Solid Oxide Fuel Cells
By using doped barium cerate material and composite cathode structure, the problem of output power reduction caused by methanol permeation is solved, and the performance improvement of methanol fuel cell is achieved and the application potential of the battery is enhanced.
Patent Information
- Application Number
- CN202110661079.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-06-15
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2041-06-15
AI Technical Summary
Methanol penetration leads to a significant reduction in the output power of direct methanol fuel cells, reaching only 20% of hydrogen fuel cells, limiting its application potential.
The receptor-doped barium cerate BaCe0.8Y0.2O3-d is used as the electrolyte membrane material, and the anode supports the electrolyte membrane and the composite cathode, including a layered compound and a catalyst that mixes oxygen ions and electron conductors, by adjusting the oxygen ions and Proton conduction ratio and electrode structure, a stable composite cathode material is prepared to avoid methanol permeation problems.
At 400°C, the current density reaches 1Acm-2 and the open circuit potential is greater than 1V, which avoids methanol penetration problem, improves the performance and stability of the battery, and enhances the potential applications of the battery.
Smart Images

Figure CN115483423B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a fuel cell, and more particularly to a solid oxide fuel cell. Background Art
[0002] Effectively solving the energy problem of future society will be one of the important foundations for the stable development of the country. In the face of growing energy demand and climate change, the transition to a reliable, sustainable and competitive energy system will be an important technical strategic solution to a series of energy problems [1]. A key issue that remains to be solved in the energy system is energy storage. Hydrogen, as an energy carrier, has been widely regarded as one of the feasible solutions. However, it must be compressed, stored, transported, and then decompressed before it can be converted back into electricity, which leads to serious energy losses in these processes. A feasible way to reduce energy losses is to use synthetic liquid hydrocarbon fuels as hydrogen carriers to significantly increase the energy conversion density. Due to its high H / C ratio, liquid properties under standard conditions, low toxicity, ability to reform at low temperatures, and high production in China, methanol has become one of the main candidates for liquid hydrocarbon fuels in my country. Direct methanol fuel cells (DMFCs) are a crucial device for converting chemical energy into electrical energy because they can directly convert methanol into electrical energy, thus avoiding the complexity of using methanol hydrogen production units and hydrogen fuel cell systems. However, DMFCs also have several problems that need to be solved, such as the low kinetics of anode methanol oxidation and transportation restrictions caused by methanol volatility. The most serious problem is the methanol permeation phenomenon in the electrolyte membrane. Methanol permeation leads to a significant reduction in output power, which is barely 20% of the power output of a fuel cell running on hydrogen, greatly limiting its potential applications. Even with the most advanced DMFC, this value is only increased to about 0.2 W cm -2 The power density of PEMFC using hydrogen fuel is usually about 1.0 to 1.5 W cm -2 The huge loss in power density of DMFC limits its potential applications.
[0003] The methanol permeation problem is caused by the fundamental properties of the electrolyte material NAFION. NAFION allows methanol to actively pass through the electrolyte, and this active permeation phenomenon worsens with increasing temperature and methanol / water ratio. Summary of the invention
[0004] The object of the present invention is to provide a solid oxide fuel cell to solve the problem mentioned in the above background technology that methanol permeation leads to a significant reduction in output power, which does not reach 20% of the power output of a fuel cell running on hydrogen as fuel, greatly limiting its potential application.
[0005] To achieve the above object, the present invention provides the following technical solutions:
[0006] A solid oxide fuel cell comprises an anode, an electrolyte membrane and a composite cathode, wherein the two ends of the electrolyte membrane are connected to the anode and the cathode respectively, the anode and the composite cathode are in contact with methanol and oxygen respectively, and the electrolyte membrane is based on acceptor-doped barium cerate BaCe 0.8 Y 0.2 O 3-d The electrolyte membrane is connected to the anode by an anode-supported electrolyte membrane, and the anode-supported electrolyte membrane is prepared by spin coating a stable suspension of nanopowder formed by burning acetate / hydrogen peroxide. The thickness of the anode-supported electrolyte membrane is less than 5 μm. The composite cathode includes mixed oxygen ions and an electronic conductor, and the electronic conductor is a layered compound with a superstoichiometric ratio. The layered compound includes Ln2NiO 4+d Double perovskite LnBaCo2O 5+d , a catalyst is provided in the anode.
