Surface treatment method for low-adsorption plastic pipette tips

The hydrophobic surface with a multi-layer structure is formed through etching and multi-layer spraying processing, which solves the problems of high cost and low use efficiency of low-adsorption plastic pipette tips, improves the surface quality and service life of the tip, reduces costs and improves efficiency. Material utilization.

CN115256781BActive Publication Date: 2024-10-22ZHEJIANG MANWINI BIOTECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210854359.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-14
Publication Date
2024-10-22
Estimated Expiration
2042-07-14

AI Technical Summary

Technical Problem

The existing low-adsorption plastic pipette tips are high in cost, low in efficiency, easy to waste materials, and need to be replaced frequently to avoid contamination and affect experimental accuracy.

Method used

Etching is used to form a multi-layer hydrophobic surface, and the hydrophobicity and service life of the tip are improved through injection molding, etching, inert drying, spray filling, plasma treatment and circulation treatment, and surface grinding.

Benefits of technology

Through multi-layer structure processing, the surface quality of the suction head is improved, materials are saved, the service life is extended, the cost is reduced, the utilization rate of materials is improved, and surface adhesion and contamination are avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115256781B_ABST
    Figure CN115256781B_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of surface treatment of low-adsorption plastic pipette tips, and specifically to a surface treatment method of low-adsorption plastic pipette tips. The treatment method comprises the following steps: injection molding, etching treatment, inert drying, spray filling, plasma treatment and circulation treatment, and surface polishing. The beneficial effects are: corrosion treatment of a plastic pipette tip is achieved by etching, and a multi-layered hydrophobic surface of the pipette tip is formed by multiple cycles of spraying, thereby saving materials and improving the utilization rate of materials while achieving the premise of improving the surface quality of the pipette tip. At the same time, the outer surface of the pipette tip is fully treated through the multi-layer treatment to avoid surface adhesion due to wear, thereby greatly improving the service life of the pipette tip, reducing costs, and improving the utilization rate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of surface treatment of low-adsorption plastic pipette tips, in particular to a surface treatment method of low-adsorption plastic pipette tips. Background Art

[0002] Low-adsorption plastic pipette tips are mostly made of hydrophobic plastic and are molded by injection molding.

[0003] The existing patent application number is CN202110215342.5, which is a surface treatment method for ultra-low adsorption pipette tips, and the patent application number is CN202111368792.4, which is a surface treatment method for achieving low adsorption plastic pipette tips. Both disclose methods for surface treatment of tips made of hydrophobic materials.

[0004] However, in actual use, pipette tips are consumable products. In order to avoid contamination and improve the accuracy of the experiment for different liquids, most of the pipette tips need to be replaced. Therefore, the use of hydrophobic materials to prepare complete pipette tips is costly, inefficient, and easily leads to waste of materials. Summary of the invention

[0005] The object of the present invention is to provide a surface treatment method for a low-adsorption plastic pipette tip, so as to solve the problem of surface hydrophobicity treatment of the pipette tip made of plastic material.

[0006] To achieve the above object, the present invention provides the following technical solutions: 1. A surface treatment method for a low-adsorption plastic pipette tip, characterized in that the treatment method comprises the following steps:

[0007] Injection molding, the plastic raw material is melted and extruded into a mold, and a conical plastic pipette tip is obtained by cooling;

[0008] Etching treatment: Place the plastic pipette tip that has been injection molded and cooled to room temperature in the etching solution for 2-4 minutes;

[0009] Inert drying: Place the etched plastic pipette tip in an inert gas environment, rinse with water, and then air dry;

[0010] Spray filling, spray the hydrophobic coating on the etched outer wall of the plastic pipette tip, after spraying, dry at high temperature and then cool to room temperature;

[0011] Plasma treatment: the sprayed plastic pipette tip is placed in a plasma surface treatment device, and a mixed gas of carbon dioxide and nitrogen is injected to ionize the surface of the spraying position;

[0012] Circular treatment, spraying the treated plastic pipette tip again and drying and cooling it, and placing the plastic pipette tip in the plasma surface treatment device again for treatment after cooling, and the cycle is repeated 3-4 times;

[0013] Surface grinding: When the spray coating thickness is flush with the outer surface of the upper end of the plastic pipette tip, grind the outer wall of the plastic pipette tip.

