A method for laying electric heating sheet on quadratic surface
By using a combined technology of polyimide film and high-strength carbon fiber cloth resin glue on the electric heating sheet, the sliding problem of the electric heating sheet on the complex curved skin is solved, and an efficient and smooth paving effect is achieved. The reliability of the anti-icing function is ensured.
Patent Information
- Application Number
- CN202111459719.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-02
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2041-12-02
AI Technical Summary
Electric heating sheets are prone to slippage and deformation during the laying process on complex curved skins, which affects the uniformity of heating and the reliability of the anti-icing function.
The finished polyimide film electric heating piece is expanded into a shape through a molding mold and laid on the matrix prepreg. It is combined with high-strength carbon fiber cloth and resin glue. The resin glue is penetrated into the gap between the electric heating pieces through a heating device. The composite is then cured to prevent slippage.
It realizes the smooth laying of electric heating sheets on the secondary curved surface, improves the laying efficiency and prevents slipping, ensuring the firm bonding and surface accuracy of the electric heating sheets.
Smart Images

Figure CN116061459B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a technique for laying an electric heating sheet, and in particular to a method for laying an electric heating sheet on a quadratic surface. Background Art
[0002] Because ice will form on the wings, rotors, air inlets and other parts of helicopters and fixed-wing aircraft during flight, thus affecting the aerodynamic shape and flight safety, anti-icing measures need to be taken in these parts to ensure flight quality. The electric heating anti-icing method requires the electric heating plate to be integrated into the skin of the parts prone to ice formation, so that the electric heating plate can be powered on during flight to increase the temperature of the skin in the parts prone to ice formation, thereby melting the ice on the skin surface. However, the electric heating plate is relatively thin, has poor rigidity, and is easy to deform. The skin in the parts prone to ice formation is mostly complex curved surfaces. In the process of applying the electric heating plate to the skin, slippage, creases, and even cracks are very likely to occur, affecting the uniformity of heating and the reliability of the anti-icing function. Therefore, an efficient and reliable laying method is urgently needed for the integration of the electric heating plate and the complex curved skin.
[0003] Patent No. CN202010915340.2 discloses a method for preparing an electric heating anti-icing coating that can be used for three-dimensional quadratic surfaces. However, the device has a defect that when the intermediate heating layer material with conductive properties is coated on the quadratic surface, slippage is prone to occur. Summary of the invention
[0004] In order to solve the defects of the prior art mentioned above, the present invention proposes a method for laying an electric heating plate on a quadratic curved surface.
[0005] The technical solution of the present invention is achieved in this way:
[0006] A method for laying an electric heating sheet on a quadratic surface, characterized in that it comprises the following steps:
[0007] The first step is to prepare the molding mold of the product, obtain the quadratic surface of the product, and arrange the electric heating plate on the quadratic surface as needed;
[0008] The second step is to extract the arrangement shape of the electric heating plate on the quadratic surface;
[0009] The third step is to unfold the arrangement shape of the electric heating plate on the curved surface into a plane;
[0010] The fourth step is to manufacture the finished product of the polyimide film electric heating sheet according to the unfolded shape of the electric heating sheet;
[0011] The fifth step is to lay the finished polyimide film electric heating sheet on the base prepreg;
[0012] Step 6: tear off the polyimide film, leaving the electric heating sheet on the base prepreg;
[0013] Step 7: Laying the composite material on the electric heating sheet, and after the laying is completed, curing the composite material;
[0014] In the eighth step, the electric heating plate and the composite material are laid on the quadratic surface.
[0015] In the method for laying the electric heating sheet on a quadratic curved surface of the present invention, the polyimide film electric heating sheet finished product is manufactured by bonding the electric heating sheet with a polyimide film.
[0016] In the method for laying the electric heating plate on a quadratic curved surface of the present invention, the matrix prepreg is formed by impregnating a high-strength carbon fiber cloth reinforcement into a resin adhesive, and the resin adhesive is a bismaleimide resin adhesive and an epoxy resin adhesive.
[0017] In the method for laying an electric heating plate on a quadratic surface of the present invention, before the fifth step, a matrix prepreg is laid on the quadratic surface of the molding die.
