Semiconductor structure and method for manufacturing the same
By designing semiconductor structures with different work function layers in dynamic random access memory, and adjusting the electric field to suppress drain leakage current, the problem of gate-induced drain leakage current caused by device size reduction is solved, and the performance and integration of the device are improved. Accumulation.
Patent Information
- Application Number
- CN202110360937.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-04-02
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2041-04-02
AI Technical Summary
In dynamic random access memory devices, as the device size shrinks, the gate-induced drain leakage (GIDL) problem becomes serious, and it is difficult to effectively solve it with existing manufacturing methods.
A semiconductor structure is adopted, which includes a substrate, a buried gate structure, a first work function layer, a barrier layer and a second work function layer. By adjusting the work function of the second work function layer to be smaller than the first work function layer, Reduce the electric field, thereby suppressing the width of the gate channel and reducing drain leakage current. The specific method includes forming a gate dielectric layer on the sidewall and bottom surface of the trench, forming a first work function layer below, forming a barrier layer on the top surface, the second work function layer is located on the barrier layer, and removing part of the barrier layers to form voids and finally an insulating layer in the trench.
By reducing the electric field caused by the second work function layer, the drain leakage current caused by the gate is effectively suppressed, and the overall performance and integration of the device are improved.
Smart Images

Figure CN115172369B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a semiconductor structure and a manufacturing method thereof, and in particular to a semiconductor structure of a dynamic random access memory and a manufacturing method thereof. Background Art
[0002] Dynamic Random Access Memory (DRAM) devices are widely used in consumer electronic products. In order to increase the device integration within the DRAM device and improve its overall performance, the current manufacturing technology of the DRAM device continues to strive towards the miniaturization of the device size. However, as the device size continues to shrink, many challenges arise. For example, improving gate induced drain leakage (GIDL). Therefore, the industry still needs to improve the manufacturing method of the DRAM device to overcome the problems caused by the reduction of device size. Summary of the invention
[0003] The present invention discloses a semiconductor structure, comprising: a substrate and a buried gate structure arranged in the aforementioned substrate. The buried gate structure includes a gate dielectric layer, a first work function layer, a barrier layer and a second work function layer. The gate dielectric layer is located on the sidewall and bottom surface of a groove in the aforementioned substrate. The first work function layer is located in the groove and contacts the sidewall and bottom surface of the aforementioned gate dielectric layer. The barrier layer is located on the top surface of the first work function layer. The second work function layer is located above the barrier layer, and the sidewall of the second work function layer is separated from the gate dielectric layer by a distance. The semiconductor structure further includes an insulating layer located in the groove and located on the aforementioned second work function layer.
[0004] The present invention discloses a method for manufacturing a semiconductor structure, comprising providing a substrate, and forming a groove extending downward in the substrate; forming a gate dielectric layer on the sidewall and bottom surface of the groove; forming a first work function layer on the lower sidewall and bottom surface of the gate dielectric layer and in the lower part of the groove; forming a barrier material layer on the upper sidewall of the gate dielectric layer and the top surface of the first work function layer; forming a second work function material layer on the barrier material layer; recessing the second work function material layer to form a second work function layer on the barrier material layer and exposing a portion of the barrier material layer located on the upper sidewall of the gate dielectric layer; removing a portion of the barrier material layer to form a barrier layer between the second work function layer and the first work function layer, and forming a gap between the sidewall of the second work function layer and the gate dielectric layer; and forming an insulating layer in the groove and located on the second work function layer.
[0005] The semiconductor structure and manufacturing method proposed in the present invention have a second work function layer with a work function different from that of the first work function layer, wherein the work function of the second work function layer is smaller than the work function of the first work function layer, thereby reducing the electric field induced by the second work function layer in the substrate, thereby adjusting the width of the gate channel to suppress the gate-induced drain leakage current. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] Figure 1A-1F Schematic cross-sectional views corresponding to different intermediate stages of manufacturing a semiconductor structure according to an embodiment of the present invention;
[0007] Figure 2 is a cross-sectional schematic diagram of an intermediate stage of manufacturing a semiconductor structure according to another embodiment of the present invention;
[0008] Figure 3 is a cross-sectional schematic diagram of an intermediate stage of manufacturing a semiconductor structure according to another embodiment of the present invention;
[0009] Figure 4 A schematic cross-sectional view of an intermediate stage of manufacturing a semiconductor structure according to another embodiment of the present invention;
[0010] Figure 5 is a cross-sectional schematic diagram of an intermediate stage of manufacturing a semiconductor structure according to an embodiment of the present invention;
[0011] Figure 6 is a top view schematic diagram of a memory device according to an embodiment of the present invention;
[0012] Figure 7 Based on Figure 6 Schematic diagram of the cross section drawn by the section line 7-7 in the figure.
