Method for forming fin-type structure on deep trench of semiconductor device
By forming a fin structure on the deep trench of the semiconductor device, the short circuit and polysilicon residue problems when the deep trench capacitor is combined with a fin type FET of several nanometers are solved, and the formation and functional speed of high-density units are achieved.
Patent Information
- Application Number
- CN202210803940.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-01
- Filing Date
- 2022-07-07
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2042-07-07
AI Technical Summary
The prior art is difficult to prevent short circuits and polysilicon residues when deep trench capacitors are combined with fin type FET transistors of several nanometer-level, especially under the requirements of increased integration density and functional speed. The existing processes are complex and difficult to achieve high Density unit.
By forming a fin-shaped structure on the deep trench of the semiconductor device, a multi-step process includes patterning fins, cutting fins, liner layer and masking treatments, forming side walls to prevent short circuits and remove polysilicon residues, including providing burial The oxide layer, patterned fins, cut fins, set up a liner layer and mask to remove the polysilicon fence to form the side wall.
The space between the deep trench and the fin type FET is effectively expanded, the stacking control requirements are reduced, the short circuit is prevented, the polysilicon residue is removed, and the integration density and functional speed are improved.
Smart Images

Figure CN115172374B_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present disclosure relate to a method for forming a semiconductor device, and more particularly, to a method for forming a fin structure of a volatile memory. Background Art
[0002] Deep trench capacitors (DTCs) are vertical semiconductor devices used to provide capacitance for various integrated circuits. Compared to packaging the package, the advantage of using DTCs is that they can be freely set or embedded as close to the target circuit as possible. In addition, DTCs can also provide higher capacitance per unit area.
[0003] Silicon-based integrated circuits, such as those containing field effect transistors (FETs) or metal oxide semiconductor FETs (MOSFETs), have been striving to provide higher speeds, higher integration densities, and more optimized functions. Fin-type FET transistors, i.e. FET transistors whose channels are formed in raised "fins" of semiconductor material, are expected to support the reduction of channel lengths to less than 50nm, and possibly even to about 10nm, thereby achieving further improvements in integration density and functional speed.
[0004] In the case where a deep trench capacitor is designed to be combined with a transistor (such as a fin FET) at a few nanometers level, it is extremely difficult to improve performance by combining the current fin FET with the deep trench capacitor when the SOI semiconductor process is reduced from 14nm to 10nm.
[0005] Furthermore, when deep trench capacitors are designed to be combined with transistors (such as fin-type FETs) fabricated at a level below tens of nanometers, it is important to have a good mechanism to prevent short circuits between deep trench capacitors or to prevent deep trench polysilicon from shorting with the deep trench sidewalls in order to meet design specification requirements.
[0006] In other aspects, a memory cell is usually formed by electrically combining a logic circuit with a memory so that data storage, writing or deletion of the memory can be achieved by controlling the logic circuit. Such a logic circuit can be a transistor and is arranged near the memory. It is known that there are various problems in the development of a groove sidewall vertical device dynamic random access memory (DRAM) cell. For example, since the groove sidewall vertical device DRAM cell requires space, it is difficult to realize a high-density cell. In addition, the groove sidewall vertical device DRAM cell is prone to bit line short circuit.
[0007] As transistor density increases and transistor channel length decreases, the alignment between the fin structure patterning mask and the fin structure above the deep trench becomes critical. For situations where the space margin between the deep trench sidewall and the fin structure of the fin FET is small, overlay control is critical. Even when the fin structure patterning mask is slightly offset, it will cause spatial asymmetry, resulting in polysilicon residue during etching.
[0008] In addition, the current fin structure cycle process uses complex process steps including a fin structure removal process / a deep trench plug formation process / an ONO cap formation process to prevent short circuits between deep trenches and between deep trenches and polysilicon.
