A SiC MOSFET, its fabrication method and integrated circuit
By using a finned field-effect transistor structure and an internally integrated Schottky barrier diode, the problems of low channel mobility and poor gate oxide reliability in SiC MOSFETs have been solved, achieving device performance with high conduction characteristics and high reliability.
Patent Information
- Application Number
- CN202210206634.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-02
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2042-03-02
AI Technical Summary
Existing SiC MOSFETs have low channel mobility and poor gate oxide reliability, resulting in insufficient device conduction characteristics and reliability.
By adopting a finned field-effect transistor structure, the gate electrode is placed on both sides of the finned channel layer. Combined with the internal integration of the floating region and the Schottky barrier diode, the fabrication process of the gate oxide layer is optimized.
It significantly improves channel mobility and gate oxide reliability, enhances device conduction and reverse conduction characteristics, and avoids bipolar degradation effects.
Smart Images

Figure CN116741825B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of semiconductor technology, and in particular to a SiC MOSFET, its fabrication method, and integrated circuit. Background Technology
[0002] Silicon carbide (SiC), as a new generation of wide-bandgap semiconductor material, exhibits extremely superior performance in the field of power semiconductors, representing the forefront and future direction of power semiconductor device development. Compared to gallium arsenide and silicon, SiC possesses overwhelmingly superior properties in high voltage and high temperature environments. SiC is a compound semiconductor material composed of silicon (Si) and carbon (C), possessing numerous excellent characteristics such as a large bandgap, high breakdown field strength, high thermal conductivity, high saturation velocity, and high maximum operating temperature. These properties enable SiC electronic devices to operate in high-voltage, high-heat-generating, and high-frequency environments. Metal-oxide-semiconductor field-effect transistors (MOSFETs) fabricated using SiC, compared to insulated-gate bipolar transistors (IGBTs) made from Si, offer smaller size, lower power consumption, and superior thermal conductivity at the same power output.
[0003] The fabrication of the gate oxide layer is a crucial step in the production of SiC MOSFETs. Currently, a common method is to directly thermally oxidize the SiC epitaxial wafer at high temperatures to form a silicon dioxide gate oxide layer on its surface. However, numerous interface states exist at the SiC / SiO2 interface (such as dangling bonds between Si and C, C-related defects, and near-interface oxide defects). These interface traps bind carriers in the inversion layer, leading to a decrease in device current density. Simultaneously, the bound carriers cause Coulomb scattering of free carriers in the channel, reducing channel mobility and lowering the device's conduction characteristics. Although subsequent nitriding of the interface after oxidation can improve channel mobility, the channel mobility remains significantly lower than that of the silicon carbide bulk material. Summary of the Invention
[0004] This application provides a SiC MOSFET, its fabrication method, and an integrated circuit for improving the channel mobility of SiC MOSFETs.
[0005] In a first aspect, this application provides a SiC MOSFET, which may include: a SiC semiconductor substrate, a drift layer, a fin channel layer (i.e., a well region), a source region, a gate electrode, a gate oxide layer, a first insulating isolation layer, a second insulating isolation layer, a source electrode, and a drain electrode. The drift layer is located on the SiC semiconductor substrate, the fin channel layer is located on the drift layer, the source region is located on the fin channel layer, and the first insulating isolation layer is located on the portion of the drift layer not covered by the fin channel layer. The fin channel layer and the source region form a stacked structure. The gate electrode is located on the first insulating isolation layer and on both sides of the stacked structure. The gate oxide layer is located between the gate electrode and the stacked structure. The second insulating isolation layer covers the outer wall and upper surface of the gate electrode. The source electrode covers the first insulating isolation layer, the second insulating isolation layer, and the source region. The drain electrode is located on the side of the SiC semiconductor substrate away from the drift layer. The first insulating isolation layer is used to isolate the gate electrode and the drift layer, the gate oxide layer is used to isolate the gate electrode and the fin channel layer and to isolate the gate electrode and the source region, and the second insulating isolation layer is used to isolate the gate electrode and the source electrode.
[0006] In this application, the finned channel layer refers to a channel layer with a strip shape and gate electrodes located on both sides of the finned channel layer. Thus, the SiC MOSFET is a Fin Field-Effect Transistor (Fin FET). Placing the gate electrodes on both sides of the finned channel layer helps to reduce the width of the finned channel layer (i.e., the distance between the two gate oxide layers on both sides of the finned channel layer), which is beneficial for global inversion of the finned channel layer. This results in the formation of a larger carrier channel in the finned channel layer, so that most of the carriers in the SiC MOSFET will travel through the electron channels formed by the finned channel layer. This reduces the number of carriers traveling at the edge of the gate oxide layer, thereby significantly improving the channel mobility and the reliability of the gate oxide layer.