[0013] 100: Base
[0014] 102: Shallow Trench Isolation Structure
[0015] 103: Groove
[0016] A A :Active Zone
[0017] BL: Bit Line
[0018] 104: word line group
[0019] 104A, 104B: buried word lines
[0020] 106: bottom surface of doped region
[0021] 107: Capacitor contact
[0022] 109: Bit line contact
[0023] 111: Mask layer
[0024] 100a,102a,111a,115a,117a,123a: Top surface
[0025] 103s,112s,117s,120s,123s: side wall
[0026] 103b,112b,117b: bottom
[0027] 112: Gate dielectric layer
[0028] 112s-2: Lower sidewall of gate dielectric layer
[0029] 112s-1: Upper sidewall of gate dielectric layer
[0030] 115: First barrier layer
[0031] WF-1: First work function layer
[0032] 117: Conductive layer
[0033] 119: Barrier material layer
[0034] 120: Second barrier layer
[0035] 122: second work function material layer
[0036] 123: Second work function layer
[0037] 125,125': Gap
[0038] 125G: Air Gap
[0039] 126,127: Insulation
[0040] 128: Insulation layer
[0041] 605: Insulation cover
[0042] 607: Spacer
[0043] 610: interlayer insulation layer
[0044] t1, t2: thickness
[0045] D1,D2,D3: Direction DETAILED DESCRIPTION
[0046] The present invention is more fully described with reference to the drawings of the embodiments of the present invention. However, the present invention may be embodied in various forms and should not be limited to the embodiments described herein. The thickness of layers and regions in the drawings are exaggerated for clarity. The same or similar device numbers represent the same or similar devices, and the following paragraphs will not be repeated one by one.
[0047] Figure 1A-1F 2 is a schematic cross-sectional view corresponding to different intermediate stages of manufacturing a semiconductor structure according to an embodiment of the present invention. Figure 6 is a top view schematic diagram of a memory device according to an embodiment of the present invention. Figure 1A-1F It corresponds to Figure 6 The cross-section line 7-7 is drawn in FIG.
[0048] Please refer to Figure 1A , a substrate 100 is provided, the substrate 100 includes a trench 103 extending downward, and a gate dielectric layer 112 is provided on the sidewall 103s and the bottom surface 103b of the trench 103. The material of the substrate 100 may include, for example, a semiconductor material. In one embodiment, the substrate 100 includes silicon, gallium arsenide, gallium nitride, silicon germanium, other suitable materials or a combination thereof. In other embodiments, the substrate 100 is a substrate with silicon on an insulating layer.
[0049] In one embodiment, a mask material layer may be formed on the substrate 100, and the mask material layer may be patterned to form a mask layer 111. The mask layer 111 may include, for example, silicon oxide or other suitable materials. The mask layer 111 may include, for example, tetraethoxysilane (TEOS). Then, the mask layer 111 is used as an etching mask, and the mask layer 111 and the substrate 100 below are etched and filled with isolation materials to form a plurality of active regions A surrounding the active regions A. A The shallow trench isolation structure 102 (such as Figure 6 Active area A A Then, at the position corresponding to the subsequent word line formation, the mask layer 111 and the underlying substrate 100 are etched to form trenches 103, wherein adjacent trenches 103 are in the direction D1 ( Figure 6 ), and each groove 103 extends horizontally along the direction D3 in the substrate 100 and extends downward along the direction D2.
[0050] Back to Figure 1A, then, a gate dielectric layer 112 is formed on the sidewalls 103s and the bottom surface 103b of the trench 103. The gate dielectric layer 112 may be formed by a thermal oxidation process, a deposition process, any suitable process, or a combination of the foregoing. In one embodiment, for example, a thermal oxidation process is performed on the silicon-containing substrate 100 to form a silicon oxide layer on the sidewalls 103s and the bottom surface 103b of the trench 103 as the gate dielectric layer 112. In other embodiments, for example, a polysilicon liner (including the sidewalls covering the mask layer 111) may be first formed in the trench 103 of the substrate 100, and then a thermal oxidation process is performed to oxidize the polysilicon liner to form the gate dielectric layer 112.