[0014] Preferably, the depth of the plastic pipette tip in the etching solution is three quarters of the height of the plastic pipette tip itself, and the etching solution is a corrosive solution that slowly corrodes the outer wall of the plastic.

[0015] Preferably, the surface of the plastic pipette tip is polished to a mirror-like smoothness, and the surface is rinsed with clean water after polishing.

[0016] Preferably, the single spraying thickness during the spray filling process does not exceed one third of the etching depth, and the hydrophobic spray coating is a silicon dioxide powder mixture.

[0017] Preferably, the high-temperature drying temperature after spray filling is 80-100 degrees Celsius, the baking position is the etched position of the sprayed plastic pipette tip, and the unetched position of the plastic pipette tip is separated by multiple groups of insulation rings.

[0018] Preferably, the temperature of the reaction chamber in the plasma surface treatment device is 25° C., the vacuum degree is 0.3 mbar, the power is 1.5 kW, and the treatment time is 20 min.

[0019] Preferably, the high temperature drying treatment is carried out by circulating hot air drying or infrared radiation drying.

[0020] Preferably, the time for flushing with clean water during the inert drying process is 5-10 minutes, and the time for flushing with clean water during the surface polishing process is 2-3 minutes.

[0021] Compared with the prior art, the present invention has the following beneficial effects:

[0022] The present invention implements corrosion treatment on a plastic pipette tip by etching, and then forms a multi-layered hydrophobic surface of the pipette tip by multiple cycles of spraying, thereby saving materials and improving material utilization while achieving the premise of improving the surface quality of the pipette tip. At the same time, the outer surface of the pipette tip is fully treated through the multi-layer treatment to avoid surface adhesion due to wear, thereby greatly improving the service life of the pipette tip, reducing costs, and improving utilization. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 The figure is a flow chart of the processing method of the present invention. DETAILED DESCRIPTION

[0024] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0025] See also Figure 1 , the present invention provides a technical solution:

[0026] Embodiment 1:

[0027] The surface treatment method of a low adsorption plastic pipette tip comprises the following steps: injection molding, etching treatment, inert drying, spray filling, plasma treatment and circulation treatment, and surface grinding.

[0028] S1: Melting the plastic raw material and extruding it into a mold, and obtaining a conical plastic pipette tip by cooling;

[0029] S2: Place the plastic pipette tip that has been injection molded and cooled to room temperature in the etching solution for 2 minutes;

[0030] S3: placing the etched plastic pipette tip in an inert gas environment, rinsing it with clean water and then air-cooling and drying it;

[0031] S4: spraying a hydrophobic coating on the etched outer wall of the plastic pipette tip, drying at high temperature and then cooling to room temperature;

[0032] S5: placing the sprayed plastic pipette tip in a plasma surface treatment device, flushing a mixed gas of carbon dioxide and nitrogen into the device to ionize the surface of the sprayed position;

[0033] S6: spraying the treated plastic pipette tip again and drying and cooling it, and placing the plastic pipette tip in the plasma surface treatment device again for treatment after cooling, and repeating the process for 3 times;

[0034] S7: When the spray coating thickness is flush with the outer surface of the upper end of the plastic pipette tip, the outer wall of the plastic pipette tip is polished.

[0035] The depth of the plastic pipette tip in the etching solution is three quarters of the height of the plastic pipette tip itself, and the etching solution is a corrosive solution that slowly corrodes the outer wall of the plastic; the surface of the plastic pipette tip is polished to a mirror-like smoothness, and the surface is rinsed with clean water after polishing. The time for clean water rinsing during inert drying is 5 minutes, and the time for clean water rinsing during surface polishing is 2 minutes; the single spraying thickness during the spray filling process does not exceed one third of the etching depth, and the hydrophobic spray coating is a mixture of silicon dioxide powder; the high-temperature drying temperature after spray filling is 80 degrees Celsius, the baking position is the etched position of the sprayed plastic pipette tip, and the unetched position of the plastic pipette tip is separated by multiple groups of insulation rings; the temperature of the reaction chamber in the plasma surface treatment device is 25°C, the vacuum degree is 0.3mbar, the power is 1.5kW, and the processing time is 20min; the high-temperature drying treatment method is circulating hot air drying or infrared radiation drying.