[0009] The U.S. patent application with publication number US2007 / 0048947A1 discloses a multi-structure silicon fin structure and a manufacturing method thereof, but the prior art only discloses how to manufacture a fin-type FET with a sidewall, does not mention a deep trench, and is not suitable for embedded dynamic random access memory (eDRAM). The U.S. patent with patent number US6620699 discloses a method for forming a nitride inner sidewall of a deep trench device DRAM cell. However, there are problems, for example, it does not solve the problem of polysilicon residue. The U.S. patent application with publication number US2005 / 0064635A1 discloses a method for preventing oxide undercutting during the metal silicide pre-cleaning process of a thin sidewall FET, but is not suitable for eDRAM.
[0010] Therefore, it is hoped to have a fin-type structure and a method for forming a fin-type structure, which can allow a large deep trench space or even an opening to be formed between the deep trench sidewall and the fin structure of the fin-type FET, reduce the stacking control requirements, prevent short circuits between deep trenches or between deep trenches and polysilicon, and enable the side walls formed on the sides of the fin-type structure to help remove polysilicon residues and overcome the problem of polysilicon residues. Summary of the invention
[0011] In view of the above-mentioned shortcomings of the prior art, the present invention provides a method for forming a fin structure on a deep trench (DT) of a semiconductor device.
[0012] According to an embodiment of the present disclosure, a method for forming a fin-type structure on a deep trench (DT) of a semiconductor device is provided, wherein the DT includes a first DT, a second DT paired with the first DT, and a third DT adjacent to the second DT, and the method includes the following steps: providing a buried oxide layer (BOX) containing the DT and polysilicon in the DT; providing a patterned fin on the BOX and the polysilicon, wherein the patterned fin extends on the first, second and third DTs, and the polysilicon has a polysilicon fence adjacent to the patterned fin; setting a first mask on the patterned fin; cutting off the Patterning the portion of the fin between the second and third DTs to form a cut fin; setting a pad layer on the BOX and the first mask, wherein the pad layer has a first portion above the cut fin, a second portion on the side of the cut fin, and a third portion on the first and second DTs and the BOX; setting a second mask on the first and second portions of the pad layer; removing the second mask and the third portion of the pad layer to expose the first and second portions of the pad layer; and removing the polysilicon fence and forming a sidewall on the side of the cut fin.
[0013] According to another embodiment of the present disclosure, a method for forming a fin structure on a deep trench (DT) of a semiconductor device is provided, wherein the DT includes a first DT, a second DT paired with the first DT, and a third DT adjacent to the second DT. The method includes the following steps: providing a buried oxide layer (BOX) containing the DT and polysilicon in the DT; providing a patterned fin on the BOX and the polysilicon, wherein the patterned fin extends on the first, second and third DTs, and the polysilicon has a polysilicon fence adjacent to the patterned fin; setting a first mask on the patterned fin; cutting off the portion of the patterned fin between the second and third DTs to form a cut fin between the first and second DTs; setting a first pad layer on the BOX and the first mask; setting a second pad layer on the first pad layer, wherein each of the first pad layer and the second pad layer has a first portion above the top of the cut fin, a second portion on the side of the cut fin, and a third portion above the first and second DTs and the BOX; setting a second mask on the first and second portions of the second pad layer; removing the second mask and the third portion of the first and second pad layers to expose the second portion of the second pad layer; and removing the polysilicon fence and forming a sidewall on the side of the cut fin.
[0014] According to another embodiment of the present disclosure, a method for forming a fin structure on a deep trench (DT) of a semiconductor device is provided. The method includes the following steps: providing a buried oxide layer (BOX) containing the DT and polysilicon in the DT; providing a fin structure on the BOX and the polysilicon, wherein the polysilicon has a polysilicon fence adjacent to the fin structure; providing a first liner layer on the fin structure; providing a liner layer on the BOX and the first mask, wherein the liner layer has a first portion above the fin structure, a second portion on the side of the fin structure, and a third portion on the DT and the BOX; providing a second mask on the first and second portions of the liner layer; removing the second mask and the third portion of the liner layer to expose the first portion and the second portion of the liner layer; and removing the polysilicon fence and forming a sidewall on the side of the fin structure.
