Elastic wave device
By employing a multi-layer structure design in the elastic wave device, and utilizing the sound velocity relationship of different film layers and reflectors, the spurious problem caused by higher-order modes was solved, achieving effective wave suppression and frequency stability improvement over a wide bandwidth.
Patent Information
- Application Number
- CN202180027856.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-04-17
- Filing Date
- 2021-04-12
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2041-04-12
AI Technical Summary
Existing elastic wave devices suffer from spurious problems caused by higher-order modes, making it difficult to effectively suppress unwanted waves over a wide frequency band.
The design employs a multilayer structure, including a silicon substrate, first and second high-velocity sound films, first and second low-velocity sound films, and a piezoelectric film, to ensure the sound velocity relationship of the bulk wave in different film layers. Elastic waves are excited by setting IDT electrodes, and reflectors are set on the piezoelectric film to suppress higher-order modes.
It effectively suppresses higher-order modes and Rayleigh waves in a wide bandwidth, improves frequency temperature characteristics and frequency stability, and enhances the suppression effect of the bandwidth.
Smart Images

Figure CN115428337B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to elastic wave devices. Background Technology
[0002] Previously, elastic wave devices have been widely used in filters for portable telephones, etc. An example of an elastic wave device is disclosed in Patent Document 1 below. In this elastic wave device, a support substrate, a high-velocity sound film, a low-velocity sound film, and a piezoelectric film are stacked sequentially. An IDT (Interdigital Transducer) electrode is disposed on the piezoelectric film. By having the above-described stacked structure, the Q value of this elastic wave device can be improved. It should be noted that silicon is an example of a material used for the support substrate.
[0003] Prior art literature
[0004] Patent documents
[0005] Patent Document 1: International Publication No. 2012 / 086639 Summary of the Invention
[0006] The problem the invention aims to solve
[0007] However, in the elastic wave device described in Patent Document 1, stray noise caused by higher-order modes may be generated.
[0008] The purpose of this invention is to provide an elastic wave device capable of suppressing unwanted waves such as higher-order modes over a wide frequency band.
[0009] means for solving problems
[0010] The elastic wave device of the present invention comprises: a silicon substrate; a first high-velocity acoustic wave membrane disposed on the silicon substrate; a first low-velocity acoustic wave membrane disposed on the first high-velocity acoustic wave membrane; a second low-velocity acoustic wave membrane disposed on the first low-velocity acoustic wave membrane; a second high-velocity acoustic wave membrane disposed on the second low-velocity acoustic wave membrane; a piezoelectric membrane disposed on the second high-velocity acoustic wave membrane; and an IDT electrode disposed on the piezoelectric membrane. The sound velocity of the bulk wave propagating on the first high-velocity acoustic wave membrane and the sound velocity of the bulk wave propagating on the second high-velocity acoustic wave membrane are higher than the sound velocity of the elastic wave propagating on the piezoelectric membrane, and the sound velocity of the bulk wave propagating on the first low-velocity acoustic wave membrane and the sound velocity of the bulk wave propagating on the second low-velocity acoustic wave membrane are lower than the sound velocity of the bulk wave propagating on the piezoelectric membrane. The material of the first low-velocity acoustic wave membrane is different from the material of the second low-velocity acoustic wave membrane.
[0011] Invention Effects
[0012] The elastic wave device according to the present invention can suppress unwanted waves such as higher-order modes in a wide frequency band. Attached Figure Description
[0013] Figure 1 This is a front cross-sectional view showing a portion of the elastic wave device according to a first embodiment of the present invention.
[0014] Figure 2 This is a top view of the elastic wave device according to the first embodiment of the present invention.
[0015] Figure 3 This is a schematic diagram illustrating the definition of the crystal axis of silicon.
[0016] Figure 4 This is a schematic diagram showing the (111) facet of silicon.
[0017] Figure 5 This is a diagram showing the crystal axis of the (111) plane of silicon when viewed from the XY plane.
[0018] Figure 6 This is a schematic diagram showing the (100) facet of silicon.
[0019] Figure 7 This is a schematic diagram showing the (110) facet of silicon.
[0020] Figure 8 It is used to describe the direction vector k 111 A schematic cross-sectional view.
[0021] Figure 9 It is used to describe the direction vector k 111 A schematic top view.
[0022] Figure 10 This is a schematic diagram showing the [11-2] orientation of silicon.
[0023] Figure 11 It is used to explain angle α 111 A schematic diagram.
[0024] Figure 12 This is a front cross-sectional view of a portion of the layer structure of a comparative example elastic wave device.
[0025] Figure 13 This is a diagram illustrating the phase characteristics of the elastic wave device according to the first embodiment and comparative example of the present invention.
[0026] Figure 14 This is a diagram illustrating the phase characteristics in Embodiments 1 and 2 of the present invention.
[0027] Figure 15 This is a diagram illustrating the phase characteristics in Embodiments 3 and 4 of the present invention.
[0028] Figure 16 This is a diagram illustrating the phase characteristics in Embodiments 5 and 6 of the present invention.
[0029] Figure 17 This is a graph showing the relationship between the cutting angle of the LiTaO3 film and the phase of the Rayleigh wave.
[0030] Figure 18 This is a diagram showing the phase characteristics of the elastic wave device according to the second embodiment of the present invention. Detailed Implementation
[0031] Hereinafter, specific embodiments of the present invention will be described with reference to the accompanying drawings, thereby making the present invention clear.
[0032] It should be noted that the embodiments described in this specification are illustrative, and it is indicated in advance that partial substitutions or combinations of structures can be made between different embodiments.
[0033] Figure 1 This is a front cross-sectional view showing a portion of the elastic wave device according to a first embodiment of the present invention. Figure 2 This is a top view of the elastic wave device according to the first embodiment. It should be noted that... Figure 1 It is along Figure 2 A sectional view along line II in the diagram.
[0034] like Figure 1 As shown, the elastic wave device 1 includes a silicon substrate 2, a first high-velocity acoustic membrane 3, a first low-velocity acoustic membrane 4, a second low-velocity acoustic membrane 5, a second high-velocity acoustic membrane 6, and a piezoelectric membrane 7. More specifically, the first high-velocity acoustic membrane 3 is disposed on the silicon substrate 2. The first low-velocity acoustic membrane 4 is disposed on the first high-velocity acoustic membrane 3. The second low-velocity acoustic membrane 5 is disposed on the first low-velocity acoustic membrane 4. The second high-velocity acoustic membrane 6 is disposed on the second low-velocity acoustic membrane 5. The piezoelectric membrane 7 is disposed on the second high-velocity acoustic membrane 6.
[0035] An IDT electrode 8 is disposed on the piezoelectric film 7. An elastic wave is excited by applying an AC voltage to the IDT electrode 8. Figure 2 As shown, a pair of reflectors 9A and 9B are disposed on both sides of the IDT electrode 8 on the piezoelectric film 7 in the direction of elastic wave propagation. The elastic wave device 1 is a surface acoustic wave resonator. However, the elastic wave device of the present invention is not limited to an elastic wave resonator, but may also be a filter device or multiplexer with an elastic wave resonator.
[0036] like Figure 2As shown, the IDT electrode 8 has a first busbar 16, a second busbar 17, a plurality of first electrode fingers 18, and a plurality of second electrode fingers 19. The first busbar 16 and the second busbar 17 are opposite to each other. One end of each of the plurality of first electrode fingers 18 is connected to the first busbar 16. One end of each of the plurality of second electrode fingers 19 is connected to the second busbar 17. The plurality of first electrode fingers 18 and the plurality of second electrode fingers 19 are inserted alternately. It should be noted that in this specification, the direction of elastic wave propagation is set as the X direction. The direction in which the first electrode fingers 18 and the second electrode fingers 19 of the IDT electrode 8 extend is set as the Y direction. The thickness direction of the IDT electrode 8, the piezoelectric film 7, and the silicon substrate 2 is set as the Z direction.
[0037] The IDT electrode 8, reflector 9A, and reflector 9B comprise a stacked metal film. More specifically, a Ti layer, an Al layer, and a Ti layer are sequentially stacked in the stacked metal film. However, the materials of the IDT electrode 8, reflector 9A, and reflector 9B are not limited to those described above. Alternatively, the IDT electrode 8, reflector 9A, and reflector 9B may also comprise a single-layer metal film.
[0038] return Figure 1 The piezoelectric film 7 is a lithium tantalate film. More specifically, the piezoelectric film 7 is a LiTaO3 film with a 40° Y-angle cut to the X-axis. It should be noted that the material and cutting angle of the piezoelectric film 7 are not limited to those described above. For example, lithium niobate can also be used as the material of the piezoelectric film 7. For example, LiNbO3 can be used as lithium niobate. When the piezoelectric film 7 is a LiTaO3 film, the Euler angles of the piezoelectric film 7 are set to (LTφ, LTθ, LTψ). It should be noted that the piezoelectric film 7 has a crystal axis (X... P Y P Z P ).
[0039] Figure 1 The first hypersonic membrane 3 and the second hypersonic membrane 6 shown are membranes with relatively high sound speeds. More specifically, the sound speed of the bulk wave propagating in the first hypersonic membrane 3 is higher than the sound speed of the elastic wave propagating in the piezoelectric membrane 7. Similarly, the sound speed of the bulk wave propagating in the second hypersonic membrane 6 is higher than the sound speed of the elastic wave propagating in the piezoelectric membrane 7. In this embodiment, both the first hypersonic membrane 3 and the second hypersonic membrane 6 are silicon nitride films. More specifically, both the first hypersonic membrane 3 and the second hypersonic membrane 6 are SiN films. It should be noted that the materials of the first hypersonic membrane 3 and the second hypersonic membrane 6 are not limited to the above; for example, a dielectric material mainly composed of hafnium oxide, tungsten oxide, or niobium pentoxide can also be used.
[0040] In this embodiment, the first hypersonic membrane 3 and the second hypersonic membrane 6 are made of the same material. However, the materials of the first hypersonic membrane 3 and the second hypersonic membrane 6 may also be different.
[0041] The first low-velocity sound film 4 and the second low-velocity sound film 5 are films with relatively low sound speeds. More specifically, the sound speed of the bulk wave propagating in the first low-velocity sound film 4 is lower than the sound speed of the bulk wave propagating in the piezoelectric film 7. Similarly, the sound speed of the bulk wave propagating in the second low-velocity sound film 5 is lower than the sound speed of the bulk wave propagating in the piezoelectric film 7. In this embodiment, the first low-velocity sound film 4 is a silicon oxide film. Silicon oxide is composed of SiO2. a The symbol 'a' represents any positive number. The silicon oxide constituting the first low-velocity film 4 in this embodiment is SiO2. On the other hand, the second low-velocity film 5 is a tantalum pentoxide film. More specifically, the second low-velocity film 5 is a Ta2O5 film. Thus, the materials of the first low-velocity film 4 and the second low-velocity film 5 are different. It should be noted that the materials of the first low-velocity film 4 and the second low-velocity film 5 are not limited to the above; for example, materials with glass, silicon oxynitride, lithium oxide, tantalum pentoxide, silicon oxide, or compounds obtained by adding fluorine, carbon, or boron to silicon oxide as the main component can be used.
