Display panel and method for manufacturing the same

CN116782697BActive Publication Date: 2024-10-18MIANYANG HKC OPTOELECTRONICS TECH CO LTD +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310741419.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-06-20
Publication Date
2024-10-18
Estimated Expiration
2043-06-20

AI Technical Summary

Technical Problem

Existing OLED display panels are prone to damage the anode or leave small particles during the pixel patterning process, causing display defects and affecting yield and display effects.

Method used

A buffer layer is provided on the anode, and a multi-layer structure is formed on the pixel defining layer. A first buffer layer and a second buffer layer are respectively provided for each pixel bit. The thickness difference is between one quarter and one time, so as to avoid pixel When removing the layer, the anode is scraped directly to ensure the cleanliness of the removal process.

Benefits of technology

It effectively avoids damage to the anode and display defects during pixel patterning, and improves the yield and display effect of the display panel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116782697B_ABST
    Figure CN116782697B_ABST
Patent Text Reader

Abstract

The present application provides a display panel and a method for preparing the same, the method comprising: providing a liner, the liner comprising a substrate, an anode and a pixel defining layer disposed on the substrate, the pixel defining layer being provided with a partition structure; the pixel defining layer comprising a first pixel position, a second pixel position and a third pixel position; forming a first buffer layer at the second pixel position, and forming a second buffer layer having a thickness greater than that of the first buffer layer at the third pixel position; arranging and patterning the first pixel layer at the pixel defining layer; removing the first pixel layer and the first buffer layer outside the first pixel position; arranging and patterning the second pixel layer at the pixel defining layer; removing the second pixel layer and the second buffer layer outside the second pixel position; arranging and patterning the third pixel layer at the pixel defining layer; removing the third pixel layer outside the third pixel position. The present application solves the problem that the existing display panel is prone to damage to the anode during pixel patterning or causes display defects to the pixel after patterning.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display technology, and in particular to a display panel and a method for preparing the same. Background Art

[0002] At present, OLED (Organic Light-Emitting Diode), also known as organic electric laser display and organic light-emitting semiconductor, is used to form display devices in many electronic devices. The deposition of organic light-emitting materials of OLED uses a fine metal mask (FMM) to deposit red, green and blue organic light-emitting materials, but this production method has the problem of high FMM prices, which leads to higher costs, and the resolution will be subject to certain limitations. In order to improve resolution and reduce costs, the industry has begun to use photolithography technology to pattern the manufacture of organic light-emitting material layers, but this method requires deposition and photolithography patterning of organic light-emitting materials three times. Each time the organic light-emitting material is patterned, the organic light-emitting material on the anode needs to be etched clean, which will damage the surface of the anode, or leave small particles on the surface of the anode, causing other sub-pixels to have larger display defects when evaporated, thereby affecting the yield and display effect. Summary of the invention

[0003] The embodiment of the present application provides a display panel and a method for preparing the same. A buffer layer is provided at the anode, and a pixel layer is fabricated on the buffer layer. When the pixel layer is removed, the anode will not be directly contacted, thereby solving the problem that the anode is easily damaged during pixel patterning or display defects are caused to the pixels after patterning in the existing display panel.

[0004] The present invention is implemented as follows: a method for preparing a display panel, comprising:

[0005] A liner is provided, the liner comprising a substrate with a driving circuit, a plurality of mutually spaced anodes disposed on the substrate, a pixel defining layer located around the anodes, and a partition structure disposed on the pixel defining layer; the pixel defining layer comprises a first pixel position, a second pixel position, and a third pixel position spaced from each other;

[0006] forming a first buffer layer at the anode corresponding to the second pixel position, and forming a second buffer layer at the anode corresponding to the third pixel position, wherein the thickness of the second buffer layer is greater than the thickness of the first buffer layer;

[0007] Disposing and patterning a first pixel layer on the pixel definition layer;

[0008] removing the first pixel layer corresponding to the second pixel position and the third pixel position, and the first buffer layer;

[0009] Disposing and patterning a second pixel layer on the pixel defining layer;

[0010] removing the second pixel layer and the second buffer layer corresponding to the first pixel position and the third pixel position;

[0011] Disposing and patterning a third pixel layer on the pixel defining layer;

[0012] The third pixel layer corresponding to the first pixel position and the second pixel position is removed.

[0013] In one embodiment, the difference between the thickness of the second buffer layer and the first buffer layer is greater than or equal to one quarter of the thickness of the first buffer layer, and less than or equal to the thickness of the first buffer layer.

[0014] In one embodiment, the step of providing and patterning a first pixel layer on the pixel defining layer comprises:

[0015] Disposing a first pixel layer on the pixel defining layer so that the first pixel layer covers the anode, the partition structure, the first buffer layer and the second buffer layer;

[0016] The first pixel layer is patterned to form a first pixel located at the first pixel position.

[0017] In one embodiment, removing the first pixel layer corresponding to the second pixel position and the third pixel position, and the first buffer layer, comprises:

[0018] forming a first anti-etching layer on the first pixel;

[0019] removing the first pixel layer corresponding to the second pixel position and the third pixel position;

[0020] removing the first buffer layer;

[0021] The first anti-corrosion layer is removed; wherein the first anti-corrosion layer and the second buffer layer are made of different materials.