[0007] Preferably, the reaction formula of the anode (1) under alkaline conditions is 3O2+12e – +6H20→12OH – The reaction formula with the cathode (3) under alkaline conditions is 2CH4O+12e – +12OH - →2CO2+10H2O, the reaction formula of the anode (1) under acidic conditions is 3O2+12e – +12H + →6H2O, the reaction formula of the cathode (3) under acidic conditions is 2CH4O-12e – +2H2O→12H++2CO2.
[0008] Preferably, the battery has a current density of 1Acm at 400°C under low steam-methanol ratio conditions. -2 , the open circuit potential is greater than 1V.
[0009] Preferably, the layered compounds are capable of providing anisotropic oxygen diffusion and high electronic conductivity as well as low activation energy temperatures required to maintain performance.
[0010] Preferably, the catalyst is a typical methanol steam reforming catalyst, including Ni, Cu, and ZnO, and the metal nanoparticles of the catalyst enter the anode through a solution infiltration method to achieve the best methanol reforming performance of the anode.
[0011] Preferably, the electrolyte membrane is doped with Ti or Zr to provide additional stability.
[0012] Compared with the prior art, the present invention has the following beneficial effects:
[0013] 1) Improved acceptor-doped barium cerate material BaCe 0.8 Y 0.2 O 3-d (abbreviated as BCY), which has the highest proton conductivity among known ceramic proton conductors (one order of magnitude higher than BZY), but due to the peculiarities in carbonaceous atmospheres, they are usually not considered for use. The proton conductivity produced by the hydration of BaCeO3 materials also leads to the problem of instability in atmospheres containing water and carbon dioxide. In this process, chemical stability is closely related to thermodynamic processes, namely the stability of cations to the perovskite structure and barium oxide to carbonates. Studies on carbonation / carbon removal have shown that CO2 adsorption and reaction occur at different kinetic stages, and carbonation will not occur at temperatures of 400°C or lower, regardless of whether in a humid or dry CO2 atmosphere. Direct use of BaCeO3 membranes for power generation at ≤400°C in this kinetic stability window can directly use methanol fuel at a temperature of 400°C, completely avoiding the problem of methanol penetration.
[0014] 2) The present invention prepares a stable composite cathode material by adjusting the ratio of oxygen ion to proton conduction and the electrode structure, which can provide high electronic conductivity, high oxygen reduction catalytic activity and low polarization resistance, thereby improving the cathode performance of the battery. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic diagram of the structure of the present invention;
[0016] Figure 2 It is a schematic diagram of the percentage of the carbonation stage of BaCeO3 with increasing temperature according to the present invention;
[0017] Figure 3 A graph showing the change in carbonation temperature of the BaCeO3 material of the present invention as a function of grain size;
[0018] Figure 4 and Figure 5 It is a schematic diagram of the in-situ scanning of the cathode pore distribution and element distribution structure of the present invention.