[0015] For those skilled in the art, the above-mentioned embodiments and advantages of the present invention will become more clearly understood after referring to the following detailed description and accompanying drawings: BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figures 1A to 1F A schematic diagram of a method for forming a fin structure on a deep trench of a semiconductor device according to a preferred embodiment of the present disclosure;
[0017] FIG. 2A to FIG. 2E A schematic diagram of a method for forming a fin structure on a deep trench of a semiconductor device according to another preferred embodiment of the present disclosure;
[0018] FIG. 3A to FIG. 3F It is a schematic diagram of a method for forming a fin structure on a deep trench of a semiconductor device according to another preferred embodiment of the present disclosure. DETAILED DESCRIPTION
[0019] When reading the following detailed description, please refer to all the drawings of the present invention, wherein all the drawings of the present invention show different embodiments of the present invention by way of example, and are intended to help those skilled in the art understand how to implement the present invention. The embodiments provided by the examples here are sufficient to show the spirit of the present invention, each embodiment does not conflict with other embodiments, and new embodiments can be realized by any combination of these embodiments, that is, the present invention is not limited to the embodiments disclosed in this specification.
[0020] Please refer to Figures 1A to 1F , which is a schematic diagram of a method for forming a fin structure FS on deep trenches (DT) 101 , 102 of a semiconductor device 10 according to a preferred embodiment of the present disclosure. Figure 1C , Figure 1D and Figure 1FEach of the embodiments has a top view and a cross-sectional view of a semiconductor device 10, wherein DT 101, 102 includes a first DT 101 and a second DT 102. Therefore, these embodiments should not be construed as limited to the specific number of DTs shown herein, but are intended to include, for example, DT number requirements resulting from manufacturing. The method includes the following steps: Figure 1A As shown, a buried oxide layer (BOX) 100 having DTs 101, 102 and polysilicon 101P, 102P located in the DTs 101, 102 is provided. Figure 1A As shown, a patterned fin FIN is provided on the BOX 100 and the polysilicon 101P, 102P, wherein the patterned fin FIN extends over the first and second DTs 101, 102, and as shown in FIG. Figure 1D As shown, the polysilicon 101P and 102P have a polysilicon fence PF adjacent to the patterned fin FIN. Figure 1A As shown in FIG. 1 , a first mask MSK1 is disposed on the patterned fin FIN. Figure 1B As shown, the cut fin CFIN is formed by cutting off the portion POT of the patterned fin FIN located between the second and first DT 102, 101. Figure 1C As shown, a liner layer LIN is disposed on BOX 100 and the first mask MSK1, wherein the liner layer LIN has a first portion PAT1 located above the cut fin CFIN, a second portion PAT2 located on the side LS of the cut fin CFIN, and a third portion PAT3 located on the first and second DTs 101, 102 and BOX 100. Figure 1D As shown, a second mask MSK2 is provided on the first and second parts PAT1, PAT2 of the pad layer LIN. Figure 1E As shown, the second mask MSK2 and the third portion PAT of the pad layer LIN are removed to expose the first portion PAT1 and the second portion PAT2 of the pad layer LIN. Figure 1F As shown, the polysilicon fence PF is removed to form a sidewall SPC on the side surface LS of the cut fin CFIN.
[0021] In any embodiment of the present disclosure, the first mask MSK1 includes a SiN hard mask, and the method further includes the step of removing the third portion PAT3 of the pad layer LIN by performing a wet etching process.
[0022] Please refer to Figure 1D In any embodiment of the present disclosure, the second mask MSK2 includes a fin structure removal process mask for protecting the cut fin CFIN and has a width MSKW2 in the range of 50-80 nm. The second mask MSK2 is used to remove the polysilicon fence PF.
[0023] In any embodiment of the present disclosure, the method further includes a process of aligning the second mask MSK2 with the cut fin CFIN by an overlay control process, wherein an opening OPN is provided between the side LS of the cut fin CFIN and the DT 101, 102, such as Figure 1F In addition, by enlarging the opening OPN, the opening OPN is made large enough to be, for example, Figures 1D to 1F Remove the fence residue PFR in DT 101, 102 of the cut fin CFIN.