[0042] The materials of the first low-velocity membrane 4 and the second low-velocity membrane 5 can be different. However, the first low-velocity membrane 4 or the second low-velocity membrane 5 is preferably a SiO2 film. In this case, the absolute value of the temperature coefficient of frequency (TCF) of the elastic wave device 1 can be reduced, and the frequency temperature characteristics can be improved.
[0043] This embodiment is characterized by the sequential stacking of a silicon substrate 2, a first high-velocity acoustic film 3, a first low-velocity acoustic film 4, a second low-velocity acoustic film 5, a second high-velocity acoustic film 6, and a piezoelectric film 7, wherein the materials of the first low-velocity acoustic film 4 and the second low-velocity acoustic film 5 are different. This allows for the suppression of unwanted waves such as higher-order modes over a wide frequency band. The details of this effect will be explained below along with the definitions of crystal axis and plane orientation.
[0044] Figure 3 This is a schematic diagram illustrating the definition of the crystal axis of silicon. Figure 4 This is a schematic diagram showing the (111) facet of silicon. Figure 5 This is a diagram showing the crystal axis of the (111) plane of silicon when viewed from the XY plane. Figure 6 This is a schematic diagram showing the (100) facet of silicon. Figure 7 This is a schematic diagram showing the (110) facet of silicon.
[0045] The silicon substrate 2 described above is a single-crystal silicon substrate. For example... Figure 3 As shown, silicon has a diamond structure. In this specification, the crystal axis of silicon constituting the silicon substrate is [X]. Si Y Si Z Si In silicon, due to the symmetry of the crystal structure, X Si Axis, Y Si Axis and Z Si The axes are equivalent. For example... Figure 5 As shown, in the (111) plane, it is three-fold in-plane symmetry, which is equivalent to a 120° rotation crystal structure.
[0046] The silicon substrate 2 in this embodiment has a face orientation of (111). The face orientation of (111) indicates that the substrate is obtained by cutting within the (111) plane, which is orthogonal to the crystal axis represented by the Miller index
[111] , in a silicon crystal structure having a diamond structure. It should be noted that the (111) plane is... Figure 4 and Figure 5 The face shown. However, it also includes other crystallographically equivalent faces.
[0047] It should be noted that the orientation of the silicon substrate 2 is not limited to the above; for example, it can also be (100) or (110). An orientation of (100) indicates that the substrate is obtained by cutting within a (100) plane, which is orthogonal to the crystal axis represented by the Miller index
[100] , in a silicon crystal structure having a diamond structure. Within the (100) plane, there is four-fold in-plane symmetry, resulting in a crystal structure equivalent to a 90° rotation. It should be noted that the (100) plane is... Figure 6 face shown.
[0048] On the other hand, the orientation (110) indicates that the substrate is obtained by cutting within the (110) plane, which is orthogonal to the crystal axis represented by the Miller index
[110] , in a silicon crystal structure with a diamond structure. Within the (110) plane, there is in-plane quadratic symmetry, resulting in a crystal structure equivalent to a 180° rotation. It should be noted that the (110) plane is... Figure 7 face shown.
[0049] The angle α and the direction vector k (described later) will be explained in detail below. It should be noted that the angle α is α... 111 α 110 and α 100 Any one of these three angles. The direction vector k is k 111 k 110 and k 100 Either of the two.
[0050] Figure 8 It is used to describe the direction vector k 111 A schematic cross-sectional view. Figure 9 It is used to describe the direction vector k 111 A schematic top view. It should be noted that... Figure 8 The orientation of the silicon substrate 2 is (111).
[0051] exist Figure 8 and Figure 9The example shown is when the Euler angle of the piezoelectric film 7 is (0°, -35°, 0°). This example shows an IDT electrode 8 disposed on the front side of the piezoelectric film 7. The (111) side of the silicon substrate 2 is in contact with the piezoelectric film 7.
[0052] Here, as Figure 8 As shown, the Z-axis of the piezoelectric material LiTaO3, which is projected onto the (111) surface of the silicon substrate 2 to form the piezoelectric film 7, is... P Let the direction vector obtained from the axis be k. 111 .like Figure 8 and Figure 9 As shown, the direction vector k 111 The direction of the electrode extension of IDT electrode 8 is parallel to the Y direction.
[0053] Figure 10 This is a schematic diagram showing the [11-2] orientation of silicon. Figure 11 It is used to explain angle α 111 A schematic diagram.
[0054] like Figure 10 As shown, the [11-2] orientation of silicon is represented as X in the crystal structure of silicon. Si Unit vector of direction, Y Si The unit vector of direction and Z Si The composite vector of a vector whose direction is -2 times that of the unit vector. For example... Figure 11 As shown, angle α 111 It is the direction vector k 111 The angle between the silicon substrate 2 and the [11-2] direction. It should be noted that, as mentioned above, due to the symmetry of the silicon crystal, the [11-2] direction, the [1-21] direction, and the [-211] direction are equivalent.
[0055] On the other hand, in a silicon substrate with a plane orientation of (110), a projection Z onto the (110) plane of the silicon substrate will be... P Let the direction vector obtained from the axis be k. i10 Angle α 110 It is the direction vector k 110 The angle between the
[001] direction and the silicon constituting the silicon substrate. It should be noted that, due to the symmetry of the silicon crystal, the
[001] direction,
[100] direction, and
[010] direction are equivalent.
[0056] In a silicon substrate with a plane orientation of (100), a projection Z is made onto the (100) plane of the silicon substrate. P Let the direction vector obtained from the axis be k. 100 Angle α 100 It is the direction vector k 100 The angle between the silicon substrate and the
[001] direction of the silicon.
[0057] It should be noted that the definitions of the direction vector k and the angle α are the same regardless of whether the silicon substrate is directly stacked on the piezoelectric film or indirectly stacked on the piezoelectric film via other layers. Figure 1 In the case shown, the silicon substrate 2 and the piezoelectric film 7 are indirectly stacked via a first high-velocity acoustic film 3, a first low-velocity acoustic film 4, a second low-velocity acoustic film 5, and a second high-velocity acoustic film 6. Even in this case, the aforementioned angle α is defined based on the surface orientation of the silicon substrate 2. 100 Angle α 110 Or angle α 111 .
[0058] By comparing this embodiment with the comparative example, it is shown that according to the elastic wave device 1, high-order modes can be suppressed in a wide frequency band.
[0059] like Figure 12 As shown, the comparative example differs from the first embodiment in its stacked structure. In the comparative example, a silicon substrate 102, a high-velocity acoustic film 103, a low-velocity acoustic film 104, and a piezoelectric film 107 are stacked sequentially.
[0060] The comparative examples include an elastic wave device having the structure of the first embodiment and its phase characteristics. The design parameters of the elastic wave device having the structure of the first embodiment are described below. It should be noted that the Euler angles of the silicon substrate 2 are set as (Siφ, Siθ, Siψ).
[0061] Silicon substrate 2: Planar orientation...(111), Euler angles (Siφ, Siθ, Siψ) in Siψ...46°
[0062] First hypersonic membrane 3: Material...SiN, thickness 300nm
[0063] First low-velocity membrane 4: Material...SiO2, thickness...100nm
[0064] Second low-velocity membrane 5: Material...Ta2O5, thickness...70nm
[0065] Second hypersonic membrane 6: Material...SiN, thickness...70nm
[0066] Piezoelectric film 7: Material...40° Y-cut X-propagated LiTaO3, thickness...350nm
[0067] Layer structure of IDT electrode 8: Layer structure... Ti layer / Al layer / Ti layer from the piezoelectric film 7 side, thickness... 12nm / 100nm / 4nm from the piezoelectric film 7 side.
[0068] The design parameters of the elastic wave device in the comparative example are as follows.
[0069] Silicon substrate 102: Planar orientation...(111), Siψ in Euler angles (Siφ, Siθ, Siψ)...73°
[0070] High-velocity acoustic film 103: Material...SiN, thickness 300nm
[0071] Low-velocity membrane 104: Material...SiO2, thickness...300nm
[0072] Piezoelectric film 107: Material...55° Y-cut X-propagation LiTaO3, thickness...400nm
[0073] Layer structure of IDT electrode 8: Layer structure... Ti layer / Al layer / Ti layer from the piezoelectric film 107 side, thickness... 12nm / 100nm / 4nm from the piezoelectric film 7 side.
[0074] Figure 13 This is a diagram showing the phase characteristics of the elastic wave device in the first embodiment and the comparative example.
[0075] like Figure 13 As indicated by arrow A, in the comparative example, higher-order modes are generated around 2.2 times the resonant frequency. In contrast, it can be seen that in the first embodiment, higher-order modes around 2.2 times the resonant frequency are suppressed. Furthermore, as indicated by arrow B, in the first embodiment, higher-order modes around 1.5 times the resonant frequency can also be suppressed. Moreover, in the first embodiment, unwanted waves such as higher-order modes can be suppressed over a wide frequency range of approximately 4000–5500 MHz compared to the comparative example. Thus, in the first embodiment, unwanted waves such as higher-order modes can be suppressed over a wide frequency band.
[0076] Here, the thickness of the first hypersonic membrane 3 is preferably greater than or equal to the thickness of the second hypersonic membrane 6. In this case, higher-order modes can be further suppressed. Details of this effect are shown below.
[0077] In the elastic wave device of the present invention, the thickness of the second hypersonic membrane 6 is fixed, while the thickness of the first hypersonic membrane 3 is varied, and phase characteristics are measured. Specifically, the thickness of the second hypersonic membrane 6 is set to 300 nm. The thickness of the first hypersonic membrane 3 is set to 100 nm or 500 nm. Thus, in one elastic wave device, the thickness of the first hypersonic membrane 3 is thinner than the thickness of the second hypersonic membrane 6. This is designated as Example 1. In another elastic wave device, the thickness of the first hypersonic membrane 3 is thicker than the thickness of the second hypersonic membrane 6. This is designated as Example 2.
[0078] Figure 14 This is a diagram showing the phase characteristics in Embodiment 1 and Embodiment 2.
[0079] like Figure 14 As shown, in both Embodiment 1 and Embodiment 2, high-order modes near 2800MHz are suppressed to less than -5deg. Furthermore, in both Embodiment 1 and Embodiment 2, unwanted waves are suppressed over a wide range of 2600–4000MHz. Here, it can be seen that in Embodiment 2, high-order modes near 2800MHz are further suppressed compared to Embodiment 1. Thus, when the thickness of the first hypersonic diaphragm 3 is greater than or equal to the thickness of the second hypersonic diaphragm 6, high-order modes can be suppressed even further.
[0080] The thickness of the first low-velocity diaphragm 4 is preferably greater than or equal to the thickness of the second low-velocity diaphragm 5. In this case, higher-order modes can be further suppressed. Details of this effect are shown below.
[0081] In the elastic wave device of the present invention, phase characteristics were measured by making the thicknesses of the first low-velocity membrane 4 and the second low-velocity membrane 5 different. Specifically, in one elastic wave device, the thickness of the first low-velocity membrane 4 was set to 100 nm, and the thickness of the second low-velocity membrane 5 was set to 300 nm. In this elastic wave device, the thickness of the first low-velocity membrane 4 was thinner than the thickness of the second low-velocity membrane 5. This is designated as Example 3. In another elastic wave device, the thickness of the first low-velocity membrane 4 was set to 300 nm, and the thickness of the second low-velocity membrane 5 was set to 100 nm. In this elastic wave device, the thickness of the first low-velocity membrane 4 was thicker than the thickness of the second low-velocity membrane 5. This is designated as Example 4.