[0007] The SiC MOSFET provided in this application can be either an N-type MOSFET or a P-type MOSFET, and is not limited thereto. When the SiC MOSFET is an N-type MOSFET, the SiC semiconductor substrate can be an N++ region, used as the drain region; the drift layer can be an N+ region, mainly used to carry high voltage; the source region can be an N++ region; and the fin channel layer can be a P region, i.e., a P-well. A P-well refers to an N-type semiconductor layer doped with a concentration sufficient to neutralize the N-type semiconductor layer and make it exhibit P-type characteristics. When the SiC MOSFET is a P-type MOSFET, the SiC semiconductor substrate can be a P++ region, used as the drain region; the drift layer can be a P+ region, mainly used to carry high voltage; the source region can be a P++ region; and the fin channel layer can be an N region, i.e., an N-well. An N-well refers to a P-type semiconductor layer doped with a concentration sufficient to neutralize the P-type semiconductor layer and make it exhibit N-type characteristics. In specific implementations, since the hole mobility is lower than the electron mobility, the SiC MOSFET is generally an N-type MOSFET, and is not limited thereto.
[0008] In practical implementation, semiconductors contain two types of charge carriers: holes in the valence band and electrons in the conduction band. Semiconductors where electrons are the primary conductors are called N-type semiconductors, and those where holes are the primary conductors are called P-type semiconductors. It should be explicitly stated that in this application, layers and regions prefixed with N or P represent electrons or holes as the majority carriers, respectively. Furthermore, a "+" sign on N or P indicates a higher doping concentration than layers or regions without a "+" sign, and the more "+" signs, the higher the doping concentration. N or P regions containing the same number of "+" signs represent similar doping concentrations, but are not limited to having the same doping concentration.
[0009] In this application, the N-type semiconductor region is mainly doped with N-type impurities, such as phosphorus (P) or nitrogen (N), while the P-type semiconductor region is mainly doped with P-type impurities, such as aluminum (Al), boron (B), gallium (Ga) or beryllium (Be).
[0010] For example, a SiC MOSFET may also include floating regions located in the drift layer and on both sides of the fin channel layer. This can weaken the electric field strength below the gate oxide layer, protect the gate oxide layer, and significantly improve the gate reliability of the device.
[0011] In practical implementation, when the SiC MOSFET is an N-type MOSFET, the floating region is a P-type semiconductor region; when the SiC MOSFET is a P-type MOSFET, the floating region is an N-type semiconductor region. The doping concentration of the floating region is generally lower than that of the fin channel layer.
[0012] Furthermore, to achieve anti-parallel connection of the freewheeling diodes inside the device, the SiC MOSFET may also include: grooves located on both sides of the fin channel layer and penetrating the first insulating isolation layer and part of the floating region; the grooves are filled with ohmic contacts. The source electrode is electrically connected to the floating region through the ohmic contacts.
[0013] In this application, the ohmic contact portion can be formed using any material capable of forming an ohmic contact with the floating region, and no limitation is made herein.
[0014] In this application, to avoid bipolar degradation in the SiC MOSFET, a Schottky barrier diode is integrated inside the SiC MOSFET to improve its reverse conduction and switching characteristics. For example, in this SiC MOSFET, at least two spaced floating regions are provided on both sides of the fin channel layer; the SiC MOSFET may also include grooves located on both sides of the fin channel layer, penetrating the first insulating isolation layer and part of the drift layer, with the grooves situated between adjacent floating regions; and Schottky contacts filling the grooves.
[0015] In practice, the Schottky contacts can be formed from any material capable of forming Schottky contacts with the drift layer, and there is no limitation herein. For example, the Schottky contacts can be formed from an alloy, and there is no limitation herein.
[0016] In specific implementation, the material of the gate electrode in this application can be polycrystalline silicon or other materials with good conductivity, such as metals, and is not limited here.
[0017] Secondly, this application provides a method for fabricating a SiC MOSFET, which may include: epitaxially forming a drift layer on a SiC semiconductor substrate; forming a fin channel layer and a source region on the fin channel layer; using the fin channel layer and the source region as a stacked structure, thermally oxidizing the sidewalls of the stacked structure to form gate oxide layers; thermally oxidizing the exposed surface of the drift layer to form a first insulating isolation layer; forming a gate electrode on the side of each gate oxide layer away from the stacked structure; depositing a second insulating isolation layer covering the outer sidewall and upper surface of the gate electrode; depositing a source electrode covering the first insulating isolation layer, the second insulating isolation layer, and the source region; and depositing a drain electrode on the side of the SiC semiconductor substrate away from the drift layer.
[0018] Optionally, to avoid oxidation of the source region's upper surface during gate oxide formation, in this application, forming a finned channel layer and a source region on the drift layer can include: epitaxially growing a channel layer on the drift layer; implanting ions into the region of the channel layer near the surface to form a source region; forming a nitride layer on the channel layer; etching the channel layer and the nitride layer to form the finned channel layer and the source region on the finned channel layer, while retaining the nitride layer on the source region. After depositing an isolation oxide layer covering the outer wall and upper surface of the gate electrode and the upper surface of the drift layer, it is also necessary to remove the nitride layer on the source region.
[0019] In one feasible implementation, before thermally oxidizing the two sidewalls of the stacked structure to form a gate oxide layer, the method further includes: accumulating an oxide protective layer covering the surface and sidewalls of the stacked structure; using the oxide protective layer as an ion implantation masking layer to implant ions in the drift layer to form floating regions on both sides of the fin channel layer; and removing the oxide protective layer.
