Welding wire, photovoltaic module welding method using the welding wire, and photovoltaic module
By using the welding wire of low-temperature and high-temperature alloy welding layer as the main gate in photovoltaic modules, combined with screen printing and lamination processes, the problem of copper wire shifting during the preparation of photovoltaic modules is solved, and copper wire and thinness are realized The stable fixation and conduction of the gate improve the preparation stability of the component.
Patent Information
- Application Number
- CN202310340459.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2043-03-31
AI Technical Summary
During the preparation of photovoltaic modules, when using copper wire as the main gate, it is prone to shifting and squirming, resulting in the inability to effectively fix and combine with the fine gate.
We use welding wires including low-temperature alloy solder layer and high-temperature alloy solder layer as the main gate, and fine grids and pads are made by screen printing, and the high-temperature alloy solder layer and pads are connected to fix the copper wire at high temperature, and then in the lamination process Under heating and pressurization, the low-temperature alloy solder layer melts, realizing the conduction between the copper wire and the fine gate.
It effectively solves the problem of copper wire shift during lamination, ensures the fixation and conduction of copper wire and fine gate, and improves the preparation stability and safety of photovoltaic modules.
Smart Images

Figure CN116329807B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of photovoltaic module preparation, and in particular to a welding wire, a photovoltaic module welding method using the welding wire, and a photovoltaic module. Background Art
[0002] Crystalline silicon photovoltaic cells (whether single-sided or double-sided, there is a grid line design) absorb incident light through the cell, generate a charge separation layer through the PN junction set on the surface, and collect current through the fine grid silver wires set on the surface shunt layer. One type of charge is collected on the front side and another reverse charge is collected on the back side, which are then collected and exported through the main grid silver wires.
[0003] At present, the conventional method is to make the fine grid and the main grid respectively by screen printing with silver paste. Usually, there are dozens to hundreds of fine grids, with a width of about 30 to 60 microns; usually, there are 3 to 12 main grid lines, with a width of 500 to 2000 microns; the main grid is set perpendicular to the direction of the fine grid and forms a conductive contact with the intersection of the fine grid.
[0004] However, the cost of silver paste is relatively high, and copper wire can be used as an alternative to the main grid. The position of the main grid needs to be fixed during the manufacturing process. Bus bars formed by hot melt adhesive can be set on the sides of the main grid and the fine grid for fixation. However, using this process, during the component manufacturing process, the main grid in the hot melt adhesive area is fixed, but the main grid in the middle part will shift and move, so that the main grid and the fine grid cannot be fixed well. Summary of the invention
[0005] In order to overcome the above technical defects, the purpose of the present invention is to provide a welding wire, a photovoltaic module welding method using the welding wire and a photovoltaic module, so as to solve the problem of deviation between the copper wire and the fine grid during the preparation process of the existing solar cell using the copper wire as the main grid.
[0006] The invention discloses a welding wire, comprising a copper wire; a first alloy welding layer is arranged on the copper wire, the melting point of the first alloy welding layer is 100-170°C; a second alloy welding layer with a gap is arranged outside the first alloy welding layer, the melting point of the second alloy welding layer is 180-350°C.
[0007] The invention discloses a photovoltaic element welding method, comprising:
[0008] Fine grids are made by screen printing on the battery cells, and several welding wires are used as main grids;
[0009] A plurality of welding pads are prepared on the battery cell, so that each welding wire passes through the corresponding welding pad and is placed vertically with the fine grid;
[0010] Heating the second alloy welding layer to melt and connect with the welding pad, so as to fix each welding wire on the battery cell;
[0011] After the series welding, the first alloy welding layer is melted by heating and pressurizing in a lamination process, so that the copper wire is connected to the fine grid to form a battery assembly.
[0012] Preferably, at 150-170° C., the first alloy layer is melted and pressurized to contact the fine grid, so that the copper wire is conductively connected to the fine grid.
[0013] Preferably, the first alloy solder layer is a solder alloy layer.
[0014] Preferably, the second alloy solder layer includes a tin-silver alloy solder layer or a lead-tin alloy solder layer.
[0015] Preferably, the pads are evenly spaced in the length direction of the copper wire.
[0016] Preferably, the pad is disposed between two adjacent fine grids.
[0017] Preferably, the pad portion is disposed on the fine grid corresponding to a connection with the main grid.
[0018] Preferably, the inner diameter of the pad is 0.3-0.8 mm.
[0019] The present invention also provides a photovoltaic assembly, comprising a plurality of battery sheets, and the battery assembly is prepared by applying the welding method.