[0082] Figure 15 This is a diagram showing the phase characteristics in Embodiments 3 and 4.
[0083] like Figure 15 As shown, in both Embodiment 3 and Embodiment 4, high-order modes near 3000MHz are suppressed to less than -55deg. Furthermore, in both Embodiment 3 and Embodiment 4, unwanted waves are suppressed over a wide range of 2600–4000MHz. Here, it can be seen that in Embodiment 4, high-order modes near 3000MHz are further suppressed compared to Embodiment 3. Thus, when the thickness of the first low-velocity diaphragm 4 is greater than or equal to the thickness of the second low-velocity diaphragm 5, high-order modes can be suppressed even further.
[0084] The thickness of the first high-velocity sound membrane 3 is preferably greater than or equal to the thickness of the first low-velocity sound membrane 4. This allows for further suppression of higher-order modes. Details of this effect are shown below.
[0085] In the elastic wave device of the present invention, phase characteristics were measured by making the thicknesses of the first high-velocity acoustic membrane 3 and the first low-velocity acoustic membrane 4 different. Specifically, in one elastic wave device, the thickness of the first high-velocity acoustic membrane 3 was set to 300 nm, and the thickness of the first low-velocity acoustic membrane 4 was set to 100 nm. In this elastic wave device, the thickness of the first high-velocity acoustic membrane 3 was thicker than the thickness of the first low-velocity acoustic membrane 4. This is designated as Example 5. In another elastic wave device, the thickness of the first high-velocity acoustic membrane 3 was set to 100 nm, and the thickness of the first low-velocity acoustic membrane 4 was set to 300 nm. In this elastic wave device, the thickness of the first high-velocity acoustic membrane 3 was thinner than the thickness of the first low-velocity acoustic membrane 4. This is designated as Example 6.
[0086] Figure 16 This is a diagram showing the phase characteristics in Embodiments 5 and 6.
[0087] like Figure 16 As shown, in both Embodiment 5 and Embodiment 6, high-order modes near 4400MHz are suppressed to less than -35deg. Furthermore, in both Embodiment 5 and Embodiment 6, unwanted waves are suppressed over a wide range of 2600–5000MHz. Here, it can be seen that in Embodiment 5, high-order modes near 4400MHz are further suppressed compared to Embodiment 6. Thus, when the thickness of the first hypersonic membrane 3 is greater than or equal to the thickness of the first hyposonic membrane 4, high-order modes can be suppressed even further.
[0088] However, as Figure 13 As indicated by arrow C in the diagram, in the comparative example, Rayleigh waves, which are unwanted waves, were generated at a frequency approximately 0.7 times the resonant frequency. In contrast, it can be seen that Rayleigh waves were suppressed in the first embodiment. This is because, in the elastic wave device 1, the piezoelectric film 7 is a LiTaO3 film with a cut angle of 40°Y. It should be noted that the same effect is achieved when the cut angle is within the range of (40±5)°Y. Therefore, when the piezoelectric film 7 is a LiTaO3 film, the cut angle is preferably within the range of (40±5)°Y. As a result, Rayleigh waves can be suppressed.
[0089] It should be noted that a dielectric film can also be provided on the piezoelectric film 7 to cover the IDT electrode 8, reflector 9A, and reflector 9B. For example, silicon oxide, silicon nitride, or silicon oxynitride can be used as the material for the dielectric film. However, the elastic wave device 1 may also not have a dielectric film.
[0090] Here, the wavelength defined by the distance between the electrode fingers of IDT electrode 8 is denoted as λ. It should be noted that the distance between the electrode fingers refers to the distance between the centers of adjacent electrode fingers. Specifically, it refers to the distance between the center points of adjacent electrode fingers in the direction of elastic wave propagation, i.e., the X-direction. When the distance between the center points of the electrode fingers is not fixed, the distance between the electrode fingers is assumed to be the average value of the distances between the center points of the electrode fingers.
[0091] Furthermore, the thickness of the first hypersonic film 3 is set to t_SiN-1[λ], and the thickness of the second hypersonic film 6 is set to t_SiN-2[λ]. The thickness of the first hyposonic film 4 is set to t_SiO2[λ], and the thickness of the second hyposonic film 5 is set to t_Ta2O5[λ]. The thickness of the piezoelectric film 7 is set to t_LT[λ]. The higher-order mode at 1.5 times the resonant frequency is set as the first higher-order mode. By varying t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], t_LT[λ], LTθ, and Siψ, the phase of the first higher-order mode is measured. It should be noted that the orientation of the silicon substrate 2 is (111). Thus, the relationship between each parameter and the phase of the first higher-order mode is derived, namely Equation 1.
[0092] [Formula 1]
[0093] Spurious phase [deg] = (-64.7738492449743) + 0.799535874292877 × (Siψ - 23.2121158601201) + (-0.00639116627879308) × (LTθ - 131.246414694454) + 228.498817195313 × ((t_LT[λ]) - 0.180166902154725) + (-551.916118464126) × ((t_SiN-2[λ]) - 0.0291537442599814) + 1142.73591823813 × ((t_Ta2O5[λ]) - 0.0421024373013005) + 155.359547985879 × ((t_SiO2[λ]) - 0.121307841752057) + (-29.8438742957074) × ((t_SiN-1[λ]) - 0.263987107029325) + (-0.0245466642133507) × ((Siψ - 23.2121158601201) × (Siψ - 23.2121158601201) - 540.379061966296) + (-0.00862413439802871) × ((Siψ - 23.2121158601201) × (LTθ - 131.246414694454)) + 0.249067774425361 × ((LTθ - 131.246414694454) × (LTθ - 131.246414694454) - 5.81473016925011) + 6.93659125135011 × ((Siψ - 23.2121158601201) × ((t_LT[λ]) - 0.180166902154725)) + 10.0784200297745 × ((LTθ - 131.246414694454) × ((t_LT[λ]) - 0.180166902154725)) + 116.492602498829 × (((t_LT[λ]) - 0.180166902154725) × ((t_LT[λ]) - 0.180166902154725) - 0.000346559038760835) + 6.96592368109737 × ((Siψ - 23.2121158601201) × ((t_SiN-2[λ]) - 0.0291537442599814)) + (-15.0647392900912) × ((LTθ - 131.246414694454) × ((t_SiN-2[λ]) - 0.0291537442599814))+3185.48452246456×(((t_LT[λ])-0.180166902154725)×((t_SiN-2[λ])-0.0291537442599814))+6533.48929488482×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiN-2[λ])-0.0291537442599814)-0.000458154170897422)+7.78801893149455×((Siψ-23.212115860120 1)×((t_Ta2O5[λ])-0.0421024373013005))+53.7418010590521×((LTθ-131.246414694454)×((t_Ta2O5[λ])-0.0421024373013005))+6146.78344504674×(((t_LT[λ])-0.180166902154725)×((t_Ta2O5[λ])-0.0421024373013005))+(-14578.5920718871)×(((t_SiN-2[λ])-0.02915374425998 14)×((t_Ta2O5[λ])-0.0421024373013005))+28614.912170246×(((t_Ta2O5[λ])-0.0421024373013005)×((t_Ta2O5[λ])-0.0421024373013005)-0.000324766882084902)+4.59563385312738×((Siψ-23.2121158601201)×((t_SiO2[λ])-0.121307841752057))+1.7616110343796×((LTθ-131.24 6414694454)×((t_SiO2[λ])-0.121307841752057))+1984.12416812403×(((t_LT[λ])-0.180166902154725)×((t_SiO2[λ])-0.121307841752057))+(-202.795292688935)×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiO2[λ])-0.121307841752057))+5166.03124069752×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiO2[λ])-0.121307841752057))+(-346.648683117878)×(((t_SiO2[λ])-0.1213078 41752057)×((t_SiO2[λ])-0.121307841752057)-0.0017442053041025)+1.13949852542765×((Siψ-23.212115 8601201)×((t_SiN-1[λ])-0.263987107029325))+(-2.10309868792554)×((LTθ-131.246414694454)×((t_SiN -1[λ])-0.263987107029325))+342.49568371403×(((t_LT[λ])-0.180166902154725)×((t_SiN-1[λ])-0.26398 7107029325))+735.741591105701×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiN-1[λ])-0.2639871070293 25))+(-2014.8497951455)×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiN-1[λ])-0.263987107029325))+13 1.054784086532×(((t_SiO2[λ])-0.121307841752057)×((t_SiN-1[λ])-0.263987107029325))+145.44196544 8516×(((t_SiN-1[λ])-0.263987107029325)×((t_SiN-1[λ])-0.263987107029325)-0.0132035793109828)…Equation 1.
[0094] When the plane orientation of the silicon substrate 2 is (111), the phase derived by Equation 1 is preferably -70 degrees or less. More specifically, t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], t_LT[λ], LTθ, and Siψ are preferably thicknesses and angles within the range where the phase derived by Equation 1 is -70 degrees or less. As a result, the phase of the first higher-order mode can be made -70 degrees or less more reliably. Therefore, the first higher-order mode can be suppressed more reliably and effectively.
[0095] The higher-order mode at a frequency 2.2 times the resonant frequency is designated as the second higher-order mode. The phases of the first and second higher-order modes were measured in the same manner as in the derivation of Equation 1. It should be noted that the plane orientation of the silicon substrate 2 is (111). Therefore, the relationship between each parameter and the phases of the first and second higher-order modes is derived, namely Equation 2.