[0020] Furthermore, after depositing a second insulating layer covering the outer wall and upper surface of the gate electrode, the process may further include: forming a groove penetrating the first insulating layer and a portion of the floating region; and filling the groove with an ohmic contact.
[0021] In another feasible implementation, before thermally oxidizing the sidewalls of the stacked structure to form the gate oxide layer, the method further includes: depositing an oxide protective layer covering the surface and sidewalls of the stacked structure; forming at least one photoresist material blocking portion on each of the drift layers on both sides of the oxide protective layer; using the oxide protective layer and the photoresist material blocking portion as ion implantation masking layers to implant ions in the drift layers, forming at least two floating regions on both sides of the fin channel layer; and then removing the oxide protective layer and the photoresist material blocking portion.
[0022] Furthermore, after depositing a second insulating layer covering the outer wall and upper surface of the gate electrode, the process may further include: forming a groove penetrating the first insulating layer and a portion of the drift layer at a location corresponding to the region between adjacent floating regions; and filling the groove with a Schottky contact portion.
[0023] Thirdly, this application also provides an integrated circuit including a circuit board and a SiC MOSFET disposed on the circuit board. The SiC MOSFET may be a SiC MOSFET as described in the first aspect or various embodiments of the first aspect, or a SiC MOSFET prepared as described in the second aspect or various embodiments of the second aspect.
[0024] The technical effects that can be achieved in the third aspect mentioned above can be described with reference to the technical effects that can be achieved by any possible design in the first aspect mentioned above, and will not be repeated here. Attached Figure Description
[0025] Figure 1 This is a schematic diagram of the structure of a SiC MOSFET provided in an embodiment of this application;
[0026] Figure 2 This is a schematic diagram of another SiC MOSFET structure provided in an embodiment of this application;
[0027] Figure 3 A schematic diagram of another SiC MOSFET provided in the embodiments of this application;
[0028] Figure 4 A schematic diagram of another SiC MOSFET provided in the embodiments of this application;
[0029] Figure 5 A schematic flowchart illustrating a method for fabricating a SiC MOSFET, provided in an embodiment of this application;
[0030] Figures 6a to 6j This is a schematic diagram of a process for fabricating a SiC MOSFET, provided in an embodiment of this application.
[0031] Figures 7a to 7j This is a schematic diagram of another process for fabricating SiC MOSFETs provided in an embodiment of this application;
[0032] Figures 8a to 8k This is a schematic diagram of another process for fabricating SiC MOSFETs provided in this application embodiment. Detailed Implementation
[0033] To make the objectives, technical solutions, and advantages of this application clearer, a further detailed description of this application will be provided below in conjunction with the accompanying drawings. However, the exemplary embodiments can be implemented in various forms and should not be construed as limited to the embodiments set forth herein; rather, these embodiments are provided to make this application more comprehensive and complete, and to fully convey the concept of the exemplary embodiments to those skilled in the art. The same reference numerals in the drawings denote the same or similar structures, and therefore repeated descriptions of them will be omitted. Terms describing position and direction as described in this application are illustrative based on the accompanying drawings, but changes may be made as needed, and all such changes are included within the scope of protection of this application. The accompanying drawings of this application are for illustrating relative positional relationships only and do not represent actual scale.
[0034] It should be noted that specific details are set forth in the following description to provide a full understanding of this application. However, this application can be implemented in many ways other than those described herein, and those skilled in the art can make similar extensions without departing from the spirit of this application. Therefore, this application is not limited to the specific embodiments disclosed below. The following descriptions are preferred embodiments for carrying out this application; however, these descriptions are for the purpose of illustrating the general principles of this application and are not intended to limit the scope of this application. The scope of protection of this application shall be determined by the appended claims.
[0035] To facilitate understanding of the SiC MOSFET provided in this application embodiment, its application scenarios will be introduced first below.
[0036] Compared to silicon (Si), silicon carbide (SiC) materials offer advantages such as a wider bandgap, higher critical breakdown electric field, higher thermal conductivity, and higher electron saturation drift velocity. These properties enable silicon carbide electronic devices to operate under high voltage, high heat generation, and high frequency conditions. MOSFETs made with SiC offer advantages over IGBTs made with Si, including smaller size, lower power consumption, and better thermal conductivity for the same power output. Therefore, they can be widely used in electric vehicles, charging stations, uninterruptible power supplies (UPS), and smart grids.
[0037] The fabrication of the gate oxide layer is a crucial step in the production of SiC MOSFETs. Currently, a common method is to directly thermally oxidize the SiC epitaxial wafer at high temperatures to form a silicon dioxide gate oxide layer on its surface. However, numerous interface states exist at the SiC / SiO2 interface (such as dangling bonds between Si and C, C-related defects, and near-interface oxide defects). These interface traps bind carriers in the inversion layer, leading to a decrease in device current density. Simultaneously, the bound carriers cause Coulomb scattering of free carriers in the channel, reducing channel mobility and lowering the device's conduction characteristics. Although subsequent nitriding of the interface after oxidation can improve channel mobility, the channel mobility remains significantly lower than that of the silicon carbide bulk material.
