A method for processing fuel injection O-ring

Through the simultaneous punching technology of mold molding and punching mechanism, the problem of removing the inner hole and outer flash of the fuel injection O-ring is solved, efficient processing effect is achieved, and the strict size and appearance requirements of the automotive field are met.

CN115284389BActive Publication Date: 2024-10-18ANHUI YAXINKE SEALING TECH CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202210886514.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-26
Publication Date
2024-10-18
Estimated Expiration
2042-07-26

AI Technical Summary

Technical Problem

The existing technology cannot effectively remove the inner hole flash of the fuel injection O-ring, and the O-ring with a small inner hole is difficult to process with manual edge tearing and groove processing, and cannot meet the strict size and appearance requirements of the automotive field.

Method used

A fuel injection O-ring processing method is designed. The O-ring with flash is obtained through mold pressing. The inner hole and the outer punching unit of the punching mechanism are used to perform synchronous punching to remove the flash, and the flash is removed through the blowing assembly. Flash debris realizes the separation of the inner hole and the outer flash.

Benefits of technology

It achieves efficient removal of the inner hole and outer flash of small-diameter O-rings, has fast processing speed and good punching effect, and meets the strict size and appearance requirements in the automotive field.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115284389B_ABST
    Figure CN115284389B_ABST
Patent Text Reader

Abstract

The invention discloses a fuel injection O-ring processing method. First, a rubber material is molded by a mold, and an O-ring with a flash is obtained by using a tearing groove connected with a cavity; then a plurality of O-rings are arranged and stored by using a placing table; then, an inner hole punching unit is used to synchronously punch the plurality of O-rings to remove the flash of the inner hole of the O-ring; then, an outer edge punching unit is used to synchronously punch the plurality of O-rings to push the O-ring body to separate it from the outer flash of the O-ring, and push the O-ring into a discharge chute; the invention connects the tearing groove and the cavity of the product by designing a mold groove, and there is no gap between the tearing groove and the cavity. The inner cavity cross section of the tearing groove is an arc groove, so that after two mold cores are butted, the two tearing grooves enclose a cavity with thin sides in the middle, so that the formed flash can be easily separated from the O-ring body.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of rubber sealing component production and processing, in particular to a fuel injection O-ring processing method. Background Art

[0002] O-rings are widely used in the fields of automobiles, aerospace, and home appliances. Among them, the requirements for O-rings in the automotive field are relatively strict, especially the appearance and size requirements are high. Due to the small inner diameter and large wire diameter of the product, the conventional flash removal process cannot remove the flash of the inner hole, and cannot meet the flash requirements of 0.1*0.1mm in length and width on the drawing. And because the inner hole diameter is only φ0.825mm, the normal tearing groove width is more than 1mm, and the distance from the cavity is more than 0.2mm, so according to the previous technology, the inner hole cannot be processed with the tearing groove. And for O-rings with small inner holes, manual flash tearing is impossible. Conventional flash removal processes, such as freezing, water grinding, polishing, etc., cannot be driven in when the frozen particles are larger than 0.8mm. If the particles are small, they are easy to get stuck in the inner hole. Even smaller particles cannot remove the flash of the inner hole. The inner hole polishing has also been verified, and no suitable object can be found for inner hole polishing. The water grinding particles are much larger than the inner diameter, and it is impossible to remove the flash of the inner hole. Therefore, the present invention provides a fuel injection O-ring processing method, which uses a specially designed tearing groove and a flash removal method to solve the above problems. Summary of the invention

[0003] The object of the present invention is to provide a fuel injection O-ring processing method to solve the problems raised in the above background technology.

