pixelated electrode layer or optionally on a second layer is not particularly limited, wherein gaps are formed between the tiles and the tiles can be appropriately attached, for example by pressing, gluing or also by placing the tiles on a lower layer before they are hardened (for example, on the second layer before recrystallization or hardening).
[0132] According to certain embodiments, as described above, the tiles in the first layer include at least a second perovskite as a material that absorbs and converts electromagnetic radiation.
[0133] According to some embodiments, the size of the puzzle piece is 1x1cm 2 Up to 50x50cm 2 within the range.
[0134] According to certain embodiments, the number of tiles in the first layer is between 2 and 1000 and inclusive, preferably between 2 and 100 and inclusive, more preferably between 2 and 50 and inclusive.
[0135] According to certain embodiments, the tilt angle between tiles of two adjacent tiles in the first layer is between 0° and 5° inclusive. This enables good filling of the gap.
[0136] Furthermore, the thickness of the patch is not particularly limited, and for example may be between 10 μm and 10,000 μm, preferably between 50 μm and 3,000 μm, more preferably between 100 μm and 1,500 μm, for example between 100 μm and 1,000 μm.
[0137] According to some embodiments, the gaps between the tiles are completely filled. However, it is not excluded that a small amount of the gaps are not completely filled, for example if another layer (e.g. an intermediate layer) is arranged on top of the first layer, or if, for example, a metal in electrical contact with the second electrode layer is arranged on the material in the gaps in the case where the second electrode layer is arranged on top of the first layer. However, it is preferred that the material in the gaps has the same height / thickness as the thickness of the tiles. Furthermore, it is not excluded that the material in the gaps is porous, i.e. the material in the gaps has a certain porosity, for example less than 10 vol%, less than 5 vol%, or even less than 2 vol%, for example even less than 1 vol%, of the total volume of the material in the gaps.
[0138] In such a case, i.e. if the gap is not completely filled in terms of height, porosity etc., then preferably less than 10 vol%, preferably less than 5 vol%, more preferably less than 2 vol%, especially less than 1 vol% of the gap may not be filled. If the entire gap is filled, then the thickness of the material in the gap is preferably substantially the same as the thickness of the block.
[0139] According to some embodiments, the gap size g between tiles depends on the pixel pitch P g According to certain embodiments, the following applies:
[0140] P g / 100≤g≤P g *1000; preferably, P g / 10≤g≤P g *100; more preferably, P g ≤g≤P g *10.
[0141] According to certain embodiments, the gaps between tiles have a width of 0.1 pixel pitch to 50 pixel pitch, wherein the length of the pixel pitch is between and including 10 μm and 1000 μm.
[0142] In the present method, the step of applying a material comprising at least a first semiconductor and / or at least a first perovskite in the gap until the gap is filled is also not particularly limited, wherein the tiles and the filled gap form a first layer.
[0143] According to certain embodiments, the gap is filled with a liquid material, paste or powder comprising at least a first semiconductor and / or at least a first perovskite. As described above, the material comprising at least a first semiconductor and / or at least a first perovskite may be in the form of a liquid (e.g., as a solution), a liquid semiconductor or a liquefied perovskite, a paste or a solid (e.g., in the form of a powder), and the material is filled in the gap using a suitable applicator (e.g., a dispensing device). According to certain embodiments, the applicator that fills the gap between the tiles with a liquid semiconductor and / or a liquefied perovskite and / or a solution comprising at least a first semiconductor and / or at least a first perovskite is a dispensing robot, which may optionally be controlled by artificial intelligence to automatically detect the gap and fill the gap. According to certain embodiments, the material comprising at least a first semiconductor and / or at least a first perovskite may also be applied, for example, in the form of a liquid in several steps, for example, layer by layer, to appropriately fill the gap and / or achieve the desired layer thickness.
[0144] Finally, the step of applying the second electrode layer on the first layer is not particularly restricted.
[0145] According to certain embodiments, a surface layer such as glass and / or encapsulation may be applied on the second electrode layer opposite to the first layer for protection, which is not particularly limited.
[0146] According to some embodiments, the method further comprises: applying at least one intermediate layer between the first pixelated electrode layer and the optional second layer, and / or between the optional second layer and the first layer, or between the first pixelated electrode layer and the first layer, and / or between the first layer and the second electrode layer. The application of the intermediate layer is not particularly limited, and the intermediate layer can be made of materials as described above for the detector.