[0038] Based on this, the present application provides a SiC MOSFET and integrated circuit that can improve channel mobility, which will be described in detail below with reference to specific drawings and embodiments.
[0039] In practical implementation, semiconductors contain two types of charge carriers: holes in the valence band and electrons in the conduction band. Semiconductors where electrons are the primary conductors are called N-type semiconductors, and those where holes are the primary conductors are called P-type semiconductors. It should be explicitly stated that in this application, layers and regions prefixed with N or P represent electrons or holes as the majority carriers, respectively. Furthermore, a "+" sign on N or P indicates a higher doping concentration than layers or regions without a "+" sign, and the more "+" signs, the higher the doping concentration. N or P regions containing the same number of "+" signs represent similar doping concentrations, but are not limited to having the same doping concentration.
[0040] See Figure 1 , Figure 1 This illustration shows a schematic diagram of a SiC MOSFET provided in one embodiment of this application. A SiC MOSFET typically includes one or more well regions. Figure 1 The diagram illustrates a SiC MOSFET with two well regions as an example. Specifically, the SiC MOSFET may include: a SiC semiconductor substrate 10, a drift layer 11, a fin channel layer 12 (i.e., a well region), a source region 13, a gate electrode 14, a gate oxide layer 15, a first insulating isolation layer 16, a second insulating isolation layer 17, a source electrode 18, and a drain electrode 19. The drift layer 11 is located on the SiC semiconductor substrate 10, the fin channel layer 12 is located on the drift layer 11, the source region 13 is located on the fin channel layer 12, and the first insulating isolation layer 16 is located on the portion of the drift layer 11 not covered by the fin channel layer 12. The finned channel layer 12 and source region 13 form a stacked structure. The gate electrode 14 is located on the first insulating isolation layer 16 and on both sides of the stacked structure. The gate oxide layer 15 is located between the gate electrode 14 and the stacked structure. The second insulating isolation layer 17 covers the outer wall and upper surface of the gate electrode 14. The source electrode 18 covers the first insulating isolation layer 16, the second insulating isolation layer 17, and the source region 13. The drain electrode 19 is located on the side of the SiC semiconductor substrate 10 away from the drift layer 11. Thus, the first insulating isolation layer 16 is used to isolate the gate electrode from the drift layer 11, the gate oxide layer 15 is used to isolate the gate electrode 14 from the finned channel layer 12 and from the source region 13, and the second insulating isolation layer 17 is used to isolate the gate electrode 14 from the source electrode 18.
[0041] In this application, the fin channel layer 12 refers to a channel layer with a strip shape, and the gate electrode 14 is located on both sides of the fin channel layer 12, thus the SiC MOSFET is a Fin FET. Placing the gate electrode 14 on both sides of the fin channel layer 12 helps to reduce the width of the fin channel layer 12 (i.e., the distance between the two gate oxide layers on both sides of the fin channel layer 12), which is beneficial for global inversion of the fin channel layer 12, thereby forming a larger carrier channel in the fin channel layer 12. In this way, most of the carriers in the SiC MOSFET will travel through the electron channel formed by the fin channel layer 12, thereby reducing the number of carriers traveling at the edge of the gate oxide layer 15, which can significantly improve the channel mobility and also improve the reliability of the gate oxide layer 15.
[0042] The SiC MOSFET provided in this application embodiment can be either an N-type MOSFET or a P-type MOSFET, and is not limited thereto. When the SiC MOSFET is an N-type MOSFET, the SiC semiconductor substrate 10 can be an N++ region, used as the drain region; the drift layer 11 can be an N+ region, mainly used to carry high voltage; the source region 13 can be an N++ region; and the fin channel layer 12 can be a P region, i.e., a P-well. A P-well refers to a P-type impurity doped into an N-type semiconductor layer at a concentration sufficient to neutralize the N-type semiconductor layer and make it exhibit P-type characteristics. When the SiC MOSFET is a P-type MOSFET, the SiC semiconductor substrate 10 can be a P++ region, used as the drain region; the drift layer 11 can be a P+ region, mainly used to carry high voltage; the source region 13 can be a P++ region; and the fin channel layer 12 can be an N region, i.e., an N-well. An N-well refers to an N-type impurity doped into a P-type semiconductor layer at a concentration sufficient to neutralize the P-type semiconductor layer and make it exhibit N-type characteristics. In practical implementation, since the hole mobility is lower than the electron mobility, SiC MOSFETs are generally N-type MOSFETs, and this is not a limitation here.
[0043] It should be noted that the accompanying drawings in this application specification are all based on the example of an N-type SiC MOSFET. For the case of a P-type SiC MOSFET, the N-region in the N-type MOSFET can be replaced with the P-region, and the P-region in the N-type MOSFET can be replaced with the N-region.
[0044] In this application, the N-type semiconductor region is mainly doped with N-type impurities, such as phosphorus (P) or nitrogen (N), while the P-type semiconductor region is mainly doped with P-type impurities, such as aluminum (Al), boron (B), gallium (Ga) or beryllium (Be).
