A kind of reconstituted tobacco leaf and preparation method thereof
By preparing coating layers on the surface of reconstructed tobacco leaves and using hydrophobic agents and other materials to form barrier barriers, the problem of unstable hygroscopic properties is solved, the moisture absorption performance and moisture stability are improved, the processing resistance and sensory quality of heated cigarettes are improved, and the process resistance and sensory quality of heated cigarettes are extended. Storage cycle.
Patent Information
- Application Number
- CN202211413499.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-11
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2042-11-11
AI Technical Summary
The moisture absorption performance of reconstructed tobacco leaves is unstable, resulting in moisture absorption or desorption, affecting the quality of the wire making process, rolling process and moisture content fluctuations in the storage process, resulting in unstable sensory quality and short storage period.
By preparing a coating layer as the upper and lower epidermis on the surface of the reconstructed tobacco leaves, it is coated and dried using a coating liquid composed of hydrophobic agent, adhesive, dispersant and water to form a barrier to prevent moisture absorption or loss and improve moisture absorption Performance and moisture stability.
It improves the moisture absorption and moisture stability of the rebuilt tobacco leaves, enhances the processing resistance, sensory quality stability and storage cycle, extends the shelf life, and ensures the stability of product quality and consumer experience.
Smart Images

Figure CN115777979B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of tobacco products, and in particular to a reconstituted tobacco leaf and a preparation method thereof. Background Art
[0002] Reconstituted tobacco is the main core material used in heated cigarettes and is also the core raw material of heated cigarettes. Heated cigarettes are one of the important forms of new tobacco products. Unlike traditional cigarettes that generate flavor substances by burning tobacco, heated cigarettes use external heat sources to heat rather than ignite, so that the core segment generates an aerosol containing nicotine and characteristic flavor substances for smoking.
[0003] The production processes of reconstituted tobacco mainly include roller pressing, thick slurry method, papermaking method, dry method, etc. Roller pressing reconstituted tobacco is to crush tobacco stems, tobacco dust, tobacco leaf fragments and other tobacco materials, and then mix them with adhesives, enhancers, humectants, water and other materials in a certain proportion to form loose granules, and then roll them through a roller press to form sheets for drying, and finally cut them into reconstituted tobacco shreds by a shredder. Thick slurry reconstituted tobacco is to crush tobacco materials and mix them into an aqueous solution with adhesives, enhancers, humectants and water, and then stir them evenly to form a slurry, which is evenly spread on a stainless steel belt for drying, and then formed into reconstituted tobacco after shoveling. Papermaking reconstituted tobacco is made by soaking tobacco stems, fragments, and tobacco dust in hot water for extraction and solid-liquid separation. The obtained extract is vacuum concentrated and then mixed into a coating liquid. The remaining solid residue is pulped and formed into a sheet base on a specific paper machine. The coating liquid is then evenly coated on the surface of the sheet base and dried to form reconstituted tobacco. The dry reconstituted tobacco process uses airflow as a fiber carrier and produces reconstituted tobacco through processes such as air settling, hot rolling, spray drying, etc.
[0004] Hygroscopicity is one of the basic physical properties of reconstituted tobacco. A large amount of polyols (glycerol, propylene glycol, etc.) need to be introduced as smoke-generating agents during the production process of reconstituted tobacco. Polyols containing hydrophilic hydroxyl structures cause the hygroscopic properties of reconstituted tobacco to be significantly different from those of traditional tobacco. The hygroscopic properties of reconstituted tobacco are directly related to the operating conditions of the wet heat treatment unit during the production process, the physical and mechanical properties of the formed sheet base, the quality of heated cigarette products, storage and transportation in special environments, storage under high temperature and high humidity conditions, shelf life storage, and consumers' smoking experience.
