A triazine-containing compound and an organic electroluminescent device containing the same
By using triazine-containing compounds in OLED devices, problems with device voltage, current efficiency and lifetime are solved, achieving more efficient carrier injection and energy transfer, extending high-temperature lifetime and reducing efficiency roll-off.
Patent Information
- Application Number
- CN202110595172.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-05-28
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2041-05-28
AI Technical Summary
Existing triplet light-emitting OLED devices have needs for improvement in terms of device voltage, current efficiency and lifespan, especially the problems of efficiency roll-off at high current density and insufficient high-temperature lifespan.
Provides a triazine-containing compound for use in the light-emitting layer of an organic electroluminescent device. The compound has suitable HOMO and LUMO energy levels, higher T1 energy level and stereoscopicity to ensure carrier injection efficiency and energy transfer efficiency. , at the same time, the molecules are not easy to crystallize, suitable for low evaporation temperature, and have good film forming properties.
It improves the low voltage, high efficiency and long life performance of the device, especially extends the device life under high temperature conditions, and reduces the efficiency roll-off under high current density.
Smart Images

Figure CN115403586B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of semiconductor technology, in particular to a triazine-containing compound and an organic electroluminescent device containing the same. Background Art
[0002] There may be a hole transport region between the anode and the light-emitting layer of the organic electroluminescent device, and there may be an electron transport region between the light-emitting layer and the cathode. Holes from the anode may migrate to the light-emitting layer through the hole transport region, and electrons from the cathode may migrate to the light-emitting layer through the electron transport region, and the holes and electrons recombine in the light-emitting layer to generate excitons. According to the principles of quantum mechanics, organometallic compound materials as doping materials can achieve an internal quantum yield of 100%.
[0003] Nevertheless, there is still a need for improvement in device voltage, current efficiency and lifespan for triplet luminescent phosphorescent OLEDs. The performance of the host material in the light-emitting layer usually affects the above-mentioned key properties of the organic electroluminescent device to a large extent. According to the prior art, the compounds used as host materials usually contain triazine groups. When the existing triazine derivatives are used as host materials, there is a need for improvement in device voltage, current efficiency, especially in turn-on voltage and device lifespan.
[0004] For phosphorescent OLED, there is usually an imbalance between holes and electrons in the light-emitting layer, and the device efficiency roll-off is serious under high current density. The present invention also provides a combination of two host materials, which can effectively solve the above-mentioned drawbacks. Summary of the invention
[0005] In view of the above problems existing in the prior art, a triazine-containing compound is provided. The present invention provides a compound which is applied to an organic electroluminescent device to make the device have a long life, especially a longer high-temperature life.
[0006] The technical solution of the present invention is: a triazine-containing compound, the compound structure is shown in the general formula (1):
[0007]
[0008] In the general formula (1), L, L0, and L1 are each independently a single bond or a phenylene group;
[0009] Z1 is represented by C-R3 or N;
[0010] Z2 is represented by C-R4 or N, and Z1 and Z2 at the connection are represented by C;
[0011] One of R0 and R represents a structure represented by general formula (1-1) or (1-2), and the other represents H;
[0012]
[0013] In general formula (1-1) and general formula (1-2), m and n are 0, 1 or 2 respectively;
[0014] When R0 is represented by H, L0 is represented by phenylene;
[0015] When L1 represents a single bond, at least one Z1 represents N;
[0016] When L1 represents a phenylene group, R0 represents a structure represented by the general formula (1-1) or (1-2), L0 represents a single bond, and at least one Z2 represents N;
[0017] R1-R4 are independently hydrogen, deuterium, phenyl or cyano.
[0018] The present invention also provides an organic electroluminescent device, comprising a first electrode, a second electrode and a functional layer, wherein the functional layer is located between the first electrode and the second electrode, and at least one functional layer in the organic electroluminescent device contains the triazine-containing compound.
[0019] Compared with the prior art, the beneficial technical effects of the present invention are:
[0020] 1) The compound provided by the present invention has suitable HOMO and LUMO energy levels, which can ensure efficient injection and recombination of carriers in the light-emitting layer, and ensure low voltage and high efficiency of the device.
[0021] 2) The higher T1 energy level of the compound provided by the present invention can ensure the energy transfer efficiency between the host and the guest.
[0022] 3) The compound provided by the present invention has strong stereochemistry and weak intermolecular interactions, so it has the characteristics of being difficult to crystallize, having a low evaporation temperature, and having good film-forming properties, and has excellent industrial processing performance.
[0023] 4) Device life, especially high-temperature device life, has always restricted the promotion of OLED displays in various application fields. The compounds provided by the present invention have high chemical stability, which helps to reduce the efficiency roll-off under high current density and also helps to increase device life and high-temperature device life. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 This is a schematic diagram of the structure of an OLED device in which the materials listed in the present invention are applied;
[0025] Among them, 1 is a transparent substrate layer, 2 is an anode layer, 3 is a hole injection layer, 4 is a hole transport layer, 5 is an electron blocking layer, 6 is a light-emitting layer, 7 is an electron transport layer, 8 is an electron injection layer, 9 is a cathode layer, and 10 is a CPL layer. DETAILED DESCRIPTION
[0026] The principles and features of the present invention are described below in conjunction with the accompanying drawings and embodiments. The examples given are only used to explain the present invention and are not used to limit the scope of the present invention.
[0027] In the present invention, unless otherwise specified, HOMO means the highest occupied orbital of a molecule, and LUMO means the lowest unoccupied orbital of a molecule. In addition, in the present invention, HOMO and LUMO energy levels are expressed in absolute values, and the comparison between energy levels is also a comparison of the magnitude of their absolute values. Those skilled in the art know that the greater the absolute value of an energy level, the lower the energy of the energy level.