[0004] To achieve the above object, the present invention provides the following technical solutions:

[0005] A fuel injection O-ring processing method comprises the following steps:

[0006] Step 1: The rubber material is molded by a mold, and an O-ring with a flash is obtained by using a tearing groove connected to the cavity;

[0007] Step 2: Move the O-ring to the loading station of the punching mechanism, and arrange and store several O-rings on a placement table;

[0008] Step 3: Drive the placement table to move to the inner hole punching position, and use the inner hole punching unit to synchronously punch several O-rings to remove the flash of the inner hole of the O-ring;

[0009] Step 4: Drive the placement table to move to the outer edge punching position, use the outer edge punching unit to synchronously punch several O-rings, push the O-ring body to separate it from the outer edge of the O-ring, and push the O-ring into the unloading chute;

[0010] Step 5: Drive the placement table to move to the blowing station, and use the blowing component to blow away the cut burrs and debris.

[0011] The mold in step 1 comprises an upper mold plate and a lower mold plate, the upper mold plate and the lower mold plate have the same structure, the lower mold plate is provided with a plurality of grooves arranged at equal intervals, a mold core is placed inside the groove, a plurality of mold grooves arranged at equal intervals are provided on the top of the mold core, the mold groove comprises a mold cavity for molding the O-ring body, a tearing groove is provided on the inner side of the mold cavity, and the outer side of the tearing groove is connected to the mold cavity;

[0012] The punching mechanism includes a dividing plate, the edge of the top of the dividing plate is fixedly connected with a placing platform, the placing platform includes a limiting seat, the top of the limiting seat is provided with a plurality of limiting grooves arranged at equal intervals, the number and arrangement of the limiting grooves correspond to the number and arrangement of the mold grooves on the mold core, the shape of the inner wall of the limiting groove is consistent with the shape of the O-ring body, a through hole is provided in the middle of the inner wall of the limiting groove, the bottom of the through hole extends downward and passes through the dividing plate, the inner diameter of the through hole is consistent with the outer diameter of the O-ring body; the top edge of the through hole is provided with a sharp edge;

[0013] The edge of the indexing plate is provided with an inner hole punching unit and an outer edge punching unit in sequence along its rotation direction, the initial position of the placement table is the loading station, the position of the inner hole punching unit is the inner hole punching position, and the position of the outer edge punching unit is the outer edge punching position;

[0014] The inner hole punching unit comprises a first mounting frame, a first punching cylinder is fixedly mounted on the top of the first mounting frame, an ejector fixing plate is fixedly connected to the output end of the first punching cylinder, a plurality of punching ejectors are fixedly connected to the bottom of the ejector fixing plate, a limit plate is fixedly mounted on the bottom of the mounting frame, a plurality of limit sleeves are fixedly connected to the top of the limit plate, the indexing plate drives the placing table to pass through between the bottom of the punching ejector and the top of the limit sleeve, and during punching, the plurality of punching ejectors pass through the plurality of through holes and enter the plurality of limit sleeves;

[0015] The outer punching unit comprises a second mounting frame, a second punching cylinder is fixedly mounted on the top of the second mounting frame, a pressing plate is fixedly connected to the output end of the second punching cylinder, a plurality of equally spaced pressing rods are fixedly connected to the bottom of the pressing plate, the diameter of the pressing rods is slightly smaller than the inner diameter of the through hole, and an inclined unloading trough is fixedly connected to the bottom of the second mounting frame, and the higher end of the unloading trough is arranged corresponding to the lower side of the pressing plate;

[0016] The blowing assembly includes a blowing pipe, one end of which is connected to an external air supply assembly, a pipe opening is opened in the middle of the dividing plate, the other end of the blowing pipe is passed through and bent by the pipe opening, and the port of the blowing pipe after horizontal bending faces the limit seat, and the position where the port at the end of the blowing pipe faces is set as a blowing station; the dividing plate drives the placing table installed thereon to move, so that it circulates along the loading station, the inner hole punching position, the outer edge punching position and the blowing station in sequence.