[0005] At present, the moisture absorption / desorption performance of the surface of reconstituted tobacco leaves is unstable, and it is easy to absorb or desorb moisture with the change of ambient temperature and humidity, which in turn has an adverse effect on the shred-making process of heated cigarettes, the quality of the rolling process, the fluctuation of moisture content during the storage process of cigarettes, and even the stability of the sensory quality of heated cigarettes. Improving the moisture absorption performance of reconstituted tobacco leaves and solving the problems of poor adaptability to machines and fluctuation of sensory quality caused by moisture absorption are important issues that need to be solved in the field of reconstituted tobacco leaves. Summary of the invention
[0006] In order to solve the above technical problems, the first purpose of the present invention is to provide a method for preparing reconstituted tobacco leaves; the second purpose of the present invention is to provide reconstituted tobacco leaves prepared by the above preparation method; the reconstituted tobacco leaves and the preparation method thereof provided by the present invention, through the epidermis reconstruction technology, prepare a coating layer as the upper epidermis and the lower epidermis on the surface of the reconstituted tobacco leaf body, through the barrier effect of the upper epidermis and the lower epidermis, prevent the reconstituted tobacco leaves from absorbing too much water or losing water, maintain the stability of water content, solve the problems of poor processing resistance, sensory quality fluctuations and short shelf life due to poor hygroscopicity, so that the prepared reconstituted tobacco leaves have more moderate hygroscopic properties, and improve the hygroscopic properties and water stability of the reconstituted tobacco leaves.
[0007] The technical solution provided by the present invention is as follows:
[0008] A method for preparing reconstituted tobacco leaves comprises the following steps:
[0009] preparing a coating solution, the coating solution comprising a hydrophobic agent, an adhesive, a dispersant and water;
[0010] obtaining a reconstituted tobacco leaf body;
[0011] The coating liquid is sequentially coated on the upper and lower surfaces of the reconstituted tobacco leaf body and dried to form coating layers on both sides.
[0012] Preferably, the coating liquid has a solid content of 1%-20% and a viscosity of 50-2000 mPa·s.
[0013] Preferably, the coating liquid further comprises any one or more of tobacco extract, food additives, and tobacco flavors.
[0014] Preferably, the coating solution comprises the following raw materials in parts by weight:
[0015] 1-15 parts by weight of a hydrophobic agent, 1-10 parts by weight of an adhesive, 1-3 parts by weight of a dispersant, 1-10 parts by weight of a tobacco extract, 1-5 parts by weight of a food additive, 1-3 parts by weight of a tobacco flavor and 70-95 parts by weight of water.
[0016] Preferably, the hydrophobic agent is one or more of paraffin wax, rice bran wax, hard mineral wax, shellac, sunflower wax, candelilla wax, and carnauba wax;
[0017] The adhesive is one or more of carrageenan, xanthan gum, guar gum, carob bean gum, locust bean gum, pectin, sodium carboxymethyl cellulose, methyl cellulose, hydroxymethyl cellulose, hydroxyethyl cellulose, hydroxypropyl methyl cellulose, cationic starch, and alginate;
[0018] The dispersant is one or more of polyethylene glycol, sodium carboxymethyl starch, sodium polyacrylate, hydroxyethyl starch, gum arabic, and sodium lignin sulfonate.
[0019] Preferably, the tobacco extract is one or more of flue-cured tobacco extract, sun-cured tobacco extract, burley tobacco extract, and oriental tobacco extract;
[0020] The food additive is one or more of glyceryl monostearate, glyceryl distearate, glyceryl tristearate, etc.;
[0021] The tobacco flavor is two or more of vanillin, menthol, geraniol and citronellol.
[0022] Preferably, the basis weight of the reconstituted tobacco leaf body is 40-200 g / m 2 The mass fraction of the smoke generating agent in the reconstituted tobacco leaf body is 0-30%.
[0023] Preferably, the reconstituted tobacco leaf body is made by one or more processes including rolling method, thick pulp method, papermaking method and dry method.
