A stress concentration analysis method for metal materials with defect interactions
The three-dimensional structural image of metal materials is obtained by scanning the scanner and the stress concentration coefficient is calculated, which solves the problem of stress concentration analysis errors in the prior art adjacent defect interaction, provides more accurate stress concentration evaluation, and enhances the accuracy and engineering of the analysis significance.
Patent Information
- Application Number
- CN202211028885.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-26
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2042-08-26
AI Technical Summary
In the prior art, when analyzing the stress concentration caused by the interaction of two adjacent defects, it is usually equivalent to a large defect, resulting in errors between the results and the actual situation.
The three-dimensional structural image of the metal material is obtained by a scanner, the equivalent radius, adjacent distance and aspect ratio of the defect are calculated, and the stress concentration coefficient is calculated using the formula, and the impact of defect interaction on stress concentration is evaluated.
By considering the equivalent radius and adjacent distance of the defect, this method provides more accurate stress concentration coefficient values, reduces errors, and the stress concentration coefficient when the material does not contain defects is zero, improving the accuracy and engineering significance of the analysis .
Smart Images

Figure CN115452218B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of material failure analysis and safety assessment, and specifically provides a metal material stress concentration analysis method which avoids defect interactions from affecting analysis results. Background Art
[0002] In metal materials, defects will reduce the plastic deformation capacity of the material and easily cause local stress concentration. In the case of failure analysis, material defects are one of the main ways to cause material failure. In particular, material segregation will cause a large number of defects to appear locally, and these defects will interact with each other, causing premature fracture and failure of the service material. Therefore, evaluating the stress concentration caused by the interaction of defects plays an important role in the safe service performance of the material.
[0003] At present, the most direct method for studying stress concentration is to use strain gauges to measure the deformation of local performance. For metal materials, the increase in strain directly reflects the increase in stress in the measurement area, indicating that stress concentration occurs locally. The strain gauge measurement method is simple to operate and has been widely used in engineering. Although this method has more accurate measurement results for defects, the characteristic information such as the various shapes and sizes of defects cannot be quantified, and the relationship between material defects and stress concentration cannot be established.
[0004] In order to characterize the stress concentration of materials, the stress concentration coefficient is used to indicate the degree of stress concentration. For common defect types in engineering, you can refer to the Stress Concentration Coefficient Manual. For example, for an elliptical defect, the stress concentration coefficient is Kt=1+2a / b, where a / b is the ratio of the major axis to the minor axis of the ellipse. For the stress concentration coefficient caused by a single defect type, you can use the empirical equation Calculate. In this formula, when R d When the value is zero, that is, when there are no defects inside the material, the stress concentration factor calculated according to the empirical formula is zero, which is obviously inconsistent with the facts.
[0005] For the stress concentration caused by the interaction between two adjacent defects, the two defects are usually represented as one large defect. The results obtained by this method have a certain error from the actual results. This is because the interaction between adjacent defects is mainly affected by the adjacent distance, that is, the smaller the adjacent distance, the more obvious the stress concentration. For large defects, the stress is concentrated at the place where the curvature changes greatly. Therefore, in most cases, it is unreasonable to use the defect equivalence method. Summary of the invention
[0006] The main purpose of the present invention is to provide a stress concentration analysis method for metal materials containing defect interactions, and the problem to be solved is: for the stress concentration caused by the interaction between two adjacent defects, the two defects are usually represented as equivalent to one large defect. The results obtained by this method have a certain error compared with the actual results.
[0007] In order to solve the above technical problems, the present invention provides a new analysis method for stress concentration caused by the interaction between two adjacent defects, namely, a stress concentration analysis method for metal materials containing defect interactions, so as to avoid the error caused by treating two defects as one large defect. The above stress concentration analysis method for metal materials containing defect interactions is used to perform stress analysis on a metal material sample to be analyzed containing adjacent defects, i.e., containing adjacent defects. The analysis method is implemented by the following steps:
[0008] Step 1: Scan the metal material sample with a scanner, and then reconstruct the internal three-dimensional structure image of the sample using three-dimensional imaging software based on the scanning results;
[0009] Step 2: According to the 3D structure image, obtain the equivalent radius (c), adjacent distance (D) and aspect ratio (R d );
[0010] Step 3: List the following formula 1, and transform the above equivalent radius (c), adjacent distance (D) and aspect ratio (R d ) is imported into Formula 1 to calculate the stress concentration factor, and then evaluate the influence of defect interaction on stress concentration;
[0011] Formula 1:
[0012]
[0013] Preferably, the scanner is an X-ray scanner or an ultrasonic scanner.