[0022] In one embodiment, the step of providing and patterning a second pixel layer on the pixel defining layer comprises:

[0023] Disposing a second pixel layer on the pixel defining layer so that the second pixel layer covers the anode, the partition structure, the first pixel and the second buffer layer;

[0024] The second pixel layer is patterned to form a second pixel located at the second pixel position.

[0025] In one embodiment, removing the second pixel layer and the second buffer layer corresponding to the first pixel position and the third pixel position includes:

[0026] forming a second anti-etching layer on the second pixel;

[0027] Removing the second pixel layer corresponding to the first pixel position and the third pixel position;

[0028] removing the second buffer layer;

[0029] The second resist layer is removed.

[0030] In one embodiment, the step of providing and patterning a third pixel layer on the pixel defining layer comprises:

[0031] Disposing a third pixel layer on the pixel defining layer so that the third pixel layer covers the anode, the partition structure, the first pixel and the second pixel;

[0032] The third pixel layer is patterned to form a third pixel located at the third pixel position.

[0033] In one embodiment, removing the third pixel layer corresponding to the first pixel position and the second pixel position includes:

[0034] forming a third anti-etching layer on the third pixel;

[0035] Removing the third pixel layer corresponding to the first pixel position and the second pixel position;

[0036] The third resist layer is removed.

[0037] In one embodiment, after removing the third anti-etching layer, the method further comprises:

[0038] Setting a filling layer, wherein the filling layer covers the first pixel, the second pixel and the third pixel;

[0039] A cover plate is mounted on the filling layer or a thin film packaging layer is formed.

[0040] The beneficial effect of the preparation method of the display panel provided by the present application is that: compared with the prior art, the present application sets a first buffer layer at the anode corresponding to the second pixel position, and sets a second buffer layer at the anode corresponding to the third pixel position, and the thickness of the second buffer layer is greater than the thickness of the first buffer layer, so that after the first pixel layer is formed and patterned, the anode will not be directly scraped when the first pixel layer corresponding to the second pixel position and the third pixel position is removed, and after the second pixel layer is formed and patterned, the anode will not be directly scraped when the second pixel layer corresponding to the first pixel position and the third pixel position is removed, thereby effectively avoiding damage to the anode during pixel patterning, or causing display defects to the pixel after the pixel is patterned, which can greatly improve the yield and display effect of the display panel.

[0041] An embodiment of the present application also provides a display panel, which is prepared according to the method described in any of the above embodiments, and includes a substrate, a pixel defining layer and a partition structure, wherein the substrate has a driving circuit; the pixel defining layer is arranged on the substrate, and the pixel defining layer includes a plurality of pixel positions spaced apart from each other, and each of the pixel positions is provided with a pixel; the partition structure includes a conductive first partition layer and a non-conductive second partition layer stacked on the pixel defining layer; the pixel includes an organic light-emitting layer, a cathode and an encapsulation layer stacked, the organic light-emitting layer and the partition structure are spaced apart from each other, and the cathode is connected to the first partition layer of the adjacent partition structure; there are three types of the plurality of pixel positions, namely a first pixel position, a second pixel position and a third pixel position, and the light-emitting colors of the organic light-emitting layers of the pixels provided at the first pixel position, the second pixel position and the third pixel position are different.

[0042] The beneficial effect of the display panel provided by the present application lies in that: it is prepared by the above-mentioned preparation method. Compared with the prior art, the present application sets a first buffer layer at the anode corresponding to the second pixel position, and sets a second buffer layer at the anode corresponding to the third pixel position, and the thickness of the second buffer layer is greater than the thickness of the first buffer layer. In this way, after the first pixel layer is formed and patterned, the anode will not be directly scraped when the first pixel layer corresponding to the second pixel position and the third pixel position is removed, and after the second pixel layer is formed and patterned, the anode will not be directly scraped when the second pixel layer corresponding to the first pixel position and the third pixel position is removed, thereby effectively avoiding damage to the anode during pixel patterning, or causing display defects to the pixel after the pixel is patterned, which can greatly improve the yield and display effect of the display panel. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] Figure 1 is a flow chart of a method for preparing a display panel provided in an embodiment of the present application;

[0044] Figure 2 is a device diagram after completing the operation of step S101;

[0045] Figure 3 is a device diagram after the operation of step S102 is completed;

[0046] Figure 4 yes Figure 1 Specific flow diagram of step S101;

[0047] Figure 5 yes Figure 1 Specific flow diagram of step S103;

[0048] Figure 6 is the device diagram after completing the operation of step S1032;

[0049] Figure 7 yes Figure 1 Specific flow diagram of step S104;

[0050] Figure 8-1 is the device diagram after completing the operation of step S1041;

[0051] Figure 8-2 is the device diagram after completing the operation of step S1042;

[0052] Figure 8-3 is the device diagram after completing the operation of step S1043;

[0053] Figure 8-4 is the device diagram after completing the operation of step S1044;

[0054] Fig. 9 yes Figure 1 Specific flow diagram of step S105;

[0055] Fig.10 is the device diagram after completing step S1052;

