Semiconductor Components and Their Manufacturing Methods
By forming multiple trenches on a semiconductor substrate and alternately epitaxially growing semiconductor layers, combined with photolithography, multilayer stacking and nanostructures are fabricated, solving the problems of alignment error and coverage error in the semiconductor industry, and improving the integration density and performance of components.
Patent Information
- Application Number
- CN202210500767.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-08
- Filing Date
- 2022-05-09
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2042-05-09
AI Technical Summary
In the semiconductor industry, as the minimum feature size decreases, existing technologies struggle to effectively address alignment and coverage errors when multiple layers are stacked on semiconductor substrates to form circuit elements, affecting component integration density and performance.
By forming multiple trenches on a semiconductor substrate and epitaxially growing first and second semiconductor layers alternately on them to form a multilayer stack, and patterning these layers using photolithography, multiple fins and nanostructures are fabricated, and alignment and coverage accuracy are improved by utilizing alignment structures.
It improves the alignment and coverage accuracy of semiconductor components, enhances the integration density and performance of components, reduces errors in the manufacturing process, and improves the quality of semiconductor components.
Smart Images

Figure CN115472502B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to a semiconductor device and a method for manufacturing the same. Background Technology
[0002] Semiconductor components are used in a variety of electronic applications, such as personal computers, mobile phones, digital cameras, and other electronic devices. Specifically, semiconductor components are manufactured by sequentially depositing an insulating or dielectric layer, a conductive layer, and a semiconductor layer on a semiconductor substrate, and then patterning these multiple layers using photolithography to form circuit elements and components on top of them.
[0003] The semiconductor industry continues to increase the integration density of various electronic components (such as transistors, resistors, capacitors, etc.) by continuously reducing the minimum feature size, which allows more components to be integrated into a given area. However, the additional problems that arise when the minimum size is reduced must be addressed. Summary of the Invention
[0004] A method of manufacturing a semiconductor device includes: forming a plurality of trenches in a first region of a substrate; forming a multilayer stack over the first region and a second region of the substrate, wherein the multilayer stack extends into the trenches, wherein the multilayer stack includes at least one first semiconductor layer and at least one second semiconductor layer alternately stacked; and patterning the multilayer stack and the substrate to form a plurality of first nanostructures over a plurality of first fins in the first region and a plurality of second nanostructures over a plurality of second fins in the second region, wherein the trenches are located in the corresponding counterparts of the respective first fins.
[0005] A method of manufacturing a semiconductor device includes: forming a plurality of trenches in a first region of a substrate; annealing the substrate in H2 or a mixture of H2 and N2; epitaxially growing a plurality of alternating first semiconductor layers and second semiconductor layers over the first and second regions of the substrate after annealing, wherein the alternating first semiconductor layers and second semiconductor layers extend into the trenches; patterning the alternating first semiconductor layers and second semiconductor layers to form a plurality of nanostructures in the first and second regions; and forming a plurality of gate structures over respective portions of the nanostructures located in the second region.
[0006] A semiconductor device includes a substrate, a gate structure, and an alignment structure. The substrate has a diced region and a wafer region. The gate structure is disposed in the wafer region. The alignment structure is disposed in the diced region. The alignment structure includes a plurality of fins and a plurality of nanostructures. The fins protrude from the substrate. The nanostructures are disposed above the fins. Each nanostructure includes a plurality of alternately stacked first semiconductor layers and a plurality of second semiconductor layers. Attached Figure Description
[0007] The best understanding of this disclosure can be obtained by reading it in conjunction with the accompanying figures, as described in the following detailed description. It should be noted that, in accordance with industry standard practice, the various features are not drawn to scale. In fact, the dimensions of the various features may be arbitrarily increased or decreased for clarity of explanation.
[0008] Figure 1 A top view of a semiconductor device illustrated according to some embodiments of this disclosure;
[0009] Figure 2 A three-dimensional view illustrating an example of a nanoFET according to an embodiment of this disclosure;
[0010] Figure 3A , Figure 4A , Figure 6A , Figure 7A , Figure 8A , Figure 9A , Figure 10A , Figure 11 , Figure 12A , Figure 13A , Figure 14A , Figure 15A , Figure 16A , Figure 17 , Figure 18A , Figure 19A , Figure 3B , Figure 4B , Figure 6B , Figure 7B , Figure 8B , Figure 9B , Figure 10B , Figure 12B , Figure 13B , Figure 14B , Figure 15B , Figure 16B , Figure 18B , Figure 19B as well as Figure 20 Multiple cross-sectional side views illustrating intermediate stages of fabricating nanoFETs according to some embodiments of this disclosure;
[0011] Figure 5 A top view of an alignment structure illustrated according to some embodiments of the present disclosure.
[0012] [Symbol Explanation]
[0013] 10: Substrate
[0014] 10N: N-type region
[0015] 10P: P-type region
[0016] 12: First mask layer
[0017] 14: Second masking layer
[0018] 20: Substrate alignment structure
[0019] 20', 105, 1105: Alignment structure
[0020] 22,1120,1122: Trench
[0021] 30, 32, 48: Patterned photoresist layers
[0022] 40: Multi-layer stacking
[0023] 42, 42a, 42b, 42c: First semiconductor layer
[0024] 44, 44a, 44b: Second semiconductor layer
[0025] 46: Third semiconductor layer
[0026] 30A, 32A, 48A: First part
[0027] 30B, 32B, 48B: Second part
[0028] 50, 50A, 50B, 1150B: Fins
[0029] 50S, 1150S: Upper surface
[0030] 55, 55A, 55B, 1155B: Nanostructures
[0031] 60: Insulation layer
[0032] 62: Isolation Features
[0033] 70: Virtual Dielectric Layer
[0034] 72: Virtual Gate Layer
[0035] 80: Source / Drain Characteristics
[0036] 82: Main sidewall spacers
[0037] 85: Groove
[0038] 90: Gate dielectric layer
[0039] 92: Gate electrode
[0040] 100: Semiconductor components
[0041] 101: Wafer
[0042] 102: Chip Area
[0043] 102A, 102B, 102C, 102D: Chips
[0044] 103: Cutting Area
[0045] A-A', B-B', C-C': Section lines
[0046] d: depth
[0047] W1: First width
[0048] W2: Second width Detailed Implementation
[0049] The following disclosure provides numerous different embodiments or instances for implementing various features of the provided subject matter. Specific examples of components and arrangements are described below to simplify this disclosure. Of course, these are merely examples and are not intended to be limiting. For instance, in the following description, the formation of a first feature on or on a second feature may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which additional features may be formed between the first and second features such that the first and second features are not in direct contact. Furthermore, element symbols and / or letters may be repeated in various instances in this disclosure. This repetition is for simplicity and clarity and does not in itself represent a relationship between the various embodiments and / or configurations discussed.