[0096] [Formula 2]
[0097] Spurious phase [deg] = (-49.4236088933048) + 0.927126211958592 × (Siψ - 23.2121158601201) + 0.680023816107774 × (LTθ - 131.246414694454) + 213.742276430449 × ((t_LT[λ]) - 0.180166902154725) + (-606.139116757393) × ((t_SiN-2[λ]) - 0.0291537442599814) + 692.814216558718 × ((t_Ta2O5[λ]) - 0.0421024373013005) + 195.183979143557 × ((t_SiO2[λ]) - 0.121307841752057) + (-83.0452792358909) × ((t_SiN-1[λ]) - 0.263987107029325) + (-0.0279599052855905) × ((Siψ - 23.2121158601201) × (Siψ - 23.2121158601201) - 540.379061966296) + (-0.0139285317562481) × ((Siψ - 23.2121158601201) × (LTθ - 131.246414694454)) + 0.293983576167198 × ((LTθ - 131.246414694454) × (LTθ - 131.246414694454) - 5.81473016925011) + 9.82906312217327 × ((Siψ - 23.2121158601201) × ((t_LT[λ]) - 0.180166902154725)) + 20.4897039882144 × ((LTθ - 131.246414694454) × ((t_LT[λ]) - 0.180166902154725)) + (-1822.1825017687) × (((t_LT[λ]) - 0.180166902154725) × ((t_LT[λ]) - 0.180166902154725) - 0.000346559038760835) + 6.57985243569614 × ((Siψ - 23.2121158601201) × ((t_SiN-2[λ]) - 0.0291537442599814)) + (-16.3487857288392) × ((LTθ - 131.246414694454) × ((t_SiN-2[λ]) - 0.0291537442599814))+3022.4142953683×(((t_LT[λ])-0.180166902154725)×((t_SiN-2[λ])-0.0291537442599814))+6106.28960321182×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiN-2[λ])-0.0291537442599814)-0.000458154170897422)+7.61287198883346×((Siψ-23.2121158601201) ×((t_Ta2O5[λ])-0.0421024373013005))+32.0420324509525×((LTθ-131.246414694454)×((t_Ta2O5[λ])-0.0421024373013005))+(-5600.23059801591)×(((t_LT[λ])-0.180166902154725)×((t_Ta2O5[λ])-0.0421024373013005))+(-12480.4143612638)×(((t_SiN-2[λ])-0.02915374425998 14)×((t_Ta2O5[λ])-0.0421024373013005))+9462.56388912554×(((t_Ta2O5[λ])-0.0421024373013005)×((t_Ta2O5[λ])-0.0421024373013005)-0.000324766882084902)+4.75660770269025×((Siψ-23.2121158601201)×((t_SiO2[λ])-0.121307841752057))+3.138310645423×((LTθ-131.246 414694454)×((t_SiO2[λ])-0.121307841752057))+782.245112149574×(((t_LT[λ])-0.180166902154725)×((t_SiO2[λ])-0.121307841752057))+(-1849.48045553917)×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiO2[λ])-0.121307841752057))+(-657.25929805289)×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiO2[λ])-0.121307841752057))+(-111.444658339511)×(((t_SiO2[λ])-0.1213078 41752057)×((t_SiO2[λ])-0.121307841752057)-0.0017442053041025)+1.37817174855647×((Siψ-23.2121158 601201)×((t_SiN-1[λ])-0.263987107029325))+(-1.7087256650039)×((LTθ-131.246414694454)×((t_SiN-1[ λ])-0.263987107029325))+(-396.636995545448)×(((t_LT[λ])-0.180166902154725)×((t_SiN-1[λ])-0.2639 87107029325))+434.882453748749×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiN-1[λ])-0.263987107029 325))+(-1660.0685005439)×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiN-1[λ])-0.263987107029325))+1 06.322544176659×(((t_SiO2[λ])-0.121307841752057)×((t_SiN-1[λ])-0.263987107029325))+172.37224683 1877×(((t_SiN-1[λ])-0.263987107029325)×((t_SiN-1[λ])-0.263987107029325)-0.0132035793109828)…Equation 2.
[0098] When the plane orientation of the silicon substrate 2 is (111), the phase derived by Equation 2 is preferably -70 degrees or less. More specifically, t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], t_LT[λ], LTθ, and Siψ are preferably thicknesses and angles within the range where the phase derived by Equation 2 is -70 degrees or less. As a result, the phases of the first higher-order mode and the second higher-order mode can be made less than -70 degrees more reliably. Therefore, the first higher-order mode and the second higher-order mode can be suppressed more reliably and effectively.
[0099] The phases of the Rayleigh wave, the first higher-order mode, and the second higher-order mode were measured in the same manner as in the derivation of Equation 1. It should be noted that the orientation of the silicon substrate 2 is (111). Thus, the relationship between each parameter and the phases of the Rayleigh wave, the first higher-order mode, and the second higher-order mode is derived, namely Equation 3.
[0100] [Formula 3]
[0101] Spurious phase [deg] = (-49.446344512493) + 0.926632614160644 × (Siψ-23.2121158601201) + 0.689805009201412 × (LTθ-131.246414694454) + 213.186056884304 × ((t_LT[λ])-0.180166902154725) + (-605.162234862408) × ((t_SiN-2[λ])-0.0291537442599814) + 693.090367188157 × ((t_Ta2O5[λ])-0.0421024373013005) + 194.973246854906 × ((t_SiO2[λ])-0.121307841752057) + (-82.9891258698242) × ((t_SiN-1[λ])-0.263987107029325) + (-0.0279312228697236) × ((Siψ-23.2121158601201) × (Siψ-23.2121158601201)-540.379061966296) + (-0.0129242968044351) × ((Siψ-23.2121158601201) × (LTθ-131.246414694454)) + 0.285438486600616 × ((LTθ-131.246414694454) × (LTθ-131.246414694454)-5.81473016925011) + 9.7873873803375 × ((Siψ-23.2121158601201) × ((t_LT[λ])-0.180166902154725)) + 20.1009127346539 × ((LTθ-131.246414694454) × ((t_LT[λ])-0.180166902154725)) + (-1845.21253448418) × (((t_LT[λ])-0.180166902154725) × ((t_LT[λ])-0.180166902154725)-0.000346559038760835) + 6.50543677488646 × ((Siψ-23.2121158601201) × ((t_SiN-2[λ])-0.0291537442599814)) + (-17.1312681888354) × ((LTθ-131.246414694454) × ((t_SiN-2[λ])-0.0291537442599814))+3096.79723705848×(((t_LT[λ])-0.180166902154725)×((t_SiN-2[λ])-0.0291537442599814))+6184.77577365764×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiN-2[λ])-0.0291537442599814)-0.000458154170897422)+7.56134934721394×((Siψ-23.2121158601201) ×((t_Ta2O5[λ])-0.0421024373013005))+31.4231915519825×((LTθ-131.246414694454)×((t_Ta2O5[λ])-0.0421024373013005))+(-5550.14180216517)×(((t_LT[λ])-0.180166902154725)×((t_Ta2O5[λ])-0.0421024373013005))+(-12378.8114606327)×(((t_SiN-2[λ])-0.029153744259981 4)×((t_Ta2O5[λ])-0.0421024373013005))+9488.76758932007×(((t_Ta2O5[λ])-0.0421024373013005)×((t_Ta2O5[λ])-0.0421024373013005)-0.000324766882084902)+4.72906984538813×((Siψ-23.2121158601201)×((t_SiO2[λ])-0.121307841752057))+2.92834698440594×((LTθ-131.246 414694454)×((t_SiO2[λ])-0.121307841752057))+795.397518262681×(((t_LT[λ])-0.180166902154725)×((t_SiO2[λ])-0.121307841752057))+(-1810.07736779714)×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiO2[λ])-0.121307841752057))+(-633.635642829976)×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiO2[λ])-0.121307841752057))+(-115.182409805846)×(((t_SiO2[λ])-0.1213078 41752057)×((t_SiO2[λ])-0.121307841752057)-0.0017442053041025)+1.36398286740725×((Siψ-23.2121158 601201)×((t_SiN-1[λ])-0.263987107029325))+(-1.83297695480188)×((LTθ-131.246414694454)×((t_SiN-1 [λ])-0.263987107029325))+(-387.007695236215)×(((t_LT[λ])-0.180166902154725)×((t_SiN-1[λ])-0.263 987107029325))+456.19886315614×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiN-1[λ])-0.2639871070293 25))+(-1644.59679209231)×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiN-1[λ])-0.263987107029325))+1 13.144234117703×(((t_SiO2[λ])-0.121307841752057)×((t_SiN-1[λ])-0.263987107029325))+173.43876195 1382×(((t_SiN-1[λ])-0.263987107029325)×((t_SiN-1[λ])-0.263987107029325)-0.0132035793109828)…Equation 3.
[0102] When the plane orientation of the silicon substrate 2 is (111), the phase derived by Equation 3 is preferably -70 degrees or less. More specifically, the thicknesses and angles of t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], t_LT[λ], LTθ, and Siψ are preferably within the range where the phase derived by Equation 3 is -70 degrees or less. As a result, the phases of the Rayleigh wave, the first higher-order mode, and the second higher-order mode can be made -70 degrees or less more reliably. Therefore, the Rayleigh wave, the first higher-order mode, and the second higher-order mode can be suppressed more reliably and effectively.
[0103] With the orientation of the silicon substrate 2 set to (110), the phase of the first higher-order mode was measured in the same manner as in the derivation of Equation 1. Thus, the relationship between each parameter and the phase of the first higher-order mode was derived, namely Equation 4.
[0104] [Formula 4]
[0105] Spurious phase [deg] = (-35.4828976785632) + (-565.645491469017) × ((t_SiN-2[λ]) - 0.0350204955532028) + 1015.0372961359 × ((t_Ta2O5[λ]) - 0.0349996340079728) + 144.752343074804 × ((t_SiO2[λ]) - 0.125000914980053) + (-46.0415586945303) × ((t_SiN-1[λ]) - 0.224927716575792) + 1.04686816500004 × ((Siψ) - 45.0067708523954) + 10682.9573639156 × (((t_SiN-2[λ]) - 0.0350204955532028) × ((t_SiN-2[λ]) - 0.0350204955532028) - 0.000399831223602513) + (-13343.4260197881) × (((t_SiN-2[λ]) - 0.0350204955532028) × ((t_Ta2O5[λ]) - 0.0349996340079728)) + 14953.0137418577 × (((t_Ta2O5[λ]) - 0.0349996340079728) × ((t_Ta2O5[λ]) - 0.0349996340079728) - 0.000400054898669248) + 739.132582722994 × (((t_SiN-2[λ]) - 0.0350204955532028) × ((t_SiO2[λ]) - 0.125000914980053)) + 4235.91445978005 × (((t_Ta2O5[λ]) - 0.0349996340079728) × ((t_SiO2[λ]) - 0.125000914980053)) + 209.756610061409 × (((t_SiO2[λ]) - 0.125000914980053) × ((t_SiO2[λ]) - 0.125000914980053) - 0.00250052611269396) + 575.276037855751 × (((t_SiN-2[λ]) - 0.0350204955532028) × ((t_SiN-1[λ]) - 0.224927716575792)) + (-1900.54066286617) × (((t_Ta2O5[λ]) - 0.0349996340079728)×((t_SiN-1[λ])-0.224927716575792))+(-361.044865348212)×(((t_SiO2 [λ])-0.125000914980053)×((t_SiN-1[λ])-0.224927716575792))+(-12.6866065936889)×(((t _SiN-1[λ])-0.224927716575792)×((t_SiN-1[λ])-0.224927716575792)-0.0131316741294957 )+(-15.0286853820076)×(((t_SiN-2[λ])-0.0350204955532028)×((Siψ)-45.0067708523954)) +2.30649064625795×(((t_Ta2O5[λ])-0.0349996340079728)×((Siψ)-45.0067708523954))+(- 2.93242042531494)×(((t_SiO2[λ])-0.125000914980053)×((Siψ)-45.0067708523954))+0.490 207176672433×(((t_SiN-1[λ])-0.224927716575792)×((Siψ)-45.0067708523954))+0.0236394 426428729×(((Siψ)-45.0067708523954)×((Siψ)-45.0067708523954)-825.841735805153)…Equation 4.
[0106] When the plane orientation of the silicon substrate 2 is (110), the phase derived by Equation 4 is preferably -70 degrees or less. More specifically, the thickness and angle of t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], and Siψ are preferably within the range where the phase derived by Equation 4 is -70 degrees or less. As a result, the phase of the first higher-order mode can be made to be -70 degrees or less more reliably. Therefore, the first higher-order mode can be suppressed more reliably and effectively.