[0056] Fig.11 yes Figure 1 Specific flow diagram of step S106;

[0057] Figure 12-1 is the device diagram after completing the operation of step S1061;

[0058] Figure 12-2 is the device diagram after the operation of step S1062 is completed;

[0059] Figure 12-3 is the device diagram after completing the operation of step S1063;

[0060] Figure 12-4 is the device diagram after completing step S1064;

[0061] Fig.13 yes Figure 1 Specific flow diagram of step S107;

[0062] Fig.14 is the device diagram after the operation of step S1072 is completed;

[0063] Fig.15 yes Figure 1 Specific flow diagram of step S108;

[0064] Figure 16-1 is the device diagram after completing step S1081;

[0065] Figure 16-2 is the device diagram after completing the operation of step S1082;

[0066] Figure 16-3 is the device diagram after completing the operation of step S1083;

[0067] Fig.17 It is a schematic diagram of the structure of the display panel provided in the embodiment of the present application.

[0068] Reference numerals: 100, liner; 1, substrate; 10, drive circuit;

[0069] 2. Anode; 701. Organic light-emitting layer; 702. Cathode; 703. Encapsulation layer;

[0070] 3. Pixel defining layer; 31. First pixel position; 32. Second pixel position; 33. Third pixel position;

[0071] 4. Partition structure; 41. First partition layer; 42. Second partition layer;

[0072] 5. The first buffer layer; 6. The second buffer layer;

[0073] 7. first pixel layer; 70. first pixel; 71. first anti-etching layer;

[0074] 8. second pixel layer; 80. second pixel; 81. second anti-etching layer;

[0075] 9. third pixel layer; 90. third pixel; 91. third anti-etching layer;

[0076] 200, filling layer; 300, cover plate. DETAILED DESCRIPTION

[0077] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.

[0078] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it can be directly on the other element or indirectly on the other element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.

[0079] It should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0080] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0081] It should also be noted that, in the embodiments of the present application, the same figure mark is used to represent the same component or the same part. For the same parts in the embodiments of the present application, the figure may only mark one of the parts or components as an example. It should be understood that the figure mark also applies to other identical parts or components.

[0082] The embodiments of the present application provide a display panel and a method for manufacturing the same, which solve the problem that the anode of the conventional display panel is easily damaged during pixel patterning or causes display defects to the pixels after patterning.

[0083] refer to Figure 1 The method for preparing a display panel provided in the embodiment of the present application comprises the following steps:

[0084] S101. Provide a backing plate 100, which includes a substrate 1 with a driving circuit 10, a plurality of mutually spaced anodes 2 arranged on the substrate 1, a pixel defining layer 3 located around the anodes 2, and a partition structure 4 arranged on the pixel defining layer 3; the pixel defining layer 3 includes a first pixel position 31, a second pixel position 32, and a third pixel position 33 spaced from each other.

[0085] Figure 2 This is a diagram of the device after the operation of step S101 is completed.

[0086] S102 , forming a first buffer layer 5 at the anode 2 corresponding to the second pixel position 32 , and forming a second buffer layer 6 at the anode 2 corresponding to the third pixel position 33 , wherein the thickness of the second buffer layer 6 is greater than that of the first buffer layer 5 .

[0087] Figure 3 It is a device diagram after completing step S102. The first buffer layer 5 and the second buffer layer 6 can be made of the same material, which can avoid changing the material back and forth and improve the production efficiency of the first buffer layer 5 and the second buffer layer 6. Specifically, the material of the first buffer layer 5 and the second buffer layer 6 can be a material similar to photoresist, which is easy to remove. When removing, dry etching or wet etching can be used, and the etching process conditions are milder, and it is not easy to damage the anode 2 or leave residue, thereby ensuring that the original shape of the surface of the anode 2 remains unchanged.

[0088] There are many ways to prepare the first buffer layer 5 and the second buffer layer 6, such as deposition or spraying, which are not specifically limited in the embodiments of the present application. When preparing the first buffer layer 5 and the second buffer layer 6, it should be noted that the anode 2 corresponding to the second pixel position 32 and the third pixel position 33 must be completely covered, so as to ensure that the anode 2 will not be etched when the organic light-emitting material is removed after the patterned pixels, and the anode 2 will not be damaged. The first buffer layer 5 and the second buffer layer 6 in the embodiment of the present application are formed on the anode 2 and extend to contact the adjacent partition structure 4, so that the area of ​​the first buffer layer 5 and the area of ​​the second buffer layer 6 will be much larger than the area of ​​the corresponding anode 2, which can better protect the anode 2 from damage when the organic light-emitting material is removed after the patterned pixels, and can avoid the problem of display defects caused by the unclean removal of the organic light-emitting material on the anode 2.

[0089] S103 , disposing and patterning a first pixel layer 7 on the pixel defining layer 3 .

[0090] S104 , removing the first pixel layer 7 and the first buffer layer 5 corresponding to the second pixel position 32 and the third pixel position 33 .

[0091] S105 , disposing and patterning a second pixel layer 8 on the pixel defining layer 3 .

[0092] S106 , removing the second pixel layer 8 and the second buffer layer 6 corresponding to the first pixel position 31 and the third pixel position 33 .