[0028] In the present invention, when describing electrodes and organic electroluminescent devices, as well as other structures, the words "upper", "lower", "top" and "bottom" used to indicate orientation only indicate the orientation in a certain state, and do not mean that the related structure can only exist in the orientation described; on the contrary, if the structure can change its position, such as inverted, the orientation of the structure will be changed accordingly. Specifically, in the present invention, the "bottom" or "lower" side of the electrode refers to the side of the electrode close to the substrate during the preparation process, and the opposite side away from the substrate is the "top" or "upper" side.
[0029] Compound represented by general formula (1)
[0030]
[0031] In the general formula (1), L, L0, and L1 are each independently a single bond or a phenylene group;
[0032] Z1 is represented by C-R3 or N;
[0033] Z2 is represented by C-R4 or N, and Z1 and Z2 at the connection are represented by C;
[0034] One of R0 and R represents a structure represented by general formula (1-1) or (1-2), and the other represents H;
[0035]
[0036] In general formula (1-1) and general formula (1-2), m and n are 0, 1 or 2 respectively;
[0037] When R0 is represented by H, L0 is represented by phenylene;
[0038] When L1 represents a single bond, at least one Z1 represents N;
[0039] When L1 represents a phenylene group, R0 represents a structure represented by the general formula (1-1) or (1-2), L0 represents a single bond, and at least one Z2 represents N;
[0040] R1-R4 are independently hydrogen, deuterium, phenyl or cyano.
[0041] The preferred technical solution is that the compound structure is shown in general formula (1):
[0042]
[0043] In the general formula (1), L and L0 are independently a single bond or a phenylene group;
[0044] Z1 is C, N or C-R3, and at least one Z1 is N;
[0045] Z2 is represented by C, N or C-R4, and Z1 and Z2 at the connection point are represented by C;
[0046] One of R0 and R represents a structure represented by general formula (1-1) or (1-2), and the other represents H;
[0047]
[0048] In general formula (1-1) and general formula (1-2), m and n are 0, 1 or 2 respectively;
[0049] R1-R4 are independently hydrogen, deuterium, phenyl or cyano.
[0050] In the preferred technical solution, in the general formula (1), two Z1 are represented by N.
[0051] A preferred technical solution is that in the general formula (1), there is only one Z1 represented by N, and there is only one Z2 represented by N.
[0052] In a preferred technical solution, the compound structure is represented by any one of the general formulas (2-1) to (2-4):
[0053]
[0054]
[0055] In the general formulas (2-1) to (2-4), L and L0 are each independently a single bond or a phenylene group;
[0056] Z1 is represented by C-R3 or N, and at least one Z1 is represented by N;
[0057] Z2 is represented by C-R4 or N, and Z1 and Z2 at the connection are represented by C;
[0058] R0, R represents H;
[0059] L0 connected to R0 is represented by a phenylene group;
[0060] m and n are 0, 1 or 2 respectively;
[0061] R1-R4 are independently hydrogen, deuterium, phenyl, or cyano;
[0062] In the general formulas (2-5) and (2-6), L represents a single bond or a phenylene group;
[0063] Z1 is represented by C-R3 or N;
[0064] Z2 is represented by C-R4 or N, and at least one Z2 is represented by N; Z1 and Z2 at the connection point are represented by C;
[0065] R represents H;
[0066] m and n are 0, 1 or 2 respectively;
[0067] R1-R4 are independently hydrogen, deuterium, phenyl or cyano.
[0068] In a preferred technical solution, the compound structure is represented by any one of the general formulas (3-1) to (3-12):
[0069]
[0070]
[0071] In the general formulas (3-1) to (3-12),
[0072] Z1 is represented by C-R3 or N, and at least one Z1 is represented by N;
[0073] Z2 is represented by C-R4 or N, and Z1 and Z2 at the connection are represented by C;
[0074] m and n are 0, 1 or 2 respectively;
[0075] R1-R4 are independently hydrogen, deuterium, phenyl, or cyano;
[0076] In the general formulas (3-13) and (3-16),
[0077] Z1 is represented by C-R3 or N;
[0078] Z2 is represented by C-R4 or N, and at least one Z2 is represented by N; Z1 and Z2 at the connection point are represented by C;
[0079] m and n are 0, 1 or 2 respectively;
[0080] R1-R4 are independently hydrogen, deuterium, phenyl or cyano.
[0081] The preferred technical solution is that the compound structure is represented by the general formula (4-1):
[0082]
[0083] In the general formula (4-1), Z1 is represented by C, N or C-R3, and at least one Z1 is represented by N; Z2 is represented by C, N or C-R4, and Z1 and Z2 at the connection point are represented by C;
[0084] m and n are 0, 1 or 2 respectively;
[0085] R1, R3, and R4 are independently hydrogen, deuterium, phenyl, and cyano.
[0086] The preferred technical solution is that the specific structure of the compound is any one of the following structures:
[0087]
[0088]
[0089]
[0090]
[0091]
[0092]
[0093]
[0094]
[0095]
[0096] Organic electroluminescent devices
[0097] The present invention provides an organic electroluminescent device, comprising a first electrode, a second electrode and a functional layer, wherein the functional layer is located between the first electrode and the second electrode, and at least one functional layer in the organic electroluminescent device contains a triazine-containing compound represented by general formula (1).
[0098] In a preferred embodiment of the present invention, the functional layer comprises a light-emitting layer, and the light-emitting layer contains a triazine-containing compound represented by the general formula (1).
[0099] In a preferred embodiment of the present invention, the light-emitting layer contains a light-emitting host material, and the light-emitting host material is a mixture of a triazine-containing compound represented by general formula (1) and a compound represented by general formula (A) or general formula (B).
