A lubricating oil solvent dewaxing method
Through multi-stage dilution solvent system and evaporation separation technology, solvent recycling and temperature control are optimized, and the problems of high cost and high energy consumption in the existing solvent dewaxing methods are solved, and the yield and production efficiency of lubricating oil are improved.
Patent Information
- Application Number
- CN202211162732.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-23
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2042-09-23
AI Technical Summary
The existing solvent dewaxing methods lead to increased raw material costs, increased recovery system load, high energy consumption, low product oil wax yield and large oil production under by-product wax, and high processing costs.
Using a multi-stage dilution solvent system, gradually add one, second and third dilution solvents to reduce the viscosity of the raw materials. Through evaporation separation and recovery system, solvent recycling and temperature control are optimized to reduce the amount of ketobenzene solvent and energy consumption and improve dewaxing. Yields of oil and deoiling wax.
It reduces the processing cost of lubricant oil, improves the yield of dewaxed oil, reduces the thermal load and energy consumption of the recovery system, reduces the yield of oil under wax by-products, and optimizes the production efficiency of lubricant oil.
Smart Images

Figure CN115651700B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of petroleum oil product processing, and in particular to a lubricating oil solvent dewaxing method. Background Art
[0002] In the lubricant production process, in order to reduce the freezing point of the lubricant and increase the viscosity of the lubricant so as to meet the use requirements of the lubricant under various mechanical conditions, it is often necessary to remove the high melting point wax components. At the same time, the removed high melting point wax components also provide raw materials for the subsequent production of paraffin. There are generally two methods for lubricant dewaxing in industrial production, namely solvent dewaxing and hydrogenation dewaxing. Solvent dewaxing is the earliest method used in lubricant production and is also the most widely used method now.
[0003] The existing solvent dewaxing method is to use a mixed solvent, such as a binary mixture of butanone and toluene (hereinafter referred to as ketone-benzene solvent), which has different solubility for the oil and wax in the raw material. The solvent is added gradually during the cooling process of the raw material to reduce the viscosity of the raw material, improve its fluidity, and create suitable conditions for the wax crystallization, so that the wax forms uniform and dense crystals, which is convenient for separating the oil and wax by filtering. The filtrate, wax liquid and wax oil liquid separated by filtration are sent to the recovery system respectively. The solvent is recycled and reused by using the difference in boiling points between the solvent and the oil, wax and wax oil to obtain the oil, wax and wax oil without the solvent. The process flow of the existing solvent dewaxing method is shown in the figure below. Figure 2 .
[0004] In the existing solvent dewaxing method, the raw oil uses the recovery solvent as a diluent to reduce the viscosity of the raw oil during the filtering stage, which increases the amount of ketone benzene solvent used and the raw material cost; and a large amount of ketone benzene solvent enters the recovery system, which increases the load of the recovery system and increases energy consumption. In short, the existing solvent dewaxing method can separate the lubricating oil from the high melting point wax component, but the yield of the product oil and wax is low, the output of the by-product wax oil is large, the energy consumption of the recovery system is high, and the lubricating oil processing cost is high. Summary of the invention
[0005] In order to solve the above technical problems, the present invention provides a lubricating oil solvent dewaxing method.
[0006] The technical solution adopted by the present invention is:
[0007] A lubricating oil solvent dewaxing method comprises the following steps:
[0008] 1) The crude oil is gradually and slowly cooled to the dewaxing filtration temperature in the crystallization system and then enters the filtration system. During the cooling process, the primary dilution solvent and the secondary dilution solvent are sequentially added. After the temperature drops to the dewaxing filtration temperature, the tertiary dilution solvent is added to form a mixed material;
[0009] 2) After dewaxing and filtration, the mixed material is divided into two parts: oil-containing wax liquid and filtrate. A part of the filtrate is recycled as a tertiary dilution solvent, and the remaining part of the filtrate is sent to a filtrate recovery system to produce dewaxed oil;
[0010] 3) The oily wax liquid is mixed with the first-stage deoiling dilution solvent and then filtered through the first-stage deoiling to produce two materials, first-stage deoiled wax and first-stage wax oil. A portion of the first-stage wax oil is returned to the crystallization system as a primary dilution solvent and a secondary dilution solvent for recycling, and the remaining first-stage wax oil is sent to the wax oil recovery system to produce a by-product wax oil;
[0011] 4) The first-stage deoiled wax is divided into two parts after the second-stage deoiling and filtering, and the second-stage wax oil is recycled as the first-stage deoiling dilution solvent, and the second-stage deoiled wax enters the wax liquid recovery system to produce deoiled wax;
[0012] 5) The filtrate recovery system, wax liquid recovery system and wax oil recovery system separate the material and the solvent through evaporation. The evaporated solvent enters the solvent recovery system for solvent recovery. The recovered solvent is used as the supplementary solvent for the primary dilution solvent, the secondary dilution solvent and the tertiary dilution solvent.
