High temperature resistant fire retardant coating and preparation method thereof

By heating and stirring raw materials in the stirring barrel, rolling out the material flat, adding and mixing additives to it, the preparation of paint is achieved by rotating the double arc plate, and the problems of low uniformity and efficiency in the preparation of existing fire-retardant coatings are solved, and the problems of low uniformity and efficiency in the preparation of existing fire-retardant coatings are improved. The preparation efficiency and performance of the coating are achieved.

CN116239907BActive Publication Date: 2024-11-12ZHOUSHAN TENGYU AEROSPACE NEW MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310321284.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-03-29
Publication Date
2024-11-12
Estimated Expiration
2043-03-29

AI Technical Summary

Technical Problem

Existing fire-retardant coatings cannot achieve uniform flat laying and rapid reactions during the additive reaction process, resulting in low preparation efficiency.

Method used

Multi-step method is adopted: first heat and stir the raw materials in the mixing barrel, push the materials to be laid flat, then evenly add the mixed additives to the laying material, and mix thoroughly through the rotation of the double arc plate, and finally collect and prepare high-temperature fire-resistant coatings .

Benefits of technology

The uniform reaction between additives and raw materials is achieved, the preparation efficiency and performance of the coating is improved, and the rapid uniformity of the coating and high-temperature fire resistance are ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116239907B_ABST
    Figure CN116239907B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of coatings, and more specifically, to a high-temperature resistant fireproof coating and a preparation method thereof. The method comprises the following steps: Step 1: heating a plurality of raw materials in a stirring barrel and fully stirring them; Step 2: pushing the stirred materials out and spreading them flat; Step 3: uniformly adding the mixed additives to the spread materials; Step 4: fully heating the materials in Step 3; Step 5: fully mixing the raw materials and additives by rotating a double arc plate to achieve the preparation of the high-temperature resistant fireproof coating and then collecting them. The plurality of raw materials in Step 1 are composed of three or more raw materials selected from chromium carbide, shell powder, titanium dioxide, expanded vermiculite and fireproof short fibers, deionized water and flame-retardant amino resin. The additives and raw materials can be fully spread flat, which is convenient for the rapid reaction of the additives and raw materials.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of coatings, and more particularly to a high temperature resistant fire retardant coating and a preparation method thereof. Background Art

[0002] Building fire protection is an important field of fire science and technology, and fire-retardant coatings are an important part of fire-resistant building materials. Fire-retardant coatings are a type of coating applied to the surface of objects to prevent fires, stop the spread of fires, isolate fire sources, prolong the ignition time of the substrate, or increase insulation performance to delay structural damage. However, the fire-retardant coatings currently prepared cannot evenly spread the additives and other raw materials during the reaction process of the additives, and react quickly and evenly to obtain the coating. Summary of the invention

[0003] In order to overcome the deficiencies of the prior art, the present invention provides a high temperature resistant fire retardant coating and a preparation method thereof, which can fully spread additives and raw materials and facilitate rapid reaction of the additives and raw materials.

[0004] The technical solution adopted by the present invention to solve its technical problem is:

[0005] A method for preparing a high temperature resistant fire retardant coating, the method comprising the following steps:

[0006] Step 1: Heat the various raw materials in a mixing barrel and stir them thoroughly;

[0007] Step 2: Push the stirred material out and spread it flat;

[0008] Step 3: Evenly add the mixed additives to the flat material;

[0009] Step 4: fully heating the material in step 3;

[0010] Step 5: The raw materials and additives are fully mixed by rotating the double arc plates to prepare the high temperature resistant fire retardant coating and then collected.

[0011] Furthermore, the multiple raw materials in step one are composed of three or more raw materials selected from chromium carbide, shell powder, titanium dioxide, expanded vermiculite and fire-resistant short fibers, deionized water and flame-retardant amino resin.

[0012] Furthermore, the additives in step three are composed of five or more additives selected from the group consisting of a wetting agent, an antioxidant, a film former, a regulator, a defoaming agent, a dispersant, a flame retardant and a thickener.

[0013] Furthermore, the double arc plate is rotatably connected in the flat frame, the flat frame is rotatably connected with a gear ring, an upper plate is fixedly connected to the gear ring, a plurality of atomization tubes are fixedly connected to the upper plate, a mixing frame is fixedly connected to the plurality of atomization tubes, the double arc plate is rotatably connected to the upper plate, and a mixing rack for mixing additives is fixedly connected to the double arc plate. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] The present invention is further described in detail below with reference to the accompanying drawings and specific implementation methods.