[0100]
[0101] In the general formula (A), A1 to A4 independently represent a substituted or unsubstituted C6-C 20 The aromatic rings,
[0102] X1 represents O, S, N (R a )、C(R b )(R c ), where R a is substituted or unsubstituted C6-C 30 Aryl, substituted or unsubstituted C3-C 30 Heteroaryl, where R b and R c are independently hydrogen, substituted or unsubstituted C1-C6 alkyl, substituted or unsubstituted C6-C 30 Aryl or substituted or unsubstituted C3-C 30 Heteroaryl, R b and R c Can be the same or different,
[0103] L1 represents the following groups: single bond, substituted or unsubstituted C6-C 30 Arylene, substituted or unsubstituted C3-C 30 Heteroarylene,
[0104] b1, b2, b3, b4, b5 independently represent 0, 1, 2, 3 or 4;
[0105] R5 represents a substituted or unsubstituted C1-C 10 Alkyl, substituted or unsubstituted C3-C 10 Cycloalkyl, substituted or unsubstituted C6-C 30 Aryl, substituted or unsubstituted C3-C 30 Heteroaryl,
[0106] R6 to R9 independently represent hydrogen, deuterium, halogen, hydroxyl, cyano, nitro, amino, substituted or unsubstituted C1-C 10 Alkyl, substituted or unsubstituted C3-C 10 Cycloalkyl, substituted or unsubstituted C6-C 30 Aryl, substituted or unsubstituted C6-C 30 Aryloxy, substituted or unsubstituted C3-C 30 heteroaryl;
[0107] In the general formula (B),
[0108] Ar1 and Ar2 are independently a single bond, a substituted or unsubstituted C6-C 30 Arylene, substituted or unsubstituted C2-C 30 Heteroarylene,
[0109] R 14 and R 15 are independently substituted or unsubstituted C6-C 30 Aryl, substituted or unsubstituted C2-C 30 Heterocyclic group,
[0110] R 10 -R 13 are independently hydrogen, deuterium, cyano, halogen, substituted or unsubstituted C1-C 20 Alkyl, substituted or unsubstituted C6-C 30 Aryl, substituted or unsubstituted C2-C 30 Heterocyclic group.
[0111] In a preferred embodiment of the present invention, the functional layer of the organic electroluminescent device comprises a light-emitting layer, the light-emitting layer contains a light-emitting host material, the light-emitting host material comprises a first host material and a second host material, the first host material is selected from a triazine-containing compound represented by the general formula (1), and the second host material is selected from any one or more of compounds GH-1 to GH-170, and the specific structures of the compounds GH-1 to GH-170 are:
[0112]
[0113]
[0114]
[0115]
[0116]
[0117] In an exemplary embodiment of the present invention, the organic electroluminescent device may include an anode, a hole transport region, a light emitting region, an electron transport region and a cathode. In addition to using the triazine compound modified with azadibenzofuran of the present invention in the organic electroluminescent device, the organic electroluminescent device can be prepared by conventional methods and materials for preparing organic electroluminescent devices.
[0118] As the substrate of the organic electroluminescent device of the present invention, any substrate commonly used in organic electroluminescent devices can be used. Examples are transparent substrates such as glass or transparent plastic substrates; opaque substrates such as silicon substrates; flexible PI film substrates. Different substrates have different mechanical strengths, thermal stability, transparency, surface smoothness, and waterproofness. Depending on the properties of the substrate, its use direction is different. In the present invention, a transparent substrate is preferably used. The thickness of the substrate is not particularly limited.
[0119] A first electrode is formed on a substrate, and the first electrode and the second electrode may be opposite to each other. The first electrode may be an anode. The first electrode may be a transmissive electrode, a semi-transmissive electrode or a reflective electrode. When the first electrode is a transmissive electrode, it may be formed using a transparent metal oxide, such as indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO) or indium tin zinc oxide (ITZO). When the first electrode is a semi-transmissive electrode or a reflective electrode, it may include Ag, Mg, Al, Pt, Pd, Au, Ni, Nd, Ir, Cr or a metal mixture. The thickness of the first electrode layer depends on the material used, and is typically 50-500nm, preferably 70-300nm and more preferably 100-200nm.
[0120] The organic functional material layer disposed between the first electrode and the second electrode includes, from bottom to top, a hole transport region, a light emitting layer and an electron transport region.
[0121] Herein, the hole transport region constituting the organic electroluminescent device can be exemplified by a hole injection layer, a hole transport layer, an electron blocking layer, and the like.
[0122] As the material for the hole injection layer, the hole transport layer, and the electron blocking layer, any material can be selected from known related materials used for OLED devices.
[0123] Examples of the above materials include phthalocyanine derivatives, triazole derivatives, triarylmethane derivatives, triarylamine derivatives, oxazole derivatives, oxadiazole derivatives, hydrazone derivatives, stilbene derivatives, pyridoline derivatives, polysilane derivatives, imidazole derivatives, phenylenediamine derivatives, amino-substituted quilone derivatives, styryl anthracene derivatives, styrylamine derivatives and the like, fluorene derivatives, spirofluorene derivatives, silazane derivatives, aniline copolymers, porphyrin compounds, carbazole derivatives, polyarylalkane derivatives, polyphenylene vinyl and its derivatives, polythiophene and its derivatives, poly-N-vinylcarbazole derivatives, thiophene oligomers and the like, conductive polymer oligomers, aromatic tertiary amine compounds, styrene amination compounds, compounds, triamines, tetraamines, benzidines, propargyl diamine derivatives, p-phenylenediamine derivatives, m-phenylenediamine derivatives, 1,1'-bis(4-diarylaminophenyl)cyclohexane, 4,4'-bis(diarylamino)biphenyls, bis[4-(diarylamino)phenyl]methanes, 4,4'-bis(diarylamino)terphenyls, 4,4'-bis(diarylamino)quaterphenyls, 4,4'-bis(diarylamino)diphenyl ethers, 4,4'-bis(diarylamino)diphenylsulfanes, bis[4-(diarylamino)phenyl]dimethylmethanes, bis[4-(diarylamino)phenyl]-bis(trifluoromethyl)methanes, or 2,2-diphenylethylene compounds.
