A defect repair method for large composite material packaging box

Using laser ultrasonic inspection and imaging technology to quickly locate defects in the inner skin of composite packaging boxes, combined with fiber fabric repair agents and vacuum compaction technology, the problem of poor sealing of composite packaging boxes was solved, improving repair efficiency and reducing costs.

CN115817977BActive Publication Date: 2024-10-22AEROSPACE INST OF ADVANCED MATERIALS & PROCESSING TECH
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202211413658.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-11
Publication Date
2024-10-22
Estimated Expiration
2042-11-11

AI Technical Summary

Technical Problem

The sealing effect of large composite packaging boxes is poor after being formed. The traditional manual leak detection method has low detection efficiency, takes a long time, and cannot fundamentally solve the internal air leakage problem. Especially due to the large size of the packaging box, the positioning efficiency is low.

Method used

Laser ultrasonic testing technology combined with imaging technology is used to quickly locate defects in the inner skin of the packaging box, and the required scanning area and the vacuum area are divided for efficient scanning. The fiber fabric and adhesive are used to prepare a repair agent for repair, and a vacuum compaction device is used to ensure sealing. Sanded and sprayed.

Benefits of technology

The efficiency of defect location and repair has been significantly improved, the repair cost has been reduced, and the time to repair 100 defects has been reduced from 400 hours to 201 hours, improving efficiency by 49.75%.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115817977B_ABST
    Figure CN115817977B_ABST
Patent Text Reader

Abstract

The present invention discloses a defect repair method for a large composite material packaging box, which relates to the technical field of composite materials. For a large composite material packaging box to be repaired, its historical repair data is obtained in advance, and the scanning area is divided according to the leakage probability, and the area with a leakage probability exceeding 10% is set as a must-scan area, and the remaining scanning area is divided into a random scanning area; then the packaging box is scanned by laser ultrasonic detection technology, and then the scanning result is imaged in real time by imaging technology, and the imaging result is observed to locate the defect position of the packaging box; then a repair agent is configured to repair the defect position. The present invention can quickly locate the defect position of the inner skin of the packaging box, and then take subsequent repair measures to create a complete inner skin for the inside of the packaging box, solve the leakage problem of the packaging box, and reduce the repair cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of composite materials, and in particular to a method for solving the airtightness problem and repairing defects of a large composite material structure packaging box product with airtightness requirements. Background Art

[0002] At present, large composite packaging boxes are mostly made through VARI molding process, which can realize the storage, packaging, transportation, etc. of the products in the packaging box. However, since the composite packaging box is a sandwich structure ("inner skin + sandwich material + outer skin"), the internal structure is complex. Due to many uncertain factors in the molding process (human operation error, resin introduction, etc.), the sealing effect of the packaging box after molding is poor, which affects the functional performance of the products in the packaging box. Therefore, a method is urgently needed to make the packaging box have good sealing performance to meet the use requirements.

[0003] At present, the leak detection of large composite packaging boxes mostly adopts the traditional method of manually applying leak detection liquid. First, fill the packaging box with 15kPa-20kPa dry gas, then use a brush to dip the leak detection liquid and brush the outer surface of the packaging box, observe the position of the bubbles on the outer surface of the packaging box to determine the leak position of the packaging box, and improve the airtightness of the packaging box by repairing the outer surface of the packaging box. This method has the disadvantages of low detection efficiency, long detection time, and large human resource investment. In addition, since the packaging box is internally pressurized, if the inner skin defects of the packaging box are not solved, the leakage problem of the packaging box cannot be fundamentally solved.

[0004] Due to the large size of composite packaging boxes, if manual leak detection is used to locate the defective position, the workload is large and the positioning efficiency is low. Therefore, there is an urgent need for a method to quickly locate the defective position of the inner skin of the packaging box and repair it so that the packaging box has a complete inner skin, fundamentally solving the airtightness problem of the packaging box. Summary of the invention

[0005] The purpose of the present invention is to provide a defect repair method for a large composite material packaging box, which can quickly locate the defect position of the inner skin of the packaging box, and then take subsequent repair measures to create a complete inner skin inside the packaging box, solve the air leakage problem of the packaging box, and reduce the repair cost.