[0050] Additionally, for simplicity, spatial relative terms such as “below,” “under,” “lower,” “above,” “upper,” and similar terms may be used herein to describe the relationship between one element or feature and another (other) element or feature, as shown in the figures. These spatial relative terms are intended to cover different orientations of elements in use or operation, in addition to those depicted in the figures. Devices may be oriented in other ways (rotated 90 degrees or otherwise), and the spatial relative descriptive terms used herein may be interpreted accordingly.
[0051] Figure 1This is a top view of a semiconductor device 100 illustrated according to some embodiments of the present disclosure. In some embodiments, the semiconductor device 100 includes a wafer 101. The wafer 101 may include a plurality of wafer regions 102 (also referred to as active regions) spaced apart from each other by a plurality of dicing regions 103. In some embodiments, each wafer region 102 may include a semiconductor device. Such semiconductor devices may include transistors such as nanoFETs, FinFETs, other multi-gate transistors, planar transistors, bipolar transistors, or other types of components such as resistors, capacitors, inductors, diodes, fuses, static random-access memory (SRAM), and / or other logic circuits. The dicing regions 103 may also be referred to as segmentation regions or isolation regions. In some embodiments, the wafer 101 may be diced along the dicing regions 103 to separate it from the wafer regions 102 and form a plurality of independent wafers. In some embodiments, the semiconductor device 100 further includes an alignment structure 105 disposed in the dicing regions 103. In some embodiments, the alignment structure 105 may be disposed at one edge of the wafer 101. In other embodiments, the alignment structure 105 may be disposed at multiple corners of the wafer region 102. In still other embodiments, the alignment structure 105 may be disposed at multiple edges of the wafer region 102. The alignment structure 105 may also be referred to as an alignment mark. In some embodiments, when the alignment structure 105 is formed in the dicing region 103, the alignment structure 105 may be damaged or destroyed by dicing.
[0052] In some embodiments, each wafer region 102 contains one or more wafers. For example, in Figure 1 In several of the illustrated embodiments, each wafer region 102 includes four wafers, such as wafers 102A, 102B, 102C, and 102D. In other embodiments, each wafer region 102 may include more or fewer than four wafers, depending on design requirements. In some embodiments, when each wafer region 102 includes multiple wafers, alignment structures 105 may be disposed between adjacent wafers in the wafer region 102. In this embodiment, the alignment structures 105 are not damaged or destroyed during the dicing process and remain in the final product.
[0053] Figure 2This is a three-dimensional view illustrating an example of a nanoFET (e.g., nanowire FET, nanosheet FET, or the like) according to one embodiment of the present disclosure. The nanoFET includes nanostructures 55 (e.g., nanosheets, nanowires, or the like) located above fins 50 on a substrate 10 (e.g., a semiconductor substrate), wherein the nanostructures 55 serve as channel regions of the nanoFET. The nanostructures 55 may comprise P-type nanostructures, N-type nanostructures, or combinations thereof. Isolation features 62 are disposed between adjacent fins 50, which may protrude above the space between adjacent isolation features 62. Although isolation features 62 are described / illustrated as separate from the substrate 10, the term "substrate" as used herein may refer to a single semiconductor substrate or a combination of a semiconductor substrate and an isolation feature. Furthermore, although the lower portion of the fins 50 and the substrate 10 are illustrated as a single, continuous material, the lower portion of the fins 50 and / or the substrate 10 may comprise a single material or multiple materials. In this document, fins 50 refer to the extensions between adjacent isolation features 62.
[0054] A gate dielectric layer 90 is located above multiple top surfaces of the fins 50 and along multiple top surfaces, multiple sidewalls, and multiple bottom surfaces of the nanostructure 55. A gate electrode 92 is located above the multiple gate dielectric layers 90. Source / drain features 80 are disposed above the multiple fins 50 on opposite sides of the gate dielectric layers 90 and the gate electrode 92.
[0055] Figures 3A to 19B Multiple cross-sectional side views illustrating an intermediate stage in the fabrication of a nanoFET in wafer region 102 and dicing region 103, according to some embodiments of this disclosure. Figure 3A , Figure 4A , Figures 6A to 10A , Figure 11 , Figures 12A to 16A , Figure 18A as well as Figure 19A This is illustrated by the cross-section line A-A' shown in the wafer region 102. The cross-section line A-A' runs along the longitudinal axis of the gate electrode 92 and in one direction, for example, perpendicular to the dielectric. Figure 2 The direction of current flow between the source / drain features 80 of the nanoFET is illustrated. Figure 17 This is illustrated by section line B-B', which is drawn in wafer region 102. Section line B-B' is parallel to section line A-A' and extends through it. Figure 2 The source / drain characteristics of the nanoFET are illustrated in Figure 80. Figure 3B , Figure 4B , Figures 6B to 10B , Figures 12B to 16B , Figure 18B as well as Figure 19BThis is illustrated by section line C-C' drawn in the cutting area 103. Section line C-C' runs parallel to section line A-A' and extends through the cutting area 103.
[0056] Reference Figure 3A as well as Figure 3B The substrate 10 has a wafer region 102 and is provided with a dicing region 103. The substrate 10 can be a semiconductor substrate, such as a bulk semiconductor, a semiconductor-on-insulator (SOI) substrate, or the like, which may be doped (e.g., using P-type or N-type dopants) or undoped. The substrate 10 can be a wafer, such as a silicon wafer. Generally, an SOI substrate is a semiconductor layer formed on an insulating layer. The insulating layer can be, for example, a buried oxide (BOX) layer, a silicon oxide layer, or the like. The insulating layer is provided on the substrate, particularly a silicon or glass substrate. Other substrates, such as multilayer or gradient substrates, may also be used. In some embodiments, the semiconductor material of the substrate 10 may include silicon; germanium; semiconductor compounds including silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide and / or indium antimonide; alloy semiconductors including silicon and germanium, gallium arsenide phosphide, indium aluminum arsenide, aluminum gallium arsenide, indium gallium arsenide, indium gallium phosphide and / or gallium indium arsenide phosphide; or combinations thereof.