[0020] The invention also provides a welding wire device for executing the welding method.
[0021] Compared with the prior art, the above technical solution has the following beneficial effects:
[0022] The welding wire and photovoltaic module provided in the present application are characterized by screen-printing fine grids and welding pads on the battery cell, and forming the welding wire as the main grid by arranging a low-temperature alloy welding layer and a high-temperature alloy welding layer outside the copper wire. The high-temperature alloy layer and the welding pad are melted and connected at high temperature on the battery plate, so that after the copper wire and the battery cell are fixed, they are welded in series, and heating and pressurizing are performed in a lamination process to melt the low-temperature alloy welding layer, thereby achieving conduction between the copper wire and the fine grid, thereby solving the problem that the main grid and the fine grid are easily offset during lamination in the existing battery cell preparation process. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a flow chart of the welding wire of the present invention, a photovoltaic module welding method using the welding wire, and a photovoltaic module embodiment 1;
[0024] Figure 2 The welding wire of the present invention, the photovoltaic module welding method using the welding wire, and the schematic diagram of the solar panel structure in the photovoltaic module embodiment 1, 2 or 3;
[0025] Figure 3This is a schematic diagram of the welding wire of the present invention, a photovoltaic module welding method using the welding wire, and a welding pad structure in Embodiments 1, 2 or 3 of the photovoltaic module.
[0026] Reference numerals:
[0027] 1-battery cell; 2-copper wire; 21-first alloy welding layer; 22-second alloy welding layer; 3-welding pad; 4-fine grid. DETAILED DESCRIPTION
[0028] The advantages of the present invention are further described below in conjunction with the accompanying drawings and specific embodiments.
[0029] Exemplary embodiments will be described in detail herein, examples of which are shown in the accompanying drawings. When the following description refers to the drawings, the same numbers in different drawings represent the same or similar elements unless otherwise indicated. The embodiments described in the following exemplary embodiments do not represent all embodiments consistent with the present disclosure. Instead, they are merely examples of devices and methods consistent with some aspects of the present disclosure as detailed in the appended claims.
[0030] The terms used in this disclosure are for the purpose of describing specific embodiments only and are not intended to limit the disclosure. The singular forms of "a", "said" and "the" used in this disclosure and the appended claims are also intended to include plural forms unless the context clearly indicates otherwise. It should also be understood that the term "and / or" used herein refers to and includes any or all possible combinations of one or more associated listed items.
[0031] It should be understood that although the terms first, second, third, etc. may be used in the present disclosure to describe various information, such information should not be limited to these terms. These terms are only used to distinguish the same type of information from each other. Depending on the context, the word "if" as used herein can be interpreted as "at the time of" or "when" or "in response to determining".
[0032] In the description of the present invention, it is necessary to understand that the terms "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0033] In the description of the present invention, unless otherwise specified and limited, it should be noted that the terms "installed", "connected" and "connected" should be understood in a broad sense. For example, it can be a mechanical connection or an electrical connection, or it can be the internal connection between two components. It can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms can be understood according to the specific circumstances.
[0034] In the following description, the suffixes such as "module", "component" or "unit" used to represent elements are only used to facilitate the description of the present invention, and have no specific meanings. Therefore, "module" and "component" can be used interchangeably.
[0035] Embodiment 1: This embodiment discloses a welding method for a photovoltaic element, which is a battery cell. Specifically, the welding method is mainly used to solve the problem that in the preparation process of the existing battery cell assembly, copper wire is used as the main grid, and the copper wire is fixed in the hot melt adhesive area around the fine grid and the main grid, but the copper wire in the middle part will deviate and move, so that the copper wire and the fine grid cannot be fixed and combined well. Specifically, it includes:
[0036] S1: Screen printing is performed on the battery cell to produce a fine grid (S1-1), and a number of pre-prepared welding wires described in the following embodiment 3 are used as main grids;
[0037] Specifically, fine grids are made on both sides of the battery cell by screen printing silver paste. This step can be achieved by existing technical means. The fine grid is used to collect current on the surface of the battery panel, and the main grid described below is used to derive current. Specifically, after the fine grids are made on both sides of the above-mentioned battery cell, the main grid can also be set on the front and back of the battery cell accordingly. The number of fine grids is 80 to 160, and the number of welding wires used as the main grid is 15 to 50, where the copper wire diameter is 0.05 to 0.3 mm. It should be noted that in the subsequent process, the main grid needs to be fixed on the battery cell through the welding pad by melting the high-temperature layer outside the copper wire. However, high-temperature melting will melt the high-temperature alloy welding layer (i.e., the second alloy welding layer described below) of the part where the welding pad is connected to it, and will not affect the arrangement of the fine grid and the subsequent connection with the copper wire.