[0093] S107 , disposing and patterning a third pixel layer 9 on the pixel defining layer 3 .

[0094] S108 , remove the third pixel layer 9 corresponding to the first pixel position 31 and the second pixel position 32 .

[0095] In the process of preparing the display panel according to the preparation method of the embodiment of the present application, after patterning the first pixel layer 7, when removing the first pixel layer 7 corresponding to the second pixel position 32 and the third pixel position 33, since the second pixel position 32 is provided with the first buffer layer 5 and the third pixel position 33 is provided with the second buffer layer 6, no damage is caused to the anode 2, and the first pixel layer 7 to be removed is in contact with the first buffer layer 5 and the second buffer layer 6, so the first pixel layer 7 can be removed more cleanly. After patterning the second pixel layer 8, when removing the second pixel layer 8 corresponding to the first pixel position 31 and the third pixel position 33, since the third pixel position 33 is provided with the second buffer layer 6, no damage is caused to the anode 2, and the second pixel layer 8 to be removed is in contact with the second buffer layer 6, so the second pixel layer 8 can be removed more cleanly.

[0096] It should be noted that, in the embodiment of the present application, after removing the first pixel layer 7 corresponding to the second pixel position 32 and the third pixel position 33, before setting the second pixel layer 8, it is necessary to first remove the first buffer layer 5 set at the second pixel position 32 to expose the anode 2 at the second pixel position 32. Since the first buffer layer 5 and the second buffer layer 6 are made of the same material, a portion of the second buffer layer 6 will also be removed when the first buffer layer 5 is removed. In order to avoid that the anode 2 at the third pixel position 33 cannot be well protected after a portion of the second buffer layer 6 is removed, it is necessary to set the thickness of the second buffer layer 6 to be greater than the thickness of the first buffer layer 5, so that after a portion of the second buffer layer 6 is removed, the remaining portion can still play a role in protecting the anode 2. However, considering the material cost of making the buffer layer and the difficulty of removing the buffer layer, the difference between the thickness of the second buffer layer 6 and the thickness of the first buffer layer 5 is particularly important.

[0097] If the difference between the thickness of the second buffer layer 6 and the thickness of the first buffer layer 5 is too large, that is, the thickness of the second buffer layer 6 exceeds the thickness of the first buffer layer 5 by too much, for example, the thickness of the second buffer layer 6 is twice the thickness of the first buffer layer 5, then more materials will be needed to make the first buffer layer 5 and the second buffer layer 6, the setting time will also be longer, the overall production cost will increase, and the time and difficulty required to remove the second buffer layer 6 will also be greater, thereby reducing the production efficiency of the display panel.

[0098] If the difference between the thickness of the second buffer layer 6 and the thickness of the first buffer layer 5 is too small, that is, the thickness of the second buffer layer 6 exceeds the thickness of the first buffer layer 5 by too little, for example, the distance by which the thickness of the second buffer layer 6 exceeds the thickness of the first buffer layer 5 is one-fifth of the thickness of the first buffer layer 5, then after removing the first buffer layer 5, the thickness of the remaining part of the second buffer layer 6 is only one-fifth of the thickness of the first buffer layer 5. When the second buffer layer 6 is removed, the anode 2 may be etched due to its too small thickness, or the etching difficulty may increase due to the too small thickness of the second buffer layer 6, thereby reducing the preparation efficiency of the display panel.

[0099] Therefore, reference Figure 3 , the difference between the thickness of the second buffer layer 6 and the first buffer layer 5 in the embodiment of the present application is greater than or equal to one quarter of the thickness of the first buffer layer 5, and less than or equal to the thickness of the first buffer layer 5. In this way, not only will the manufacturing cost of the buffer layer not be increased too much, but also after the first buffer layer 5 is removed, the remaining part of the second buffer layer 6 can also well protect the anode 2, and at the same time, the difficulty of removing the remaining part of the second buffer layer 6 will not increase, and will not have a negative impact on the manufacturing efficiency of the display panel.

[0100] For further reference, Figure 4 The above step S101 may specifically include the following steps:

[0101] S1011 , providing a substrate 1 with a driving circuit 10 .

[0102] S1012 , forming a plurality of mutually spaced anodes 2 and a pixel defining layer 3 located around the anodes 2 on the substrate 1 .

[0103] The pixel defining layer 3 includes a first pixel position 31 , a second pixel position 32 and a third pixel position 33 which are spaced apart from each other.

[0104] S1013 , depositing a first partition layer 41 on the substrate 1 , so that the first partition layer 41 covers the pixel defining layer 3 and the anode 2 .

[0105] S1014 , depositing a second isolation layer 42 on the first isolation layer 41 .

[0106] S1015 , disposing and patterning a resist on the second barrier layer 42 .