[0057] Reference Figure 4A as well as Figure 4B According to some embodiments of this disclosure, a first masking layer 12 is formed over a substrate 10. According to some embodiments of this disclosure, a second masking layer 14 is formed over the first masking layer 12. The first masking layer 12 may comprise an oxide layer (e.g., silicon oxide). For example, the first masking layer 12 may comprise a thermally grown oxide, an oxide deposited by chemical vapor deposition (CVD), and / or an oxide deposited by atomic layer deposition (ALD). As just one example, the first masking layer 12 may have a thickness between about 2 nm and about 30 nm, or between about 5 nm and about 10 nm. In some embodiments, the second masking layer 14 comprises silicon nitride, aluminum nitride, or other suitable materials. The second masking layer 14 may be deposited by CVD, plasma-enhanced CVD (PECVD), or other suitable deposition techniques. In some embodiments, the second masking layer 14 may have a thickness between about 1 nm and about 100 nm.
[0058] An etching process is then applied to form a substrate alignment structure 20. The substrate alignment structure 20 may include a plurality of trenches 22 in the substrate 10. The etching process may include anisotropic etching processes such as reactive ion etching or ion beam etching. In some embodiments, each trench 22 has a depth d between about 50 nm and about 250 nm, or between about 80 nm and about 100 nm. In some embodiments, the trenches 22 have an aspect ratio of about 10:1 to about 1:1, or, for example, about 5:2. A second masking layer 14 may be removed after the substrate alignment structure 20 is formed.
[0059] Figure 5 This is a top view illustrating a substrate alignment structure 20 according to some embodiments of the present disclosure. In some embodiments, the substrate alignment structure 20 includes regions 20A, 20B, 20C, and 20D. In some embodiments, regions 20A and 20C of the substrate alignment structure 20 may have the same first pattern. In some embodiments, regions 20B and 20D of the substrate alignment structure 20 may have the same second pattern, and in some embodiments, the first pattern rotated 90 degrees will resemble the second pattern. The substrate alignment structure 20 has a first width W1 and a second width W2. In some embodiments, the first width W1 is equal to the second width W2. In some other embodiments, the first width W1 is different from the second width W2. In some embodiments, the first width W1 is between about 50 nm and about 1000 nm. In some embodiments, the second width W2 is between about 50 nm and about 1000 μm. In some embodiments, the ratio of W1 / W2 is approximately equal to 1. By aligning a photomask with the substrate alignment structure 20 in a subsequent photolithography process, registration errors and coverage errors can be reduced.
[0060] exist Figure 6A as well as Figure 6B In this process, suitable wells are formed in the substrate 10. In some embodiments, P-type wells are formed in N-type regions 10N, and N-type wells are formed in P-type regions 10P. In some other embodiments, both P-type and N-type wells are formed in N-type regions 10N and P-type regions 10P. In embodiments with different types of wells, different placement steps of N-type regions 10N and P-type regions 10P can be achieved using photolithography or other masking methods. For example, referring to... Figure 6A as well as Figure 7A A first photolithography step is performed to pattern a P-type well located in an N-type region 10N. A second photolithography step is performed to pattern an N-type well located in a P-type region 10P. It should be understood that the first and second photolithography steps can be performed in any order; for example, the N-type well located in the P-type region 10P can be placed before the P-type well located in the N-type region 10N.
[0061] Performing the first photolithography step may include forming a photoresist layer over the substrate 10, exposing the photoresist layer according to a photomask pattern, performing a pre-exposure baking process, and developing the photoresist layer to form a patterned photoresist layer 30. In some embodiments, such as Figure 6A as well as Figure 6B As illustrated, the patterned photoresist layer 30 has a first portion 30A located in the wafer region 102 and a second portion 30B located in the dicing region 103. The second portion 30B of the patterned photoresist layer 30 may be deposited over the trench 22 and has a plurality of protrusions aligned with the trench 22 and protruding over the substrate 10. The second portion 30B of the patterned photoresist layer 30 can be used to infer the correct position of the first portion 30A of the patterned photoresist layer 30 (e.g., a P-type implanted mask) located in the wafer region 102. For example, the positional offset of the first portion 30A of the patterned photoresist layer 30 located in the wafer region 102 can be inferred by measuring the offset of the overlap position between the second portion 30B of the patterned photoresist layer 30 and the substrate alignment structure 20.
[0062] After the patterned photoresist layer 30 is formed, an ion implantation process is performed in the N-type region 10N to form a P-type well, while the P-type region 10P is retained by being masked by the patterned photoresist layer 30. For example, the P-type dopant implanted into the P-type well via the ion implantation process can comprise boron, aluminum, gallium, indium, or other P-type acceptor materials. After the ion implantation process, the patterned photoresist layer 30 can be removed, for example, by solvent, photoresist, ashing, or other suitable techniques. The dose of the P-type dopant implanted in the N-type region 10N is equal to or less than 10-1. 15 cm -2 , such as between about 10 12 cm -2 To about 10 15 cm -2 In some embodiments, the P-type dopant can be implanted at an implantation energy between about 1 keV and about 10 keV.
[0063] Subsequently, in some embodiments, a second photolithography process is performed, which may include forming a photoresist layer over the substrate 10, exposing the photoresist layer according to a photoresist pattern, performing a pre-exposure baking process, and developing the photoresist layer to form a patterned photoresist layer 32. In some embodiments, such as Figure 7A as well as Figure 7BAs illustrated, the patterned photoresist layer 32 has a first portion 32A located in the wafer region 102 and a second portion 32B located in the dicing region 103. The second portion 32B of the patterned photoresist layer 32 can be deposited over the trench 22 and has a plurality of protrusions aligned with the trench 22 and protruding over the substrate 10. The second portion 32B of the patterned photoresist layer 32 can be used to infer the correct position of the first portion 32A of the patterned photoresist layer 32 (e.g., an N-type implanted mask) located in the wafer region 102. For example, the positional offset of the first portion 32A of the patterned photoresist layer 32 located in the wafer region 102 can be inferred by measuring the offset of the overlap position between the second portion 32B of the patterned photoresist layer 32 and the substrate alignment structure 20.