[0045] In practical applications, SiC MOSFETs have a high electric field in the drift region when in the blocking state. The curvature effect at the bottom of the fin channel layer 12 causes the electric field below the gate oxide layer 15 to be particularly concentrated. The long-term high electric field stress will cause the quality of the gate oxide layer 15 to degrade and the device to fail.
[0046] Therefore, for example, see Figure 2 , Figure 2 A schematic diagram of a SiC MOSFET provided in another embodiment of this application is shown. This SiC MOSFET may further include floating regions 20 located in the drift layer 11 and on both sides of the fin channel layer 12. This weakens the electric field strength below the gate oxide layer 15, protects the gate oxide layer 15, and significantly improves the gate reliability of the device.
[0047] In practical implementation, when the SiC MOSFET is an N-type MOSFET, the floating region 20 is a P-type semiconductor region; when the SiC MOSFET is a P-type MOSFET, the floating region 20 is an N-type semiconductor region. The doping concentration of the floating region 20 is generally less than the doping concentration of the fin channel layer 12.
[0048] Furthermore, to achieve anti-parallel connection of the freewheeling diodes inside the device, see [reference needed]. Figure 3 , Figure 3 This diagram illustrates the structure of a SiC MOSFET according to another embodiment of the present application. The SiC MOSFET may further include: grooves located on both sides of the fin channel layer 12 and penetrating the first insulating isolation layer 16 and a portion of the floating region 20; the grooves are filled with ohmic contacts 21. The source electrode 18 is electrically connected to the floating region 20 through the ohmic contacts 21.
[0049] In this application, the ohmic contact portion can be formed of any material capable of forming an ohmic contact with the floating region 20, and no limitation is made herein.
[0050] In practical implementation, bipolar degradation may occur in SiC MOSFETs. This effect is mainly triggered by pre-existing substrate dislocations on the SiC crystal. During bipolar operation, the energy released by the recombination of electrons and holes causes stacking faults to propagate at the substrate dislocations. These stacking faults propagate to the surface of the semiconductor material and then stop propagating. The area covered by the expanded stacking faults can no longer conduct electricity, thus shrinking the effective active region of the SiC MOSFET.
[0051] To avoid bipolar degradation in SiC MOSFETs, a Schottky barrier diode (SBD) can be connected in antiparallel for reverse freewheeling, thus preventing bipolar degradation. However, the externally connected SBD inevitably increases packaging cost and stray inductance, thereby degrading the device's switching characteristics.
[0052] Therefore, in this application, to avoid bipolar degradation in SiC MOSFETs, a Schottky barrier diode is integrated inside the SiC MOSFET to improve reverse conduction and switching characteristics. For example, see [link to example]. Figure 4 , Figure 4 A schematic diagram of a SiC MOSFET provided in another embodiment of this application is shown. In this SiC MOSFET, at least two spaced floating regions 20 are provided on both sides of the fin channel layer 12; the SiC MOSFET may also include grooves located on both sides of the fin channel layer 12 and penetrating the first insulating isolation layer 16 and part of the drift layer 11, and the grooves are located between adjacent floating regions 20; Schottky contacts 22 are filled in the grooves.
[0053] In specific implementations, the Schottky contact 22 can be formed of any material capable of forming a Schottky contact with the drift layer 11, and is not limited thereto. For example, the Schottky contact 22 can be formed of an alloy, and is not limited thereto.
[0054] In specific implementation, the material of the gate electrode in this application can be polycrystalline silicon or other materials with good conductivity, such as metals, and is not limited here.
[0055] For example, the gate electrode in a SiC MOSFET is typically formed using polysilicon.
[0056] It should be noted that the comparison of doping concentration between the two regions in this application refers only to the comparison of the concentration of impurities doped in the two regions, and the composition of the impurities is not limited. That is, the composition of the impurities can be the same or different; the substrate material used for doping the impurities is SiC.
[0057] In one embodiment, the drift layer 11, the finned channel layer 12, and the source region 13 can be formed by ion doping of epitaxially grown SiC material. The gate oxide layer 15 and the first insulating isolation layer 16 are formed by thermally oxidizing the SiC material to form SiO2. The material of the second insulating isolation layer 17 can be at least one of silicon oxide and silicon nitride.
[0058] See Figure 5 , Figure 5This is a schematic flowchart illustrating a method for fabricating a SiC MOSFET according to an embodiment of this application. The fabrication method may include the following steps:
[0059] Step S101, as follows Figure 6a As shown, a drift layer 11 is epitaxially formed on a SiC semiconductor substrate 10.
[0060] For example, the SiC semiconductor substrate 10 can be an N-type semiconductor. In a specific implementation, SiC can be epitaxially formed on the SiC semiconductor substrate first, and then N-type ions can be implanted into the SiC to form an offset layer.
[0061] Step S102: Form a fin-shaped channel layer and a source region located on the fin-shaped channel layer on the drift layer.
[0062] like Figure 6b As shown, a channel layer 12' can be epitaxially grown on the drift layer 11. For example, the channel layer 12' can be SiC doped with P-type ions.
[0063] like Figure 6c As shown, ion source regions 13 are implanted into the region near the surface of the channel layer 12'; for example, N-type ion source regions 13 can be implanted only into the region corresponding to the region where the fin channel layer will be formed.