[0024] Please refer to Figure 1C In any embodiment of the present disclosure, the liner layer LIN includes an oxide liner layer with a thickness LINT of 2 to 4 nm, and the opening OPN can be adjusted and scaled in size by the thickness of the oxide liner layer.
[0025] In any embodiment of the present disclosure, the step of removing the polysilicon fence PF is performed by a reactive ion etching (RIE) process, such as a non-uniform directional etching process.
[0026] Please refer to Figure 1A In any embodiment of the present disclosure, each of the DTs 101 , 102 has a diameter DIM in the range of 50 nm to 100 nm, and a depth DTD in the range of 2 to 5 μm.
[0027] Please refer to Figure 1C In any embodiment of the present disclosure, the cut fin CFIN has a thickness FINT in the range of 10-20 nm, a height FINH in the range of 30-50 nm, and a width FINW in the range of 150-400 nm.
[0028] Please refer to Figure 1F In any embodiment of the present disclosure, each sidewall SPC has a width SPCW in the range of 10 to 30 nm, and by providing the sidewall SPC, the polysilicon fence PF is effectively removed.
[0029] In any embodiment of the present disclosure, the cutting of the fin structure FIN may be performed before or after the sidewall SPC is formed.
[0030] In any embodiment of the present disclosure, the method further comprises the step of removing the first portion PAT1 of the pad layer LIN by wet etching.
[0031] Please refer to FIG. 2A to FIG. 2E , which is a schematic diagram of a method for forming a fin structure FS on deep trenches (DT) 201 , 202 of a semiconductor device 20 according to another preferred embodiment of the present disclosure. Figure 2C , Figure 2D and Figure 2E Each of the embodiments has a top view and a cross-sectional view of a semiconductor device 20, wherein DT 201, 202 includes a first DT 201 and a second DT 202. Therefore, these embodiments should not be understood as being limited to the specific number of DTs shown herein, but are intended to include, for example, DT number requirements resulting from manufacturing. The method includes the following steps: Figure 2A As shown, a buried oxide layer (BOX) 200 having DTs 201, 202 and polysilicon 201P, 202P located in the DTs 201, 202 is provided. Figure 2A As shown, a patterned fin FIN is provided on the BOX 200 and the polysilicon 201P, 202P, wherein the patterned fin FIN extends over the first, second and third DTs 201, 202, and as shown in FIG. Figure 2D As shown, the polysilicon 201P and 202P have a polysilicon fence PF adjacent to the patterned fin FIN. Figure 2A As shown in FIG. 1 , a first mask MSK1 is disposed on the patterned fin FIN. Figure 2B As shown, a portion of the patterned fin FIN located between the second and first DTs 202 and 201 is cut off to form a cut fin CFIN located between the first and second DTs 201 and 202. Figure 2C In the embodiment, a first pad layer LIN1 is disposed on BOX200 and the first mask MSK1. Figure 2C As shown, a second pad layer LIN2 is disposed on the first pad layer LIN1, wherein each of the first pad layer LIN1 and the second pad layer LIN2 has a first portion PAT1 located on the top of the cut fin CFIN, a second portion PAT2 located on the side LS of the cut fin CFIN, and a third portion PAT3 located on the first and second DTs 201, 202 and the BOX 200. Figure 2D As shown, a second mask MSK2 is disposed on the first and second parts PAT1, PAT2 of the second pad layer LIN2. Figure 2E As shown, the second mask MSK2 and the third portion PAT3 of the first and second pad layers LIN1, LIN2 are removed to expose the second portion PAT2 of the second pad layer LIN2. Figure 2E As shown, the polysilicon fence PF is removed, and a sidewall SPC is formed on the side surface LS of the cut fin CFIN.
[0032] In any embodiment of the present disclosure, if Figure 2DAs shown, a step of removing the third portion PAT3 of the second liner layer LIN2 is performed by a wet etching process or reactive ion etching (RIE) with an undercut UCUT around the second portion PAT2 of the second liner layer LIN2 in DT 201, 202. In addition, a step of removing the polysilicon fence PF is performed by RIE.