[0006] To achieve the above object, the present invention adopts the following technical solutions:

[0007] A defect repair method for a large composite material packaging box comprises the following steps:

[0008] 1) Defect location: For large composite packaging boxes to be repaired, obtain their historical maintenance data in advance, divide the scanning area according to the leakage probability, set the area with a leakage probability of more than 10% as the must-scan area, and divide the remaining area into the spot-scan area; then use laser ultrasonic detection technology to scan the packaging box, perform 100% scanning on the must-scan area, and perform random scanning on the spot-scan area. Then use imaging technology to perform real-time imaging of the scanning results, observe the imaging results, and locate the defect position of the packaging box;

[0009] 2) Pretreatment of defect location: Drill a hole at the defect location according to the size of the defect. The hole is a repair hole, and then the repair hole location and the surrounding area are cleaned with a cleaning agent;

[0010] 3) Preparation of repair agent: Cut the fiber fabric of the same material as the packaging box into pieces, and then mix it with the adhesive to prepare the repair agent;

[0011] 4) Repair and solidify defective parts: Fill the repairing hole with the repairing agent fully, and make sure that the repairing agent that is higher than the plane completely covers the repairing hole. Use a vacuum compaction device to vacuum and compact the repairing agent, so that the repairing agent is tightly connected to the packaging box body, and then solidify it;

[0012] 5) Grinding of defective parts: After the repair agent is completely cured, remove the vacuum compaction device and grind the repaired parts with sandpaper of different coarseness and fineness until the repaired parts are smooth and flat with the packaging box body;

[0013] 6) Re-test the defective part: Re-test the repaired part using the test method of step 1) to determine whether the defective position is repaired completely. If it is repaired completely, proceed to the next step. If there is a defect, return to step 2) to continue processing;

[0014] 7) Spraying the repaired area: Prepare paint of the same color as the packaging box body, and spray the repaired area after the repair is completed.

[0015] Preferably, the types of defects are divided into crack defects and pore defects; for crack defects, V-shaped holes are punched; for pore defects, conical holes are punched.

[0016] Preferably, the diameter of the repair hole is 5 mm to 10 mm larger than the defect size.

[0017] Preferably, the cleaning agent is acetone.

[0018] Preferably, the fiber fabric is cut into small squares of 5 mm×5 mm; and the volume ratio of the adhesive to the fiber fabric is 3:1.

[0019] Preferably, a foot knife or other sharp tools are used to fill the repair agent into the repair hole.

[0020] Preferably, the vacuum compacting device uses a vacuum bag, and the method of vacuuming and compacting is: attaching the cut demoulding cloth and the vacuum bag to the repair agent in sequence, connecting the guide tube, connecting the guide tube to the vacuum pump, and turning on the vacuum pump for vacuuming and compacting.

[0021] Preferably, the scanning area is gradiently divided according to the probability of defect occurrence, and is divided into a first-level scanning area, a second-level scanning area, and a third-level scanning area according to the probability of defect occurrence from large to small. The first-level scanning area is scanned first. If no defects are scanned, the next-level scanning area is scanned, and so on.

[0022] The technical effects achieved by the present invention are as follows:

[0023] The size of a large glass composite material packaging box is very large. If the entire interior of the packaging box is scanned, it is difficult to quickly locate the defect position, and the scanning result data will increase significantly, the computer processing speed will slow down, and resources will be wasted. The innovation of the present invention lies in calling up historical repair data and dividing the scanning area into a must-scan area and a spot-scan area according to the leakage probability. Specifically, the position where the leakage probability exceeds 10% is set as the must-scan area, and the other positions are set as the spot-scan area, wherein the must-scan area is scanned 100%, and the spot-scan area is scanned randomly, which can significantly improve the positioning speed and reduce the scanning data, significantly reduce the scanning time and the data processing time of modeling and imaging, improve the processing speed, and reduce the processing cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 The present invention is a defect repair flow chart of a large composite material packaging box according to an embodiment of the present invention.

[0025] Figures 2 to 4 It is a schematic diagram of a specific repair process of an embodiment of the present invention. DETAILED DESCRIPTION

[0026] In order to make the above features and advantages of the present invention more obvious and easy to understand, embodiments are given below and described in detail with reference to the accompanying drawings.