[0015] Figure 1 A flow chart of a method for preparing a coating;

[0016] Figure 2 A diagram of raw materials for preparing coatings;

[0017] Figure 3 It is a structural diagram of mixed raw materials;

[0018] Figure 4 for Figure 3 A partial enlarged view of the structure shown;

[0019] Figure 5 It is the heating structure diagram;

[0020] Figure 6 This is the insulation structure diagram;

[0021] Figure 7 A structural diagram for tiling raw materials;

[0022] Figure 8 It is the structural diagram of the mixed additive;

[0023] Fig. 9 It is the structural diagram of the transmission;

[0024] Fig.10 A structural diagram for adding atomizing additives;

[0025] Fig.11 Structural diagram to facilitate material transportation;

[0026] Fig.12 Structural diagram for preparing coating.

[0027] The paving frame 11; the pushing pipe 12; the feeding pipe 13; the heat preservation frame 14; the speed change wheel 21; the sealing pipe 22; the bracket 31; the mixing barrel 32; the gathering pipe 33; the end plate 34; the middle pipe 41; the spiral plate 42; the supply frame 43; the connecting frame 51; the vortex pipe 52; the double arc plate 61; the mixing frame 62; the mixing wheel 63; the gear ring 71; the upper plate 72; the atomizing pipe 73; the mixing frame 74; the side wheel 81; the pushing frame 82. DETAILED DESCRIPTION

[0028] refer to Figure 1, detailed description of the method for preparing high temperature resistant fire retardant coating:

[0029] A method for preparing a high temperature resistant fire retardant coating, the method comprising the following steps:

[0030] Step 1: Heat the various raw materials in the stirring barrel 32 and stir them fully. Heating can increase the activity of the raw material molecules, and stirring can achieve sufficient mixing to perform preliminary preparation of the high temperature resistant fire retardant coating;

[0031] Step 2: Push the stirred material out and spread it flat to achieve the dispersion of the high temperature resistant fire retardant coating, which is convenient for subsequent modification and processing;

[0032] Step 3: uniformly adding the mixed additives into the flattened material, and changing the performance of the preliminarily prepared high temperature resistant fire retardant coating through the additives;

[0033] Step 4: fully heating the material in step 3 to ensure that the additives react fully and achieve the modification of the performance of the preliminarily prepared high temperature resistant fire retardant coating;

[0034] Step 5: The double arc plate 61 is rotated to fully mix the raw materials and additives to prepare the high temperature resistant fire retardant coating and then collect it.

[0035] refer to Figure 2 , detailed description of the raw material composition for the preliminary preparation of high temperature resistant fire retardant coating:

[0036] The multiple raw materials in step one are composed of three or more of chromium carbide, shell powder, titanium dioxide, expanded vermiculite and fire-resistant short fibers, deionized water and flame-retardant amino resin. Deionized water and flame-retardant amino resin are the main components of high-temperature resistant fire-resistant coatings, while chromium carbide, shell powder, titanium dioxide, expanded vermiculite and fire-resistant short fibers have high-temperature resistant and fire-resistant properties, and can be used to prepare high-temperature resistant and fire-resistant coatings.

[0037] refer to Figure 2 , detail the preparation ingredients of the additive:

[0038] The additives in step three are composed of five or more additives selected from the group consisting of wetting agent, antioxidant, film former, regulator, defoamer, dispersant, flame retardant and thickener. The antioxidant can prevent the prepared coating from fading due to oxidation and ensure the color of the coating. The defoamer can prevent a large number of bubbles in the coating, making the coating bubble-free and having a smooth surface after application. The flame retardant can prevent the coating from burning, thereby processing a high-temperature resistant and fire-retardant coating.

[0039] refer to Figure 3 , 4 , 7 and 12, detailing the implementation process of tiling raw material mixing:

[0040] The double arc plate 61 is rotatably connected in the paving frame 11, and a plurality of slots are processed at intervals on the double arc plate 61. When the double arc plate 61 rotates, it can push the preliminarily prepared high-temperature resistant fire-retardant coating and additives to be spread flat, and with the rotation of the double arc plate 61, the preparation of the high-temperature resistant fire-retardant coating is achieved. A gear ring 71 is rotatably connected to the paving frame 11, and an upper plate 72 is fixedly connected to the gear ring 71. A plurality of atomizing tubes 73 are fixedly connected to the upper plate 72, and a mixing frame 74 is fixedly connected to the plurality of atomizing tubes 73. The double arc plate 61 is rotatably connected to the upper plate 72, and a mixing frame 62 for mixing additives is fixedly connected to the double arc plate 61. Additives are added into the mixing frame 74, and when the mixing frame 62 rotates, the additives added into the mixing frame 74 are fully mixed. Mixing to achieve preliminary mixing of additives, and the mixed additives flow out from multiple atomizing tubes 73, and multiple atomizing tubes 73 are fixedly connected with atomizers, which can atomize the mixed additives through the atomizer, and then add them from multiple atomizing tubes 73 into the preliminarily prepared high-temperature resistant fire-retardant coating on the paving frame 11, and then the additives and other raw materials are fully mixed by rotating the double arc plate 61 to achieve the preparation of high-temperature resistant fire-retardant coating, the ring gear 71 can rotate around its own axis, the ring gear 71 drives the upper plate 72 to rotate, and the upper plate 72 drives the multiple atomizing tubes 73 to rotate, so that the atomized additives are added at different positions on the paving frame 11, so that the additives are added more evenly, thereby accelerating the rapid preparation of high-temperature resistant fire-retardant coating.