[0014] Preferably, the volume (V), the maximum diameter (d max ) and minimum diameter (d min ). Average diameter (d avg ) is the maximum diameter (d max ) and minimum diameter (d min )’s mean.
[0015]
[0016] The equivalent radius (c) of the defect is calculated using fractal dimension;
[0017]
[0018] The adjacent distance (D) is the distance between the center points of the adjacent defect equivalent diameter, and the aspect ratio (Rd) is the maximum diameter of the defect (d max ) and minimum diameter (d min ) ratio.
[0019]
[0020] Preferably, the equivalent radii (c) of two adjacent defects are at the same order of magnitude.
[0021] Preferably, the equivalent radius (c) and the aspect ratio (R d ) is substituted into the larger defect calculation value, that is, the two adjacent defects, and the equivalent radius (c) and aspect ratio (R d ), in the above calculation formula, select the larger equivalent radius (c) and aspect ratio (R d ).
[0022] The stress concentration analysis method for metal materials with defect interactions provided by the present invention has the following beneficial effects compared with the prior art method of treating two adjacent defects as one large defect:
[0023] When calculating the stress at adjacent defects in metal material samples, not only the aspect ratio is collected, but also the equivalent radius and adjacent distance of the defect are obtained. The influence of the equivalent radius and adjacent distance of the defect on stress concentration is added to the calculation of the stress concentration factor to obtain a more reasonable stress concentration factor value. The equivalent radius (c) takes into account the comprehensive influence of factors such as the volume and diameter of the defect; when the adjacent distance (D) is taken as ∞, the obtained stress concentration factor is caused by a single defect, which can represent the stress concentration factor caused by a single defect; in the stress concentration factor caused by a single defect, the problem of the stress concentration factor being zero when the material does not contain defects is corrected, making the application of this method more engineering meaningful. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art are briefly introduced below.
[0025] Obviously, the drawings described below are only some specific embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without any creative work.
[0026] Figure 1 It is a line chart showing the ratio of the stress concentration factor to the adjacent distance (D) and the equivalent radius (c) in Example 2 of the present invention.
[0027] Figure 2 is the stress concentration factor and the aspect ratio (R d ) between the lines. DETAILED DESCRIPTION
[0028] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.
[0029] Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in the field without making any creative work shall fall within the scope of protection of the present invention.
[0030] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back, etc.) are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.
[0031] In addition, in the present invention, descriptions such as "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0032] In the present invention, unless otherwise clearly specified and limited, the terms "connection", "fixation", etc. should be understood in a broad sense. For example, "fixation" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0033] In addition, the technical solutions between the various embodiments of the present invention can be combined with each other, but it must be based on the fact that ordinary technicians in the field can implement it. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0034] Example 1
[0035] This embodiment uses a variety of magnesium alloys in the market as metal material samples. In this embodiment, CT three-dimensional imaging is first performed on the defects in the magnesium-zinc alloy, and the three-dimensional distribution of the defects is obtained through image reconstruction. Based on morphological analysis, four adjacent defects where stress concentration occurs are selected for stress concentration analysis. The adjacent distance (D), volume (V), and maximum diameter (d max ) and minimum diameter (d min ) and calculate the equivalent radius (c), adjacent distance (D) and aspect ratio (R d ) and other parameters, the corresponding stress concentration factor (Kt) is calculated according to the following formula 1 provided by this method;
[0036] Formula 1:
[0037] In the table, the k value obtained according to the formula is Kt.