[0051] In one embodiment, the gate dielectric layer 112 may be a single-layer structure or a multi-layer structure, and its material may include silicon oxide, silicon nitride, other suitable materials or a combination thereof. For example, the gate dielectric layer 112 may be a silicon oxide / silicon nitride / silicon oxide structure (ONO structure), or a NONON structure. To simplify the diagram, a single-layer gate dielectric layer 112 is depicted for ease of description. In one example, the gate dielectric layer 112 is a silicon oxide layer.
[0052] Afterwards, a first work function layer WF-1 is formed in the lower portion of the trench 103. The first work function layer WF-1 may include a single layer or multiple layers of material, such as a single layer of metal layer, or a combination of a metal nitride layer and a metal layer. In this embodiment, the first work function layer WF-1 includes, for example (but not limited to), a first barrier layer 115 and a conductive layer 117. Figure 1A A first barrier material layer (not shown) may be conformably deposited on the substrate 100 and the gate dielectric layer 112 of the trench 103, and then a conductive material layer (not shown) may be formed on the substrate 100 and the first barrier material layer to fill the trench 103. Thereafter, the first barrier material layer and the conductive material layer outside the trench 103 may be removed by, for example, a chemical mechanical polishing (CMP) process, an etching back process, or other suitable processes. Thereafter, the first barrier material layer and the conductive material layer within the trench 103 may be recessed by, for example, a selective etching process, and the first barrier material layer and the conductive material layer remaining in the lower portion of the trench 103 may form a first barrier layer 115 and a conductive layer 117, respectively, and a top surface 115a of the first barrier layer 115 and a top surface 117a of the conductive layer 117 may be substantially coplanar.
[0053] like Figure 1AAs shown, the first barrier layer 115 and the conductive layer 117 are formed in the lower portion of the trench 103 and constitute the first work function layer WF-1. The first barrier layer 115 contacts the gate dielectric layer 112 and is formed between the gate dielectric layer 112 and the conductive layer 117. Specifically, the first barrier layer 115 is located between the lower sidewall 112s-2 and the bottom surface 112b of the gate dielectric layer 112 and the sidewall 117s and the bottom surface 117b of the conductive layer 117.
[0054] In one embodiment, the material of the first barrier layer 115 includes a conductive metal, such as a metal, a metal alloy, a metal nitride, or a metal silicide. In one embodiment, the material of the first barrier layer 115 includes titanium nitride (TiN), titanium silicon nitride (TiSiN), tantalum nitride (TaN), tungsten nitride (WN), tantalum (Ta), titanium (Ti), tungsten (W), ruthenium (Ru), aluminum (Al), or other suitable conductive materials. In one embodiment, the first barrier layer 115 can be formed by using a deposition process, such as a physical vapor deposition (PVD) process, a chemical vapor deposition (CVD) process, or an atomic layer deposition (ALD) process.
[0055] In one embodiment, the material of the conductive layer 117 includes a conductive metal, such as a metal, a metal alloy, a metal nitride, or a metal silicide. In one embodiment, the material of the conductive layer 117 includes tungsten, tantalum, titanium, ruthenium, aluminum, tungsten nitride, titanium nitride, titanium silicon nitride, tantalum nitride, or other suitable conductive materials. In one embodiment, the conductive layer 117 can be formed by using a deposition process, such as PVD, CVD, or ALD.
[0056] Then, if Figure 1B As shown, a barrier material layer 119 is conformally formed on the substrate 100 and the upper portion of the trench 103. In one embodiment, the barrier material layer 119 is formed on the upper sidewall 112s-1 of the gate dielectric layer 112, the top surface 115a of the first barrier layer 115, and the top surface 117a of the conductive layer 117. Figure 1B As shown, the barrier material layer 119 extends to above the substrate 100 , for example, extends to the top surface 111 a of the mask layer 111 .
[0057] In one embodiment, the first barrier layer 115 has a substantially uniform thickness, such as thickness t1; the barrier material layer 119 has a substantially uniform thickness, such as thickness t2. According to the manufacturing method proposed in the embodiment, the thickness t2 of the barrier material layer 119 defines the gap formed in the subsequent process (such as the subsequent Figure 1E , Figure 2The width of the gaps 125, 125' shown in the figure in the direction D1 further affects the distance between the buried gate structure and the gate dielectric layer 112 on the sidewall of the trench 103. The thicker the barrier material layer 119 is, the thicker the second work function layer (such as the one formed later) will be. Figure 1E , Figure 2 The greater the distance between the second work function layer 123 and the gate dielectric layer 112, the smaller the electric field induced by the second work function layer 123 in the substrate, which can narrow the channel width formed in the substrate, thereby suppressing gate-induced drain leakage current.