[0124] Furthermore, according to the device matching requirements, the hole transport film layer between the hole transport auxiliary layer and the hole injection layer constituting the organic electroluminescent device can be a single film layer or a superposition structure of multiple hole transport materials. In this article, for the above-mentioned hole carrier conduction film layers with different functions, their film thickness is not particularly limited.
[0125] The hole injection layer contains a main organic material that can conduct holes, and also contains a P-type dopant material with a deep HOMO energy level (the corresponding LUMO energy level will also be very deep). Based on empirical summary, in order to achieve smooth injection of holes from the anode to the organic film layer, the HOMO energy level of the main organic material that conducts holes used in the anode interface buffer layer must have certain characteristics with the P-doped material, so that the charge transfer state between the main material and the doped material can be realized, the ohmic contact between the buffer layer and the anode can be achieved, and the efficient injection from the electrode to the hole injection conduction can be achieved. This feature is summarized as: main material HOMO energy level - P dopant material LUMO energy level ≤ 0.4eV.
[0126] In view of the above empirical summary, for hole-type host materials with different HOMO energy levels, different P-doped materials need to be selected to match them in order to achieve ohmic contact at the interface and improve the hole injection effect.
[0127] Therefore, in one embodiment of the present invention, in order to better inject holes, the hole injection layer also includes a P-type doping material with charge conductivity selected from the following: quinone derivatives, such as tetracyanoquinodimethane (TCNQ) and 2,3,5,6-tetrafluoro-tetracyano-1,4-benzoquinodimethane (F4-TCNQ); or hexaazatriphenylene derivatives, such as 2,3,6,7,10,11-hexacyano-1,4,5,8,9,12-hexaazatriphenylene (HAT-CN); or cyclopropane derivatives, such as 4,4',4"-((1E,1'E,1"E)-cyclopropane-1,2,3-trimethylenetris(cyanoformyl))tris(2,3,5,6-tetrafluorobenzyl); or metal oxides, such as tungsten oxide and molybdenum oxide, but not limited to these.
[0128] In the hole injection layer of the present invention, the ratio of the hole transport material to the P-type doping material used is 99:1-95:5, preferably 99:1-97:3, based on mass.
[0129] The thickness of the hole injection layer of the present invention may be 5-100 nm, preferably 5-50 nm, and more preferably 5-20 nm, but the thickness is not limited to this range.
[0130] The thickness of the hole transport layer of the present invention may be 5 to 200 nm, preferably 10 to 150 nm, and more preferably 20 to 100 nm, but the thickness is not limited to this range.
[0131] The thickness of the electron blocking layer of the present invention may be 1-20 nm, preferably 5-10 nm, but the thickness is not limited to this range.
[0132] After forming the hole injection layer, the hole transport layer and the electron blocking layer, a corresponding light emitting layer is formed on the electron blocking layer.
[0133] As the host material of the light-emitting layer, a triazine-containing compound represented by the general formula (1) of the present invention is used.
[0134] In addition, the luminescent material may also include a phosphorescent material. Specific examples of phosphorescent materials include metal complexes of iridium, platinum, etc. For example, green phosphorescent materials such as Ir(ppy)3[fac-tris(2-phenylpyridine)iridium], blue phosphorescent materials such as FIrpic, FIr6, and red phosphorescent materials such as Btp2Ir(acac) can be used.
[0135] In the light-emitting layer of the present invention, the ratio of the host material to the guest material used is 99:1-70:30, preferably 99:1-85:15 and more preferably 97:3-87:13, based on mass.
[0136] The thickness of the light-emitting layer can be adjusted to optimize the light-emitting efficiency and the driving voltage. The preferred thickness range is 5 nm to 50 nm, more preferably 10-50 nm, and more preferably 15-30 nm, but the thickness is not limited to this range.
[0137] In the present invention, the electron transport region may include, from bottom to top, a hole blocking layer, an electron transport layer, and an electron injection layer disposed on the light emitting layer, but is not limited thereto.
[0138] The hole blocking layer is a layer that blocks the holes injected from the anode from passing through the light-emitting layer and entering the cathode, thereby extending the life of the device and improving the efficiency of the device. The hole blocking layer of the present invention can be arranged on the light-emitting layer. As the hole blocking layer material of the organic electroluminescent device of the present invention, compounds with hole blocking effects known in the prior art can be used, for example, phenanthroline derivatives such as bathocuproin (referred to as BCP), metal complexes of hydroxyquinoline derivatives such as aluminum (III) bis (2-methyl-8-quinoline) -4-phenylphenolate (BAlq), various rare earth complexes, oxazole derivatives, triazole derivatives, triazine derivatives, 9,9'-(5-(6-([1,1'-biphenyl]-4-yl)-2-phenylpyrimidin-4-yl)-1,3-phenylene)bis(9H-carbazole) (CAS No.: 1345338-69-3 ) and other pyrimidine derivatives, etc. The thickness of the hole blocking layer of the present invention may be 2-200 nm, preferably 5-150 nm, and more preferably 10-100 nm, but the thickness is not limited to this range.