[0024] Preferably, the coating liquid is coated on the surface of the reconstituted tobacco leaf body by one or more of the following processes: roller coating, size pressing, metering rod film transfer coating, dip coating, spray coating, curtain coating, multi-layer slide coating, slit coating, and extrusion coating.
[0025] Preferably, in the reconstituted tobacco, the mass fraction of the coating layer is 1-10%, and the mass fraction of the reconstituted tobacco body is 90-99%.
[0026] Preferably, during coating, the coating rate is 1-15% and the coating amount is 1-15 g / m 2 .
[0027] Preferably, the static contact angle of the coating layer is 70-120°.
[0028] Preferably, the drying is carried out by hot air drying, and the hot air temperature is 80-110°C.
[0029] Reconstituted tobacco leaves prepared by any of the preparation methods described above.
[0030] The present application provides a method for preparing reconstituted tobacco, comprising the following steps: preparing a coating liquid, the coating liquid comprising a hydrophobic agent, an adhesive, a dispersant and water; obtaining a reconstituted tobacco body; applying the coating liquid sequentially on the upper and lower surfaces of the reconstituted tobacco body and drying to form coating layers on both sides. The method for preparing reconstituted tobacco provided by the present application sequentially transfers the coating liquid to the upper and lower surfaces of the reconstituted tobacco body, dries to form coating layers, i.e., forms a reconstituted tobacco consisting of three parts, namely, an upper epidermis, a lower epidermis and a reconstituted tobacco body located between the upper and lower epidermis. The upper epidermis and the lower epidermis are tightly combined with the reconstituted tobacco body through coating and drying processes, and the barrier hydrophobic effect of the upper epidermis and the lower epidermis is utilized to effectively solve the hygroscopicity problem of existing reconstituted tobacco, thereby forming a bionic reconstituted tobacco that meets the requirements of cigarette hygroscopic / dehumidification performance and sensory quality.
[0031] In the present application, there is no order requirement for the steps of obtaining the reconstituted tobacco leaf body or preparing the coating liquid. In the present application, the reconstituted tobacco leaf body can be prepared by itself or purchased from outside.
[0032] Existing types of reconstituted tobacco include rolling method, thick pulp method, papermaking method, dry method and reconstituted tobacco obtained by combination or extension of these methods. The existing manufacturing methods or processes of reconstituted tobacco do not involve the epidermis problem of reconstituted tobacco. They only produce a reconstituted tobacco body equivalent to the mesophyll tissue in plant leaves, which lacks upper and lower epidermis. Therefore, there is a lack of a "barrier" to prevent moisture absorption and release, which causes the moisture absorption / release performance of the reconstituted tobacco to be unstable. During the cigarette processing process, the moisture content fluctuates easily due to changes in environmental temperature and humidity, which leads to poor processing resistance, moisture absorption, adhesion, mildew and serious impact on the sensory quality of cigarettes.
[0033] At present, the roller-pressed, thick pulp, papermaking and dry-process reconstituted tobacco leaves used for heated cigarettes all contain 10%-30% by mass of glycerin, propylene glycol and other smoking agents. Smoking agents such as glycerin and propylene glycol have moisturizing and hygroscopic effects. After the humectants are mixed with tobacco particles, they are directly exposed to the air. When the ambient temperature and humidity conditions change, for example, when the humidity is greater than 60%, the reconstituted tobacco leaves will absorb moisture from the environment, which is called hygroscopicity; when the humidity is less than 40%, the reconstituted tobacco leaves will release moisture from the inside to the outside, which is called desorption or dehumidification.
[0034] The existing reconstituted tobacco leaves and preparation methods thereof have the following problems:
[0035] (1) The main part of the reconstituted tobacco leaf has no epidermis to protect the internal structure. The smoke-generating agent or tobacco extract is directly exposed to the air, causing moisture absorption, which affects the processing resistance of the reconstituted tobacco leaf during the shredding, rolling and packaging processes.