[0017] Compared with the prior art, the beneficial effects of the present invention are as follows: the present invention connects the tearing groove and the product's cavity together by designing the die groove, leaving no gap between the tearing groove and the cavity, and the inner cavity cross-section of the tearing groove is an arc-shaped groove, so that after the two mold cores are butted, the two tearing grooves enclose a cavity in the middle with thin sides, so that the formed flash is easy to separate from the O-ring body; when performing the deburring operation, the present invention drives the O-ring to be punched through each station in turn through the dividing plate, so that the punching operation can be carried out continuously, and the inner hole punching unit uses the ejector pin fixing plate to press down, driving several punching ejectors to correspondingly pass through the inner holes of several O-rings, thereby realizing the removal of the flash of the inner hole of the small-diameter O-ring; then the outer edge punching unit pushes several O-rings, and simultaneously completes the separation of the outer flash of the O-ring and the pushing and unloading operation of the O-ring body, with fast overall processing speed and good punching effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a flowchart of the present invention;

[0019] Figure 2 It is a structural schematic diagram of the template of the present invention;

[0020] Figure 3 A top view of the mold core of the present invention;

[0021] Figure 4 It is a structural schematic diagram of the mold groove of the present invention;

[0022] Figure 5 It is a structural schematic diagram of the punching mechanism of the present invention;

[0023] Figure 6 It is a structural schematic diagram of the placement table of the present invention;

[0024] Figure 7 It is a schematic structural diagram of the inner punching unit of the present invention.

[0025] In the figure: 1. lower template; 2. groove; 3. mold core; 4. cavity; 5. tearing edge groove; 6. dividing plate; 7. limit seat; 8. limit groove; 9. through hole; 10. first mounting bracket; 11. first punching cylinder; 12. ejector fixing plate; 13. punching ejector; 14. limit sleeve; 15. second mounting bracket; 16. second punching cylinder; 17. pressing plate; 18. blowing pipe. DETAILED DESCRIPTION

[0026] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0027] See also Figure 1-Figure 7 In an embodiment of the present invention, a fuel injection O-ring processing method includes the following steps:

[0028] Step 1: The rubber material is molded by a mold, and an O-ring with a flash is obtained by using a tearing groove 5 connected to the cavity 4;

[0029] Step 2: Move the O-ring to the loading station of the punching mechanism, and arrange and store several O-rings on a placement table;

[0030] Step 3: Drive the placement table to move to the inner hole punching position, and use the inner hole punching unit to synchronously punch several O-rings to remove the flash of the inner hole of the O-ring;

[0031] Step 4: Drive the placement table to move to the outer edge punching position, use the outer edge punching unit to synchronously punch several O-rings, push the O-ring body to separate it from the outer edge of the O-ring, and push the O-ring into the unloading chute;

[0032] Step 5: Drive the placement table to move to the blowing station, and use the blowing component to blow away the cut burrs and debris.

[0033] See also Figure 2 The mold in step 1 includes an upper template and a lower template 1, the upper template and the lower template 1 have the same structure, and the lower template 1 is provided with a plurality of grooves 2 arranged at equal distances. In this embodiment, 9 grooves 2 are provided and arranged in a rectangular array of 3 rows and 3 columns;

[0034] A mold core 3 is placed inside the groove 2, and a plurality of mold grooves arranged at equal intervals are opened on the top of the mold core 3. Figure 3-Figure 4In this embodiment, there are 25 mold grooves arranged in a rectangular array of 5 rows and 5 columns. The mold groove includes a mold cavity 4 for molding the O-ring body. A tearing groove 5 is provided on the inner side of the mold cavity 4. The outer side of the tearing groove 5 is connected to the edge of the mold cavity 4. The inner cavity cross-section of the tearing groove 5 is an arc groove, so that after the two mold cores 3 are connected, the two tearing grooves enclose a cavity with thin sides in the middle, so that the formed flash is easy to separate from the O-ring body; when working, the rubber extrusion mechanism feeds the rubber between the upper mold plate and the lower mold plate 1, and then drives the upper mold plate and the lower mold plate 1 close to extrude the rubber. The extrusion mechanism and the driving mechanism for driving the upper mold plate and the lower mold plate 1 to move are implemented by existing technical means. After the rubber material is molded, a sheet-like connection body consisting of flash and 25 O-ring bodies is obtained. The mold of the present invention receives a plurality of mold cores 3 through a plurality of grooves 2 at the same time, and cooperates with a plurality of mold grooves on the mold core 3, so that a plurality of O-rings are obtained in one molding operation. In this embodiment, 225 O-rings without cutting flash are obtained in one molding operation; when punching operation is required, the sheet-like connection body in each groove 2 is manually taken out and sent to the punching mechanism;