[0013] Preferably, the mass ratio of the primary dilution solvent to the feedstock oil is 0.6-1.0, the mass ratio of the secondary dilution solvent to the feedstock oil is 1.0-1.2, and the mass ratio of the tertiary dilution solvent to the feedstock oil is 1.1-1.3.
[0014] When the primary solvent ratio is relatively large, it is beneficial to speed up the flow rate of the crude oil, but the wax oil content increases and the dewaxed oil yield decreases. Therefore, the amount of primary solvent added should be as low as possible while ensuring the normal flow of materials; increasing the secondary dilution ratio can increase the amount of oil dissolved at low temperatures, but too high a solvent amount will increase the recovery load and increase the cost of the device; tertiary dilution can further reduce the viscosity of the solution and dissolve the oil on the surface of the wax crystals, but if the tertiary solvent ratio is further increased, the solubility of the wax will also increase, increasing the dewaxing temperature difference. Therefore, it is necessary to reasonably control the mass ratio of the primary, secondary, and tertiary dilution solvents to the crude oil.
[0015] Preferably, the temperature of the primary dilution solvent is 26-30°C, the temperature of the secondary dilution solvent is 3-5°C, and the temperature of the tertiary dilution solvent is -22.5°C±0.5.
[0016] The solvent temperature at the dilution solvent addition point should be 2°C to 3°C lower than the raw oil temperature. If the solvent temperature is higher than the oil temperature, the wax crystals will melt and affect the growth of the crystal nuclei. If the solvent temperature is too low, the wax oil content will increase and the dewaxed oil yield will decrease. Therefore, it is necessary to reasonably control the addition temperature of the primary dilution solvent and the secondary dilution solvent; in principle, the temperature of the tertiary dilution agent should not be higher than the dewaxing feed temperature. On the basis of ensuring that the pour point of the dewaxed oil is qualified, the temperature of the tertiary dilution agent should be appropriately increased to prevent excess product quality, reduce the refrigeration load, and save energy and reduce consumption. Therefore, it is necessary to reasonably control the temperature of the tertiary dilution solvent.
[0017] Preferably, the mass ratio of the dilution solvent to the raw oil in the first stage of deoiling is 2.2 to 2.4, which is beneficial to reducing the yield of oil under wax and improving the product yield.
[0018] Preferably, the temperature of the dilution solvent in the deoiling stage is 7-8° C., which is beneficial to reducing the load of the recovery system and further reducing energy consumption.
[0019] Preferably, the content of ketone benzene solvent in the first-stage wax oil is 90-92%, and the content of ketone benzene solvent in the second-stage wax oil is 80-82%; this is beneficial to further reduce the amount of ketone benzene solvent used and reduce the processing cost of lubricating oil while fully ensuring oil-wax separation.
[0020] The beneficial effects of the present invention are as follows: the present invention uses the first-stage wax oil to replace the ketone benzene solvent as the primary and secondary dilution solvent, and uses the second-stage wax oil to replace the ketone benzene solvent as the tertiary dilution solvent, thereby greatly reducing the total amount of the ketone benzene solvent entering the recovery system for evaporation, reducing the heat load of the recovery system, reducing energy consumption, and further reducing the processing cost of the lubricating oil; at the same time, since part of the first-stage wax oil and the second-stage wax oil are mixed with the raw materials as the dilution solvent and then enter the crystallization and filtration system again, the lubricating oil and high-melting-point wax carried in the first-stage wax oil and the second-stage wax oil can be recycled again, thereby improving the product yield of dewaxed oil and deoiled wax, and can increase the dewaxed oil yield by 1.5% to 2%, and reduce the yield of the by-product wax oil, thereby reducing the processing cost of the lubricating oil. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 The present invention is a schematic flow diagram of a lubricating oil solvent dewaxing method.
[0022] Figure 2 It is a schematic flow diagram of the existing lubricating oil solvent dewaxing method.
[0023] Figure numerals: raw oil A, 102-mixed material A, 103-oil-containing wax liquid A, 104-filtrate A, 105-first stage deoiled wax A, 106-first stage wax oil-removed A, 107-second stage wax oil-removed A, 108-second stage deoiled wax A, 109-ketone benzene solvent A, 201-raw oil B, 202-mixed material B, 203-oil-containing wax liquid B, 204-filtrate B, 205-first stage deoiled wax B, 206-first stage wax oil-removed B, 207-second stage wax oil-removed B, 208-second stage deoiled wax B, 209-ketone benzene solvent B. DETAILED DESCRIPTION
[0024] The technical solution of the present invention is further described below by taking the processing of three-line wax oil as an example to facilitate the understanding of the present invention, but the present invention is not limited thereto.