[0147] Exemplary methods of the present invention are Figures 11 to 14 is shown in Fig.11 In the embodiment, a portion of the first layer 2, which has two tiles as abutting conversion layers, is applied to the first pixelated electrode layer 1, optionally with a second layer (not shown) as an adhesion promoting layer between the first layer 2 and the first pixelated electrode layer 1, leaving a gap 4 between the abutting conversion layer tiles. Fig.12 In the embodiment of the present invention, the gap 4 is then filled with an exemplary liquid material comprising at least a first semiconductor and / or at least a first perovskite 5' using an applicator 5", and then Fig.13In the example, the liquefied perovskite is recrystallized, the solvent evaporates, etc., to harden the exemplary liquid material, so as to obtain a solid material including at least the first semiconductor and / or at least the first perovskite 5 in the gap, for example, by using a suitable time, temperature, atmospheric pressure, etc., and the applicator 5" is, for example, a dispensing device for filling the gap with the liquefied radiation conversion material (semiconductor). In the case of filling the gap with powder, glue, a top layer, etc. can be applied to close the gap. Thereafter, in Fig.14 In , the second electrode layer 3 is applied on top of the gap.
[0148] exist Figures 15 to 17 Another schematic top view of filling gaps in an exemplary radiation detector with four butted conversion layer tiles is shown in , which shows states before, during and after the process of filling the gaps between tiles using, for example, liquefied radiation conversion material as semiconductor. Fig.15 In the figure, a first pixelated electrode layer 1 is shown, for example in the form of an active matrix backplane substrate (glass or silicon with a-Si, IGZO or CMOS TFT circuitry), which also includes the bottom electrode for each pixel, to which a second layer 6 is applied as an adhesion promoting layer using, for example, a suitable semiconductor, and on top of the second layer 6 four tiles of the first layer 2 are applied as butt-jointed conversion layer tiles with gaps between the four tiles. Then, in Fig.15 In the gap, an exemplary liquid material comprising at least a first semiconductor and / or at least a first perovskite 5′ is then filled into the gap using an applicator 5″, which is, for example, a dispensing device for filling the gap with a liquefied radiation conversion material (semiconductor). After hardening, a material in a solid state, such as a recrystallized perovskite, is obtained in the gap.
[0149] If appropriate, the above embodiments may be combined arbitrarily. Other possible embodiments and implementations of the present invention also include combinations of features not explicitly mentioned above or below with respect to the examples of the present invention. In particular, those skilled in the art will also add corresponding aspects as improvements or additions to the corresponding basic forms of the present invention.
[0150] The present invention will now be described in detail with reference to several examples of the present invention. However, these examples are illustrative and do not limit the scope of the present invention.
[0151] On the first electrode layer with electrode pixels made of, for example, ITO or Pt, a structure is formed using SU-8 as a photoresist. During hardening, MAPI (CH3NH3PbI3) is filled in the structure, for example as a powder, liquefied using MA gas, and then recrystallized, thereby filling the structure. On top of the structure is placed, for example, Fig.15 4 soft sintered tiles made of MAPI (CH3NH3PbI3) are shown in the figure, with gaps formed between the tiles. The gaps are then filled with MAPI as a powder, liquefied using MA gas, or filled with MAPI in liquefied form, and the MAPI in the gaps is then recrystallized and hardened. A second electrode made of, for example, Cr, Ti or ITO is applied on top of the gaps.
[0152] The MAPI in the gaps is different from the MAPI in the soft sintered tiles in terms of morphology, and differences in grain size, grain boundaries, density and porosity can also be observed, and the material in the tiles and the material in the gaps can be clearly distinguished. Therefore, when the signal from the tiles and the signal from the material in the gaps are compared, the electrical signal (corresponding sensitivity) is also different. However, the material in the gaps still contributes to the signal in the imaging. In addition, the MAPI filled in the structure has a different morphology, etc. compared to the MAPI in the tiles.
[0153] In the present detector, tiles comprising radiation absorbing and converting materials can be used, which tiles can be produced at low cost using smaller pressing tools, for example when using a low-pressure hydraulic press and / or an isostatic press. In particular, when perovskites are used in the tiles, the tiles are easier to handle than large absorber layers due to their brittleness, resulting in better efficiency. Since the gaps between the tiles are then filled with semiconductors or even radiation absorbing materials, when the detector is used in imaging, no blind areas are obtained in the original image that produce defective lines, rows or columns, because the gaps are filled and no longer represent blind areas. With the detector, additionally higher sensitivity and resolution are also possible, since the tiles can be produced more easily and with higher precision.