[0027] This embodiment specifically discloses a defect repair method for a large composite material packaging box, and the process is as follows: Figure 1 As shown, the specific steps include:

[0028] 1) Defect location: In the inner cavity of a large glass fiber composite packaging box, an ultrasonic probe is used to scan the packaging box skin using laser ultrasonic detection technology. Based on the scanning results, the inner skin of the packaging box is imaged using the ultrasonic attenuation principle, and the defect position of the inner skin of the packaging box is quickly located based on the imaging results. Due to the large size of the product, if the entire interior of the product is scanned, the scanning result data will increase, the computer processing speed will slow down, and resources will be wasted. Therefore, the scanning area of ​​the entire packaging box is divided into a must-scan area and a spot-scan area to reduce the scanning data. Based on the previous experience summary of the product leakage parts, that is, the historical maintenance data, the positions where the leakage probability exceeds 10% are set as must-scan areas, and other positions are set as spot-scan areas. The must-scan areas are scanned 100%, and the spot-scan areas are scanned randomly. Since the packaging boxes adopt the same process, the laying of glass fiber cloth, the ratio of resin, the arrangement of guide tubes, the vacuum pump vacuum pressure (-01Mpa ~ -0.08Mpa), the molding environment temperature (25℃ + 2℃) and other conditions are basically consistent, so the historical maintenance data is reliable for determining the must-sweep area. More than 90% of the locations where defects exist in the packaging boxes are concentrated in the must-sweep area. For the case where the defects are not in the scanning area, the entire inner skin is divided into a must-sweep area and a sweeping area, in which the sweeping area is gradiently divided according to the probability of the defect location according to experience, 5%-10% for the first-level sweeping, 1%-5% for the second-level sweeping, 0%-1% for the third-level sweeping, and the first-level sweeping area is scanned first. If the defect location cannot be detected in the scanned area, the unscanned part of the next level in the sweeping area is scanned again to find the defect, so that the defects that are not in the scanning area can be scanned, and this gradient division can save a lot of scanning area and scanning time.

[0029] 2) Pretreatment of defect position: Drill holes according to the size of the pore defect at the defect position. The types of defects are divided into crack defects and pore defects (see Figure 2 For crack defects, V-shaped holes are used; for pore defects, conical holes are used (see Figure 3 ), which is convenient for subsequent repairs. The maximum hole diameter must be 5mm-10mm larger than the defect size, the drill bit diameter is 3mm, and the hole depth is 30mm-40mm. After drilling, clean it with a vacuum cleaner first, and then clean it with acetone or other cleaning agents.

[0030] 3) Preparation of repair agent: The repair agent is mainly composed of 914A / B adhesive and glass fiber cloth. First, cut the glass fiber cloth into small cubes of about 5mm×5mm for use, mix the 914A / B adhesive in a ratio of 2:1, and finally mix the glass fiber small cubes and the adhesive thoroughly. The volume ratio of adhesive to glass fiber is 3:1.

[0031] 4) Repair and solidify the defective position: fill the prepared repair agent into the hole to be repaired, use a foot knife or other sharp tools to force the repair agent into the repair hole until the repair agent completely fills the repair hole (see Figure 4 ). Cut the vacuum bag mold and demoulding cloth to an area slightly larger than the area of ​​the tapered hole, stick a circle of sealing tape around the filler 10mm, stick the cut demoulding cloth and vacuum bag on the repair agent in turn, connect the guide tube, connect the guide tube to the vacuum pump, turn on the vacuum pump to vacuum and compact, and cure at room temperature (20℃-30℃) for at least 6 hours.

[0032] 5) Grinding of defective parts: After the repair agent is completely cured, remove the vacuum compaction device (release cloth and vacuum bag stickers). Use sandpaper of different coarseness and fineness to grind the repaired part until the repaired part is smooth and flat with the packaging box body.

[0033] 6) Re-test the defective part: Use the test method of step 1) to re-test the repaired part to determine whether the defective position is repaired completely. If the repair is complete, proceed to the next step. If there is a defect, return to step 2) to continue processing.

[0034] 7) Spraying the repaired area: Prepare paint of the same color as the packaging box body, and spray the repaired area after the repair is completed.