[0058] In one embodiment, the thickness t2 of the barrier material layer 119 is substantially equal to the thickness t1 of the first barrier layer 115. Figure 1B In other embodiments, the thickness t2 is greater than the thickness t1. In one example, the thickness t1 is, for example, in the range of 3.5 nm to 5.5 nm, such as 4 nm to 5 nm; the thickness t2 is, for example, in the range of 4.5 nm to 7.5 nm, such as 5 nm to 7 nm.
[0059] In one embodiment, the material of the barrier material layer 119 includes a conductive metal, such as a metal, a metal alloy, a metal nitride, or a metal silicide. In one embodiment, the material of the barrier material layer 119 includes titanium nitride, titanium silicon nitride, tantalum nitride, tungsten nitride, tantalum, titanium, tungsten, ruthenium, aluminum, or other suitable conductive materials. In one embodiment, the barrier material layer 119 can be formed by a deposition process, such as PVD, CVD, or ALD.
[0060] In one embodiment, the barrier material layer 119 and the first barrier layer 115 include the same conductive material. In other embodiments, the barrier material layer 119 and the first barrier layer 115 include different conductive materials. Furthermore, in one embodiment, the barrier material layer 119 is a material different from that of the conductive layer 117, and the work function of the barrier material layer 119 is smaller than that of the conductive layer 117. In one embodiment, the first barrier layer 115 and the barrier material layer 119 include titanium nitride, and the conductive layer 117 includes tungsten.
[0061] Then, if Figure 1C As shown, a second work function material layer 122, which includes, for example, a conductor material, is formed on the barrier material layer 119. The second work function material layer 122, for example, fills the remaining space of the trench 103 and directly contacts the barrier material layer 119. In one embodiment, the conductive layer 117 is isolated from the second work function material layer 122 by the barrier material layer 119; that is, the second work function material layer 122 does not contact the conductive layer 117.
[0062] In one embodiment, the second work function material layer 122 includes, for example, doped or undoped polysilicon, or metal, metal alloy, metal nitride, metal silicide, etc. In one embodiment, the material of the second work function material layer 122 includes polysilicon, titanium nitride, titanium silicon nitride, tantalum nitride, tungsten nitride, tantalum, titanium, tungsten, ruthenium, aluminum, or other suitable conductive materials. In one embodiment, the second work function material layer 122 can be formed by using a deposition process, such as PVD, CVD, ALD, etc.
[0063] In one embodiment, the second work function material layer 122 is different from the material of the first barrier layer 115, the material of the conductive layer 117 and the material of the barrier material layer 119. Furthermore, in one embodiment, the work function of the second work function material layer 122 is smaller than the work function of the conductive layer 117.
[0064] Then, if Figure 1D As shown, the second work function material layer 122 located above the substrate 100 is removed, and the second work function material layer 122 located in the groove 103 is recessed to form a second work function layer 123. In one embodiment, the second work function layer 123 formed corresponds to the top surface 117a of the conductive layer 117, and the second work function layer 123 and the conductive layer 117 are isolated from each other by a portion of the barrier material layer 119. In one embodiment, a portion of the second work function material layer 122 located outside the groove 103 can be removed by CMP, an etch-back process, a selective etching process, other suitable processes or a combination of the foregoing, and then a portion of the second work function material layer 122 located in the groove 103 is recessed to remove, so as to form the second work function layer 123. In one embodiment, the top surface 123a of the second work function layer 123 is not higher than the horizontal height of the bottom surface of the doped region (not shown) in the active region (for example, as the source / drain region) to increase the distance between the bottom of the doped region and the buried gate structure, thereby helping to reduce leakage current.
[0065] Then, if Figure 1E As shown, in one embodiment, a portion of the barrier material layer 119 is removed, and the remaining portion of the barrier material layer 119 forms a second barrier layer 120. The formed second barrier layer 120 is, for example, located between the second work function layer 123 and the conductive layer 117. Furthermore, after removing a portion of the barrier material layer 119, a gap 125 is formed between the sidewall 123s of the second work function layer 123 and the gate dielectric layer 112.
[0066] In one embodiment, the exposed portion of the barrier material layer 119 and at least a portion of the barrier material layer 119 between the sidewall 123s of the second work function layer 123 and the gate dielectric layer 112 may be removed to form a gap 125. In one embodiment, a selective etching process is used to remove the barrier material layer 119. For example, an etchant or etching gas that is selective to the material of the second work function layer 123 may be used to wet-etch or dry-etch the barrier material layer 119.