[0018] In the method of laying the electric heating plate on the quadratic surface of the present invention, before the seventh step, the electric heating plate is uniformly heated by a heating device so that the resin in the matrix prepreg can penetrate into the gaps of the electric heating plate.
[0019] In the method of laying the electric heating plate on the quadratic curved surface of the present invention, the heating device is any one of resistance heating, induction heating, arc heating, electron beam heating, infrared heating, and dielectric heating.
[0020] In the method of laying the electric heating plate on the quadratic curved surface of the present invention, the composite material is the skin material for the wings, rotors, air inlets and other parts, and is made of at least one of high-strength aluminum, magnesium alloy, titanium alloy and the like.
[0021] In the method for laying the electric heating plate on a quadratic surface of the present invention, the mass of the resin glue in the matrix prepreg accounts for 36%-42% of the total mass of the matrix prepreg.
[0022] The method of laying the electric heating plate on the quadratic surface of the present invention has the following beneficial effects: the method of laying the electric heating plate on the quadratic surface not only achieves the flatness of the laying of the electric heating plate and improves the laying efficiency, but also prevents slippage. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 The process flow chart of laying the electric heating plate on the quadratic surface of the present invention;
[0024] Figure 2 It is a schematic diagram of the arrangement of electric heating plates on a quadratic surface;
[0025] Figure 3 for Figure 2 Schematic diagram of the expansion of the Zhongdian heating sheet;
[0026] Figure 4 This is a schematic diagram of laying a polyimide film electric heating sheet;
[0027] Figure 5 Schematic diagram of polyimide film electric heating sheet laid on base prepreg;
[0028] Figure 6 Schematic diagram of tearing off the polyimide film. DETAILED DESCRIPTION
[0029] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the accompanying drawings in the embodiments of the present invention.
[0030] like Figures 1 to 6 As shown, the method of laying the electric heating sheet on the quadratic surface of the present invention is used to lay the electric heating sheet on the quadratic surface so that the electric heating sheet is laid evenly on the quadratic surface. The method includes the following steps:
[0031] The first step is to prepare a molding mold 5 of the product, obtain a quadratic surface 1 of the product, and arrange electric heating plates 42 on the quadratic surface 1 as needed.
[0032] The second step is to extract the arrangement shape of the electric heating plate 42 on the quadratic surface 1, such as Figure 2 shown.
[0033] The third step is to unfold the arrangement shape of the electric heating plate 42 on the curved surface into a plane, such as Figure 3 shown.
[0034] In the fourth step, the finished product of the polyimide film electric heating sheet 4 is manufactured according to the unfolded shape of the electric heating sheet 42. The finished product of the polyimide film electric heating sheet 4 is manufactured by bonding the electric heating sheet 42 to the polyimide film 41. Since the electric heating sheet 42 is thin, has poor rigidity, and is easy to deform, the polyimide film 41 has a high tensile strength, so that the electric heating sheet 42 is not easy to deform in the next step, and the flatness of the electric heating sheet 42 is maintained.
[0035] In the fifth step, the matrix prepreg 6 is firstly laid on the quadratic surface 1 of the molding die 5, and then the finished polyimide film electric heating sheet 4 is laid on the matrix prepreg 6, such as Figure 4-5 shown.
[0036] It should be noted that the side of the polyimide film electric heating sheet 4 with the electric heating sheet 42 faces the base prepreg 6, and then the polyimide film electric heating sheet 4 is evenly attached to the base prepreg 6. The length of the electric heating sheet 42 is consistent with the base prepreg 6 in direction, the length of the electric heating sheet 42 is smaller than the length of the base prepreg 6, and the width of the electric heating sheet 42 is smaller than the width of the base prepreg 6, so that the electric heating sheet 42 is completely attached to the base prepreg 6, so that the electric heating sheet 42 is completely laid on the quadratic surface 1.
[0037] The matrix prepreg 6 is formed by impregnating high-strength carbon fiber cloth reinforcement into epoxy resin glue or bismaleimide resin glue. The mass of the resin glue in the matrix prepreg 6 accounts for 36%-42% of the total mass of the matrix prepreg 6.