Claims
1. A detector for electromagnetic radiation, the detector for electromagnetic radiation comprising: - a first pixelated electrode layer, the first pixelated electrode layer comprising a plurality of electrode pixels, a first layer comprising a plurality of tiles comprising a material that absorbs and converts electromagnetic radiation, wherein the first layer comprises gaps between the tiles, wherein the gaps are filled with a material comprising at least a first semiconductor and / or at least a first perovskite, and - A second electrode layer.
2. A detector for electromagnetic radiation according to claim 1, wherein: The tiles in the first layer include at least a second perovskite as a material that absorbs and converts electromagnetic radiation.
3. The detector for electromagnetic radiation according to claim 1 or 2, further comprising at least one intermediate layer between the first pixelated electrode layer and the first layer and / or between the first layer and the second electrode layer.
4. The detector for electromagnetic radiation according to claim 1 or 2, further comprising a second layer between the first pixelated electrode layer and the first layer, wherein The second layer is an adhesion promoting layer.
5. A detector for electromagnetic radiation according to claim 4, wherein: The second layer comprises at least a second semiconductor and / or conductor and / or a third perovskite.
6. A detector for electromagnetic radiation according to claim 4, wherein: The detector for electromagnetic radiation comprises at least one intermediate layer between the first pixelated electrode layer and the second layer and / or between the second layer and the first layer.
7. The detector for electromagnetic radiation according to claim 4, wherein: The second layer is a structured layer, which includes a structure and a material, wherein the material includes a second semiconductor and / or a conductor and / or a third perovskite at least filled in and / or surrounding the structure.
8. A detector for electromagnetic radiation according to claim 1 or 2, wherein: The size of the puzzle is 1x1 cm 2 Up to 50x50 cm 2 within the range.
9. A detector for electromagnetic radiation according to claim 1 or 2, wherein: The gaps between the tiles have a width of 0.1 pixel pitch to 50 pixel pitch, wherein the length of the pixel pitch is between and including 10 μm and 1000 μm.
10. A detector for electromagnetic radiation according to claim 1 or 2, wherein: The tilt angle between tiles of two adjacent tiles in the first layer is between 0° and 5°, inclusive.
11. The detector for electromagnetic radiation according to claim 1, wherein: The detectors for electromagnetic radiation include X-ray detectors and / or gamma ray detectors.
12. A method of producing a detector for electromagnetic radiation, comprising: - providing a first pixelated electrode layer comprising a plurality of electrode pixels, - applying a second layer on the first pixelated electrode layer, wherein the second layer is an adhesion promoting layer, wherein the second layer comprises at least a second semiconductor and / or conductor and / or a third perovskite, - applying a plurality of tiles comprising a material that absorbs and converts electromagnetic radiation on the first pixelated electrode layer or on the second layer, wherein gaps are formed between the tiles, - applying a material comprising at least a first semiconductor and / or at least a first perovskite in the gap until the gap is filled, wherein the tiles and the filled gap form a first layer, and - Applying a second electrode layer on said first layer.
13. The method according to claim 12, wherein: The tiles in the first layer include at least a second perovskite as a material that absorbs and converts electromagnetic radiation.
14. The method according to claim 12 or 13, wherein: Applying the second layer comprises: applying a structure; and filling and / or surrounding a material comprising the second semiconductor and / or the conductor and / or the third perovskite at least in and / or around the structure.
15. The method according to claim 12 or 13, wherein: The size of the puzzle piece is 1x1cm 2 Up to 50x50 cm 2 within the range.
16. The method according to claim 12 or 13, further comprising: At least one intermediate layer is applied between the first pixelated electrode layer and the second layer and / or between the second layer and the first layer or between the first pixelated electrode layer and the first layer and / or between the first layer and the second electrode layer.
17. The method according to claim 12 or 13, wherein: The gaps between the tiles have a width of 0.1 pixel pitch to 50 pixel pitch, wherein the length of the pixel pitch is between and including 10 μm and 1000 μm, and / or wherein the gaps are filled with a liquid material, paste or powder comprising at least the first semiconductor and / or at least the first perovskite.
18. The method according to claim 12 or 13, wherein: Two adjacent tiles are applied in the first layer in such a way that the angle of inclination between the tiles is between 0° and 5° inclusive.
19. The method according to claim 12, wherein: The detectors for electromagnetic radiation include X-ray detectors and / or gamma ray detectors.
Citation Information
Patent Citations
Gas-induced perovskite formation
EP3304611B1
Radiation detector and manufacturing method for radiation detector
EP3376260A1
Pastes For Photoelectric Conversion Layers Of X-Ray Detectors, X-Ray Detectors And Methods Of Manufacturing The Same
US20120181440A1
Optoelectronic device
WO2014045021A1
Photodetector
CN104570041A