[0107] The resist is disposed on the second isolation layer 42. The resist is a positive resist or a negative resist. The positive resist includes a portion of the resist, which, when exposed to light radiation, after the pattern is written into the resist using light radiation, the portion irradiated by light is soluble in the resist developer applied to the resist, and the portion not irradiated by light is left to form a resist pattern. The negative resist includes a portion of the resist, which, when exposed to light radiation, after the pattern is written into the resist using light radiation, the portion not irradiated by light will be dissolved in the resist developer applied to the resist, and the portion irradiated by light is insoluble in the resist developer applied to the resist to form a resist pattern. The chemical composition of the resist determines whether the resist is a positive resist or a negative resist. The resist is patterned to form pixel openings corresponding to the first pixel position 31, the second pixel position 32, and the third pixel position 33. Patterning is one of photolithography, digital lithography or laser ablation.

[0108] S1016 , removing the pixel opening portion of the second partition layer 42 and the first partition layer 41 corresponding to the anode 2 .

[0109] The second partition layer 42 exposed by the pixel opening may be removed by a dry etching process, and the first partition layer 41 exposed by the pixel opening may be removed by a wet etching process.

[0110] S1017, remove the resist to obtain a partition structure 4.

[0111] After removing the pixel opening portions of the second isolation layer 42 and the first isolation layer 41 corresponding to the anode 2, the portions of the second isolation layer 42 and the first isolation layer 41 covered by the resist form an isolation structure 4, so the remaining resist on the second isolation layer 42 can be removed to obtain the isolation structure 4.

[0112] Specifically, the specific implementation steps of the above step S102 may be: using a mask to form a first buffer layer 5 on the anode 2 corresponding to the second pixel position 32, and then using another mask to form a second buffer layer 6 on the anode 2 corresponding to the third pixel position 33.

[0113] The specific implementation steps of the above-mentioned step S102 may also be: using a mask template to simultaneously set buffer material on the anode 2 corresponding to the second pixel position 32 and the anode 2 corresponding to the third pixel position 33, so as to form a first buffer layer 5 at the anode 2 corresponding to the second pixel position 32, and form a part of the second buffer layer 6 at the anode 2 corresponding to the third pixel position 33; and then using another mask template to continue to set buffer material on a part of the second buffer layer 6, so as to form a second buffer layer 6 at the anode 2 corresponding to the third pixel position 33.

[0114] For further reference, Figure 5, the above step S103 may specifically include the following steps:

[0115] S1031 , disposing a first pixel layer 7 on the pixel defining layer 3 , so that the first pixel layer 7 covers the anode 2 , the partition structure 4 , the first buffer layer 5 and the second buffer layer 6 .

[0116] It should be noted that the first pixel layer 7 includes an organic light-emitting layer 701, a cathode 702 and an encapsulation layer 703 which are stacked, and the light-emitting color of the organic light-emitting layer 701 of the first pixel layer 7 can be red. Specifically, the specific operation mode of setting the first pixel layer 7 is: firstly, an organic light-emitting layer 701 is formed on the pixel defining layer 3, so that the organic light-emitting layer 701 covers the anode 2, the partition structure 4, the first buffer layer 5 and the second buffer layer 6, and the organic light-emitting layer 701 at the corresponding position of the anode 2 and the partition structure 4 are spaced from each other; then, a cathode 702 is formed on the organic light-emitting layer 701, and the cathode 702 at the corresponding position of the anode 2 is connected to the partition structure 4; finally, an encapsulation layer 703 is formed on the cathode 702, and the encapsulation layer 703 extends along the side wall of the partition structure 4.

[0117] The organic light emitting layer 701 is formed by evaporation deposition, specifically by depositing OLED materials (including a hole injection layer (HIL), a hole transport layer (HTL), an emission layer (EML) and an electron transport layer (ETL)).

[0118] The cathode 702 is formed by evaporation deposition, and the partition structure 4 limits the deposition angle for each of the OLED material and the cathode 702 , that is, provides a shadowing effect during evaporation deposition, so that the OLED material does not contact the partition structure 4 , and the cathode 702 contacts the partition structure 4 .

[0119] S1032 , patterning the first pixel layer 7 to form a first pixel 70 located at the first pixel position 31 .

[0120] Figure 6 is a device diagram after the step S1032 operation is completed, wherein the first pixel 70 is a red pixel.

[0121] refer to Figure 7 , the above step S104 may specifically include the following steps:

[0122] S1041 , forming a first anti-etching layer 71 in the first pixel 70 .

[0123] Figure 8-11 is a device diagram after the step S1041 is completed. The material for making the first anti-etching layer 71 is an anti-etching agent. The first anti-etching layer 71 is made on the encapsulation layer 703 of the first pixel 70.

[0124] S1042 , remove the first pixel layer 7 corresponding to the second pixel position 32 and the third pixel position 33 .

[0125] Figure 8-2 3 is a device diagram after completing step S1042. The first pixel layer 7 corresponding to the second pixel position 32 and the third pixel position 33 can be removed by a dry etching process. Since the first pixel 70 is formed with the first anti-etching layer 71, the first pixel 70 will not be damaged when the first pixel layer 7 corresponding to the second pixel position 32 and the third pixel position 33 is etched.

[0126] S1043 , removing the first buffer layer 5 .

[0127] Figure 8-3 The device diagram after step S1043 is completed. After the first pixel 70 is completed, the second pixel 80 needs to be manufactured. Therefore, the first buffer layer 5 needs to be removed to expose the anode 2 corresponding to the second pixel position 32 so as to prepare for the manufacturing of the second pixel 80.