[0033] Please refer to Figure 2C In any embodiment of the present disclosure, the first liner layer LIN1 includes a SiN liner layer with a thickness LINT1 in the range of 2 to 4 nm, the second liner layer LIN2 includes an oxide liner layer with a thickness LINT2 in the range of 2 to 4 nm, and the first mask MSK1 includes a SiN hard mask.
[0034] Please refer to Figure 2D In any embodiment of the present disclosure, the second mask MSK2 includes a fin structure removal process mask for protecting the cut fin CFIN and has a width MSKW2 in the range of 50-80 nm. The second mask MSK2 is used to remove the polysilicon fence PF.
[0035] Please refer to Figure 2D In any embodiment of the present disclosure, the method further comprises the following steps: controlling the alignment of the second mask MSK2 and the cut fin CFIN through an overlay control process, wherein: Figure 2E As shown, there is an opening OPN between the side and the DT. In addition, by enlarging the opening OPN, the opening OPN is made large enough to remove the fence residue PFR in the DT 201 and 202.
[0036] Please refer to Figure 2C and Figure 2E In any embodiment of the present disclosure, the opening OPN may be adjusted and scaled by the thickness LINT2 of the second liner layer LIN2, and the step of removing the polysilicon fence PF is performed by a reactive ion etching (RIE) process.
[0037] Please refer to Figure 2E In any embodiment of the present disclosure, by providing a sidewall SPC, the polysilicon fence PF is effectively removed.
[0038] Please refer to FIG. 3A to FIG. 3F , which is a schematic diagram of a method for forming a fin structure FS on deep trenches (DT) 301, 302 of a semiconductor device 30 according to another preferred embodiment of the present disclosure. Therefore, these embodiments should not be understood as being limited to the specific number of DTs shown here, but are intended to include, for example, DT number requirements resulting from manufacturing. Figure 3B , Figure 3C and Figure 3EEach of them has a top view and a cross-sectional view of the semiconductor device 30. The method comprises the following steps: Figure 3A As shown, a buried oxide layer (BOX) 300 having DTs 301, 302 and polysilicon 301P, 302P located in the DTs 301, 302 is provided. Figure 3A As shown, a fin structure FIN is provided on BOX 300 and polysilicon 301P, 302P, wherein FIG. 3B to FIG. 3C As shown, the polysilicon 301P, 302P has a polysilicon fence PF adjacent to the fin structure FIN. Figure 3A As shown in FIG. 1 , a first mask MAK1 is disposed on the fin structure FIN. Figure 3B As shown, a liner layer LIN is disposed on BOX 300 and the first mask MSK1, wherein the liner layer LIN has a first portion PAT1 located above the fin structure FIN, a second portion PAT2 located on the side LS of the fin structure FIN, and a third portion PAT3 located on DT 301, 302 and BOX 300. Figure 3C As shown, a second mask MSK2 is provided on the first and second parts PAT1, PAT2 of the pad layer LIN. Figure 3D As shown, the second mask MSK2 and the third portion PAT3 of the pad layer LIN are removed to expose the first portion PAT1 and the second portion PAT2 of the pad layer LIN. Figure 3E As shown, the polysilicon fence PF is removed, and a sidewall SPC is formed on the side surface LS of the fin structure FIN.
[0039] In any embodiment of the present disclosure, the method further comprises the following steps: aligning the second mask MSK2 with the fin structure FIIN through an overlay control process, wherein an opening OPN is provided between the side LS and the DT 301 , 302 of the fin structure FIN, for example Figure 3E In addition, by enlarging the opening OPN, the opening OPN is large enough to be, for example, FIG. 3B to FIG. 3E The fence residue PFR in DT 301 and 302 of the fin structure FIN is removed.
[0040] In any embodiment of the present disclosure, the method further comprises the step of removing the third portion PAT3 of the pad layer LIN by a wet etching process.
[0041] Please refer to Figure 3F In any embodiment of the present disclosure, the method further comprises the following step: removing the polysilicon fence PF by a reactive ion etching (RIE) process. In addition, the portion of the fin structure FIN between DT 301 and 302 is cut off to form a cut fin CFIN.