[0067] It is worth mentioning that the width of the gap 125 in the direction D1 is determined by the thickness t2 of the barrier material layer 119. Therefore, the distance between the second work function layer 123 and the substrate 100 in the direction D1 can be controlled by controlling the thickness t2, thereby controlling the electric field formed by the second work function layer 123 to suppress the path of GIDL.
[0068] In addition, the depth of the formed gap 125 can be appropriately controlled and adjusted according to actual application conditions. For example, in this embodiment, the gap 125 can completely expose the sidewall 123s (such as Figure 1E Specifically, the portion of the barrier material layer 119 not covered by the second work function layer 123 is completely removed, so that the gap 125 formed exposes a portion of the gate dielectric layer 112, all sidewalls 123s of the second work function layer 123, and the top surface 115a of the first barrier layer 115. In another embodiment, the gap 125 may only expose a portion of the sidewalls 123s of the second work function layer 123 (e.g., Figure 2 In other embodiments, the gap 125 may also extend downward to expose a portion of the sidewall 117s of the conductive layer 117 .
[0069] Please refer to Figure 1E After the aforementioned step of removing a portion of the barrier material layer 119, the sidewall 123s of the second work function layer 123 is substantially coplanar with the sidewall 120s of the formed second barrier layer 120. In addition, in one embodiment, after the aforementioned step of removing a portion of the barrier material layer 119, the conductive layer 117 is surrounded by the first barrier layer 115 and the second barrier layer 120.
[0070] Figure 2 FIG. 1 is a cross-sectional view of an intermediate stage of manufacturing a semiconductor structure according to another embodiment of the present invention. Figure 1E An alternative embodiment of the steps of Figure 1E Here, only a portion of the barrier material layer 119 located next to the sidewall 123 s of the second work function layer 123 may be removed. Therefore, the gap 125 ′ only exposes a portion of the sidewall 123 s of the second work function layer 123 .
[0071] Next, refer to Figure 1F , in forming a gap 125 ( Figure 1E ), an insulating layer 128 is formed in the trench 103 and above the second work function layer 123 to cover the second work function layer 123, the second barrier layer 120, and the first barrier layer 115. In this embodiment, the insulating layer 128 further fills the gap 125 between the sidewall 123s of the second work function layer 123 and the gate dielectric layer 112. In other embodiments, the insulating layer 128 may also partially fill the gap 125 or retain the complete gap 125 (such as Figure 3 In addition, in other embodiments, multiple layers of insulating material may be filled into the trench 103. That is, the insulating layer 128 includes multiple layers of insulating material (such as Figure 4 ).
[0072] The material of the insulating layer 128 includes, for example, nitride, oxide, other suitable dielectric materials, or a combination thereof. In one embodiment, the material of the insulating layer 128 includes silicon nitride, silicon oxide, other suitable materials, or a combination thereof. The insulating layer 128 may be a single layer or multiple layers of insulating material. In one embodiment, the insulating layer 128 includes an insulating material different from that of the gate dielectric layer 112. Furthermore, the insulating layer 128 may be formed by PVD, CVD, ALD, spin coating, other suitable processes, or a combination thereof.
[0073] Figure 3 FIG. 4 is a schematic cross-sectional view of an intermediate stage of manufacturing a semiconductor structure according to another embodiment of the present invention. Figure 4 FIG. 4 is a schematic cross-sectional view of an intermediate stage of manufacturing a semiconductor structure according to another embodiment of the present invention. Figure 3 and Figure 4 As Figure 1F An alternative embodiment of the steps of.
[0074] Please refer to Figure 3 , the insulating layer 128 formed here only partially fills or does not fill the gap 125, so there is an air gap 125G between the sidewall 123s of the second work function layer 123 and the gate dielectric layer 112, and the insulating layer 128 is located above the top surface 123a of the second work function layer 123 and the air gap 125G. In this embodiment, since the dielectric constant of air is higher than that of the insulating layer 128, Figure 1F For the embodiment of the present invention, the air gap 125G can further reduce the leakage current.