[0036] (2) As the ambient temperature and humidity change, the reconstituted tobacco leaves absorb or desorb moisture, causing the moisture content to increase or decrease, resulting in fluctuations in the sensory quality of heated cigarettes or cigarettes, leading to serious quality defects.
[0037] (3) Unstable moisture content of reconstituted tobacco leaves will affect the storage cycle and shelf life of heated cigarettes or cigarettes, causing quality problems such as mold spots, adhesion, and deterioration.
[0038] The biological structure of plant leaves consists of three parts: epidermis, mesophyll and veins. The epidermis is the lifelong protective tissue of the leaf, covering the surface of the leaf, and is divided into the upper epidermis and the lower epidermis. The epidermal cells are composed of a dormant cuticle and a wax layer. The main function of the wax layer is to retain water and prevent the non-stomatal loss of water in plant tissues. The present invention proposes a bionic reconstructed tobacco leaf based on the structure of a plant leaf. Through the epidermis reconstruction technology, the upper epidermis and the lower epidermis are given to the reconstructed tobacco leaf body, which effectively solves a series of problems caused by the moisture absorption of existing reconstructed tobacco leaves.
[0039] Specifically, the present invention has the following beneficial effects:
[0040] (1) The bionic reconstructed tobacco leaf based on the plant leaf structure prepared by the present invention has greatly improved hygroscopic performance, and the bionic reconstructed tobacco leaf shows good processing resistance in the processes of shredding, cutting, adding materials and flavoring, rolling and forming, packaging and storage.
[0041] (2) The bionic reconstructed tobacco leaves prepared by the present invention based on the plant leaf structure have been greatly improved in terms of sensory quality stability, and the smoke concentration, fullness, fullness, and thickness are significantly enhanced. The tobacco flavor is strong, mellow and natural, and the smoke irritation and dryness are reduced. Compared with the existing reconstructed tobacco leaves, the number of effective puffs is increased from 7-8 puffs to 10-12 puffs, and the puff persistence and aroma texture stability are significantly enhanced.
[0042] (3) The bionic reconstructed tobacco leaves based on the plant leaf structure prepared by the present invention can greatly extend the storage period and shelf life after being used in cigarettes or heated cigarettes, thereby ensuring the stability of product quality and the consumer experience.
[0043] (4) The bionic reconstructed tobacco leaf with regenerated epidermis provided by the present invention has further improved surface strength and tensile strength, reduced hair and powder loss rate, and further enhanced adaptability to machine operation.
[0044] Preferably, the coating liquid has a solid content of 1% to 20% and a viscosity of 50 to 2000 mPa·s.
[0045] Preferably, the tobacco extract, food additives and tobacco flavors are also included.
[0046] It is further preferred that the coating liquid comprises the following raw materials in parts by weight: 1-15 parts by weight of a hydrophobic agent, 1-10 parts by weight of an adhesive, 1-3 parts by weight of a dispersant, 1-10 parts by weight of a tobacco extract, 1-5 parts by weight of a food additive, 1-3 parts by weight of a tobacco flavor and 70-95 parts by weight of water.
[0047] Hydrophobic agents, adhesives, dispersants, tobacco extracts, and food additives can be selected from one or more of a variety of substances. Adhesives are used to bond the components in the coating liquid and to bond the coating liquid to the reconstituted tobacco leaves. Dispersants are used to prevent the particles of the coating liquid from agglomerating with each other and to improve the stability of the coating liquid. Tobacco extracts are used to increase the tobacco flavor of the reconstituted tobacco leaves and improve the sensory quality evaluation. Food additives are used to give the reconstituted tobacco leaves more flavors and are added according to demand. Tobacco flavors are selected from two or more of vanillin, menthol, geraniol, and citronellol, and are used to flavor and correct the reconstituted tobacco leaves to produce a beautiful aroma and a comfortable taste.