[0107] With the orientation of the silicon substrate 2 set to (110), the phases of the first and second higher-order modes were measured in the same manner as in the derivation of Equation 1. Thus, the relationship between each parameter and the phases of the first and second higher-order modes was derived, namely Equation 5.
[0108] [Formula 5]
[0109] Spurious phase [deg] = (-21.043074633666) + (-607.846047314191) × ((t_SiN-2[λ])-0.0350204955532028) + 835.570016969633 × ((t_Ta2O5[λ])-0.0349996340079728) + 218.780632745606 × ((t_SiO2[λ])-0.125000914980053) + (-72.9770468417362) × ((t_SiN-1[λ])-0.224927716575792) + 0.771180072449541 × ((Siψ)-45.0067708523954) + 9068.29091824635 × (((t_SiN-2[λ])-0.0350204955532028) × ((t_SiN-2[λ])-0.0350204955532028)-0.000399831223602513) + (-13159.8293417283) × (((t_SiN-2[λ])-0.0350204955532028) × ((t_Ta2O5[λ])-0.0349996340079728)) + (-12965.3688204255) × (((t_Ta2O5[λ])-0.0349996340079728) × ((t_Ta2O5[λ])-0.0349996340079728)-0.000400054898669248) + (-902.346601423572) × (((t_SiN-2[λ])-0.0350204955532028) × ((t_SiO2[λ])-0.125000914980053)) + (-104.997375301657) × (((t_Ta2O5[λ])-0.0349996340079728) × ((t_SiO2[λ])-0.125000914980053)) + 372.567242377661 × (((t_SiO2[λ])-0.125000914980053) × ((t_SiO2[λ])-0.125000914980053)-0.00250052611269396) + 278.515543336254 × (((t_SiN-2[λ])-0.0350204955532028) × ((t_SiN-1[λ])-0.224927716575792)) + (-2340.42700220237) × (((t_Ta2O5[λ])-0.0349996340079728)×((t_SiN-1[λ])-0.224927716575792))+58.3334367716085×(((t_SiO2[λ] ])-0.125000914980053)×((t_SiN-1[λ])-0.224927716575792))+21.2408634563023×(((t_SiN -1[λ])-0.224927716575792)×((t_SiN-1[λ])-0.224927716575792)-0.0131316741294957)+(- 12.3569961396514)×(((t_SiN-2[λ])-0.0350204955532028)×((Siψ)-45.0067708523954))+6. 43899440226174×(((t_Ta2O5[λ])-0.0349996340079728)×((Siψ)-45.0067708523954))+(-4.0 5208515458274)×(((t_SiO2[λ])-0.125000914980053)×((Siψ)-45.0067708523954))+0.85160 2997008135×(((t_SiN-1[λ])-0.224927716575792)×((Siψ)-45.0067708523954))+0.01866300 77404119×(((Siψ)-45.0067708523954)×((Siψ)-45.0067708523954)-825.841735805153)…Equation 5.
[0110] When the plane orientation of the silicon substrate 2 is (110), the phase derived by Equation 5 is preferably -70 degrees or less. More specifically, t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], and Siψ are preferably thicknesses and angles within the range where the phase derived by Equation 5 is -70 degrees or less. As a result, the phases of the first higher-order mode and the second higher-order mode can be made to be -70 degrees or less more reliably. Therefore, the first higher-order mode and the second higher-order mode can be suppressed more reliably and effectively.
[0111] It should be noted that when the silicon substrate 2 is oriented at (110) and the piezoelectric film 7 is a LiTaO3 film, the cutting angle of the piezoelectric film 7 is preferably within the range of 28°Y or higher and 48°Y or lower. Therefore, in addition to suppressing the first and second higher-order modes, Rayleigh waves can also be suppressed. Details of the effect of suppressing Rayleigh waves are shown below.
[0112] Figure 17 This is a graph showing the relationship between the cutting angle of the LiTaO3 film and the phase of the Rayleigh wave.
[0113] like Figure 17 As shown, when the piezoelectric film 7 is a LiTaO3 film and the cutting angle of the piezoelectric film 7 is within the range of 28°Y or higher and 48°Y or lower, the phase of the Rayleigh wave is less than -72°. This allows for the suppression of Rayleigh waves.
[0114] When the phase derived from Equation 4 is -70° or less and the cleavage angle of the LiTaO3 film as piezoelectric film 7 is 28°Y or more and 48°Y or less, Rayleigh waves and at least the first higher-order mode can be suppressed. When the phase derived from Equation 5 is -70° or less and the cleavage angle of the LiTaO3 film as piezoelectric film 7 is 28°Y or more and 48°Y or less, Rayleigh waves, the first higher-order mode, and the second higher-order mode can be suppressed.
[0115] With the orientation of the silicon substrate 2 set to (100), the phase of the first higher-order mode was measured in the same manner as in the derivation of Equation 1. Thus, the relationship between each parameter and the phase of the first higher-order mode was derived, namely Equation 6.
[0116] [Formula 6]
[0117] Spurious phase [deg] = 4.23722010895326+(-957.681500681962)×((t_SiN-2[λ])-0.032371987951807)+585.864572529366×((t_Ta2O5[λ])-0.0343161281489591)+(-70.8133543143104)×((t_SiO2[λ])-0.124755271084337)+(-16.2945641374395)×((t_SiN-1[λ])-0.224798055859809)+(-0.502977915315552)×(Siψ-25.0116374589266)+8018.80873572765×(((t_SiN-2[λ])-0.032371987951807)×((t_SiN-2[λ])-0.032371987951807)-0.000382941581152127)+(-9183.68752253472)×(((t_SiN-2[λ])-0.032371987951807)×((t_Ta2O5[λ])-0.0343161281489591))+(-3967.44233744993)×(((t_Ta2O5[λ])-0.0343161281489591)×((t_Ta2O5[λ])-0.0343161281489591)-0.000397417039992328)+(-219.740749864906)×(((t_SiN-2[λ])-0.032371987951807)×((t_SiO2[λ])-0.124755271084337))+2921.19191101444×(((t_Ta2O5[λ])-0.0343161281489591)×((t_SiO2[λ])-0.124755271084337))+71.8751971324423×(((t_SiO2[λ])-0.124755271084337)×((t_SiO2[λ])-0.124755271084337)-0.00251119250370505)+(-277.396742510064)×(((t_SiN-2[λ])-0.032371987951807)×((t_SiN-1[λ])-0.224798055859809))+(-345.970595680112)×(((t_Ta2O5[λ])-0.0343161281489591)×((t_SiN-1[λ])-0.224798055859809))+(-178.32292070599)×(((t_SiO 2[λ])-0.124755271084337)×((t_SiN-1[λ])-0.224798055859809))+76.2377854978502×(((t _SiN-1[λ])-0.224798055859809)×((t_SiN-1[λ])-0.224798055859809)-0.01313009339161 87)+8.30689126408323×(((t_SiN-2[λ])-0.032371987951807)×(Siψ-25.0116374589266))+( -37.8147686019012)×(((t_Ta2O5[λ])-0.0343161281489591)×(Siψ-25.0116374589266))+( -9.06470966220628)×(((t_SiO2[λ])-0.124755271084337)×(Siψ-25.0116374589266))+0.15 2787017528357×(((t_SiN-1[λ])-0.224798055859809)×(Siψ-25.0116374589266))+0.05320 78049680315×((Siψ-25.0116374589266)×(Siψ-25.0116374589266)-291.798878808268)…Equation 6.
[0118] When the plane orientation of the silicon substrate 2 is (100), the phase derived by Equation 6 is preferably -70 degrees or less. More specifically, the thickness and angle of t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], and Siψ are preferably within the range where the phase derived by Equation 6 is -70 degrees or less. As a result, the phase of the first higher-order mode can be made to be -70 degrees or less more reliably. Therefore, the first higher-order mode can be suppressed more reliably and effectively.
[0119] With the orientation of the silicon substrate 2 set to (100), the phases of the first and second higher-order modes were measured in the same manner as in the derivation of Equation 1. Thus, the relationship between each parameter and the phases of the first and second higher-order modes was derived, namely Equation 7.
[0120] [Formula 7]
[0121] Spurious phase [deg] = 7.99511640601924+(-921.506922121376)×((t_SiN-2[λ])-0.032371987951807)+586.197692765577×((t_Ta2O5[λ])-0.0343161281489591)+(-19.6299727359544)×((t_SiO2[λ])-0.124755271084337)+(-38.2671139134079)×((t_SiN-1[λ])-0.224798055859809)+(-0.384667404398566)×(Siψ-25.0116374589266)+7292.21326291196×(((t_SiN-2[λ])-0.032371987951807)×((t_SiN-2[λ])-0.032371987951807)-0.000382941581152127)+(-8838.66675333011)×(((t_SiN-2[λ])-0.032371987951807)×((t_Ta2O5[λ])-0.0343161281489591))+(-11789.7264976743)×(((t_Ta2O5[λ])-0.0343161281489591)×((t_Ta2O5[λ])-0.0343161281489591)-0.000397417039992328)+(-28.4853757228835)×(((t_SiN-2[λ])-0.032371987951807)×((t_SiO2[λ])-0.124755271084337))+1749.37647871597×(((t_Ta2O5[λ])-0.0343161281489591)×((t_SiO2[λ])-0.124755271084337))+594.755965541834×(((t_SiO2[λ])-0.124755271084337)×((t_SiO2[λ])-0.124755271084337)-0.00251119250370505)+(-486.955268584051)×(((t_SiN-2[λ])-0.032371987951807)×((t_SiN-1[λ])-0.224798055859809))+(-829.859217960196)×(((t_Ta2O5[λ])-0.0343161281489591)×((t_SiN-1[λ])-0.224798055859809))+(-285.613819272102)×(((t_SiO 2[λ])-0.124755271084337)×((t_SiN-1[λ])-0.224798055859809))+118.153648828838×(((t _SiN-1[λ])-0.224798055859809)×((t_SiN-1[λ])-0.224798055859809)-0.013130093391618 7)+9.20315325922817×(((t_SiN-2[λ])-0.032371987951807)×(Siψ-25.0116374589266))+(- 39.0707606971878)×(((t_Ta2O5[λ])-0.0343161281489591)×(Siψ-25.0116374589266))+(-6 .93828445692585)×(((t_SiO2[λ])-0.124755271084337)×(Siψ-25.0116374589266))+(-0.32 7228438235882)×(((t_SiN-1[λ])-0.224798055859809)×(Siψ-25.0116374589266))+0.04714 26960942093×((Siψ-25.0116374589266)×(Siψ-25.0116374589266)-291.798878808268)…Equation 7.
[0122] When the plane orientation of the silicon substrate 2 is (100), the phase derived by Equation 7 is preferably -70 degrees or less. More specifically, the thickness and angle of t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], and Siψ are preferably within the range where the phase derived by Equation 7 is -70 degrees or less. As a result, the phase of the first higher-order mode and the second higher-order mode can be made to be -70 degrees or less more reliably. Therefore, the first higher-order mode and the second higher-order mode can be suppressed more reliably and effectively.