[0075] Please refer to Figure 4 , the insulating layer 128 formed here includes two insulating portions 126 and 127. Specifically, Figure 1EAfter the step of forming the insulating portion 126 on the substrate 100 and in the trench 103, the insulating portion 127 may be formed on the substrate 100 and in the trench 103 in a blanket manner. As shown in the figure, the insulating portion 126 is located in the trench 103 and on the second work function layer 123, and the insulating portion 126 fills the gap 125 between the sidewall 123s of the second work function layer 123 and the gate dielectric layer 112. The insulating portion 126 further covers the top surface 123a and the sidewall 123s of the second work function layer 123. In one embodiment, the insulating portion 126 and the insulating portion 127 may include different materials. For example, the insulating portion 126 is an oxide layer, and the insulating portion 127 is a nitride layer. In another embodiment, the insulating portion 126 may include the same insulating material as the gate dielectric layer 112, such as silicon oxide. In this embodiment, by forming a multi-layered insulating layer 128, insulating materials with different dielectric constants can be further selected to increase the dielectric constant of the insulating layer 128 as a whole. Figure 1F For the embodiment of the present invention, the leakage current can be further reduced.
[0076] Figure 5 is a cross-sectional schematic diagram of an intermediate stage of manufacturing a semiconductor structure according to an embodiment of the present invention. Figure 1F After forming the insulating layer 128, a planarization process may be performed to remove a portion of the insulating layer 128 until the top surface 111a of the mask layer 111 is exposed. Figure 5 As shown, after planarization, the first work function layer WF-1, the second work function layer 123, and the second barrier layer 120 located below the remaining insulating layer 128 in the trench 103 constitute the buried gate structure of the present invention. In this embodiment, the first work function layer WF-1 includes the first barrier layer 115 and the conductive layer 117. In other embodiments, the first work function layer WF-1 may also include only the conductive layer 117.
[0077] The buried gate structure of the embodiment of the present invention can be applied to a dynamic random access memory (DRAM) device as a buried word line. The following is an example to illustrate the subsequent process of manufacturing a DRAM device after forming the buried gate structure of the embodiment. Please refer to Figure 6 , Figure 7 . Figure 6 is a top view schematically showing a memory device according to an embodiment of the present invention, Figure 7 Based on Figure 6 Schematic diagram of the cross section drawn by the section line 7-7 in the figure.
[0078] Figure 6 , Figure 7 Zhongyu Figure 1A-1F , Figure 2-Figure 5The same or similar components are denoted by the same or similar reference numerals for the sake of clarity. Figure 7 The buried gate structure shown is based on the aforementioned Figure 5 The buried gate structure is described below, but the present invention is not limited thereto.
[0079] like Figure 6 As shown, the memory device includes a substrate 100, a plurality of shallow trench isolation structures 102, a plurality of active regions A A , a plurality of bit lines BL, a plurality of word line groups 104, a plurality of capacitor contacts 107 and a plurality of bit line contacts 109. A plurality of doped regions are formed in the substrate 100 as active regions A. A , each active area A A The substrate 100 is generally arranged along a direction D1 (eg, the X direction) and forms an angle with the direction D1. A In this embodiment, the active region A A The plurality of lines are alternately formed in a wave-like manner in the direction D1 , but the present invention is not limited thereto.
[0080] A plurality of bit lines BL are formed above the substrate 100, each bit line BL extends along a direction D1, and adjacent bit lines BL are arranged in a direction D3. A plurality of word line groups 104 are formed in the substrate 100, each extending along a direction D3. In one embodiment, each word line group 104 has two buried word lines 104A and 104B, and adjacent buried word lines 104A and 104B are arranged in a direction D1. The cross-sectional structure of each buried word line 104A / 104B is similar to Figure 5 The buried gate structure shown is the same and will not be described again here.
[0081] like Figure 6 As shown, each active area A A Across a corresponding word line group 104 (eg, including buried word lines 104A and 104B), each active region A A has an overlapping area (eg, active area A) with the corresponding bit line BL. A In each active area A A Each of the two non-overlapping regions with the bit line BL has a capacitor contact 107 electrically connected to the capacitor (not shown) above. Each capacitor contact 107 is located between two adjacent bit lines BL. In one embodiment, the capacitor contact 107 is located on the substrate 100 and contacts a portion of the upper surface of the doped region of the substrate 100. For example Figure 6 , Figure 7 As shown, corresponding to an active area A AThe two capacitor contacts 107 are respectively arranged in the active area A A The two sides of the word line group 104 are electrically connected to the doped regions (active region A) adjacent to the two sides of the word line group 104. A ). Therefore, the capacitor contact 107 contacts the doped region of the substrate 100 to serve as the source / drain region of the memory device.