[0035] See also Figure 5-Figure 6 The punching mechanism includes a dividing plate 6, the edge of the top of the dividing plate 6 is fixedly connected with a placing table, the placing table includes a limiting seat 7, and a plurality of limiting grooves 8 are provided on the top of the limiting seat 7. The number and arrangement of the limiting grooves 8 correspond to the number and arrangement of the mold grooves on the mold core 3;

[0036] The inner wall shape of the limiting groove 8 is consistent with the shape of the O-ring body, and when the sheet-like connector is placed on the placement table, it is ensured that the O-ring body corresponds to the limiting groove 8 one by one;

[0037] The inner hole punching unit and the outer edge punching unit are sequentially arranged along the rotation direction of the dividing plate 6. The initial position of the placement table is the loading station, the position of the inner hole punching unit is the inner hole punching position, and the position of the outer edge punching unit is the outer edge punching position. The rotation of the dividing plate 6 drives the placement table installed thereon to move, so that it passes through each station in turn, so that the punching operation can be carried out continuously.

[0038] See also Figure 7The inner hole punching unit includes a first mounting frame 10, a first punching cylinder 11 is fixedly mounted on the top of the first mounting frame 10, an output end of the first punching cylinder 11 is fixedly connected to a pin fixing plate 12, a plurality of punching pins 13 are fixedly connected to the bottom of the pin fixing plate 12, a limiting plate is fixedly mounted on the bottom of the mounting frame, a plurality of limiting sleeves 14 are fixedly connected to the top of the limiting plate, and the indexing plate 6 drives the placement table to pass between the bottom of the punching pin 13 and the top of the limiting sleeve 14; the first punching cylinder 11 drives the pin fixing plate 12 to be pressed down, and drives a plurality of punching pins 13 to pass through the inner holes of a plurality of O-rings to remove the flash of the inner holes of the O-rings; when the pin fixing plate 12 is pressed down for punching, the punching pins 13 pass through a plurality of through holes 9 and enter a plurality of limiting sleeves 14, and the limiting sleeves 14 guide and limit the movement of the punching pins 13 to ensure the accuracy of the punching operation;

[0039] The outer punching unit includes a second mounting frame 15, a second punching cylinder 16 is fixedly mounted on the top of the second mounting frame 15, a pressing plate 17 is fixedly connected to the output end of the second punching cylinder 16, a plurality of equally spaced pressing rods are fixedly connected to the bottom of the pressing plate 17, a through hole 9 is opened in the middle of the inner wall of the limiting groove 8, the bottom of the through hole 9 extends downward and passes through the dividing plate 6, the inner diameter of the through hole 9 is consistent with the outer diameter of the O-ring body; the diameter of the pressing rod is slightly smaller than the inner diameter of the through hole 9; the bottom of the second mounting frame 15 is fixedly connected to an inclined discharge trough, the higher end of the discharge trough is arranged corresponding to the lower side of the pressing plate 17;

[0040] In this way, it is ensured that when the pressing rod is pressed down, the O-ring body can be sent into the through hole 9. When the outer punching unit performs punching, the second punching cylinder 16 drives the pressing plate 17 to press down, thereby driving a number of lifting rods to press down a number of O-ring bodies synchronously. During the pressing process, the O-ring body is separated from the outer flash edge of the O-ring by the sharp edge of the edge of the through hole 9, so that the O-ring body passes through the through hole 9 on the placement table and falls into the unloading trough. The punched O-ring body is temporarily stored by the receiving box arranged at the lower end of the unloading trough, and is collected in real time by the operator.