[0038] At the same time, the 3D image data was remodeled and imported into the finite element software for static analysis to study the stress concentration caused by defects and calculate the stress concentration factor (K). The results are shown in Table 1. From the comparison of the results, it can be seen that the stress concentration factor calculated by this method is basically consistent with the results of the finite element analysis, which proves that this method has high reliability in analyzing the stress concentration caused by the interaction of adjacent defects.
[0039] Table 1
[0040]
[0041] Example 2
[0042] Based on Example 1, the defects with different equivalent radius (c), adjacent distance (D) and aspect ratio (R d ) and other parameters are used to build a model, and then imported into finite element software for numerical simulation to analyze the stress concentration caused by the interaction of adjacent defects. Figure 1 As shown: According to the above formula 1, determine R d The relationship between D / c and Kt is obtained, and the relationship between R d The value changes and multiple broken lines are drawn. d According to the above modeling and numerical simulation in finite element software, a dot graph of D / c and Kt is drawn. From the results, it can be seen that with the increase of the ratio of the adjacent distance (D) to the equivalent radius (c), the stress concentration factor tends to a constant value, that is, when two adjacent defects reach a certain distance, the interaction can be ignored, and the stress concentration is caused by the larger defect. By comparing the calculation of this method with the finite element numerical simulation, it is proved that the accuracy of the stress concentration factor calculated by this method is high.
[0043] Example 3
[0044] In Example 2, when the distance between adjacent defects reaches a certain level, the interaction can be ignored. Therefore, the formula provided by this method is used to analyze the stress concentration caused by a single defect, that is, the first term in the formula provided by this method is 0. d ) defect was modeled, and the stress concentration generated was analyzed by finite element analysis, and compared with the calculation results of this method. The results are shown in Figure 2 As can be seen from the figure, the result of the finite element analysis, i.e. the dot graph, is consistent with the result of the calculation of formula 1, i.e. the broken line Figure 1 Therefore, the method used to calculate the stress concentration caused by a single defect has a high accuracy. It is worth noting that in this method, when the aspect ratio (R d ) takes a value of 0, that is, when the metal material contains no defects, the calculated value of the stress concentration factor is 1, and the stress inside the material is uniform, which is consistent with the actual situation.
[0045] Of course, the above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. All equivalent structural changes made by using the contents of the present invention specification and drawings under the inventive concept of the present invention, or directly / indirectly used in other related technical fields are included in the patent protection scope of the present invention and should be protected by the present invention.
Claims
1. A method for analyzing stress concentration of metal materials with defect interactions, used for performing stress analysis on a metal material sample to be analyzed with adjacent defects, characterized in that: This is accomplished by following these steps: Step 1: Scan the metal material sample with a scanner, and then reconstruct the internal three-dimensional structure image of the sample using three-dimensional imaging software based on the scanning results; Step 2: Based on the 3D structure image, obtain the equivalent radius c, adjacent distance D and aspect ratio R of the defect d ; Step 3: List the following formula 1, substituting the equivalent radius c, adjacent distance D and aspect ratio R d Import into formula 1 to calculate the stress concentration factor, and then evaluate the effect of defect interaction on stress concentration; Formula 1: The volume V and maximum diameter d of the defect are obtained by three-dimensional imaging software. max and minimum diameter d min , average diameter d avg The maximum diameter d max and minimum diameter d min The mean of The equivalent radius c of the defect is calculated using fractal dimension; The adjacent distance D is the distance between the center points of the adjacent defect equivalent diameters, and the aspect ratio R d is the maximum diameter of the defect d max and minimum diameter d min The ratio of 2. The stress concentration analysis method for metal materials with defect interactions according to claim 1 is characterized in that: The scanner is an X-ray scanner or an ultrasonic scanner.
3. The stress concentration analysis method for metal materials with defect interactions according to claim 1, characterized in that: For two adjacent defects, the equivalent radii c of the two defects are at the same order of magnitude.
4. The stress concentration analysis method for metal materials with defect interactions according to claim 1, characterized in that: Equivalent radius c and aspect ratio R d Substitute the larger calculated defect value into the value.