[0019] In the figure: 1 anode, 2 electrolyte membrane, 3 composite cathode. DETAILED DESCRIPTION
[0020] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0021] In the description of the present invention, it is necessary to understand that the terms "upper", "lower", "front", "back", "left", "right", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0022] Example:
[0023] See also Figure 1-5 The solid oxide fuel cell of the present invention comprises an anode 1, an electrolyte membrane 2 and a composite cathode 3, wherein the two ends of the electrolyte membrane 2 are connected to the anode 1 and the cathode 3 respectively, the anode 1 and the composite cathode 3 are in contact with methanol and oxygen respectively, and the electrolyte membrane 2 is based on acceptor-doped barium cerate BaCe 0.8 Y 0.2 O 3-d The electrolyte membrane 2 is connected to the anode 1 and provided with an anode supporting electrolyte membrane, and the anode supporting electrolyte membrane is prepared by spin coating a stable suspension of nanopowder formed by burning acetate / hydrogen peroxide, and the thickness of the anode supporting electrolyte membrane is less than 5 μm, and the composite cathode 3 includes mixed oxygen ions and electronic conductors, and the electronic conductor is a layered compound with a superstoichiometric ratio, and the layered compound includes Ln2NiO 4+d Double perovskite LnBaCo2O 5+d The layered compound can provide anisotropic oxygen diffusion and high electronic conductivity as well as the low activation energy temperature required to maintain performance. The anode 1 is provided with a catalyst, which is a typical methanol steam reforming catalyst, including Ni, Cu or ZnO. The metal nanoparticles of the catalyst enter the anode 1 through a solution infiltration method to achieve the optimal methanol reforming performance of the anode 1.
[0024] The reaction formula of the anode 1 under alkaline conditions is 3O2+12e – +6H20→12OH – The reaction formula with cathode 3 under alkaline conditions is 2CH4O+12e – +12OH - →2CO2+10H2O, the reaction formula of the anode 1 under acidic conditions is 3O2+12e – +12H + →6H2O, the reaction formula of the cathode 3 under acidic conditions is 2CH4O-12e –+2H2O→12H++2CO2, methanol is converted into carbon dioxide, protons and electrons at the anode, just like a standard proton exchange membrane fuel cell, protons pass through the proton exchange membrane and react with oxygen at the cathode, and electrons reach the cathode through the external circuit and do work.
[0025] The battery has a current density of 1Acm at 400°C under low steam-methanol ratio conditions. -2 , the open circuit potential is greater than 1V, the electrolyte membrane 1 is doped with Ti and Zr, if the expected stability result of the electrolyte BCY is lower than the required operating temperature, i.e., the stability of 400°C, the modification of the electrolyte will be carried out by doping strategy or changing its morphology; for example, if carbonation starts at the grain boundaries, a sintering additive such as Co will be added to promote grain growth; the improvement of thermodynamic stability can also be achieved by doping smaller cations at the B site, such as a small amount of Ti or Zr, to increase the perovskite tolerance factor, thereby improving the stability of the electrolyte BCY.
[0026] BaCeO3 has high proton conductivity, but barium-cerium-based electrolytes are generally not considered for use in carbon-containing atmospheres because they may decompose with the formation of carbonates. Nevertheless, at low temperatures, especially ≤400°C, this carbonation decomposition reaction is kinetically limited and can be avoided by modification, etc., see Figure 2 is the percentage of BaCeO3 in the carbonation stage at a heating rate of 3°C / min. As the temperature increases, Ba deficiency is caused in the BaCeO3 phase, and the molecular composition changes to Ba 1-x CeO3, and the carbonation in this stage mainly occurs on the surface of the particles. No obvious weight increase is observed below 470°C. In the first stage, carbonation is thermodynamically favorable. However, due to strong kinetic limitations, only a small weight increase is observed, and the perovskite structure remains intact. This carbonation stage is mainly BaO reaction, generating a small amount of carbonate. Therefore, this project uses the kinetic limitations in this steam / methanol mixture to investigate and use chemical methods to improve the stability of BaCeO3-based thin film electrolytes at 400°C, while providing additional stability through a small amount of doping strategy (Ti, Zr). See Figure 3 The starting temperature of the first stage of carbonation is affected by the morphology of the BaCeO3 sample. The larger the particle size, the higher the reaction temperature. Therefore, the stability of BCY can be adjusted by changing the morphology and size.