[0123] It should be noted that when the plane orientation of the silicon substrate 2 is (100) and the piezoelectric film 7 is a LiTaO3 film, the cutting angle of the piezoelectric film 7 is preferably in the range of 28°Y or more and 48°Y or less. Therefore, with... Figure 17Similarly, Rayleigh waves can also be suppressed as shown. More specifically, when the phase derived from Equation 6 is -70° or less and the cut angle of the LiTaO3 film as the piezoelectric film 7 is 28°Y or more and 48°Y or less, Rayleigh waves and at least the first higher-order mode can be suppressed. When the phase derived from Equation 7 is -70° or less and the cut angle of the LiTaO3 film as the piezoelectric film 7 is 28°Y or more and 48°Y or less, Rayleigh waves, the first higher-order mode, and the second higher-order mode can be suppressed.
[0124] The above example illustrates a case where the piezoelectric film 7 is a LiTaO3 film. The following is cited... Figure 1 An example is shown where the piezoelectric film 7 is a LiNbO3 film.
[0125] The second embodiment of the present invention differs from the first embodiment in that the piezoelectric film 7 is a LiNbO3 film. Apart from the aspects described above, the elastic wave device of the second embodiment has the same structure as the elastic wave device of the first embodiment.
[0126] Here, the phase characteristics of the elastic wave device having the structure of the second embodiment were measured. The design parameters of this elastic wave device are described below.
[0127] Silicon substrate 2: Planar orientation...(111), Euler angles (Siφ, Siθ, Siψ) in Siψ...46°
[0128] First hypersonic membrane 3: Material...SiN, thickness 500nm
[0129] First low-velocity membrane 4: Material...SiO2, thickness...100nm
[0130] Second low-velocity membrane 5: Material...Ta2O5, thickness...10nm
[0131] Second hypersonic membrane 6: Material...SiN, thickness...10nm
[0132] Piezoelectric film 7: Material...30° Y-cut X-propagated LiNbO3, thickness...400nm
[0133] Layer structure of IDT electrode 8: Layer structure... Ti layer / Al layer / Ti layer from the piezoelectric film 7 side, thickness... 12nm / 100nm / 4nm from the piezoelectric film 7 side.
[0134] Figure 18 This is a diagram showing the phase characteristics of the elastic wave device according to the second embodiment.
[0135] like Figure 18As shown, in the second embodiment, the phase of unwanted waves such as higher-order modes is suppressed to less than -75 degrees in a wide bandwidth of 2200–6000 MHz. Thus, in the second embodiment, similar to the first embodiment, unwanted waves such as higher-order modes can be suppressed in a wide bandwidth. Furthermore, as… Figure 18 As shown, it can be seen that the bandwidth of the main mode can be widened.
[0136] Explanation of reference numerals in the attached figures
[0137] 1...elastic wave device;
[0138] 2...silicon substrate;
[0139] 3...First hypersonic membrane;
[0140] 4...First low-velocity membrane;
[0141] 5...Second low-velocity membrane;
[0142] 6...Second hypersonic membrane;
[0143] 7...piezoelectric film;
[0144] 8...IDT electrode;
[0145] 9A, 9B... reflectors;
[0146] 16...First busbar;
[0147] 17...Second busbar;
[0148] 18...First electrode finger;
[0149] 19...Second electrode finger;
[0150] 102...silicon substrate;
[0151] 103...high-speed acoustic membrane;
[0152] 104...low-velocity membrane;
[0153] 107... piezoelectric film.
Claims
1. An elastic wave device, comprising: Silicon substrate; A first hypersonic membrane is disposed on the silicon substrate; A first low-velocity membrane is disposed on the first high-velocity membrane; The second low-velocity membrane is disposed on the first low-velocity membrane; The second high-velocity diaphragm is disposed on the second low-velocity diaphragm; A piezoelectric film disposed on the second hypersonic film; and An IDT electrode is disposed on the piezoelectric film. The sound speed of the bulk wave propagating on the first hypersonic membrane and the second hypersonic membrane is higher than the sound speed of the elastic wave propagating on the piezoelectric membrane. The sound speed of the bulk wave propagating on the first low-velocity membrane and the second low-velocity membrane is lower than the sound speed of the bulk wave propagating on the piezoelectric membrane. The material of the first low-velocity membrane is different from that of the second low-velocity membrane.
2. The elastic wave device according to claim 1, wherein, The thickness of the first hypersonic membrane is greater than or equal to the thickness of the second hypersonic membrane.
3. The elastic wave device according to claim 1 or 2, wherein, The thickness of the first low-velocity membrane is greater than or equal to the thickness of the second low-velocity membrane.
4. The elastic wave device according to any one of claims 1 to 3, wherein, The thickness of the first high-velocity diaphragm is greater than or equal to the thickness of the first low-velocity diaphragm.
5. The elastic wave device according to any one of claims 1 to 4, wherein, The first low-velocity film or the second low-velocity film is a SiO2 film.
6. The elastic wave device according to any one of claims 1 to 5, wherein, The piezoelectric film is a LiTaO3 film or a LiNbO3 film.
7. The elastic wave device according to any one of claims 1 to 5, wherein, The orientation of the silicon substrate is (111). Both the first and second high-velocity acoustic films are SiN films, the first low-velocity acoustic film is a SiO2 film, the second low-velocity acoustic film is a Ta2O5 film, and the piezoelectric film is a LiTaO3 film. Let λ be the wavelength defined by the electrode finger spacing of the IDT electrodes, let t_SiN-1[λ] be the thickness of the first hypersonic film, let t_SiN-2[λ] be the thickness of the second hypersonic film, let t_SiO2[λ] be the thickness of the first hyposonic film, let t_Ta2O5[λ] be the thickness of the second hyposonic film, let t_LT[λ] be the thickness of the piezoelectric film, let (LTφ, LTθ, LTψ) be the Euler angle of the piezoelectric film, and let (Siφ, Siθ, Siψ) be the Euler angle of the silicon substrate. Then, t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], t_LT[λ], LTθ, and Siψ are thicknesses and angles within a range of -70°[deg] derived from Equation 1 below. [Formula 1] Stray phase [deg] =(-64.7738492449743)+0.799535874292877×(Siψ-23.2121158601201)+(-0.00639116627879308)×(LTθ-131.246414694454)+228.498817195313×((t_LT[λ])-0.180166902154725)+(-551.916118464126)×((t_SiN-2[λ])-0.0291537442599814)+1142.73591823813×((t_Ta2O5[λ])-0.042 1024373013005)+155.359547985879×((t_SiO2[λ])-0.121307841752057)+(-29.8438742957074)×((t_SiN-1[λ])-0.263987107029325)+(-0.0245466642133507)×((Siψ-23.2121158601201)×(Siψ-23.2121158601201)-540.379061966296)+(-0.00862413439802871)×((Siψ-23.2121158601 201)×(LTθ-131.246414694454))+0.249067774425361×((LTθ-131.246414694454)×(LTθ-131.246414694454)-5.81473016925011)+6.93659125135011×((Siψ-23.2121158601201)×((t_LT[λ])-0.180166902154725))+10.0784200297745×((LTθ-131.246414694454)×((t_LT[λ])-0.18016690 2154725))+116.492602498829×(((t_LT[λ])-0.180166902154725)×((t_LT[λ])-0.180166902154725)-0.000346559038760835)+6.96592368109737×((Siψ-23.2121158601201)×((t_SiN-2[λ])-0.0291537442599814))+(-15.0647392900912)×((LTθ-131.246414694454)×((t_SiN-2[λ])-0.0291537442599814))+3185.48452246456×(((t-LT[λ])-0.180166902154725)×((t_SiN-2[λ])-0.0291537442599814))+6533.48929488482×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiN-2[λ])-0.0291537442599814)-0.000458154170897422)+7.78801893149455×((Siψ-23.212115860120 1)×((t_Ta2O5[λ])-0.0421024373013005))+53.7418010590521×((LTθ-131.246414694454)×((t_Ta2O5[λ])-0.0421024373013005))+6146.78344504674×(((t_LT[λ])-0.180166902154725)×((t_Ta2O5[λ])-0.0421024373013005))+(-14578.5920718871)×(((t_SiN-2[λ])-0.02915374425998 14)×((t_Ta2O5[λ])-0.0421024373013005))+28614.912170246×(((t_Ta2O5[λ])-0.0421024373013005)×((t_Ta2O5[λ])-0.0421024373013005)-0.000324766882084902)+4.59563385312738×((Siψ-23.2121158601201)×((t_SiO2[λ])-0.121307841752057))+1.7616110343796×((LTθ-131.24 6414694454)×((t_SiO2[λ])-0.121307841752057))+1984.12416812403×(((t_LT[λ])-0.180166902154725)×((t_SiO2[λ])-0.121307841752057))+(-202.795292688935)×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiO2[λ])-0.121307841752057))+5166.03124069752×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiO2[λ])-0.121307841752057))+(-346.648683117878)×(((t_SiO2[λ])-0.121307841752057)×((t_SiO2[λ])-0.121307841752057)-0.0017442053041025)+1.13949852542765×((Siψ-23.21211 58601201)×((t_SiN-1[λ])-0.263987107029325))+(-2.10309868792554)×((LTθ-131.246414694454)×((t_SiN-1[λ])-0.263987107029325))+342.49568371403×(((t_LT[λ])-0.180166902154725)×((t_SiN-1[λ])-0.263 987107029325))+735.741591105701×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiN-1[λ])-0.263987107029325))+(-2014.8497951455)×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiN-1[λ])-0.263987107029325)) +131.054784086532×(((t_SiO2[λ])-0.121307841752057)×((t_SiN-1[λ])-0.263987107029325))+145.441965448516×(((t_SiN-1[λ])-0.263987107029325)×((t_SiN-1[λ])-0.263987107029325)-0.0132035793109828) …equation 1.