[0128] S1044, removing the first anti-etching layer 71; wherein the first anti-etching layer 71 and the second buffer layer 6 are made of different materials.

[0129] Figure 8-4 This is a diagram of the device after the operation of step S1044 is completed.

[0130] It should be noted that the removal of the first anti-etching layer 71 can be carried out by dry etching or stripping. If the first anti-etching layer 71 is made of the same material as the first buffer layer 5 and the second buffer layer 6, the second buffer layer 6 will be removed together when the first anti-etching layer 71 is removed. In this way, the anode 2 corresponding to the third pixel position 33 cannot be protected by the second buffer layer 6, and the second pixel layer 8 will directly cover the anode 2 corresponding to the third pixel position 33. When the second pixel layer 8 corresponding to the third pixel position 33 is removed, the anode 2 will inevitably be etched, causing damage to the anode 2, and sometimes it is easy to leave organic light-emitting materials that have not been removed cleanly on the anode 2, causing display defects of the pixel set at the third pixel position 33. Therefore, it is necessary to set the materials of the first anti-etching layer 71 and the second buffer layer 6 to be different in order to perform the operation of the above step S1044.

[0131] In some embodiments, after completing the above step S1043, step S1044 may not be performed, that is, the first anti-etching layer 71 is left at the first pixel position 31, and when the second pixel layer 8 is set next, the second pixel layer 8 corresponding to the first pixel position 31 is set on the first anti-etching layer 71, and the first anti-etching layer 71 is removed together when the second buffer layer 6 is removed. In this case, the first anti-etching layer 71 and the first buffer layer 5 and the second buffer layer 6 can be made of the same material.

[0132] Test Fig. 9 , the above step S105 may specifically include the following steps:

[0133] S1051 , disposing a second pixel layer 8 on the pixel defining layer 3 , so that the second pixel layer 8 covers the anode 2 , the partition structure 4 , the first pixel 70 and the second buffer layer 6 .

[0134] It should be noted that the second pixel layer 8 includes an organic light-emitting layer 701, a cathode 702 and an encapsulation layer 703 which are stacked, and the light-emitting color of the organic light-emitting layer 701 of the second pixel layer 8 can be green. Specifically, the specific operation mode of setting the second pixel layer 8 is as follows: firstly, an organic light-emitting layer 701 is formed on the pixel defining layer 3, so that the organic light-emitting layer 701 covers the anode 2, the partition structure 4, the first pixel 70 and the second buffer layer 6, and the organic light-emitting layer 701 at the corresponding position of the anode 2 and the partition structure 4 are spaced from each other; then, a cathode 702 is formed on the organic light-emitting layer 701, and the cathode 702 at the corresponding position of the anode 2 is connected to the partition structure 4; finally, an encapsulation layer 703 is formed on the cathode 702, and the encapsulation layer 703 extends along the side wall of the partition structure 4.

[0135] S1052 , patterning the second pixel layer 8 to form a second pixel 80 located at the second pixel position 32 .

[0136] Fig.10 is a device diagram after the step S1052 operation is completed, wherein the second pixel 80 is a green pixel.

[0137] refer to Fig.11 , the above step S106 may specifically include the following steps:

[0138] S1061 , forming a second anti-etching layer 81 in the second pixel 80 .

[0139] Figure 12-1 The device diagram after the step S1061 is completed. The second anti-etching layer 81 is made of a resist. The second anti-etching layer 81 is made on the encapsulation layer 703 of the second pixel 80.

[0140] S1062 , remove the second pixel layer 8 corresponding to the first pixel position 31 and the third pixel position 33 .

[0141] Figure 12-2 3 is a device diagram after completing step S1062. The second pixel layer 8 corresponding to the first pixel position 31 and the third pixel position 33 can be removed by a dry etching process. Since the second pixel 80 is formed with the second anti-etching layer 81, the second pixel 80 will not be damaged when the second pixel layer 8 corresponding to the first pixel position 31 and the third pixel position 33 is etched.

[0142] S1063 , removing the second buffer layer 6 .

[0143] Figure 12-3 The device diagram after step S1063 is completed. After the second pixel 80 is completed, the third pixel 90 needs to be manufactured. Therefore, the second buffer layer 6 needs to be removed to expose the anode 2 corresponding to the third pixel position 33 so as to prepare for the manufacturing of the third pixel 90.

[0144] S1064 , remove the second anti-etching layer 81 .

[0145] Figure 12-4 This is a diagram of the device after the operation of step S1064 is completed.

[0146] refer to Fig.13 , the above step S107 may specifically include the following steps:

[0147] S1071 , setting a third pixel layer 9 on the pixel defining layer 3 , so that the third pixel layer 9 covers the anode 2 , the partition structure 4 , the first pixel 70 and the second pixel 80 .