[0027] At low temperatures, close attention must also be paid to ohmic polarization and electrode polarization losses to maximize cell voltage and efficiency. Regarding ohmic polarization losses, Steele points out that for a conductivity of 10 -2 Scm -1The electrolyte has an ideal electrode thickness of less than 15 μm, which requires the battery to be in an electrode-supported form. Therefore, it is clear that even with an ultra-thin electrolyte with low ohmic resistance, the control of electrode polarization resistance is also one of the important guarantee conditions for achieving the desired performance. The reaction kinetics of oxygen reduction are slower than the reaction kinetics of anode fuel oxidation, so the electrode polarization resistance mainly comes from the cathode. The present invention prepares a stable composite cathode material by adjusting the ratio of oxygen ion to proton conduction and the electrode structure, which can provide high electronic conductivity, high oxygen reduction catalytic activity and low polarization resistance, thereby improving the cathode performance of the battery.
[0028] See Figure 4 and Figure 5 For sufficiently thin electrolytes, cathode polarization resistance may become a limiting factor for battery performance at 400°C; therefore, a suitable cathode composite material is customized by adjusting the ratio of oxygen ion to proton conduction, and finally a mixed conductor with proton conductivity and oxygen ion + electron conductivity is synthesized and tested under different pH2O, pO2 and temperature parameters to obtain important information on the effect of the presence of oxygen ion and proton conduction on cathode performance.
[0029] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. For those skilled in the art, it is obvious that the present invention is not limited to the details of the above exemplary embodiments, and the present invention can be implemented in other specific forms without departing from the spirit or basic features of the present invention; therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive. The scope of the present invention is limited by the attached claims rather than the above description. Therefore, it is intended to include all changes within the meaning and scope of the equivalent elements of the claims in the present invention, and any figure marks in the claims should not be regarded as limiting the claims involved.
[0030] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A solid oxide fuel cell comprising an anode (1), an electrolyte membrane (2) and a composite cathode (3), characterized in that: The two ends of the electrolyte membrane (2) are respectively connected to the anode (1) and the cathode (3); the anode (1) and the composite cathode (3) are respectively in contact with methanol and oxygen; the electrolyte membrane (2) is based on acceptor-doped barium cerate BaCe 0.8 Y 0.2 O 3-d The electrolyte membrane (2) is connected to the anode (1) with an anode supporting electrolyte membrane, and the anode supporting electrolyte membrane is prepared by spin coating a stable suspension of nanopowder formed by burning acetate / hydrogen peroxide, and the thickness of the anode supporting electrolyte membrane is less than 5 μm. The composite cathode (3) includes mixed oxygen ions and an electronic conductor, and the electronic conductor is a layered compound with a superstoichiometric ratio, and the layered compound includes Ln2NiO 4+d Double perovskite LnBaCo2O 5+d The anode (1) is provided with a catalyst.
2. The solid oxide fuel cell according to claim 1, characterized in that: The reaction formula of the anode (1) under alkaline conditions is 3O2+12e – +6H20→12OH – The reaction formula with the cathode (3) under alkaline conditions is 2CH4O+12e – +12OH - →2CO2+10H2O, the reaction formula of the anode (1) under acidic conditions is 3O2+12e – +12H + →6H2O, the reaction formula of the cathode (3) under acidic conditions is 2CH4O-12e – +2H2O→12H++2CO2.
3. The solid oxide fuel cell according to claim 1, characterized in that: The battery has a current density of 1Acm at 400°C under low steam-methanol ratio conditions. -2 , the open circuit potential is greater than 1V.
4. The solid oxide fuel cell according to claim 1, characterized in that: The layered compounds are able to provide anisotropic oxygen diffusion and high electronic conductivity as well as the low activation energy temperature required to maintain performance.
5. The solid oxide fuel cell according to claim 1, characterized in that: The catalyst is a typical methanol steam reforming catalyst, including Ni, Cu or ZnO, and the metal nanoparticles of the catalyst enter the anode (1) through a solution infiltration method to achieve the best methanol reforming performance of the anode (1).
6. The solid oxide fuel cell according to claim 1, characterized in that: The electrolyte membrane (1) is doped with Ti and / or Zr to provide additional stability.
Citation Information
Patent Citations
Fuel cells
CN101432921A
Membrane electrode complex of direct methanol fuel cell and preparation method and direct methanol fuel cell thereof
CN102361088A