[0139] The electron transport layer may be disposed on the light emitting layer or (if present) the hole blocking layer. The electron transport layer material is a material that easily receives electrons from the cathode and transfers the received electrons to the light emitting layer. Preferably, the material has a high electron mobility. As the electron transport layer of the organic electroluminescent device of the present invention, the electron transport layer materials for organic electroluminescent devices known in the prior art can be used, for example, metal complexes of hydroxyquinoline derivatives represented by Alq3, BAlq and Liq, various rare earth metal complexes, triazole derivatives, 2,4-bis(9,9-dimethyl-9H-fluorene-2-yl)-6-(naphthalene-2-yl)-1,3,5-triazine (CAS No.: 1459162-51-6) and other triazine derivatives, 2-(4-(9,10-di(naphthalene-2-yl)anthracene-2-yl)phenyl)-1-phenyl-1H-benzo[d]imidazole (CAS No.: 561064-11-7, commonly known as LG201) and other imidazole derivatives, oxadiazole derivatives, thiadiazole derivatives, carbodiimide derivatives, quinoxaline derivatives, phenanthroline derivatives, silicon-based compound derivatives, etc. The thickness of the electron transport layer of the present invention may be 10-80 nm, preferably 20-60 nm, and more preferably 25-45 nm, but the thickness is not limited to this range.
[0140] The electron injection layer may be disposed above the electron transport layer. The electron injection layer material is generally preferably a material having a low work function so that electrons are easily injected into the organic functional material layer. As the electron injection layer material of the organic electroluminescent device of the present invention, the electron injection layer material for organic electroluminescent devices known in the prior art can be used, for example, lithium; lithium salts such as 8-hydroxyquinoline lithium, lithium fluoride, lithium carbonate or lithium azide; or cesium salts, cesium fluoride, cesium carbonate or cesium azide. The thickness of the electron injection layer of the present invention may be 0.1-5 nm, preferably 0.5-3 nm and more preferably 0.8-1.5 nm, but the thickness is not limited to this range.
[0141] The second electrode may be disposed above the electron transport region. The second electrode may be a cathode. The second electrode may be a transmissive electrode, a semi-transmissive electrode or a reflective electrode. When the second electrode is a transmissive electrode, the second electrode may include, for example, Li, Yb, Ca, LiF / Ca, LiF / Al, Al, Mg, BaF, Ba, Ag, or a compound or mixture thereof; when the second electrode is a semi-transmissive electrode or a reflective electrode, the second electrode may include Ag, Mg, Yb, Al, Pt, Pd, Au, Ni, Nd, Ir, Cr, Li, Ca, LiF / Ca, LiF / Al, Mo, Ti, or a compound or mixture thereof, but is not limited thereto. The thickness of the cathode depends on the material used, and is typically 10-50 nm, preferably 15-20 nm.
[0142] In order to improve the light extraction efficiency of the organic electroluminescent device, a light extraction layer (i.e., CPL layer, also called covering layer) may be added to the second electrode of the device. According to the principles of optical absorption and refraction, the refractive index of the CPL covering layer material should be as high as possible, and the absorption coefficient should be as small as possible. Any material known in the art can be used as the CPL layer material, such as Alq3, or N4,N4'-diphenyl-N4,N4'-di(9-phenyl-3-carbazolyl)biphenyl-4,4'-diamine. The thickness of the CPL covering layer is generally 5-300nm, preferably 20-100nm and more preferably 40-80nm.
[0143] The organic electroluminescent device of the present invention may further include an encapsulation structure. The encapsulation structure may be a protective structure that prevents foreign substances such as moisture and oxygen from entering the organic layer of the organic electroluminescent device. The encapsulation structure may be, for example, a can, such as a glass can or a metal can; or a thin film covering the entire surface of the organic layer.
[0144] The organic electroluminescent device may be any element that converts electrical energy into light energy or light energy into electrical energy without particular limitation, and may be, for example, an organic electroluminescent device, an organic light emitting diode, an organic solar cell, and an organic photoconductor. Herein, an organic light emitting diode is described as an example of an organic electroluminescent device (but the present invention is not limited thereto), and may be applied to other organic electroluminescent devices in the same manner.
[0145] In the case where the organic electroluminescent device is a top emission type, the first electrode may be a reflective electrode, and the second electrode may be a transmissive electrode or a semi-transmissive electrode. In the case where the organic electroluminescent device is a bottom emission type, the first electrode may be a transmissive electrode or a semi-transmissive electrode, and the second electrode may be a reflective electrode.
[0146] The present invention also relates to a method for preparing an organic electroluminescent device, which comprises laminating an anode, a hole injection layer, a hole transport layer, an electron blocking layer, an organic film layer, an electron transport layer, an electron injection layer and a cathode successively on a substrate, and optionally a covering layer. In this regard, vacuum deposition, vacuum evaporation, spin coating, casting, LB method, inkjet printing, laser printing or LITI methods can be used, but are not limited thereto. In the present invention, it is preferred to use a vacuum evaporation method to form the various layers. Those skilled in the art can conventionally select various process conditions in the vacuum evaporation method according to actual needs.
[0147] Exemplary embodiments have been disclosed herein, and although specific terms are used therein, these terms are used and interpreted only as general and descriptive meanings, and not for limiting purposes. In some cases, as will be apparent to those of ordinary skill in the art with the filing of this application, unless specifically indicated, the features, characteristics, and / or elements described in conjunction with a particular embodiment may be used alone or in combination with the features, characteristics, and / or elements described in conjunction with other embodiments. Accordingly, it will be understood by those skilled in the art that various changes may be made in form and detail without departing from the spirit and scope of the invention.
[0148] The raw materials involved in the synthesis examples of the present invention can be purchased from the market or obtained by conventional preparation methods in the art.