[0025] Example 1
[0026] See also Figure 1 This embodiment provides a lubricating oil solvent dewaxing method, comprising the following steps:
[0027] (1) 35 tons of crude oil A101 is gradually and slowly cooled in a crystallization system. During the cooling process, 24.5 tons of a primary dilution solvent and 38.5 tons of a secondary dilution solvent are sequentially added to the crude oil A101. When the temperature drops to the dewaxing filtration temperature, 42 tons of a tertiary dilution solvent is added. Finally, 140 tons of a mixed material A102 is formed and enters the filtration system.
[0028] (2) After dewaxing and filtration, the mixed material A102 produces two parts, namely 62.02 tons of oil-containing wax liquid A103 and 123.48 tons of filtrate A104. After cooling, 42 tons of filtrate A104-01 is used as a tertiary dilution solvent and sent to the crystallization system to mix with A101. The remaining 81.48 tons of filtrate A104-02 is sent to the filtrate recovery system for solvent recovery to produce 22.75 tons of product dewaxed oil;
[0029] (3) 62.02 tons of the oil-containing wax liquid A103 was mixed with 80.5 tons of the first-stage deoiling dilution solvent and then filtered through the first-stage deoiling to produce two materials, namely 61.69 tons of the first-stage deoiled wax A105 and 122.83 tons of the first-stage wax lower oil A106; 24.5 tons of the first-stage wax lower oil A106-01 was cooled and used as the primary dilution solvent to be pumped into the crystallization system and mixed with the raw oil A101, 38.5 tons of the first-stage wax lower oil A106-02 was cooled and used as the secondary dilution solvent to be pumped into the crystallization system and mixed with the raw oil A101, and the remaining 59.83 tons of the first-stage wax lower oil A106-03 was sent to the wax lower oil recovery system for solvent recovery to produce 3.5 tons of by-product wax lower oil;
[0030] (4) After the second stage deoiling and filtration, 61.69 tons of the first stage deoiled wax A105 is divided into two parts, namely 21.19 tons of the second stage deoiled wax A108 and 80.5 tons of the second stage wax lower oil A107. The 80.5 tons of the second stage wax lower oil A107 is sent to the front road to be used as the first stage deoiling dilution solvent, and the 21.19 tons of the second stage deoiled wax A108 enters the wax liquid recovery system for solvent recovery to produce 10.5 tons of product deoiled wax.
[0031] (5) The filtrate recovery system, wax liquid recovery system and wax oil recovery system utilize the different boiling points of the solvent and the material to separate the material from the solvent through heating and evaporation. The evaporated solvent enters the solvent recovery system for cooling and recovery. The recovered solvent can be used for cold washing of the filter machine and for solvent replenishment for the first, second and third dilutions.
[0032] In this embodiment, the mass ratio of the first dilution solvent to the raw oil A101 is 0.7, the mass ratio of the second dilution solvent to the raw oil 101 oil A is 1.1, and the mass ratio of the tertiary dilution solvent to the raw oil A101 is 1.2; the mass ratio of the first dilution solvent for deoiling to the oil-containing wax liquid is 2.3; the temperature of the first dilution solvent for deoiling is 7°C.
[0033] In this embodiment, the ketone benzene solvent content in the first-stage wax oil A106 is between 90 and 92%, and the ketone benzene solvent content in the second-stage wax oil A107 is between 80 and 82%. The temperature of the first-stage wax oil A106 as a primary dilution solvent is controlled at 28 to 30°C, the temperature of the second-stage wax oil A107 as a secondary dilution solvent is controlled at 3 to 5°C, and the temperature of the filtrate A104 as a tertiary dilution solvent is controlled at about -23°C.