[0082] like Figure 6 , Figure 7 As shown, each active area A A A bit line contact 109 is provided at the overlapped region with the bit line BL. In one embodiment, the bit line contact 109 is buried between the insulating layer 128 of two adjacent buried word lines 104A and 104B, wherein the bottom surface of the bit line contact 109 is in contact with the doped region of the substrate 100. The manufacturing method of the bit line contact 109 is, for example, to form an opening between the insulating layer 128 of the two adjacent buried word lines 104A and 104B, and the aforementioned opening exposes a portion of the doped region of the substrate 100, then deposit polysilicon on the substrate and in the aforementioned opening, and then deposit one or more conductive materials such as titanium, tungsten, tantalum, titanium nitride, tungsten nitride, and an insulating material such as silicon nitride, and then deposit photoresist and mask materials and perform photolithography and etching processes to form a stacked structure including the bit line contact 109, the bit line BL and the insulating cap layer 605. It is worth mentioning that the polysilicon located in the aforementioned opening serves as the bit line contact 109, and the bit line BL located on the bit line contact 109 may include one or more conductive materials such as titanium, tungsten, tantalum, titanium nitride, tantalum nitride, tungsten nitride, etc., and the bit line BL extends along the direction D1.
[0083] like Figure 6 , Figure 7 As shown, each bit line BL can be electrically connected to the corresponding two buried word lines 104A and 104B by a bit line contact 109 when crossing the corresponding word line group 104. For example, the bottom of the bit line contact 109 contacts the upper surface of the doped region of the substrate 100 between the two word lines.
[0084] Furthermore, if Figure 7As shown, spacers 607 (whose materials include, for example, one or more materials such as silicon oxide, silicon nitride, and air gaps) may be formed on the sidewalls of the insulating cap layer 605 and the bit line BL. For example, after the aforementioned photolithography and etching process, a liner (such as silicon nitride) may be conformably deposited on the substrate and dry-etched to form spacers 607 on the sidewalls of the insulating cap layer 605 and the bit line BL. Next, after the insulating material is fully formed on the substrate, a planarization process is performed using the insulating cap layer 605 as a stop layer to form an interlayer insulating layer 610 on both sides of the bit line BL. Thereafter, a contact hole (not shown) penetrating the interlayer insulating layer 610 and the mask layer 111 is formed by processes such as photolithography and etching to expose a portion of the doped region of the substrate 100. Next, one or more conductive materials including polysilicon, titanium nitride or tungsten are deposited in the contact hole, and excess conductive materials on the interlayer insulating layer 610 are removed by, for example, CMP to form the capacitor contact 107. In one embodiment, the capacitor contact 107, the bit line contact 109, the bit line BL, and the insulating cap layer 605 are formed in the interlayer insulating layer 610, and the top surface of the capacitor contact 107 and the top surface of the insulating cap layer 605 can be substantially coplanar with the top surface of the interlayer insulating layer 610.
[0085] In summary, the semiconductor structure and manufacturing method thereof proposed in the present invention have a second work function layer 123 with a work function different from that of the first work function layer WF-1, wherein the work function of the second work function layer 123 is smaller than the work function of the first work function layer WF-1, thereby reducing the electric field induced by the second work function layer 123 in the substrate, thereby adjusting the width of the gate channel to suppress the gate-induced drain leakage current.
[0086] In addition, the present invention can further control the distance between the second work function layer 123 and the substrate 100 by controlling the width of the gap 125 / 125' (i.e., the thickness t2 of the barrier material layer), thereby adjusting the electric field induced by the second work function layer 123 in the substrate to suppress the gate-induced drain leakage current. In addition, the present invention can also form dielectrics of different structures above the second work function layer 123 and between the second work function layer 123 and the substrate 100 to suppress the gate-induced drain leakage current. For example, a single-layer structure (such as Figure 1E Insulating layer 128) or a multi-layer structure (such as Figure 3 The air gap 125G and the insulating layer 128, or Figure 4 The dielectric of the insulating portion 128 including the insulating portions 126 and 127 is used to suppress the gate induced drain leakage current.
[0087] Although the present invention has been described above with several preferred embodiments, they are not intended to limit the present invention. Any person skilled in the art may make any changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention shall be determined by the scope of the appended claims.
Claims
1. A semiconductor structure, characterized in that: include: a base; A buried gate structure is disposed in the substrate, and the buried gate structure includes: a gate dielectric layer disposed on the sidewalls and bottom surface of a trench in the substrate; a first work function layer located in the trench and contacting the sidewall and bottom surface of the gate dielectric layer; a barrier layer located on a top surface of the first work function layer; and a second work function layer, located above the barrier layer, and a sidewall of the second work function layer is spaced a distance from the gate dielectric layer; and an insulating layer located in the trench and on the second work function layer; An air gap is provided between the side wall of the second work function layer and the gate dielectric layer, and the insulating layer is located on the top surface of the second work function layer and above the air gap.