[0038] In the above steps, the welding wire includes a copper wire; a first alloy welding layer is provided on the copper wire, and the melting point of the first alloy welding layer is 100-170°C; a second alloy welding layer with a gap is provided outside the first alloy welding layer, and the melting point of the second alloy welding layer is 180-350°C, that is, the specific preparation process of the above main grid includes: a plurality of copper wires (S1-2):
[0039] S11: preparing a first alloy welding layer on the copper wire, wherein the melting point of the first alloy welding layer is 100-170° C.;
[0040] Specifically, the first alloy solder layer is a solder alloy layer, which is tin or an alloy thereof with one or more of lead, bismuth, and silver. The first alloy solder layer adopts a low-temperature soldering process, i.e., the above-mentioned 100-170°C, preferably an alloy solder layer that can be melted at a temperature of 150°C. The use of this solder alloy layer reduces the melting point and reduces the cost at the same time. It should be noted that, whether it is the above-mentioned first alloy solder layer or the second alloy solder layer in the following S400, the preparation process sprays the first alloy solder layer / second alloy solder layer outside the copper wire / first alloy solder layer, so its preparation temperature is higher than the melting point of the corresponding alloy solder layer.
[0041] S12: preparing a second alloy welding layer with a gap outside the first alloy welding layer on the copper wire, wherein the melting point of the second alloy welding layer is 180-350° C.;
[0042] Specifically, the second alloy solder layer includes but is not limited to a tin-silver alloy solder layer, a lead-tin alloy solder layer, etc. The second alloy is different from the first alloy in that the melting point of the second alloy is higher than that of the first alloy, that is, the melting point of the second alloy is higher than that of the solder layer outside the copper wire, and the alloy solder layer with a melting point of 230°C is preferred. It should be noted that the second alloy solder layer has a gap, that is, the first alloy solder layer is partially exposed, so that it can be melted at low temperature under lamination during the following preparation process to make the copper wire and the fine grid conductive. If the second alloy solder layer completely wraps the first alloy solder layer, the subsequent melting of the first alloy solder layer at low temperature cannot be achieved, and it can be arranged so that the connection between the copper wire and the fine grid is located within the gap.
[0043] Furthermore, the second alloy welding layer is set to be a high-temperature alloy welding layer. Considering that the second alloy welding layer is used to connect with the welding pad on the battery cell described below, so that the copper wire is fixed on the battery cell, the copper wire is fixed to the welding pad after high-temperature melting, and then can be melted at a low temperature in the lamination process to make the copper wire and the fine grid conductive. Since the temperature is controlled to be lower than the melting point of the second alloy welding layer during lamination, the fixation of the copper wire and the battery cell will not be affected in this process, so that the copper wire is fixed to the battery cell when the battery cell is laminated and will not be offset.
[0044] As an illustration, the preparation of the first alloy welding layer and the second alloy welding layer on the copper wire serving as the main grid in the above steps S110 and S120 can be completed in advance, independent of the above steps S100-S200, that is, the pretreatment of the copper wire, and the copper wire coated with the first alloy welding layer and the second alloy welding layer can be directly obtained for use during the preparation process.
[0045] S2: A plurality of welding pads are prepared on the battery cell, so that each welding wire (i.e., copper wire) passes through the corresponding welding pad and is placed vertically on the fine grid;
[0046] In this embodiment, the above-mentioned pad is prepared by screen printing, and the pad can be prepared at the same time as the above-mentioned fine grid is prepared. It can be various shapes such as glue drop shape, round or square, and the inner diameter of the pad is 0.3~0.8mm, so that the pad exceeds the main grid line diameter, so that the main grid is fixed on the pad to achieve positioning, reducing the offset of the middle area of the main grid during the lamination process, and at the same time, it can be fixed on its side by hot melt adhesive, or it can be directly set and fixed by the pad.
[0047] Specifically, the welding pad corresponds to the copper wire arrangement, and the copper wire (main grid) is arranged perpendicular to the fine grid, and the welding pad is arranged perpendicular to the direction of the fine grid. Preferably, the above-mentioned welding pads are evenly spaced in the length direction of the copper wire. Specifically, 8 to 10 welding pads can be arranged corresponding to one copper wire. The evenly spaced distribution can make the stress at the connection point between each welding pad and the main grid uniform after the main grid (copper wire) is fixed by the welding pad, thereby improving the positioning stability of the main grid and thereby increasing the safety of the battery cell preparation process.