[0064] After the patterned photoresist layer 32 is formed, an ion implantation process is performed in the P-type region 10P to form an N-type well, while the N-type region 10N is retained by being masked by the patterned photoresist layer 32. For example, the N-type dopant implanted into the N-type well via the ion implantation process can comprise boron, aluminum, gallium, indium, or other N-type donor materials. After the ion implantation process, the patterned photoresist layer 32 can be removed, for example, by solvent, photoresist, ashing, or other suitable techniques. The dose of the N-type dopant implanted in the P-type region 10P is equal to or less than 10. 15 cm -2 , such as between about 10 12 cm -2 To about 10 15 cm -2 In some embodiments, the N-type dopant can be implanted at an implantation energy between about 1 keV and about 10 keV.
[0065] After the implantation process of N-type region 10N and P-type region 10P, an annealing process is performed to activate the implanted P-type and / or N-type dopants. The annealing process can be performed in an atmospheric environment containing air and oxygen. The annealing process can be performed at a temperature between about 1000 °C and about 1250 °C for about 1 second to about 30 seconds. According to some embodiments of this disclosure, the first masking layer 12 is removed by wet etching after the implantation process and before or after the annealing process.
[0066] Reference Figure 8A as well as Figure 8B According to some embodiments disclosed herein, the multilayer stack 40 includes additional layers comprising first semiconductor layers 42a, 42b, 42c (collectively referred to as first semiconductor layer 42) and second semiconductor layers 44a, 44b (collectively referred to as second semiconductor layer 44), formed over the substrate 10 and in the trench 22. Figure 8A as well as Figure 8B In the illustration, the multilayer stack 40, shown for illustrative purposes only, comprises three first semiconductor layers 42a, 42b, and 42c and two second semiconductor layers 44a and 44b stacked alternately. Figure 8A as well as Figure 8B The number of first semiconductor layers 42 and second semiconductor layers 44 shown is merely an example. Other numbers may also be used and are all included within the scope of this disclosure.
[0067] Each layer in the multilayer stack 40 can be epitaxially grown by rapid thermal chemical vapor deposition (RTCVD), metal-organic chemical vapor deposition (MOCVD), vapor phase epitaxy (VPE), molecular beam epitaxy (MBE), or other suitable methods. For example, in one embodiment, the first semiconductor layer 42a is the bottom layer of an additional layer, such as... Figure 8A as well as Figure 8B As illustrated, a first semiconductor layer 42a is epitaxially grown from the upper surface of the substrate 10 and in the trench; a second semiconductor layer 44a is epitaxially grown above the upper surface of the first semiconductor layer 42a; another first semiconductor layer 42b is epitaxially grown above the upper surface of the second semiconductor layer 44a; and other semiconductor layers are alternately epitaxially grown above the first semiconductor layer 42b. In some embodiments, the first semiconductor layers 42a, 42b, 42c and the second semiconductor layers 44a, 44b are conformally formed above the substrate 10 and in the trench 22, thus having a contour line substantially identical to that of the trench 22 (i.e., the substrate alignment structure 20).
[0068] In some embodiments, the first semiconductor layer 42 is formed of a first semiconductor material different from the material of the substrate 10. In some embodiments, the first semiconductor material further has a bandgap of less than about 1.1 eV. For example, the first semiconductor material may be silicon-germanium with a germanium atom concentration between about 20% and about 70%. In some embodiments, each of the first semiconductor layers 42a, 42b, 42c has a thickness between about 1 nm and about 50 nm. In some embodiments, the second semiconductor layer 44 is formed of a second semiconductor material different from the material of the first semiconductor layer 42. Furthermore, the first semiconductor material and the second semiconductor material may be materials that have high etch selectivity to each other. In this way, in subsequent processes, the first semiconductor layer 42 formed of the first semiconductor material may be removed without significantly removing the second semiconductor layer 44 formed of the second semiconductor material, or vice versa. In some embodiments, the second semiconductor layer 44 and the substrate 10 have the same material. In some embodiments, the material of the second semiconductor layer 44 comprises silicon, silicon carbide, or the like. According to some embodiments of this disclosure, each of the second semiconductor layers 44a, 44b has a thickness between about 1 nm and about 50 nm.
[0069] exist Figure 9A as well as Figure 9B In some embodiments disclosed herein, a third semiconductor layer 46 is formed on top of the multilayer stack 40. For example... Figure 9B As shown, the multilayer stack 40 may not completely fill the trench 22, and the trench 22 may be filled by a third semiconductor layer 46. The third semiconductor layer 46 may be formed of a second semiconductor material and may be formed by a method similar to that used to form the second semiconductor material. In some embodiments, the third semiconductor layer 46 has a thickness sufficient to completely fill the trench 22. For example, the third semiconductor layer 46 may have a thickness between about 1 nm and 100 nm.
[0070] Reference Figure 10A as well as Figure 10B A planarization process is performed. In some embodiments, the planarization process includes a chemical mechanical polishing (CMP) process or any other suitable etching process. According to some embodiments of this disclosure, the planarization process removes a third semiconductor layer 46 located outside the trench 22. In some embodiments, a portion of the third semiconductor layer 46 located outside the trench 22 in the dicing region 103, as well as all the third semiconductor layers 46 located in the wafer region 102, are removed, exposing the multilayer stack 40 and leaving a substantially planar upper surface of the third semiconductor layer 46 located in the trench 22. Figure 10A as well as Figure 10BAs shown, the flat upper surface of this third semiconductor layer 46 can be substantially flush with the upper surface of the multilayer stack 40 outside the trench 22, as is the position of the upper surface of the first semiconductor layer 42c located outside the trench 22. In some embodiments, in Figure 10A as well as Figure 10B In the illustrated embodiment, the first semiconductor layer 42c can serve as a polishing termination point. In this document, the trench 22 and the first semiconductor layer 42, the second semiconductor layer 44, and the third semiconductor layer 46 filled in and located above the trench 22 are collectively referred to as alignment structure 20'.