[0064] like Figure 6d As shown, a nitride layer 31 is formed on the channel layer 12'. The function of the nitride layer 31 is to prevent the upper surface of the source region from being oxidized when the gate oxide layer is formed.
[0065] like Figure 6e As shown, the channel layer 12' and the nitride layer 31 are etched to form the fin-shaped channel layer 12 and the source region 13 located on the fin-shaped channel layer 12, while retaining the nitride layer 31 located on the source region 13.
[0066] Step S103, as follows Figure 6f As shown, the fin channel layer 12 and the source region 13 are used as a stacked structure, and the two sidewalls of the stacked structure are subjected to thermal oxidation treatment to form the gate oxide layer 15.
[0067] Step S104, as follows Figure 6f As shown, the exposed surface of the drift layer 11 is subjected to thermal oxidation treatment to form the first insulating layer 16.
[0068] For example, steps S103 and S104 can be performed simultaneously.
[0069] Step S105, as follows Figure 6g As shown, a gate electrode 14 is formed on the side of each gate oxide layer 15 away from the stacked structure.
[0070] For example, the material of the gate electrode 14 may be polycrystalline silicon, which is not limited here.
[0071] Step S106, as follows Figure 6h As shown, a second insulating layer 17 is deposited covering the outer wall and upper surface of the gate electrode 14.
[0072] For example, the second insulating layer 17 may be formed of at least one of silicon oxide or silicon nitride, without limitation herein.
[0073] Optionally, such as Figure 6i As shown, the nitride layer 31 located on the source region 13 is removed.
[0074] Step S107, as follows Figure 6j As shown, a source electrode 18 is deposited covering the first insulating isolation layer 16, the second insulating isolation layer 17, and the source region 13.
[0075] For example, the source electrode can be formed of a conductive material such as a metal.
[0076] Step S108: Deposit a drain electrode 19 on the side of the SiC semiconductor substrate 10 away from the drift layer 11, forming a structure as shown in the figure. Figure 1 The SiC MOSFET shown.
[0077] For example, the drain electrode can be formed of a conductive material such as a metal.
[0078] It should be noted that in this application, step S108 may also be formed before any of the steps S101 to S107, and this is not limited here.
[0079] Optionally, in this application, before performing thermal oxidation treatment on the two sidewalls of the stacked structure to form a gate oxide layer in step S103, the process may further include: depositing an oxide protective layer covering the surface and sidewalls of the stacked structure; using the oxide protective layer as an ion implantation masking layer to implant ions in the drift layer to form floating regions on both sides of the channel layer; and removing the oxide protective layer.
[0080] The following describes this application in detail using an N-type SiC MOSFET as an example, in conjunction with specific embodiments. It should be noted that these embodiments are for better explanation of the invention and do not limit the scope of this application. To facilitate understanding of the field-effect transistors provided in the embodiments of this application, their fabrication methods are described in detail below with reference to the accompanying drawings.
[0081] In one embodiment of this application, combined with Figures 6a-6e , Figures 7a to 7j SiC MOSFETs can be fabricated using the following method, which includes the following steps:
[0082] Step S201, as follows Figure 6a As shown, a drift layer 11 is epitaxially formed on a SiC semiconductor substrate 10.
[0083] Step S202, as follows Figure 6b As shown, a channel layer 12' is epitaxially grown on the drift layer 11.
[0084] Step S203, as follows Figure 6c As shown, N-type ions are implanted into the region near the surface of the channel layer 12' to form the source region 13.
[0085] Step S204, as Figure 6d As shown, a nitride layer 31 is formed on the channel layer 12'.
[0086] Step S205, as follows Figure 6e As shown, the channel layer 12' and the nitride layer 31 are etched to form the fin-shaped channel layer 12 and the source region 13 located on the fin-shaped channel layer 12, while retaining the nitride layer 31 located on the source region 13.
[0087] Step S206, as follows Figure 7a As shown, an oxide protective layer 32 covers the surface and sidewalls of the laminated structure.
[0088] For example, the oxide protective layer 32 can be made of silicon dioxide. The function of the oxide protective layer 32 is to prevent the subsequent floating area from spreading below the fin channel layer 12.
[0089] Step S207, as follows Figure 7b As shown, P-type ions are injected into the drift layer 11 using the oxide protective layer 32 as an ion implantation masking layer, thereby forming floating regions 20 on both sides of the fin channel layer 12.
[0090] Using oxide protective layer 32 as an ion implantation masking layer can save a mask plate used to prepare the floating region.
[0091] Step S208, as follows Figure 7c As shown, the oxide protective layer 32 is removed.
[0092] Step S209, as follows Figure 7d As shown, the fin channel layer 12 and the source region 13 are stacked structures. The two sidewalls of the stacked structure are thermally oxidized to form the gate oxide layer 15, and the exposed surface of the drift layer 11 is thermally oxidized to form the first insulating isolation layer 16.
[0093] Step S210, as follows Figure 7e As shown, a gate electrode 14 is formed on the side of each gate oxide layer 15 away from the stacked structure.