[0149] Preparation of reactant B-1:
[0150]
[0151] The raw material H-1 (50 mmol), the raw material S-1 (50 mmol) and potassium carbonate (150 mmol) were added to a mixture solvent of 300 mL toluene and 150 mL distilled water, stirred, and blown with N2 for 30 min. Pd(pph3)4 (1.0 mmol) was added to the solution, and the mixed solution was refluxed for 24 h. The mixed solution was cooled to room temperature, extracted with ethyl acetate and distilled water, and the organic layer was dried over anhydrous magnesium sulfate. The crude product was obtained by rotary evaporation in vacuum, and n-hexane / ethyl acetate (3:1) was used as the eluent. Purification was performed by silica gel column chromatography to obtain intermediate G-1;
[0152] Intermediate G-1 (35 mmol), tetrahydrofuran (60 mL) and glacial acetic acid (90 mL) were mixed and stirred at -10°C for 20 min. Tert-butyl nitrosate (105 mmol) was added via a syringe within 20 min. After stirring at -10°C for 1 h, the mixture was heated to 0°C and stirred for 12 h. The reaction mixture was heated to room temperature and diluted with 150 mL of water. The precipitated material was filtered and dried to obtain intermediate T-1.
[0153] In a three-necked flask, under nitrogen protection, 3 mmol of intermediate T-1, 6 mmol of bipyraclostrobin, 9 mmol of potassium acetate, 0.6 mmol of Sphos, and 0.12 mmol of Pd2(dba)3 were added to 150 mL of dioxane, and the reaction was refluxed for 8 h. The reaction system was cooled to room temperature, and the reaction mixture was diluted with ethyl acetate, washed with water, dried over anhydrous magnesium sulfate, and distilled under reduced pressure. Using n-heptane / ethyl acetate (9:1) as the eluent, it was purified by silica gel column chromatography to obtain reactant B-1.
[0154] Preparation of reactant B-2:
[0155]
[0156] The preparation method of reactant B-2 is the same as that of reactant B-1, except that raw material H-2 is used instead of raw material H-1.
[0157] Preparation of reactant B-3:
[0158]
[0159] The preparation method of reactant B-3 is the same as that of reactant B-1, except that raw material S-2 is used to replace raw material S-1, and raw material H-3 is used to replace raw material H-1.
[0160] Preparation of reactant B-4:
[0161]
[0162] The preparation method of reactant B-4 is the same as that of reactant B-1, except that raw material S-3 is used to replace raw material S-1, and raw material H-4 is used to replace raw material H-1.
[0163] Preparation of reactant B-5:
[0164]
[0165] The preparation method of reactant B-5 is the same as that of reactant B-1, except that raw material S-4 is used instead of raw material S-1.
[0166] Preparation of reactant B-6:
[0167]
[0168] The preparation method of reactant B-6 is the same as that of reactant B-3, except that raw material H-5 is used instead of raw material H-3.
[0169] Preparation of reactant B-7:
[0170]
[0171] The preparation method of reactant B-7 is the same as that of reactant B-3, except that raw material H-6 is used instead of raw material H-3.
[0172] Preparation of reactant B-8:
[0173]
[0174] The preparation method of reactant B-8 is the same as that of reactant B-3, except that raw material S-5 replaces raw material S-2, and raw material H-7 replaces raw material H-3.
[0175] Preparation of reactant B-9:
[0176]
[0177] The preparation method of reactant B-9 is the same as that of reactant B-3, except that raw material H-7 is used instead of raw material H-3.
[0178] Preparation of reactant B-10:
[0179]
[0180] The preparation method of reactant B-10 is the same as that of reactant B-3, except that raw material S-6 replaces raw material S-2, and raw material H-8 replaces raw material H-3.
[0181] Example 1: Preparation of Compound 15:
[0182]
[0183] In a 500ml three-necked flask, under nitrogen protection, add 0.01mol of reactant A-1, 0.01mol of reactant B-1, 0.03mol of sodium carbonate, 150mL of toluene, 30mL of ethanol, and 30mL of water, stir to mix, and then add 1.5×10 -4 mol Pd(pph3)4, heated to 105°C, refluxed for 10 hours, sampled, the reaction was complete, cooled naturally to room temperature, filtered, the filtrate was evaporated under reduced pressure (-0.09MPa, 85°C), passed through a neutral silica gel column (silica gel 100-200 mesh, eluent: chloroform: n-hexane = 1:3 (volume ratio)), to obtain compound 15.
[0184] Example 2: Preparation of Compound 16:
[0185]
[0186] The preparation method of compound 16 is the same as that of Example 1, except that reactant B-2 is used to replace reactant B-1.
[0187] Example 3: Preparation of Compound 26:
[0188]
[0189] The preparation method of compound 26 is the same as that of Example 1, except that reactant B-3 is used to replace reactant B-1.
[0190] Example 4: Preparation of Compound 31:
[0191]
[0192] The preparation method of compound 31 is the same as that of Example 1, except that reactant B-4 is used instead of reactant B-1.
[0193] Example 5: Preparation of Compound 79:
[0194]
[0195] The preparation method of compound 79 is the same as that of Example 1, except that reactant B-5 is used instead of reactant B-1.
[0196] Example 6: Preparation of Compound 87:
[0197]
[0198] The preparation method of compound 87 is the same as that of Example 1, except that reactant B-6 is used instead of reactant B-1.
[0199] Example 7: Preparation of Compound 105:
[0200]
[0201] The preparation method of compound 105 is the same as that of Example 1, except that reactant A-2 is used to replace reactant A-1, and reactant B-7 is used to replace reactant B-1.
[0202] Example 8: Preparation of Compound 106:
[0203]
[0204] The preparation method of compound 106 is the same as that of Example 1, except that reactant A-2 is used to replace reactant A-1, and reactant B-2 is used to replace reactant B-1.
[0205] Example 9: Preparation of Compound 108:
[0206]
[0207] The preparation method of compound 108 is the same as that of Example 1, except that reactant A-2 is used to replace reactant A-1, and reactant B-3 is used to replace reactant B-1.