8. The elastic wave device according to any one of claims 1 to 5, wherein, The orientation of the silicon substrate is (111). Both the first and second high-velocity acoustic films are SiN films, the first low-velocity acoustic film is a SiO2 film, the second low-velocity acoustic film is a Ta2O5 film, and the piezoelectric film is a LiTaO3 film. Let λ be the wavelength defined by the electrode finger spacing of the IDT electrodes, let t_SiN-1[λ] be the thickness of the first hypersonic film, let t_SiN-2[λ] be the thickness of the second hypersonic film, let t_SiO2[λ] be the thickness of the first hyposonic film, let t_Ta2O5[λ] be the thickness of the second hyposonic film, let t_LT[λ] be the thickness of the piezoelectric film, let (LTφ, LTθ, LTψ) be the Euler angle of the piezoelectric film, and let (Siφ, Siθ, Siψ) be the Euler angle of the silicon substrate. Then, t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], t_LT[λ], LTθ, and Siψ are thicknesses and angles within a range of -70°[deg] derived from Equation 2 below. [Formula 2] Stray phase [deg] =(-49.4236088933048)+0.927126211958592×(Siψ-23.2121158601201)+0.680023816107774×(LTθ-131.246414694454)+213.742276430449×((t_LT[λ])-0.180166902154725)+(-606.139116757393)×((t_SiN-2[λ])-0.0291537442599814)+692.814216558718×((t_Ta2O5[λ])-0.0421024 373013005)+195.183979143557×((t_SiO2[λ])-0.121307841752057)+(-83.0452792358909)×((t_SiN-1[λ])-0.263987107029325)+(-0.0279599052855905)×((Siψ-23.2121158601201)×(Siψ-23.2121158601201)-540.379061966296)+(-0.0139285317562481)×((Siψ-23.2121158601201) ×(LTθ-131.246414694454))+0.293983576167198×((LTθ-131.246414694454)×(LTθ-131.246414694454)-5.81473016925011)+9.82906312217327×((Siψ-23.2121158601201)×((t_LT[λ])-0.180166902154725))+20.4897039882144×((LTθ-131.246414694454)×((t_LT[λ])-0.18016690215 4725))+(-1822.1825017687)×(((t_LT[λ])-0.180166902154725)×((t_LT[λ])-0.180166902154725)-0.000346559038760835)+6.57985243569614×((Siψ-23.2121158601201)×((t_SiN-2[λ])-0.0291537442599814))+(-16.3487857288392)×((LTθ-131.246414694454)×((t_SiN-2[λ])-0.0291537442599814))+3022.4142953683×(((t_LT[λ])-0.180166902154725)×((t_SiN-2[λ])-0.0291537442599814))+6106.28960321182×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiN-2[λ])-0.0291537442599814)-0.000458154170897422)+7.61287198883346×((Siψ-23.2121158601201) ×((t_Ta2O5[λ])-0.0421024373013005))+32.0420324509525×((LTθ-131.246414694454)×((t_Ta2O5[λ])-0.0421024373013005))+(-5600.23059801591)×(((t_LT[λ])-0.180166902154725)×((t_Ta2O5[λ])-0.0421024373013005))+(-12480.4143612638)×(((t_SiN-2[λ])-0.02915374425998 14)×((t_Ta2O5[λ])-0.0421024373013005))+9462.56388912554×(((t_Ta2O5[λ])-0.0421024373013005)×((t_Ta2O5[λ])-0.0421024373013005)-0.000324766882084902)+4.75660770269025×((Siψ-23.2121158601201)×((t_SiO2[λ])-0.121307841752057))+3.138310645423×((LTθ-131.246 414694454)×((t_SiO2[λ])-0.121307841752057))+782.245112149574×(((t_LT[λ])-0.180166902154725)×((t_SiO2[λ])-0.121307841752057))+(-1849.48045553917)×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiO2[λ])-0.121307841752057))+(-657.25929805289)×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiO2[λ])-0.121307841752057))+(-111.444658339511)×(((t_SiO2[λ])-0.121307841752057)×((t_SiO2[λ])-0.121307841752057)-0.0017442053041025)+1.37817174855647×((Siψ-23.21211586 01201)×((t_SiN-1[λ])-0.263987107029325))+(-1.7087256650039)×((LTθ-131.246414694454)×((t_SiN-1[λ])-0.263987107029325))+(-396.636995545448)×(((t_LT[λ])-0.180166902154725)×((t_SiN-1[λ])-0.26398 7107029325))+434.882453748749×(((t_.SiN-2[λ])-0.0291537442599814)×((t_SiN-1[λ])-0.263987107029325))+(-1660.0685005439)×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiN-1[λ])-0.263987107029325))+10 6.322544176659×(((t_SiO2[λ])-0.121307841752057)×((t_SiN-1[λ])-0.263987107029325))+172.372246831877×(((t_SiN-1[λ])-0.263987107029325)×((t_SiN-1[λ])-0.263987107029325)-0.0132035793109828)…equation 2.
9. The elastic wave device according to any one of claims 1 to 5, wherein, The orientation of the silicon substrate is (111). Both the first and second high-velocity acoustic films are SiN films, the first low-velocity acoustic film is a SiO2 film, the second low-velocity acoustic film is a Ta2O5 film, and the piezoelectric film is a LiTaO3 film. Let λ be the wavelength defined by the electrode finger spacing of the IDT electrodes, let t_SiN-1[λ] be the thickness of the first hypersonic film, let t_SiN-2[λ] be the thickness of the second hypersonic film, let t_SiO2[λ] be the thickness of the first hyposonic film, let t_Ta2O5[λ] be the thickness of the second hyposonic film, let t_LT[λ] be the thickness of the piezoelectric film, let (LTφ, LT0, LTψ) be the Euler angle of the piezoelectric film, and let (Siφ, Si0, Siψ) be the Euler angle of the silicon substrate. Then, t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], t_LT[λ], LTθ, and Siψ are thicknesses and angles within a range of -70°[deg] derived from Equation 3 below. [Formula 3] Stray phase [deg] =(-49.446344512493)+0.926632614160644×(Siψ-23.2121158601201)+0.689805009201412×(LTθ-131.246414694454)+213.186056884304×((t_LT[λ])-0.180166902154725)+(-605.162234862408)×((t_SiN-2[λ])-0.0291537442599814)+693.090367188157×((t]Ta2O5[λ])-0.04210243 73013005)+194.973246854906×((t_SiO2[λ])-0.121307841752057)+(-82.9891258698242)×((t_SiN-1[λ])-0.263987107029325)+(-0.0279312228697236)×((Siψ-23.2121158601201)×(Siψ-23.2121158601201)-540.379061966296)+(-0.0129242968044351)×((Siψ-23.2121158601201)× (LTθ-131.246414694454))+0.285438486600616×((LTθ-131.246414694454)×(LTθ-131.246414694454)-5.81473016925011)+9.7873873803375×((Siψ-23.2121158601201)×((t_LT[λ])-0.180166902154725))+20.1009127346539×((LTθ-131.246414694454)×((t_LT[λ])-0.180166902154 725))+(-1845.21253448418)×(((t_LT[λ])-0.180166902154725)×((t_LT[λ])-0.180166902154725)-0.000346559038760835)+6.50543677488646×((Siψ-23.2121158601201)×((t_SiN-2[λ])-0.0291537442599814))+(-17.1312681888354)×((LTθ-131.246414694454)×((t_SiN-2[λ])-0.0291537442599814))+3096.79723705848×(((t_LT[λ])-0.180166902154725)×((t_SiN-2[λ])-0.0291537442599814))+6184.77577365764×(((t_.SiN-2[λ])-0.0291537442599814)×((t_SiN-2[λ])-0.0291537442599814)-0.000458154170897422)+7.56134934721394×((Siψ-23.2121158601201 )×((t_Ta2O5[λ])-0.0421024373013005))+31.4231915519825×((LTθ-131.246414694454)×((t_Ta2O5[λ])-0.0421024373013005))+(-5550.14180216517)×(((t_LT[λ])-0.180166902154725)×((t_Ta2O5[λ])-0.0421024373013005))+(-12378.8114606327)×(((t_SiN-2[λ])-0.02915374425998 14)×((t_Ta205[λ])-0.0421024373013005))+9488.76758932007×(((t_Ta2O5[λ])-0.0421024373013005)×((t_Ta2O5[λ])-0.0421024373013005)-0.000324766882084902)+4.72906984538813×((Siψ-23.2121158601201)×((t_SiO2[λ])-0.121307841752057))+2.92834698440594×((LTθ-131.24 6414694454)×((t_SiO2[λ])-0.121307841752057))+795.397518262681×(((t_LT[λ])-0.180166902154725)×((t_SiO2[λ])-0.121307841752057))+(-1810.07736779714)×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiO2[λ])-0.121307841752057))+(-633.635642829976)×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiO2[λ])-0.121307841752057))+(-115.182409805846)×(((t_SiO2[λ])-0.121307841752057)×((t_SiO2[λ])-0.121307841752057)-0.0017442053041025)+1.36398286740725×((Siψ-23.212115 8601201)×((t_SiN-1[λ])-0.263987107029325))+(-1.83297695480188)×((LTθ-131.246414694454)×((t_SiN-1[λ])-0.263987107029325))+(-387.007695236215)×(((t_LT[λ])-0.180166902154725)×((t_SiN-1[λ])-0.2 63987107029325))+456.19886315614×(((t_SiN-2[λ])-0.0291537442599814)×((t_SiN-1[λ])-0.263987107029325))+(-1644.59679209231)×(((t_Ta2O5[λ])-0.0421024373013005)×((t_SiN-1[λ])-0.263987107029325) )+113.144234117703×(((t_SiO2[λ])-0.121307841752057)×((t_SiN-1[λ])-0.263987107029325))+173.438761951382×(((t_SiN-1[λ])-0.263987107029325)×((t_SiN-1[λ])-0.263987107029325)-0.0132035793109828) …equation 3.
10. The elastic wave device according to any one of claims 1 to 5, wherein, The orientation of the silicon substrate is (110). Both the first and second high-velocity acoustic films are SiN films, the first low-velocity acoustic film is a SiO2 film, the second low-velocity acoustic film is a Ta2O5 film, and the piezoelectric film is a LiTaO3 film. Let λ be the wavelength defined by the electrode finger spacing of the IDT electrodes, let t_SiN-1[λ] be the thickness of the first hypersonic film, let t_SiN-2[λ] be the thickness of the second hypersonic film, let t_SiO2[λ] be the thickness of the first hyposonic film, let t_Ta2O5[λ] be the thickness of the second hyposonic film, let t_LT[λ] be the thickness of the piezoelectric film, and let (Siφ, Siθ, Siψ) be the Euler angle of the silicon substrate. Then, t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], and Siψ are thicknesses and angles within the range of -70°[deg] derived from Equation 4 below. [Formula 4] Stray phase [deg] =(-35.4828976785632)+(-565.645491469017)×((t_SiN-2[λ])-0.0350204955532028)+1015.0372961359×((t_Ta2O5[λ])-0.0349996340079728)+144.752343074804×((t_SiO2[λ])-0.125000914980053)+(-46.0415586945303)×((t_SiN-1[λ])-0.224927716575792)+1.0468681650000 4×((Siψ)-45.0067708523954)+10682.9573639156×(((t_SiN-2[λ])-0.0350204955532028)×((t_SiN-2[λ])-0.0350204955532028)-0.000399831223602513)+(-13343.4260197881)×(((t_SiN-2[λ])-0.0350204955532028)×((t_Ta2O5[λ])-0.0349996340079728))+14953.0137418577×( ((t_Ta2O5[λ])-0.0349996340079728)×((t_Ta2O5[λ])-0.0349996340079728)-0.000400054898669248)+739.132582722994×(((t_SiN-2[λ])-0.0350204955532028)×((t_SiO2[λ])-0.125000914980053))+4235.91445978005×(((t_Ta2O5[λ])-0.0349996340079728)×((t_SiO2[λ])-0.1 25000914980053))+209.756610061409×(((t_SiO2[λ])-0.125000914980053)×((t_SiO2[λ])-0.125000914980053)-0.00250052611269396)+575.276037855751×(((t_SiN-2[λ])-0.0350204955532028)×((t_SiN-1[λ])-0.224927716575792))+(-1900.54066286617)×(((t_Ta2O5[λ])-0.0349996340079728)×((t_SiN-1[λ])-0.224927716575792))+(-361.044865348212)×(((t_SiO2[λ])-0.125000914980053)×((t_SiN-1[λ])-0.224927716575792))+(-12.6866065936889)×(((t _SiN-1[λ])-0.224927716575792)×((t_SiN-1[λ])-0.224927716575792)-0.0131316741294957)+(-15.0286853820076)×(((t_SiN-2[λ])-0.0350204955532028)×((Siψ)-45.0067708523954))+ 2.30649064625795×(((t_Ta2O5[λ])-0.0349996340079728)×((Siψ)-45.0067708523954))+(-2.93242042531494)×(((t_SiO2[λ])-0.125000914980053)×((Siψ)-45.0067708523954))+0.4902 07176672433×(((t_SiN-1[λ])-0.224927716575792)×((Siψ)-45.0067708523954))+0.0236394426428729×(((Siψ)-45.0067708523954)×((Siψ)-45.0067708523954)-825.841735805153)…equation 4.