[0036] Embodiment 2:

[0037] The surface treatment method of a low adsorption plastic pipette tip comprises the following steps: injection molding, etching treatment, inert drying, spray filling, plasma treatment and circulation treatment, and surface grinding.

[0038] S1: Melting the plastic raw material and extruding it into a mold, and obtaining a conical plastic pipette tip by cooling;

[0039] S2: Place the plastic pipette tip that has been injection molded and cooled to room temperature in the etching solution for 3 minutes;

[0040] S3: placing the etched plastic pipette tip in an inert gas environment, rinsing it with clean water and then air-cooling and drying it;

[0041] S4: spraying a hydrophobic coating on the etched outer wall of the plastic pipette tip, drying at high temperature and then cooling to room temperature;

[0042] S5: placing the sprayed plastic pipette tip in a plasma surface treatment device, flushing a mixed gas of carbon dioxide and nitrogen into the device to ionize the surface of the sprayed position;

[0043] S6: spraying the treated plastic pipette tip again and drying and cooling it, and placing the plastic pipette tip in the plasma surface treatment device again for treatment after cooling, and repeating the process for 3 times;

[0044] S7: When the spray coating thickness is flush with the outer surface of the upper end of the plastic pipette tip, the outer wall of the plastic pipette tip is polished.

[0045] The depth of the plastic pipette tip in the etching solution is three quarters of the height of the plastic pipette tip itself, and the etching solution is a corrosive solution that slowly corrodes the outer wall of the plastic; the surface of the plastic pipette tip is polished to a mirror-like smoothness, and the surface is rinsed with clean water after polishing. The time for clean water rinsing during inert drying is 8 minutes, and the time for clean water rinsing during surface polishing is 3 minutes; the single spraying thickness during the spray filling process does not exceed one third of the etching depth, and the hydrophobic spray coating is a mixture of silicon dioxide powder; the high-temperature drying temperature after spray filling is 90 degrees Celsius, the baking position is the etched position of the sprayed plastic pipette tip, and the unetched position of the plastic pipette tip is separated by multiple groups of insulation rings; the temperature of the reaction chamber in the plasma surface treatment device is 25°C, the vacuum degree is 0.3mbar, the power is 1.5kW, and the treatment time is 20min; the high-temperature drying treatment method is circulating hot air drying or infrared radiation drying.

[0046] Embodiment 3:

[0047] The surface treatment method of a low adsorption plastic pipette tip comprises the following steps: injection molding, etching treatment, inert drying, spray filling, plasma treatment and circulation treatment, and surface grinding.

[0048] S1: Melting the plastic raw material and extruding it into a mold, and obtaining a conical plastic pipette tip by cooling;

[0049] S2: Place the plastic pipette tip that has been injection molded and cooled to room temperature in the etching solution for 4 minutes;

[0050] S3: placing the etched plastic pipette tip in an inert gas environment, rinsing it with clean water and then air-cooling and drying it;

[0051] S4: spraying a hydrophobic coating on the etched outer wall of the plastic pipette tip, drying at high temperature and then cooling to room temperature;

[0052] S5: placing the sprayed plastic pipette tip in a plasma surface treatment device, flushing a mixed gas of carbon dioxide and nitrogen into the device to ionize the surface of the sprayed position;

[0053] S6: spraying the treated plastic pipette tip again and drying and cooling it, and placing the plastic pipette tip in the plasma surface treatment device again for treatment after cooling, and repeating the process for 4 times;

[0054] S7: When the spray coating thickness is flush with the outer surface of the upper end of the plastic pipette tip, the outer wall of the plastic pipette tip is polished.

[0055] The depth of the plastic pipette tip in the etching solution is three quarters of the height of the plastic pipette tip itself, and the etching solution is a corrosive solution that slowly corrodes the outer wall of the plastic; the surface of the plastic pipette tip is polished to a mirror-like smoothness, and the surface is rinsed with clean water after polishing. The time for clean water rinsing during inert drying is 10 minutes, and the time for clean water rinsing during surface polishing is 3 minutes; the single spraying thickness during the spray filling process does not exceed one third of the etching depth, and the hydrophobic spray coating is a mixture of silicon dioxide powder; the high-temperature drying temperature after spray filling is 100 degrees Celsius, the baking position is the etched position of the sprayed plastic pipette tip, and the unetched position of the plastic pipette tip is separated by multiple groups of insulation rings; the temperature of the reaction chamber in the plasma surface treatment device is 25°C, the vacuum degree is 0.3mbar, the power is 1.5kW, and the processing time is 20min; the high-temperature drying treatment method is circulating hot air drying or infrared radiation drying.