2. The semiconductor structure according to claim 1, wherein: The insulating layer is filled in a part of the gap between the side wall of the second work function layer and the gate dielectric layer and is located above the air gap.
3. The semiconductor structure according to claim 1, wherein: The insulation layer comprises: a first insulating portion, located in the trench and on the second work function layer, and the first insulating portion fills a gap between the sidewall of the second work function layer and the gate dielectric layer; as well as A second insulating portion is located in the groove and on the first insulating portion.
4. The semiconductor structure according to claim 3, characterized in that The first insulating portion further covers the top surface and the side wall of the second work function layer, and the second insulating portion and the second work function layer are separated from each other by the first insulating portion.
5. The semiconductor structure according to claim 3, wherein: The first insulating portion includes the same material as the gate dielectric layer, and the first insulating portion and the second insulating portion include different materials.
6. The semiconductor structure according to claim 1, wherein: The first work function layer comprises: a first barrier layer located in the trench and on the sidewalls and the bottom surface of the gate dielectric layer; and a conductive layer located in the trench, and the first barrier layer surrounds the sidewall and bottom surface of the conductive layer, The barrier layer located on the top surface of the first work function layer is a second barrier layer.
7. The semiconductor structure according to claim 6, wherein: The work function of the second barrier layer is smaller than the work function of the conductive layer, but larger than the work function of the second work function layer.
8. A method for manufacturing a semiconductor structure, characterized in that: include: Providing a substrate, and forming a groove extending downward in the substrate; forming a gate dielectric layer on the sidewalls and bottom surface of the trench; forming a first work function layer on the lower sidewall and bottom surface of the gate dielectric layer and in the lower portion of the trench; forming a barrier material layer on the upper sidewall of the gate dielectric layer and the top surface of the first work function layer; forming a second work function material layer on the barrier material layer; recessing the second work function material layer to form a second work function layer on the barrier material layer and exposing a portion of the barrier material layer located on the upper sidewall of the gate dielectric layer; removing a portion of the barrier material layer to form a barrier layer between the second work function layer and the first work function layer, and forming a gap between a sidewall of the second work function layer and the gate dielectric layer; and An insulating layer is formed in the trench and on the second work function layer.
9. The method for manufacturing a semiconductor structure according to claim 8, wherein: When the second work function material layer is formed on the barrier material layer, the second work function material layer directly contacts the aforementioned portion of the barrier material layer located on the upper sidewall of the gate dielectric layer.
10. The method for manufacturing a semiconductor structure according to claim 8, wherein: The insulating layer fills the gap between the side wall of the second work function layer and the gate dielectric layer.
11. The method for manufacturing a semiconductor structure according to claim 8, wherein: The insulation layer comprises: a first insulating portion, located in the trench and on the second work function material layer, and the first insulating portion fills the gap between the sidewall of the second work function layer and the gate dielectric layer, and the first insulating portion further covers the top surface and the sidewall of the second work function layer; and A second insulating portion is located in the trench and on the first insulating portion, wherein the second insulating portion and the second work function layer are separated from each other by the first insulating portion.
12. The method for manufacturing a semiconductor structure according to claim 8, wherein: An air gap is provided between the side wall of the second work function layer and the gate dielectric layer, and the insulating layer is located on the top surface of the second work function layer and above the air gap.
13. The method for manufacturing a semiconductor structure according to claim 8, wherein: Forming the first work function layer includes: A first barrier layer is formed on the lower sidewall and the bottom surface of the gate dielectric layer, and a conductive layer is formed in the lower portion of the trench, and the first barrier layer surrounds the sidewall and the bottom surface of the conductive layer, wherein the first barrier layer and the conductive layer form the first work function layer, The barrier material layer is formed on the upper sidewall of the gate dielectric layer, the top surface of the first barrier layer and the top surface of the conductive layer, The barrier layer formed after removing part of the barrier material layer is a second barrier layer.
14. The method for manufacturing a semiconductor structure according to claim 13, wherein: The work function of the barrier material layer is smaller than the work function of the conductive layer, but larger than the work function of the second work function material layer.
Citation Information
Patent Citations
Semiconductor device, method for manufacturing the same, memory cell and electronic device
CN106935650A
Memory transistor, word line structure of memory transistor and word line preparing method
CN110610940A