[0094] Step S211, as follows Figure 7fAs shown, a second insulating layer 17 is deposited covering the outer wall and upper surface of the gate electrode 14.
[0095] Step S212, as follows Figure 7g As shown, a groove is formed that penetrates the first insulating isolation layer 16 and part of the floating area 20.
[0096] Step S213, as follows Figure 7h As shown, the groove is filled with ohmic contact portion 21.
[0097] Step S214, as follows Figure 7i As shown, the nitride layer 31 located on the source region 13 is removed.
[0098] Step S215, as follows Figure 7j As shown, a source electrode 18 is deposited covering the first insulating isolation layer 16, the second insulating isolation layer 17, and the source region 13.
[0099] Step S216: Deposit a drain electrode 19 on the side of the SiC semiconductor substrate 10 away from the drift layer 11, forming a structure as shown in Figure 19. Figure 3 The SiC MOSFET shown.
[0100] In another embodiment of this application, combined with Figures 6a-6e , Figures 8a to 8k SiC MOSFETs can be fabricated using the following method, which includes the following steps:
[0101] Step S301, as follows Figure 6a As shown, a drift layer 11 is epitaxially formed on a SiC semiconductor substrate 10.
[0102] Step S302, as follows Figure 6b As shown, a channel layer 12' is epitaxially grown on the drift layer 11.
[0103] Step S303, as follows Figure 6c As shown, N-type ions are implanted into the region near the surface of the channel layer 12' to form the source region 13.
[0104] Step S304, as Figure 6d As shown, a nitride layer 31 is formed on the channel layer 12'.
[0105] Step S305, as follows Figure 6e As shown, the channel layer 12' and the nitride layer 31 are etched to form the fin-shaped channel layer 12 and the source region 13 located on the fin-shaped channel layer 12, while retaining the nitride layer 31 located on the source region 13.
[0106] Step S306, as follows Figure 8a As shown, an oxide protective layer 32 covers the surface and sidewalls of the laminated structure.
[0107] Step S307, as follows Figure 8b As shown, at least one photoresist material blocking portion 33 is formed on each of the drift layers 11 on both sides of the oxide protective layer 32.
[0108] In practical implementation, the number of photoresist material blocking portions 33 on each side of the stacked structure can be determined according to the number of floating areas to be formed on that side of the stacked structure. For example, if n floating areas need to be formed on that side of the stacked structure, then n-1 photoresist material blocking portions 33 need to be formed on that side, where n is an integer greater than 1.
[0109] Step S308, as Figure 8c As shown, P-type ions are injected into the drift layer using the oxide protective layer 32 and the photoresist material blocking portion 33 as ion implantation masking layers, thereby forming at least two floating regions 20 on both sides of the fin channel layer 12.
[0110] Step S309, as Figure 8d As shown, the photoresist material blocking part and oxide protective layer 32 are removed.
[0111] Step S310, as follows Figure 8e As shown, the fin channel layer 12 and the source region 13 are stacked structures. The two sidewalls of the stacked structure are thermally oxidized to form the gate oxide layer 15, and the exposed surface of the drift layer 11 is thermally oxidized to form the first insulating isolation layer 16.
[0112] Step S311, as follows Figure 8f As shown, a gate electrode 14 is formed on the side of each gate oxide layer 15 away from the stacked structure.
[0113] Step S312, as follows Figure 8g As shown, a second insulating layer 17 is deposited covering the outer wall and upper surface of the gate electrode 14.
[0114] Step S313, as follows Figure 8h As shown, a groove is formed at a location corresponding to the area between the adjacent floating areas, penetrating the first insulating isolation layer and part of the drift layer.
[0115] Step S314, as follows Figure 8i As shown, the groove is filled with Schottky contact portion 22.
[0116] Step S315, as follows Figure 8j As shown, the nitride layer 31 located on the source region 13 is removed.
[0117] Step S316, as follows Figure 8k As shown, a source electrode 18 is deposited covering the first insulating isolation layer 16, the second insulating isolation layer 17, and the source region 13.
[0118] Step S317: Deposit a drain electrode 19 on the side of the SiC semiconductor substrate 10 away from the drift layer 11, forming a structure as shown in Figure 19. Figure 4 The SiC MOSFET shown.
[0119] The SiC MOSFET provided in this embodiment has its gate electrode 14 located on both sides of the fin channel layer 12, thus making it a FinFET. Placing the gate electrode 14 on both sides of the fin channel layer 12 helps reduce the width of the fin channel layer 12, facilitating global inversion and forming a larger carrier channel within it. This allows most carriers in the SiC MOSFET to travel through the electron channels formed by the fin channel layer 12, reducing the number of carriers traveling at the edge of the gate oxide layer 15. This significantly improves channel mobility and enhances the reliability of the gate oxide layer 15. Furthermore, a floating region 20 is provided in the drift layer 11 of this SiC MOSFET, which weakens the electric field strength below the gate oxide layer 15, protecting it and significantly improving the gate reliability of the device. Additionally, this application integrates a Schottky barrier diode inside the SiC MOSFET, preventing bipolar degradation and improving reverse conduction and switching characteristics.