[0071] It should be understood that, in some embodiments, an annealing process is performed to round the bottom corners of the trench 22 before forming the multilayer stack 40. The annealing process can result in the trench 1122 having multiple rounded corners. Rounded corners can mitigate or prevent stacking errors in the multilayer stack 40 or in the alternating layers between the multilayer stack 40 and the third semiconductor layer 46. For example, in Figure 11 The diagram shows an alignment structure 1120 with a circular trench 1122. The alignment structure 1120 may include a first semiconductor layer 42, a second semiconductor layer 44, and a third semiconductor layer 46 formed in the circular trench 1122. According to some embodiments of this disclosure, the annealing process of the plurality of corners of the circular trench 1122 is performed in an environment containing H2 or a mixture of H2 and N2. For example, the annealing process is performed in H2 or a mixture of H2 and N2. In some embodiments, the annealing process of the plurality of corners of the circular trench 1122 is performed at a lower temperature than an annealing process that activates P-type / N-type dopants located in P-type / N-type wells. In some embodiments, the annealing process of the plurality of corners of the circular trench 1122 is performed at a temperature of about 700 °C to about 1200 °C for about 1 second to about 600 seconds. For example, Figure 20 The final structure of this embodiment with the rounded groove 1122 is illustrated.
[0072] exist Figure 12A as well as Figure 12B In this process, a patterned photoresist layer 48 is formed over a multilayer stack 40 through one or more photolithography steps. The photolithography steps may include forming the photoresist layer over the multilayer stack 40 located in the wafer region 102 and the dicing region 103, exposing the photoresist layer according to a photoresist pattern, performing a pre-exposure baking process, and developing the photoresist layer to form the patterned photoresist layer 48. In some embodiments, such as Figure 12A as well as Figure 12BAs shown, the patterned photoresist layer 48 has a first portion 48A located in the wafer region 102 and a second portion 48B located in the dicing region 103. According to some embodiments of this disclosure, the first portion 48A of the patterned photoresist layer 48 is used to define the fin 50 and the nanostructure 55A located in the wafer region 102. The second portion 48B of the patterned photoresist layer 48 can be deposited over and aligned with the alignment structure 20'. The second portion 48B of the patterned photoresist layer 48 can be used to infer the correct position of the first portion 48A of the patterned photoresist layer 48 (e.g., a mask defining the fin 50 and the nanostructure 55A) in the wafer region 102. For example, the positional offset of the first portion 48A of the patterned photoresist layer 48 in the wafer region 102 can be inferred by measuring the overlap positional offset between the second portion 48B of the patterned photoresist layer 48 and the alignment structure 20'. Generally, photolithography processes can also be applied using dual-patterning or multi-patterning processes. In some embodiments where a deviation greater than a predetermined value or an overlap position offset of the patterned photoresist layer 48 forming the window is measured, the patterned photoresist layer 48 can be removed and the step of forming the patterned photoresist layer 48 can be performed again.
[0073] In some embodiments, because the first semiconductor layer 42 and the second semiconductor layer 44 are conformally formed over the substrate 10 and along the trench 22, the contour of the trench 22 can be measured by detecting the contour of the first semiconductor layer 42 or the second semiconductor layer 44. Therefore, the accuracy of the contour of the alignment structure 20' (e.g., the trench 22) can be improved compared to an alignment structure having a trench 22 filled with a thick layer of semiconductor material (e.g., a silicon layer or silicon oxide). The thick layer filling the trench 22 will affect the measurement accuracy and sensitivity of the trench 22 contour because the detection light used to measure the trench 22 contour will be absorbed by the thick layer, especially when the thick layer is formed with the same material as the substrate. In some embodiments, forming one or more thin layers (e.g., the first semiconductor layer 42) with a material different from that of the substrate 10 can reduce or avoid this problem. For example, in one embodiment, the first semiconductor layer 42a is formed of silicon-germanium and the second semiconductor layers 44a, 44b and the third semiconductor layer 46 are formed of silicon. Essentially all detection light can pass through the second semiconductor layer 44 and the third semiconductor layer 46 to reach the bottom multilayer stack 40 and the first semiconductor layer 42a. Because the first semiconductor layer 42 has a bandgap of less than 1.1 eV, it can be detected by light with wavelengths greater than 1.1 μm and is not absorbed by other thin silicon layers (e.g., the second semiconductor layers 44a, 44b and the third semiconductor layer 46) in the nano-FET channel layer. Therefore, with this configuration, the accurate trench 22 profile and the precise overlap offset between the alignment structure 20' and the photoresist pattern used to define the fins 50 and the nanostructure 55 can be measured.
[0074] In some embodiments, the first semiconductor layer 42 or the second semiconductor layer 44 can serve as a channel layer for nanostructures in wafer region 102. Therefore, the alignment structure 20' can be formed without adding additional layers and can be easily integrated into any semiconductor device and its manufacturing process. In a further embodiment, due to the formation of the third semiconductor layer 46, the second portion 48B of the patterned photoresist layer 48 can be situated on a flat upper surface, which will reduce the probability of pattern deformation caused by deposition on an uneven surface.
[0075] exist Figure 13A as well as Figure 13B In some embodiments disclosed herein, fins 50A and nanostructures 55A in wafer region 102, and fins 50B and nanostructures 55B in dicing region 103, are formed through a patterning process. The fins 50A, 50B, and nanostructures 55A, 55B can be formed by etching the substrate 10 according to the first portion 48A and the second portion 48B of the patterned photoresist layer 48. Figure 13AIn this structure, each fin 50A has a substantially flat upper surface, and the corresponding nanostructure 55A includes a first semiconductor layer 42 and a second semiconductor layer 44 disposed above the flat upper surface of the fin 50A. The fin 50A can be formed from the substrate 10 and has the same material as the substrate 10. It should be noted that... Figure 13A For illustrative purposes, the fins 50A and nanostructures 55A have substantially equal widths. In some embodiments, the width of the fin 50A in the N-type region 10N may be greater than or less than the width of the fin 50A in the P-type region 10P. Furthermore, while each fin 50A and nanostructure 55A is depicted to always have equal widths, in other embodiments, the fins 50A and / or nanostructures 55A may have tapered sidewalls such that the width of each fin 50A and / or nanostructure 55A continuously increases in one direction toward the substrate 10. In this embodiment, the fins 50A and the corresponding nanostructures 55A located above the fins 50A may have different widths and be trapezoidal.