[0056] Embodiment 4:

[0057] Based on Example 1, the high temperature drying temperature after spray filling is 90 degrees Celsius.

[0058] Embodiment 5:

[0059] Based on Example 2, the high temperature drying temperature after spray filling is 100 degrees Celsius.

[0060] Embodiment 6:

[0061] Based on Example 3, the soaking time is 3 minutes.

[0062] Comparative Example:

[0063] Under the conditions of a soaking time of 3 minutes and a drying temperature of 90 degrees Celsius, a one-time spray molding processing method is adopted.

[0064] Soaking time Drying temperature Cycle times Molding quality Example 1 2 80 3 medium Example 2 3 90 3 high Example 3 4 100 4 Partial carbonization Example 4 2 90 3 high Example 5 3 100 3 Carbonization Example 6 3 100 4 medium Comparative Example 3 90 1 Low

[0065] In summary, a multi-layered hydrophobic surface of the pipette tip is formed through multiple cycles of spraying, thereby saving materials and improving material utilization while achieving the premise of improving the surface quality of the pipette tip. At the same time, through multi-layer treatment, the outer surface of the pipette tip is fully treated to avoid surface adhesion due to wear, which greatly improves the service life of the pipette tip, reduces costs, and improves utilization.

[0066] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A surface treatment method for a low-adsorption plastic pipette tip, characterized in that: The processing method comprises the following steps: Injection molding, the plastic raw material is melted and extruded into a mold, and a conical plastic pipette tip is obtained by cooling; Etching treatment: Place the plastic pipette tip that has been injection molded and cooled to room temperature in the etching solution for 2-4 minutes; Inert drying: Place the etched plastic pipette tip in an inert gas environment, rinse with water, and then air dry; Spray filling, spraying the hydrophobic coating on the etched outer wall of the plastic pipette tip, after spraying, drying at high temperature and then cooling to room temperature, the single spraying thickness during the spray filling process does not exceed one third of the etching depth, and the hydrophobic spray coating is a mixture of silicon dioxide powder; Plasma treatment: the sprayed plastic pipette tip is placed in a plasma surface treatment device, and a mixed gas of carbon dioxide and nitrogen is injected to ionize the surface of the sprayed position; Circular treatment, spraying the treated plastic pipette tip again and drying and cooling it, and placing the plastic pipette tip in the plasma surface treatment device again for treatment after cooling, and the cycle is repeated 3-4 times; Surface grinding: When the spray coating thickness is flush with the outer surface of the upper end of the plastic pipette tip, grind the outer wall of the plastic pipette tip.

2. The surface treatment method of a low-adsorption plastic pipette tip according to claim 1, characterized in that: The depth of the plastic liquid transfer pipette tip in the etching liquid is three quarters of the height of the plastic liquid transfer pipette tip itself, and the etching liquid is a corrosive liquid that slowly corrodes the outer wall of the plastic.

3. The surface treatment method of a low-adsorption plastic pipette tip according to claim 1, characterized in that: The surface of the plastic liquid transfer tip is polished to a mirror-like smoothness, and the surface is rinsed with clean water after polishing.

4. The surface treatment method of a low-adsorption plastic pipette tip according to claim 1, characterized in that: The high-temperature drying temperature after spraying and filling is 80-100 degrees Celsius, the baking position is the etched position of the sprayed plastic pipette tip, and the unetched position of the plastic pipette tip is separated by multiple groups of insulation rings.

5. The surface treatment method of a low-adsorption plastic pipette tip according to claim 1, characterized in that: The temperature of the reaction chamber in the plasma surface treatment device is 25° C., the vacuum degree is 0.3 mbar, the power is 1.5 kW, and the treatment time is 20 min.

6. The surface treatment method of a low-adsorption plastic pipette tip according to claim 1, characterized in that: The high temperature drying treatment is carried out by circulating hot air drying or infrared radiation drying.