[0048] The preparation method of reconstituted tobacco provided by the present application, the reconstituted tobacco body used can be made by one or more processes of existing conventional methods, such as roller pressing, thick pulp method, papermaking method, and dry method. The present application solves the problem of tobacco leaf moisture absorption by coating the upper and lower surfaces of the reconstituted tobacco body with coating liquid and drying respectively to form a coating layer. The coating process can adopt one or more of roller coating, size pressing, metering rod film transfer coating, dip coating, spray coating, curtain coating, multi-layer slide coating, slit coating, and extrusion coating. Depending on the coating process, it can be selected whether to coat and dry one side first, or to coat and dry both sides at the same time. For example, spray coating is to coat the upper surface first, dry, and then coat the lower surface and dry. Dip coating is to coat both sides at the same time, and then dry both sides at the same time. It can be flexibly selected according to the needs of the actual process.
[0049] Preferably, in the reconstituted tobacco leaf formed after drying, the coating layer accounts for 1-10% by mass, and the reconstituted tobacco leaf body accounts for 90-99% by mass. The mass of the reconstituted tobacco leaf body here refers to the absolute dry mass of the reconstituted tobacco leaf.
[0050] Preferably, the coating rate is 1-15% and the coating amount is 1-15g / m 2 After drying, the static contact angle of the coating layer is 70-120°.
[0051] Preferably, the drying is carried out by hot air drying, the hot air temperature is 80-110° C., the drying time is 20-40 minutes, and the moisture content of the reconstituted tobacco leaves is 8-12%.
[0052] The weight of reconstituted tobacco leaves is 40-200g / m 2The mass fraction of the smoke-generating agent in the reconstituted tobacco leaf is 0-30%, and the weight of the reconstituted tobacco leaf product obtained after coating and drying is 50-210g / m 2 The mass fraction of the smoke agent in the finished product is 0-20%, and the tensile strength of the finished product is ≥350N / m. BRIEF DESCRIPTION OF THE DRAWINGS
[0053] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0054] Figure 1 is the static contact angle of the tobacco leaf reconstituted by the bionic roller pressing method according to Example 1 of the present invention;
[0055] Figure 2 is the static contact angle of the tobacco leaf reconstituted by the bionic thick pulp method according to Example 2 of the present invention;
[0056] Figure 3 is the static contact angle of the tobacco leaf reconstituted by the bionic papermaking method according to Example 3 of the present invention;
[0057] Figure 4 This is the static contact angle of the traditional reconstituted tobacco leaf used as a comparative example of the present invention. DETAILED DESCRIPTION
[0058] In order to enable those skilled in the art to better understand the technical solutions in this application, the technical solutions in the embodiments of this application will be clearly and completely described below. Obviously, the described embodiments are only part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0059] It should be noted that when an element is referred to as being "fixed on" or "set on" another element, it can be directly on the other element or indirectly set on the other element; when an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.
[0060] It should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0061] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, "multiple" and "several" mean two or more, unless otherwise clearly and specifically defined.
[0062] It should be noted that the structures, proportions, sizes, etc. illustrated in the drawings of this specification are only used to match the contents disclosed in the specification for people familiar with this technology to understand and read, and are not used to limit the conditions under which this application can be implemented. Therefore, they have no substantive technical significance. Any structural modification, change in proportional relationship or adjustment of size should still fall within the scope of the technical content disclosed in this application without affecting the effects and purposes that can be achieved by this application.
[0063] Example 1
[0064] The coating liquid formula is: in parts by weight, 5 parts by weight of hydrophobic agent paraffin, 2 parts by weight of adhesive sodium carboxymethyl cellulose, 1 part by weight of dispersant sodium lignin sulfonate, 4 parts by weight of tobacco extract flue-cured tobacco extract, 2 parts by weight of food additive glyceryl monostearate, 1 part by weight of tobacco flavoring vanillin and 85 parts by weight of water;
[0065] The coating liquid had a solid content of 3% and a viscosity of 450 mPa·s.