[0076] exist Figure 13B In some embodiments disclosed herein, trench 22 is disposed above one of the corresponding fins 50B. Each fin 50B may have an upper surface that is equal to the contour of the trench 22. For example, each fin 50B may have a recessed upper surface 50S. The recessed upper surface 50S may have a depth d between about 50 nm and about 250 nm, or between about 80 nm and about 100 nm. In some embodiments, because the first semiconductor layer 42, the second semiconductor layer 44, and the third semiconductor layer 46 are formed in the trench 22, the bottom surfaces of the first semiconductor layer 42, the second semiconductor layer 44, and the nanostructure 55B are conformally formed on the recessed upper surface 50S of the fin 50B. The fin 50B is formed from the substrate 10 and has the same material as the substrate 10. In some embodiments, the patterned photoresist layer 48 may be removed, for example, by solvent, anti-stripping agent, ashing, or other suitable techniques. In this document, the nanostructure 55B and the fins 50B are collectively referred to as alignment structure 105.
[0077] exist Figure 14A as well as Figure 14BIn this embodiment, an insulating layer 60 is deposited over the substrate 10, fins 50A and 50B, and nanostructures 55A and 55B. The insulating layer 60 can be an oxide, such as silicon oxide, nitrides, the like, or combinations thereof, and can be formed by high-density plasma CVD (HDP-CVD), flowable CVD (FCVD), the like, or combinations thereof. Other insulating materials formed by any acceptable process can also be used. In the illustrated embodiment, the insulating material is silicon oxide formed by an FCVD process. An annealing process can be performed after the insulating layer 60 is formed. Although the insulating material is illustrated as a single layer, some embodiments may be applied as multiple layers. For example, in some embodiments, a liner layer (not shown separately) can be formed first along the surfaces of the substrate 10, fins 50A and 50B, and nanostructures 55A and 55B. Subsequently, a filler material, such as those discussed above, can be formed over the liner layer.
[0078] exist Figure 15A as well as Figure 15B In this process, a removal process is applied to the insulating layer 60 located in wafer region 102 to form an isolation feature 62 adjacent to the fin 50A. In some embodiments, the isolation feature 62 is a shallow trench isolation (STI) feature. According to some embodiments of this disclosure, the removal process includes removing excess insulating layer 60 over and adjacent to nanostructure 55A in wafer region 102, but without removing insulating layer 60 over and adjacent to nanostructure 55B in dicing region 103. In some embodiments, the removal process may be an etch-back process or a combination of an etch-back process and a CMP process. In some embodiments, a photoresist layer may be applied over dicing region 103 before performing the removal process, simultaneously exposing wafer region 102.
[0079] exist Figure 16A as well as Figure 16BIn this embodiment, a dummy dielectric layer 70 is formed over the fins 50A and / or nanostructures 55A located in wafer region 102. According to some embodiments of this disclosure, the dummy dielectric layer 70 may be, for example, silicon oxide, silicon nitride, combinations thereof, or similar materials, and may be deposited or thermally grown. A dummy gate layer 72 is formed over the dummy dielectric layer 70. The dummy gate layer 72 may be deposited over the dummy dielectric layer 70 and planarized, such as through CMP. The dummy gate layer 72 may be a conductive or non-conductive material and may be selected from a group including amorphous silicon, polysilicon, poly-SiGe, metal nitrides, metal silicides, metal oxides, and metals. The dummy gate layer 72 may be deposited by physical vapor deposition (PVD), CVD, sputtering deposition, or other techniques for depositing selected materials. The dummy gate layer 72 may be made of other materials that have high etch selectivity relative to the etching of the isolation feature 62. It should be noted that, for illustration purposes, the dummy dielectric layer 70 is shown to cover only the fin 50A and the nanostructure 55A. In some embodiments, the dummy dielectric layer 70 may be deposited such that the dummy dielectric layer 70 covers the isolation feature 62, such that the dummy dielectric layer 70 extends between the dummy gate layer 72 and the isolation feature 62.
[0080] Reference Figure 17 Source / drain features 80 are formed on opposite sides of nanostructure 55A. In some embodiments, the source / drain features 80 are formed by epitaxially growing a semiconductor material layer on the opposite sides of nanostructure 55A on substrate 10. In some embodiments, the portions of fin 50A and nanostructure 55A not covered by the dummy gate layer 72 are etched to create grooves between the plurality of isolation features 62. In some embodiments, the source / drain features 80 are epitaxially grown in the plurality of grooves and above the plurality of isolation features 62, such as Figure 17As illustrated. In some embodiments, dummy sidewall spacers (not shown) may be formed before epitaxial growth of the source / drain and removed after epitaxial growth of the source / drain. Additionally, in some embodiments, primary sidewall spacers 82 may be formed, as described above, after epitaxial growth of the source / drain. In some embodiments, source / drain features 80 may be formed in the P-type region 10P to provide a PMOSFET, and the source / drain features 80 contain a material subjected to tensile strain in the channel region, such as silicon, SiC, SiCP, SiP, or the like. In some embodiments, source / drain features 80 may be formed in the N-type region 10N to provide an NMOSFET, and the source / drain features 80 contain a material subjected to compressive strain in the channel region, such as SiGe, SiGeB, Ge, GeSn, or the like. The source / drain features 80 may have multiple surfaces rising from corresponding surfaces of multiple fins and may have multiple facets. In some embodiments, after the source / drain feature 80 is formed, an annealing process can be performed to activate the dopants in the source / drain feature 80. For example... Figure 17 As illustrated, according to some embodiments of this disclosure, the source / drain features 80 are separated from each other. In some embodiments, some source / drain features 80 may be combined or physically connected to each other.
[0081] exist Figure 18A as well as Figure 18B In this process, the dummy gate layer 72 is removed by one or more etching steps, resulting in a recess 85 formed in the wafer region 102. Multiple portions of the dummy dielectric layer 70 located in the recess 85 are also removed. In some embodiments, the dummy gate layer 72 and the dummy dielectric layer 70 are removed via an anisotropic dry etching process. For example, the etching process may include a dry etching process utilizing (multiple) reactive gases, such as reactive ion etching. Each recess 85 exposes and / or covers the nanostructure 55A located in the wafer region 102. During removal, the dummy dielectric layer 70 may serve as an etch stop layer while the dummy gate layer 72 is being etched. The dummy dielectric layer 70 may be removed immediately after the dummy gate layer 72 is removed.
[0082] exist Figure 18A as well as Figure 18BIn this embodiment, the first semiconductor layer 42 located in wafer region 102 can be removed, while the second semiconductor layer 44 located in wafer region 102 can be retained and will serve as the channel region in the N-type region 10N and the P-type region 10P of the nanoFET. In this embodiment, the channel regions in the N-type region 10N and the P-type region 10P can have the same material composition (e.g., silicon or another semiconductor material). Tetramethylammonium hydroxide (TMAH), ammonium hydroxide (NH4OH), or the like can be used to remove the first semiconductor layer 42.