[0148] It should be noted that the third pixel layer 9 includes an organic light-emitting layer 701, a cathode 702 and an encapsulation layer 703 which are stacked, and the light-emitting color of the organic light-emitting layer 701 of the third pixel layer 9 can be blue. Specifically, the specific operation mode of setting the third pixel layer 9 is as follows: firstly, an organic light-emitting layer 701 is formed on the pixel defining layer 3, so that the organic light-emitting layer 701 covers the anode 2, the partition structure 4, the first pixel 70 and the second pixel 80, and the organic light-emitting layer 701 at the corresponding position of the anode 2 and the partition structure 4 are spaced from each other; then, a cathode 702 is formed on the organic light-emitting layer 701, and the cathode 702 at the corresponding position of the anode 2 is connected to the partition structure 4; finally, an encapsulation layer 703 is formed on the cathode 702, and the encapsulation layer 703 extends along the side wall of the partition structure 4.

[0149] S1072 , patterning the third pixel layer 9 to form a third pixel 90 located at the third pixel position 33 .

[0150] Fig.14 is a device diagram after the step S1072 operation is completed, wherein the third pixel 90 is a blue pixel.

[0151] refer to Fig.15 , the above step S108 may specifically include the following steps:

[0152] S1081 , forming a third anti-etching layer 91 in the third pixel 90 .

[0153] Figure 16-1 The device diagram after the step S1081 is completed. The third anti-etching layer 91 is made of a material of resist. The third anti-etching layer 91 is made on the encapsulation layer 703 of the third pixel 90.

[0154] S1082 , remove the third pixel layer 9 corresponding to the first pixel position 31 and the second pixel position 32 .

[0155] Figure 16-2 3 is a device diagram after completing the operation of step S1082. The third pixel layer 9 corresponding to the first pixel position 31 and the second pixel position 32 can be removed by a dry etching process. Since the third pixel 90 is formed with the third anti-etching layer 91, the third pixel 90 will not be damaged when the third pixel layer 9 corresponding to the first pixel position 31 and the second pixel position 32 is etched.

[0156] S1083, remove the third anti-etching layer 91.

[0157] Figure 16-3 is a device diagram after completing step S1083. After completing the manufacturing steps of the first pixel 70, the second pixel 80 and the third pixel 90, the third anti-etching layer 91 is removed, and the first pixel 70, the second pixel 80 and the third pixel 90 are exposed, thereby completing the manufacturing of the display panel. Figure 16-3 It is also a schematic diagram of the structure of a display panel prepared by the method for preparing a display panel according to an embodiment of the present application.

[0158] In some embodiments, after completing step S1083, the following steps may also be included:

[0159] A filling layer 200 is provided, and the filling layer 200 covers the first pixel 70 , the second pixel 80 , and the third pixel 90 ; a cover plate 300 is mounted on the filling layer 200 or a thin film encapsulation layer is formed.

[0160] Fig.17 3 is a device diagram after the above-mentioned operation of setting the filling layer 200 and the cover plate 300 is completed. After the above-mentioned steps of setting the filling layer 200 and the cover plate 300, the final OLED complete device can be formed. The cover plate 300 can be a glass cover plate or a plastic film made of PET material.

[0161] refer to Figure 16-3The embodiment of the present application provides a display panel, which is prepared according to the method of the above embodiment, including a substrate 1, a pixel defining layer 3 and a partition structure 4, wherein the substrate 1 has a driving circuit 10; the pixel defining layer 3 is arranged on the substrate 1, and the pixel defining layer 3 includes a plurality of pixel positions spaced apart from each other, and each pixel position is provided with a pixel; the partition structure 4 includes a conductive first partition layer 41 and a non-conductive second partition layer 42 stacked on the pixel defining layer 3; the pixel includes a stacked organic light-emitting layer 701, a cathode 702 and an encapsulation layer 703, the organic light-emitting layer 701 and the partition structure 4 are spaced apart from each other, and the cathode 702 is connected to the first partition layer 41 of the adjacent partition structure 4; there are three types of the plurality of pixel positions, namely a first pixel position 31, a second pixel position 32 and a third pixel position 33, and the light-emitting colors of the organic light-emitting layer 701 of the pixels provided with the first pixel position 31, the second pixel position 32 and the third pixel position 33 are different.

[0162] The display panel of the embodiment of the present application is prepared by the above-mentioned display panel preparation method. Since the first buffer layer 5 and the second buffer layer 6 are set in the production process, it is effectively avoided that the anode 2 is damaged when the organic light-emitting material on the anode 2 of other pixels is removed after each pixel is patterned. In addition, the problem of display defects in pixels caused by residual small particles of organic light-emitting material on the anode 2 not being removed cleanly will not occur, which greatly improves the yield and display effect of the display panel.

[0163] The above is only a specific implementation of the present application, but the protection scope of the present application is not limited thereto. Any person skilled in the art who is familiar with the present technical field can easily think of changes or substitutions within the technical scope disclosed in the present application, which should be included in the protection scope of the present application. Therefore, the protection scope of the present application should be based on the protection scope of the claims.