[0041] refer to Figure 3 and 12 , detailing the implementation process of raw material processing into coatings:

[0042] The tiling frame 11 is fixedly connected with a bracket 31, and a stirring barrel 32 is fixedly connected with the bracket 31. The stirring barrel 32 is mainly used for stirring and heating raw materials. A gathering pipe 33 is fixedly connected with the stirring barrel 32, and the gathering pipe 33 discharges the stirred raw materials. The gathering pipe 33 is rotatably connected with a sealing pipe 22, and the sealing pipe 22 is rotatably connected with a discharge pipe 13. The discharge pipe 13 is fixedly connected to the push pipe 12, and the push pipe 12 is fixedly connected to the tiling frame 11. The raw materials flowing out of the gathering pipe 33 flow through the sealing pipe 22 at the lower end and then flow into the discharge pipe 13, and then flow into the push pipe 12, and then are pushed into the tiling frame 11, and then the atomized additives are evenly added and rotated and mixed by the double arc plate 61 to realize the preparation of high temperature resistant fire retardant coating.

[0043] refer to Figure 3 , 4 , 5, 7 and 9, detail the implementation process of heating raw materials and power transmission:

[0044] The mixing barrel 32 is fixedly connected to an end plate 34, to which a middle tube 41 is rotatably connected, the middle tube 41 is fixedly connected to an output shaft of a reduction motor I, the reduction motor I is fixedly connected to the end plate 34, the middle tube 41 is connected and communicated with an externally arranged heating device, and a heat flow is provided to the middle tube 41 through the externally arranged heating device to heat the raw materials, the middle tube 41 is fixedly connected to a sealed tube 22, a speed change wheel 21 is fixedly connected to the sealed tube 22, a mixing wheel 63 is fixedly connected to a mixing frame 62, the speed change wheel 21 and the mixing wheel 63 are meshed for transmission, the reduction motor I is started, the reduction motor I drives the middle tube 41 to rotate, the middle tube 41 drives the sealed tube 22 to rotate, the sealed tube 22 drives the speed change wheel 21 to rotate, the speed change wheel 21 meshes and drives the mixing wheel 63 to rotate, the mixing wheel 63 drives the mixing frame 62 and the double arc plate 61 to rotate, so as to achieve mixing of additives and paving and mixing of the mixed additives and the stirred raw materials, thereby achieving preparation of high temperature resistant fire retardant coating.

[0045] refer to Fig.12 , detailing the implementation process of heating and mixing raw materials:

[0046] Two spiral plates 42 are fixedly connected to the middle tube 41. Both spiral plates 42 are provided with cavities. The two spiral plates 42 are connected to the middle tube 41. When the middle tube 41 rotates, the two spiral plates 42 are driven to rotate, thereby achieving stirring of the raw materials. The heat flow in the middle tube 41 flows into the two spiral plates 42, and the raw materials are heated while being stirred, thereby achieving rapid mixing of the raw materials.

[0047] refer to Figure 5 and 12 , detailing the implementation process of heating additives and raw materials:

[0048] The middle tube 41 is fixedly connected with a supply rack 43, the supply rack 43 is rotatably connected to a connecting frame 51, the connecting frame 51 is fixedly connected with a vortex tube 52, the tiling frame 11 is fixedly connected with an insulation frame 14, the vortex tube 52 is fixedly connected to the insulation frame 14, the heat flow in the middle tube 41 flows into the supply rack 43, and then flows into the vortex tube 52 to heat the lower end of the tiling frame 11, the tiling frame 11 is evenly heated to accelerate the reaction of the additive and the raw material, the insulation frame 14 can keep the heat warm to prevent heat loss.

[0049] refer to Fig.10 , details the implementation process of uniformly adding atomized additives:

[0050] The pushing tube 12 is rotatably connected with a pushing rack 82, which is fixedly connected to the output shaft of the reduction motor II. The reduction motor II is fixedly connected to the pushing tube 12. When the reduction motor II is started, the reduction motor II drives the pushing rack 82 to rotate. The pushing rack 82 is spiral-shaped, and the rotation pushes the raw materials to flow, thereby realizing the transportation of the raw materials. The paving frame 11 is rotatably connected with a side wheel 81, and the side wheel 81 and the ring gear 71 are engaged for transmission. The side wheel 81 is fixedly connected to the output shaft of the reduction motor III. The reduction motor III is fixedly connected to the paving frame 11. When the reduction motor III is started, the reduction motor III drives the side wheel 81 to rotate, and the side wheel 81 engages to drive the ring gear 71 to rotate, thereby realizing the rotation of multiple atomizing tubes 73 and realizing the uniform addition of atomized additives.