[0208] Example 10: Preparation of Compound 143:
[0209]
[0210] The preparation method of intermediate T-10 is the same as that of intermediate T-1, except that raw material S-1 is replaced by raw material S-10, and raw material H-1 is replaced by raw material H-10 to obtain intermediate T-10;
[0211] In a 500ml three-necked flask, under nitrogen protection, add 0.01mol of raw material M-10, 0.01mol of intermediate T-10, 0.03mol of sodium carbonate, 150mL of toluene, 30mL of ethanol, and 30mL of water, stir and mix, then add 1.5×10 -4 mol Pd(pph3)4, heated to 105°C, refluxed for 10 hours, sampled, reacted completely, cooled naturally to room temperature, filtered, the filtrate was evaporated under reduced pressure (-0.09MPa, 85°C), passed through a neutral silica gel column (silica gel 100-200 mesh, eluent: chloroform: n-hexane = 1:3 (volume ratio)), to obtain intermediate N-10;
[0212] 0.01 mol of raw material D-1 and 0.012 mol of intermediate N-10 were added to 150 mL of toluene solvent. -5 mol Pd2(dba)3,5×10 -5 mol P(t-Bu)3, 0.03 mol sodium tert-butoxide, reflux reaction at 105°C for 24 h in a nitrogen atmosphere. Take a sample and confirm that the reaction is complete. After cooling to room temperature, the reaction mixture is filtered through a celite pad, rinsed with chloroform, and the filtrate is evaporated in vacuo. The crude product is passed through a silica gel column to obtain compound 143;
[0213] Example 11: Preparation of Compound 157:
[0214]
[0215] The preparation method of compound 157 is the same as that of Example 10, except that starting material S-11 is used instead of starting material S-10.
[0216] Example 12: Preparation of Compound 247:
[0217]
[0218] In a 500ml three-necked flask, under nitrogen protection, add 0.01mol of reactant A-3, 0.01mol of reactant B-3, 0.03mol of sodium carbonate, 150mL of toluene, 30mL of ethanol, and 30mL of water, stir to mix, and then add 1.5×10 -4 mol Pd(pph3)4, heated to 105°C, refluxed for 10 hours, sampled, reacted completely, cooled naturally to room temperature, filtered, the filtrate was evaporated under reduced pressure (-0.09MPa, 85°C), passed through a neutral silica gel column (silica gel 100-200 mesh, eluent: chloroform: n-hexane = 1:3 (volume ratio)), to obtain intermediate F-1;
[0219] In a 500ml three-necked flask, under nitrogen protection, add 0.01mol intermediate F-1, 0.01mol raw material D-2, 0.03mol sodium carbonate, 150mL toluene, 30mL ethanol, 30mL water, stir and mix, then add 1.5×10 -4 mol Pd(pph3)4, heated to 105°C, refluxed for 10 hours, sampled, reacted completely, cooled naturally to room temperature, filtered, the filtrate was evaporated under reduced pressure (-0.09 MPa, 85°C), passed through a neutral silica gel column (silica gel 100-200 mesh, eluent: chloroform: n-hexane = 1:3 (volume ratio)), to obtain compound 247;
[0220] Example 13: Preparation of Compound 291:
[0221]
[0222] The preparation method of compound 291 is the same as that of Example 1, except that reactant A-4 is used instead of reactant A-1.
[0223] Example 14: Preparation of Compound 306:
[0224]
[0225] The preparation method of compound 306 is the same as that of Example 1, except that reactant B-8 is used instead of reactant B-1.
[0226] Example 15: Preparation of Compound 307:
[0227]
[0228] The preparation method of compound 307 is the same as that of Example 1, except that reactant B-9 is used instead of reactant B-1.
[0229] Example 16: Preparation of Compound 308:
[0230]
[0231] The preparation method of compound 308 is the same as that of Example 1, except that reactant A-5 is used to replace reactant A-1, and reactant B-1 is used to replace reactant B-10.
[0232] Example 17: Preparation of Compound 309:
[0233]
[0234] The preparation method of compound 309 is the same as that of Example 1, except that reactant A-5 is used to replace reactant A-1, and reactant B-1 is used to replace reactant B-1.
[0235] Reactants B-8, B-9, and B-11 can also be obtained by conventional reactions using existing compounds (such as CAS: 2407622-24-4, 1589534-43-9, and 2271177-16-1) as raw materials and boron reagents.
[0236] In order to perform structural analysis on the compounds prepared in the examples, the molecular weights were measured by LC-MS as shown in Table 1:
[0237] Table 1
[0238]
[0239]
[0240] The compounds of the present invention are used in light-emitting devices and can be used as light-emitting layer materials. The compounds prepared in the above embodiments of the present invention were tested for their physicochemical and photoelectric properties, and the test results are shown in Table 2:
[0241] Table 2
[0242]
[0243]
[0244] Note: The triplet energy level T1 is tested by Horiba's Fluorolog-3 series fluorescence spectrometer, and the material test sample is 2*10 -5 mol / L toluene solution; the glass transition temperature Tg is measured by differential scanning calorimetry (DSC, DSC204F1 differential scanning calorimeter of NETZSCH, Germany), with a heating rate of 10°C / min; the highest occupied molecular orbital HOMO energy level is tested by an ionization energy test system (IPS-3), and the test is an atmospheric environment; Eg is tested by a double-beam UV-visible spectrophotometer (model: TU-1901), LUMO=HOMO+Eg. The electron mobility test is to make the material of the present invention into a single-charge device and measure it by the SCLC method.
[0245] From the data in the above table, it can be seen that the organic compound of the present invention has a high glass transition temperature (Tg), which can improve the phase stability and high temperature stability of the material film; the organic compound of the present invention has suitable HOMO and LUMO energy levels, which can reduce the injection barrier of carriers, reduce the device voltage and improve the device efficiency. The organic compound of the present invention has a higher T1 energy level, and can be used as a host material to ensure the energy transfer efficiency between the host and the guest, inhibit energy loss, and the organic compound of the present invention also has a higher electron mobility.