[0042] Please refer to Figure 3C , in any embodiment of the present disclosure, if Figure 3C As shown, the second mask MSK2 includes a fin structure removal process mask for protecting the fin structure FIN, and has a width FINW in the range of 50 to 80 nm. In addition, the second mask MSK2 is used to remove the polysilicon fence PF.
[0043] Please refer to Figure 3B and Figure 3E In any embodiment of the present disclosure, the liner layer LIN includes an oxide liner layer having a thickness LINT in the range of 2 to 4 nm, and the opening OPN can be adjusted and scaled by the thickness LINT of the oxide liner layer.
[0044] Please refer to FIG. 3A to FIG. 3B In any embodiment of the present disclosure, each of the DTs 301 , 302 has a diameter DIM in the range of 50 nm to 100 nm, and a depth DTD in the range of 2 to 5 μm.
[0045] Please refer to FIG. 3B to FIG. 3C In any embodiment of the present disclosure, the fin structure FIN has a thickness FINT in the range of 10 to 20 nm, a height FINH in the range of 30 to 50 nm, and a width in the range of 200 to 300 nm.
[0046] Please refer to Figure 3E In any embodiment of the present disclosure, each sidewall SPC has a width SPCW in the range of 10 to 30 nm. By providing the sidewall SPC, the polysilicon fence PF is effectively removed.
[0047] Although the present invention has been described above by what is currently considered to be the most practical and preferred embodiment, it should be understood that the present invention is not necessarily limited to the disclosed embodiment. On the contrary, it is intended to cover various modifications and similar structures included in the spirit and scope of the following claims, and the spirit and scope should be consistent with the broadest interpretation to cover all such modifications and similar structures.
Claims
1. A method for forming a fin structure on a deep trench of a semiconductor device, wherein: The deep trench comprises a first deep trench and a second deep trench, and the method comprises the following steps: Providing a buried oxide layer, wherein the buried oxide layer has the deep trench, and polysilicon is arranged in the deep trench; providing a patterned fin on the buried oxide layer and the polysilicon, wherein the patterned fin extends over the first deep trench and the second deep trench, and the polysilicon has a polysilicon fence adjacent to the patterned fin; disposing a first mask on the patterned fin; cutting away a portion of the patterned fin between the second deep trench and the first deep trench to form a cut fin; Disposing a liner layer on the buried oxide layer and the first mask, wherein the liner layer has a first portion located above the cut fin, a second portion located on a side of the cut fin, and a third portion located on the first deep trench, the second deep trench and the buried oxide layer; disposing a second mask on the first portion and the second portion of the liner layer; removing the second mask and the third portion of the liner layer to expose the first portion and the second portion of the liner layer; and removing the polysilicon fence and forming a sidewall on the side of the cut fin, The method further comprises the steps of: By performing an overlay control process, the second mask is aligned with the cut fin, wherein an opening is provided between the side surface of the cut fin and the deep trench; and The opening is enlarged so that the opening is large enough to remove fence residues within the deep trench of the cutting fin.
2. The method according to claim 1, characterized in that The first mask comprises a SiN hard mask, and the method further comprises: The third portion of the liner layer is removed by performing a wet etching process.
3. The method according to claim 1, characterized in that: The second mask includes a fin structure removal process mask for protecting the cut fin and has a width in the range of 50 to 80 nm; The second mask is used to remove the polysilicon fence.
4. The method according to claim 1, characterized in that: The liner layer comprises an oxide liner layer having a thickness in the range of 2 to 4 nm; The opening may be adjusted and scaled in size by the thickness of the oxide liner layer.
5. The method according to claim 4, characterized in that The step of removing the polysilicon fence is performed by a reactive ion etching process.
6. The method according to claim 1, characterized in that The diameter of each of the deep trenches is within a range of 50 nm to 100 nm, and the depth is within a range of 2 to 5 μm.
7. The method according to claim 1, characterized in that The cut fin has a thickness in the range of 10 to 20 nm, a height in the range of 30 to 50 nm, and a width in the range of 150 to 400 nm.