[0048] It should also be noted that the above-mentioned second alloy welding layer and the welding pad are distributed in correspondence, including but not limited to position correspondence, shape correspondence and size correspondence. Specifically, since the second alloy welding layer needs to be connected and fixed to each welding pad, the second alloy welding layer is arranged on the side of the copper wire facing the solar panel. The second alloy welding layer can be set to be similar in size and shape to the connection part of the welding pad, that is, a number of spaced block welding layers are formed on the copper wire, or it can be set to be circumferentially coated around the copper wire, that is, a number of spaced annular ring welding layers are formed on the copper wire, which does not affect the subsequent connection between the first alloy welding layer and the fine grid. The specific welding layer position, size and shape can be set according to the welding pad, actual preparation equipment or needs.
[0049] S3: heating to melt the second alloy welding layer and connect it to the welding pad, and fixing each welding wire (i.e., copper wire) on the battery cell;
[0050] In the above steps, the heating is high-temperature heating, and the heating temperature needs to exceed the melting point of the second alloy, that is, the second alloy is melted and contacts the pad. A certain pressure / thrust can be applied, or the gravity of the main grid itself is used to fix the two through the melted second alloy welding layer, thereby reducing the movement of the copper wire relative to the battery panel during the subsequent lamination process. As mentioned above, since the temperature fixed to the pad is higher than the temperature in the subsequent lamination process, the stability of the connection between the main grid and the pad will be maintained during the lamination process.
[0051] Based on the above, the pad is arranged between the cell and the main grid, and is used to position the main grid on the cell through the second alloy. The fine grid is also distributed on the cell board, and the main grid is vertically placed on the fine grid. Therefore, the position of the pad may overlap with the position of the fine grid, but the distribution of the fine grid does not substantially affect the positioning of the pad. Specifically, in an optional embodiment, the pad can be respectively located between two adjacent fine grids, that is, the fine grid and the pad do not interfere with each other. In another optional embodiment, the pad is partially placed on the fine grid corresponding to the connection with the main grid. At this time, the pad is prepared with conductive silver paste, and the second alloy welding layer also has a certain conductivity, so it will not affect the conduction between the wire and the fine grid during the subsequent lamination process.
[0052] S4: After multiple battery cells are welded in series, the first alloy welding layer is melted by heating and pressurizing under a lamination process, so that the copper wire is connected to the fine grid to form a battery assembly.
[0053] Specifically, heating and pressurizing can be regarded as a lamination process. In the above steps, at 150-170°C, the first alloy layer is melted and pressurized to contact the fine grid, so that the copper wire and the fine grid are connected. In this embodiment, it should be noted that the subsequent preparation process of the battery cell is consistent with the existing one, including but not limited to welding, stacking, lamination, EL testing, framing, junction box installation, clearing, IV testing, finished product inspection, packaging, etc. Here, multiple battery cells are welded in series, which can be achieved by a string welding machine. First, the excess part of the front copper wire of one of the two adjacent battery cells is bent in a Z shape to be welded together with the copper wire of the other piece (or if a bus bar is formed by fixing the copper wire circumferentially with hot melt adhesive, the bus bar is used here instead). After multiple battery cells are welded in series, a battery assembly is formed. Then, the first alloy layer is melted during lamination to weld the copper wire and the fine grid to achieve single-sided production on the battery cell. If fine grids and main grids are provided on both sides, the preparation of the entire battery cell can be achieved. The copper wire of the battery cell prepared by the above steps can be positioned through the outer second alloy welding layer and a plurality of welding pads distributed on the battery cell, thereby reducing the deviation and movement of the copper wire located in the middle of the battery cell during the lamination process.
[0054] Embodiment 2: The present invention also provides a photovoltaic module, including a plurality of cells, and the battery module is prepared by the welding method described in embodiment 1. A plurality of battery modules can be produced in batches by using a string welding machine and a laminating device, and the specific number and distribution of the string welding cells can be set according to the actual use scenario. The battery module prepared by the above embodiment 1, for any cell therein, the cell is provided with mutually perpendicular fine grids and main grids (copper wires / welding wires), and a plurality of uniformly / unevenly spaced welding pads are also distributed, and a first alloy welding layer and a second alloy welding layer are sequentially arranged outside the copper wire, the first alloy welding layer is a low-temperature alloy welding layer, and the second alloy welding layer is a high-temperature alloy welding layer, and the second alloy welding layer is connected to the welding pad by high temperature, so that the copper wire is fixed on the cell, and each cell is laminated after being string welded, so that the copper wire is connected to the fine grid after the first alloy welding layer is heated and pressurized, and the heating temperature at this time will not exceed the melting point of the second alloy welding layer, and will not affect the fixation of the copper wire to the cell panel, so that the copper wire will not be offset after pressure is applied during the lamination process.