[0066] The roll-pressed reconstituted tobacco leaf body is prepared by the roller-pressed production process, and the basis weight of the roller-pressed reconstituted tobacco leaf body is 85g / m 2 The mass fraction of the smoke-generating agent glycerol in the reconstituted tobacco leaf body is 15%.
[0067] The prepared coating liquid is first sprayed on the upper surface of the reconstituted tobacco leaf body by spray coating, and then sent to the oven for hot air drying at 90℃; then sprayed on the lower surface of the reconstituted tobacco leaf body, and then sent to the oven for hot air drying at 90℃. The spraying amount is 2.5g / m 2 The total coating rate of the coating process is 5.5%, and the total coating amount is 5g / m 2The bionic reconstructed tobacco leaf having an upper epidermis and a lower epidermis was obtained, and the moisture content of the reconstructed tobacco leaf was controlled to be 10%. The obtained bionic reconstructed tobacco leaf was tested for physical properties, hydrophobic properties and hygroscopic properties, and the test results are shown in Table 1.
[0068] Example 2
[0069] The coating liquid formula is: in parts by weight, 10 parts by weight of paraffin wax as a hydrophobic agent, 1 part by weight of sodium carboxymethyl cellulose as an adhesive, 1 part by weight of sodium lignin sulfonate as a dispersant, 1 part by weight of a tobacco extract, 1 part by weight of a flue-cured tobacco extract, 1 part by weight of a food additive, 1 part by weight of glyceryl monostearate, 1 part by weight of a tobacco flavoring, and 85 parts by weight of water;
[0070] The coating liquid had a solid content of 5% and a viscosity of 238 mPa·s.
[0071] The thick pulp production process was used to prepare the reconstituted tobacco leaf body, and the basis weight of the roller-pressed reconstituted tobacco leaf body was 135g / m 2 The mass fraction of the smoke-generating agent glycerol in the reconstituted tobacco leaf body is 18%.
[0072] The prepared coating liquid is first sprayed on the upper surface of the reconstituted tobacco leaf body by spray coating, and then sent to the oven for hot air drying at 95℃; then sprayed on the lower surface of the reconstituted tobacco leaf body, and then sent to the oven for hot air drying at 95℃. The spraying amount is 4g / m 2 The total coating rate of the coating process is 5.6%, and the total coating amount is 8g / m 2 The bionic reconstructed tobacco leaf having an upper epidermis and a lower epidermis was obtained, and the moisture content of the reconstructed tobacco leaf was controlled to be 10%. The obtained bionic reconstructed tobacco leaf was tested for physical properties, hydrophobic properties and hygroscopic properties, and the test results are shown in Table 1.
[0073] Example 3
[0074] The coating liquid formula is: in parts by weight, 15 parts by weight of hydrophobic agent paraffin, 1 part by weight of adhesive sodium carboxymethyl cellulose, 1 part by weight of dispersant sodium lignin sulfonate, 1 part by weight of tobacco extract flue-cured tobacco extract, 1 part by weight of food additive glyceryl monostearate, 1 part by weight of tobacco flavor vanillin and 80 parts by weight of water;
[0075] The coating liquid had a solid content of 10% and a viscosity of 856 mPa·s.
[0076] The thick slurry production process was used to prepare the reconstituted tobacco leaf body, and the basis weight of the roller-pressed reconstituted tobacco leaf body was 97g / m 2 The mass fraction of the smoke-generating agent glycerol in the reconstituted tobacco leaf body is 16%.