11. The elastic wave device according to any one of claims 1 to 5, wherein, The orientation of the silicon substrate is (110). Both the first and second high-velocity acoustic films are SiN films, the first low-velocity acoustic film is a SiO2 film, the second low-velocity acoustic film is a Ta2O5 film, and the piezoelectric film is a LiTaO3 film. Let λ be the wavelength defined by the electrode finger spacing of the IDT electrodes, let t_SiN-1[λ] be the thickness of the first hypersonic film, let t_SiN-2[λ] be the thickness of the second hypersonic film, let t_SiO2[λ] be the thickness of the first hyposonic film, let t_Ta2O5[λ] be the thickness of the second hyposonic film, let t_LT[λ] be the thickness of the piezoelectric film, and let (Siφ, Siθ, Siψ) be the Euler angle of the silicon substrate. Then, t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], and Siψ are thicknesses and angles within the range of -70°[deg] derived from Equation 5 below. [Formula 5] Stray phase [deg] =(-21.043074633666)+(-607.846047314191)×((t_SiN-2[λ])-0.0350204955532028)+835.570016969633×((t_Ta2O5[λ])-0.0349996340079728)+218.780632745606×((t_SiO2[λ])-0.125000914980053)+(-72.9770468417362)×((t_SiN-1[λ])-0.224927716575792)+0.771180072449541× ((Siψ)-45.0067708523954)+9068.29091824635×(((t_SiN-2[λ])-0.0350204955532028)×((t_SiN-2[λ])-0.0350204955532028)-0.000399831223602513)+(-13159.8293417283)×(((t_SiN-2[λ])-0.0350204955532028)×((t_Ta2O5[λ])-0.0349996340079728))+(-12965.3688204255)×(( (t_Ta2O5[λ])-0.0349996340079728)×((t_Ta2O5[λ])-0.0349996340079728)-0.000400054898669248)+(-902.346601423572)×(((t_SiN-2[λ])-0.0350204955532028)×((t_SiO2[λ])-0.125000914980053))+(-104.997375301657)×(((t_Ta2O5[λ])-0.0349996340079728)×((t_SiO2[λ])- 0.125000914980053))+372.567242377661×(((t_SiO2[λ])-0.125000914980053)×((t_SiO2[λ])-0.125000914980053)-0.00250052611269396)+278.515543336254×(((t_SiN-2[λ])-0.0350204955532028)×((t_SiN-1[λ])-0.224927716575792))+(-2340.42700220237)×(((t_Ta2O5[λ])-0.0349996340079728)×((t_SiN-1[λ])-0.224927716575792))+58.3334367716085×(((t_SiO2[λ])-0.125000914980053)×((t_SiN-1[λ])-0.224927716575792))+21.2408634563023×(((t_SiN- 1[λ])-0.224927716575792)×((t_SiN-1[λ])-0.224927716575792)-0.0131316741294957)+(-12.3569961396514)×(((t_SiN-2[λ])-0.0350204955532028)×((Siψ)-45.0067708523954))+6.4 3899440226174×(((t_Ta2O5[λ])-0.0349996340079728)×((Siψ)-45.0067708523954))+(-4.05208515458274)×(((t_SiO2[λ])-0.125000914980053)×((Siψ)-45.0067708523954))+0.851602 997008135×(((t_SiN-1[λ])-0.224927716575792)×((Siψ)-45.0067708523954))+0.0186630077404119×(((Siψ)-45.0067708523954)×((Siψ)-45.0067708523954)-825.841735805153)…Expression 5.
12. The elastic wave device according to any one of claims 1 to 5, wherein, The orientation of the silicon substrate is (100). Both the first and second high-velocity acoustic films are SiN films, the first low-velocity acoustic film is a SiO2 film, the second low-velocity acoustic film is a Ta2O5 film, and the piezoelectric film is a LiTaO3 film. Let λ be the wavelength defined by the electrode finger spacing of the IDT electrodes, let t_SiN-1[λ] be the thickness of the first hypersonic film, let t_SiN-2[λ] be the thickness of the second hypersonic film, let t_SiO2[λ] be the thickness of the first hyposonic film, let t_Ta2O5[λ] be the thickness of the second hyposonic film, let t_LT[λ] be the thickness of the piezoelectric film, and let (Siφ, Siθ, Siψ) be the Euler angle of the silicon substrate. Then, t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], and Siψ are thicknesses and angles within the range of -70°[deg] derived from Equation 6 below. [Formula 6] Stray phase [deg] =4.23722010895326+(-957.681500681962)×((t_SiN-2[λ])-0.032371987951807)+585.864572529366×((t_Ta2O5[λ])-0.0343161281489591)+(-70.8133543143104)×((t_SiO2[λ])-0.124755271084337)+(-16.2945641374395)×((t_SiN-1[λ])-0.224798055859809)+(-0.5029779153155 52)×(Siψ-25.0116374589266)+8018.80873572765×(((t_SiN-2[λ])-0.032371987951807)×((t_SiN-2[λ])-0.032371987951807)-0.000382941581152127)+(-9183.68752253472)×(((t_SiN-2[λ])-0.032371987951807)×((t_Ta2O5[λ])-0.0343161281489591))+(-3967.44233744993)×(( (t_Ta2O5[λ])-0.0343161281489591)×((t_Ta2O5[λ])-0.0343161281489591)-0.000397417039992328)+(-219.740749864906)×(((t_SiN-2[λ])-0.032371987951807)×((t_SiO2[λ])-0.124755271084337))+2921.19191101444×(((t_Ta2O5[λ])-0.0343161281489591)×((t_SiO2[λ])-0.1 24755271084337))+71.8751971324423×(((t_SiO2[λ])-0.124755271084337)×((t_SiO2[λ])-0.124755271084337)-0.00251119250370505)+(-277.396742510064)×(((t_SiN-2[λ])-0.032371987951807)×((t_SiN-1[λ])-0.224798055859809))+(-345.970595680112)×(((t_Ta2O5[λ])-0.0343161281489591)×((t_SiN-1[λ])-0.224798055859809))+(-178.32292070599)×(((t_SiO2[λ])-0.124755271084337)×((t_SiN-1[λ])-0.224798055859809))+76.2377854978502×(((t _SiN-1[λ])-0.224798055859809)×((t_SiN-1[λ])-0.224798055859809)-0.0131300933916187)+8.30689126408323×(((t_SiN-2[λ])-0.032371987951807)×(Siψ-25.0116374589266))+( -37.8147686019012)×(((t_Ta2O5[λ])-0.0343161281489591)×(Siψ-25.0116374589266))+(-9.06470966220628)×(((t_SiO2[λ])-0.124755271084337)×(Siψ-25.0116374589266))+0.15 2787017528357×(((t_SiN-1[λ])-0.224798055859809)×(Siψ-25.0116374589266))+0.0532078049680315×((Siψ-25.0116374589266)×(Siψ-25.0116374589266)-291.798878808268)… Equation 6.
13. The elastic wave device according to any one of claims 1 to 5, wherein, The orientation of the silicon substrate is (100). Both the first and second high-velocity acoustic films are SiN films, the first low-velocity acoustic film is a SiO2 film, the second low-velocity acoustic film is a Ta2O5 film, and the piezoelectric film is a LiTaO3 film. Let λ be the wavelength defined by the electrode finger spacing of the IDT electrodes, let t_SiN-1[λ] be the thickness of the first hypersonic film, let t_SiN-2[λ] be the thickness of the second hypersonic film, let t_SiO2[λ] be the thickness of the first hyposonic film, let t_Ta2O5[λ] be the thickness of the second hyposonic film, let t_LT[λ] be the thickness of the piezoelectric film, and let (Siφ, Siθ, Siψ) be the Euler angle of the silicon substrate. Then, t_SiN-1[λ], t_SiN-2[λ], t_SiO2[λ], t_Ta2O5[λ], and Siψ are thicknesses and angles within the range of -70°[deg] derived from Equation 7 below. [Formula 7] Stray phase [deg] =7.99511640601924+(-921.506922121376)×((t_SiN-2[λ])-0.032371987951807)+586.197692765577×((t_Ta2O5[λ])-0.0343161281489591)+(-19.6299727359544)×((t_SiO2[λ])-0.124755271084337)+(-38.2671139134079)×((t_SiN-1[λ])-0.224798055859809)+(-0.3846674043985 66)×(Siψ-25.0116374589266)+7292.21326291196×(((t_SiN-2[λ])-0.032371987951807)×((t_SiN-2[λ])-0.032371987951807)-0.000382941581152127)+(-8838.66675333011)×(((t_SiN-2[λ])-0.032371987951807)×((t_Ta2O5[λ])-0.0343161281489591))+(-11789.7264976743)×(( (t_Ta2O5[λ])-0.0343161281489591)×((t_Ta2O5[λ])-0.0343161281489591)-0.000397417039992328)+(-28.4853757228835)×(((t_SiN-2[λ])-0.032371987951807)×((t_SiO2[λ])-0.124755271084337))+1749.37647871597×(((t_Ta2O5[λ])-0.0343161281489591)×((t_SiO2[λ])-0.1 24755271084337))+594.755965541834×(((t+SiO2[λ])-0.124755271084337)×((t_SiO2[λ])-0.124755271084337)-0.00251119250370505)+(-486.955268584051)×(((t_SiN-2[λ])-0.032371987951807)×((t_SiN-1[λ])-0.224798055859809))+(-829.859217960196)×(((t_Ta2O5[λ])-0.0343161281489591)×((t_SiN-1[λ])-0.224798055859809))+(-285.613819272102)×(((t_SiO2[λ])-0.124755271084337)×((t_SiN-1[λ])-0.224798055859809))+118.153648828838×(((t _SiN-1[λ])-0.224798055859809)×((t_SiN-1[λ])-0.224798055859809)-0.0131300933916187)+9.20315325922817×(((t_SiN-2[λ])-0.032371987951807)×(Siψ-25.0116374589266))+(- 39.0707606971878)×(((t_Ta2O5[λ])-0.0343161281489591)×(Siψ-25.0116374589266))+(-6.93828445692585)×(((t_SiO2[λ])-0.124755271084337)×(Siψ-25.0116374589266))+(-0.32 7228438235882)×(((t_SiN-1[λ])-0.224798055859809)×(Siψ-25.0116374589266))+0.0471426960942093×((Siψ-25.0116374589266)×(Siψ-25.0116374589266)-291.798878808268)…equation 7.
Citation Information
Patent Citations
Elastic wave device and production method thereof
WO2012086639A1
Elastic wave device and method for manufacturing the same
CN106209007A
Elastic wave device
US20150102705A1