[0083] In other embodiments, the second semiconductor layer 44 located in the N-type region 10N and the P-type region 10P will be removed (not shown in the figures). Furthermore, the first semiconductor layer 42 located in the N-type region 10N and the P-type region 10P will be retained and will serve as the channel regions in the P-type region 10P and the N-type region 10N of the nanoFET.
[0084] exist Figure 19A as well as Figure 19B In this embodiment, a gate dielectric layer 90 and a gate electrode 92 are formed to replace multiple gates. The gate dielectric layer 90 is conformally deposited in a recess 85. In the illustrated embodiment, the gate dielectric layer 90 may be formed on multiple top surfaces and multiple sidewalls of multiple fins 50A and multiple top surfaces, multiple sidewalls, and multiple bottom surfaces of multiple nanostructures 55A, for example, on multiple top surfaces, multiple sidewalls, and multiple bottom surfaces of the second semiconductor layer 44.
[0085] According to some embodiments of this disclosure, the gate dielectric layer 90 comprises one or more dielectric layers, such as oxides, metal oxides, the like, or combinations thereof. For example, in some embodiments, the gate dielectric layer 90 may comprise a silicon oxide layer and a metal oxide layer situated above the silicon oxide layer. In some embodiments, the gate dielectric layer 90 comprises a high-k dielectric material, and in these embodiments, the gate dielectric layer 90 may have a k-value greater than about 7.0, and it may comprise a metal oxide or a silicate formed from hafnium, aluminum, zirconium, lanthanum, manganese, barium, titanium, lead, and combinations thereof. Methods for forming the gate dielectric layer 90 may include molecular-beam deposition (MBD), ALD, PECVD, and the like.
[0086] The formation of the gate dielectric layer 90 in the N-type region 10N and the P-type region 10P can occur simultaneously, such that the gate dielectric layer 90 in the N-type region 10N and the P-type region 10P is formed of the same material, and the formation of the gate electrode 92 can also occur simultaneously, such that the gate electrode 92 in the N-type region 10N and the P-type region 10P is formed of the same material. In some embodiments, the gate dielectric layer 90 in the N-type region 10N and the P-type region 10P can be formed through different processes, such that the gate dielectric layer 90 can have different materials and / or different numbers of sublayers, and / or the gate electrode 92 in the N-type region 10N and the P-type region 10P can be formed through different processes, such that the gate electrode 92 in the N-type region 10N and the P-type region 10P can have different materials and / or different numbers of sublayers. When using different processes, multiple masking steps can be used to cover and expose appropriate areas.
[0087] After filling the trench 85, a planarization process, such as CMP, can be performed to remove multiple portions of the gate dielectric layer 90 and the gate electrode 92. The remaining portions of the gate dielectric layer 90 and the gate electrode 92 thus form the alternative gate structure of the final nanoFET. The gate dielectric layer 90 and the gate electrode 92 can be collectively referred to as the "gate structure".
[0088] Figure 20 Illustrations based on some embodiments disclosed herein Figure 2 The image shows a cross-sectional side view of the nanoFET along section line C-C'. Figure 20 In this context, the same component symbols are represented as follows: Figures 3A to 19B Similar elements formed by similar processes. For example, the nanoFETs in these embodiments may have multiple alignment structures 1105, and each alignment structure 1105 may include a nanostructure 1155B disposed above a fin 1150B. The nanostructure 1155B is similar to the nanostructure 55B discussed above, and the fin 1150B is similar to the fin 50B discussed above, wherein the fin 1150B has a rounded recessed upper surface 1150S. The nanostructure 1155B has a bottom surface conformally bound to the rounded recessed upper surface 1150S. The rounded recessed upper surface 1150S can mitigate or prevent stacking errors from occurring in the alternating multilayers of the nanostructure 1155B.
[0089] In one embodiment, a method of manufacturing a semiconductor device includes: providing a substrate having a first region and a second region; forming a plurality of trenches in the first region of the substrate; forming a multilayer stack over the substrate and in the trenches; and patterning the multilayer stack and the substrate to form a plurality of first nanostructures over a plurality of first fins in the first region and a plurality of second nanostructures over a plurality of second fins in the second region, wherein the plurality of trenches are located in corresponding counterparts of the respective first fins. In some embodiments, the method further includes forming an insulating layer over the first nanostructures and the second nanostructures; and etching the insulating layer in the second region but not the insulating layer in the first region. In some embodiments, the insulating layer exposes the second nanostructures in the second region, and the method further includes forming respective gate structures over the insulating layer and across the second nanostructures. In some embodiments, the method further includes removing a first semiconductor layer in the second region but not removing a first semiconductor layer in the first region before forming the gate structure. In some embodiments, at least the second semiconductor layer is made of the same material as the substrate. In some embodiments, the first region is a diced region. In some embodiments, each trench has a depth ranging from 50 nm to 250 nm. In some embodiments, the method further includes: forming a third semiconductor layer over the multilayer stack in the first and second regions, wherein the third semiconductor layer extends into the trench; and performing a polishing process, wherein after the polishing process, the upper surface of the third semiconductor layer in the first region is aligned with the upper surface of the multilayer stack. In some embodiments, the polishing process includes completely removing the third semiconductor layer in the second region. In some embodiments, the polishing process includes using the first or second semiconductor layer as a polishing stop layer. In some embodiments, the method further includes rounding multiple corners of the trench before forming the multilayer stack. In some embodiments, rounding the corners of the trench includes performing an annealing process on the substrate before forming the multilayer stack in H2 or a mixture of H2 and N2.
[0090] In another embodiment, a method of manufacturing a semiconductor device includes: forming a plurality of trenches in a first region of a substrate; annealing the substrate in H2 or a mixture of H2 and N2; epitaxially growing a plurality of alternating first and second semiconductor layers over the first and second regions of the substrate after annealing, wherein the alternating first and second semiconductor layers extend into the trenches; patterning the alternating first and second semiconductor layers to form a plurality of nanostructures in the first and second regions; and forming a plurality of gate structures over respective portions of the nanostructures located in the second region. In some embodiments, the method further includes annealing the substrate in an oxygen-containing atmospheric environment before forming the trenches. In some embodiments, the step of annealing the substrate in H2 or a mixture of H2 and N2 is performed at a lower temperature than the step of annealing the substrate in an oxygen-containing atmospheric environment.