Claims

1. A method for preparing a display panel, characterized in that: include: A backing plate (100) is provided, the backing plate (100) comprising a substrate (1) with a driving circuit (10), a plurality of mutually spaced anodes (2) arranged on the substrate (1), a pixel defining layer (3) located around the anodes (2), and a partition structure (4) arranged on the pixel defining layer (3); the pixel defining layer (3) comprises a first pixel position (31), a second pixel position (32), and a third pixel position (33) spaced from each other; A first buffer layer (5) is formed on the anode (2) corresponding to the second pixel position (32), and a second buffer layer (6) is formed on the anode (2) corresponding to the third pixel position (33), wherein the thickness of the second buffer layer (6) is greater than the thickness of the first buffer layer (5); Arranging and patterning a first pixel layer (7) on the pixel defining layer (3); removing the first pixel layer (7) and the first buffer layer (5) corresponding to the second pixel position (32) and the third pixel position (33); Arranging and patterning a second pixel layer (8) on the pixel defining layer (3); removing the second pixel layer (8) and the second buffer layer (6) corresponding to the first pixel position (31) and the third pixel position (33); Arranging and patterning a third pixel layer (9) on the pixel defining layer (3); The third pixel layer (9) corresponding to the first pixel position (31) and the second pixel position (32) is removed.

2. The method for preparing a display panel according to claim 1, characterized in that: The difference between the thickness of the second buffer layer (6) and the first buffer layer (5) is greater than or equal to one quarter of the thickness of the first buffer layer (5), and less than or equal to the thickness of the first buffer layer (5).

3. The method for preparing a display panel according to claim 1 or 2, characterized in that: The method of arranging and patterning a first pixel layer (7) on the pixel defining layer (3) comprises: A first pixel layer (7) is arranged on the pixel defining layer (3), so that the first pixel layer (7) covers the anode (2), the partition structure (4), the first buffer layer (5) and the second buffer layer (6); The first pixel layer (7) is patterned to form a first pixel (70) located at the first pixel position (31).

4. The method for preparing a display panel according to claim 3, characterized in that: The removing of the first pixel layer (7) and the first buffer layer (5) corresponding to the second pixel position (32) and the third pixel position (33) comprises: forming a first anti-etching layer (71) on the first pixel (70); removing the first pixel layer (7) corresponding to the second pixel position (32) and the third pixel position (33); removing the first buffer layer (5); The first anti-corrosion layer (71) is removed; wherein the first anti-corrosion layer (71) and the second buffer layer (6) are made of different materials.

5. The method for preparing a display panel according to claim 4, characterized in that: The second pixel layer (8) is arranged and patterned on the pixel defining layer (3), comprising: A second pixel layer (8) is arranged on the pixel defining layer (3), so that the second pixel layer (8) covers the anode (2), the partition structure (4), the first pixel (70) and the second buffer layer (6); The second pixel layer (8) is patterned to form a second pixel (80) located at the second pixel position (32).

6. The method for preparing a display panel according to claim 5, characterized in that: The removing of the second pixel layer (8) and the second buffer layer (6) corresponding to the first pixel position (31) and the third pixel position (33) comprises: forming a second anti-etching layer (81) on the second pixel (80); removing the second pixel layer (8) corresponding to the first pixel position (31) and the third pixel position (33); removing the second buffer layer (6); The second resist layer (81) is removed.

7. The method for preparing a display panel according to claim 6, characterized in that: The method of arranging and patterning a third pixel layer (9) on the pixel defining layer (3) comprises: A third pixel layer (9) is arranged on the pixel defining layer (3), so that the third pixel layer (9) covers the anode (2), the partition structure (4), the first pixel (70) and the second pixel (80); The third pixel layer (9) is patterned to form a third pixel (90) located at the third pixel position (33).

8. The method for preparing a display panel according to claim 7, characterized in that: The removing of the third pixel layer (9) corresponding to the first pixel position (31) and the second pixel position (32) comprises: forming a third anti-etching layer (91) on the third pixel (90); removing the third pixel layer (9) corresponding to the first pixel position (31) and the second pixel position (32); The third resist layer (91) is removed.

9. The method for preparing a display panel according to claim 8, characterized in that: After removing the third anti-etching layer (91), the method further comprises: Providing a filling layer (200), wherein the filling layer (200) covers the first pixel (70), the second pixel (80) and the third pixel (90); A cover plate (300) is mounted on the filling layer (200) or a thin film encapsulation layer is formed.

10. A display panel, characterized in that: The method according to any one of claims 1 to 9 comprises: A substrate (1) having a driving circuit (10); A pixel defining layer (3) is arranged on the substrate (1), the pixel defining layer (3) comprising a plurality of pixel positions spaced apart from each other, each of the pixel positions being provided with a pixel; A partition structure (4), comprising a first conductive partition layer (41) and a second non-conductive partition layer (42) stacked on the pixel defining layer (3); The pixel comprises an organic light-emitting layer (701), a cathode (702) and an encapsulation layer (703) which are stacked, the organic light-emitting layer (701) and the partition structure (4) being spaced apart from each other, and the cathode (702) being connected to the first partition layer (41) of the adjacent partition structure (4); The plurality of pixel positions are of three types, namely a first pixel position (31), a second pixel position (32) and a third pixel position (33), and the organic light-emitting layer (701) of the pixels provided with the first pixel position (31), the second pixel position (32) and the third pixel position (33) have different light-emitting colors.

Citation Information

Patent Citations

  • OLED panel with inorganic pixel encapsulation barrier layer

    CN114514626A

  • Organic electroluminescent display device and fabrication method thereof

    US20040239238A1