[0041] The blowing assembly includes a blowing pipe 18, one end of which is connected to an external air supply assembly, a pipe opening is opened in the middle of the dividing plate 6, and the other end of the blowing pipe 18 is passed through and bent by the pipe opening, and the end of the horizontally bent blowing pipe 18 faces the limit seat 7, and air is supplied through the air supply assembly, and the blowing pipe 18 is used to blow away the burrs remaining on the top surface of the placement table.

[0042] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still fall within the scope of the technical solution of the present invention.

Claims

1. A fuel injection O-ring processing method, characterized in that: The following steps are involved: Step 1: molding the rubber material through a mold, and obtaining an O-ring with a flash edge by using a tearing groove (5) connected to the mold cavity (4); Step 2: Move the O-ring to the loading station of the punching mechanism, and arrange and store several O-rings on a placement table; Step 3: Drive the placement table to move to the inner hole punching position, and use the inner hole punching unit to synchronously punch several O-rings to remove the flash of the inner hole of the O-ring; Step 4: Drive the placement table to move to the outer edge punching position, use the outer edge punching unit to synchronously punch several O-rings, push the O-ring body to separate it from the outer edge of the O-ring, and push the O-ring into the unloading chute; Step 5: Drive the placement table to move to the blowing station, and use the blowing assembly to blow air to remove the cut burrs and debris; The mold in step 1 comprises an upper mold plate and a lower mold plate, the upper mold plate and the lower mold plate have the same structure, the lower mold plate is provided with a plurality of grooves arranged at equal intervals, a mold core is placed inside the groove, a plurality of mold grooves arranged at equal intervals are provided on the top of the mold core, the mold groove comprises a mold cavity for forming the O-ring body, a tearing edge groove is provided on the inner side of the mold cavity, and the outer side of the tearing edge groove is connected to the mold cavity; the inner cavity cross section of the tearing edge groove is an arc groove, and after the two mold cores are butt-jointed, the two tearing edge grooves enclose a cavity with a middle and thin sides; In step three, the inner hole punching unit drives the ejector fixing plate (12) to be pressed down, thereby driving a plurality of punching ejectors (13) to pass through the inner holes of a plurality of O-rings to remove the flash of the inner holes of the O-rings; when the ejector fixing plate (12) is pressed down, the inner hole punching unit guides and limits the plurality of punching ejectors (13) through a limiting member provided below the ejector fixing plate (12).

2. A fuel injection O-ring processing method according to claim 1, characterized in that: In step 2, the punching mechanism drives the placement table mounted thereon to move by rotating the indexing plate (6), so that it circulates along the loading station, the inner hole punching station, the outer edge punching station and the blowing station in sequence.

3. A fuel injection O-ring processing method according to claim 1, characterized in that: In step 4, the outer edge punching unit drives a plurality of lifting rods to synchronously press down a plurality of O-ring bodies, so that they pass through the through hole (9) on the placement table and fall into the unloading chute. During the pressing process, the sharp edge of the through hole (9) is used to separate the O-ring body from the outer flash of the O-ring.

4. A fuel injection O-ring processing method according to claim 1, characterized in that: In step five, the blowing assembly uses a bent blowing pipe (18) to blow air from a horizontal direction toward the placement table to remove the cut burrs and debris.

5. A fuel injection O-ring processing method according to claim 1, characterized in that: In step one, the mold simultaneously receives a plurality of mold cores (3) through a plurality of grooves (2), and a plurality of O-rings are obtained in one molding operation by utilizing a plurality of mold grooves on the mold core (3).

Citation Information

Patent Citations

  • Rubber product flash removing apparatus and inner and outer flash removing method thereof

    CN103552194A

  • Integrated trimming and notching device

    CN111113747A

  • Rubber sealing ring manufacturing process

    CN112109353A

  • O-shaped seal ring mold

    CN204309164U