[0091] In yet another embodiment, a semiconductor device includes: a substrate having a diced region and a wafer region, a gate structure disposed in the wafer region, and an alignment structure disposed in the diced region. The alignment structure includes: a plurality of fins protruding from the substrate and a plurality of nanostructures disposed above the fins, wherein each nanostructure includes a plurality of alternately stacked first semiconductor layers and a plurality of second semiconductor layers. In some embodiments, each fin has a recessed upper surface. In some embodiments, the recessed upper surface is an arcuate surface. In some embodiments, the first semiconductor layers and the second semiconductor layers are a plurality of conformal layers located above the respective recessed upper surface of the fin. In some embodiments, the recessed upper surface has a depth ranging from 50 nm to 250 nm.
[0092] The foregoing outlines features of several embodiments to enable those skilled in the art to better understand the nature of this disclosure. Those skilled in the art should understand that they can readily use this disclosure as a basis for designing or modifying other processes and structures to achieve the same purpose and / or attain the same advantages of the embodiments described herein. Those skilled in the art should also recognize that these equivalent constructions do not depart from the spirit and scope of this disclosure, and that they can make various changes, substitutions, and replacements herein without departing from the spirit and scope of this disclosure.
Claims
1. A method for manufacturing a semiconductor device, characterized in that, The method includes: Multiple trenches are formed in a first region of a substrate; A multilayer stack is formed over the first region and the second region of the substrate, wherein the multilayer stack extends into the trenches, and wherein the multilayer stack includes at least one first semiconductor layer and at least one second semiconductor layer stacked alternately. as well as The multilayer stack and the substrate are patterned to form a plurality of first nanostructures over a plurality of first fins in the first region and a plurality of second nanostructures over a plurality of second fins in the second region, wherein the trenches are located in corresponding counterparts of the respective first fins, and wherein the first fins in the first region have recessed upper surfaces.
2. The method for manufacturing a semiconductor device as described in claim 1, characterized in that, Further includes: An insulating layer is formed above the first nanostructure and the second nanostructure; and The insulating layer located in the second region is etched, but the insulating layer located in the first region is not etched.
3. The method for manufacturing a semiconductor device as described in claim 2, characterized in that, The step of etching the insulating layer located in the second region exposes the second nanostructure in the second region, and the method further includes forming individual gate structures over the insulating layer and across the second nanostructure.
4. The method for manufacturing a semiconductor device as described in claim 3, characterized in that, The method further includes removing the first semiconductor layer located in the second region but not removing the first semiconductor layer located in the first region before forming the gate structures.
5. The method for manufacturing a semiconductor device as described in claim 1, characterized in that, The at least one second semiconductor layer is made of the same material as the substrate.
6. The method for manufacturing a semiconductor device as described in claim 1, characterized in that, The first region is a segmented area.
7. The method for manufacturing a semiconductor device as claimed in claim 1, characterized in that, Each of these trenches has a depth ranging from 50 nm to 250 nm.
8. The method for manufacturing a semiconductor device as claimed in claim 1, characterized in that, Further includes: A third semiconductor layer is formed over the multilayer stack in the first region and the second region, wherein the third semiconductor layer extends into the trenches; as well as A polishing process is performed, wherein after the polishing process, an upper surface of the third semiconductor layer located in the first region is aligned with an upper surface of the multilayer stack.
9. The method for manufacturing a semiconductor device as described in claim 8, characterized in that, The polishing process involves completely removing the third semiconductor layer located in the second region.
10. The method for manufacturing a semiconductor device as described in claim 8, characterized in that, The polishing process includes using the first semiconductor layer or the second semiconductor layer as a polishing stop layer.
11. The method for manufacturing a semiconductor device as claimed in claim 1, characterized in that, Further, this includes rounding the corners of these trenches before forming the multi-layered stack.
12. The method of manufacturing a semiconductor device as claimed in claim 11, characterized in that, Before the corners of the rounded trenches are contained in H2 or a mixture of H2 and N2 to form the multilayer stack, an annealing process is performed on the substrate.
13. A method for manufacturing a semiconductor device, characterized in that, The method includes: Multiple trenches are formed in a first region of a substrate; Anneal the substrate in H2 or a mixture of H2 and N2; After annealing, a plurality of alternating first semiconductor layers and second semiconductor layers are epitaxially grown over the first region and a second region of the substrate, wherein the alternating first semiconductor layers and second semiconductor layers extend into the trenches; The alternating first and second semiconductor layers are patterned to form a plurality of first nanostructures over a plurality of first fins in the first region and a plurality of second nanostructures over a plurality of second fins in the second region, wherein the trenches are located in corresponding counterparts of the respective first fins, and wherein the first fins in the first region have recessed upper surfaces; and Multiple gate structures are formed above individual portions of the second nanostructures located in the second region.
14. The method of manufacturing a semiconductor device as described in claim 13, characterized in that, The substrate is further annealed in an atmosphere containing oxygen before the trenches are formed.
15. The method of manufacturing a semiconductor device as described in claim 14, characterized in that, The step of annealing the substrate in H2 or a mixture of H2 and N2 is performed at a lower temperature than the step of annealing the substrate in an atmospheric environment containing oxygen.
16. A semiconductor element, characterized in that, Include: A substrate having a dicing region and a wafer region; A gate structure is disposed in the wafer region; and An alignment structure is disposed in the cutting area, wherein the alignment structure comprises: Multiple fins protruding from the substrate, wherein each of the fins has a recessed upper surface; and Multiple nanostructures are disposed above the fins, wherein each of the nanostructures comprises multiple first semiconductor layers and multiple second semiconductor layers stacked alternately.
17. The semiconductor device as claimed in claim 16, characterized in that, The upper surface of the depression has a depth ranging from 80 nm to 100 nm.
18. The semiconductor element as claimed in claim 16, characterized in that, The upper surface of the depression is an arc surface.
19. The semiconductor element as claimed in claim 16, characterized in that, The first semiconductor layer and the second semiconductor layer are multiple conformal layers located above the individual recessed upper surfaces of the fins.
20. The semiconductor device as claimed in claim 16, characterized in that, The upper surface of the depression has a depth ranging from 50 nm to 250 nm.
Citation Information
Patent Citations
Semiconductor device and method of manufacturing the same
US20210134677A1