[0035] Compared with the traditional repair method, the repair method proposed by the present invention has the following advantages:

[0036] The traditional modification method requires 3 people to repair a single large composite material packaging box, and the average repair time is about 4 hours (2 hours to find defects and 2 hours to repair). Moreover, it can only be repaired in series, and the total repair time consumed to repair 100 defects is usually about 400 hours. However, the repair method of the present invention requires 3 people to repair a single packaging box, and the average repair time is about 3 hours (1 hour to find defects and 2 hours to repair). Parallel repair can be performed, and the total repair time consumed to repair 100 defects is about 201 hours, which improves the efficiency by 49.75%.

[0037] The above is only a specific embodiment of the present invention and does not limit the present invention in any form. Any simple modification or equivalent change made to the above embodiment based on the design method of the invention is still within the protection scope of the technical solution of the present invention.

Claims

1. A defect repair method for a large composite material packaging box, characterized in that: The following steps are involved: 1) Defect location: For large composite packaging boxes to be repaired, obtain their historical maintenance data in advance, divide the scanning area according to the leakage probability, set the area with a leakage probability of more than 10% as the must-scan area, and divide the remaining area into the spot-scan area; then use laser ultrasonic detection technology to scan the packaging box, perform 100% scanning on the must-scan area, and perform random scanning on the spot-scan area. Then use imaging technology to perform real-time imaging of the scanning results, observe the imaging results, and locate the defect position of the packaging box; 2) Pretreatment of defect location: Drill a hole at the defect location according to the size of the defect. The hole is a repair hole, and then the repair hole location and the surrounding area are cleaned with a cleaning agent; 3) Preparation of repair agent: Cut the fiber fabric of the same material as the packaging box into pieces, and then mix it with the adhesive to prepare the repair agent; 4) Repair and solidify defective parts: Fill the repairing hole with the repairing agent fully, and make sure that the repairing agent that is higher than the plane completely covers the repairing hole. Use a vacuum compaction device to vacuum and compact the repairing agent, so that the repairing agent is tightly connected to the packaging box body, and then solidify it; 5) Grinding of defective parts: After the repair agent is completely cured, remove the vacuum compaction device and grind the repaired parts with sandpaper of different coarseness and fineness until the repaired parts are smooth and flat with the packaging box body; 6) Re-test the defective part: Use the test method of step 1) to re-test the repaired part to determine whether the defective position is repaired completely. If it is repaired completely, proceed to the next step. If there is a defect, return to step 2) to continue processing; 7) Spraying the repaired area: Prepare paint of the same color as the packaging box body, and spray the repaired area after the repair is completed.

2. The method according to claim 1, characterized in that The types of defects are divided into crack defects and pore defects; for crack defects, V-shaped holes are punched; for pore defects, conical holes are punched.

3. The method according to claim 1, characterized in that The diameter of the repair hole is 5 mm to 10 mm larger than the defect size.

4. The method according to claim 1, characterized in that The cleaning agent is acetone.

5. The method according to claim 1, characterized in that The fiber fabric is cut into small squares of 5 mm×5 mm; the volume ratio of the adhesive to the fiber fabric is 3:

1.

6. The method according to claim 1, characterized in that Use a foot knife to fill the repair agent into the repair hole.

7. The method according to claim 1, characterized in that The vacuum compaction device uses a vacuum bag, and the vacuum compaction method is: the cut demoulding cloth and the vacuum bag are attached to the repair agent in sequence, and the guide tube is connected, the guide tube is connected to the vacuum pump, and the vacuum pump is turned on for vacuum compaction.

8. The method according to claim 1, characterized in that The scanning area is gradiently divided according to the probability of defect occurrence, and is divided into a primary scanning area, a secondary scanning area, and a tertiary scanning area according to the probability of defect occurrence from large to small. The primary scanning area is scanned first. If no defects are scanned, the next level scanning area is scanned, and so on.

Citation Information

Patent Citations

  • Method for repairing surface bubbles and glue shortage defects of resin-reinforced carbon fiber composite material

    CN109454905A

  • Structure and function integrated composite material product repairing method

    CN114055814A

  • Increasing and decreasing composite intelligent repairing method for metal parts of medical apparatus and instruments

    CN114511604A

  • Method for repairing damaged part

    JP2007237322A

  • KR20200048599A