[0077] The prepared coating liquid is sprayed on the upper surface of the reconstituted tobacco leaf body by spray coating, and then sent to the oven for hot air drying at 90℃; then it is sprayed on the lower surface of the reconstituted tobacco leaf body and sent to the oven for hot air drying at 90℃. The spraying amount is 5g / m 2 The total coating rate of the coating process is 9.3%, and the total coating amount is 10g / m 2 The bionic reconstructed tobacco leaf having an upper epidermis and a lower epidermis was obtained, and the moisture content of the reconstructed tobacco leaf was controlled to be 10%. The obtained bionic reconstructed tobacco leaf was tested for physical properties, hydrophobic properties and hygroscopic properties, and the test results are shown in Table 1.
[0078] The test methods and standards for the various physical and chemical properties recorded in Table 1 are as follows:
[0079] GB / T 451.2-2002 Determination of basis weight of paper and paperboard;
[0080] GB / T12914-2008 Determination of tensile strength and elongation of paper and paperboard;
[0081] YC / T 243-2008 Determination of 1,2-propylene glycol and glycerol in tobacco and tobacco products - Gas chromatography
[0082] YC / T 31-1996 Preparation of tobacco and tobacco products samples and determination of moisture content by oven method
[0083] The physical and chemical performance indicators of the three bionic reconstituted tobacco leaves prepared in the above embodiments were experimentally determined. The sensory quality evaluation was carried out in accordance with "YC / T 498-2014 Sensory Evaluation Method for Reconstituted Tobacco Leaves (Papermaking Process)" and with reference to "GB 5606.4-2005 Cigarette Part 4 Sensory Technical Requirements". The sensory quality was compared with the traditional reconstituted tobacco leaves (uncoated) prepared by the existing thick pulp method. The results are shown in Table 1.
[0084]
[0085] As can be seen from Table 1, compared with traditional reconstructed tobacco leaves, the physical properties, hydrophobic properties, hygroscopic properties and sensory quality of the bionic reconstructed tobacco leaves of the three embodiments have been significantly improved. Under the premise that the smoke-generating agent content of the bionic reconstructed tobacco leaves is higher than that of the control sample, the static contact angles of the bionic reconstructed tobacco leaves prepared by the roller pressing method, the bionic reconstructed tobacco leaves by the thick pulp method and the bionic reconstructed tobacco leaves by the papermaking method prepared by the epidermal reconstruction technology are increased from 45° to 80°, 90° and 109° respectively, indicating that the upper epidermis and lower epidermis of the bionic reconstructed tobacco leaves have certain hydrophobic properties.
[0086] The moisture absorption experiment further proved that the moisture absorption rate and moisture release rate of the bionic reconstructed tobacco leaves were lower than those of the control sample, indicating that the moisture absorption performance of the bionic reconstructed tobacco leaves has been improved. From the perspective of sensory quality score, due to the addition of a certain amount of tobacco extracts to the upper and lower epidermis of the bionic reconstructed tobacco leaves, new aroma components were introduced, so its sensory quality score was slightly improved. In addition, due to the addition of a certain amount of adhesives to the coating liquid, the tensile strength of the bionic reconstructed tobacco leaves was also increased, which is conducive to improving its processing resistance in the processes of shredding, adding materials and flavoring, rolling and wrapping. In summary, compared with traditional reconstructed tobacco leaves, the physical properties, hydrophobic properties, hygroscopic properties and sensory quality of bionic reconstructed tobacco leaves have been significantly improved, which has better solved the common problems of moisture absorption of existing reconstructed tobacco leaves.
[0087] Example 4
[0088] The same as Example 1, except that the coating liquid formula is: in parts by weight, 5 parts by weight of hard mineral wax as a hydrophobic agent, 2 parts by weight of xanthan gum as an adhesive, 1 part by weight of sodium carboxymethyl starch as a dispersant, 4 parts by weight of burley tobacco extract as a tobacco extract, 2 parts by weight of glyceryl distearate as a food additive, 1 part by weight of menthol as a tobacco flavor, and 85 parts by weight of water.