8. The method according to claim 1, characterized in that: The width of each of the sidewalls is in the range of 10 to 30 nm; By providing the sidewall spacer, the polysilicon fence can be effectively removed.
9. A method for forming a fin structure on a deep trench of a semiconductor device, wherein: The deep trench comprises a first deep trench and a second deep trench, and the method comprises the following steps: Providing a buried oxide layer, wherein the buried oxide layer has the deep trench, and polysilicon is arranged in the deep trench; providing a patterned fin on the buried oxide layer and the polysilicon, wherein the patterned fin extends over the first deep trench and the second deep trench, and the polysilicon has a polysilicon fence adjacent to the patterned fin; disposing a first mask on the patterned fin; Cutting off a portion of the patterned fin between the second deep trench and the first deep trench to form a cut fin between the first deep trench and the second deep trench; Disposing a first liner layer on the buried oxide layer and the first mask; Disposing a second liner layer on the first liner layer, wherein each of the first liner layer and the second liner layer has a first portion located above the top of the cut fin, a second portion located on a side of the cut fin, and a third portion located above the first deep trench, the second deep trench and the buried oxide layer; disposing a second mask on the first portion and the second portion of the second liner layer; removing the second mask and the third portions of the first liner layer and the second liner layer to expose the second portion of the second liner layer; and removing the polysilicon fence and forming a sidewall on the side of the cut fin, The method further comprises the steps of: By performing an overlay control process, the second mask is controlled to be aligned with the cutting fin, wherein an opening is provided between the side surface and the deep trench; and The opening is enlarged so that the opening is large enough to remove fence residues within the deep trench.
10. The method according to claim 9, characterized in that: The step of removing the third portion of the second liner layer is performed by a wet etching process with an undercut near the second portion of the second liner layer in the deep trench, or by reactive ion etching; and The step of removing the polysilicon fence is performed by the reactive ion etching.
11. The method according to claim 9, characterized in that: The first liner layer comprises a SiN liner layer having a thickness in the range of 2 to 4 nm; The second liner layer comprises an oxide liner layer having a thickness in the range of 2 to 4 nm; The first mask includes a SiN hard mask.
12. The method according to claim 9, characterized in that: The second mask includes a fin structure removal process mask for protecting the cut fin and has a width in the range of 50 to 80 nm; The second mask is used to remove the polysilicon fence.
13. The method according to claim 9, characterized in that: The opening can be adjusted and sized by the thickness of the second liner layer, and the step of removing the polysilicon fence is performed by a reactive ion etching process.
14. The method according to claim 9, wherein: By providing the sidewall spacer, the polysilicon fence can be effectively removed.
15. A method for forming a fin structure on a deep trench of a semiconductor device, characterized in that: The steps include: Providing a buried oxide layer, wherein the buried oxide layer has the deep trench, and polysilicon is arranged in the deep trench; providing a fin structure on the buried oxide layer and the polysilicon, wherein the polysilicon has a polysilicon fence adjacent to the fin structure; Disposing a first mask on the fin structure; Disposing a liner layer on the buried oxide layer and the first mask, wherein the liner layer has a first portion located above the fin structure, a second portion located on a side of the fin structure, and a third portion located on the deep trench and the buried oxide layer; disposing a second mask on the first portion and the second portion of the liner layer; removing the second mask and the third portion of the liner layer to expose the first portion and the second portion of the liner layer; and removing the polysilicon fence and forming a sidewall on the side of the fin structure, The method further comprises the steps of: By performing an overlay control process, the second mask is aligned with the fin structure, wherein an opening is provided between the side surface and the deep trench; and The opening is enlarged so that the opening is large enough to remove fence residues within the deep trench.
16. The method according to claim 15, characterized in that The method further includes the following step: removing the third portion of the liner layer through a wet etching process.
17. The method according to claim 15, characterized in that The following steps are also included: Removing the polysilicon fence by a reactive ion etching process; and The portion of the fin structure between the deep trenches is cut away to form a cut fin.