[0120] Accordingly, this application also provides an integrated circuit, which may include a circuit board and any of the SiC MOSFETs provided in the above embodiments of this application, wherein the SiC MOSFET is disposed on the circuit board. Since the principle by which this electronic circuit solves the problem is similar to that of the aforementioned SiC MOSFET, the implementation of this electronic circuit can refer to the implementation of the aforementioned SiC MOSFET, and repeated details will not be described again.
[0121] Obviously, those skilled in the art can make various modifications and variations to this application without departing from the spirit and scope of this application. Therefore, if such modifications and variations fall within the scope of the claims of this application and their equivalents, this application also intends to include such modifications and variations.
Claims
1. A SiC Metal-Oxide-Semiconductor Field-Effect Transistor (MOSFET), characterized by, include: SiC semiconductor substrate; A drift layer located on the SiC semiconductor substrate; Fin-shaped channel layer located on the drift layer; The source region is located on the fin channel layer; A first insulating layer located above the portion of the drift layer not covered by the fin channel layer; With the finned channel layer and the source region forming a stacked structure, the SiC MOSFET further includes: Gate electrodes located on the first insulating layer and respectively on both sides of the stacked structure; The gate oxide layer located between the gate electrode and the stacked structure; A second insulating layer covering the outer wall and upper surface of the gate electrode; A source electrode covers the first insulating isolation layer, the second insulating isolation layer, and the source region; the channel layer and the source electrode are not in direct contact. The drain electrode is located on the side of the SiC semiconductor substrate away from the drift layer; The SiC MOSFET further includes floating regions located in the drift layer and on both sides of the fin channel layer. The surface of the floating region facing the source electrode does not exceed the plane of the surface of the channel layer facing the drift layer. The floating region is located on the side of the gate electrode facing the drift layer. The first insulating isolation layer extends continuously on the surface of the floating region and isolates the floating region from the source electrode.
2. The SiC MOSFET as described in claim 1, characterized in that, The gate electrode is made of polycrystalline silicon.
3. A method of fabricating a SiC MOSFET, characterized by, include: A drift layer is epitaxially formed on a SiC semiconductor substrate; A fin-shaped channel layer and a source region located on the fin-shaped channel layer are formed on the drift layer; Using the fin-shaped channel layer and the source region as a stacked structure, thermal oxidation treatment is performed on the two sidewalls of the stacked structure to form a gate oxide layer; The exposed surface of the drift layer is subjected to thermal oxidation treatment to form a first insulating layer; A gate electrode is formed on the side of each gate oxide layer away from the stacked structure; A second insulating layer is deposited covering the outer wall and upper surface of the gate electrode; A source electrode is deposited covering the first insulating isolation layer, the second insulating isolation layer, and the source region; the channel layer and the source electrode are not in direct contact. A drain electrode is deposited on the side of the SiC semiconductor substrate away from the drift layer; Before thermally oxidizing the two sidewalls of the stacked structure to form a gate oxide layer, the method further includes: An oxide protective layer is deposited covering the surface and sidewalls of the stacked structure; Using the oxide protective layer as an ion implantation masking layer, ions are implanted in the drift layer to form floating regions on both sides of the fin channel layer. Remove the oxide protective layer; wherein the surface of the floating region facing the source electrode does not exceed the plane of the surface of the channel layer facing the drift layer, the floating region is located on the side of the gate electrode facing the drift layer, the first insulating isolation layer extends continuously on the surface of the floating region, and the first insulating isolation layer isolates the floating region and the source electrode.
4. The production method according to claim 3, wherein A finned channel layer and a source region located on the finned channel layer are formed on the drift layer, including: A channel layer is epitaxially grown on the drift layer; Ions are implanted into the region of the channel layer near the surface to form a source region; A nitride layer is formed on the channel layer; The channel layer and the nitride layer are etched to form a fin channel layer and the source region located on the fin channel layer, while retaining the nitride layer located on the source region; The preparation method further includes: after depositing an isolation oxide layer covering the outer wall and upper surface of the gate electrode and the upper surface of the drift layer, removing the nitride layer located on the source region.
5. The production method according to claim 3, wherein After depositing an oxide protective layer covering the surface and sidewalls of the stacked structure, the process further includes: At least one photoresist material blocking portion is formed on each of the drift layers on both sides of the oxide protective layer; Using the oxide protective layer as an ion implantation masking layer, ions are implanted in the drift layer to form floating regions on both sides of the fin channel layer, including: Ions are implanted into the drift layer using the oxide protective layer and the photoresist material blocking portion as ion implantation masking layers, forming at least two floating regions on both sides of the fin channel layer; the photoresist material blocking portion is then removed.
6. An integrated circuit, characterized by It includes a circuit board and a SiC MOSFET disposed on the circuit board; the SiC MOSFET is the SiC MOSFET as described in claim 1 or 2, or the SiC MOSFET is formed using the fabrication method described in any one of claims 3-5.
Citation Information
Patent Citations
Insulated gate semiconductor device and method for manufacturing same
CN103875076A
Semiconductor device
CN108140674A
Trench type SiC device
CN111627983A