[0051] The high-temperature resistant fireproof coating is composed of the following components in weight proportion: 180-250 parts of flame-retardant amino resin; 15-25 parts of chromium carbide; 14-18 parts of shell powder; 16-21 parts of titanium dioxide; 15-18 parts of expanded vermiculite; 10-15 parts of fireproof short fibers; 6-15 parts of wetting agent; 10-16 parts of antioxidant; 4-6 parts of film-forming agent; 6-12 parts of regulator; 15-18 parts of defoaming agent; 4-8 parts of dispersant; 11-13 parts of flame retardant; 5-8 parts of thickener; and 120-130 parts of deionized water.

Claims

1. A method for preparing a high temperature resistant fire retardant coating, characterized in that: The method comprises the following steps: Step 1: heating the various raw materials in a mixing barrel (32) and fully mixing them; Step 2: Push the stirred material out and spread it flat; Step 3: Evenly add the mixed additives to the flat material; Step 4: fully heating the material in step 3; Step 5: The raw materials and additives are fully mixed by rotating the double arc plate (61) to prepare the high temperature resistant fireproof coating and then collect the mixture; the double arc plate (61) is rotatably connected to the paving frame (11), a gear ring (71) is rotatably connected to the paving frame (11), an upper plate (72) is fixedly connected to the gear ring (71), a plurality of atomizing tubes (73) are fixedly connected to the upper plate (72), a mixing frame (74) is fixedly connected to the plurality of atomizing tubes (73), and the double arc plate (61) is rotatably connected to the paving frame (11). 1) is rotatably connected to the upper plate (72), a mixing frame (62) for mixing additives is fixedly connected to the double arc plate (61), a bracket (31) is fixedly connected to the flattening frame (11), a mixing barrel (32) is fixedly connected to the bracket (31), a gathering pipe (33) is fixedly connected to the mixing barrel (32), a sealing pipe (22) is rotatably connected to the gathering pipe (33), a feeding pipe (13) is rotatably connected to the sealing pipe (22), and the feeding pipe (13) is fixedly connected to the pushing pipe ( The material pushing tube (12) is fixedly connected to the flattening frame (11), the mixing barrel (32) is fixedly connected to an end plate (34), a middle tube (41) is rotatably connected to the end plate (34), the middle tube (41) is fixedly connected to a sealing tube (22), a speed change wheel (21) is fixedly connected to the sealing tube (22), a mixing wheel (63) driven by the speed change wheel (21) is fixedly connected to the mixing frame (62), and two mixing wheels (63) connected to the middle tube (41) are fixedly connected to the middle tube (41). The spiral plate (42) is fixedly connected to a supply rack (43) on the middle tube (41), the supply rack (43) is rotatably connected to a connecting frame (51), a vortex tube (52) is fixedly connected to the connecting frame (51), an insulation frame (14) covering the vortex tube (52) is fixedly connected to the flattening frame (11), a pusher rack (82) is rotatably connected to the pusher tube (12), and a side wheel (81) for driving the gear ring (71) to rotate is rotatably connected to the flattening frame (11).

2. The method for preparing a high temperature resistant fire retardant coating according to claim 1, characterized in that: The multiple raw materials in step 1 are composed of three or more raw materials selected from chromium carbide, shell powder, titanium dioxide, expanded vermiculite and fireproof short fibers, deionized water and flame-retardant amino resin.

3. The method for preparing a high temperature resistant fire retardant coating according to claim 1, characterized in that: The additives in step three are composed of five or more additives selected from the group consisting of a wetting agent, an antioxidant, a film former, a regulator, a defoaming agent, a dispersant, a flame retardant and a thickener.

4. The high temperature resistant fire retardant coating prepared by the high temperature resistant fire retardant coating preparation method according to claim 1, characterized in that: The high-temperature resistant fireproof coating is composed of the following components in weight proportion: 180-250 parts of flame-retardant amino resin; 15-25 parts of chromium carbide; 14-18 parts of shell powder; 16-21 parts of titanium dioxide; 15-18 parts of expanded vermiculite; 10-15 parts of fireproof short fibers; 6-15 parts of wetting agent; 10-16 parts of antioxidant; 4-6 parts of film-forming agent; 6-12 parts of regulator; 15-18 parts of defoaming agent; 4-8 parts of dispersant; 11-13 parts of flame retardant; 5-8 parts of thickener; and 120-130 parts of deionized water.