[0055] Embodiment 3: The present invention also provides a welding wire, such as Figure 3 , including a copper wire; a first alloy welding layer is provided on the copper wire, and the melting point of the first alloy welding layer is 100-170°C; a second alloy welding layer with a gap is provided outside the first alloy welding layer, and the melting point of the second alloy welding layer is 180-350°C, which is applied to the welding method of the photovoltaic element in the first embodiment as a main grid, and the photovoltaic module in the above-mentioned second embodiment is prepared by the welding method in the first embodiment. It can be prepared in advance so as to be applied to step S10 in the first embodiment, and the preparation process includes: preparing a first alloy welding layer on the copper wire, and the melting point of the first alloy welding layer is 100-170°C; preparing a second alloy welding layer with a gap outside the first alloy welding layer on the copper wire, and the melting point of the second alloy welding layer is 180-350°C. The welding wire is provided with a low-temperature alloy welding layer and a high-temperature alloy welding layer outside the copper wire, which are used to be fixed after melting with the high-temperature alloy through the welding pad, so that the welding wire can be fixed on the solar panel as a main grid, and is connected with the fine grid through the melting of the low-temperature alloy welding layer during subsequent lamination. It is different from the existing main grid prepared by silver paste printing, which effectively reduces the cost. At the same time, when used as a main grid, the provision of the second alloy welding layer can also reduce the movement relative to the fine grid during the preparation of photovoltaic modules.
[0056] It should be noted that the embodiments of the present invention have better practicability and do not impose any form of limitation on the present invention. Any technician familiar with the field may use the technical content disclosed above to change or modify it into an equivalent effective embodiment. However, any modification or equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.
Claims
1. A welding wire, characterized in that: Used to connect with battery cells and fine grids: Including copper wire; The copper wire is provided with a first alloy welding layer; A second alloy welding layer with a gap is provided outside the first alloy welding layer; The melting point of the second alloy is higher than that of the first alloy, the melting point of the first alloy welding layer is 100-170° C., and the melting point of the second alloy welding layer is 180-350° C.; The copper wire is used to be fixed to the battery cell by melting the second alloy welding layer, and then to be connected to the fine grid by melting the first alloy welding layer.
2. A photovoltaic module welding method, characterized in that: The welding wire according to claim 1 comprises: Screen printing is used to make fine grids on the battery sheet, and a number of the welding wires are used as main grids; A plurality of welding pads are prepared on the battery cell, so that each welding wire passes through the corresponding welding pad and is placed vertically with the fine grid; Heating the second alloy welding layer to melt and connect with the welding pad, so as to fix each welding wire on the battery cell; After string welding, the first alloy welding layer is melted by heating and pressurizing under a lamination process, so that the copper wire and the fine grid are connected to form a battery assembly, wherein the temperature for heating and melting the second alloy welding layer is higher than the melting point of the second alloy, and the temperature for heating and melting the first alloy welding layer is lower than the melting point of the second alloy.
3. The welding method according to claim 2, characterized in that: At 150-170° C., the first alloy layer melts and is pressed to contact the fine grid, so that the copper wire is connected to the fine grid.
4. The welding method according to claim 2, characterized in that: The first alloy solder layer is a solder alloy layer.
5. The welding method according to claim 2, characterized in that: The second alloy solder layer includes a tin-silver alloy solder layer and a lead-tin alloy solder layer.
6. The welding method according to claim 2, characterized in that: The pads are evenly spaced in the length direction of the copper wire.
7. The welding method according to claim 2, characterized in that: The pad is arranged between two adjacent fine grids.
8. The welding method according to claim 2, characterized in that: The pad portion is disposed on the fine grid corresponding to a connection with the main grid.
9. The welding method according to claim 2, characterized in that: The inner diameter of the pad is 0.3-0.8 mm.
10. A photovoltaic module, characterized in that: The battery assembly comprises a plurality of battery cells and is prepared by using the welding method described in any one of claims 2 to 9.