[0034] Comparative Example 1
[0035] See also Figure 2 The existing lubricating oil solvent dewaxing method comprises the following steps:
[0036] 1) 35 tons of crude oil B201 is gradually and slowly cooled in a crystallization system. During the cooling process, crude oil B201 is sequentially mixed with 24.5 tons of primary dilution solvent, 38.5 tons of secondary dilution solvent and 42 tons of tertiary dilution solvent to form 140 tons of mixed material B102;
[0037] 2) 140t of mixed material B202 is dewaxed and filtered to produce two parts, namely 62.02t of oil-containing wax liquid A103 and 123.48t of filtrate B204. 123.48t of filtrate B204 is sent to the filtrate recovery system for solvent recovery to produce 19.7t of product dewaxed oil;
[0038] 3) 62.02 tons of oil-containing wax liquid B203 is mixed with the first-stage deoiling dilution solvent and then filtered through the first-stage deoiling to be divided into two parts: the first-stage deoiled wax B205 and the first-stage wax oil B206; 117.54 tons of the first-stage wax oil B206 is sent to the wax oil recovery system for solvent recovery to produce 17.4 tons of by-product wax oil;
[0039] 4) 66.98t of the first stage deoiled wax B205 is divided into 26.48t of the second stage deoiled wax B208 and 80.5t of the second stage wax oil B207 after second stage deoiling and filtration. 80.5t of the second stage wax oil B207 is returned to the previous process as the first stage deoiling dilution solvent; 26.48t of the second stage deoiled wax B208 enters the wax liquid recovery system for solvent recovery to produce 10.12t of product deoiled wax;
[0040] 5) The solvent after evaporation of 123.48t of filtrate B204, 117.54t of first-stage wax oil B206, and 26.48t of second-stage deoiled wax B208 enters the solvent recovery system for cooling, and the recovered ketone benzene solvent B209 is reused as the primary, secondary, and tertiary dilution solvent.
[0041] In Comparative Example 1, the mass ratio of the dilution solvent to the raw oil, the temperature of the dilution solvent, the ketone benzene solvent content in the first-stage wax oil and the second-stage wax oil, the mass ratio of the first-stage deoiling dilution solvent to the oil-containing wax liquid, and the temperature of the first-stage deoiling dilution solvent are the same as those in Example 1.
[0042] From the statistics of the product yields and energy consumption of Example 1 and Comparative Example 1, it can be seen that the comprehensive yield of the dewaxed oil and deoiled wax of Example 1 is increased from 85.2% in Comparative Example 1 to 93.13%, the yield of the by-product wax oil is reduced from 14.8% in Comparative Example 1 to 6.87%, and the energy consumption of the entire system is reduced from 92.66 kgEo / t in Comparative Example 1 to about 89.58 kgEo / t.
[0043] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications are also within the protection scope of the present invention.
Claims
1. A lubricating oil solvent dewaxing method, characterized in that: The following steps are involved: 1) The feedstock oil (101) is gradually and slowly cooled to a dewaxing filtration temperature in a crystallization system and then enters a filtration system. During the continuous cooling process, a primary dilution solvent and a secondary dilution solvent are sequentially added. After the temperature drops to a dewaxing filtration temperature, a tertiary dilution solvent is added to form a mixed material (102); 2) After dewaxing and filtration, the mixed material (102) is separated into two parts: oil-containing wax liquid (103) and filtrate (104), a part of the filtrate (104-01) is recycled as a tertiary dilution solvent, and the remaining part of the filtrate (104-02) is sent to a filtrate recovery system to produce dewaxed oil; 3) The oily wax liquid (103) is mixed with the first-stage deoiling dilution solvent and then filtered through the first-stage deoiling to produce two materials, namely, the first-stage deoiled wax (105) and the first-stage wax oil (106). A portion of the first-stage wax oil (106) is returned to the crystallization system for recycling as the first dilution solvent (106-01) and the second dilution solvent (106-02), and the remaining first-stage wax oil (106-03) is sent to the wax oil recovery system to produce the by-product wax oil; 4) The first-stage deoiled wax (105) is separated into two parts, namely, the second-stage deoiled wax (108) and the second-stage wax oil (107), after being filtered through the second-stage deoiling. The second-stage wax oil (107) is recycled as a dilution solvent for the first-stage deoiling, and the second-stage deoiled wax (108) enters a wax liquid recovery system to produce deoiled wax; 5) The filtrate recovery system, wax liquid recovery system and wax oil recovery system separate the material and the solvent through evaporation. The evaporated solvent enters the solvent recovery system for solvent recovery. The recovered solvent is used as the supplementary solvent for the primary dilution solvent, the secondary dilution solvent and the tertiary dilution solvent; The mass ratio of the primary dilution solvent to the raw oil is 0.6-1.0, the mass ratio of the secondary dilution solvent to the raw oil is 1.0-1.2, the mass ratio of the tertiary dilution solvent to the raw oil is 1.1-1.3; the mass ratio of the first dilution solvent to the oil-containing wax liquid is 2.2-2.4; The content of ketone benzene solvent in the first-stage wax oil (106) is 90-92%, and the content of ketone benzene solvent in the second-stage wax oil (107) is 80-82%.
2. A lubricating oil solvent dewaxing method according to claim 1, characterized in that: The temperature of the primary dilution solvent is 26-30°C, the temperature of the secondary dilution solvent is 3-5°C, and the temperature of the tertiary dilution solvent is -22.5°C±0.
5.