[0038] When the resin glue is epoxy resin glue, the mass of epoxy resin glue in the matrix prepreg 6 accounts for 38%±2% of the total mass of the matrix prepreg 6, and the thickness of the prepared matrix prepreg 6 is 0.2mm, and the surface density is 210g / m2; when the resin glue is bismaleimide resin glue, the mass of bismaleimide resin glue in the matrix prepreg 6 accounts for 40%±2% of the mass of the matrix prepreg 6, and the thickness of the prepared matrix prepreg 6 is 0.2mm, and the surface density is 210g / m2. By controlling the content of resin glue in the prepreg, the performance requirements of the final product can be effectively guaranteed.
[0039] The number of layers of the matrix prepreg 6 is 1 to 5. When the layer thickness is such, the bonding quality between the matrix prepreg 6 and the electric heating plate 42 can be ensured, local debonding can be further avoided, and the surface accuracy of the final product can be ensured.
[0040] Step 6: tear off the polyimide film 41, leaving the electric heating plate 42 on the base prepreg 6. Figure 6 shown.
[0041] The seventh step is to uniformly heat the electric heating plate 42 through a heating device so that the resin in the matrix prepreg 6 can penetrate into the gaps of the electric heating plate 42; then, the composite material is laid on the electric heating plate 42, and after the laying is completed, the composite material is cured.
[0042] Composite materials are used to make the skin materials of wings, rotors, air inlets and other parts, and are made of at least one of the following materials: high-strength aluminum, magnesium alloy, titanium alloy and the like.
[0043] The heating device is any one of resistance heating, induction heating, arc heating, electron beam heating, infrared heating, and dielectric heating. Due to the high adhesion of the resin in the matrix prepreg liquid, the electric heating plate 42 and the matrix prepreg 6 can be basically laid and bonded by heating before curing.
[0044] The curing treatment is a heat treatment method, which includes any one of resistance heating, induction heating, arc heating, electron beam heating, infrared heating, etc.
[0045] In the eighth step, the electric heating plate 42 and the composite material are laid on the quadratic surface 1 .
[0046] The present invention realizes the smooth laying of the electric heating plate 42 and the composite material on the quadratic surface 1, thereby improving the laying efficiency; in addition, due to the high viscosity of the matrix prepreg 6 in the electric heating plate 42, it can be firmly bonded to the quadratic surface 1, preventing the electric heating plate 42 from slipping.
[0047] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for laying an electric heating sheet on a quadratic surface, characterized in that: The steps include: The first step is to prepare the molding mold of the product, obtain the quadratic surface of the product, and arrange the electric heating plate on the quadratic surface as needed; The second step is to extract the arrangement shape of the electric heating plate on the quadratic surface; The third step is to unfold the arrangement shape of the electric heating plate on the curved surface into a plane; The fourth step is to manufacture the finished product of the polyimide film electric heating sheet according to the unfolded shape of the electric heating sheet; The fifth step is to lay the finished polyimide film electric heating sheet on the base prepreg; Step 6: tear off the polyimide film, leaving the electric heating sheet on the base prepreg; Step 7: Laying the composite material on the electric heating sheet, and after the laying is completed, curing the composite material; Step 8: The electric heating sheet and the composite material are laid on the quadratic surface; Before the fifth step, a matrix prepreg is laid on the quadratic surface of the molding die. Before the seventh step, the electric heating sheet is uniformly heated by a heating device so that the resin in the matrix prepreg can penetrate into the gap of the electric heating sheet. The heating device is any one of resistance heating, induction heating, arc heating, electron beam heating, infrared heating, and dielectric heating. The matrix prepreg is formed by impregnating a high-strength carbon fiber cloth reinforcement into a resin adhesive, wherein the resin adhesive is a bismaleimide resin adhesive or an epoxy resin adhesive. The composite material is a skin material for making wings, rotors, and air inlet parts, and is made of at least one of high-strength aluminum, magnesium alloy, and titanium alloy.
2. The method for laying an electric heating sheet on a quadratic surface according to claim 1, characterized in that: The polyimide film electric heating sheet finished product is manufactured by bonding the polyimide film to the electric heating sheet.
3. The method for laying an electric heating sheet on a quadratic surface according to claim 1, characterized in that: The mass of the resin glue in the matrix prepreg accounts for 36%-42% of the total mass of the matrix prepreg.