[0246] The following describes in detail the application effect of the OLED material synthesized by the present invention in the device through device examples 1-29 and device comparative examples 1-8. The device manufacturing process of the device examples 2-29 and device comparative examples 1-8 of the present invention is exactly the same as that of device example 1, and the same substrate material and electrode material are used, and the film thickness of the electrode material is also the same. The difference is that the light-emitting layer in the device is replaced.
[0247] Device Example 1
[0248] like Figure 1As shown, the transparent substrate layer 1 is a transparent PI film, and the anode layer 2 (ITO (15nm) / Ag (150nm) / ITO (15nm)) is washed, that is, washed with a detergent (SemiClean M-L20), washed with pure water, dried, and then washed with ultraviolet-ozone to remove organic residues on the surface of the anode layer. On the anode layer 2 after the above washing, HT-1 and P-1 are evaporated on the anode layer 2 using a vacuum evaporation device as a hole injection layer 3, with a film thickness of 10nm, and a mass ratio of HT-1 to P-1 of 97:3. Then HT-1 is evaporated as a hole transport layer 4 with a thickness of 130nm. Subsequently, EB-1 is evaporated as an electron blocking layer 5 with a thickness of 40nm. After the evaporation of the electron blocking layer material is completed, the light-emitting layer 6 of the OLED light-emitting device is prepared, and its structure includes the compound 15 and GH-1 used in the OLED light-emitting layer 6 as the main materials, GD-1 as the doping material, compound 15:GH-1:GD-1=47:47:6 (mass ratio), and the thickness of the light-emitting layer is 40nm. After the above-mentioned light-emitting layer 6, ET-1 and Liq are vacuum evaporated, the mass ratio of ET-1 and Liq is 1:1, the film thickness is 35nm, and this layer is the electron transport layer 7. On the electron transport layer 7, a LiF layer with a film thickness of 1nm is prepared by a vacuum evaporation device, and this layer is the electron injection layer 8. On the electron injection layer 8, a Mg:Ag electrode layer with a film thickness of 15nm is prepared by a vacuum evaporation device, and the mass ratio of Mg to Ag is 1:9, and this layer is the cathode layer 9. On the cathode layer 9, CP-1 is vacuum evaporated as the CPL layer 10, with a thickness of 70nm. The organic electroluminescent device 1 is obtained.
[0249] The molecular structure formula of the relevant materials is shown below:
[0250]
[0251]
[0252] After the OLED light-emitting device is completed as described above, the anode and cathode are connected with a known driving circuit, and the voltage, current efficiency, luminescence spectrum and device life of the device are measured. The device examples and comparative examples prepared by the same method are shown in Table 3; the voltage, current efficiency and 20 mA / cm 2 The test results of LT95 life under the conditions are shown in Table 4.
[0253] Table 3
[0254]
[0255]
[0256]
[0257] Table 4
[0258]
[0259]
[0260] Note: Voltage and current efficiency are calculated at a current density of 10 mA / cm 2 The test was conducted under the following conditions: IVL (current-voltage-luminance) test system (Suzhou Fushida Scientific Instrument Co., Ltd.); the life test system was EAS-62C OLED device life tester from Japan System Technology Co., Ltd.; the device life LT95 refers to the device life under the condition of current density of 20mA / cm 2 The device brightness decays to 95% of the initial brightness when the current density is 20mA / cm 2 When the temperature is 85°C, the time taken for the device brightness to decay to 95% of the initial brightness; the start-up voltage refers to the driving voltage of the device when the device brightness is 1 nit.
[0261] It can be seen from the device data results in Table 4 that compared with device comparison examples 1-4 and device comparison examples 5-8, the organic light-emitting devices using the compounds of the present invention have very obvious improvements in device life, and the degree of improvement is unexpected.
[0262] In order to compare the efficiency attenuation of different devices at high current density, the efficiency attenuation coefficient φ of each device is defined, φ=(μ m -μ 50 ) / μ m ; where μ m Expressed as the maximum current efficiency of the device, μ 50 Indicates that the driving current is 50mA / cm 2 The current efficiency of the device at the time of the current density is φ. The larger the φ value, the more serious the efficiency roll-off of the device. Conversely, it means that the problem of rapid attenuation of the device at high current density has been controlled. The present invention measured the efficiency attenuation coefficient φ of the device obtained in device embodiments 1-29 and device comparison examples 1-8, and the results are shown in Table 5:
[0263] Table 5
[0264]
[0265] It can be seen from the data in Table 5 that the organic light-emitting device prepared using the compound of the present invention has a smaller efficiency attenuation coefficient than that of the comparative example, indicating that the organic electroluminescent device prepared using the compound of the present invention can effectively reduce the efficiency roll-off of the device at high current density.
[0266] In summary, the above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. An organic electroluminescent device, comprising a first electrode, a second electrode and a functional layer, wherein the functional layer is located between the first electrode and the second electrode, the functional layer comprises a light-emitting layer, the light-emitting layer contains a light-emitting host material, and the light-emitting host material is a mixture of a triazine-containing compound and a compound shown in GH-1 to GH-170, characterized in that: The specific structure of the triazine-containing compound is any one of the following structures: The compounds represented by GH-1 to GH-170 are selected from any one of the following specific structures:
Citation Information
Patent Citations
Material for organic electroluminescent elements, organic electroluminescent element using same, and electronic device
CN105283977A
Compound for organic electronic element, and organic electronic element and electronic device using same
CN106573938A
Organic compound and application thereof in preparation of organic electroluminescence element
CN109912610A
Condensed cyclic compound and organic light-emitting device including the same
CN110642835A
Heterocyclic compound and organic light-emitting device comprising same
CN111278833A