[0089] Example 5
[0090] The same as Example 1, except that the coating liquid formula is: in parts by weight, 5 parts by weight of hydrophobic agent candelilla wax, 2 parts by weight of adhesive hydroxypropyl methylcellulose, 1 part by weight of dispersant polyethylene glycol, 4 parts by weight of tobacco extract sun-dried tobacco extract, 2 parts by weight of food additive distearin, 1 part by weight of tobacco flavoring citronellol and 85 parts by weight of water.
[0091] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A method for preparing reconstituted tobacco, characterized in that: The following steps are involved: preparing a coating solution, the coating solution comprising a hydrophobic agent, an adhesive, a dispersant and water; obtaining a reconstituted tobacco leaf body; The coating liquid is sequentially coated on the upper and lower surfaces of the reconstituted tobacco leaf body and dried to form coating layers on both sides; The hydrophobic agent is one or more of paraffin wax, rice bran wax, hard mineral wax, shellac, sunflower wax, candelilla wax, and carnauba wax; The adhesive is one or more of carrageenan, xanthan gum, guar gum, carob bean gum, locust bean gum, pectin, sodium carboxymethyl cellulose, methyl cellulose, hydroxymethyl cellulose, hydroxyethyl cellulose, hydroxypropyl methyl cellulose, cationic starch, and alginate; The dispersant is one or more of polyethylene glycol, sodium carboxymethyl starch, sodium polyacrylate, hydroxyethyl starch, gum arabic, and sodium lignin sulfonate; The reconstituted tobacco leaf body is made by one or more processes including roller pressing, thick pulping, papermaking and dry method. The basis weight of the reconstituted tobacco leaf body is 40-200 g / m 2 , the mass fraction of the smoke-generating agent in the reconstituted tobacco leaf is 0-30%; In reconstituted tobacco, the coating layer accounts for 1-10% by mass, and the reconstituted tobacco body accounts for 90-99% by mass; The basis weight of the reconstituted tobacco obtained after coating and drying is 50-210g / m 2 , the mass fraction of smoke agent is 0-20%, and the tensile strength is ≥350N / m; The static contact angle of the coating layer is 70-120°.
2. The method for preparing reconstituted tobacco according to claim 1, characterized in that: The coating liquid has a solid content of 1%-20% and a viscosity of 50-2000 mPa·s.
3. The method for preparing reconstituted tobacco according to claim 2, characterized in that: The coating liquid also includes any one or more of tobacco extract, food additives, and tobacco flavors; Wherein, the tobacco extract is one or both of flue-cured tobacco extract and sun-dried tobacco extract; The food additive is one or more of glyceryl monostearate, glyceryl distearate, and glyceryl tristearate; The tobacco flavor is two or more of vanillin, menthol, geraniol and citronellol.
4. The method for preparing reconstituted tobacco according to claim 3, characterized in that: The coating solution includes the following raw materials in parts by weight: 1-15 parts by weight of a hydrophobic agent, 1-10 parts by weight of an adhesive, 1-3 parts by weight of a dispersant, 1-10 parts by weight of a tobacco extract, 1-5 parts by weight of a food additive, 1-3 parts by weight of a tobacco flavor and 70-95 parts by weight of water.
5. The method for preparing reconstituted tobacco according to claim 1, characterized in that: The coating liquid is coated on the surface of the reconstituted tobacco leaf body by one or more of the following processes: roller coating, size pressing, metering rod film transfer coating, dipping coating, spray coating, curtain coating, multi-layer slide coating, slit coating, and extrusion coating.
6. The method for preparing reconstituted tobacco according to claim 1, characterized in that: When coating, the coating rate is 1-15% and the coating amount is 1-15g / m 2 .
7. The method for preparing reconstituted tobacco according to claim 1, characterized in that: The drying is carried out by hot air drying, the hot air temperature is 80-110°C, the drying time is 20-40min, and the moisture content of the reconstituted tobacco leaves is dried to 8-12%.
8. A reconstituted tobacco leaf produced by the preparation method according to any one of claims 1 to 7.